Growth equipment

By designing porous partitions and opening and closing mechanisms in silicon carbide growth equipment, the replenishment of silicon materials and gas component control is achieved, the problem of insufficient silicon supplementation in the PVT process is solved, and the quality and stability of silicon carbide crystals are significantly improved.

CN115595657BActive Publication Date: 2024-11-19SHENZHEN TRENCH R SEMIC CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211336957.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-10-28
Publication Date
2024-11-19
Estimated Expiration
2042-10-28

AI Technical Summary

Technical Problem

The existing PVT process of silicon carbide single crystal growth method cannot supplement silicon during growth, resulting in low crystal quality and high defect density, making it difficult to meet the needs of high power and radiation-resistant devices.

Method used

A growth device is designed, including a crystal growth cavity, a gas buffer cavity and a silicon source replenishment cavity in the crucible. The communication and isolation of the gas and the silicon source are controlled through a porous partition and a closing mechanism, and the first and second heating members are used. Adjust the temperature to achieve the replenishment of silicon material and control of gas component ratio.

Benefits of technology

By replenishing silicon materials during the growth process and adjusting the carbon-rich growth environment, the crystal quality is significantly improved, the defect density is reduced, the stable growth of the crystal is maintained, and the quality of 4H-SiC crystal is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115595657B_ABST
    Figure CN115595657B_ABST
Patent Text Reader

Abstract

The present invention provides a growth device, including a crucible, wherein the crucible includes a crystal growth chamber, a gas buffer chamber and a silicon source supplement chamber arranged in sequence from top to bottom; a porous partition and an opening and closing mechanism are arranged in the crucible, the porous partition is arranged between the crystal growth chamber and the gas buffer chamber, and the opening and closing mechanism is arranged between the gas buffer chamber and the silicon source supplement chamber; a first heating component and a second heating component are arranged outside the crucible, the first heating component is arranged corresponding to the growth chamber and the gas buffer chamber, and the second heating component is arranged corresponding to the silicon source supplement chamber. When a carbon-rich state occurs, the second heating component can be turned on to heat and sublimate the silicon material in the silicon source supplement chamber, and the opening and closing mechanism is opened at the same time, and the sublimated silicon material enters the gas buffer chamber through the opening and closing mechanism; the first heating component makes the silicon material reach the same temperature as the crystal growth chamber, and then slowly releases it into the crystal growth chamber through the porous partition, thereby achieving the purpose of replenishing silicon and improving the quality of the crystal.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor preparation, and in particular to a growth device. Background Art

[0002] As a third-generation wide bandgap semiconductor material, silicon carbide has the characteristics of high thermal conductivity, high breakdown electric field, high radiation resistance, etc. Since 4H-SiC has better electrical properties among many crystal forms and meets the needs of today's technological development for substrate materials such as high-power and radiation-resistant devices, how to grow high-quality 4H-SiC crystals has become a primary issue.

[0003] At present, the main growth method for producing silicon carbide single crystals in industry is physical vapor transport (PVT). Since this growth method is carried out in a closed graphite crucible, the gas in the crucible has more carbon elements due to long-term high temperature, and the carbon-silicon ratio of the gas phase components affects the crystal morphology and crystal quality, so it is particularly important to reasonably control the gas phase component ratio in the later stage of growth.

[0004] The current PVT process cannot replenish silicon during growth. In order to improve crystal quality and reduce defect density, a growth crucible that can replenish the silicon source is needed. Summary of the invention

[0005] The present invention provides a growth device, which can supplement silicon material during the growth process and improve the crystal quality.

[0006] The present invention provides a growth device for growing silicon carbide material, comprising a crucible, wherein the crucible comprises a crystal growth chamber, a gas buffer chamber and a silicon source supplement chamber which are arranged in sequence from top to bottom;

[0007] A porous partition and an opening and closing mechanism are arranged in the crucible, wherein the porous partition is arranged between the crystal growth chamber and the gas buffer chamber, and the opening and closing mechanism is arranged between the gas buffer chamber and the silicon source replenishing chamber, and is used to control the connection and isolation between the gas buffer chamber and the silicon source replenishing chamber;

[0008] The crucible is provided with a first heating component and a second heating component, the first heating component is provided corresponding to the growth chamber and the gas buffer chamber, and the second heating component is provided corresponding to the silicon source supplement chamber.

