A planar gate IGBT device and its manufacturing method
Patent Information
- Application Number
- CN202211021554.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-24
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2042-08-24
AI Technical Summary
The presence of excess carriers during turn-off of existing SiC IGBT devices results in a significant increase in turn-off time and loss, making it difficult to reduce the on-resistance and conduction loss without affecting the breakdown voltage and gate oxide electric field strength.
Design a planar gate IGBT device with a SiC/Si heterojunction on the back. The heterojunction stores and conducts residual carriers, improving the device's turn-off speed and reducing turn-off loss. The device includes a P-type collector layer, a polysilicon layer, an isolation layer, an N-type buffer layer, an N-type drift layer, an N-type current expansion layer and a metal layer. The P-well region and the heavily doped source region are formed through ion implantation to form a heterogeneous Mass junctions store and conduct carriers.
The device's turn-off time and turn-off loss are significantly reduced, while the breakdown voltage and gate oxide electric field strength are maintained, achieving a compromise between the device's forward conduction voltage drop and turn-off loss.
Smart Images

Figure CN115425075B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor devices, and in particular to a planar gate IGBT device and a preparation method thereof. Background Art
[0002] The third generation wide bandgap semiconductor silicon carbide (SiC) has the characteristics of larger bandgap, higher critical breakdown field strength, higher thermal conductivity and faster electron saturation speed, and has extensive research value and application value in power electronic devices. Silicon-Carbide Insulated Gate Bipolar Transistor (SiC IGBT) is the latest power electronic device, which marks the technological frontier of power semiconductors. IGBT combines the advantages of metal-oxide-semiconductor field effect transistor (Metal-Oxide-Semiconductor Field Effect Transistor, MOSFET) and bipolar junction transistor (Bipolar Junction Transistor, BJT). The switch of BJT is controlled by MOS tube, so the device has high switching frequency and large input impedance. When turned off, the thyristor structure has a higher breakdown voltage. When turned on, the internal PIN structure introduces conductivity modulation effect, the forward conduction voltage drop is reduced, and the overall power consumption is small, which makes the whole device have the advantages of working at high frequency, high voltage and high current. It is widely used in ship drive, rail transportation, smart grid, AC frequency conversion, aerospace, wind power generation, new energy, motor transmission, automobile and other high-voltage control fields.
[0003] Due to early process defects, P-type silicon carbide substrates were difficult to form, and the research team mainly focused on the research and preparation of P-type IGBTs. However, the electron mobility in silicon carbide is much greater than that of holes, so in recent years, with the development of technology, people have begun to pay attention to N-type IGBTs. Until the American CREE company produced an N-type IGBT with a breakdown voltage of 27kV, the breakdown characteristics had reached expectations, and the focus of the overall device design shifted to the compromise between reliability and device performance. The dynamic characteristics of the device have been increasingly valued in SiCIGBTs.
[0004] IGBT has two basic structures, namely planar gate structure and trench gate structure. Although the trench gate IGBT eliminates the JFET area, reduces resistance, increases channel density, and greatly improves the conduction characteristics, the silicon carbide material itself has high hardness and strong corrosion resistance, and it is difficult to form a trench structure with a smooth interface in the process. Therefore, in practical applications, the main structure of SiC IGBT is a planar gate structure. For SiC IGBT devices, the introduction of conductivity modulation effect greatly reduces the on-resistance and conduction loss. However, there are excess carriers inside the device. When the device is turned off, it takes a lot of time to wait for the excess carriers to recombine to form a depletion region and eventually turn off the device, which will cause the device's turn-off time and turn-off loss to increase significantly. Therefore, considering the actual device application scenario, it is necessary to compromise the conduction characteristics and switching characteristics of SiC IGBT. Summary of the invention
[0005] In order to overcome the problems existing in the prior art, the purpose of the present invention is to provide a planar gate IGBT device, which has a heterojunction on the back, and stores and conducts residual carriers through the heterojunction, thereby greatly improving the turn-off speed of the device, significantly reducing the turn-off time and turn-off loss of the device, while not affecting the breakdown voltage and gate oxide electric field strength of the device, thereby better achieving a compromise between the forward conduction voltage drop and turn-off loss of the device.
[0006] In order to achieve the above objectives, the present invention provides the following technical solutions.
