Display panel and manufacturing method thereof, and display device

By using anode and binding pads with acid-resistant densification layers in the display panel, the problem of oxidation of copper alloy metal traces is solved, binding stability and manufacturing efficiency are improved, and manufacturing costs are reduced.

CN115000332BActive Publication Date: 2024-11-05SHENZHEN CHINA STAR OPTOELECTRONICS SEMICON DISPLAY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210771124.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-06-30
Publication Date
2024-11-05
Estimated Expiration
2042-06-30

AI Technical Summary

Technical Problem

The existing display panels are easily oxidized due to the copper or copper alloy metal traces reacting and oxidizing with air oxygen and water vapor, which affects the binding effect with the flexible circuit board, increasing manufacturing processes and manufacturing costs.

Method used

Using anode and binding pads with acid-resistant densification layer, the indium tin oxide crystal layer is formed by high-temperature annealing. The anode and binding pads are made of the same material, reducing manufacturing processes and materials, reducing manufacturing time and manufacturing cost.

Benefits of technology

Improve the structural stability of the bonded pads, avoid oxidation or vulcanization failure, reduce the manufacturing process and material use of the display panel, and significantly reduce the manufacturing time and manufacturing cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115000332B_ABST
    Figure CN115000332B_ABST
Patent Text Reader

Abstract

The present application provides a display panel, a preparation method thereof, and a display device, in which both the anode and the binding pad are set to be an acid-resistant densification layer, which can avoid the problem of failure of the anode or the binding pad due to oxidation or sulfurization, so as to improve the structural stability of the binding pad. In addition, the anode and the binding pad can be made of the same material, that is, they can be made of the same material through the same process, so that there is no need to prepare the binding pad separately after the anode is made. Therefore, compared with the display panel of the prior art, which has an additional manufacturing process of using molybdenum or molybdenum alloy to make the binding pad, the present invention can reduce the manufacturing process and required manufacturing materials of the display panel, and greatly reduce the manufacturing time and manufacturing cost of the display panel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the field of display technology, and in particular, relates to a display panel and a manufacturing method thereof, and a display device. Background Art

[0002] In the display panel of the prior art, copper (Cu) or copper alloy has good electrical conductivity, so the display panel uses it as metal wiring. In addition to being the circuit wiring of the thin film transistor of the display panel, the metal wiring is also used to electrically connect the flexible circuit board outside the display panel to access external signals. However, since the material of the metal wiring is copper or copper alloy, which is a material that easily reacts with oxygen and water vapor in the air, the part of the metal wiring exposed outside the display panel for electrical connection with the flexible circuit board will be easily oxidized, thereby affecting the binding effect between the display panel and the flexible circuit board.

[0003] In order to solve the above technical problems, the prior art uses a material with low activity and corrosion resistance such as molybdenum (Mo) or a molybdenum alloy as a bonding pad, and covers the exposed metal traces to isolate the metal traces from reacting with oxygen and water vapor in the air. However, this structural design will increase the manufacturing process of the display panel, and increase the manufacturing time and manufacturing cost of the display panel. Summary of the invention

[0004] Embodiments of the present application provide a display panel and a method for manufacturing the same, as well as a display device, to solve the problems of long manufacturing time and high manufacturing cost of existing display panels.

[0005] In a first aspect, an embodiment of the present application provides a display panel, including:

[0006] an anode electrically connected to the thin film transistor of the display panel, the anode comprising a first densification layer, the first densification layer having acid resistance; and

[0007] The binding pad is electrically connected to the metal wiring of the display panel, and the binding pad includes a second densification layer, and the second densification layer is acid-resistant; the first densification layer and the second densification layer are formed by the same process.

[0008] Optionally, the first densification layer and the second densification layer include crystalline layers of indium tin oxide.

[0009] Optionally, the anode further includes a reflective layer and a transparent conductive oxide layer, wherein the reflective layer is disposed on a side of the first densification layer away from the thin film transistor, and the transparent conductive oxide layer is disposed on a side of the reflective layer away from the first densification layer.

