A SERS detection method for furfural in transformer oil

By using SERS detection method in transformer oil, using the chemical reaction of nano-gold substrate and 4-aminothiophenylthiophenol, the problems of insufficient sensitivity and low efficiency of furfural detection in the prior art are solved, and high sensitivity and efficient furfural detection are achieved , suitable for field applications.

CN115684122BActive Publication Date: 2024-12-06ELECTRIC POWER RES INST OF GUANGXI POWER GRID CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211173941.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-09-26
Publication Date
2024-12-06
Estimated Expiration
2042-09-26

AI Technical Summary

Technical Problem

The prior art when detecting the furfural content in transformer oil, the sensitivity is insufficient, the detection efficiency is low, and it is not suitable for on-site analysis. In particular, traditional methods have problems such as difficulty in elution, complex operation, large errors or the use of toxic substances.

Method used

Using SERS-based detection method, the substrate is prepared by loading nano-gold on a glass substrate, combining the chemical reaction of 4-aminothiophenylsulfanol and concentrated hydrochloric acid, Raman spectroscopy detects the characteristic peaks of furfural, establish a calibration curve, and realizes the transformer Fast and accurate detection of furfural concentration in oil.

Benefits of technology

The detection sensitivity reaches 0.1mg/L, which is suitable for on-site inspection, with a detection range covering 0.1~100mg/L, avoiding large-scale fixed instruments in the laboratory, and using a portable Raman spectrometer, improving detection efficiency and safety.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure HDA0003864568090000011
    Figure HDA0003864568090000011
  • Figure HDA0003864568090000012
    Figure HDA0003864568090000012
  • Figure HDA0003864568090000013
    Figure HDA0003864568090000013
Patent Text Reader

Abstract

The present invention relates to the technical field of furfural detection and analysis in transformer oil, and specifically discloses a SERS detection method for furfural in transformer oil, comprising the following steps: (1) substrate preparation; (2) furfural standard oil sample preparation; (3) placing the substrate obtained in step (1) into a mixed solution of 4-aminothiophenol ethanol solution and concentrated hydrochloric acid for soaking treatment; (4) soaking the substrate obtained in step (3) in a furfural standard oil sample or an oil sample to be tested, and after constant temperature soaking for a period of time, using a Raman spectrometer to collect spectra; (5) establishing a calibration curve based on the Raman spectrum of the furfural standard oil sample, and obtaining the furfural concentration of the oil sample to be tested according to the Raman spectrum of the oil sample to be tested and the calibration curve. The SERS detection method for furfural in transformer oil of the present invention utilizes a highly specific chemical reaction to achieve extraction-free separation, and can realize on-site detection of furfural in transformer oil in combination with a portable Raman spectrometer, and the detection limit is better than 0.1 mg / L.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of furfural detection and analysis in transformer oil, and particularly relates to a SERS detection method for furfural in transformer oil. Background Art

[0002] As an accurate, non-destructive and efficient detection method, Raman spectroscopy has been widely used in many fields such as petrochemicals, environmental protection, food identification, and medicine. Due to the small Raman scattering cross section, the signal intensity is generally only 10 times the incident light intensity. -10 , which restricted the application and development of Raman spectroscopy in the field of trace detection for a long time. The discovery of the surface enhanced Raman scattering (SERS) effect effectively solved the problem of low sensitivity of Raman spectroscopy in surface science and trace analysis. At present, SERS has developed into a powerful and effective analytical tool, which is widely used in the monitoring of heterogeneous catalytic reactions, the detection of drugs, explosives, environmental pollutants, food / water toxic substances, cancer markers, etc., as well as single cell, animal, plant in vivo imaging and many other fields. It also has certain applications in the power industry, especially in oil quality analysis.

[0003] In the power industry, after long-term operation of oil-immersed transformers, the internal paper insulation material will gradually age and its insulation level will decrease. Furfural is one of the main characteristic products generated during the degradation of transformer paper insulation materials. Its content is related to the degree of polymerization of paper insulation materials, so it can effectively reflect the aging state of transformer insulation materials. my country's power industry standard DL / T 984-2018 "Guidelines for Determining Insulation Aging of Oil-Immersed Transformers" also lists furfural content as an important criterion for the aging state of paper insulation. The power industry standard DL / T 596-2021 "Preventive Test Procedures for Power Equipment" points out that when the furfural content in transformer oil reaches 4 mg / L, the aging of paper insulation is already serious; in addition, for oil-immersed transformers with an operating life of 1 to 5 years, 5 to 10 years, 10 to 15 years, and 15 to 20 years, if the furfural content in the oil exceeds 0.1 mg / L, 0.2 mg / L, 0.4 mg / L, and 0.75 mg / L, respectively, the paper insulation has abnormal aging. Therefore, rapid and accurate detection of furfural content in transformer oil is of great significance for timely understanding the insulation health status of transformers and improving the safety production level of power grid enterprises.