[0007] A planar gate IGBT device, comprising:
[0008] collector;
[0009] A P-type collector layer, the P-type collector layer covers a portion of the upper surface of the collector electrode;
[0010] a polysilicon layer, the polysilicon layer being disposed above the collector electrode;
[0011] an isolation layer, wherein the isolation layer isolates the polysilicon layer from the P-type collector layer and isolates the polysilicon layer from the collector electrode;
[0012] An N-type buffer layer, the N-type buffer layer covers the upper surfaces of the polysilicon layer and the P-type collector layer, and the N-type buffer layer forms a heterojunction with the polysilicon layer;
[0013] An N-type drift layer, wherein the N-type drift layer is disposed on an upper surface of the N-type buffer layer;
[0014] An N-type current spreading layer, wherein the N-type current spreading layer is arranged on the upper surface of the N-type drift layer, and a P-well region is arranged on the surface layer of the upper surface of the N-type current spreading layer, and a first N-type heavily doped source region, a P-type heavily doped contact region, and a second N-type heavily doped source region are arranged in a shallow layer on the upper surface of the P-well region from left to right;
[0015] a metal layer, the metal layer being in contact with the first N-type heavily doped source region, the P-type heavily doped contact region, and the second N-type heavily doped source region;
[0016] a gate, the gate comprising a first gate and a second gate, and the first gate and the second gate are arranged on both sides of the metal layer; and
[0017] A gate dielectric layer, the gate dielectric layer includes an oxide layer and an interlayer dielectric layer, the oxide layer is arranged between the first gate and the N-type current spreading layer and between the second gate and the N-type current spreading layer, the interlayer dielectric layer is arranged between the first gate and the metal layer and between the second gate and the metal layer, and the interlayer dielectric layer covers the upper surfaces of the first gate and the second gate.
[0018] Another object of the present invention is to provide a method for preparing the above-mentioned planar gate IGBT device, comprising:
[0019] A P-type collector layer, an N-type buffer layer and an N-type drift layer are sequentially formed on the upper surface of the N-type substrate from bottom to top;
[0020] forming an N-type current spreading layer on the surface layer of the upper surface of the N-type drift layer by ion implantation;
[0021] Forming a P-well region on the surface layer of the upper surface of the N-type current spreading layer by ion implantation;
[0022] Forming an oxide layer and a gate in sequence from bottom to top on the upper surface of the N-type current spreading layer;
[0023] Etching the gate and the oxide layer to expose a portion of the upper surface of the P-well region to form a source opening, and then forming an interlayer dielectric layer on the gate;
[0024] Forming a first N-type heavily doped source region, a P-type heavily doped contact region, and a second N-type heavily doped source region in a shallow layer on an upper surface of the P-well region by ion implantation;
[0025] removing the N-type substrate;
[0026] Etching the P-type collector layer to expose a portion of the lower surface of the N-type buffer layer to form a first window;
[0027] forming an isolation layer at the first window, and then etching upward from the lower surface of the isolation layer to form a second window;
[0028] forming a polysilicon layer at the second window, and passivating the lower surface of the polysilicon layer;
[0029] forming a collector electrode below the P-type collector layer; and
[0030] A metal layer is formed at the source opening.
[0031] Compared with the prior art, the present invention has the following beneficial effects:
[0032] 1. The present invention provides a planar gate IGBT device, which has a heterojunction on the back. The heterojunction stores and conducts excess carriers, greatly improving the device's turn-off speed, significantly reducing the device's turn-off time and turn-off loss, while not affecting the device's breakdown voltage and gate oxide electric field strength, thereby better achieving a compromise between the device's forward conduction voltage drop and turn-off loss.
[0033] 2. The present invention provides a method for preparing a planar gate IGBT device, which is compatible with the traditional SiC IGBT preparation process. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:
[0035] Figure 1 It is a schematic structural diagram of the planar gate IGBT device of the present invention.
[0036] Figure 2-Figure 17 This is a schematic diagram of the structure obtained in each step of the preparation method provided in Example 1 of the present invention.
[0037] Fig.18 It is a turn-off curve diagram of the planar gate IGBT device of the present invention and the traditional SiC IGBT.
[0038] Fig.19 Schematic diagram of the traditional planar gate SiC IGBT structure.
[0039] Description of reference numerals:
[0040] 100 is a collector, 200 is a P-type collector layer, 300 is a polysilicon layer, 400 is an isolation layer, 500 is an N-type buffer layer, 600 is an N-type drift layer, 700 is an N-type current spreading layer, 710 is a P-well region, 711 is a first N-type heavily doped source region, 712 is a second N-type heavily doped source region, 713 is a P-type heavily doped contact region, 800 is a metal layer, 900 is a gate, 900a is a first gate, 900b is a second gate, 1000 is a gate dielectric layer, 1001 is an oxide layer, 1002 is an interlayer dielectric layer, 1100 is an N-type substrate, 1200 is a source opening, 1300 is a first window, and 1400 is a second window. DETAILED DESCRIPTION
[0041] Hereinafter, embodiments of the present disclosure will be described with reference to the accompanying drawings. However, it should be understood that these descriptions are exemplary only and are not intended to limit the scope of the present disclosure. In addition, in the following description, descriptions of well-known structures and technologies are omitted to avoid unnecessary confusion of the concepts of the present disclosure.
