A thermophotovoltaic system based on multilayer film selective emitter and its preparation method
By depositing multi-layer films on the surface of the thermal emitter of the thermal photovoltaic system, the emission spectrum is regulated to match the response band of the photovoltaic cell, the problem of mismatch between the photovoltaic cell and the emitter emission spectrum is solved, and the thermoelectric conversion efficiency and thermal energy utilization of the system are improved. Rate.
Patent Information
- Application Number
- CN202211408168.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-10
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-11-10
AI Technical Summary
The mismatch between the band gap of the photovoltaic cell in the thermal photovoltaic system and the emitter emission spectrum leads to low thermoelectric conversion efficiency, mainly due to the insufficient matching of the spectrum of the heat emitter and the band gap width of the photovoltaic cell, resulting in heat loss and low system efficiency.
Using a multilayer film selective emitter design, by depositing a multilayer film composed of alternating metal layer and dielectric layer on the surface of the heat emitter, the emission spectrum is regulated to match the response band of the photovoltaic cell, increasing the emissivity and reducing heat loss.
It achieves high emissivity (can reach more than 0.85) and high energy conversion efficiency, improves the system's utilization rate of heat energy, and maintains the compactness and applicability of the system, making it suitable for industrial production.
Smart Images

Figure CN115692532B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of thermal photovoltaic power generation. Background Art
[0002] Thermophotovoltaic technology uses narrow-bandgap photovoltaic cells to convert infrared radiation from high-temperature heat sources into electrical energy, with a high theoretical conversion efficiency. In a thermophotovoltaic system, when heat is supplied to the thermal emitter, the thermal emitter drives the radiation emission to the cold-side photovoltaic cell, and the high-energy (in-band) photon absorption in the photovoltaic cell unit excites electron-hole pairs, while the low-energy (out-of-band) thermal radiation can be suppressed or reflected to minimize heat input, and finally separate the photoexcited carriers, induce voltage on the PN junction, and drive the current on the load. Compared with traditional photovoltaic technology, thermophotovoltaic technology has great application value in deep space and deep sea exploration due to its good ability to adapt to various heat sources, portability, low maintenance, noiseless operation and high power density, without being restricted by solar energy stability, various geographical factors and its volume, and can be used in extreme environments.
[0003] Thermophotovoltaic technology has been studied since the late 1950s, but has not yet been widely commercialized. The main obstacle to the commercialization of the system is the low system efficiency, mainly due to the poor matching of the spectrum of the thermal emitter with the bandgap width of the photovoltaic cell. Thermophotovoltaic systems operate in a narrow parameter range, which is reflected in the fact that the thermal emitter must be hot enough (>800℃) so that a large amount of the emitted power is in the bandgap of the photovoltaic cell. However, when the bandgap energy of the photovoltaic cell is reduced to below 0.6eV, its internal quantum efficiency decreases significantly. Even at the most favorable extreme of these limits, according to the Wien displacement law, the peak of the 1000℃ black body is 2.27μm, which is lower than the 2.06μm bandgap wavelength of the 0.6eV photovoltaic cell, and only 20% of the photons are emitted in the bandgap. If the emission temperature is increased, the blackbody spectrum is better aligned with the photovoltaic cell, but only certain materials with ideal optical properties have a high enough melting point to meet the requirements of use, and even then, their optical properties when hot are different from those at room temperature. If high-quality low-bandgap photovoltaic materials are used, the system cost increases significantly, making it difficult to put into practical application. Summary of the invention
[0004] The present invention aims to solve the problem of heat loss caused by mismatch between absorption band gap and emission spectrum of existing photovoltaic cells, and further provide a thermophotovoltaic system based on multilayer film selective emitter and a preparation method thereof.
[0005] A thermophotovoltaic system based on a multilayer film selective emitter, comprising a heat source, a heat emitter, a heat conductive steel and a photovoltaic cell, wherein the heat conductive steel is located between the heat source and the heat emitter;
[0006] The thermal emitter is composed of a metal substrate and a multi-layer film, and the multi-layer film is located on the surface of the metal substrate;
[0007] The multilayer film is composed of alternating metal layers and dielectric layers, wherein the metal layer in contact with the metal substrate has a thickness of 50nm to 150nm, the thickness of the other metal layers is 5nm to 10nm, and the thickness of each dielectric layer is 30nm to 200nm.
