A process for removing impurities in the distillation process of organic silicon monomer

By using a fixed bed reactor combined with a high boiling tower during the distillation of silicone monomer, the Pd-Ni/MoFs catalyst is used to convert ethyl hydrogen silicon into high boiling point chlorosilane, which solves the difficulty of ethyl hydrogen silicon impurities. The removal of problems improves product quality and purity and is suitable for applications in small-scale devices.

CN114853801BActive Publication Date: 2024-11-26HUBEI XINGRUI SILICON MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210468289.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-29
Publication Date
2024-11-26
Estimated Expiration
2042-04-29

AI Technical Summary

Technical Problem

During the distillation of existing silicone monomers, it is difficult to effectively remove ethyl hydrogen silicon impurities, resulting in low purity and product quality of dimethyl dichlorosilane. The existing methods consume high energy and cost high equipment, which is not conducive to Large-scale continuous production.

Method used

Using a process of combining a fixed bed reactor with a high boiling tower, the ethyl hydrogen silicon in crude dimethyl dichlorosilane is converted into high boiling point chlorosilane through a catalyst, and circulated through the condenser reflux tank, using Pd-Ni Directed removal of catalysts such as /MoFs improves the removal efficiency of ethyl silicon hydrogen and reduces the saturated partial pressure in the system.

Benefits of technology

Without increasing energy consumption and changing the monomer separation process of the existing device, the purity and product quality of dimethyl dichlorosilane are improved, the removal of ethyl hydrogen silicon is reduced, and efficient decomposition is achieved Effective, suitable for small-scale devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114853801B_ABST
    Figure CN114853801B_ABST
Patent Text Reader

Abstract

The invention discloses a process for removing impurities in a distillation process of an organosilicon monomer, and belongs to the technical field of organosilicon production. The process is that the liquid from the bottom of a high-boiling tower is used as the feed of a high-boiling tower, crude dimethyldichlorosilane is extracted through the gas phase at the top of the high-boiling tower, and high-boiling substances are extracted from the bottom of the tower. The crude dimethyldichlorosilane in the gas phase at the top of the high-boiling tower and the chlorine source material are fully mixed in a pipeline mixer and then enter a fixed bed reactor, and the hydrogen-containing silane in the crude dimethyldichlorosilane is converted into the corresponding high-boiling chlorosilane. After the reaction, the mixed gas enters a condenser, and the mixed gas is condensed into a liquid state using circulating water as a refrigerant, and enters a reflux tank. A part of the liquid in the reflux tank participates in the reflux of the high-boiling tower, and a part is extracted to separate the distillation of the high-boiling tower. By using the technical solution of the present invention, the device investment is small, the energy consumption is not increased during the operation process, the one-time impurity removal efficiency is greater than 98%, and the hydrogen-containing silane content in dimethyldichlorosilane can be made less than 15ppm.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of organosilicon production, and in particular to a process and a device for removing impurities in an organosilicon monomer distillation process. Background Art

[0002] Organic silicon materials are mainly divided into four categories: silicone rubber, silicone oil, silane coupling agent, and silicone resin. They are widely used in aerospace, medical engineering, machinery manufacturing and other industries. More than 90% of the raw materials for producing organic silicon materials are polysiloxanes obtained by hydrolysis and cracking of dimethyldichlorosilane. When preparing silicone oil and silicone rubber, the purity of the monomer (CH3)2SiCl2 used is required to be above 99.9%. If the amount of impurities contained in the three functional groups of silicone rubber exceeds 0.05%, high molecular weight chain polymers cannot be obtained, and only polymers with three-dimensional structures can be obtained. This polymer with a cross-linked structure is not easy to mix evenly with the filler during mixing, so it will seriously affect the thermal stability, electrical insulation, mechanical strength and other properties of silicone rubber.

[0003] The methylchlorosilane mixed monomer synthesized by the "direct method" has many components, small boiling point differences, and high separation requirements, so the separation and purification of the monomers is quite difficult. The boiling point difference between dimethyldichlorosilane ((CH3)2SiCl2, boiling point 70.2℃) and its subsequent key component ethyldichlorosilane (CH3CH2SiHCl2, boiling point 74.0℃) is only 3.8℃, and the distillation requirements are high. If direct distillation separation is required, the energy consumption is high. The content of EtSiHCl2 in the mixed monomer is extremely low, and the boiling point is far different from that of high-boiling substances (mixtures with boiling points higher than 70℃), so it is not easy to remove it in the high-boiling step. CN 105906659 A discloses a purification process and system for dimethyldichlorosilane. The crude dimethyldichlorosilane with low boiling points removed enters the lower tower of the degassing tower to remove high boiling points. The gas phase at the top of the tower is mixed with hydrogen chloride gas and passed into a fixed bed reactor. The reactor then enters the upper tower of the degassing tower for rectification to remove high boiling points. The purity of dimethyldichlorosilane can reach more than 99.98%, and the removal rate of impurities can reach more than 99.9%. However, this method requires two degassing towers to perform two distillations to remove high boiling points, which has high energy consumption and high equipment cost. CN 111097194 A discloses a selective adsorption method and device for purifying dimethyldichlorosilane. This method requires all raw materials to be gasified, which has high energy consumption, large adsorption device, low efficiency, and is not conducive to large-scale continuous production. Summary of the invention