[0010] Optionally, the display panel further includes a passivation layer and a planarization layer, the passivation layer is disposed on the thin film transistor and covers the thin film transistor, the passivation layer includes a first through hole opened on the thin film transistor; the planarization layer is disposed on the passivation layer, and the planarization layer includes a second through hole corresponding to the first through hole;

[0011] The anode passes through the first through hole and the second through hole to be electrically connected to the thin film transistor.

[0012] Optionally, the metal wiring is arranged in the same layer as the source and drain of the thin film transistor, and the binding pad is electrically connected to the thin film transistor through the metal wiring;

[0013] Wherein, the passivation layer further includes a third through hole opened on the metal wiring, and the binding pad passes through the third through hole to be electrically connected to the metal wiring.

[0014] In a second aspect, an embodiment of the present application further provides a display device, comprising a controller and a display panel as described above, wherein the controller is electrically connected to the display panel.

[0015] In a third aspect, an embodiment of the present application further provides a method for preparing a display panel, comprising the following steps:

[0016] providing a substrate;

[0017] Depositing a conductive material layer on the substrate; the conductive material layer is electrically connected to the thin film transistors and metal wiring of the display panel respectively;

[0018] Etching and patterning the conductive material layer to form an anode conductive material layer and a pad conductive material layer;

[0019] The anode conductive material layer and the pad conductive material layer are subjected to high temperature annealing treatment to form a first densification layer of the anode and a second densification layer of the pad.

[0020] Optionally, the conductive material layer comprises a first transparent material layer, a reflective material layer and a second transparent material layer;

[0021] The step of depositing a conductive material layer on the substrate comprises:

[0022] Depositing the first transparent material layer, the reflective material layer and the second transparent material layer on the substrate in sequence; wherein the first transparent material layer can be crystallized after being heated;

[0023] The step of performing high temperature annealing on the anode conductive material layer and the pad conductive material layer comprises:

[0024] The anode conductive material layer and the pad conductive material layer are subjected to high temperature annealing treatment to make the first transparent material layer crystallized and dense.

[0025] Optionally, after the step of performing high temperature annealing on the anode conductive material layer and the pad conductive material layer, the step further includes:

[0026] The pad conductive material layer is etched to etch away the reflective material layer and the second transparent material layer of the pad conductive material layer.

[0027] Optionally, the step of etching and patterning the conductive material layer includes:

[0028] The conductive material layer is exposed using a grayscale mask, wherein the grayscale mask comprises a light-transmitting area and a semi-light-transmitting area;

[0029] The exposed conductive material layer is etched to form an anode conductive material layer corresponding to the light-transmitting area and a pad conductive material layer corresponding to the semi-light-transmitting area.

[0030] Optionally, in the step of performing high temperature annealing treatment on the anode conductive material layer and the pad conductive material layer, the treatment temperature is set to 200° C. to 300° C.; and / or the treatment time is set to 1 hour to 3 hours.

[0031] The display panel provided in the embodiment of the present application sets both the anode and the binding pad as an acid-resistant densification layer, which can avoid the problem of failure of the anode or the binding pad due to oxidation or sulfurization, so as to improve the structural stability of the binding pad. In addition, the anode and the binding pad can be made of the same material, that is, they can be made of the same material through the same process, so that there is no need to prepare the binding pad separately after the anode is made. Therefore, compared with the display panel of the prior art, which has an additional manufacturing process of using molybdenum or molybdenum alloy to make the binding pad, the present invention can reduce the manufacturing process and required manufacturing materials of the display panel, and greatly reduce the manufacturing time and manufacturing cost of the display panel. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present application, and those skilled in the art can obtain other drawings based on these drawings without creative work.

[0033] In order to more completely understand the present application and its beneficial effects, the following description will be given in conjunction with the accompanying drawings. In the following description, the same reference numerals represent the same parts.

[0034] Figure 1 A schematic cross-sectional view of a display panel provided in an embodiment of the present application.

[0035] Figure 2 to Figure 4 A structural schematic diagram of the manufacturing process of the display panel provided in an embodiment of the present application.

[0036] Figure 5 A schematic flow chart of a method for preparing a display panel provided in an embodiment of the present application.

[0037] Figure 6 A detailed schematic diagram of a method for preparing a display panel provided in an embodiment of the present application.