[0042] Various structural schematic diagrams according to embodiments of the present disclosure are shown in the accompanying drawings. These figures are not drawn to scale, and some details are magnified and some details may be omitted for the purpose of clear expression. The shapes of various regions and layers shown in the figures and the relative sizes and positional relationships therebetween are only exemplary, and may deviate in practice due to manufacturing process or technical limitations, and those skilled in the art may further design regions / layers with different shapes, sizes, and relative positions according to actual needs.
[0043] In the context of the present disclosure, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element or an intervening layer / element may exist therebetween. In addition, if a layer / element is "on" another layer / element in one orientation, the layer / element may be "below" the other layer / element when the orientation is reversed.
[0044] Since the existing planar gate IGBT device cannot reduce the on-resistance and conduction loss without affecting the breakdown voltage of the device and the electric field strength of the gate 900 oxide, the present invention provides an improved planar gate IGBT device.
[0045] Figure 1 A schematic diagram of the structure of the planar gate IGBT device of the present invention is given. Specifically, Figure 1As shown, the planar gate IGBT device of the present invention includes: a collector 100; a P-type collector layer 200, the P-type collector layer 200 covers a portion of the upper surface of the collector 100; a polysilicon layer 300, the polysilicon layer 300 is arranged on the collector 100; an isolation layer 400, the isolation layer 400 isolates the polysilicon layer 300 from the P-type collector layer 200, and isolates the polysilicon layer 300 from the collector 100; an N-type buffer layer 500, the N-type buffer layer 500 covers the polysilicon layer 300; 00 and the upper surface of the P-type collector layer 200, and the N-type buffer layer 500 forms a heterojunction with the polysilicon layer 300; an N-type drift layer 600, the N-type drift layer 600 is arranged on the upper surface of the N-type buffer layer 500; an N-type current expansion layer 700, the N-type current expansion layer 700 is arranged on the upper surface of the N-type drift layer 600, and the surface layer of the upper surface of the N-type current expansion layer 700 is provided with a P-well region 710, and the shallow surface layer of the upper surface of the P-well region 710 is provided with a first N-type heavily doped The first N-type heavily doped source region 711, the P-type heavily doped contact region 713 and the second N-type heavily doped source region 712; the metal layer 800, the metal layer 800 is in contact with the first N-type heavily doped source region 711, the P-type heavily doped contact region 713 and the second N-type heavily doped source region 712; the gate 900, the gate 900 includes a first gate 900a and a second gate 900b, and the first gate 900a and the second gate 900b are arranged on both sides of the metal layer 800; and the gate dielectric layer 1000, the gate dielectric Layer 1000 includes an oxide layer 1001 and an interlayer dielectric layer 1002, the oxide layer 1001 is arranged between the first gate 900a and the N-type current spreading layer 700 and between the second gate 900b and the N-type current spreading layer 700, the interlayer dielectric layer 1002 is arranged between the first gate 900a and the metal layer 800 and between the second gate 900b and the metal layer 800, and the interlayer dielectric layer 1002 covers the upper surfaces of the first gate 900a and the second gate 900b.
[0046] Preferably, the collector 100 is a metal material, such as a metal or a metal alloy. Preferably, the thickness of the collector 100 may be 4-6 μm, preferably 4.5-5.5 μm. In one embodiment of the present invention, the collector 100 is a titanium aluminum alloy. Of course, according to actual needs, the collector 100 may be any desired metal that can form an ohmic contact with the P-type collector layer 200.
[0047] Preferably, the P-type collector layer 200 is a P-type heavily doped layer, and the doping ions are preferably Al ions. Preferably, the P-type collector layer 200 is a P-type heavily doped SiC layer, which is preferably formed by epitaxy by chemical vapor deposition. Preferably, the doping concentration of the P-type collector layer 200 can be 1×10 19 -5×10 19 cm -3 , preferably 1×10 19 -2×1019 cm -3 ; The thickness can be 3-7μm, preferably 4-5μm.