[0009] Wherein, the volume ratio of the crystal growth chamber to the gas buffer chamber is 1.8:1-2.2:1, and the volume ratio of the gas buffer chamber to the silicon source supplement chamber is 1.8:1-2.2:1.

[0010] Wherein, the first heating member surrounds the outer wall of the crucible; and the hole density of the peripheral area of ​​the porous partition is greater than the hole density of the central area thereof.

[0011] Wherein, the second heating component is arranged around the outer wall of the crucible; or the thickness of the porous partition is 0.5-1.5 cm.

[0012] Wherein, the opening and closing mechanism includes a silicon source partition, and the silicon source partition is provided with an opening and closing seam, and the opening and closing seam is a multiple bend shape arranged along the plate surface of the silicon source partition; the silicon source partition is divided into two sub-partitions through the opening and closing seam, and at least one of the sub-partitions is movably connected to the crucible so that the two sub-partitions can abut and separate; when the two sub-partitions are abutted, the opening and closing seam is in a closed state, and the gas buffer chamber is isolated from the silicon source replenishing chamber; when the first sub-partition is separated from the second sub-partition, the gas buffer chamber is connected with the silicon source replenishing chamber through the opening and closing seam.

[0013] Wherein, the opening and closing seam is in a square wave shape, or a sawtooth shape, or a sine wave shape, or a trapezoidal wave shape.

[0014] The two sub-partitions are respectively a first sub-partition and a second sub-partition, the first sub-partition is slidably disposed on the crucible along the axial direction of the crucible, and the second sub-partition is fixed to the crucible.

[0015] Among them, the growth equipment also includes a driving rod, and a driving hole is provided on the crucible, the driving hole connects the outer wall of the crucible and the silicon source replenishing chamber, the driving rod passes through the driving hole, one end of the driving rod is connected to the first sub-partition, and the other end is connected to a driving device; the driving device is arranged on the outside of the crucible, and is used to drive the driving rod to move, so that the driving rod drives the first sub-partition to move along the axial direction of the crucible.

[0016] Wherein, the driving hole is arranged on the side wall of the crucible, the driving rod is connected to the driving hole by rotating around its own axis, a cam is fixed to one end of the driving rod, and the circumferential surface of the cam abuts against the first sub-partition; the driving device is a motor to drive the driving rod to rotate around its own axis, so that the cam drives the first sub-partition to move in the vertical direction; or,

[0017] The driving hole is arranged on the bottom wall of the crucible, the driving rod is slidably connected to the driving hole in a vertical direction, and the driving device is a cylinder to drive the driving rod to move in a vertical direction, thereby causing the first sub-partition plate to move in a vertical direction.

[0018] Wherein, the opening and closing seam has two opening and closing surfaces arranged opposite to each other, and the two opening and closing surfaces are respectively arranged on the two sub-partitions; when the two sub-partitions are in contact, the two opening and closing surfaces are in contact with each other; when the two sub-partitions are separated, the two opening and closing surfaces are separated;

[0019] The direction in which the two sub-partitions move relative to each other is an opening and closing direction, and the angle between the two opening and closing surfaces and the opening and closing direction is an acute angle.

