Single wafer cleaning process to improve chemical oxide film thickness and Haze uniformity of polished silicon wafers
By using a two-step process of high-speed rotation and spraying ozone water and hydrofluoric acid in a single-wafer cleaning machine, the problem of Haze uniformity on the surface of the silicon wafer is solved, and the Haze uniformity on the surface of the silicon wafer is significantly improved and easy to operate and run. Good stability effect.
Patent Information
- Application Number
- CN202211070830.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-01
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-09-01
AI Technical Summary
In the existing technology, the cleaning method of polished silicon wafers and silicon epitaxial wafers has problems of reverse contamination and cross-contamination caused by liquid circulation and batch methods, and it is difficult to meet the stringent requirements of logic and memory devices for the uniformity of Haze values on the silicon wafer surface.
A single-wafer cleaning machine is used to clean the silicon wafer by combining high-speed rotation of the silicon wafer and spraying ozone water (O3DIW) and hydrofluoric acid (HF) from fixed-position nozzles. The attached particles and metal are peeled off through repeated cycles of O3DIW → HF, and the redox potential is used. An electric field is formed to promote the uniform growth of the SiOx oxide film, and a two-step method is used to control the oxide film thickness and Haze uniformity.
It significantly improves the Haze uniformity on the silicon wafer surface, realizes a single-chip cleaning process with simple operation and good operation stability, and meets the stringent requirements of logic and memory devices on the Haze level of silicon substrates.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of cleaning silicon polishing wafers and silicon epitaxial wafers for semiconductors, and in particular to a single-wafer cleaning process for improving chemical oxidation film thickness and Haze uniformity of polished silicon wafers. Background Art
[0002] Polished silicon wafers and silicon epitaxial wafers for semiconductors use laser scattering method to measure particles on the surface of silicon wafers (such as KLA Surfscan series, Hitachi LS series and Zhongke Feice, etc.). In the particle detection results, there is an important parameter called Haze. The Haze value is defined as the ratio of the backscattered light of the silicon wafer (or epitaxial wafer) to the incident laser intensity, which reflects the micro-roughness level of the silicon wafer surface at the atomic scale.
[0003] The micro-roughness of the silicon wafer surface has a great impact on GOI (Gate Oxide Integrity) (especially for ultra-thin gate dielectric layers (~several nm thick)). The deterioration of the SiO2 / Si interface morphology caused by the roughness of the silicon substrate will cause a decrease in the breakdown strength and reliability (TDDB) of the gate dielectric layer. Therefore, chip companies (especially storage and logic devices) have strict requirements on the Haze level and uniformity of the silicon substrate.
[0004] In the process of polishing silicon wafers, the polishing, post-polishing cleaning and final cleaning processes will affect the Haze value (micro-roughness) of the final product. The impact of polishing on Haze is not within the scope of this patent. For silicon wafer cleaning, its essence is etching. The SC1 (NH4OH+H2O2) and O3DIW→HF steps commonly used in the field of silicon wafer cleaning will increase the haze value of silicon wafers. At present, there are two main cleaning methods for polished silicon wafers and silicon epitaxial wafers: tank cleaning and single-wafer cleaning. Tank cleaning is mostly an improvement on the traditional RCA process, and the main chemicals used are SC1 (NH4OH+H2O2), SC2 (HCl+H2O2), O3DIW, HF, etc. Tank cleaning machines have their inherent weaknesses. Due to the use of chemical liquid circulation and batch mode (usually 25 pieces / Batch), there is a problem of reverse contamination of metal and particles of silicon wafers by chemical liquid, as well as cross contamination between silicon wafers, which makes it difficult to meet the metal and particle requirements of logic and storage devices. Summary of the invention
[0005] The present invention mainly solves the deficiencies in the prior art and provides a single-wafer cleaning process for improving the thickness of chemical oxide film and Haze uniformity of polished silicon wafers, which has the characteristics of simple operation, good running stability and significant effect, so that the Haze uniformity of the silicon wafer surface is significantly improved.