[0004] The invention discloses a process for removing impurities in a distillation process of an organic silicon monomer, which can remove ethyl silicon hydride impurities enriched in the distillation process of the organic silicon monomer in a targeted manner, reduce the accumulation of ethyl silicon hydride in the system, thereby reducing the saturated partial pressure of ethyl silicon hydride, reduce the amount of ethyl silicon hydride carried out in dimethyldichlorosilane, improve the product quality of dimethyldichlorosilane, do not increase any energy consumption, and do not change the monomer separation process flow of the existing device.

[0005] A process for removing impurities in a distillation process of an organic silicon monomer is used to remove ethyl silicon hydride impurities enriched in the distillation process of the organic silicon monomer, thereby reducing the accumulation of ethyl silicon hydride in the system, thereby reducing the saturated partial pressure of ethyl silicon hydride, reducing the amount of ethyl silicon hydride carried over in dimethyldichlorosilane, and improving the product quality of dimethyldichlorosilane without increasing any energy consumption or changing the monomer separation process flow of the existing device.

[0006] The present invention also provides a process for removing impurities during the distillation process of an organosilicon monomer, comprising the following steps:

[0007] (1) The kettle liquid from the high-boiling tower is used as the feed of the high-boiling tower, and crude dimethyldichlorosilane is extracted through the gas phase at the top of the high-boiling tower;

[0008] (2) The crude dimethyldichlorosilane in the high-boiling tower top gas phase is fully mixed with the chlorine source material in the pipeline mixer and then enters the fixed bed reactor. Under the action of the catalyst, the hydrogen-containing silane in the crude dimethyldichlorosilane is converted into high-boiling point chlorosilane; after the reaction, the mixed gas enters the condenser, and the circulating water is used as the refrigerant to condense the mixed gas into a liquid state and enter the reflux tank.

[0009] The kettle liquid of the high-boiling tower is a mixture of dimethyldichlorosilane and high-boiling substances with a boiling point greater than 70.2°C, wherein the mass ratio of dimethyldichlorosilane to the high-boiling substances with a boiling point greater than 70.2°C is 1:1 to 1:4.

[0010] The high boiling tower is heated by medium-pressure steam, with a top pressure of 0.05-0.15MPa and a top temperature of 70-105°C; the temperature of the top gas phase pipe and the chlorine source material is controlled to be consistent with the top temperature of the high boiling tower when they are mixed in the pipeline mixer and enter the fixed bed reactor.

[0011] The two gaseous reactants, the high boiling tower top extraction and the chlorine source additive, are evenly mixed in the pipeline mixer and then fed into the fixed bed reactor to fully contact and react with the catalyst. The temperature of the pipeline mixer and the fixed bed reactor is controlled at 70-105°C to avoid the temperature being lower than the boiling point of the reactants, which will cause the gaseous reactants to liquefy. At the same time, avoid pressure fluctuations caused by excessive temperature, which will lead to obstruction of material transportation, excessive flow rate of reactants, and incomplete reaction.

[0012] The catalyst is a supported metal catalyst synthesized from one or more of palladium, platinum, copper and nickel supported on a carbon carrier, an aluminum oxide carrier or a metal organic framework (MoFs), and the metal loading is 5%-20%. Preferably, a composite supported metal catalyst of palladium and nickel supported on MoFs is used, and the total loading of palladium and nickel is 10%, wherein the ratio of palladium to nickel is 1:0.3.

[0013] The preparation method of the catalyst comprises the following steps: preparing a MoFs carrier by a hydrothermal method, ultrasonically immersing the carrier in a mixed solution of palladium and nickel for a certain period of time, adding a sodium hydroxide solution for precipitation, washing and collecting the precipitate, reducing the metal particles with hydrogen after vacuum drying, passivating with nitrogen, collecting the finished catalyst and sealing and preserving it.