[0008] A method for preparing a thermophotovoltaic system based on a multilayer film selective emitter is carried out in the following steps:
[0009] A multilayer film is deposited on the surface of a metal substrate to obtain a heat emitter, which is fixed on the outer surface of a heat-conducting steel, and finally a heat source is fixed inside the hollow of the heat-conducting steel; the multilayer film is composed of alternating metal layers and dielectric layers, wherein the metal layer in contact with the metal substrate has a thickness of 50nm to 150nm, the thickness of the remaining metal layers is 5nm to 10nm, and the thickness of each dielectric layer is 30nm to 200nm.
[0010] The beneficial effects of the present invention are:
[0011] In order to solve the defect of low thermoelectric conversion efficiency caused by the mismatch between the band gap of photovoltaic cells and the emission spectrum of emitters in traditional thermophotovoltaic systems, the present invention achieves selective regulation of the emission spectrum by depositing multiple layers of films on the surface of the emitter and superimposing the optical properties of different thin film materials. By adjusting the number of layers and the thickness of each layer, high emission is achieved in the response band of the corresponding photovoltaic cell, especially its optimal response band. The emissivity can reach above 0.85 in the optimal response band, so that the emission spectrum of the thermal emitter is matched with the band gap of the photovoltaic cell as much as possible, reducing heat loss and further increasing the temperature of the heat source, thereby improving the energy conversion efficiency of the thermophotovoltaic system and improving the system's utilization of thermal energy.
[0012] Compared with other methods of improving system efficiency, the present invention does not need to add other components, and only needs to deposit a multilayer film on the surface of the thermal emitter, thereby ensuring the compactness of the overall system. In addition, there are many ways to deposit a multilayer film with spectral selectivity on the surface of the thermal emitter, which are universal and can be prepared on a large area, suitable for industrial applications. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 A cross-sectional view of a thermophotovoltaic system based on a multilayer film selective emitter according to the present invention;
[0014] Figure 2 A top view of a thermophotovoltaic component in a thermophotovoltaic system based on a multilayer film selective emitter according to the present invention;
[0015] Figure 3 is an absorptivity curve diagram of the heat emitter in Example 1;
[0016] Figure 4 Schematic diagram of the thickness of the first layer, the second layer, the fourth layer and the sixth layer in the multi-layer thin film on the surface of the heat emitter in Example 1;
[0017] Figure 5 Schematic diagram of the thickness of the third and fifth layers in the multi-layer film on the surface of the thermal emitter in Example 1. DETAILED DESCRIPTION
[0018] Specific implementation method 1: This implementation method is a thermophotovoltaic system based on a multilayer film selective emitter, which includes a heat source, a heat emitter, a heat conductive steel and a photovoltaic cell, and the heat conductive steel is located between the heat source and the heat emitter;
[0019] The thermal emitter is composed of a metal substrate and a multi-layer film, and the multi-layer film is located on the surface of the metal substrate;
[0020] The multilayer film is composed of alternating metal layers and dielectric layers, wherein the metal layer in contact with the metal substrate has a thickness of 50nm to 150nm, the thickness of the other metal layers is 5nm to 10nm, and the thickness of each dielectric layer is 30nm to 200nm.
[0021] The beneficial effects of this embodiment are:
[0022] In order to solve the defect of low thermoelectric conversion efficiency caused by the mismatch between the band gap of photovoltaic cells and the emission spectrum of emitters in traditional thermophotovoltaic systems, this specific implementation method realizes selective regulation of the emission spectrum by depositing multiple layers of films on the surface of the emitter and superimposing the optical properties of different thin film materials. By adjusting the number of layers and the thickness of each layer, high emission is achieved in the response band of the corresponding photovoltaic cell, especially its optimal response band. The emissivity can reach above 0.85 in the optimal response band, so that the emission spectrum of the thermal emitter is matched with the band gap of the photovoltaic cell as much as possible, reducing heat loss and further increasing the temperature of the heat source, thereby improving the energy conversion efficiency of the thermophotovoltaic system and improving the system's utilization of thermal energy.