[0006] The above technical problems of the present invention are mainly solved by the following technical solutions:
[0007] A single-wafer cleaning process for improving the thickness of chemical oxide film and Haze uniformity of polished silicon wafers, wherein the single-wafer cleaning machine uses a method of high-speed rotation (Spin) of silicon wafers combined with spraying (Spray) of chemical liquid (O3DIW and HF) from a nozzle at a fixed position to clean the silicon wafer; during cleaning, ozone water (O3DIW) is used to form an oxide film on the surface of the silicon wafer, and then HF is sprayed on the surface of the silicon wafer to etch the formed oxide film, and through repeated cycles of O3DIW→HF, particles and metals attached to the surface of the silicon wafer are stripped; when O3DIW reacts with Si, under the action of redox potential, the silicon substrate will lose electrons, and the electrons pass through the formed SiO x Oxide film reaches SiO x / O3DIW solid-liquid interface, and form a negative monovalent O with the oxygen atoms produced by the decomposition of O3 - , because the silicon substrate loses electrons, x An electric field pointing toward O3DIW is formed in the oxide film layer;
[0008] The SiO was grown using a two-step method. x Oxide film:
[0009] In the first step, O3DIW moves at a constant speed from the edge of the silicon wafer to the center of the silicon wafer, and O3DIW is sprayed during this process; the concentration of O3DIW at the moment of contact with the silicon wafer at different radii is the same. After O3DIW contacts the silicon wafer, it will flow to the edge of the silicon wafer under the action of high-speed spin;
[0010] In the second step, at the end of the first step, the thickness of the oxide film (h1(r)) will show a trend of being high at the edge and low in the center; the O3DIWNozzle stays in the center of the silicon wafer for a few seconds and sprays O3DIW, and the newly added oxide film thickness (h2(r)) will show the characteristics of being high in the center and low at the edge.
[0011] As a preference, O - Attracted by the electric field, ions move toward SiO x / Si interface diffusion and form new SiO x Therefore, the reaction between Si and O3DIW is not only a diffusion-controlled process, because the diffusion process is driven by the concentration gradient, but also a so-called "field-imposed drift" process; the Fehnler formula can be used to describe its kinetic process:
[0012] t ox =E ln(1+Ft)
[0013] Among them, t oxis the thickness of the silicon oxide film, t is the reaction time, E and F are constants that depend on the O3 concentration; the Fehnler formula was used to fit the experimental results and a good fitting result was obtained.
[0014] As a preference, the oxidation of Si in chemical solutions such as O3DIW, H2O2, and SC1 has a so-called "Self-limiting Oxide Growth" mechanism, that is, when SiO x When the film thickness reaches a certain level, the growth of the oxide film will stop, and the thickness will not increase even if the time is extended.
[0015] Preferably, under the conditions of O3 concentration of 1ppm, 5ppm, 15ppm and oxidation time of 20min, SiO x The thicknesses are and The decrease in the solubility of O3 in static water conforms to the law of negative exponential change:
[0016] [O3]=[O a ]0 exp(-k d t)
[0017] Where [O3]0 is the initial concentration of O3, k d It is a constant related to pH value. Stirring has a significant effect on the decomposition of O3 in water. When stirring intensifies, the decomposition of O3 in water increases significantly.
[0018] As a preference, during the single-wafer cleaning process, the time for O3DIW to flow from the center of the silicon wafer to the edge of the silicon wafer is extremely short. However, due to the stirring effect and the high specific surface area, O3 decomposes and volatilizes in DIW. There should be a decreasing O3 flow rate from the center of the silicon wafer to the edge of the silicon wafer. 3 Concentration gradient.
[0019] Preferably, in the first oxidation step, the factor affecting the final oxide film thickness is the movement rate ν of the O3DIW Nozzle; in the second oxidation step, the factor affecting the thickness of the newly added oxide film is the time t that the O3DIW Nozzle stays at the center of the silicon wafer; through a reasonable combination of the two, an optimized oxide film thickness (h(r)=h1(r)+h2(r)) uniformity will be obtained.
[0020] The present invention can achieve the following effects:
[0021] The present invention provides a single-wafer cleaning process for improving the thickness of chemical oxide film and Haze uniformity of polished silicon wafers, which has the characteristics of simple operation, good running stability and significant effect compared with the prior art, so that the Haze uniformity of the silicon wafer surface is significantly improved. DETAILED DESCRIPTION
[0022] The technical solution of the invention is further specifically described below through embodiments.