[0038] 10. Thin film transistor; 11. Source; 12. Drain; 13. Gate; 20. Anode; 21. Indium tin oxide layer; 30. Binding pad; 22. Reflective layer; 23. Transparent conductive oxide layer; 40. Passivation layer; 50. Planarization layer; 60. Metal trace; 70. Grayscale mask; 71. Fully transparent area; 72. Semi-transparent area. DETAILED DESCRIPTION

[0039] The technical solutions in the embodiments of the present application will be described clearly and completely below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present application.

[0040] In the display panel of the prior art, copper (Cu) or copper alloy has good electrical conductivity, so the display panel uses it as the metal trace 60. In addition to being the circuit trace of the thin film transistor 10 of the display panel, the metal trace 60 is also used to electrically connect the flexible circuit board outside the display panel to access external signals. However, since the material of the metal trace 60 is copper or copper alloy, which is a material that easily reacts with oxygen and water vapor in the air, the part of the metal trace 60 exposed outside the display panel for electrical connection with the flexible circuit board will be easily oxidized, thereby affecting the binding effect between the display panel and the flexible circuit board.

[0041] In order to solve the above technical problems, the prior art uses a material with low activity and corrosion resistance such as molybdenum (Mo) or a molybdenum alloy as the bonding pad 30, and covers the exposed portion of the metal trace 60 to isolate the metal trace 60 from reacting with oxygen and water vapor in the air. However, this structural design will increase the manufacturing process of the display panel, and increase the manufacturing time and manufacturing cost of the display panel.

[0042] The embodiments of the present application provide a display panel and a display device to solve the problems of long manufacturing cycle and high manufacturing cost of existing display panels, which will be described below with reference to the accompanying drawings.

[0043] The display panel provided in the embodiment of the present application can be applied to a display device. Figure 1 , Figure 1 The cross-sectional schematic diagram of the display panel provided in the embodiment of the present application. The display panel includes a thin film transistor 10, which serves as a driving switch for making the pixels of the display panel emit light, and includes a source 11, a drain 12, a gate 13, a channel, and an insulating layer of the gate 13. By controlling the input voltage of the gate 13, the thin film transistor 10 can control the on and off of the current at both ends of the source 11 and the drain 12.

[0044] like Figure 1 As shown, the display panel further includes an anode 20, a light-emitting layer, and a cathode. The light-emitting layer is disposed between the anode 20 and the cathode. The anode 20 and the cathode are disposed in pairs. At the same time, the anode 20 is electrically connected to one of the source 11 and the drain 12 of the thin film transistor 10. Therefore, when the thin film transistor 10 controls the on and off of the current at both ends of the source 11 and the drain 12, a current or an electric field is generated between the anode 20 and the cathode, and the light-emitting layer works according to the current.

[0045] In one embodiment, the display panel further includes a planarization layer 50 and a passivation layer 40. The planarization layer 50 is disposed on the passivation layer 40. The passivation layer 40 includes a first through hole opened on one of the source electrode 11 and the drain electrode 12 of the thin film transistor 10. The planarization layer 50 includes a second through hole corresponding to the first through hole. The anode 20 passes through the first through hole and the second through hole to electrically connect one of the source electrode 11 and the drain electrode 12 of the thin film transistor 10.

[0046] In one embodiment, the display panel of the present invention includes an organic light-emitting diode (OLED) display panel. In other words, the anode 20, the light-emitting layer, and the cathode together constitute an organic light-emitting diode. The light-emitting layer also includes a hole injection layer, a hole transport layer, a light-emitting material layer, an electron transport layer, and an electron injection layer. When the thin film transistor 10 controls the current to be conducted to the anode 20, the current is generated between the anode 20 and the cathode. Under the action of the current, the electrons and holes in the light-emitting layer will combine in the light-emitting material layer and excite light, thereby achieving the bright and dark display of the pixels of the display panel. It should be noted that the cathode of the present invention includes an electrode material arranged on the entire surface, so the cathode can be prepared on the light-emitting layer by an evaporation process, thereby simplifying the structure and process of the display panel.