[0004] Traditionally, there are several methods for detecting furfural in transformer oil: liquid chromatography, spectrophotometry and colorimetry. Among them, liquid chromatography has high detection accuracy and good repeatability, and is the method recommended by my country's power industry standard DL / T 1355-2014. However, it also has limitations such as difficult elution, complex and time-consuming operation, and "extra-column effect". It is only suitable for precise laboratory analysis, not for rapid on-site analysis; spectrophotometry has fast testing speed and easy miniaturization of instruments, which is suitable for on-site analysis, but is easily interfered by other organic matter in transformer oil and has low stability; colorimetry is convenient and inexpensive, but has large errors and cannot be used as a basis for quantitative measurement, and the aniline or 4-aminotoluene used are toxic substances.

[0005] In recent years, some scholars at home and abroad have tried to use Raman spectroscopy to detect furfural in transformer oil and have achieved preliminary results. However, there are still deficiencies in detection sensitivity, speed or feasibility of on-site analysis. In 2015, Japanese scholar T. Somekawa first proposed a laboratory method for directly determining the concentration of furfural in transformer oil by laser Raman spectroscopy without extraction and enrichment, with a detection limit of about 14.4 mg / L. Chen Weigeng and other scholars from Chongqing University used methanol for rapid extraction and enrichment and then used a laboratory research-level Raman spectroscopy platform for furfural detection. The estimated detection limit was 0.10 mg / L. Qiao Shengya and other researchers from the Guangzhou Power Supply Bureau of the Southern Grid used similar methods and platforms to compare the effects of methanol and deionized water as extraction agents, and reported a detection limit of 1~3 mg / L. Based on various SER The direct detection technology of furfural in transformer oil based on S substrate or improved data processing algorithm is also developing rapidly. For example, Patent 201910322173.8 uses a gold-based silver ball surface enhancement material to detect the minimum concentration of furfural in transformer oil at 1.06 mg / L, but a laboratory research-level confocal Raman spectroscopy detection platform is required; Patent 201710412021.8 discloses a method for measuring furfural in transformer oil based on a silver-based sponge substrate, but the detection limit is unknown, and the silver-based sponge substrate needs to be immersed in the oil sample for dozens of hours before measurement. At present, there is still a lack of a method for detecting furfural in transformer oil that takes into account detection sensitivity (the detection limit is at least 0.1 mg / L), accuracy, and detection efficiency, and is suitable for on-site detection. Summary of the invention

[0006] The purpose of the present invention is to provide a SERS detection method for furfural in transformer oil to overcome the defects of the prior art.

[0007] To achieve the above object, the present invention provides a SERS detection method for furfural in transformer oil, comprising the following steps:

[0008] (1) Substrate preparation: The substrate is prepared by loading nano-gold on a glass substrate;

[0009] (2) Preparation of furfural standard oil sample;

[0010] (3) placing the substrate obtained in step (1) into a mixed solution of 4-aminothiophenol ethanol solution and concentrated hydrochloric acid for immersion treatment, taking out, washing, and drying;

[0011] (4) soaking the substrate obtained in step (3) in a furfural standard oil sample or an oil sample to be tested, taking it out after soaking it at a constant temperature for a period of time, and collecting spectra using a Raman spectrometer;

[0012] (5) A calibration curve is established based on the Raman spectrum of the furfural standard oil sample, and the furfural concentration of the oil sample to be tested is obtained according to the Raman spectrum of the oil sample to be tested and the calibration curve.