[0048] Preferably, the upper surface of the polysilicon layer 300 is higher than the upper surface of the P-type collector layer 200. Preferably, the height difference between the upper surface of the polysilicon layer 300 and the upper surface of the P-type collector layer 200 may be 0.5-1 μm, for example, 0.5 μm, 0.6 μm, 0.7 μm, 0.8 μm, 0.9 μm or 1 μm. The width of the polysilicon layer 300 is 0.8-1.2 μm and the thickness is 1.5-2 μm. In the present application, the polysilicon layer 300 is not subjected to metal deposition to form an ohmic contact. The polysilicon layer 300 does not need to be doped. The reason for isolating the polysilicon from the metal electrode with an isolation layer is that once the polysilicon contacts the electrode, a large number of carriers will flow into the polysilicon and the on-resistance will increase. After isolation, the polysilicon only exists as a recombination center. This design will improve dynamic loss and have less impact on conduction.
[0049] Preferably, the isolation layer 400 is silicon dioxide. The polysilicon layer 300 is isolated from the P-type collector layer 200, and the two do not form a heterojunction. The width of the isolation layer 400 portion between the polysilicon layer 300 and the P-type collector layer 200 is 0.1-0.3 μm. The thickness of the isolation layer 400 portion between the polysilicon layer 300 and the collector 100 is 0.1-0.5 μm, preferably 0.1-0.2 μm.
[0050] Preferably, the N-type buffer layer 500 is an N-type SiC layer, which is preferably formed by epitaxy by chemical vapor deposition. The doping ions of the N-type buffer layer 500 are preferably N ions. Preferably, the doping concentration of the N-type buffer layer 500 is 1×10 17 -5×10 17 cm -3 , preferably 1×10 17 -2×10 17 cm -3 ; The thickness can be 2-5μm, preferably 2-3μm.
[0051] Preferably, the N-type drift layer 600 is an N-type SiC layer, which is preferably formed by epitaxy by chemical vapor deposition. Preferably, the doping ions of the N-type drift layer 600 are preferably N ions. Preferably, the doping concentration of the N-type drift layer 600 may be 2×10 14 -8×10 14 cm -3 , for example 2×10 14 -6×10 14 cm -3 ; The thickness can be 100-130μm, preferably 100-120μm.
[0052] Preferably, the doping concentration of the N-type current spreading layer 700 may be 1×10 15 -5×10 16 cm -3 , preferably 8×10 15 -2×10 16 cm -3 ; The thickness can be 2-10μm, preferably 2-5μm.
[0053] Preferably, the doping concentration of the P-well region 710 is in the range of 1×10 16 ~1×10 18 The doping of the P-well region 710 may be, for example, uniform doping, and the uniform doping concentration may be 1×10 17 ~5×10 17 , preferably 4×10 17 ~5×10 17 The doping ions are preferably Al ions. The thickness of the P-well region 710 may be 0.8-1.2 μm, preferably 0.9-1.1 μm.
[0054] Preferably, the doping concentration of the first N-type heavily doped source region 711 may be 5×10 19 ~1×10 20 , preferably 8×10 19 ~1×10 20 The doping ions are preferably N ions. The thickness of the first N-type heavily doped source region 711 may be 0.4-0.6 μm, preferably 0.45-0.55 μm.
[0055] Preferably, the doping concentration of the P-type heavily doped contact region 713 may be 1×10 20 ~2×10 20 , preferably 1×10 20 ~1.2×10 20 The doping ions are preferably Al ions. The thickness of the P-type heavily doped contact region 713 may be 0.2-0.5 μm, preferably 0.45-0.55 μm.
[0056] Preferably, the doping concentration of the second N-type heavily doped source region 712 may be 5×10 19 ~1×10 20 , preferably 8×10 19 ~1×10 20 The doping ions are preferably N ions. The thickness of the second N-type heavily doped source region 712 may be 0.4-0.6 μm, preferably 0.45-0.55 μm. The two N-type heavily doped regions are symmetrical structures, using the same process steps, and have the same concentration and thickness.
[0057] In the present application, the P-type heavily doped contact region 713 is disposed between the first N-type heavily doped source region 711 and the second N-type heavily doped source region 712, and is in contact with them respectively. Figure 1 described.
[0058] Preferably, the gate 900 is made of polysilicon. In some specific embodiments, the first gate 900a and the second gate 900b are both made of polysilicon.
[0059] Preferably, the metal layer 800 is a metal material, such as a metal or a metal alloy. In one embodiment of the present invention, the metal layer 800 is a nickel-titanium-aluminum alloy. Of course, according to actual needs, the metal layer 800 can be any desired metal that can form an ohmic contact with the N-type heavily doped source region.
[0060] In some specific embodiments, the metal layer 800 covers a portion of the upper surface of the first N-type heavily doped source region 711 and the second N-type heavily doped source region 712, and covers the entire upper surface of the P-type heavily doped contact region 713. The electrode formed by this design can suppress the latch effect of the IGBT, and has a self-alignment process in the process, which is relatively easy to implement.