[0047] The light-emitting layer of the present invention is not limited to the above-mentioned embodiments. In other embodiments, the light-emitting layer may also include electroluminescent quantum dots (ELQDs), mini-light-emitting diodes (mini-LEDs), or micro-light-emitting diodes (micro-LEDs).

[0048] The following takes the display panel being an organic light emitting diode display panel as an example to further illustrate the specific implementation of the present invention.

[0049] The channel of the thin film transistor 10 is electrically connected to the source 11 and the drain 12. In one embodiment, the channel is made of a semiconductor material, in particular, made of indium gallium zinc oxide (IGZO). The electron mobility of the indium gallium zinc oxide used in this embodiment is 20-30 times that of traditional amorphous silicon semiconductors, thereby significantly improving the charge and discharge rate and response speed of the thin film transistor 10. Using the indium gallium zinc oxide as the channel of the thin film transistor 10 can achieve a faster refresh rate of the display panel. At the same time, the indium gallium zinc oxide has good driving capability, so the driving power consumption of the thin film transistor 10 is low, making the display panel more energy-efficient and power-saving, and greatly increasing the battery life of the display panel.

[0050] In one embodiment, the thin film transistor 10 includes a top gate 13 type thin film transistor 10. In other words, in the structural design of the thin film transistor 10, the channel is the bottom layer, and the gate 13 is the top layer. The top gate 13 type thin film transistor 10 can reduce the manufacturing process of the display panel, thereby reducing the manufacturing cost. It should be noted that the thin film transistor 10 of the present invention is not limited to the top gate 13 type thin film transistor 10, and can also be a bottom gate 13 type thin film transistor 10, or a thin film transistor 10 of other structures.

[0051] In the embodiment of the present application, the anode 20 includes a first densification layer 21, which is acid-resistant; the specific material of the first densification layer 21 is not limited, as long as the first densification layer 21 is transparent, conductive and acid-resistant. The first densification layer 21 can be a natural densification material, or it can be formed by a common transparent conductive material through a preset process; for example, the first densification layer 21 includes a crystalline layer of indium tin oxide (ITO), which can be crystallized and solidified after high-temperature treatment.

[0052] In one embodiment, the anode 20 further includes a reflective layer 22 and a transparent conductive oxide layer 23. The reflective layer 22 is disposed on a side of the first densification layer 21 away from the thin film transistor 10, and the transparent conductive oxide layer 23 is disposed on a side of the reflective layer 22 away from the first densification layer 21.

[0053] The reflective layer 22 and the transparent conductive oxide layer 23 can be made by continuously depositing materials through a magnetron sputtering process of physical vapor deposition (PVD). The manufacturing method of the anode 20 of the present invention is not limited to this, and can also be other methods in the physical vapor deposition, or even chemical vapor deposition (CVD). In this embodiment, the reflective layer 22 includes a metal with a high reflectivity such as silver metal; the transparent conductive oxide layer 23 includes an indium zinc oxide layer (IZO) or an indium tin oxide (ITO).

[0054] In one embodiment, the display panel of the present invention further includes a bonding pad 30 and a metal trace 60. The metal trace 60 is disposed in the same layer as the source 11 and the drain 12 of the thin film transistor 10, and is used to transmit the power and signals required for the display panel to work, such as Vdd and Vss. In order to achieve a narrow frame design, the display panel adopts a chip on film (COF) technology, so the metal trace 60 is electrically connected to the bonding pad 30 at the side area of ​​the display panel to provide a flexible circuit board of the chip on film for bonding the metal trace 60.

[0055] The passivation layer 40 further includes a third through hole opened on the metal trace 60. The bonding pad 30 passes through the third through hole to be electrically connected to the metal trace 60.

[0056] The binding pad 30 is electrically connected to the source 11, the drain 12, the gate 13 of the thin film transistor 10, and one of the cathodes of the display panel through the metal trace 60. It should be noted that in actual implementation, the display panel includes a plurality of thin film transistors 10, a plurality of metal traces 60, and a plurality of binding pads 30. The power supply and the signal required for the display panel to work are connected from the flexible circuit board of the chip-on-film outside the display panel through each of the binding pads 30, and transmitted to the cathode of the display panel, and each of the source 11, each of the drain 12, and each of the gates 13 of each of the thin film transistors 10.