[0023] Embodiment: A single-wafer cleaning process for improving the thickness of chemical oxide film and Haze uniformity of polished silicon wafers, wherein a single-wafer cleaning machine uses a method of high-speed rotation (Spin) of silicon wafers combined with a nozzle at a fixed position to spray (Spray) chemical liquid (O3DIW and HF) to clean the silicon wafer; during cleaning, ozone water (O3DIW) is used to form an oxide film on the surface of the silicon wafer, and then HF is sprayed on the surface of the silicon wafer to etch the formed oxide film, and through repeated cycles of O3DIW→HF, particles and metals attached to the surface of the silicon wafer are stripped; when O3DIW reacts with Si, under the action of redox potential, the silicon substrate will lose electrons, and the electrons pass through the formed SiO x Oxide film reaches SiO x / O3DIW solid-liquid interface, and form a negative monovalent O with the oxygen atoms produced by the decomposition of O3 - , because the silicon substrate loses electrons, x An electric field pointing to O3DIW is formed in the oxide film layer. - Attracted by the electric field, ions move toward SiO x / Si interface diffusion and form new SiO x Therefore, the reaction between Si and O3DIW is not only a diffusion-controlled process, because the diffusion process is driven by the concentration gradient, but also a so-called "field-imposed drift" process; the Fehnler formula can be used to describe its kinetic process:
[0024] t ox =E ln(1+Ft)
[0025] Among them, t ox is the thickness of the silicon oxide film, t is the reaction time, E and F are constants that depend on the O3 concentration; the Fehnler formula was used to fit the experimental results and a good fitting result was obtained.
[0026] The oxidation of Si in chemical solutions such as O3DIW, H2O2, and SC1 has a so-called "Self-limiting Oxide Growth" mechanism, that is, when SiO x When the film thickness reaches a certain level, the growth of the oxide film will stop, and the thickness will not increase even if the time is extended. Under the conditions of O3 concentration of 1ppm, 5ppm, 15ppm and oxidation time of 20min, SiO x The thicknesses are and The decrease in the solubility of O3 in static water conforms to the law of negative exponential change:
[0027] [O3]=[O a ]0 exp(-k d t)
[0028] Where [O3]0 is the initial concentration of O3, k d is a constant related to pH value. Stirring has a significant effect on the decomposition of O3 in water. When the stirring is intensified, the decomposition of O3 in water increases significantly. During the single-wafer cleaning process, the time for O3DIW to flow from the center of the silicon wafer to the edge of the silicon wafer is extremely short, but due to the stirring effect and the high specific surface area, O3 decomposes and volatilizes in DIW, and there should be a decreasing O3 concentration gradient from the center of the silicon wafer to the edge of the silicon wafer.
[0029] The SiO was grown using a two-step method. x Oxide film:
[0030] In the first step, O3DIW moves at a constant speed from the edge of the silicon wafer to the center of the silicon wafer, and O3DIW is sprayed during this process; the concentration of O3DIW at the moment of contact with the silicon wafer at different radii is the same. After O3DIW contacts the silicon wafer, it will flow to the edge of the silicon wafer under the action of high-speed spin;
[0031] In the second step, at the end of the first step, the thickness of the oxide film (h1(r)) will show a trend of being high at the edge and low in the center; the O3DIWNozzle stays in the center of the silicon wafer for a few seconds and sprays O3DIW, and the newly added oxide film thickness (h2(r)) will show the characteristics of being high in the center and low at the edge.
[0032] In the first oxidation step, the factor affecting the final oxide film thickness is the movement rate v of the O3DIW Nozzle; in the second oxidation step, the factor affecting the thickness of the newly added oxide film is the time t that the O3DIW Nozzle stays at the center of the silicon wafer; through a reasonable combination of the two, an optimized oxide film thickness (h(r)=h1(r)+h2(r)) uniformity will be obtained.
[0033] In summary, the single-wafer cleaning process for improving the chemical oxide film thickness and Haze uniformity of polished silicon wafers has the characteristics of simple operation, good operation stability and significant effect, so that the Haze uniformity of the silicon wafer surface is significantly improved.
