A method and device for cutting a crystal rod
By dynamically adjusting the mortar temperature, the problem that the mortar temperature cannot be effectively controlled in the prior art is solved according to the relationship between the cutting depth and the contact area, the warpage of the silicon carbide wafer is significantly reduced and the cutting quality is improved.
Patent Information
- Application Number
- CN202211079693.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-05
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2042-09-05
AI Technical Summary
In the processing of semiconductor materials, the mortar temperature cannot be dynamically adjusted during the cutting process, resulting in a small contact area in the initial cutting. The contact area increases after deep cutting, and the heat generation is greatly increased. The mortar temperature cannot be effectively controlled, which affects silicon carbide. The quality of the wafer, especially the warpage of the wafer, is difficult to control.
By obtaining the mortar temperature information sprayed on the cutting line, the mortar temperature is dynamically adjusted based on the negative correlation between the contact area and the cutting depth to ensure the temperature stability of the cutting line and the crystal rod at different cutting positions, and reducing the warpage of the wafer.
The mortar temperature is maintained throughout the cutting process, avoiding defects caused by insufficient cutting capacity, significantly reducing the warpage of the silicon carbide wafer and improving the processing quality of the wafer.
Smart Images

Figure CN115416170B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor material processing, and more specifically, to a crystal rod cutting method and a cutting device. Background Art
[0002] At present, the mortar temperature for multi-wire cutting is usually set to a fixed temperature, and the mortar temperature is controlled by a cooler. However, it does not take into account that the cutting process is dynamic. At the beginning of cutting, the contact area between the steel wire and the crystal rod is small, and the heat generation is relatively small. As the cutting process progresses, the contact area between the steel wire and the crystal rod gradually increases, and the heat generation also increases significantly. At this time, it is obviously unreasonable to control the mortar temperature to be the same as the initial cutting stage. Finding the appropriate mortar temperature at each stage of the cutting process is an important challenge faced by improving the surface shape of silicon carbide wafers. Summary of the invention
[0003] In view of this, the present application provides a method and a device for cutting a crystal rod, and the scheme is as follows:
[0004] A method for cutting a crystal rod, the cutting method comprising:
[0005] During the process of cutting the crystal rod, obtaining temperature information of the cutting line sprayed with mortar;
[0006] Based on the temperature information, the temperature of the mortar sprayed on the cutting line is controlled, and the temperature of the mortar sprayed on the cutting line is controlled to be negatively correlated with the contact area between the cutting line and the crystal rod.
[0007] Preferably, in the above cutting method, before obtaining the temperature information of the cutting line, the method further comprises:
[0008] Mounting the crystal rod on a workbench, and moving the workbench to a cutting start position;
[0009] Turn on the mortar spraying device, spray the mortar on the surface of the cutting line, and start cutting.
[0010] Preferably, in the above cutting method, the method for obtaining the temperature information of the cutting line includes:
[0011] The temperature information of the cutting line sprayed with mortar in the cutting machine cabin is obtained by a temperature sensor placed in the cutting machine cabin.
[0012] Preferably, in the above-mentioned cutting method, controlling the temperature of the mortar sprayed on the cutting line to be negatively correlated with the contact area between the cutting line and the crystal rod comprises:
[0013] When the cutting depth is not greater than R / 2, the temperature of the mortar decreases as the cutting depth of the crystal rod increases, and the end diameter of the cut position of the crystal rod is R;
[0014] When the cutting depth is not less than R / 2, the temperature of the mortar increases with the increase of the cutting depth of the crystal rod.
[0015] Preferably, in the above cutting method, reducing the temperature of the mortar as the cutting depth of the crystal rod increases comprises:
[0016] During the cutting process of the crystal rod from 0 to R / 3, the temperature of the mortar decreases as the cutting depth increases, and the temperature decrease range is no more than 1°C;
[0017] During the cutting process of the crystal rod with a cutting depth from R / 3 to R / 2, the temperature of the mortar decreases as the cutting depth increases, and the temperature decrease range is no more than 0.5°C.
[0018] Preferably, in the above cutting method, increasing the temperature of the mortar as the cutting depth of the crystal rod increases comprises:
[0019] During the cutting process of the crystal rod from R / 2 to 2R / 3, the temperature of the mortar increases with the increase of the cutting depth, and the temperature increase range is not greater than 0.5°C;
[0020] During the cutting process of the crystal rod from 2R / 3 to R, the temperature of the mortar increases with the increase of the cutting depth, and the temperature increase range is not greater than 1°C.
