A method for preparing a 10-500 μm particle concentration marked tablet

By screening and pretreating the particles, combining lactose and cellulose, the number of particles in each tablet is ensured to be accurate, and the problems of inaccurate particle concentration measurement and environmental pollution in the prior art are solved, and the quality and transportation safety of the tablet are improved.

CN114894583BActive Publication Date: 2024-12-03NANTONG UNIV
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202210574524.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-05-25
Publication Date
2024-12-03
Estimated Expiration
2042-05-25

AI Technical Summary

Technical Problem

Existing spore sheets of lilac pine are prone to damage, resulting in inaccurate amount of spore powder, microplastics pollute the environment and are costly, making it difficult to accurately measure the concentration of 10-500μm particles.

Method used

By selecting particles of the appropriate particle size for screening and pretreatment, combining lactose and cellulose, stirring evenly with a blower, and coating the tablet press after the tableting is coated. High-precision counters are used to ensure the accurate number of particles in each tablet, reducing the number of particles in each tablet. Transportation damaged.

Benefits of technology

Improve the accuracy and quality of tablets, reduce environmental pollution, reduce transportation costs, and ensure the accuracy of the label content in each tablet through statistical methods.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114894583B_ABST
    Figure CN114894583B_ABST
Patent Text Reader

Abstract

The present invention discloses a preparation method of a 10-500 μm particle concentration marker tablet, comprising the following steps: step one: selecting particles of suitable particle size; step two: pre-treating the particles: for distinguishing a small amount of particles existing in the detection area that are the same as the reference; step three: counting the particles by a counter: determining the number of particles for tableting; step four: stirring the raw materials by a blower; step five: making tablets of suitable particle size: tableting with a tablet press, and coating according to the situation after tableting; step six: selecting a small amount of tablets for uniformity inspection. The present invention improves the tablet quality by updating the tablet filler, and by statistical methods, the content of the marker in each tablet is counted, thereby improving the tablet accuracy; it uses natural products, and there is almost no environmental pollution; by increasing the coating process, the yield rate of the tablet is increased, the damage of the tablet in the environment such as transportation is reduced, and the transportation cost is reduced to a certain extent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for preparing a 10-500 μm particle concentration identification tablet, belonging to the technical field of preparation of 10-500 μm microparticle (spore pollen) concentration identification tablets. Background Art

[0002] Particles of 10-500μm are common in nature, such as pollen and microplastics. Most of the pollen particles are between 10-300μm in size, have strong resistance to high temperature and corrosion, and can be retained for a long time. From the types of local pollen, we can deduce the local plant species and vegetation types, and thus infer the local climate type. Now there are mature methods to extract particles, but how to measure their concentration is a puzzling problem. Concentration is used as a comparison of the same type of particle indicators between different regions. Different levels are divided by concentration to make the indicators more intuitive. At present, particle research has an important position in many scientific fields, especially in environment and geology. In pollen identification, a reference is needed to infer the size, quantity and concentration of pollen. This reference should be as different from the morphology of local pollen as possible, and there should be no reference pollen in the local environment as much as possible. Lycopodium spores are obviously different from the morphology of most pollen in nature. There is another advantage of choosing Lycopodium as a pollen reference. Lycopodium spores are easy to collect, which will relatively reduce the difficulty of production.

[0003] The existing Lycopodium spore tablets in China use calcium carbonate as a filler, without an outer coating, and are very low in cost. Lycopodium spore tablets are prone to powder loss, especially during transportation, when the road is bumpy, which can easily cause the spore tablets to break, resulting in inaccurate spore powder counts in the spore tablets, which has a great impact on pollen identification. The number of spores in the spore tablets has not been accurately identified, and their credibility needs to be verified.