[0020] The growth device provided by the present invention can open the second heating component to heat and sublimate the silicon material in the silicon source replenishing chamber when a carbon-rich state occurs, and at the same time open the opening and closing mechanism to connect the silicon source replenishing chamber with the gas buffer chamber, and the sublimated silicon material enters the gas buffer chamber through the opening and closing mechanism; the first heating component can heat the sublimated silicon material to the same temperature as the crystal growth chamber, and then slowly release it into the crystal growth chamber through the porous partition, thereby achieving the purpose of replenishing silicon, adjusting the carbon-rich growth environment, avoiding defects caused by carbon-rich growth, and improving the crystal quality; by setting up the gas buffer chamber, the silicon material can enter the crystal growth chamber after being heated to the growth temperature, avoiding crystal field fluctuations caused by the supplemented silicon, and maintaining the stable growth of the crystal. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for use in the embodiments. The drawings described below are only drawings corresponding to some embodiments of the present invention.

[0022] Figure 1 is a structural cross-sectional view of a growth device provided by a preferred embodiment of the present invention;

[0023] Figure 2 yes Figure 1 Top view of the meso-growth device;

[0024] Figure 3 yes Figure 1 Bottom view of the meso-growth device;

[0025] Figure 4 yes Figure 1 A schematic diagram of the structure of the opening and closing mechanism of the meso-growth device;

[0026] Figure 5 yes Figure 1 A cross-sectional view of the structure of the mid-growth device when replenishing silicon;

[0027] Figure 6 yes Figure 4 Schematic diagram of the structure of the middle opening and closing mechanism when replenishing silicon;

[0028] Figure 7It is a structural cross-sectional view of a growth device provided by another embodiment of the present invention.

[0029] Figure 8 yes Figure 7 A cross-sectional view of the structure of the mid-growth device when replenishing silicon;

[0030] Fig. 9 is a structural schematic diagram of an opening and closing mechanism provided by yet another embodiment of the present invention;

[0031] Fig.10 yes Fig. 9 Schematic diagram of the structure of the middle opening and closing mechanism when replenishing silicon. DETAILED DESCRIPTION

[0032] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.

[0033] The terms "first", "second", etc. in the present invention are used for descriptive purposes only and should not be understood as indicating or implying relative importance, and should not be used as a limitation on the order of precedence.

[0034] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0035] See also Figure 1 A preferred embodiment of the present invention provides a growth device, including a crucible 10. The cavity in the crucible 10 is used to generate crystals and replenish silicon sources. A heating component is arranged outside the crucible 10 to heat the material in the cavity to provide a generation temperature.

[0036] The crucible 10 includes a crystal growth chamber 101, a gas buffer chamber 102, and a silicon source supplement chamber 103 for placing silicon materials, which are arranged in sequence from top to bottom. A porous partition 20 and an opening and closing mechanism 30 are arranged in the crucible 10. The porous partition 20 is arranged between the crystal growth chamber 101 and the gas buffer chamber 102. The porous partition 20 is made of a porous loose material with air permeability to ensure uniform gas penetration. Preferably, the porous partition 20 is made of graphite.

[0037] In this embodiment, the growth device is mainly used to grow silicon carbide materials, such as silicon carbide substrates or crystals.

[0038] The crystal growth chamber 101 is used to place silicon carbide powder 109, the porous partition 20 is used to carry the silicon carbide powder 109, and the seed crystal 108 is pasted on the inner side of the top of the crystal growth chamber 101. The gas buffer chamber 102 is located in the middle part of the crucible 10, and the gas buffer chamber 102 and the crystal growth chamber 101 are separated by the porous partition 20. The bottom of the crucible 10 is the silicon source replenishment chamber 103, and the opening and closing mechanism 30 is arranged between the gas buffer chamber 102 and the silicon source replenishment chamber 103, which is used to control the connection and isolation between the gas buffer chamber 102 and the silicon source replenishment chamber 103. The required silicon material is placed in the silicon source replenishment chamber 103.

[0039] The crucible 10 is provided with a first heating member 41 and a second heating member 42. The first heating member 41 is provided corresponding to the growth chamber and the gas buffer chamber 102, and the second heating member 42 is provided corresponding to the silicon source replenishing chamber 103. The first heating member 41 and the second heating member 42 are both induction coils.