[0021] Preferably, in the above cutting method, the temperature range of the mortar is 20-25°C.
[0022] The present application also proposes a crystal rod cutting device, the scheme of which is as follows:
[0023] A crystal rod cutting device, the cutting device comprising:
[0024] cutting the cabin;
[0025] A groove wheel located in the cutting machine cabin is used to drive the cutting line to rotate;
[0026] A controller is used to obtain temperature information of a cutting line sprayed with mortar during cutting of the crystal rod, and based on the temperature information, control the temperature of the mortar sprayed on the cutting line, and control the temperature of the mortar sprayed on the cutting line to be negatively correlated with the contact area between the cutting line and the crystal rod.
[0027] Preferably, in the above-mentioned cutting device, the cutting device further comprises:
[0028] a temperature sensor located within the cutting chamber;
[0029] The controller is connected to the temperature sensor and is used for obtaining temperature information of the cutting line sprayed with mortar through the temperature sensor.
[0030] Preferably, in the above-mentioned cutting device, when the cutting depth is not greater than R / 2, the controller is used to reduce the temperature of the mortar as the cutting depth of the crystal rod increases, and the end face diameter of the cut position of the crystal rod is R;
[0031] When the cutting depth is not less than R / 2, the controller is used to increase the temperature of the mortar as the cutting depth of the crystal rod increases.
[0032] From the above, it can be known that the present application proposes a method and a device for cutting a crystal rod, the cutting method comprising: obtaining temperature information of a cutting line sprayed with mortar during the process of cutting the crystal rod; based on the temperature information, controlling the temperature of the mortar sprayed on the cutting line, and controlling the temperature of the mortar sprayed on the cutting line to be negatively correlated with the contact area between the cutting line and the crystal rod. In the present application, as the cutting line is closer to the middle position of the crystal rod, the temperature of the mortar is gradually reduced, and as the cutting line is away from the center position of the crystal rod, the temperature of the mortar is gradually increased, so that the temperature of the crystal rod and the cutting line at different cutting positions remains stable, thereby achieving the purpose of reducing the warpage of the wafer, that is, dynamically adjusting the temperature of the mortar according to the different cutting depths of the cutting line, so that the cutting ability of the cutting line remains stable during the entire cutting process, avoiding defects caused by insufficient cutting ability, thereby achieving the purpose of reducing the warpage of the wafer. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] In order to more clearly illustrate the technical solutions in the embodiments of the present application or the related technologies, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying any creative work.
[0034] The structures, proportions, sizes, etc. illustrated in the drawings of this specification are only used to match the contents disclosed in the specification so as to facilitate understanding and reading by persons familiar with this technology. They are not used to limit the conditions under which this application can be implemented, and therefore have no substantive technical significance. Any structural modification, change in proportion or adjustment of size, without affecting the effects and purposes that can be achieved by this application, should still fall within the scope of the technical contents disclosed in this application.
[0035] Figure 1 A schematic diagram of the principle of multi-wire cutting of a crystal rod;
[0036] Figure 2 A schematic diagram of a process for cutting a crystal rod provided in the present application;
[0037] Figure 3 A schematic diagram of a process flow of another crystal rod cutting method provided in the present application;
[0038] Figure 4 A schematic diagram of a process flow of another crystal rod cutting method provided in the present application;
[0039] Figure 5 This is a graph showing the change of mortar temperature with cutting depth in the embodiment of the present application;
[0040] Figure 6 A schematic structural diagram of a crystal rod cutting device provided in an embodiment of the present application. DETAILED DESCRIPTION
[0041] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the embodiments in the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.
[0042] With the rapid development of semiconductor technology and optoelectronic technology, the demand for silicon carbide wafers has increased year by year. The main manufacturing process of silicon carbide wafers is: crystal growth - cutting (slicing) - grinding - polishing. Among them, the cutting process is one of the key processes in the manufacturing and processing of silicon carbide wafers. The quality of cutting processing directly affects the quality of subsequent processing. Among the wafers obtained in the cutting process, the wafer warp (Warp) is an important indicator for evaluating wafer deformation. The wafer warp usually refers to the distance between the highest point and the lowest point of the middle surface of the wafer without the influence of external force. In actual production, the wafer warp is usually difficult to repair, and it will cause the wafer axis to deviate from the crystal axis in subsequent processing, affecting the quality of subsequent processing. Therefore, during the cutting process, the value of the wafer warp needs to be strictly controlled. Among them, multi-wire cutting technology is currently the most advanced silicon carbide wafer processing technology in the world.
