Foam cement plugging method

By using foam cement during the drilling process, the problems of high density of conventional cement slurry and poor cement injection accuracy are solved, and a low-cost, high-success-rate plugging effect is achieved. By reducing the liquid column pressure and improving the strength of the cement stone, the formation of Effective cement tape seals formation cracks.

CN115405254BActive Publication Date: 2024-10-01SINOPEC OILFIELD SERVICE CORPORATION +2
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202210950732.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-08-09
Publication Date
2024-10-01
Estimated Expiration
2042-08-09

AI Technical Summary

Technical Problem

During the drilling process, due to the formation of caves, cracks or connection with the groundwater system, conventional cement slurry has high density and high liquid column pressure, resulting in the cement being unable to effectively seal the leaking layer, and the accuracy of cement injection is poor, which can easily lead to repeated leakage.

Method used

Foam cement is used as the leakage plugging material, and a low-density cement slurry is prepared by mixing surfactant into conventional or double-fast cement and filling it with nitrogen to reduce the wellbore liquid column pressure, optimize the fluidity and solidification time of cement, and first inject conventional The foam cement forms cement stone, and then the double-fast foam cement is squeezed back to increase the strength of the cement stone and form an effective cement belt to seal the formation.

Benefits of technology

It achieves the effects of low cost, simple operation and high leakage plugging success rate, effectively reduces the wellbore liquid column pressure, improves the retention and filling capacity of cement in the leakage layer, and ensures the success and durability of leakage plugging.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure GDA0004894999340000041
    Figure GDA0004894999340000041
Patent Text Reader

Abstract

The present invention discloses a foam cement plugging method, which solves the problems of high leakage rate and easy re-leakage in traditional cement plugging. The method comprises the following steps: lowering the drilling tool to the bottom of the well, injecting 10-20m of plugging slurry 3 ; Inject the foam cement of the borehole volume at the bottom of the well; After the injection is completed, quickly lift the drill to the wellhead, close the well sealer and perform back-squeezing cement construction; Back-squeeze the foam cement of the borehole volume, drill down to sweep the plug, and sweep the plug to the bottom of the well without leakage, then the plugging is successful. The invention has low cost, simple operation, low column pressure, strong compressibility, good cement stone plasticity, high displacement efficiency, and high plugging success rate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of drilling in the oil drilling industry, in particular to a plugging method for leaking wells that occurs during the drilling process. Background Art

[0002] Due to the presence of caves, cracks or connections with underground water systems in the strata, return leakage often occurs during drilling. For return leakage, conventional plugging materials have small particles and cannot effectively seal the leaking layer. Even if the plugging is successful, the strength is low and it is easy to leak again. The commonly used ordinary cement slurry for plugging has the following problems: (1) The cement slurry has a high density, high liquid column pressure, and low formation pressure bearing capacity, which easily leads to cement leakage from cracks, caves and water systems, and cannot form an effective cement plug. (2) To inject conventional cement, the drill pipe must be lowered to the vicinity of the leaking layer. Since the leaking layer is often near the liquid surface in the well, it is not easy to observe. It cannot be guaranteed that the drill pipe can be accurately aligned with the leaking layer, and it cannot be guaranteed that the cement slurry can be accurately injected into the leaking layer, which can easily lead to failure of the plugging construction; (3) The strength of conventional cement decreases after mixing with the fluid in the well, which can easily lead to re-leakage. Summary of the invention

[0003] The purpose of the present invention is to solve the above technical problems and to provide a foam cement plugging method which has the advantages of low cost, simple operation, low column pressure, strong compressibility, good cement stone plasticity, high displacement efficiency and high plugging success rate.

[0004] The method of the present invention comprises the following steps:

[0005] 1) Lower the drilling tool to the bottom of the well and inject plugging slurry 10-20m 3 ;

[0006] 2) Inject the foam cement in the amount of the wellbore volume at the bottom of the well;

[0007] 3) After the positive injection is completed, the drilling tool is quickly lifted to the wellhead, and the well sealer is closed to carry out cement back-squeezing construction;

[0008] 4) Back-squeeze the foam cement to the volume of the wellbore, drill down to sweep the plug, and sweep the plug to the bottom of the well without leakage, then the plugging is successful.