[0040] Two independently controlled heating components, a first heating component 41 and a second heating component 42, are arranged outside the crucible 10. The first heating component 41 provides the temperature required for crystal growth, and can heat the temperature in the crystal growth chamber 101 and the gas buffer chamber 102 to about 2700°C. The second heating component 42 is used to provide the temperature required for sublimation of silicon material, and can heat the silicon source replenishment chamber 103 to about 1400°C.

[0041] In the early stage of crystal growth, Figure 1 and Figure 2 As shown, the first heating member 41 is in the open state, the opening and closing mechanism 30 is in the closed state, and the crystal growth in the crystal growth chamber 101 is in a state where the silicon component and the carbon component are in balance. As the crystal growth proceeds, the gas phase components in the crystal growth chamber 101 gradually become unbalanced and carbon-rich. At this time, the second heating member 42 is turned on to heat and sublimate the silicon material in the silicon source replenishment chamber 103, and the opening and closing mechanism 30 is opened at the same time. Figure 5 and Figure 6 As shown, the silicon source replenishing chamber 103 is connected to the gas buffer chamber 102, so that the sublimated silicon material enters the gas buffer chamber 102 through the opening and closing mechanism 30; the first heating component 41 can heat the sublimated silicon material to reach the same temperature as the crystal growth chamber 101, and then slowly release it into the crystal growth chamber 101 through the porous partition 20, thereby achieving the purpose of replenishing silicon material, adjusting the carbon-rich growth environment, avoiding defects caused by carbon-rich growth, and improving crystal quality.

[0042] Since the temperature in the crystal growth chamber 101 is much higher than the temperature in the silicon source supplement chamber 103, a gas buffer chamber 102 is required to perform temperature transition to prevent the silicon material with a lower temperature from directly entering the crystal growth chamber 101 and affecting the crystal growth. By setting up the gas buffer chamber 102, the silicon material can enter the crystal growth chamber 101 after being heated to the growth temperature, thereby avoiding the crystal field fluctuation caused by the supplement silicon and maintaining the stable growth of the crystal.

[0043] The silicon carbide crystal growth crucible provided by the present invention can solve the technical problems caused by the carbon-rich environment during the crystal growth process by supplementing silicon material during the growth process, and at the same time avoids the growth environment fluctuation caused by the introduction of external gas during the production process, so that the PVT method for growing 4H-SiC greatly improves the crystal quality.

[0044] The volume ratio of the crystal growth chamber 101 to the gas buffer chamber 102 is 1.8:1-2.2:1, and the volume ratio of the gas buffer chamber 102 to the silicon source replenishing chamber 103 is 1.8:1-2.2:1. In this embodiment, the volume ratios of the crystal growth chamber 101, the gas buffer chamber 102, and the silicon source replenishing chamber 103 are 4:2:1 respectively. The volume ratios of the three make the gas buffer chamber 102 have a suitable size, so that the silicon source gas can be effectively heated in the gas buffer chamber 102 before entering the crystal growth chamber 101, and the overall volume of the crucible 10 will not be too large.

[0045] In this embodiment, the crucibles 10 are all in the shape of straight cylinders, and their cross-sections at all axial locations are the same. Therefore, the height ratio of the crystal growth chamber 101, the gas buffer chamber 102, and the silicon source replenishment chamber 103 is the volume ratio of the three, which is convenient for setting the proportions of the three and allows the silicon-containing gas to move upward more evenly.

[0046] like Figure 2 As shown, the first heating member 41 surrounds the outer wall of the crucible 10, that is, the first heating member 41 surrounds the outer wall of the growth chamber 101 and the gas buffer chamber 102, so as to fully heat the crystal growth chamber 101 and the gas buffer chamber 102. Here, in other embodiments, the first heating member can also be attached to the inner wall of the growth chamber and the gas buffer chamber.

[0047] The pore density of the peripheral area 20b of the porous partition 20 is greater than the pore density of the central area 20a thereof. It can be understood that the peripheral area 20b of the porous partition 20 refers to an area relatively close to the side wall of the crucible 10, and the central area of ​​the porous partition 20 refers to the central position area of ​​the porous partition 20, which is relatively far away from the side wall of the crucible 10.