[0043] refer to Figure 1 , Figure 1This is a schematic diagram of the principle of multi-wire cutting of a crystal rod. The basic principle of multi-wire cutting is that the groove wheel 1 drives the cutting wire 2 wound on the groove wheel 1 to move at high speed to drive the high-hardness abrasive particles to grind and remove the material to achieve slicing of the material. The sand particles move and roll during the cutting process. The high-hardness abrasive particles exist in the form of mortar, and the choice of the cutting wire 2 is mostly steel wire.
[0044] like Figure 1 As shown, during the multi-wire cutting process, a large amount of heat will be generated as the cutting wire 2, mortar and crystal rod 3 continue to move relative to each other. The mortar as a cutting medium must take away the generated heat to maintain the normal operating temperature of the system. Otherwise, the generated heat will accumulate, causing the temperature of the mortar and the crystal rod to gradually increase, and eventually have a serious impact on the quality of the chip (such as total thickness change, warpage, etc.), and even cause wire breakage in severe cases. Therefore, controlling the temperature of the mortar during the cutting process is particularly important for improving the quality of the chip.
[0045] The prior art usually sets a fixed mortar temperature and uses a cooling machine to control the mortar temperature. However, the cutting process is changing. At the beginning of cutting, the contact area between the cutting line 2 and the crystal rod 3 is small, and the heat generation is relatively small. As the cutting process progresses, the contact area between the cutting line 2 and the crystal rod 3 gradually increases, and the heat generation also increases significantly.
[0046] Based on the above-mentioned problems, the present application proposes a method and device for cutting a crystal rod. In the cutting method, during the process of cutting the crystal rod 3, the temperature information of the cutting line 2 sprayed with mortar is obtained; based on the temperature information, the temperature of the mortar sprayed on the cutting line 2 is controlled, and the temperature of the mortar sprayed on the cutting line 2 is controlled to be negatively correlated with the contact area between the cutting line 2 and the crystal rod 3. In the present application, as the cutting line 2 is closer to the middle position of the crystal rod 3, the temperature of the mortar is gradually reduced, and as the cutting line 2 is away from the center position of the crystal rod 3, the temperature of the mortar is gradually increased, so that the temperature of the crystal rod 3 and the cutting line 2 at different cutting positions is kept stable, thereby achieving the purpose of reducing the warpage of the wafer, that is, the temperature of the mortar is dynamically adjusted according to the different cutting depths of the cutting line 2, so that the cutting ability of the cutting line is maintained stable during the entire cutting process, avoiding defects caused by insufficient cutting ability, thereby achieving the purpose of reducing the warpage of the silicon carbide wafer.
[0047] In order to make the above-mentioned objects, features and advantages of the present application more obvious and easy to understand, the present application is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0048] refer to Figure 2 , Figure 2A schematic diagram of a process flow of a crystal rod cutting method provided in the present application, wherein the cutting method comprises:
[0049] Step S13: during the process of cutting the crystal rod 3, obtaining temperature information of the cutting line 2 sprayed with mortar;
[0050] Step S14: Based on the temperature information, the temperature of the mortar sprayed on the cutting line 2 is controlled, and the temperature of the mortar sprayed on the cutting line 2 is controlled to be negatively correlated with the contact area between the cutting line 2 and the crystal rod 3 .
[0051] During the cutting process of the crystal rod 3, the temperature information of the cutting line 2 sprayed with mortar is obtained. The temperature information can be obtained by setting the temperature information in the controller 5; or by setting the temperature sensor 6 in the cutting cabin 4, and obtaining the temperature information of the mortar sprayed on the cutting line 2 through the temperature sensor 6 in the cutting cabin 4. Based on the temperature information, the temperature of the mortar sprayed on the cutting line 2 is controlled, so that the temperature of the mortar sprayed on the cutting line 2 is negatively correlated with the contact area between the cutting line 2 and the crystal rod 3, that is, the larger the contact area between the cutting line 2 and the crystal rod 3, the smaller the mortar temperature on the cutting line 2; the smaller the contact area between the cutting line 2 and the crystal rod 3, the larger the mortar temperature on the cutting line 2. Through this method, the total temperature of the crystal rod 3 and the cutting wire 2 sprayed with mortar at different cutting positions is kept stable during the entire cutting process, thereby achieving the purpose of reducing the warpage of the chip formed by cutting. That is, the above method dynamically adjusts the temperature of the mortar according to the cutting wire 2 at different cutting depths, so that the cutting ability of the cutting wire 2 remains stable during the entire cutting process, avoiding defects caused by insufficient cutting ability, thereby achieving the purpose of reducing the warpage of the chip.