[0013] Preferably, in the above-mentioned SERS detection method for furfural in transformer oil, in step (1), the preparation of the substrate comprises the following steps:

[0014] S1. Process 4 to 8 hemispherical microcavities with a diameter of 1 to 1.5 mm on the upper surface of a quartz glass substrate, with an interval of 2 to 3 mm between adjacent microcavities;

[0015] S2. The processed substrate was washed with aqua regia, alkali solution, and deionized water, dried, and then soaked in an aqueous solution of 3-aminopropyltrimethoxysilane for 15 to 30 minutes, washed with water, and dried;

[0016] S3. The substrate obtained in step S2 is immersed in an aqueous solution of gold nanoparticles having a diameter of 5 to 10 nm for 8 to 12 h, taken out, washed with water, and dried;

[0017] S4. The substrate obtained in step S3 is immersed in a mixed aqueous solution of chloroauric acid and hydroxylamine hydrochloride, wherein the concentration of chloroauric acid in the mixed aqueous solution is 0.5-1.5 mmol / L, and the concentration of hydroxylamine hydrochloride is 2-3 mmol / L; the substrate is oscillated at a rotation speed of 1000-1500 rpm for 10-20 min to complete the first growth cycle, and then washed and dried;

[0018] S5. The substrate obtained in step S4 is immersed in a mixed aqueous solution of chloroauric acid and hydroxylamine hydrochloride, wherein the concentration of chloroauric acid in the mixed aqueous solution is 0.1 to 0.5 mmol / L, and the concentration of hydroxylamine hydrochloride is 0.5 to 1 mmol / L; the mixture is oscillated at an oscillation speed of 1000 to 1500 rpm for 10 to 20 min to complete the second growth cycle;

[0019] S6. Continue to carry out 2 growth cycles according to the parameters and conditions of the second growth cycle, and complete 4 growth cycles in total, wash and dry; then soak in a potassium iodide aqueous solution with a concentration of 0.5~2mmol / L for 15~30min to remove impurities on the surface of the substrate to make the detection background signal cleaner; wash and dry to obtain the substrate.

[0020] For the substrate used for detection, a hemispherical microcavity array is first processed on a quartz glass substrate. On the one hand, it can increase the contact area between the sample to be tested and the surface of the device, so that the sample to be tested is enriched inside the cavity, which can enhance the enhancement effect. On the other hand, the microcavity structure is convenient for fixing the detection area and ensuring the repeatability of focusing, thereby improving the repeatability and reliability of the detection results. However, it is difficult for a planar substrate to find the same area for detection every time, which is not conducive to ensuring the repeatability of the detection results. The substrate is treated with 3-aminopropyltrimethoxysilane to ensure that an appropriate amount of nanogold seeds are tightly adsorbed on the surface of the substrate material. Then, the gold nanoparticles are immersed in an aqueous solution and grown in a mixed aqueous solution of chloroauric acid and hydroxylamine hydrochloride, and the parameters such as the immersion time and solution concentration are optimized. Finally, a single-layer nanogold film with uniform morphology and small gaps between nanoparticles is obtained, which is conducive to improving subsequent detection effects.

[0021] Preferably, in the above-mentioned SERS detection method for furfural in transformer oil, in the step (2), the furfural standard oil sample is prepared as follows: 1 mg of furfural standard is added to 10 mL of blank transformer oil without furfural, and ultrasonicated for 30 minutes to fully dissolve the furfural to prepare a 100 mg / L mother liquor; and then diluted with blank transformer oil in sequence to obtain 5 different concentrations of furfural standard oil samples of 100 mg / L, 10 mg / L, 5 mg / L, 1 mg / L, and 0.1 mg / L.

[0022] Preferably, in the above-mentioned SERS detection method for furfural in transformer oil, in the step (3), the concentration of the 4-aminothiophenol ethanol solution is 0.5-1.5 mmol / L, and the volume ratio of the 4-aminothiophenol solution to concentrated hydrochloric acid is 1:0.02-0.06.

[0023] Preferably, in the above-mentioned SERS detection method for furfural in transformer oil, in the step (4), the constant temperature is 40-60° C., and the immersion time is 15-120 min.

[0024] Preferably, in the above-mentioned SERS detection method for furfural in transformer oil, in the step (4), the constant temperature is 50° C. and the immersion time is 30 min.

[0025] Preferably, in the above-mentioned SERS detection method for furfural in transformer oil, in the step (4), the excitation light of the Raman spectrometer is focused to the center position of the bottom of the microcavity of the substrate to collect the spectrum.

[0026] Preferably, in the above-mentioned SERS detection method for furfural in transformer oil, the excitation light wavelength of the Raman spectrometer is 785 nm, the excitation light wavelength of the Raman spectrometer is 785 nm, the laser power is 150 mW, the integration time is 10 s, the number of integrations is 1, and the Raman spectrum detection range is 200-1800 cm -1 .