[0048] Since the first heating member 41 is located at the periphery of the porous partition 20, the pore density of the peripheral region 20b of the porous partition 20 is greater than the pore density of the central region 20a, which can enhance the heat flow at the periphery, thereby making the temperature of the silicon source entering the crystal growth region more uniform. Here, in other embodiments, the porous partition 20 can also be a graphite plate with uniform pore density.

[0049] like Figure 3 As shown, the second heating component 42 surrounds the outer wall of the crucible 10, that is, the second heating component 42 is arranged around the outer wall of the silicon source replenishing chamber 103 to fully heat the silicon source replenishing chamber 103 on all sides. In other embodiments, the second heating component can be arranged around the inner wall of the silicon source replenishing chamber 103; the second heating component 42 can also be set at the bottom of the crucible 10, or the second heating component 42 can be set on all sides and the bottom of the crucible 10.

[0050] The thickness of the porous partition 20 is 0.5-1.5 cm, so that the porous partition 20 can have a certain bearing capacity, effectively support the silicon carbide raw material, and allow the silicon source to better pass through the porous partition 20, and the thickness of the porous partition 20 will not have a significant impact on the volume of the entire crucible 10.

[0051] In this embodiment, Figure 4 and Figure 6 As shown, the opening and closing mechanism 30 includes a silicon source separator, and an opening and closing seam 301 is arranged on the silicon source separator, and the opening and closing seam 301 is a multiple bending shape arranged along the plate surface of the silicon source separator. As a preference, the silicon source separator is also made of graphite.

[0052] The silicon source partition is divided into two sub-partitions by an opening and closing seam 301. In this embodiment, for the convenience of description, the two sub-partitions are respectively a first sub-partition 31 and a second sub-partition 32. At least one of the sub-partitions is movably connected to the crucible 10, so that the first sub-partition 31 and the second sub-partition 32 can abut and separate; when the first sub-partition 31 and the second sub-partition 32 abut, the opening and closing seam 301 is in a closed state, and the gas buffer chamber 102 is isolated from the silicon source supplement chamber 103; when the first sub-partition 31 and the second sub-partition 32 are separated, the gas buffer chamber 102 and the silicon source supplement chamber 103 are connected through the opening and closing seam 301.

[0053] When the two sub-partitions move relative to each other, the two sub-partitions can abut or separate from each other, so that the opening and closing slit 301 is closed or opened. The opening and closing slit 301 is a multi-bend shape, which can increase the length of the opening and closing slit 301, so that the silicon source can enter the gas replenishment chamber more evenly from the bottom, and the opening size can be adjusted by the longitudinal distance between the sub-partitions.

[0054] In this embodiment, the opening and closing seam 301 is in a square wave shape for easy processing and preparation. Here, in other embodiments, the opening and closing seam 301 may also be in a sawtooth shape, a sine wave shape, or other reciprocating bending shapes, and the opening and closing seam may also be in other forms of multiple bending shapes, for example, the opening and closing seam may be in a spiral bending shape similar to a mosquito coil, or a zigzag bending shape, etc.

[0055] In this embodiment, the first sub-partition 31 is slidably disposed on the crucible 10 along the axial direction of the crucible 10, and the second sub-partition 32 is fixedly disposed on the crucible 10. A sliding structure may be provided between the first sub-partition 31 and the crucible 10 to achieve relative sliding between the two. For example, a protrusion may be provided on the first sub-partition 31, and a strip groove is provided vertically on the inner wall of the crucible 10. The protrusion is slidably disposed in the strip groove to achieve sliding cooperation between the two. The cooperation between the protrusion and the strip groove may be multiple groups to achieve the stability of the sliding of the first sub-partition 31.