[0052] refer to Figure 3 , Figure 3 Based on the application provided Figure 2 A flow chart of another ingot cutting method is provided, wherein in the above cutting method, before obtaining the temperature information of the cutting line 2, the method further includes:
[0053] Step S11: installing the crystal rod 3 on a workbench, and moving the workbench to a cutting start position;
[0054] Step S12: Turn on the mortar spraying device 7, spray the mortar on the surface of the cutting line 2, and start cutting.
[0055] refer to Figure 3Before obtaining the temperature information of the cutting line 2, the crystal rod 3 to be cut needs to be clamped on the workbench located in the cutting machine cabin 4, with the cutting direction of the crystal rod 3 to be cut being the seed crystal facing outward, and then the workbench with the crystal rod 3 to be cut installed is moved to the starting cutting position, and the mortar dispensing button is turned on, so that the mortar spraying device 7 located in the cutting machine cabin 4 evenly sprays the mortar on the surface of the high-speed moving cutting line 2. The mortar is pumped out of the mortar tank 8 outside the cutting machine by an electric pump. After the mortar is evenly sprayed on the surface of the cutting line 2, cutting begins.
[0056] In the above cutting method, the method for obtaining the temperature information of the cutting line 2 includes:
[0057] The temperature information of the cutting line 2 sprayed with mortar in the cutting cabin 4 is obtained by the temperature sensor 6 disposed in the cutting cabin 4 .
[0058] In the cutting method described above, it is necessary to obtain the temperature information of the cutting line 2. The method for obtaining the temperature information includes setting the temperature sensor 6 in the cutting cabin 4, and obtaining the temperature information of the cutting line 2 sprayed with mortar in the cutting cabin 4 by setting the temperature sensor 6. Based on the method for obtaining temperature information described above, controlling the temperature of the mortar sprayed on the surface of the cutting line 2 includes: setting the temperature sensor 6 in the cutting cabin 4 and in the mortar tank 8, the temperature sensor 6 in the cutting cabin 4 senses the temperature of the mortar sprayed on the surface of the cutting line 2, and feeds back the sensed temperature to the controller 5, and the controller 5 adjusts the mortar temperature in the mortar tank 8 according to the set process parameters.
[0059] In the above-mentioned cutting method, controlling the temperature of the mortar sprayed on the cutting line 2 to be negatively correlated with the contact area between the cutting line 2 and the crystal rod 3 includes:
[0060] When the cutting depth is not greater than R / 2, the temperature of the mortar decreases as the cutting depth of the crystal rod 3 increases, and the end diameter of the cut position of the crystal rod 3 is R;
[0061] When the cutting depth is not less than R / 2, the temperature of the mortar increases with the increase of the cutting depth of the crystal rod 3 .
[0062] In the above-mentioned cutting method, the temperature of the mortar sprayed on the cutting line 2 is controlled to be negatively correlated with the contact area between the cutting line 2 and the crystal rod 3. Wherein, the temperature of the mortar sprayed on the cutting line 2 is controlled by adjusting the temperature of the mortar through the process parameters set in the controller 5. The mortar temperature on the cutting line 2 is negatively correlated with the contact area between the cutting line 2 and the crystal rod 3, including: during the cutting process, when the cutting depth is 0 to R / 2, the mortar temperature is gradually reduced so that it always keeps a monotonically decreasing trend with the cutting depth of the crystal rod 3, even if the temperature of the mortar decreases as the cutting depth of the crystal rod 3 increases; when the cutting depth is R / 2 to R, the mortar temperature is gradually increased so that it always keeps a monotonically increasing trend with the cutting depth of the crystal rod 3, even if the temperature of the mortar increases as the cutting depth of the crystal rod 3 increases; wherein, the end face diameter of the cut position of the crystal rod 3 is R.
[0063] In the above-mentioned cutting method, reducing the temperature of the mortar as the cutting depth of the crystal rod 3 increases includes:
[0064] During the cutting process of the crystal rod 3 from a cutting depth of 0 to R / 3, the temperature of the mortar decreases as the cutting depth increases, and the temperature decrease range is no more than 1°C;
[0065] During the cutting process of the crystal rod 3 from a cutting depth of R / 3 to R / 2, the temperature of the mortar decreases as the cutting depth increases, and the temperature decrease range is no more than 0.5°C.