[0027] Preferably, in the above-mentioned SERS detection method for furfural in transformer oil, in step (5), the characteristic peak of furfural in the Raman spectrum is 1658 cm -1 Furfural reacts with 4-aminothiophenol to form a condensation reaction at 1658 cm -1 New characteristic peaks are generated.

[0028] Preferably, in the above-mentioned SERS detection method for furfural in transformer oil, in step (5), the Raman spectrum of the furfural standard oil sample is 1658 cm -1 With 1080cm -1 The ratio of the characteristic peak intensity at 1658 / I 1080 The average value of is taken as the ordinate and the logarithm of the furfural concentration in the standard oil sample is taken as the abscissa. A linear model is selected and a calibration curve is established using the least squares method.

[0029] Preferably, in the above-mentioned SERS detection method for furfural in transformer oil, the Raman spectrum of the oil sample to be tested is calculated at 1658 cm -1 With 1080cm -1 The ratio of the characteristic peak intensity at 1658 / I 1080 The furfural concentration in the oil sample to be tested is calculated based on the calibration curve.

[0030] Compared with the existing technology, the present invention has the following beneficial effects:

[0031] 1. The SERS detection method of furfural in transformer oil of the present invention has an excitation light wavelength of 785 nm, which is a common excitation light wavelength of commercial portable Raman spectrometers, and is convenient for miniaturization of the test instrument. Compared with the standard detection method of furfural in transformer oil recommended by the power industry standard DL / T 1355-2014 and the detection method of furfural in transformer oil based on laboratory research-level Raman spectrometer, the present invention can select a commercial portable Raman spectrometer, thereby avoiding the use of large laboratory fixed instruments, and is convenient for on-site detection.

[0032] 2. The SERS detection method for furfural in transformer oil of the present invention has a detection limit of furfural in transformer oil that is better than 0.1 mg / L, high detection sensitivity, and a detection range that can cover at least 0.1~100 mg / L, which can meet the requirements for the detection range of furfural concentration in power industry standards such as DL / T 596-2021 "Preventive Test Procedure for Power Equipment".

[0033] 3. The SERS detection method of furfural in transformer oil of the present invention is based on the highly specific chemical reaction of 4-aminothiophenol and furfural to achieve extraction-free separation. The selected Raman characteristic peak is unique to furfural, which is highly selective to furfural and has strong anti-interference. In view of the problems that transformer oil has high viscosity at room temperature and it takes a long time for the target molecules to diffuse to the vicinity of the hot spot, the diffusion rate and capture efficiency of the target molecules are accelerated by constant temperature heating, which greatly shortens the time required for the substrate to be immersed in the oil sample before detection, and improves the detection efficiency.

[0034] 4. The SERS detection method for furfural in transformer oil of the present invention uses a nano-gold substrate, which is more stable than the existing disclosed SERS-based detection method for furfural in transformer oil which mainly uses a silver-based substrate or a gold-silver composite substrate. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] Figure 1 This is a SEM electron microscope image of the substrate prepared in Example 1 of the present invention.

[0036] Figure 2 It is a schematic diagram of the furfural detection principle in the present invention.

[0037] Figure 3 The Raman spectrum and calibration curve of the furfural standard oil sample in Example 1 of the present invention are shown.

[0038] Figure 4 The Raman spectra of Examples 1 to 3 of the present invention and 1658 / I 1080 Value comparison chart.

[0039] Figure 5 The Raman spectra obtained in Example 1 and Comparative Example 1 of the present invention are shown in FIG. 1658 / I 1080 Value comparison chart.

[0040] Figure 6 This is a comparison chart of the test results of seven different aldehydes in Test Example 1 of the present invention.

[0041] Figure 7 This is a stability test diagram of the SERS substrate in Experimental Example 2 of the present invention.

[0042] Figure 8The Raman spectra under different reaction conditions in Comparative Example 2 of the present invention are shown.

[0043] Fig. 9 These are SEM images of substrates prepared at different immersion times in Comparative Example 3 of the present invention. DETAILED DESCRIPTION

[0044] The specific embodiments of the present invention are described in detail below, but it should be understood that the protection scope of the present invention is not limited by the specific embodiments.