[0056] The silicon carbide crystal growth crucible also includes a driving rod 51. A driving hole 105 is provided on the crucible 10. The driving hole 105 connects the outer wall of the crucible 10 with the silicon source replenishing chamber 103. The driving rod 51 movably passes through the driving hole 105. One end of the driving rod 51 is connected to the first sub-partition 31 of the opening and closing mechanism 30, and the other end is connected to the driving device 52. The driving device 52 is arranged on the outside of the crucible 10.

[0057] The driving device 52 can drive the driving rod 51 to move, so that the driving rod 51 can drive the first sub-partition 31 to move along the axial direction of the crucible 10, thereby realizing the opening and closing of the opening and closing gap 301. The driving rod 51 can be made of a high temperature resistant material, and the driving device 52 is arranged outside the crucible 10 to avoid the influence of the high temperature environment on the driving device 52.

[0058] More specifically, in this embodiment, Figure 1 As shown, the driving hole 105 is arranged on the side wall of the crucible 10, and the driving rod 51 is connected to the driving hole 105 by rotating around its own axis. A cam 53 is fixed to one end of the driving rod 51, and the circumferential surface of the cam 53 abuts against the first sub-partition 31. The driving device 52 is a motor. The driving device 52 drives the driving rod 51 to rotate around its own axis, and the driving rod 51 drives the cam 53 to rotate. The cooperation between the circumferential surface of the cam 53 and the first sub-partition 31 is utilized to realize the up and down movement of the first sub-partition 31. When the first sub-partition 31 moves to be higher than or lower than the second sub-partition 32, the first sub-partition 31 is separated from the second sub-partition 32, the opening and closing seam 301 is opened, and the gas buffer chamber 102 is connected to the silicon source replenishing chamber 103, and the silicon source in the silicon source replenishing chamber 103 can enter the gas buffer chamber 102.

[0059] When the present invention realizes silicon source replenishment, the second heating component 42 is first turned on to sublimate the silicon material in the silicon source replenishment chamber 103 into silicon-containing gas, and then the opening and closing mechanism 30 is turned on to form a gas passage to the gas buffer chamber 102. The silicon atmosphere in the gas buffer chamber 102 is adjusted to the same temperature as the crystal growth chamber 101 by the first heating component 41, and is slowly released into the crystal growth chamber 101 through the porous partition 20, thereby replenishing the silicon source, adjusting the carbon-rich growth environment, and avoiding defects caused by carbon-rich growth. Setting the gas buffer chamber 102 can avoid the crystal temperature field fluctuation caused by the replenishment of the silicon source and maintain the stable growth of the crystal.

[0060] In the above embodiment, a motor is used as a driving device, the driving hole 105 is located on the side wall of the crucible 10, the driving rod 51 is rotatably disposed in the driving hole, and the relative movement of the two sub-partitions is achieved by the cooperation between the driving rod 51 and the cam 53. Figure 7 and Figure 8 As shown, the driving hole 105a can also be set on the bottom wall of the crucible 10a, and the driving rod 51a is slidably connected to the driving hole 105a in the vertical direction. One end of the driving rod 51a is connected to the first sub-partition 31a, and the other end is connected to the driving device 52a. The driving device 52a is a cylinder, and the cylinder is used to drive the driving rod 51a to move up and down, thereby moving the first sub-partition 31a up and down. This structure can make the cylinder located at the bottom of the crucible 10a, further away from the second heating member, to prevent its operation from being affected by high temperature. Furthermore, a sealed shell 11a can be provided on the outer wall of the crucible 10a, and the sealed shell 11a covers the outside of the driving hole 105a, the driving device 52a is arranged on the outside of the sealed shell 11a, and the driving rod 51a passes through the sealed shell 11a; since there may be a gap between the driving hole 105a and the driving rod 51a, causing a small amount of vaporized silicon source to leak out, the sealed shell 11a can be used to accommodate the leaked silicon source, and a sealing structure can be set between the driving rod 51a and the sealed shell 11a, and the sealing structure is relatively far away from the silicon source replenishing chamber 103a to ensure the sealing performance.