[0057] The bonding pad 30 includes a second densification layer, which is acid-resistant; that is, the material of the bonding pad 30 is the same as the material of the anode 20. For example, the second densification layer includes a crystalline layer of indium tin oxide, which can enhance the overall material's ability to resist water vapor, high temperature, sulfurization, oxidation, and other elements, thereby preventing the metal trace 60 made of copper or copper alloy from being oxidized by direct contact with air.

[0058] Since the bonding pad 30 and the anode 20 are configured to be made of the same material, and the first densification layer 21 and the second densification layer are formed by the same process, the bonding pad 30 can be formed in the same process as the anode 20. Therefore, compared with the display panel of the prior art, which has an additional manufacturing process of using molybdenum (Mo) or a molybdenum alloy to make the bonding pad 30, the present invention can reduce one manufacturing process and manufacturing materials (such as a photomask) of the display panel, thereby significantly reducing the manufacturing time and manufacturing cost of the display panel.

[0059] Exemplarily, the present application also provides a display device, including a controller and a display panel as described above, wherein the controller is electrically connected to the display panel. The display device can be any product or component with a display function, such as an electronic paper, a mobile phone, a tablet computer, a television, a monitor, a laptop computer, a digital photo frame, a navigator, etc.

[0060] For example, see Figure 5 , Figure 5 The present invention also provides a method for manufacturing a display panel, including:

[0061] S100, providing a substrate;

[0062] S200, depositing a conductive material layer on a substrate; the conductive material layer is electrically connected to the thin film transistor 10 and the metal wiring 60 of the display panel respectively;

[0063] S300, etching and patterning the conductive material layer to form an anode 20 conductive material layer and a pad conductive material layer;

[0064] S400 , performing high temperature annealing treatment on the conductive material layer of the anode 20 and the conductive material layer of the pad to form a first densification layer 21 of the anode 20 and a second densification layer of the pad.

[0065] Specifically, in step S100, the substrate is a thin film transistor 10 substrate. In the process of manufacturing the thin film transistor 10 substrate, a buffer layer is first formed on a glass substrate. Then, the channel, the gate 13 insulating layer, the gate 13, the source 11, and the drain 12 are sequentially arranged on the buffer layer, so as to form the thin film transistor 10 of the display panel.

[0066] The metal wiring 60 is formed in the same manufacturing process as the source 11 and the drain 12 of the thin film transistor 10 and is electrically connected to each other. The metal wiring 60 is used to transmit power and signals required by the display panel when it is working.

[0067] After the source electrode 11, the drain electrode 12, and the metal wiring 60 are formed, the passivation layer 40 will be formed thereon. The passivation layer 40 covers the source electrode 11 and the drain electrode 12 of the thin film transistor 10. The passivation layer 40 has both an insulating effect and gives the display panel toughness when it is bent, so as to protect the display panel.

[0068] The present invention then forms the planarization layer 50 on the passivation layer 40. It should be noted that the planarization layer 50 does not cover the side area of ​​the display panel when it is formed. The display panel adopts the chip-on-film technology to achieve a narrow frame design, so the side area of ​​the display panel must reserve space to provide a flexible circuit board of the chip-on-film to bind the metal trace 60.

[0069] The planarization layer 50 is then patterned. The present invention opens the second through hole at a position on the planarization layer 50 corresponding to one of the source 11 and the drain 12 of the thin film transistor 10 to expose the passivation layer 40 under the second through hole.

[0070] The passivation layer 40 is then patterned. The present invention opens the first through hole at a position on the passivation layer 40 corresponding to the second through hole to expose one of the source 11 and the drain 12 of the thin film transistor 10. At the same time, the present invention also opens the third through hole at a position on the passivation layer 40 corresponding to the metal wiring 60 to expose the metal wiring 60 under the passivation layer 40. In other words, the first through hole and the third through hole are opened by the same process. The third through hole is located in the side area of ​​the display panel, that is, the area where the flexible circuit board providing the flip chip film is bound to the metal wiring 60.