[0045] Example 1

[0046] A SERS detection method for furfural in transformer oil comprises the following steps:

[0047] (1) Substrate preparation:

[0048] S1. Six hemispherical microcavities with a diameter of 1 mm were processed on a quartz glass sheet with a size of 10×20×3 mm, and the interval between adjacent microcavities was 2.5 mm;

[0049] S2. The processed quartz glass sheet was washed with aqua regia, saturated ethanol solution of sodium hydroxide, and deionized water, dried with nitrogen, and then vertically immersed in a 0.1% mass percentage concentration of 3-aminopropyltrimethoxysilane aqueous solution for 20 min, removed and washed with deionized water and dried with nitrogen;

[0050] S3. The quartz glass sheet obtained in step S2 was immersed in an aqueous solution of gold nanoparticles having a diameter of 5 nm for 10 h, removed, washed with water, and dried;

[0051] S4. Place the quartz glass sheet obtained in step S3 vertically into an empty EP tube with a volume of 5 mL, add 2.4 mL of a mixed aqueous solution of chloroauric acid and hydroxylamine hydrochloride, wherein the concentration of chloroauric acid in the mixed aqueous solution is 0.625 mmol / L, and the concentration of hydroxylamine hydrochloride is 2.5 mmol / L, and the mixed aqueous solution of chloroauric acid and hydroxylamine hydrochloride is prepared and used immediately; immediately place the EP tube in a constant temperature mixer, oscillate at an oscillation speed of 1500 rpm for 15 min, take it out, wash it with deionized water, and blow it dry with nitrogen to complete the first growth cycle;

[0052] S5. Place the quartz glass sheet obtained in step S4 vertically into a 5 mL EP tube, add 2.12 mL of a mixed aqueous solution of chloroauric acid and hydroxylamine hydrochloride, wherein the concentration of chloroauric acid in the mixed aqueous solution is 0.17 mmol / L, and the concentration of hydroxylamine hydrochloride is 0.71 mmol / L; immediately place the EP tube in a constant temperature mixer and oscillate at 1500 rpm for 15 min to complete the second growth cycle;

[0053] S6. Continue to perform 2 growth cycles according to the parameters and conditions of the second growth cycle, and complete 4 growth cycles in total. Take out, wash with deionized water, and blow dry with nitrogen. Then soak in a potassium iodide aqueous solution with a concentration of 1mmol / L for 20min, take out, wash with deionized water, and blow dry with nitrogen to obtain a substrate. The SEM electron microscope image of the prepared SERS substrate is shown in Figure 1 As shown;

[0054] (2) Preparation of furfural standard oil samples: add 1 mg of furfural standard to 10 mL of blank transformer oil without furfural, and ultrasonicate for 30 min to fully dissolve the furfural to prepare a 100 mg / L mother liquor; then dilute with blank transformer oil to obtain 5 different concentrations of furfural standard oil samples: 100 mg / L, 10 mg / L, 5 mg / L, 1 mg / L, and 0.1 mg / L;

[0055] (3) The substrate prepared in step (1) was placed vertically in an empty EP tube with a volume of 5 mL, and 2 mL of 1 mmol / L 4-aminobenzenethiol solution and 40 μL of concentrated hydrochloric acid were added in sequence. After standing in the dark for 15 min, the substrate was taken out and blown dry with nitrogen. The substrate was then placed vertically in an empty EP tube with a volume of 5 mL, and 2 mL of furfural standard oil sample or oil sample to be tested was added. The substrate was soaked at a constant temperature of 50°C for 0.5 h and then taken out. The excitation light of the Raman spectrometer was focused to the center of the bottom of the microcavity of the substrate for spectrum acquisition. The wavelength of the excitation light was 785 nm, the laser power was 150 mW, the integration time was 10 s, the number of integrations was 1, and the Raman spectrum detection range was 200~1800 cm -1 ;

[0056] (4) Figure 2 Schematic diagram of the furfural detection principle. Based on the Schiff base reaction, furfural and p-aminothiophenol undergo condensation reaction to form a new molecule containing an imine group (-RC=N-). The Raman band of the carbon-nitrogen double bond is at 1658 cm -1 A new characteristic peak is formed at 1658 cm -1 With 1080cm -1 The ratio of the characteristic peak intensity at 1658 / I 1080 The average value is taken as the ordinate y (in percentage %), and the logarithm of the furfural concentration in the standard oil sample is taken as the abscissa x. A linear model is selected and a calibration curve is established using the least squares method. The calibration curve equation is y=4.42x+10.26, and the determination coefficient is R 2 =0.9862. Figure 3 The Raman spectrum and calibration curve of furfural standard oil sample;

[0057] (5) Calculate the Raman spectrum of the oil sample to be tested at 1658 cm -1 With 1080cm-1 The ratio of the characteristic peak intensity at 1658 / I 1080 The furfural concentration in the oil sample to be tested is calculated based on the calibration curve.