[0014] The catalyst is added with the co-catalyst nickel to improve the ability of the main catalyst Pd to adsorb -H and activate Cl-C bonds, thereby improving the catalyst activity and selectivity, and effectively improving the poisoning and deactivation of the main catalyst Pd.

[0015] The amount of hydrogen-containing chlorosilane in the crude dimethyldichlorosilane extracted from the high-boiling tower top gas phase is 1000-6000 ppm, and the molar ratio of the chlorine source substance to the hydrogen-containing chlorosilane in the crude dimethyldichlorosilane is 2-10:1.

[0016] The chlorine source is selected from hydrogen chloride or chlorobenzene, and the chlorine source is fed in the form of gas. If chlorobenzene is selected as the chlorine source, the chlorobenzene needs to be gasified and then fed into the mixer.

[0017] The crude dimethyldichlorosilane and the chlorine source are in contact with the active components of the catalyst in the fixed bed for 10 minutes to 60 minutes. The contact time is shortened as much as possible to improve the reaction efficiency while ensuring that the reaction is fully carried out.

[0018] A device for removing impurities in a distillation process of an organic silicon monomer, wherein the bottom discharge port of a high-boiling tower is connected to the feed port of a high-boiling tower, a flow meter and an infusion pump are arranged on the connected pipeline, the high-boiling tower is connected to the feed port of a fixed-bed reactor via a pipeline, a catalyst is installed in the fixed bed, hydrogen-containing silane in crude dimethyldichlorosilane is converted into corresponding chlorosilane, a chlorine source material feed pipe is also arranged on the pipeline, the fixed-bed reactor is connected to a condenser inlet, and the condenser outlet is connected to a reflux tank.

[0019] A pipeline mixer is provided on the connecting pipeline between the high boiling tower and the fixed bed reactor for uniformly mixing the two fluids, and the chlorine source material feed pipe is connected to the pipeline mixer.

[0020] The reflux tank is connected to the feed port of the degassing tower and the reflux port of the high boiling tower respectively, and the pipelines between them are equipped with flow meters and infusion pumps. There is a vent at the top of the reflux tank.

[0021] In the impurity removal device, a vent is provided at the top of the reflux tank, and the pressure at the top of the high boiling tower is controlled by venting through a regulating valve, and non-condensable gas is discharged.

[0022] The beneficial effects of the present invention are:

[0023] This technical solution can be simply modified on the basis of the original monomer separation process, adding a fixed bed reactor and a small number of pipelines, with low investment and easy operation. This technical solution does not change the operating parameters of the high-removal tower system and does not increase energy consumption. 3. This technical solution optimizes the impurity removal process entry point in the organic silicon distillation process, has a high impurity removal efficiency, can effectively reduce the accumulation of ethylsilane in the system, and can achieve a good impurity removal effect under small-scale equipment, achieving the goal of reducing the impurity content in the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 The device is used for removing impurities in the distillation process of organic silicon monomer, including: 1. a high-removal tower; 2. a high-boiling tower; 3. a pipeline mixer; 4. a fixed-bed reactor; 5. a condenser; 6. a reflux tank; and 7. a chlorine source material feed pipe. DETAILED DESCRIPTION

[0025] Example 1

[0026] Preparation of Pd-Ni / MoFs catalyst: (1) Preparation of MoFs carrier: 0.52 mmol zirconium chloride and 0.96 mmol terephthalic acid were dissolved in N,N-dimethylformamide solution, and then 60 mL acetic acid was added to the solution and stirred for 1 hour until it was mixed evenly. After ultrasonic treatment for 30 minutes, the solution was transferred to a polytetrafluoroethylene liner and sealed. The synthesis was heated at 120 °C in a microwave hydrothermal synthesis instrument for 24 hours. After the crystal phase synthesis was completed, the reaction product was collected by centrifugation and then washed three times with N,N-dimethylformamide solution and methanol solution to remove the residue. The product sample was dried at 100 °C for 24 hours to obtain a white crystalline powder. (2) Preparation of Pd-Ni / MoFs: 0.13 g of palladium chloride and 0.07 g of nickel nitrate were dissolved in 20 mL of water to prepare a metal precursor solution. 1.0 g of MoFs carrier was ultrasonically dispersed in the metal precursor solution and stirred for 30 min. Then, 20 mL of 10 mol / L sodium hydroxide solution was added to precipitate the solution. The solution was centrifuged and filtered. After multiple washings, the solution was vacuum dried and the metal particles were reduced with hydrogen. After passivation with nitrogen, the finished catalyst was collected and sealed for storage.