[0066] In the above method, the temperature of the mortar decreases as the cutting depth of the crystal rod 3 increases, that is, during the cutting process of the cutting depth of the crystal rod 3 from 0 to R / 3, the temperature of the mortar will show a decreasing trend, and the temperature drop interval of the mortar is 0-1°C; during the cutting process of the cutting depth of the crystal rod 3 from R / 3 to R / 2, the temperature of the mortar will decrease as the cutting depth increases, and the temperature drop interval is 0-0.5°C. The cutting method described in the embodiment of the present application can be used for silicon carbide crystal rods with an outer diameter ranging from 50.8mm to 200mm. When cutting the silicon carbide crystal rod with an outer diameter in the range of 50.8mm to 200mm, the temperature of the mortar decreases with the increase of the cutting depth of the silicon carbide crystal rod. The specific changes are: under the preset mortar temperature value, in the stage of cutting depth of 0-R / 5, the temperature of the mortar will gradually decrease by 0.97°C; in the cutting process of cutting depth of R / 5-R / 3, the temperature of the mortar will gradually decrease by 0.39°C; in the cutting process of cutting depth of R / 3-2R / 5, the temperature of the mortar will gradually decrease by 0.11°C; in the stage of cutting depth of 2R / 5-R / 2, the temperature of the mortar will gradually decrease by 0.06°C.
[0067] In the above-mentioned cutting method, increasing the temperature of the mortar as the cutting depth of the crystal rod 3 increases includes:
[0068] During the cutting process of the crystal rod 3 from a cutting depth of R / 2 to 2R / 3, the temperature of the mortar increases with the increase of the cutting depth, and the temperature increase range is not greater than 0.5° C.;
[0069] During the cutting process of the crystal rod 3 from a cutting depth of 2R / 3 to R, the temperature of the mortar increases with the increase of the cutting depth, and the temperature increase range is not greater than 1°C.
[0070] In the cutting method described above, during the cutting process of the crystal rod 3 with a cutting depth from R / 2 to 2R / 3, the temperature of the mortar shows an increasing trend, even if the temperature of the mortar increases with the increase of the cutting depth, the increase range of the mortar temperature is 0-0.5°C; during the cutting process of the crystal rod 3 with a cutting depth from 2R / 3 to R, the temperature of the mortar shows an increasing trend, even if the temperature of the mortar increases with the increase of the cutting depth, the increase range of the mortar temperature is 0-1°C.
[0071] When cutting the silicon carbide crystal rod with an outer diameter in the range of 50.8mm to 200mm, the temperature of the mortar increases with the increase of the cutting depth of the silicon carbide crystal rod. The specific changes are: at the temperature at the cutting depth of R / 2, during the cutting process of the cutting depth of R / 2-3R / 5, the temperature of the mortar gradually increases by 0.06°C; during the cutting process of the cutting depth of 3R / 5-2R / 3, the temperature of the mortar gradually increases by 0.11°C; during the cutting process of the cutting depth of 2R / 3-4R / 5, the temperature of the mortar gradually increases by 0.39°C; during the cutting process of the cutting depth of 4R / 5-R, the temperature of the mortar gradually increases by 1.01°C.
[0072] Obviously, the cutting method described in the embodiment of the present application is not limited to silicon carbide crystal rods, but can also be used for cutting other semiconductor crystal rods, such as single crystal silicon or polycrystalline silicon. The outer diameter of the crystal rod is not limited to 50.8 mm to 200 mm.
[0073] In the above cutting method, the temperature range of the mortar is 20-25°C.
[0074] In multi-wire cutting, the mortar has the functions of cutting, sticking and cooling, so the mortar has a great influence on the effect of multi-wire cutting. During the cutting process, the quality and production efficiency of silicon wafers can be effectively improved by setting the parameters of the mortar. Among them, the function of the mortar is affected by the viscosity, but the temperature directly affects its viscosity. Therefore, the cutting ability of the mortar can be controlled by controlling the temperature, but the temperature of the mortar needs to be controlled within an appropriate temperature range. The temperature of the mortar is generally controlled at 20-25°C. Within this temperature range, the cutting ability of the mortar is the best, and the cutting quality of the wafer formed by cutting is relatively ideal.
[0075] Based on the above cutting method, the present application proposes another specific embodiment:
[0076] refer to Figure 4 , Figure 4 A schematic flow chart of another method for cutting a crystal rod provided in the present application. The method described above is used to cut a silicon carbide crystal rod with an outer diameter of 150±1 mm. The specific steps are as follows:
[0077] Step S21: clamping the silicon carbide crystal rod to be cut on a workbench in a cutting cabin, with the cutting direction of the silicon carbide crystal rod being such that the seed crystal side faces outwards;
[0078] Step S22: moving the workbench to a cutting start position, turning on a mortar dispensing button, and evenly coating the mortar on the surface of the cutting line 2;
[0079] Step S23: starting cutting, and adjusting the temperature of the mortar during the cutting process;
[0080] Step S24: After the cutting is completed, the workbench is lifted from the cutting line to the loading position and then removed.