[0061] In the above two embodiments, the cooperation of the driving device and the driving rod can effectively realize the up and down movement of the first sub-partition. Here, as another embodiment, the driving device and the driving rod may not be provided. When the second heating component is started, a vaporized silicon source is formed in the silicon source replenishing chamber, and the pressure in the silicon source replenishing chamber increases. The air pressure can be used to push open the first sub-partition, so that the first sub-partition moves upward. Here, the first sub-partition can be made thinner, so that the thickness of the first sub-partition is less than that of the second sub-partition, so as to facilitate the upward movement of the first sub-partition under the action of air pressure.

[0062] In the above embodiment, the first sub-partition needs to be moved to be completely offset from the second sub-partition before the opening and closing gap can be opened. In order to facilitate the opening and closing gap, the present invention also provides another embodiment of the opening and closing mechanism. In this embodiment, Fig. 9 and Fig.10 As shown, the opening and closing seam 301b has two opening and closing surfaces 200b arranged opposite to each other, and the two opening and closing surfaces are respectively arranged on the first sub-partition 31b and the second sub-partition 32b. When the first sub-partition 31b and the second sub-partition 32b are in contact, the two opening and closing surfaces 200b are in contact with each other; when the first sub-partition 31b and the second sub-partition 32b are separated, the two opening and closing surfaces 200b are separated.

[0063] The direction of relative movement of the two sub-partitions is the opening and closing direction, and the angle between the two opening and closing surfaces and the opening and closing direction is an acute angle, so that the opening and closing surfaces are neither parallel nor perpendicular to the opening and closing direction. When the two opening and closing surfaces move relatively for a small distance, the two can be separated, so that the first sub-partition 31b and the second sub-partition 32b do not need to be completely staggered to open the opening and closing seam 301. As in the aforementioned embodiment, the opening and closing direction is vertical, and the opening and closing surface 200b is inclined.

[0064] In the above embodiment, the first sub-partition is slidably arranged, the second sub-partition is fixedly arranged, and the driving device 52 drives the first sub-partition to move, which has a simple structure and is easy to process and prepare. Here, in other examples, the first sub-partition and the second sub-partition can be both slidably connected to the inner wall of the crucible. In the embodiment in which the driving rod cooperates with the cam, the part of the driving rod located in the crucible is provided with two cams. When the driving rod rotates around its own axis, one cam drives the first sub-partition to move upward, and the other cam drives the second sub-partition to move downward; in the embodiment in which the driving rod cooperates with the cylinder, the driving rod and the cylinder can be two groups, which respectively drive the two sub-partitions to move in opposite directions.

[0065] In the above embodiment, the first sub-partition is slidably arranged in the vertical direction. As another embodiment, the first sub-partition can also move in the horizontal direction, the horizontal direction is the opening and closing direction, the opening and closing seam can be trapezoidal wave-shaped, and the two waist edges of the trapezoidal wave are inclined, so that the angle between the opening and closing surface of the opening and closing seam and the horizontal direction is an acute angle, so that the first sub-partition can open the opening and closing seam by moving a small distance. In order to facilitate the sliding of the first sub-partition, the opening and closing mechanism also includes a third sub-partition, which is fixed to the crucible, and the end of the first sub-partition far from the seam is slidably connected to the third sub-partition. The third sub-partition can also be used to block the gap between the second sub-partition and the side wall of the crucible when the opening and closing seam is closed.

[0066] In summary, although the present invention has been disclosed as above in terms of preferred embodiments, the above preferred embodiments are not intended to limit the present invention. A person skilled in the art may make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention shall be based on the scope defined in the claims.