[0027] In the technical solution of the present application, Pd-Cu / MoFs is a homemade product. 0.13 g of palladium chloride and 0.07 g of copper nitrate are dissolved in 20 mL of water to prepare a metal precursor solution. 1.0 g of MoFs carrier is ultrasonically dispersed in the metal precursor solution and stirred for 30 min. Then, 20 mL of 10 mol / L sodium hydroxide solution is added thereto for precipitation. The solution is centrifugally filtered, washed multiple times, and vacuum dried. The metal particles are then reduced with hydrogen. After passivation with nitrogen, the finished catalyst is collected and sealed for storage.

[0028] Pd / MOFs is a homemade product. 0.13 g of palladium chloride is dissolved in 20 mL of water to prepare a metal precursor solution. 1.0 g of MoFs carrier is ultrasonically dispersed in the metal precursor solution and stirred for 30 min. Then 20 mL of 10 mol / L sodium hydroxide solution is added to it for precipitation. The solution is centrifuged and filtered. After multiple washings, it is vacuum dried and the metal particles are reduced with hydrogen. After passivation with nitrogen, the finished catalyst is collected and sealed for storage.

[0029] Pd / C was purchased from Shaanxi Ruike New Materials Co., Ltd. The product model is: D5H5A, activated carbon is used as the carrier, and the palladium loading is 5%.

[0030] Pt / C was purchased from Shaanxi Ruike New Materials Co., Ltd. The product model is: T5H1L, activated carbon is used as the carrier, and the platinum loading is 5%.

[0031] Ni / Al2O3 was purchased from Shanghai Xunkai New Material Technology Co., Ltd. The product model is: SNCAT-5000P, Al2O3 is used as the carrier, and the nickel content is 48%.

[0032] Pt / Al2O3 was purchased from Shaanxi Ruike New Materials Co., Ltd., Al2O3 was used as the carrier, and the platinum loading was 5%.

[0033] Pd / Al2O3 was purchased from Yichang Supeng Technology Co., Ltd., product model: SC-A06, Al2O3 was used as the carrier, and the platinum loading was 0.3%.

[0034] Pd-Cu / Al2O3 was purchased from Shanghai Xunkai New Material Technology Co., Ltd. Al2O3 was used as the carrier, the loading amount of platinum was 4.5%, and the loading amount of Cu was 20%.

[0035] Pd-Ni / Al2O3 was purchased from Shanghai Xunkai New Material Technology Co., Ltd. Al2O3 was used as the carrier, the loading amount of platinum was 4.5%, and the loading amount of Ni was 20%.

[0036] Example 2

[0037] The impurity removal device for the 100,000 tons / year organic silicon monomer distillation process, the bottom discharge port of the high-boiling tower is connected to the feed port of the high-boiling tower, and the top discharge port of the high-boiling tower and the chlorine source pipeline are connected to the inlet of the pipeline mixer, which is used to mix the two fluids evenly. The outlet of the pipeline mixer is connected to the feed port of the fixed bed, and the catalyst is installed in the fixed bed to convert the hydrogen-containing silane in the crude dimethyldichlorosilane into the corresponding chlorosilane. The fixed bed outlet is connected to the condenser inlet, the condenser outlet is connected to the reflux tank inlet, and the reflux tank outlet is connected to the high-boiling tower reflux port and the high-boiling tower feed port. The high-boiling tower kettle is connected to the high-boiling tower, and a flow meter and an infusion pump are provided on the pipeline between them. The reflux tank is connected to the high-boiling tower and the high-boiling tower, and a flow meter and an infusion pump are provided on the pipeline between them.

