A carbon-coated weak fiber grating array and its preparation method
By coating the surface of the optical fiber with a carbon film and polyimide layer, and using the method of direct writing of the grating array with femtosecond laser, the problem of poor performance of the fiber grating sensor in high temperature, high pressure, and high humidity environments has been solved, and the optical fiber has been realized. Long-term stable operation and improvement of mechanical strength.
Patent Information
- Application Number
- CN202211180484.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-27
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2042-09-27
AI Technical Summary
Conventional fiber Bragg grating sensors cannot work stably for a long time in the underground environment of high temperature, pressure, and high humidity, and the traditional preparation process will cause mechanical damage to the fiber surface.
A carbon-coated weak fiber grating array is used. By coating the fiber surface with a carbon film and a polyimide layer, the thermal CVD method and femtosecond laser are used to directly write the grating array to avoid mechanical damage during the stripping process and improve the resistance of the fiber. Thermal and mechanical strength.
Effectively prevents the impact of moisture and hydrogen on optical fibers, extends the service life of optical fibers in high temperature environments, and improves the mechanical strength and stability of the sensor.
Smart Images

Figure CN115453681B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a carbon-coated weak optical fiber grating array and a preparation method thereof, and belongs to the field of optical fiber grating sensing. Background Art
[0002] Weak fiber Bragg grating sensing technology has the advantages of strong anti-electromagnetic interference ability, high measurement accuracy, and the ability to achieve multi-parameter, long-distance, and distributed measurement. It has been widely used in the field of oil exploration.
[0003] The downhole environment of oil and gas wells is harsh. Conventional optical fiber coatings cannot prevent the influence of moisture and hydrogen on the mechanical strength and optical properties of optical fibers. The reason is that water molecules will diffuse to the surface of quartz optical fibers and react to cause surface defects of optical fibers, resulting in a decrease in optical fiber strength. Therefore, conventional grating sensors cannot adapt to the high-pressure and high-humidity environment downhole.
[0004] Conventional optical fiber coatings are polyurethane or acrylate, and the typical operating temperature of optical fiber is -40℃ ~ 85℃. This type of weak grating sensor cannot adapt to the high temperature environment underground.
[0005] In addition, traditional fiber gratings are prepared offline. After the fiber is prepared, the coating is removed, and then the grating is engraved with a laser, and finally the coating is applied. This "strip-write-recoat" method will cause greater mechanical damage to the surface of the optical fiber, making the sensor strength lower.
[0006] Therefore, in order to ensure that the weak fiber Bragg grating sensor can work stably for a long time in harsh environments such as high temperature, high pressure, and high humidity, it is necessary to study a weak fiber Bragg grating array and its preparation method for special environments. Summary of the invention
[0007] The purpose of the present invention is to provide a carbon-coated weak fiber grating array to solve the problems of poor performance and poor preparation process of the existing weak grating array under specific environments.
[0008] In the carbon-coated weak fiber grating array of the present invention, a layer of carbon film is coated on the surface of the optical fiber. The carbon film has a blocking effect on moisture and hydrogen, has small shrinkage on the surface of the optical fiber, has stable chemical properties, can effectively slow down the growth of micro cracks on the surface of the optical fiber, and delays the fatigue process of mechanical strength, thereby increasing the service life of the optical fiber.
[0009] In the carbon-coated weak fiber grating array of the present invention, the carbon film is coated with a polyimide layer. Polyimide is a polymer material with high heat resistance, good mechanical strength and excellent comprehensive performance. Polyimide is used as a fiber coating material and can work at 300°C to 350°C for a long time, thereby extending the service life of the optical fiber in a high temperature environment.
[0010] Specifically, the carbon-coated weak fiber grating array provided by the present invention comprises a core and a cladding outside the core;
[0011] The cladding is sequentially coated with a carbon coating, a first polyimide coating and a second polyimide coating;
[0012] A weak fiber grating array is engraved on the fiber core;
[0013] The thickness of the carbon coating is 30 to 50 nm;
[0014] The thickness of the first polyimide coating is 3-5 um, and the thickness of the second polyimide coating is 5-10 um.
[0015] The reflectivity of the weak fiber grating array is less than 1%.
[0016] The carbon-coated weak fiber grating array provided by the present invention can be prepared according to the following method:
[0017] S1, preparing a bare optical fiber comprising the core and the cladding;
[0018] S2, preparing the carbon coating on the surface of the bare optical fiber by a thermal CVD method;
[0019] S3, using a femtosecond laser to write a grating on the surface of the bare optical fiber through the carbon coating;
[0020] S4, sequentially preparing the first polyimide coating and the second polyimide coating outside the carbon coating by a thermal curing method;
[0021] S5, moving the bare optical fiber by a preset length to the next grating to be written, and then repeating steps S2-S4 until a final weak fiber grating array is formed.
[0022] In the above-mentioned preparation method, in step S1, the preform rod is heated and drawn on an optical fiber drawing tower to form the bare optical fiber.