[0023] Compared with other methods of improving system efficiency, this specific embodiment does not need to add other components, and only needs to deposit a multilayer film on the surface of the thermal emitter, ensuring the compactness of the overall system. In addition, there are many ways to deposit a multilayer film with spectral selectivity on the surface of the thermal emitter, which is universal and can be prepared on a large area, suitable for industrial applications.
[0024] Specific implementation method 2: This implementation method is different from specific implementation method 1 in that: the metal substrate is a tungsten substrate or a steel substrate; the metal layer is one of tungsten and titanium or a combination of the two; the dielectric layer is one of silicon dioxide and hafnium dioxide or a combination of the two. The rest is the same as specific implementation method 1.
[0025] Specific implementation method 3: This implementation method is different from specific implementation method 1 or 2 in that: in the multi-layer film, a metal layer and a dielectric layer are used as a unit layer, and the unit layer is more than one layer. The rest is the same as specific implementation method 1 or 2.
[0026] Specific embodiment 4: This embodiment differs from specific embodiments 1 to 3 in that the heat source is an isotope heat source, electric heating, a solar energy concentrator, or a chemical fuel heat source. The rest is the same as specific embodiments 1 to 3.
[0027] Specific implementation example 5: This implementation example is different from specific implementation examples 1 to 4 in that the photovoltaic cell is a Si photovoltaic cell, a GaAs photovoltaic cell, a GaSb photovoltaic cell or an InGaAs photovoltaic cell. The rest is the same as specific implementation examples 1 to 4.
[0028] Specific implementation method 6: This implementation method is different from specific implementation methods 1 to 5 in that: the heat-conducting steel is a hollow hexagonal heat-conducting steel, the heat source is arranged in the hollow part of the heat-conducting steel, the heat emitter is arranged on the outer surface of the heat-conducting steel, the photovoltaic cells are evenly arranged around the heat-conducting steel, and a cooling device is arranged on the back of the photovoltaic cells; the heat source, the heat-conducting steel, the heat emitter and the photovoltaic cells are covered with heat-insulating materials above and below, a sealed top cover is arranged above the upper heat-insulating material, and a base is arranged below the lower heat-insulating material. The rest is the same as specific implementation methods 1 to 5.
[0029] Combination Figure 1 and Figure 2 This specific implementation proposes a thermophotovoltaic system based on a multilayer film selective emitter, including a heat source 1, a heat conductive steel 2, a metal substrate 3 in the heat emitter, a photovoltaic cell 5, a cooling device 6, a heat insulating material 7, and a multilayer film 4 attached to the surface of the metal substrate 3 in the heat emitter. The metal substrate 3 and the multilayer film 4 in the heat emitter together constitute the heat emitter of the thermophotovoltaic system. The heat emitted by the heat source 1 passes through the heat conductive steel 2 and the heat emitter metal substrate 3, and is selectively spectrally regulated by the multilayer film 4. The spectral energy that is highly matched with the bandgap width of the photovoltaic cell 5 is transferred to the photovoltaic cell 5 for thermoelectric conversion. At the same time, the spectral energy that is not selectively emitted further increases the temperature of the heat source 1 and the heat conductive steel 2, thereby improving the system efficiency.
[0030] There is a liquid cooling pipe in the cooling device 6. The cooling device 6 is in close contact with the back of the photovoltaic cell 5 to take away the excess heat in time. Heat insulation materials 7 are respectively arranged above and below the heat source 1, the heat-conducting steel 2, the metal substrate 3 in the heat emitter, the multilayer film 4, and the photovoltaic cell 5. There is a sealed top cover 8 on the heat insulation material 7 located above the thermal photovoltaic system, and the heat insulation material 7 located below the system is placed on a base 9.
[0031] Specific implementation method 7: This implementation method is different from specific implementation methods 1 to 6 in that: the cooling device is a liquid cooling device, an air cooling device, a heat sink, or a phase change cooling device; the thermal insulation material is asbestos, glass fiber, rock wool, or aluminum silicate. The rest is the same as specific implementation methods 1 to 6.