[0004] The advantage of using microplastics as identification sheets is that the cost of identification sheets is low and the content of the identification material in the tablets is easy to control. However, there is a fatal problem - the pollution of the environment by microplastics. The pollution of the environment by microplastics is everywhere, because microplastics are too small to penetrate anywhere and are hard to prevent. Using degradable plastics as identification materials will face huge cost issues. Summary of the invention

[0005] In view of the problems existing in the above-mentioned prior art, the present invention provides a method for preparing a 10-500 μm particle concentration marked tablet, thereby solving the above-mentioned technical problems.

[0006] In order to achieve the above object, the technical solution adopted by the present invention is: a method for preparing a 10-500 μm particle concentration marking tablet, comprising the following steps;

[0007] Step 1: Select particles of appropriate particle size: It is used to screen the required particle size according to the needs of different experiments and different uses, and select particles of particle size suitable for their own experimental needs or environmental indicators for film making;

[0008] Step 2: Pre-process the particles: This is used to distinguish the small amount of particles that already exist in the test area and are identical to the reference particles. The natural world is in an uninterrupted cycle. In the material cycle, water cycle, and atmospheric cycle, particles will be carried to various places. Therefore, it is impossible to determine whether the test area already has reference particles. Pre-process the particles to distinguish them from the reference particles.

[0009] Step 3: Count the particles using a counter: determine the number of particles in the tablet, and then ensure that the number of reference particles in each tablet is within the appropriate range;

[0010] Step 4: Use a blower to stir the raw materials evenly: the raw materials are microparticles, lactose, and cellulose, which are stirred evenly, and the blower is used to lift the raw materials and stir them evenly in the air to make them more uniform;

[0011] Step 5: Make tablets of appropriate particle size: Use a tablet press to make tablets, and perform coating treatment according to the situation after tableting;

[0012] Step 6: Select a small number of tablets for uniformity test: used to test the qualification of tablets. Scheme 1: random sampling, dissolution, counting by counter, the number of reference particles in the tablet is less than the expected number of reference particles 2000, which is qualified, and the qualification is calculated based on this. It is convenient to improve the previous process and adjust the parameters. Scheme 2: random sampling, dissolution, counting by counter, remove the tablets with the largest and smallest numbers, draw a discrete graph, and the discrete coefficient is less than 0.5, and the whole is qualified.

[0013] Furthermore, the specific method for selecting particles of appropriate particle size in step 1 is: according to the type to be identified, the median diameter of all types of particles is selected as the diameter of the selected marker, the appropriate range is 10-100μm, and in order to ensure the quality of the film, the maximum does not exceed 500μm.

[0014] Furthermore, the specific method of pretreating the microparticles in step 2 is: first take 5g of labeled pollen, add 15mL of 10% NaOH solution; wash with water until neutral; then add 25mL of glacial acetic acid to wash away the water; then add 12.5mL of acetic acid solution (acetic anhydride and concentrated sulfuric acid in a ratio of 9:1); then add 25mL of glacial acetic acid to wash the acetic acid solution; wash with water until neutral; and finally freeze-dry in a freeze dryer.

[0015] Furthermore, in each step of the pretreatment of the microparticles in step 2, a centrifuge is used to remove moisture, and the centrifugal speed of the centrifuge is 3500 r / min.

[0016] Furthermore, the method for counting the particles in step three is: using a high-concentration particle counter and a ten-thousandth analytical balance. Take 0.01g of the marker with an analytical balance and count it with a high-concentration particle counter. The marker is a very small particle, and the specific number cannot be counted by the human eye. However, because it is necessary to ensure that the number of markers in each piece of identification sheet is 12500±500, and it is necessary to count, some high-precision instrument methods have to be used. With the help of a high-concentration particle counter, the number of markers can be accurately counted.

[0017] Furthermore, the mass fraction of the microparticles, lactose and cellulose in step 4 is 1:750:750.

[0018] Furthermore, the specific method of the uniformity test in step 5 is random sampling, dissolution, and counting by a counter. If the number of reference particles in the tablet is less than 2000 expected reference particles, it is a qualified product, and the qualification is calculated based on this.