[0058] Raman spectrum of the oil sample to be tested is 1658cm -1 With 1080cm -1 The ratio of the characteristic peak intensity at 1658 / I 1080 The average value of is 8.61, the furfural concentration in the oil sample to be tested is calculated to be 0.42 mg / L according to the calibration curve, and the furfural concentration in the oil sample to be tested is measured by liquid chromatography according to the power industry standard DL / T1355-2014 to be 0.38 mg / L, with a relative deviation of 10.5%, which is within the allowable range. The SERS detection method for furfural in transformer oil of the present invention has high detection efficiency and good stability, can meet the requirements of the power industry standard for the detection range of furfural concentration, and has the advantage of being able to be used for on-site detection compared with liquid chromatography.

[0059] Example 2

[0060] The difference between this embodiment and embodiment 1 is that the constant temperature immersion temperature in step (3) is 40° C., and the other detection steps and parameters are the same as those in embodiment 1.

[0061] Example 3

[0062] The difference between this embodiment and embodiment 1 is that the constant temperature immersion temperature in step (3) is 60° C., and the other detection steps and parameters are the same as those in embodiment 1.

[0063] The oil sample containing 100 mg / L furfural was detected by the detection methods of Example 1, Example 2 and Example 3 respectively. The Raman spectra and I 1658 / I 1080 like Figure 4 As shown. Figure 4 It can be seen that with the increase of reaction temperature, the -1 The relative intensity at 1658cm increases first and then decreases. This is because within a certain temperature range, the increase in temperature is conducive to the reaction. However, when the temperature is too high, the 4-aminothiophenol molecules stimulate the "thermal" hole effect on the gold surface, and part of the 4-aminothiophenol molecules are converted into dithioazobenzene (DMAB), resulting in the 1658cm -1 Therefore, among the above temperatures, 50℃ is the best soaking temperature.

[0064] Comparative Example 1

[0065] The SERS detection method of furfural in transformer oil of this comparative example is different from that of Example 1 in that in step (3), anhydrous ethanol is used instead of 1 mmol / L 4-aminothiophenol solution to immerse the SERS substrate, and the other detection steps and parameters are the same as those of Example 1.

[0066] The detection method of Example 1 was used to detect the blank oil sample without furfural and the oil sample containing 100 mg / L furfural. The Raman spectra were as follows: Figure 5 (A) and 5 (B); the detection method of Comparative Example 1 was used to detect an oil sample containing 100 mg / L furfural, and the Raman spectrum was as follows Figure 5 (C) shown.

[0067] Depend on Figure 5 It can be seen that in the absence of furfural, at 1143 cm -1 The azo peak is formed at 1658 cm -1 In the presence of furfural, compared with the SERS substrate treated with anhydrous ethanol, the substrate treated with 4-aminothiophenol molecules has a peak at 1658 cm -1 A new peak appears at the position of the carbon-nitrogen double bond, which is attributed to the carbon-nitrogen double bond. This proves that the peak of the carbon-nitrogen double bond generated by the Schiff base reaction between 4-aminothiophenol and furfural can be used as a characteristic peak for detecting furfural.

[0068] Test Example 1

[0069] In order to explore the effect of different aldehydes on furfural detection, 100 mg / L transformer oil solutions of furfural, glyoxal, acetone aldehyde, glutaraldehyde, formaldehyde, acetaldehyde and benzaldehyde were prepared. After being treated under the same conditions as furfural detection, SERS detection was performed. The results are as follows: Figure 6 As shown, in addition to furfural appearing at 1658 cm -1 The characteristic peaks of furfural were not found in the SERS detection method of the present invention, and the other aldehydes did not appear. This shows that the SERS detection method of the present invention has good selectivity for furfural.