[0034] The above description is only a specific embodiment of the present invention, but the structural features of the present invention are not limited thereto. Any changes or modifications made by any technician in the field of the present invention are included in the patent scope of the present invention.
Claims
1. A single-wafer cleaning process for improving the chemical oxide film thickness and Haze uniformity of polished silicon wafers. Features: In the single-chip cleaning machine, the silicon wafer is rotated at high speed and the nozzle at a fixed position is used to spray the liquid. 3 DIW and HF are used to clean the silicon wafer; when cleaning, O 3 DIW forms an oxide film on the surface of the silicon wafer, and then HF is sprayed on the surface of the silicon wafer to etch the oxide film. 3 Repeated cycles of DIW→HF remove particles and metals attached to the surface of the silicon wafer; 3 When DIW reacts with Si, the silicon substrate loses electrons under the action of redox potential. The electrons pass through the already formed SiO x Oxide film reaches SiO x / O 3 DIW solid-liquid interface and O 3 The oxygen atom produced by decomposition forms a negatively charged O - , because the silicon substrate loses electrons, x The oxide film forms a 3 The electric field of DIW; The SiO was grown using a two-step method. x Oxide film: Step 1, O 3 The DIW nozzle moves at a constant speed from the edge of the silicon wafer to the center of the silicon wafer, spraying O 3 DIW;O 3 O at different radii when DIW contacts the silicon wafer 3 The concentration is the same, O 3 After DIW contacts the silicon wafer, it will flow toward the edge of the silicon wafer under the action of high-speed rotation; Step 2: At the end of step 1, the thickness of the oxide film is h 1 (r) will show a trend of high edges and low centers; 3 The DIW nozzle stays at the center of the wafer for a few seconds and sprays O 3 DIW, additional oxide film thickness h 2 (r) will be high in the center and low at the edges.
2. The single-wafer cleaning process for improving the chemical oxide film thickness and Haze uniformity of polished silicon wafers according to claim 1, Features: O - Attracted by the electric field, ions move toward SiO x / Si interface diffusion and form new SiO x ; The Fehnler formula is used to describe its dynamic process: t ox =E ln(1+Ft) Among them, t cx is the thickness of the silicon oxide film, t is the reaction time, E and F are dependent on O 3 The concentration constant.
3. The single-wafer cleaning process for improving the chemical oxide film thickness and Haze uniformity of polished silicon wafers according to claim 1 or 2, Features: In O 3 When the concentration is 1ppm, 5ppm, 15ppm and the oxidation time is 20min, SiO x The thicknesses are and O 3 The decrease in solubility in static water conforms to the negative exponential change law: [O 3 ]=[O 3 ] 0 exp(-k d t) Among them [O 3 ] 0 O 3 The initial concentration, k d is a constant related to pH value; stirring has an effect on O 3 It has a significant decomposition effect in water. When stirring is intensified, O 3 Decomposition in water is significantly increased.
4. The single-wafer cleaning process for improving the chemical oxide film thickness and Haze uniformity of polished silicon wafers according to claim 3, Features: During the single-wafer cleaning process, 3 The time for DIW to flow from the center of the silicon wafer to the edge of the silicon wafer is extremely short, but due to the stirring effect and the high specific surface area, the O 3 Decomposition and volatilization in DIW should have a decreasing O from the center to the edge of the silicon wafer. 3 Concentration gradient.
5. The single-wafer cleaning process for improving the chemical oxide film thickness and Haze uniformity of polished silicon wafers according to claim 1, Features: In the first oxidation step, the factors that affect the final oxide film thickness are O 3 The moving speed v of the DIW nozzle; in the second oxidation step, the factor affecting the thickness of the newly added oxide film is O 3 The time t that the DIW nozzle stays at the center of the silicon wafer; through a reasonable combination of the two, an optimized oxide film thickness h(r) = h 1 (r)+h 2 (r).
Citation Information
Patent Citations
Chemical mechanical polishing method
CN113178386A
Treating solution applying method
CN1467793A
Substrate treating device and substrate treating method
CN1582489A
Method for manufacturing semiconductor device
CN1691277A
Method for processing through wafer rotation and its device
JP1998154701A