[0081] refer to Figure 5 , Figure 5 : is a graph showing the change of the mortar temperature with the cutting depth in the embodiment of the present application; wherein the specific operation of adjusting the temperature of the mortar with the change of the cutting depth of the silicon carbide crystal rod is:
[0082] When the cutting depth is 0 mm, the temperature of the mortar is set to 25° C.
[0083] During the cutting process with a cutting depth of 0-20 mm, the temperature of the mortar gradually decreased by 0.72°C;
[0084] During the cutting process with a cutting depth of 20-30 mm, the temperature of the mortar gradually dropped by 0.28°C;
[0085] During the cutting process with a cutting depth of 30-40 mm, the temperature of the mortar gradually dropped by 0.22°C;
[0086] During the cutting process with a cutting depth of 40-50 mm, the temperature of the mortar gradually decreased by 0.16°C;
[0087] During the cutting process with a cutting depth of 50-60 mm, the temperature of the mortar gradually decreased by 0.11°C;
[0088] During the cutting process with a cutting depth of 60-75 mm, the temperature of the mortar gradually decreased by 0.05°C;
[0089] During the cutting process with a cutting depth of 75-90 mm, the temperature of the mortar gradually increased by 0.06°C;
[0090] During the cutting process with a cutting depth of 90-100 mm, the temperature of the mortar gradually increased by 0.11°C;
[0091] During the cutting process with a cutting depth of 100-110 mm, the temperature of the mortar gradually increased by 0.17°C;
[0092] During the cutting process with a cutting depth of 110-120 mm, the temperature of the mortar gradually increased by 0.22°C;
[0093] During the cutting process with a cutting depth of 120-130 mm, the temperature of the mortar gradually increased by 0.28°C;
[0094] During the cutting process with a cutting depth of 130-140 mm, the temperature of the mortar gradually increased by 0.34°C;
[0095] During the cutting process with a cutting depth of 140-150 mm, the temperature of the mortar gradually increased by 0.39°C.
[0096] In this embodiment, when the cutting depth is 0mm, the mortar temperature is set to 25°C. After the cutting starts, during the cutting process with a cutting depth of 0-75mm, the temperature of the mortar gradually decreases as the cutting depth increases, and the degree of decrease gradually slows down; during the cutting process with a cutting depth of 75mm-150mm, the temperature of the mortar gradually increases as the cutting depth increases. During the cutting process of the silicon carbide crystal rod, the closer the cutting position is to the center area of the silicon carbide crystal rod, the larger the contact area between the cutting line 2 and the silicon carbide crystal rod, and the more heat is generated. The farther away from the center area, the smaller the contact area between the cutting line 2 and the silicon carbide crystal rod, and the less heat is generated. By setting the process parameters, the temperature of the mortar is changed, so that the temperature of the mortar gradually decreases as the silicon carbide crystal rod approaches the middle position, and the temperature of the mortar gradually increases as the silicon carbide crystal rod moves away from the center position. This method can neutralize the heat generated by the cutting line 2 and the silicon carbide crystal rod when cutting; thereby achieving the temperature stability of the silicon carbide crystal rod and the cutting line 2 at different cutting positions, reducing the warpage of the cut silicon carbide wafer from more than 30μm to about 20μm, achieving the purpose of reducing the warpage of the silicon carbide wafer, and maintaining the cutting ability of the cutting line 2 stable throughout the cutting process, avoiding defects caused by insufficient cutting ability, and better meeting subsequent processing requirements and improving product yield.
[0097] Based on the above-mentioned method for cutting a crystal rod, the present application also proposes another embodiment: a crystal rod cutting device.
[0098] refer to Figure 6 , Figure 6 A schematic diagram of the structure of a crystal rod cutting device provided in an embodiment of the present application, wherein the cutting device comprises:
[0099] Cutting cabin 4;
[0100] The groove wheel 1 located in the cutting machine cabin 4 is used to drive the cutting line 2 to rotate;
[0101] A controller 5 is used to obtain temperature information of a cutting line 2 sprayed with mortar during cutting of the crystal rod 3, and based on the temperature information, control the temperature of the mortar sprayed on the cutting line 2, so that the temperature of the mortar sprayed on the cutting line 2 is negatively correlated with the contact area between the cutting line 2 and the crystal rod 3.