[0038] Example 3

[0039] The impurity removal process of the organic silicon monomer distillation process is carried out using the device of Example 2, and the steps are as follows: the liquid from the kettle of the high-boiling tower 1 is adjusted by flow rate and liquid level to be taken out as the feed of the high-boiling tower (2), with a flow rate of 0.8 m³ / h, wherein the mass ratio of dimethyldichlorosilane to high-boiling substances (boiling point greater than 70.2°C) is 1:1. The high-boiling tower uses 10 kg of steam to heat the kettle, and through parameter control, the tower top pressure is 0.1 MPa, the temperature is 90°C, and the gas phase is taken out through the gas phase at the top of the high-boiling tower 2 to take out crude dimethyldichlorosilane, and the high-boiling substances are taken out from the kettle. The crude dimethyldichlorosilane in the gas phase of the high boiling tower 2 is analyzed and found to contain 6000ppm of ethyl silane and hydrogen chloride gas in a molar ratio of 1:5. After being fully mixed in the pipeline mixer 3, it enters the fixed bed reactor 4. The temperature of the pipeline mixer 3 and the fixed bed reactor 4 is controlled to be consistent with the extraction temperature of the gas phase at the top of the high boiling tower, 70-105°C. Under the action of the Pd-Ni / MoFs catalyst of Example 1, the ethyl silane is converted into the corresponding high-boiling chlorosilane. After the reaction, the mixed gas enters the condenser 5, and the mixed gas is condensed into a liquid state using circulating water as a refrigerant, and enters the reflux tank 6. 30% of the liquid in the reflux tank 6 is refluxed to the high boiling tower to continue the reaction, and 70% is extracted to the degassing tower 1 for distillation and separation. After analysis, the ethyl silane content in the reflux liquid is 8ppm, and the conversion rate is 99.9%. The material at the top of the degassing tower enters the distillation system of this field, and the ethyl silane content in the dimethyl dichlorosilane product obtained from the dimethyl tower of the distillation system is 10ppm.

[0040] Based on the device of Example 2 and the process flow of Example 3, the following examples were carried out under different process conditions:

[0041] Example 4-15 Comparison of the working conditions of changing the catalyst and the chlorine source material with those of not using the present invention

[0042]

[0043] Examples 16-21 use Pd-Ni / MoFs catalysts, change the chlorine source additive and the molar ratio of ethyl silane to chlorine source, the ethyl silane conversion rate and the ethyl silane content in the finished dimethyl formaldehyde change, and other processes and conditions are the same as Example 3.

[0044]

[0045] Examples 22-26

[0046] The temperature, pressure and fixed bed residence time at the top of the high boiling tower were controlled, and other processes and conditions were the same as those in Example 3.

[0047]

Claims

1. A process for removing impurities from the distillation process of organosilicon monomers. It is characterized in that The following steps are involved: (1) The kettle liquid from the high-boiling tower is used as the feed of the high-boiling tower, and crude dimethyldichlorosilane is produced through the gas phase at the top of the high-boiling tower. The amount of hydrogen chlorosilane in the crude dimethyldichlorosilane produced from the gas phase at the top of the high-boiling tower is 1000-6000ppm; (2) The crude dimethyldichlorosilane gas phase at the top of the high-boiling tower is fully mixed with the chlorine source material in the pipeline mixer and then enters the fixed bed reactor. Under the action of the catalyst, the hydrogen-containing silane in the crude dimethyldichlorosilane is converted into high-boiling chlorosilane; the mixed gas after the reaction enters the condenser, and the mixed gas is condensed into a liquid using circulating water as a refrigerant, and enters the reflux tank. The high-boiling tower is heated by medium-pressure steam, the tower top pressure is 0.05-0.15MPa, and the tower top temperature is 70-105℃; the temperature of the tower top gas phase and the chlorine source material when they are mixed in the pipeline mixer and enter the fixed bed reactor is controlled to be consistent with the tower top temperature of the high-boiling tower. The catalyst is a composite loaded metal catalyst of MoFs loaded with palladium and nickel, the total loading of palladium and nickel is 10%, and the palladium / nickel ratio is 1:0.

3.

2. The process for removing impurities from the organic silicon monomer distillation process as claimed in claim 1, It is characterized in that The kettle liquid of the high-boiling tower is a mixture of dimethyldichlorosilane and high-boiling substances with a boiling point greater than 70.2°C, wherein the mass ratio of dimethyldichlorosilane to the high-boiling substances with a boiling point greater than 70.2°C is 1:1 to 1:

4.

3. The process for removing impurities from the organic silicon monomer distillation process as claimed in claim 1, It is characterized in that The molar ratio of the chlorine source material to the hydrogen-containing chlorosilane in the crude dimethyldichlorosilane is 2-10:

1.

4. The process for removing impurities during the distillation of organosilicon monomers as claimed in claim 3, It is characterized in that The chlorine source is selected from hydrogen chloride or chlorobenzene, and the chlorine source is fed in the form of gas.

5. The process for removing impurities from the organic silicon monomer distillation process as claimed in claim 1, It is characterized in that The crude dimethyldichlorosilane and the chlorine source are in contact with the catalyst active components in the fixed bed for 10 minutes to 60 minutes.

6. The process for removing impurities from the organic silicon monomer distillation process as claimed in claim 1, It is characterized in that 30-40% of the liquid in the reflux tank participates in the reflux of the high boiling tower, and 60-70% is extracted and removed to the high tower for distillation separation.