[0071] Since the anode 20 to be formed subsequently will need to pass through the planarization layer 50 and the passivation layer 40 at one time to electrically connect to one of the source 11 and the drain 12 of the thin film transistor 10, the display panel must provide a through hole penetrating the planarization layer 50 and the passivation layer 40. However, the method for forming the through hole in the prior art is: first, after the passivation layer 40 is formed, a temporary through hole penetrating the passivation layer 40 is opened; then, the planarization layer 50 is formed on the passivation layer 40 to fill the temporary through hole; finally, the planarization layer 50 is exposed and developed once again to open a deep hole penetrating the planarization layer 50 and the temporary through hole at one time. It can be understood that the process difficulty of opening the deep hole is relatively large. When the exposure is incomplete, the material of the planarization layer 50 may remain in the deep hole, so that the deep hole is not completely opened, which easily leads to the problem of poor electrical signal transmission of the anode 20 formed subsequently.

[0072] The first through hole and the second through hole are opened through two processes respectively. The second through hole is opened on the planarization layer 50 first, and then the first through hole is opened on the passivation layer 40 corresponding to the second through hole, which can avoid the problem of the prior art that the material of the planarization layer 50 remains in the second through hole and the first through hole due to the deep hole opened in the planarization layer 50. Therefore, the present invention can increase the yield of the electrical connection between the anode 20 and one of the source 11 and the drain 12 of the thin film transistor 10.

[0073] At the same time, the second through hole and the first through hole with overlapping hole positions are opened on the planarization layer 50 and the passivation layer 40 in order to sequentially open the deep hole. After the second through hole is opened on the planarization layer 50, the planarization layer 50 is subjected to a high temperature baking process. Since the first through hole has not yet been opened on the passivation layer 40, the source 11 and the drain 12 of the thin film transistor 10 can be protected from corrosion by oxidation and other elements.

[0074] The anode 20 and the bonding pad 30 are then formed on the planarization layer 50 and the passivation layer 40. The anode 20 passes through the first through hole and the second through hole to electrically connect to one of the source 11 and the drain 12 of the thin film transistor 10. Furthermore, the bonding pad 30 passes through the third through hole to electrically connect to the metal trace 60.

[0075] In step S200, the conductive material layer can be deposited by a magnetron sputtering process of physical vapor deposition (PVD). In step S300, the conductive material layer can be etched and patterned by exposure and development to form a conductive material layer of the anode 20. It should be noted that the pad conductive material layer does not need to be patterned to increase the area of ​​the binding pad 30. In step S400, the display panel can be placed in a curing furnace for high-temperature treatment as a whole, and the treatment temperature is set to 200°C to 300°C, for example, 200°C, 250°C or 300°C; and / or, the treatment time is set to 1 hour to 3 hours, for example, 1 hour, 2 hours or 3 hours.

[0076] The conductive material layer after high temperature annealing can form a densified layer, which is acid-resistant. Therefore, even if the conductive material layer is etched by acidic liquid again, the first densified layer 21 and the second densified layer can be effectively retained, thereby forming a structurally stable binding pad 30.

[0077] For example, please refer to Figures 2 to 4 and Figure 6 , Figures 2 to 4 A schematic diagram of the structure of a manufacturing process of a display panel provided in an embodiment of the present application; Figure 6 A detailed schematic diagram of a method for preparing a display panel provided in an embodiment of the present application.

[0078] The conductive material layers include a first transparent material layer, a reflective material layer, and a second transparent material layer;

[0079] The step of depositing a conductive material layer on the substrate comprises:

[0080] S210, depositing the first transparent material layer, the reflective material layer and the second transparent material layer in sequence on the substrate; wherein the first transparent material layer can be crystallized after being heated;

[0081] The step of performing high temperature annealing on the anode 20 conductive material layer and the pad conductive material layer comprises:

[0082] S410 , performing high temperature annealing treatment on the anode 20 conductive material layer and the pad conductive material layer to make the first transparent material layer crystallized and densified.

[0083] Exemplarily, after the step of performing high temperature annealing on the conductive material layer of the anode 20 and the conductive material layer of the pad, the step further includes:

[0084] S500, etching the pad conductive material layer to etch away the reflective material layer and the second transparent material layer of the pad conductive material layer.