[0061] In some specific embodiments, the metal layer 800 covers the upper surface of the interlayer dielectric layer 1002 .
[0062] The gate dielectric layer 1000 includes an oxide layer 1001 and an interlayer dielectric layer 1002. Preferably, both the oxide layer 1001 and the interlayer dielectric layer 1002 can be silicon dioxide. The thickness of the oxide layer 1001 can be 50-60nm, preferably 50-55nm. If the oxide layer 1001 is too thin, it is easy to break down; if the oxide layer 1001 is too thick, the threshold voltage of the device will increase.
[0063] The advantages of the planar gate IGBT device of the present invention are: a SiC / Si heterojunction is formed at the N-type buffer layer 500. Since the bandgap width of Si is much smaller than that of SiC, a potential well of electrons and holes is formed at the interface. When the device is turned off, the heterojunction stores a large amount of excess carriers. At the same time, the smaller bandgap width can make the carriers recombine faster. Therefore, the excess carriers inside the device are reduced faster, the depletion region is formed quickly, and the turn-off time and turn-off loss of the device are reduced. For the convenience of comparison, the simulation software was used to perform the simulation under the same electrode bias conditions. Figure 1 The structure is different from the conventional planar gate SiC IGBT structure (the N-type buffer layer 500 does not form a SiC / Si heterojunction, such as Fig.19 The turn-off curve is shown in Fig.18 shown.
[0064] The above two device structures are identical except that no SiC / Si heterojunction is formed at the N-type buffer layer 500. The width and thickness of the polysilicon are 1 μm and 4 μm respectively, and the width of the isolation layer 400 between the polysilicon layer 300 and the P-type collector layer 200 is 0.1 μm. Fig.18 The turn-off curves of the two devices under the same bias conditions are given. Fig.18 It can be seen that the gate voltage of the two structures drops at the same time point, indicating that the turn-off of the two starts at the same time. The current of the planar gate SiC IGBT structure with a heterojunction on the back drops to 0 faster, and the device can be turned off faster. Similarly, the turn-off loss is further reduced.
[0065] The present invention also provides a method for preparing the planar gate IGBT device, which comprises the following steps.
[0066] First, a P-type collector layer 200 , an N-type buffer layer 500 , and an N-type drift layer 600 are sequentially formed from bottom to top on the upper surface of an N-type substrate 1100 .
[0067] Preferably, the N-type substrate 1100 is an N-type 4H-SiC substrate, and its doping concentration may be 5×10 16 ~1×10 17 cm -3 .
[0068] Preferably, the P-type collector layer 200 may be epitaxially formed by chemical vapor deposition. In some specific embodiments, the P-type collector layer 200 is epitaxially grown on the C-surface of the N-type 4H-SiC substrate by CVD.
[0069] Preferably, the N-type buffer layer 500 may be epitaxially formed by chemical vapor deposition.
[0070] Preferably, the N-type drift layer 600 may be epitaxially formed by chemical vapor deposition.
[0071] Then, an N-type current spreading layer 700 is formed on the surface layer of the upper surface of the N-type drift layer 600 by ion implantation.
[0072] Afterwards, a P-well region 710 is formed on the surface layer of the upper surface of the N-type current spreading layer 700 by ion implantation.
[0073] In the present invention, the masks used for ion implantation are all made of silicon dioxide.
[0074] Next, an oxide layer 1001 and a gate 900 are formed sequentially from bottom to top on the upper surface of the N-type current spreading layer 700 .
[0075] Preferably, the oxide layer 1001 may be formed by a thermal oxidation method.
[0076] Preferably, polysilicon may be deposited on the oxide layer 1001 by chemical vapor deposition (eg, low pressure chemical vapor deposition) to form the gate 900 .
[0077] Then, the gate 900 and the oxide layer 1001 are etched to expose a portion of the upper surface of the P-well region 710 to form a source opening 1200 , and then an interlayer dielectric layer 1002 is formed on the gate 900 .
[0078] Preferably, the etching is reactive ion etching.
[0079] In some embodiments, the interlayer dielectric layer 1002 (i.e., silicon oxide) can be formed by oxidizing the gate 900 (i.e., polysilicon). The surface layer of the upper surface and the surface layer of the sidewall of the gate 900 are oxidized to silicon oxide. In other embodiments, the interlayer dielectric layer 1002 (i.e., silicon oxide) can be directly deposited on the upper surface and sidewall of the gate 900 by chemical vapor deposition.
[0080] Afterwards, a first N-type heavily doped source region 711 , a P-type heavily doped contact region 713 , and a second N-type heavily doped source region 712 are formed in a shallow layer on the upper surface of the P-well region 710 by ion implantation.