[0102] The cutting device includes a cutting machine cabin 4, in which there are a groove wheel 1 and a controller 5, and a cutting line 2 is arranged on the groove wheel 1, and the cutting line 2 performs a reciprocating motion according to the rotation of the groove wheel 1. The controller 5 is used to control the temperature of the mortar sprayed on the cutting line 2 according to the obtained temperature information during the cutting process, so that the temperature of the mortar sprayed on the cutting line 2 changes with the cutting depth of the cutting line 2, so that the overall temperature of the crystal rod 3 and the cutting line 2 sprayed with the mortar remains stable at different cutting positions during the entire cutting process, thereby achieving the purpose of reducing the warpage of the wafer formed by cutting, that is, dynamically adjusting the temperature of the mortar according to the different cutting depths of the cutting line 2, so that the cutting ability of the cutting line 2 remains stable during the entire cutting process, avoiding defects caused by insufficient cutting ability, thereby achieving the purpose of reducing the warpage of the wafer.
[0103] refer to Figure 6 In the above-mentioned cutting device, the cutting device further comprises:
[0104] a temperature sensor 6 located in the cutting cabin 4;
[0105] The controller 5 is connected to the temperature sensor 6 and is used for obtaining temperature information of the cutting line sprayed with mortar through the temperature sensor 6 .
[0106] The cutting device also includes a temperature sensor 6. The temperature sensor 6 located in the cutting cabin 4 is connected to the controller 5 and is used to feed back the mortar temperature information on the cutting line 2 in the cutting cabin 4 to the controller 5. The controller 5 changes the temperature of the mortar in the mortar tank according to the process parameters, so that the temperature of the mortar changes with the cutting depth.
[0107] In the above-mentioned cutting device, the controller 5 controls the temperature of the mortar sprayed on the cutting line 2 to be negatively correlated with the contact area between the cutting line 2 and the crystal rod 3, including:
[0108] When the cutting depth is not greater than R / 2, the temperature of the mortar decreases as the cutting depth of the crystal rod 3 increases, and the end diameter of the cut position of the crystal rod 3 is R;
[0109] When the cutting depth is not less than R / 2, the temperature of the mortar increases with the increase of the cutting depth of the crystal rod 3 .
[0110] In the cutting device, the controller 5 is used to receive the temperature feedback from the temperature sensor 6 located in the cutting cabin 4, and control the temperature of the mortar sprayed on the surface of the cutting line 2 based on this temperature information, so that the temperature on the cutting line 2 is negatively correlated with the contact area between the cutting line 2 and the crystal rod 3.
[0111] Based on the above, the present application proposes a cutting method and a cutting device for a crystal rod 3. In the cutting method, the temperature of the mortar sprayed on the cutting line 2 is negatively correlated with the contact area between the cutting line 2 and the crystal rod 3, so that the mortar temperature can neutralize the heat generated by the increase in the contact area between the cutting line 2 and the crystal rod 3, thereby achieving the purpose of reducing the warpage of the wafer formed by cutting, that is, dynamically adjusting the temperature of the mortar according to the different cutting depths of the cutting line 2, so that the cutting ability of the cutting line 2 is maintained stable throughout the cutting process, avoiding defects caused by insufficient cutting ability, thereby achieving the purpose of reducing the warpage of the wafer.
[0112] In this specification, each embodiment is described in a progressive, parallel, or progressive and parallel manner. Each embodiment focuses on the differences from other embodiments, and the same or similar parts between the embodiments can be referred to each other. For the device disclosed in the embodiment, since it corresponds to the method disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part.
[0113] It should be noted that in the description of the present application, it should be understood that the description of the drawings and embodiments is illustrative rather than restrictive. The same drawings throughout the embodiments of the specification mark the same structure. In addition, for the sake of understanding and ease of description, the drawings may exaggerate the thickness of some layers, films, panels, regions, etc. It is also understood that when an element such as a layer, film, region or substrate is referred to as "on" another element, the element may be directly on the other element or there may be an intermediate element. In addition, "on" refers to positioning an element on or below another element, but does not essentially mean positioning on the upper side of another element according to the direction of gravity.
[0114] The terms "upper", "lower", "top", "bottom", "inner", "outer", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. When a component is considered to be "connected" to another component, it may be directly connected to the other component or there may be a centrally arranged component at the same time.
[0115] It should also be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "comprises", "comprising" or any other variants thereof are intended to cover non-exclusive inclusion, so that an article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such article or device. In the absence of further restrictions, the elements defined by the sentence "comprising a ..." do not exclude the existence of other identical elements in the article or device including the above elements.