[0070] Test Example 2

[0071] In order to test the stability of the substrate prepared in step (1) of Example 1, the newly prepared substrate was placed in a 5×10 -6 mol / L 4-mercaptobenzoic acid ethanol solution for 50 minutes, take it out and rinse it with deionized water, blow it dry with nitrogen, and focus the excitation light of the Raman spectrometer to the center of the bottom of the microcavity of the substrate to collect the spectrum. After the device is fully cleaned with anhydrous ethanol, it is sealed and stored in a light-proof place for one month, and the above immersion and test are repeated. The intensity of the characteristic peak of the Raman spectrum of 4-mercaptobenzoic acid can still maintain 92.4% of the original. Figure 7 As shown, it is proved that the prepared SERS substrate has good stability in air.

[0072] Comparative Example 2

[0073] The SERS detection method of furfural in transformer oil in this comparative example is different from that in Example 1 in that: in step (3), a saturated ethanol solution of sodium hydroxide or anhydrous ethanol is used to replace concentrated hydrochloric acid, and the other steps and conditions are the same as those in Example 1. The collected Raman spectrum is as follows: Figure 8 As shown. Figure 8 It can be seen that under the reaction conditions of adding sodium hydroxide to a saturated ethanol solution (alkaline), at 1143 cm -1 A strong azo peak will appear at 1658cm -1 No new characteristic peak was generated at 1143cm -1 A weaker azo peak will appear at 1658cm -1 No new characteristic peak was generated at 1658cm -1 A new characteristic peak is generated at 1143cm -1 No azo peak is observed. This is because under neutral and alkaline conditions, the oxides or hydroxides on the surface of gold nanoparticles can exist stably, which is conducive to the oxidation of the amino group (-NH2) of the 4-aminothiophenol molecule to form an azo group (-N=N-), inhibiting the condensation reaction of furfural and 4-aminothiophenol; while under acidic conditions, the amino group is protonated and cannot be oxidized to form an azo group, which is conducive to the condensation reaction of furfural and 4-aminothiophenol.

[0074] Comparative Example 3

[0075] The SERS detection method of furfural in transformer oil in this comparative example is different from that in Example 1 in that: the immersion time in step (1) of the substrate preparation step S3 is 5 h and 24 h, and the other steps and conditions are the same as those in Example 1. The SEM image of the substrate finally obtained is as follows: Fig. 9 As shown. Fig. 9 (a) It can be seen that the immersion time is too short (5h), and the gaps between the final substrate nanoparticles are large and not dense enough. The substrate with this morphology has a poor enhancement effect due to the insufficient number of "hot spots". Fig. 9 (c) It can be seen that the gold film on the surface of the substrate obtained after the immersion time is too long (24h) is stacked to form a multi-layer structure. Although the multi-layer gold film can also produce an enhancement effect, its morphology is uncontrollable, resulting in an uncontrollable enhancement effect, making it difficult to use for quantitative analysis; Fig. 9 (b) It can be seen that the immersion time optimized by the present application can achieve the maximum density of gold adsorption in a single layer, and what is finally obtained is a single-layer nano-gold film with uniform morphology and high-density small nanogaps. This type of SERS substrate has more "hot spots" and can produce a more ideal enhancement effect.

[0076] The foregoing description of specific exemplary embodiments of the present invention is for the purpose of illustration and demonstration. These descriptions are not intended to limit the present invention to the precise form disclosed, and it is clear that many changes and variations can be made based on the above teachings. The purpose of selecting and describing the exemplary embodiments is to explain the specific principles of the present invention and its practical application, so that those skilled in the art can realize and utilize various different exemplary embodiments of the present invention and various different selections and changes. The scope of the present invention is intended to be limited by the claims and their equivalents.