[0032] Specific embodiment 8: This embodiment is a method for preparing a thermophotovoltaic system based on a multilayer film selective emitter, which is carried out in the following steps:
[0033] A multilayer film is deposited on the surface of a metal substrate to obtain a heat emitter, which is fixed on the outer surface of a heat-conducting steel, and finally a heat source is fixed inside the hollow of the heat-conducting steel; the multilayer film is composed of alternating metal layers and dielectric layers, wherein the metal layer in contact with the metal substrate has a thickness of 50nm to 150nm, the thickness of the remaining metal layers is 5nm to 10nm, and the thickness of each dielectric layer is 30nm to 200nm.
[0034] Specific embodiment 9: This embodiment differs from specific embodiment 8 in that a multilayer thin film is deposited on the surface of a metal substrate by using a vacuum evaporation method, a magnetron sputtering coating method, an arc plasma coating method, an ion coating method or a molecular beam epitaxy method. The rest is the same as specific embodiment 8.
[0035] Specific embodiment 10: This embodiment is different from specific embodiment 8 or 9 in that when a multilayer thin film is deposited on the surface of a metal substrate by a magnetron sputtering coating method, the following steps are specifically performed: sputtering is performed under the conditions of a DC power supply with a sputtering power of 50W to 100W, a deposition temperature of room temperature to 700°C, a protective gas of argon or oxygen, a gas flow rate of 35sccm to 45sccm, and a vacuum chamber pressure of 1Pa to 2Pa; or sputtering is performed under the conditions of a RF power supply with a sputtering power of 80W to 120W, a deposition temperature of room temperature to 700°C, a protective gas of argon or oxygen, a gas flow rate of 35sccm to 45sccm, and a vacuum chamber pressure of 1Pa to 2Pa. The rest is the same as specific embodiment 8 or 9.
[0036] The following examples are used to verify the beneficial effects of the present invention:
[0037] Embodiment 1:
[0038] A thermophotovoltaic system based on a multilayer film selective emitter, comprising a heat source, a heat emitter, a heat conductive steel and a photovoltaic cell, wherein the heat conductive steel is located between the heat source and the heat emitter;
[0039] The thermal emitter is composed of a metal substrate and a multi-layer film, and the multi-layer film is located on the surface of the metal substrate;
[0040] The multilayer film has 6 layers, specifically: the first layer is a 57nm thick tungsten film, the second layer is a 47nm thick silicon dioxide film, the third layer is a 7nm thick tungsten film, the fourth layer is a 40nm thick silicon dioxide film, the fifth layer is a 7nm thick tungsten film and the sixth layer is a 25nm thick silicon dioxide film.
[0041] The metal substrate is a steel sheet.
[0042] The heat source is a silicon nitride electric heating rod.
[0043] The photovoltaic cell is a GaAs photovoltaic cell.
[0044] The heat-conducting steel is a hollow hexagonal heat-conducting steel, the heat source is arranged in the hollow part of the heat-conducting steel, the heat emitter is arranged on the outer surface of the heat-conducting steel, the photovoltaic cells are evenly arranged around the heat-conducting steel, and a cooling device is arranged on the back of the photovoltaic cells; the heat source, the heat-conducting steel, the heat emitter and the photovoltaic cells are covered with heat-insulating materials on the top and bottom, a sealed top cover is arranged above the upper heat-insulating material, and a base is arranged below the lower heat-insulating material.
[0045] The cooling device is a liquid cooling radiator, and water is used as the cooling liquid; the heat insulating material is asbestos.
[0046] The above-mentioned method for preparing a thermophotovoltaic system based on a multilayer film selective emitter is carried out according to the following steps:
[0047] A first layer of tungsten film with a thickness of 57nm, a second layer of silicon dioxide film with a thickness of 47nm, a third layer of tungsten film with a thickness of 7nm, a fourth layer of silicon dioxide film with a thickness of 40nm, a fifth layer of tungsten film with a thickness of 7nm and a sixth layer of silicon dioxide film with a thickness of 25nm are deposited in sequence on the surface of the metal substrate to obtain a thermal emitter. The thermal emitter is fixed to the outer surface of the thermal conductive steel, and finally the heat source is fixed to the hollow interior of the thermal conductive steel.