[0116] The above description of the disclosed embodiments enables those skilled in the art to implement or use the present application. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present application. Therefore, the present application will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A method for cutting a crystal rod, characterized in that: The cutting method comprises: During the process of cutting the crystal rod, obtaining temperature information of the cutting line sprayed with mortar; Based on the temperature information, the temperature of the mortar sprayed on the cutting line is controlled. The temperature of the mortar sprayed on the cutting line is controlled to be negatively correlated with the contact area between the cutting line and the crystal rod. As the cutting line approaches the middle position of the crystal rod, the temperature of the mortar gradually decreases. As the cutting line moves away from the center position of the crystal rod, the temperature of the mortar gradually increases, thereby achieving stable temperatures of the crystal rod and the cutting line at different cutting positions.
2. The cutting method according to claim 1, characterized in that: Before obtaining the temperature information of the cutting line, the method further includes: Mounting the crystal rod on a workbench, and moving the workbench to a cutting start position; Turn on the mortar spraying device, spray the mortar on the surface of the cutting line, and start cutting.
3. The cutting method according to claim 1, characterized in that: The method for obtaining the temperature information of the cutting line includes: The temperature information of the cutting line sprayed with mortar in the cutting machine cabin is obtained by a temperature sensor placed in the cutting machine cabin.
4. The cutting method according to claim 1, characterized in that: Controlling the temperature of the mortar sprayed on the cutting line is negatively correlated with the contact area between the cutting line and the crystal rod, including: When the cutting depth is not greater than R / 2, the temperature of the mortar decreases as the cutting depth of the crystal rod increases, and the end diameter of the cut position of the crystal rod is R; When the cutting depth is not less than R / 2, the temperature of the mortar increases with the increase of the cutting depth of the crystal rod.
5. The cutting method according to claim 4, characterized in that: The method of reducing the temperature of the mortar as the cutting depth of the crystal rod increases includes: During the cutting process of the crystal rod from 0 to R / 3, the temperature of the mortar decreases as the cutting depth increases, and the temperature decrease range is no more than 1°C; During the cutting process of the crystal rod with a cutting depth from R / 3 to R / 2, the temperature of the mortar decreases as the cutting depth increases, and the temperature decrease range is no more than 0.5°C.
6. The cutting method according to claim 4, characterized in that: Enabling the temperature of the mortar to increase as the cutting depth of the crystal rod increases includes: During the cutting process of the crystal rod from R / 2 to 2R / 3, the temperature of the mortar increases with the increase of the cutting depth, and the temperature increase range is not greater than 0.5°C; During the cutting process of the crystal rod from 2R / 3 to R, the temperature of the mortar increases with the increase of the cutting depth, and the temperature increase range is not greater than 1°C.
7. The cutting method according to claim 1, characterized in that: The temperature range of the mortar is 20-25°C.
8. A crystal rod cutting device, characterized in that: The cutting device comprises: cutting the cabin; A groove wheel located in the cutting machine cabin is used to drive the cutting line to rotate; A controller is used to obtain temperature information of a cutting line sprayed with mortar during cutting of the crystal rod, and based on the temperature information, control the temperature of the mortar sprayed on the cutting line, and control the temperature of the mortar sprayed on the cutting line to be negatively correlated with the contact area between the cutting line and the crystal rod, and as the cutting line approaches the middle position of the crystal rod, the temperature of the mortar gradually decreases, and as the cutting line moves away from the center position of the crystal rod, the temperature of the mortar gradually increases, thereby achieving stable temperatures of the crystal rod and the cutting line at different cutting positions.
9. The cutting device according to claim 8, characterized in that The cutting device also includes: a temperature sensor located within the cutting chamber; The controller is connected to the temperature sensor and is used for obtaining temperature information of the cutting line sprayed with mortar through the temperature sensor.
10. The cutting device according to claim 8, characterized in that When the cutting depth is not greater than R / 2, the controller is used to reduce the temperature of the mortar as the cutting depth of the crystal rod increases, and the end face diameter of the cut position of the crystal rod is R; When the cutting depth is not less than R / 2, the controller is used to increase the temperature of the mortar as the cutting depth of the crystal rod increases.
Citation Information
Patent Citations
A method for cutting silicon blocks
CN102275232A
Method for adjusting and detecting utilization proportion of old mortar in silicon wafer cutting
CN103395132A
Mortar injection control method and control system in silicon wafer cutting
CN114571617A
Multi-wire cutting method and device