[0081] In some embodiments, Al ions are first injected into the P-well region 710 from the source opening 1200 to form a P-type heavily doped contact region 713 , and then N ions are injected into the P-well region 710 from the source opening 1200 to form a first N-type heavily doped source region 711 and a second N-type heavily doped source region 712 .
[0082] In the present application, ion implantation can be performed using conventional ion implantation methods in the art, and the present application does not limit this.
[0083] Next, the N-type substrate 1100 is removed.
[0084] Preferably, the N-type substrate 1100 may be removed by grinding.
[0085] Then, the P-type collector layer 200 is etched to expose a portion of the lower surface of the N-type buffer layer 500 , so as to form a first window 1300 .
[0086] In some embodiments, the width of the first window 1300 may be 1.1-1.5 μm, preferably 1.1-1.3 μm. The height of the first window 1300 is equal to the thickness of the P-type collector layer 200 .
[0087] Afterwards, an isolation layer 400 is formed at the first window 1300 , and then etching is performed upward from the lower surface of the isolation layer 400 to form a second window 1400 .
[0088] In some embodiments, the isolation layer 400 may be deposited by chemical vapor deposition. The isolation layer 400 may be silicon dioxide. The formed isolation layer 400 may cover the lower surface of the P-type collector layer 200.
[0089] In some embodiments, the method for forming the second window 1400 includes: etching upward from the lower surface of the isolation layer 400 until a portion of the N-type buffer layer 500 is etched and then stopped. The thickness of the etched portion of the N-type buffer layer 500 may be 0.5-1 μm, for example, 0.5 μm, 0.6 μm, 0.7 μm, 0.8 μm, 0.9 μm or 1 μm.
[0090] The width of the second window 1400 is 0.1-0.3 μm, preferably 0.1-0.2 μm, smaller than the width of the first window 1300 . A remaining portion of the isolation layer 400 exists between the second window 1400 and the P-type collector layer 200 .
[0091] Next, a polysilicon layer 300 is formed at the second window 1400 , and the lower surface of the polysilicon layer 300 is passivated.
[0092] Preferably, the polysilicon may be deposited by chemical vapor deposition (eg, low pressure chemical vapor deposition).
[0093] Preferably, the passivation includes: oxidizing the lower surface of the polysilicon to form a passivation layer. The passivation layer is silicon dioxide. After the passivation, the lower surface of the remaining polysilicon layer 300 is higher than the lower surface of the P-type collector layer 200, such as Figure 1 As shown in the figure. This design can prevent polysilicon from contacting the metal electrode, which will lead to the degradation of the forward conduction characteristics and the inability to improve the dynamic characteristics. After passivation, polysilicon and SiC form a heterojunction.
[0094] In some embodiments, when the isolation layer 400 covers the lower surface of the P-type collector layer 200, it is necessary to first remove the portion of the isolation layer 400 below the P-type collector layer 200 by grinding. When removing the excess portion of the isolation layer 400, a layer of isolation layer 400 should be retained on the lower surface of the polysilicon layer 300, so that the polysilicon layer 300 and the collector 100 are separated and no ohmic contact is formed.
[0095] Thereafter, the collector electrode 100 is formed below the P-type collector layer 200 .
[0096] Preferably, after forming the collector electrode 100 , high temperature annealing is performed.
[0097] The present invention does not limit the specific parameters of high temperature annealing, which can be selected according to actual needs. The temperature of high temperature annealing can be 1600-1700°C.
[0098] In the present invention, the collector electrode 100 may be manufactured by evaporation, sputtering, etc. The present invention does not limit the method for forming the collector electrode 100, and any conventional forming method in the art may be used to form the collector electrode 100 of the present invention.
[0099] Finally, a metal layer 800 is formed at the source opening 1200 .
[0100] Preferably, after the metal layer 800 is formed, laser annealing is performed.
[0101] The present invention does not limit the specific parameters of laser annealing, which can be selected according to actual needs. The temperature of laser annealing is generally greater than 800°C.
[0102] In the present invention, the metal layer 800 may be made by evaporation, sputtering, etc. The present invention does not limit the method for forming the metal layer 800, and any conventional forming method in the art may be used to form the metal layer 800 of the present invention.
[0103] The present invention will be further described below in conjunction with specific embodiments and drawings.
[0104] Example 1
[0105] First, at a doping concentration of 5×10 16 cm -3 The P-type collector layer 200 is epitaxially formed on the C surface of the N-type 4H-SiC substrate 1100 by chemical vapor deposition. The doping concentration of the P-type collector layer 200 is 1×10 19 cm -3 , thickness is 5μm.