[0085] The first transparent material layer may be made of indium tin oxide (ITO), which can be crystallized and solidified after high-temperature treatment, thereby forming a structurally stable binding pad 30. The reflective material layer may be made of silver metal to increase the reflectivity of the reflective material layer to light. The second transparent material layer may be made of indium zinc oxide (IZO), which will not be crystallized and solidified after high-temperature treatment, thereby being etched away in a subsequent etching process, so that only the first densification layer 21 remains on the binding pad 30.

[0086] Exemplarily, the step of etching and patterning the conductive material layer includes:

[0087] S310, exposing the conductive material layer using a grayscale mask 70; the grayscale mask 70 includes a light-transmitting area 71 and a semi-light-transmitting area 72;

[0088] S320 , etching the exposed conductive material layer to form an anode 20 conductive material layer corresponding to the light-transmitting area 71 , and a pad conductive material layer corresponding to the semi-light-transmitting area 72 .

[0089] Specifically, the display panel includes a display area and a binding area, the light-transmitting area 71 corresponds to the display area, and the semi-light-transmitting area 72 corresponds to the binding area. The grayscale mask 70 is a positive photoresist, that is, the portion of the conductive material layer not covered by the grayscale mask 70 after exposure will be dissolved after exposure and development; therefore, by forming the anode 20 pattern in the light-transmitting area 71 of the grayscale mask 70 in advance, the display area can form an anode 20 conductive material layer with a corresponding pattern after exposure and development. Affected by the semi-light-transmitting area 72 of the grayscale mask 70, only the second transparent material layer and the reflective material layer in the binding area are affected by the exposure during the exposure process. It can be understood that the first etching after exposure is to obtain the pattern of the anode 20 conductive material layer, and the pad conductive material layer does not need to be patterned.

[0090] After the first etching to obtain the conductive material layer of the anode 20 located in the display area, after step S410, the first transparent material layer in the display area and the binding area will be crystallized and densified; it should be noted that crystallization and densification will not affect the performance of the first transparent material layer as the anode 20.

[0091] After the first transparent material layer is crystallized and densified, the conductive material layer is etched for the second time using an acidic solution (such as silver acid). Since the reflective material layer and the second transparent material layer forming the anode 20 pattern in the display area are not exposed, they will not be etched away in the second etching, so that the reflective material layer and the second transparent material layer of the conductive material layer of the anode 20 can be retained. The reflective material layer and the second transparent material layer in the binding area have been exposed before the first etching, so they will be etched away by the acidic solution in the second etching; the first transparent material layer in the binding area is not exposed, and is crystallized and densified by high temperature treatment, so it will not be affected by the acidic solution, and can be effectively retained in the second etching to form the binding pad 30.

[0092] In order to reduce the influence of the grayscale mask 70 on the second etching effect, illustratively, before step S500, step S420 may be further included: removing the semi-transparent area 72 of the grayscale mask 70. In this way, the reflective material layer and the second transparent material layer in the binding area can be etched more thoroughly to improve the structural stability of the binding pad 30.

[0093] The display panel provided in the embodiment of the present application sets both the anode 20 and the binding pad 30 as an acid-resistant densification layer, which can avoid the problem of failure of the anode 20 or the binding pad 30 due to oxidation or sulfurization, so as to improve the structural stability of the binding pad 30. In addition, the anode 20 and the binding pad 30 can be made of the same material, that is, they can be made of the same material through the same process, so that there is no need to prepare the binding pad 30 separately after the anode 20 is made. Therefore, compared with the display panel of the prior art, which has an additional manufacturing process of using molybdenum or molybdenum alloy to make the binding pad 30, the present invention can reduce the manufacturing process and required manufacturing materials of the display panel, and greatly reduce the manufacturing time and manufacturing cost of the display panel.

[0094] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.

[0095] In the description of the present application, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more features. The display panel provided in the embodiment of the present application is introduced in detail above. Specific examples are used in this article to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method of the present application and its core idea; at the same time, for those skilled in the art, according to the idea of ​​the present application, there will be changes in the specific implementation methods and scope of application. In summary, the content of this specification should not be understood as a limitation on the present application.