[0019] Furthermore, the specific method of the uniformity test in step five is random sampling, dissolution, counting by a counter, removing the pieces with the largest and smallest numbers, and drawing a discrete graph. If the discrete coefficient is less than 0.5, the whole piece is qualified.

[0020] The beneficial effects of the present invention are as follows: the present invention improves the tablet quality by updating the tablet filler, and uses a statistical method to count the content of the marker in each tablet, thereby improving the tablet accuracy; the present invention uses natural products and has almost no environmental pollution; by adding a coating process, the tablet yield is increased, the tablet breakage during transportation and other environments is reduced, and the transportation cost is reduced to a certain extent. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 It is a structural schematic diagram of the present invention. DETAILED DESCRIPTION

[0022] In order to make the purpose, technical solution and advantages of the present invention more clear, the present invention is further described in detail below through the accompanying drawings and embodiments. However, it should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the scope of the present invention.

[0023] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by technicians in the technical field to which the present invention belongs. The terms used in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention.

[0024] like Figure 1As shown, a method for preparing a 10-500 μm particle concentration marked tablet comprises the following steps;

[0025] Step 1: Select particles of appropriate particle size: It is used to screen the required particle size according to the needs of different experiments and different uses, and select particles of particle size suitable for their own experimental needs or environmental indicators for film making;

[0026] Step 2: Pre-process the particles: This is used to distinguish the small amount of particles that already exist in the test area and are identical to the reference particles. The natural world is in an uninterrupted cycle. In the material cycle, water cycle, and atmospheric cycle, particles will be carried to various places. Therefore, it is impossible to determine whether the test area already has reference particles. Pre-process the particles to distinguish them from the reference particles.

[0027] Step 3: Count the particles using a counter: determine the number of particles in the tablet, and then ensure that the number of reference particles in each tablet is within the appropriate range;

[0028] Step 4: Use a blower to stir the raw materials evenly: the raw materials are microparticles, lactose, and cellulose, which are stirred evenly, and the blower is used to lift the raw materials and stir them evenly in the air to make them more uniform;

[0029] Step 5: Make tablets of appropriate particle size: Use a tablet press to make tablets, and perform coating treatment according to the situation after tableting;

[0030] Step 6: Select a small number of tablets for uniformity test: used to test the qualification of tablets. Scheme 1: random sampling, dissolution, counting by counter, the number of reference particles in the tablet is less than the expected number of reference particles 2000, which is qualified, and the qualification is calculated based on this. It is convenient to improve the previous process and adjust the parameters. Scheme 2: random sampling, dissolution, counting by counter, remove the tablets with the largest and smallest numbers, draw a discrete graph, and the discrete coefficient is less than 0.5, and the whole is qualified.

[0031] In the preferred embodiment, the specific method of selecting particles of appropriate particle size in step 1 is: according to the type to be identified, the median diameter of all types of particles is selected as the diameter of the selected marker, and the appropriate range is 10-100 μm. In order to ensure the quality of the film, the maximum does not exceed 500 μm.

[0032] In the preferred embodiment of the present invention, the specific method for pretreating the microparticles in step 2 is as follows: first, take 5 g of labeled pollen, add 15 mL of 10% NaOH solution; wash with water until neutral; then add 25 mL of glacial acetic acid to wash away the water; then add 12.5 mL of acetic acid solution (acetic anhydride and concentrated sulfuric acid in a ratio of 9:1); then add 25 mL of glacial acetic acid to wash the acetic acid solution; wash with water until neutral; and finally freeze-dry in a freeze dryer.

[0033] In this embodiment, preferably, in each step of the pretreatment of the particles in step 2, a centrifuge is used to remove moisture, and the centrifugal speed of the centrifuge is 3500 r / min.

[0034] In this embodiment, the method for counting the particles in step 3 is: using a high-concentration particle counter and a ten-thousandth analytical balance. 0.01 g of the marker is taken with an analytical balance and counted with a high-concentration particle counter.

[0035] Preferably, in this embodiment, the mass fraction of the microparticles, lactose, and cellulose in step 4 is 1:750:750.