[0106] Then, an N-type buffer layer 500 is epitaxially formed on the upper surface of the P-type collector layer 200 by chemical vapor deposition. The doping concentration of the N-type buffer layer 500 is 1.5×10 17 cm -3 , thickness is 2.5μm.
[0107] Then, an N-type drift layer 600 is epitaxially formed on the upper surface of the N-type buffer layer 500 by chemical vapor deposition. The resulting structure is as shown in FIG. Figure 2 As shown. The doping concentration of the N-type drift layer 600 is 4×10 14 cm -3 , thickness is 110μm.
[0108] Next, an N-type current spreading layer 700 is formed on the surface of the N-type drift layer 600 by ion implantation. The resulting structure is as shown in FIG. Figure 3 As shown. The doping concentration of the N-type current spreading layer 700 is 1×10 16 cm -3 , thickness is 2μm.
[0109] Then, a P-well region 710 is formed on the surface of the upper surface of the N-type current spreading layer 700 by ion implantation. The resulting structure is as shown in FIG. Figure 4 As shown. The doping concentration of the P-well region 710 is 1×10 17 , thickness is 1μm.
[0110] Afterwards, a silicon dioxide oxide layer 1001 with a thickness of 50 nm is formed on the upper surface of the N-type current spreading layer 700 by thermal oxidation. The obtained structure is as follows: Figure 5 As shown. Polysilicon with a thickness of 0.8 μm is deposited on the upper surface of the oxide layer 1001 by chemical vapor deposition to form a gate 900. The resulting structure is shown in FIG. Figure 6 shown.
[0111] Next, the gate 900 and the oxide layer 1001 are etched by a reactive ion etching process to expose a portion of the upper surface of the P-well region 710 to form a source opening 1200. The resulting structure is as shown in FIG. Figure 7 Then, the gate 900 is oxidized to form an interlayer dielectric layer 1002 on the gate 900. The resulting structure is as shown in FIG. Figure 8 shown.
[0112] Then, Al ions are first injected into the P-well region 710 from the source opening 1200 to form a P-type heavily doped contact region 713, and then N ions are injected into the P-well region 710 from the source opening 1200 to form a first N-type heavily doped source region 711 and a second N-type heavily doped source region 712. The resulting structure is as shown in FIG. Fig. 9 As shown. The doping concentration of the P-type heavily doped contact region 713 is 1×10 20 The thickness is 0.5 μm. The doping concentration of the first N-type heavily doped source region 711 and the second N-type heavily doped source region 712 are both 1×10 20 , the thickness is 0.5μm.
[0113] Afterwards, the N-type substrate 1100 is removed by grinding, and the resulting structure is as follows: Fig.10 shown.
[0114] Next, the P-type collector layer 200 is etched to expose a portion of the lower surface of the N-type buffer layer 500 to form a first window 1300. The resulting structure is as shown in FIG. Fig.11 As shown, the width of the first window 1300 is 1.1 μm. The height of the first window 1300 is equal to the thickness of the P-type collector layer 200 .
[0115] Then, silicon dioxide is deposited at the first window 1300 by chemical vapor deposition to form an isolation layer 400, which covers the lower surface of the P-type collector layer 200. The resulting structure is as shown in FIG. Fig.12Afterwards, etching is performed upward from the lower surface of the isolation layer 400 at the first window 1300 until a portion of the N-type buffer layer 500 is etched and then stopped to form a second window 1400. The resulting structure is shown in FIG. Fig.13 As shown, the thickness of the etched N-type buffer layer 500 is 0.5 μm. The width of the second window 1400 is 1 μm. There is a remaining portion of the isolation layer 400 between the second window 1400 and the P-type collector layer 200 .
[0116] Then, a polysilicon layer 300 is formed at the second window 1400 by chemical vapor deposition. The resulting structure is as shown in FIG. Fig.14 As shown, the lower surface of the polysilicon layer 300 is oxidized to form a passivation layer. The resulting structure is as shown in FIG. Fig.15 As shown. After passivation, the lower surface of the remaining polysilicon layer 300 is higher than the lower surface of the P-type collector layer 200. After passivation, polysilicon and SiC form a heterojunction. After passivation, the isolation layer 400 below the P-type collector layer 200 is removed by grinding, and the resulting structure is as shown. Fig.16 shown.
[0117] Next, a collector electrode 100 with a thickness of 5 μm is formed under the P-type collector layer 200 by a sputtering process. The collector electrode 100 is made of a titanium-aluminum alloy. Then, high-temperature annealing is performed. The resulting structure is as follows: Fig.17 shown.