[0009] The foamed cement in step 2) is conventional foamed cement, and its preparation method is as follows: a surfactant is mixed into conventional cement, and nitrogen is injected to foam the cement to prepare a 0.70-0.80 g / cm 3 Low density cement slurry.

[0010] In the step 2), during the injection process, attention is paid to the slurry return at the wellhead. If slurry returns, grouting is stopped immediately and the drilling tool is quickly lifted to the wellhead.

[0011] The foamed cement in step 4) is double-fast foamed cement, and the preparation method thereof is as follows: a surfactant is mixed into the double-fast cement, and nitrogen is injected into the cement to foam the cement to prepare a 0.70-0.80 g / cm 3 Low density cement slurry.

[0012] In the step 4), if the wellhead pressure continues to rise during the back squeezing process, the back squeezing operation is stopped.

[0013] In the method of the present invention, the conventional cement is commercially available with a density of 1.50-1.90 g / cm 3 Ordinary cement; the double-fast cement is commercially available cement with the characteristics of fast setting and hardening and high hourly strength, namely the so-called "hourly cement". The surfactant can be calcium chloride, potassium chloride, soda ash, salt or sodium silicate, etc., and its addition amount is preferably 1%-3% of the cement mass.

[0014] Beneficial effects:

[0015] The present invention adopts foam cement to replace conventional cement, which has a density of 1.50-1.90 g / cm 3 The foam cement slurry has a low density and can effectively reduce the liquid column pressure in the wellbore. The foam slurry has poor fluidity and is easy to stay in the leaking layer. In addition, the optimized use of quick-setting cement has a short initial setting time. After the initial setting, it continues to accumulate and fill at the leaking point, forming a "cement belt" near the leaking zone to seal the formation cracks and achieve the purpose of plugging. According to the characteristics of foam cement, the method of the present invention first injects plugging slurry to reduce the leakage rate, then injects conventional foam cement to form cement stone in the leaking layer, and finally squeezes the double-fast foam cement of the wellbore volume to further improve the strength of the cement stone, and effectively plugs the leak after waiting for setting. The method of the present invention is extremely simple, the raw materials are easy to obtain, the amount of plugging slurry used is effectively reduced, the production cost is low, the processing cycle is short, the plugging success rate is high, and it plays an important role in the occurrence of well leakage during drilling. DETAILED DESCRIPTION

[0016] In the following examples, the conventional foamed cement is prepared by mixing a surfactant into conventional cement and injecting nitrogen to foam the cement to prepare a 0.70-0.80 g / cm 3 Low-density cement slurry. In this embodiment, the conventional cement is purchased from Jiahua with a grade G cement, a cement setting time of 240-300 minutes, and a cement slurry density of 1.50-1.90 g / cm 3 ;

[0017] The preparation method of the double-fast foamed cement is as follows: a surfactant is mixed into the double-fast cement, and nitrogen is injected to foam the cement to prepare a 0.70-0.80 g / cm 3Low-density cement slurry. In this embodiment, the double-fast cement is purchased from Jiahua with a grade G cement. By adding a coagulant, the cement setting time is 60-150 minutes, and the cement slurry density is 1.50-1.80 g / cm 3 Double fast cement.

[0018] The specific method is:

[0019] ① Lower the drilling tool to the bottom of the well and inject plugging slurry 10-20m 3 , mainly to reduce the leakage rate and provide guarantee for the effective retention of foam cement.

[0020] ② Inject the conventional foam cement of the borehole volume at the bottom of the well, the purpose is to let the cement enter the leaking layer and form cement stone in the leaking layer. During the injection process, pay attention to the slurry return from the wellhead. If there is slurry return, stop grouting immediately and quickly lift the drill tool to the wellhead.

[0021] ③ In order to prevent the cement from solidifying prematurely and causing a "flagpole", the drilling tool should be quickly lifted to the wellhead, and the well sealer should be closed to carry out reverse cement extrusion construction.