[0023] In the above preparation method, in step S2, the conditions of the thermal CVD method are as follows:
[0024] The bare optical fiber to be coated passes through a carbon coating reaction chamber, a carbon source is introduced into the carbon coating reaction chamber, and the carbon source is heated to 900° C. to 1100° C., so as to form the carbon coating on the surface of the bare optical fiber;
[0025] The carbon source is gas such as acetylene, ethylene, and methane.
[0026] In the above-mentioned preparation method, in step S3, femtosecond laser with a wavelength of 800 nm is used for writing.
[0027] In the above-mentioned preparation method, in step S4, the steps of the thermal curing method are as follows:
[0028] The grating is sequentially passed through a first polyimide coating device and a second polyimide coating device to dip-coat the polyimide coating on the surface of the optical fiber to form the first polyimide coating and the second polyimide coating.
[0029] In the above-mentioned preparation method, the viscosity of the polyimide coating prepared in the first polyimide coating device is 5000-6500 cps, and the Young's modulus is 600-1000 MPa;
[0030] The viscosity of the polyimide coating prepared in the second polyimide coating device is 6000-8000 cps, and the Young's modulus is 1.5-2.5 Gpa.
[0031] Traditional fiber gratings are mostly prepared offline. After the fiber is prepared, the coating is removed, and then the grating is written by laser, and finally the coating is applied. This "strip-write-recoat" method will cause greater mechanical damage to the fiber surface, making the sensor strength lower. The present invention adopts the method of direct writing grating array through the coating by femtosecond laser, without stripping the coating, avoiding the mechanical damage to the fiber caused by the stripping process.
[0032] The carbon-coated weak fiber grating array provided by the present invention effectively prevents moisture and hydrogen from affecting the mechanical strength and optical properties of the optical fiber by coating a layer of carbon film on the surface of the optical fiber, and prolongs the service life of the optical fiber in a high temperature environment by using polyimide as the optical fiber coating material. By directly writing the grating array through the coating with a femtosecond laser, the optical fiber surface will not be damaged, thereby improving the mechanical strength of the sensor. The present invention solves the problem that conventional weak fiber grating sensors cannot work stably for a long time in harsh environments such as high temperature, high pressure, and high humidity. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 It is a structural schematic diagram of the carbon-coated weak fiber grating array provided by the present invention.
[0034] Figure 2 It is a schematic diagram of the preparation process of the carbon-coated weak fiber grating array provided by the present invention. DETAILED DESCRIPTION
[0035] The present invention will be further described below in conjunction with the accompanying drawings, but the present invention is not limited to the following embodiments.
[0036] like Figure 1As shown, it is a schematic diagram of the structure of the carbon-coated weak fiber grating array provided by the present invention: it includes a core 1, a weak fiber grating array 2 engraved on the core 1, a cladding 3 outside the core 1, a carbon coating 4 outside the cladding, a first polyimide coating 5 outside the carbon coating 4, and a second polyimide coating 6 outside the first polyimide coating 5.
[0037] The carbon coating 4 is prepared by a thermal CVD process, and the thickness of the carbon coating 4 is 30-50 nm.
[0038] The weak fiber grating array 2 is prepared by direct writing on the fiber core 1 through a femtosecond laser through the carbon coating 4, and the wavelength of the femtosecond laser used for preparation is 800nm. The reflectivity of the weak fiber grating array 2 should be less than 1%.
[0039] The thickness of the first polyimide coating layer 5 is 3 um, and the thickness of the second polyimide coating layer 6 is 7 um.
[0040] like Figure 2 As shown, it is a schematic diagram of the preparation method of the carbon-coated weak fiber grating array provided by the present invention, which provides some key steps or devices, but these steps or devices are only examples, and other steps may need to be performed or other auxiliary devices may be used in the embodiments of the present invention.
[0041] 1) heating and drawing the preform rod 7 on the optical fiber drawing tower 8 to form a bare optical fiber including a core 1 and a cladding 3;
[0042] 2) Forming a carbon coating layer on the optical fiber surface by thermal CVD method: the bare optical fiber to be coated passes through a carbon coating reaction chamber 9, and hydrocarbon gas, such as C2H2 and CH4, is passed into the reaction chamber. These gases are heated to 900°C to 1100°C as carbon sources. The gases are repeatedly polymerized on the optical fiber surface to undergo a dehydrogenation reaction, forming an amorphous carbon film with a thickness of 30 to 50 nm - a carbon coating 4;
[0043] 3) using a femtosecond laser 10 with a wavelength of 800 nm to directly write on the core and cladding through the carbon coating layer to prepare the grating 11;
[0044] 4) Forming the first polyimide coating 5 by thermal curing: After the grating is written, the optical fiber enters the first polyimide coating device 12, which is equipped with a polyimide coating with a viscosity of 5000-6500cps and a Young's modulus of about 600Mpa. When the optical fiber passes through the device, a uniform coating solution is applied to the surface of the optical fiber, and then the first polyimide coating with a thickness of 3um is formed by thermal curing.