Claims

1. A display panel, characterized in that: include: an anode electrically connected to the thin film transistor of the display panel, wherein the anode comprises a first densification layer, and the first densification layer is acid-resistant; as well as A binding pad electrically connected to a metal trace of the display panel, wherein the binding pad is electrically connected to a thin film transistor of the display panel through the metal trace, wherein the binding pad comprises a second densification layer, wherein the second densification layer is acid-resistant; wherein the first densification layer and the second densification layer are made of the same material, wherein the first densification layer and the second densification layer are formed by the same process, wherein the first densification layer and the second densification layer comprise a crystalline layer of indium tin oxide, and wherein the second densification layer protects the metal trace to prevent the metal trace from being oxidized.

2. The display panel according to claim 1, characterized in that: The anode further comprises a reflective layer and a transparent conductive oxide layer. The reflective layer is arranged on a side of the first densification layer away from the thin film transistor, and the transparent conductive oxide layer is arranged on a side of the reflective layer away from the first densification layer.

3. The display panel according to any one of claims 1 to 2, characterized in that: The display panel further comprises a passivation layer and a planarization layer, wherein the passivation layer is disposed on the thin film transistor and covers the thin film transistor, and the passivation layer comprises a first through hole opened on the thin film transistor; the planarization layer is disposed on the passivation layer, and the planarization layer comprises a second through hole corresponding to the first through hole; The anode passes through the first through hole and the second through hole to be electrically connected to the thin film transistor.

4. The display panel according to claim 3, characterized in that: The metal wiring is arranged in the same layer as the source and drain of the thin film transistor, and the binding pad is electrically connected to the thin film transistor through the metal wiring; Wherein, the passivation layer further includes a third through hole opened on the metal wiring, and the binding pad passes through the third through hole to be electrically connected to the metal wiring.

5. A display device, characterized in that: The device comprises a controller and the display panel according to any one of claims 1 to 4, wherein the controller is electrically connected to the display panel.

6. A method for preparing a display panel, characterized in that: The following steps are involved: Providing a substrate, on which thin film transistors and metal wiring are arranged; depositing a layer of conductive material on a substrate; The conductive material layer is electrically connected to the thin film transistors and metal wiring of the display panel respectively; Etching and patterning the conductive material layer to form an anode conductive material layer and a pad conductive material layer, wherein the anode conductive material layer and the pad conductive material layer are made of the same material; The anode conductive material layer and the pad conductive material layer are subjected to high temperature annealing treatment to form a first densification layer of the anode and a second densification layer of the pad, wherein the first densification layer and the second densification layer comprise a crystalline layer of indium tin oxide, and the second densification layer protects the metal wiring to prevent the metal wiring from being oxidized.

7. The method for preparing a display panel according to claim 6, characterized in that: The conductive material layer includes a first transparent material layer, a reflective material layer, and a second transparent material layer; The step of depositing a conductive material layer on the substrate comprises: Depositing the first transparent material layer, the reflective material layer and the second transparent material layer on the substrate in sequence; wherein the first transparent material layer can be crystallized after being heated; The step of performing high temperature annealing on the anode conductive material layer and the pad conductive material layer comprises: The anode conductive material layer and the pad conductive material layer are subjected to high temperature annealing treatment to make the first transparent material layer crystallized and dense.

8. The method for preparing a display panel according to claim 7, characterized in that: After the step of performing high temperature annealing on the anode conductive material layer and the pad conductive material layer, the step further includes: The pad conductive material layer is etched to etch away the reflective material layer and the second transparent material layer of the pad conductive material layer.

9. The method for preparing a display panel according to claim 7, characterized in that: The step of etching and patterning the conductive material layer comprises: The conductive material layer is exposed using a grayscale mask, wherein the grayscale mask comprises a light-transmitting area and a semi-light-transmitting area; The exposed conductive material layer is etched to form an anode conductive material layer corresponding to the light-transmitting area and a pad conductive material layer corresponding to the semi-light-transmitting area.

10. The method for manufacturing a display panel according to claim 6, characterized in that: In the step of performing high temperature annealing treatment on the anode conductive material layer and the pad conductive material layer, the treatment temperature is set to 200° C. to 300° C.; and / or the treatment time is set to 1 hour to 3 hours.