Claims

1. A growth device for growing silicon carbide material, characterized in that: It comprises a crucible, wherein the crucible comprises a crystal growth chamber, a gas buffer chamber and a silicon source supplement chamber which are arranged in sequence from top to bottom; A porous partition and an opening and closing mechanism are arranged in the crucible, wherein the porous partition is arranged between the crystal growth chamber and the gas buffer chamber, and the opening and closing mechanism is arranged between the gas buffer chamber and the silicon source replenishing chamber, and is used to control the connection and isolation between the gas buffer chamber and the silicon source replenishing chamber; The crucible is provided with a first heating component and a second heating component, the first heating component is provided corresponding to the growth chamber and the gas buffer chamber, and the second heating component is provided corresponding to the silicon source supplement chamber; the second heating component can heat and sublimate the silicon material in the silicon source supplement chamber; the first heating component can heat the sublimated silicon material in the gas buffer chamber to make it reach the same temperature as the crystal growth chamber, and then slowly release it into the crystal growth chamber through the porous partition; The volume ratio of the crystal growth chamber to the gas buffer chamber is 1.8:1-2.2:1, and the volume ratio of the gas buffer chamber to the silicon source replenishment chamber is 1.8:1-2.2:1; The first heating member surrounds the outer wall of the crucible; and the pore density of the peripheral area of ​​the porous partition is greater than the pore density of the central area thereof.

2. The growth device according to claim 1, characterized in that The second heating member is arranged around the outer wall of the crucible; or the thickness of the porous partition is 0.5-1.5 cm.

3. The growth device according to claim 1, characterized in that The opening and closing mechanism includes a silicon source partition, an opening and closing seam is arranged on the silicon source partition, and the opening and closing seam is a multiple bend shape arranged along the plate surface of the silicon source partition; the silicon source partition is divided into two sub-partitions by the opening and closing seam, at least one of the sub-partitions is movably connected to the crucible so that the two sub-partitions can abut and separate; when the two sub-partitions are abutted, the opening and closing seam is in a closed state, and the gas buffer chamber is isolated from the silicon source replenishing chamber; when the two sub-partitions are separated, the gas buffer chamber is connected to the silicon source replenishing chamber via the opening and closing seam.

4. The growth device according to claim 3, characterized in that The opening and closing seams are in a square wave shape, a sawtooth shape, a sine wave shape, or a trapezoidal wave shape.

5. The growth device according to claim 3, characterized in that The two sub-partitions are respectively a first sub-partition and a second sub-partition. The first sub-partition is slidably disposed on the crucible along the axial direction of the crucible, and the second sub-partition is fixed to the crucible.

6. The growth device according to claim 5, characterized in that The growth equipment also includes a driving rod, and a driving hole is provided on the crucible, wherein the driving hole connects the outer wall of the crucible with the silicon source replenishing chamber, and the driving rod passes through the driving hole, and one end of the driving rod is connected to the first sub-partition, and the other end is connected to a driving device; the driving device is arranged on the outside of the crucible, and is used to drive the driving rod to move, so that the driving rod drives the first sub-partition to move along the axial direction of the crucible.

7. The growth device according to claim 6, characterized in that The driving hole is arranged on the side wall of the crucible, the driving rod is connected to the driving hole by rotating around its own axis, a cam is fixed to one end of the driving rod, and the circumference of the cam abuts against the first sub-partition; the driving device is a motor to drive the driving rod to rotate around its own axis, so that the cam drives the first sub-partition to move in the vertical direction; or, The driving hole is arranged on the bottom wall of the crucible, the driving rod is slidably connected to the driving hole in a vertical direction, and the driving device is a cylinder to drive the driving rod to move in a vertical direction, thereby causing the first sub-partition plate to move in a vertical direction.

8. The growth device according to claim 3, characterized in that The opening and closing seam has two opening and closing surfaces arranged opposite to each other, and the two opening and closing surfaces are respectively arranged on the two sub-partitions; when the two sub-partitions are in contact, the two opening and closing surfaces are in contact with each other; when the two sub-partitions are separated, the two opening and closing surfaces are separated; The direction in which the two sub-partitions move relative to each other is an opening and closing direction, and the angle between the two opening and closing surfaces and the opening and closing direction is an acute angle.