[0045] 5) Forming a second polyimide coating 6 by thermal curing: The optical fiber enters the second polyimide coating device 13, where the optical fiber is coated with a second polyimide coating with a thickness of 7 um. The viscosity of the polyimide coating used in this step is 6000-8000 cps, and the Young's modulus of the coating is 2 Gpa.
[0046] 6) By controlling the fiber take-up plate 14, the optical fiber is moved to the preset length to the next grating to be written, and then the above steps (2) to (5) are repeated until the final weak fiber grating array 2 is formed.
[0047] Optical fiber loss test:
[0048] The carbon-coated weak fiber grating array prepared in this embodiment has a length of 1 km, a closed chamber temperature of 85° C., a hydrogen pressure of 10 atmospheres, and a time of 10 days. The attenuation of the optical fiber at 1240 nm is measured, and the additional loss is less than 0.2 dB / km.
[0049] The length of G625D conventional single-mode optical fiber is 1KM, the temperature of the closed chamber is 85℃, the hydrogen pressure is 10 atmospheres, the time is 5 days, and the attenuation of the optical fiber at 1240nm is measured. The additional loss reaches 30dB / km.
Claims
1. A carbon-coated weak fiber grating array, comprising a core and a cladding outside the core; The cladding is sequentially coated with a carbon coating, a first polyimide coating and a second polyimide coating; The thickness of the carbon coating is 30-50 nm; The thickness of the first polyimide coating is 3-5 um, and the thickness of the second polyimide coating is 5-10 um; A weak fiber grating array is engraved on the fiber core; The method for preparing the carbon-coated weak fiber grating array comprises the following steps: S1, preparing a bare optical fiber comprising the core and the cladding; S2, preparing the carbon coating on the surface of the bare optical fiber by a thermal CVD method; S3, using a femtosecond laser to write a grating on the surface of the bare optical fiber through the carbon coating; S4, sequentially preparing the first polyimide coating and the second polyimide coating outside the carbon coating by a thermal curing method; In step S4, the steps of the thermal curing method are as follows: Passing the grating through a first polyimide coating device and a second polyimide coating device in sequence, so as to dip-coat the polyimide coating on the surface of the optical fiber to form the first polyimide coating and the second polyimide coating; The viscosity of the polyimide coating prepared in the first polyimide coating device is 5000-6500 cps, and the Young's modulus is 600-1000 MPa; The viscosity of the polyimide coating prepared in the second polyimide coating device is 6000-8000 cps, and the Young's modulus is 1.5-2.5 Gpa; S5, moving the bare optical fiber by a preset length to the next grating to be written, and then repeating steps S2-S4 until a final weak fiber grating array is formed.
2. The carbon-coated weak fiber grating array according to claim 1, characterized in that: The reflectivity of the weak fiber grating array is less than 1%.
3. The method for preparing the carbon-coated weak fiber grating array according to claim 1 or 2, comprising the following steps: S1, preparing a bare optical fiber comprising the core and the cladding; S2, preparing the carbon coating on the surface of the bare optical fiber by a thermal CVD method; S3, using a femtosecond laser to write a grating on the surface of the bare optical fiber through the carbon coating; S4, sequentially preparing the first polyimide coating and the second polyimide coating outside the carbon coating by a thermal curing method; In step S4, the steps of the thermal curing method are as follows: Passing the grating through a first polyimide coating device and a second polyimide coating device in sequence, so as to dip-coat the polyimide coating on the surface of the optical fiber to form the first polyimide coating and the second polyimide coating; The viscosity of the polyimide coating prepared in the first polyimide coating device is 5000-6500 cps, and the Young's modulus is 600-1000 MPa; The viscosity of the polyimide coating prepared in the second polyimide coating device is 6000-8000 cps, and the Young's modulus is 1.5-2.5 Gpa; S5, moving the bare optical fiber by a preset length to the next grating to be written, and then repeating steps S2-S4 until a final weak fiber grating array is formed.
4. The preparation method according to claim 3, characterized in that: In step S1, the preform rod is heated and drawn on an optical fiber drawing tower to form the bare optical fiber.
5. The preparation method according to claim 3 or 4, characterized in that: In step S2, the conditions of the thermal CVD method are as follows: The bare optical fiber to be coated passes through a carbon coating reaction chamber, a carbon source is introduced into the carbon coating reaction chamber, and the carbon source is heated to 900° C. to 1100° C., so as to form the carbon coating on the surface of the bare optical fiber; The carbon source is acetylene, ethylene or methane.
6. The preparation method according to claim 3 or 4, characterized in that: In step S3, femtosecond laser with a wavelength of 800 nm is used for writing.
Citation Information
Patent Citations
High-temperature resistant optical fiber and method for manufacturing same
CN101726792A
High-temperature-resistance optical fiber
CN103777269A
Packaging method for structural mechanics sensor of femtosecond laser direct writing grating
CN107560643A
Double-coated layer weak fiber grating array and preparation method thereof
CN109085675A
Special fiber Bragg grating suitable for marine environment and preparation method thereof
CN111025457A