[0036] In this embodiment, the specific method of uniformity inspection in step 5 is random sampling, dissolution, and counting by a counter. If the number of reference particles in the tablet is less than 2000 expected reference particles, it is a qualified product, and the qualification is calculated based on this.

[0037] In the preferred embodiment of the present invention, the specific method for uniformity inspection in step five is random sampling, dissolution, counting by a counter, removing the pieces with the largest and smallest numbers, and drawing a discrete graph. If the discrete coefficient is less than 0.5, the whole piece is qualified.

[0038] The present invention improves tablet quality by updating tablet fillers, and uses statistical methods to count the content of markers in each tablet, thereby improving tablet accuracy; the invention uses natural products and has almost no environmental pollution; the invention increases the yield rate of tablets by adding a coating process, reduces tablet breakage during transportation and other environments, and reduces transportation costs to a certain extent.

[0039] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modification, equivalent substitution or improvement made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for preparing a 10-500 μm particle concentration marked tablet, characterized in that: The steps include: Step 1: Select particles of appropriate particle size: It is used to screen the required particle size according to the needs of different experiments and different uses, and select particles of particle size suitable for their own experimental needs or environmental indicators for film making; Step 2: Pre-process the particles: to distinguish a small number of particles that already exist in the detection area and are identical to the reference; The specific method of pre-treating the microparticles in step 2 is as follows: first, take 5g of labeled pollen, add 15mL of 10% NaOH solution; wash with water until neutral; then add 25mL of glacial acetic acid to wash away the water; then add 12.5mL of acetic acid solution, which is a mixture of acetic anhydride and concentrated sulfuric acid in a ratio of 9:1; then add 25mL of glacial acetic acid to wash the acetic acid solution; wash with water until neutral; and finally freeze-dry in a freeze dryer; Step 3: Count the particles using a counter: determine the number of particles in the tablet, and then ensure that the number of reference particles in each tablet is within the appropriate range; Step 4: Use a blower to stir the raw materials evenly: the raw materials are microparticles, lactose, and cellulose, which are stirred evenly, and the blower is used to lift the raw materials and stir them evenly in the air to make them more uniform; Step 5: Make tablets of appropriate particle size: Use a tablet press to make tablets, and perform coating treatment according to the situation after tableting; Step 6: Select a small number of tablets for uniformity test: used to test the qualification of tablets. Option 1: Random sampling, dissolution, counting through a counter, the number of reference particles in the tablet is less than the expected number of reference particles 2000, which is a qualified product. The qualification is calculated in this way to improve the previous process and adjust the parameters. Option 2: Random sampling, dissolution, counting through a counter, remove the tablets with the largest and smallest numbers, draw a discrete graph, and the discrete coefficient is less than 0.5, which means the whole is qualified.

2. The method for preparing a 10-500 μm particle concentration marking tablet according to claim 1, characterized in that: The specific method of selecting particles of appropriate particle size in step 1 is: according to the type to be identified, the median diameter of all types of particles is selected as the diameter of the selected marker, and the appropriate range is 10-100 μm. In order to ensure the quality of the film, the maximum does not exceed 500 μm.

3. The method for preparing a 10-500 μm particle concentration marking tablet according to claim 1, characterized in that: In each step of the pretreatment of the particles in step 2, a centrifuge is used to remove moisture, and the centrifugal speed of the centrifuge is 3500 r / min.

4. The method for preparing a 10-500 μm particle concentration marking tablet according to claim 1, characterized in that: The method for counting the particles in step three is: using a high-concentration particle counter and a ten-thousandth analytical balance, taking 0.01 g of the marker with an analytical balance, and counting with a high-concentration particle counter.

5. The method for preparing a 10-500 μm particle concentration marking tablet according to claim 1, characterized in that: The mass fraction of the microparticles, lactose and cellulose in step 4 is 1:750:750.

Citation Information

Patent Citations

  • Certification method for grain counting particle standard substance

    CN108387503A

  • Particle sensor

    CN108426807A