Claims

1. A SERS detection method for furfural in transformer oil, characterized in that: The following steps are involved: (1) Substrate preparation: The substrate is prepared by loading nano-gold on a glass substrate; (2) Preparation of furfural standard oil sample; (3) placing the substrate obtained in step (1) into a mixed solution of 4-aminothiophenol ethanol solution and concentrated hydrochloric acid for immersion treatment, taking out, washing, and drying; (4) soaking the substrate obtained in step (3) in a furfural standard oil sample or an oil sample to be tested, soaking for a period of time at a constant temperature, taking it out, and collecting spectra using a Raman spectrometer; (5) establishing a calibration curve based on the Raman spectrum of the furfural standard oil sample, and obtaining the furfural concentration of the oil sample to be tested according to the Raman spectrum of the oil sample to be tested and the calibration curve; In the step (1), the preparation of the substrate comprises the following steps: S1. Process 4 to 8 hemispherical microcavities with a diameter of 1 to 1.5 mm on an inorganic material substrate, with an interval of 2 to 3 mm between adjacent microcavities; S2. The processed substrate was washed with aqua regia, alkali solution, and deionized water, dried, and then immersed in an aqueous solution of 3-aminopropyltrimethoxysilane for 15 to 30 minutes, washed with water, and dried; S3. Soak the substrate obtained in step S2 in an aqueous solution of gold nanoparticles having a diameter of 5 to 10 nm for 8 to 12 hours, remove it, wash it with water, and dry it; S4. The substrate obtained in step S3 is immersed in a mixed aqueous solution of chloroauric acid and hydroxylamine hydrochloride, wherein the concentration of chloroauric acid in the mixed aqueous solution is 0.5 to 1.5 mmol / L, and the concentration of hydroxylamine hydrochloride is 2 to 3 mmol / L; oscillate at an oscillation speed of 1000 to 1500 rpm for 10 to 20 minutes to complete the first growth cycle, wash, and dry; S5. The substrate obtained in step S4 is immersed in a mixed aqueous solution of chloroauric acid and hydroxylamine hydrochloride, wherein the concentration of chloroauric acid in the mixed aqueous solution is 0.1 to 0.5 mmol / L, and the concentration of hydroxylamine hydrochloride is 0.5 to 1 mmol / L; the mixture is oscillated at an oscillation speed of 1000 to 1500 rpm for 10 to 20 minutes to complete the second growth cycle; S6. Continue to carry out two growth cycles according to the parameters and conditions of the second growth cycle, complete a total of four growth cycles, wash and dry; then soak in a potassium iodide aqueous solution with a concentration of 0.5 to 2 mmol / L for 15 to 30 minutes, wash and dry.

2. The SERS detection method for furfural in transformer oil according to claim 1, characterized in that, In the step (2), the furfural standard oil sample is prepared as follows: 1 mg of furfural standard is added to 10 mL of blank transformer oil without furfural, and ultrasonicated for 30 minutes to fully dissolve the furfural to prepare a 100 mg / L mother liquor; and then the mother liquor is diluted with blank transformer oil in sequence to obtain 5 different concentrations of furfural standard oil samples, namely 100 mg / L, 10 mg / L, 5 mg / L, 1 mg / L, and 0.1 mg / L.

3. The SERS detection method of furfural in transformer oil according to claim 1, characterized in that, In the step (3), the concentration of the 4-aminothiophenol ethanol solution is 0.5-1.5 mmol / L, and the volume ratio of the 4-aminothiophenol solution to concentrated hydrochloric acid is 1:0.02-0.

06.

4. The SERS detection method for furfural in transformer oil according to claim 1, characterized in that, In the step (4), the constant temperature is 40 to 60° C., and the soaking time is 15 to 120 minutes.

5. The SERS detection method of furfural in transformer oil according to claim 1, characterized in that, In the step (4), the excitation light of the Raman spectrometer is focused to the center position of the bottom of the microcavity of the substrate to collect the spectrum.

6. The SERS detection method for furfural in transformer oil according to claim 1, characterized in that, The excitation wavelength of the Raman spectrometer is 785 nm, the laser power is 150 mW, the integration time is 10 s, the number of integrations is 1, and the Raman spectrum detection range is 200-1800 cm -1 .

7. The SERS detection method for furfural in transformer oil according to claim 1, characterized in that: In the step (5), the characteristic peak of furfural in the Raman spectrum is 1658 cm -1 .

8. The SERS detection method for furfural in transformer oil according to claim 7, characterized in that, In the step (5), the Raman spectrum of the furfural standard oil sample is 1658 cm -1 With 1080cm -1 The ratio of the characteristic peak intensity at I 1658 / I 1080 The average value of is taken as the ordinate and the logarithm of the furfural concentration in the standard oil sample is taken as the abscissa. A linear model is selected and a calibration curve is established using the least squares method.

9. The SERS detection method for furfural in transformer oil according to claim 8, characterized in that, Calculate the Raman spectrum of the oil sample to be tested at 1658cm -1 With 1080cm -1 The ratio of the characteristic peak intensity at I 1658 / I 1080 The furfural concentration in the oil sample to be tested is calculated based on the calibration curve.