[0022] ④ Back-squeeze the double-fast foam cement in the wellbore to squeeze the cement into the leaky layer and improve the strength of the cement stone. If the wellhead pressure continues to rise during the back-squeeze process, stop the back-squeeze operation.

[0023] ⑤ After the foam cement is plugged, wait for it to solidify for 24 hours, then drill down to sweep the plug. If there is no leakage at the bottom of the well, the plugging is successful.

[0024] Application case: Jiaoye 18-4HF well application case

[0025] 1. Basic Information Geographic location: Group 2, Xihuicang Village, Shiqiang Town, Nanchuan District, Chongqing Structural location: North of Wanxian syncline and Dongsheng anticline in the high and steep fold belt of eastern Sichuan, Sichuan Basin Well type: development well; Well type: horizontal well Designed well depth: 6058m; Horizontal section length: 1800m; Altitude 753.1m

[0026] Completed drilling layer: Wufeng-Longmaxi Formation Long 1st Section ① Upper-③ Lower Small Layer

[0027] Shengye 18-4HF Wellbore Structure Design Data

[0028]

[0029] At 22:30 on March 10, 2022, the second drilling was carried out to a depth of 762m and leakage occurred. In the Jialing River Formation, clear water was used to drill to a depth of 861m to carry out foam cement plugging work.

[0030] 2. Construction process:

[0031] ① Drill down to 790m and inject plugging slurry for 20m 3, cement slurry (conventional foam cement) is being injected 94m 3 , cement slurry density 1.85g / cm 3 (Density after nitrogen filling 0.7-0.8g / cm 3 );

[0032] ② Grab the drilling tools out of the well;

[0033] ③Double drill pipes are connected to the wellhead, and the well is shut down and reverse squeeze cement slurry (double fast foam cement) is 88m 3 , cement slurry density 1.75-1.85g / cm 3 (After nitrogen filling, the density reaches 0.8g / cm 3 );

[0034] ④ Shut in the well and hold the pressure to wait for 24 hours, then lower the drilling plug to a plug surface of 50m. Using a drilling pressure of 1-2 tons, drill the plug to a well depth of 861m without leakage, and the plugging was successful.

[0035] So far, the method of the present invention has been used to plug leaks five times in Shengli Oilfield and Fuling Shale Gas Field, with a success rate of 80%, and only one well has recurrent leakage.

Claims

1. A foam cement plugging method, characterized in that: The following steps are involved: 1) Lower the drilling tool to the bottom of the well and inject plugging slurry 10-20m 3 ; 2) injecting foam cement in an amount corresponding to the volume of the wellbore at the bottom of the well; the foam cement is conventional foam cement, and the preparation method thereof is as follows: a surfactant is mixed into conventional cement, and nitrogen is injected to foam the cement to prepare 0.70-0.80 g / cm 3 Low-density cement slurry; 3) After the positive injection is completed, quickly lift the drilling tool to the wellhead, close the well sealer and carry out reverse cementing construction; 4) Back-squeeze the foam cement of the borehole volume, drill down and sweep the plug, and when there is no leakage at the bottom of the well, the plugging is successful; the foam cement is double-fast foam cement, and its preparation method is: a surfactant is mixed into the double-fast cement, and nitrogen is filled to foam the cement to prepare 0.70-0.80g / cm 3 Low density cement slurry.

2. The foam cement plugging method according to claim 1, characterized in that: In the step 2), during the injection process, attention is paid to the slurry return at the wellhead. If slurry returns, grouting is stopped immediately and the drilling tool is quickly lifted to the wellhead.

3. The foam cement plugging method according to claim 1, characterized in that: In the step 4), if the wellhead pressure continues to rise during the back squeezing process, the back squeezing operation is stopped.

Citation Information

Patent Citations

  • Foam cement slurry system and composition

    CN103525387A

  • Positive injection back squeeze well cementation method for low pressure and leaky well

    CN106555565A

  • Fine sand plugging thick liquid annular space anti-injection anti-extrusion plugging method

    CN107035338A