[0118] Finally, a metal layer 800 is formed at the source opening 1200 by a sputtering process. The metal layer 800 is a nickel-titanium-aluminum alloy. Laser annealing is then performed. The resulting structure is as follows: Figure 1 shown.
[0119] The above is only a preferred specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention shall be based on the protection scope of the claims.
Claims
1. A planar gate IGBT device, characterized in that: include: collector; A P-type collector layer, the P-type collector layer covers a portion of the upper surface of the collector electrode; a polysilicon layer, the polysilicon layer being disposed above the collector electrode; an isolation layer, wherein the isolation layer isolates the polysilicon layer from the P-type collector layer and isolates the polysilicon layer from the collector electrode; An N-type buffer layer, the N-type buffer layer covers the upper surfaces of the polysilicon layer and the P-type collector layer, and the N-type buffer layer forms a heterojunction with the polysilicon layer; An N-type drift layer, wherein the N-type drift layer is disposed on an upper surface of the N-type buffer layer; An N-type current spreading layer, wherein the N-type current spreading layer is arranged on the upper surface of the N-type drift layer, and a P-well region is arranged on the surface layer of the upper surface of the N-type current spreading layer, and a first N-type heavily doped source region, a P-type heavily doped contact region, and a second N-type heavily doped source region are arranged in a shallow layer on the upper surface of the P-well region from left to right; a metal layer, the metal layer being in contact with the first N-type heavily doped source region, the P-type heavily doped contact region, and the second N-type heavily doped source region; A gate, the gate comprising a first gate and a second gate, and the first gate and the second gate are arranged on both sides of the metal layer; as well as a gate dielectric layer, the gate dielectric layer comprising an oxide layer and an interlayer dielectric layer, the oxide layer being arranged between the first gate and the N-type current spreading layer and between the second gate and the N-type current spreading layer, the interlayer dielectric layer being arranged between the first gate and the metal layer and between the second gate and the metal layer, and the interlayer dielectric layer covering upper surfaces of the first gate and the second gate; The upper surface of the polysilicon layer is higher than the upper surface of the P-type collector layer; the width of the polysilicon layer is 0.8-1.2μm, and the thickness is 1.5-4μm; the width of the isolation layer between the polysilicon layer and the P-type collector layer is 0.1-0.3μm, and the thickness of the isolation layer between the polysilicon layer and the collector is 0.1-0.5μm.
2. The planar gate IGBT device according to claim 1, characterized in that: The material of the P-type collector layer, the N-type buffer layer, the N-type drift layer, and the N-type current spreading layer are all SiC; and the gate is polysilicon.
3. The planar gate IGBT device according to claim 1, characterized in that: The height difference between the upper surface of the polysilicon layer and the upper surface of the P-type collector layer is 0.5-1 μm.
4. The planar gate IGBT device according to claim 1 or 2, characterized in that: The metal layer covers a portion of the upper surface of the first N-type heavily doped source region and the second N-type heavily doped source region, and covers the entire upper surface of the P-type heavily doped contact region.
5. The planar gate IGBT device according to claim 1 or 2, characterized in that: The metal layer covers the upper surface of the interlayer dielectric layer.
6. The method for preparing a planar gate IGBT device according to any one of claims 1 to 5, characterized in that: include: A P-type collector layer, an N-type buffer layer and an N-type drift layer are sequentially formed on the upper surface of the N-type substrate from bottom to top; forming an N-type current spreading layer on the surface layer of the upper surface of the N-type drift layer by ion implantation; Forming a P-well region on the surface layer of the upper surface of the N-type current spreading layer by ion implantation; Forming an oxide layer and a gate in sequence from bottom to top on the upper surface of the N-type current spreading layer; Etching the gate and the oxide layer to expose a portion of the upper surface of the P-well region to form a source opening, and then forming an interlayer dielectric layer on the gate; Forming a first N-type heavily doped source region, a P-type heavily doped contact region, and a second N-type heavily doped source region in a shallow layer on an upper surface of the P-well region by ion implantation; removing the N-type substrate; Etching the P-type collector layer to expose a portion of the lower surface of the N-type buffer layer to form a first window; forming an isolation layer at the first window, and then etching upward from the lower surface of the isolation layer to form a second window; forming a polysilicon layer at the second window, and passivating the lower surface of the polysilicon layer; forming a collector electrode below the P-type collector layer; and A metal layer is formed at the source opening.
7. The preparation method according to claim 6, characterized in that: The method for forming the second window includes: etching upward from the lower surface of the isolation layer until a portion of the N-type buffer layer is etched and then stopping.
8. The preparation method according to claim 6 or 7, characterized in that: The gate is made of polysilicon, and the method for forming the interlayer dielectric layer includes: oxidizing the gate.