[0048] A tungsten film was deposited on the surface of a metal substrate using a magnetron sputtering coating method, specifically in the following steps: a tungsten target was used as the target material, and the tungsten film was sputtered at a deposition rate of 12.5 nm per minute under the conditions of a sputtering power of 100 W for the RF power supply, a deposition temperature of room temperature, an argon protective gas, a gas flow rate of 40 sccm, and a vacuum chamber pressure of 1.5 Pa.
[0049] A silicon dioxide film was deposited on the surface of a metal substrate using a magnetron sputtering coating method, specifically in the following steps: a silicon dioxide target was used as the target material, and the silicon dioxide film was sputtered under the conditions of a sputtering power of 100 W of an RF power supply, a deposition temperature of room temperature, an argon protective gas, a gas flow rate of 40 sccm, and a vacuum chamber pressure of 1.5 Pa, with a deposition rate of 4.17 nm per minute.
[0050] The emission spectrum of the thermal emitter was measured. Compared with the emission spectrum of the thermal emitter without depositing the multilayer film, the multilayer film showed good selective high emission in the range of 1 to 2 μm. Figure 3 It is the absorptivity curve diagram of the thermal emitter in Example 1; as can be seen from the figure, in the range of 0.5 to 1.2 μm, the emissivity of the thermal emitter gradually increases from 0.85 to above 0.95, and then decreases to about 0.85. The response spectrum of the GaAs photovoltaic cell is 0.3 to 1.2 μm, and is optimal at 0.6 to 0.8 μm. Therefore, the high emissivity in this section meets the requirements for matching the bandgap width of the photovoltaic cell.
[0051] Figure 4 Schematic diagram of the thickness of the first layer, the second layer, the fourth layer and the sixth layer in the multi-layer film on the surface of the thermal emitter in Example 1. Figure 5 Schematic diagram of the thickness of the third and fifth layers in the multi-layer film on the surface of the thermal emitter in Example 1.
[0052] Embodiment 2: This embodiment is different from Embodiment 1 in that: the multilayer film has 8 layers, specifically: the first layer is a titanium film with a thickness of 100nm, the second layer is a silicon dioxide film with a thickness of 200nm, the third layer is a titanium film with a thickness of 5nm, the fourth layer is a silicon dioxide film with a thickness of 159nm, the fifth layer is a titanium film with a thickness of 10nm, the sixth layer is a silicon dioxide film with a thickness of 200nm, the seventh layer is a titanium film with a thickness of 5nm, and the eighth layer is a silicon dioxide film with a thickness of 200nm; the first layer is a titanium film with a thickness of 100nm, the second layer is a silicon dioxide film with a thickness of 200nm, the third layer is a titanium film with a thickness of 100nm, the sixth layer is a silicon dioxide film with a thickness of 200nm, the seventh layer is a titanium film with a thickness of 5nm, and the eighth layer is a silicon dioxide film with a thickness of 200nm. The first layer is a titanium film with a thickness of 5nm, the fourth layer is a silicon dioxide film with a thickness of 159nm, the fifth layer is a titanium film with a thickness of 10nm, the sixth layer is a silicon dioxide film with a thickness of 200nm, the seventh layer is a titanium film with a thickness of 5nm, and the eighth layer is a silicon dioxide film with a thickness of 200nm; the titanium film is deposited on the surface of the metal substrate by a magnetron sputtering coating method, specifically according to the following steps: using a titanium target as a target material, sputtering the titanium film under the conditions of a sputtering power of 120W of an RF power supply, a deposition temperature of room temperature, an argon protective gas, a gas flow rate of 40sccm, and a vacuum chamber pressure of 1.5Pa, and depositing 3.03nm per minute. The photovoltaic cell uses GaSb material. The rest is the same as in Example 1.
[0053] The emission spectrum of the thermal emitter was measured. Compared with the emission spectrum of the thermal emitter without depositing the multilayer film, the multilayer film showed good selective high emission in the range of 1 to 2 μm. In the range of 1 to 2 μm, the emissivity of the thermal emitter fluctuated between 0.85 and 1. The response spectrum of the GaSb photovoltaic cell was 0.3 to 1.7 μm, and the best was achieved in the range of 1 to 1.6 μm. Therefore, the high emissivity in this section met the requirements for matching the bandgap width of the photovoltaic cell.
[0054] Embodiment 3: This embodiment is different from Embodiment 2 in that: the multilayer film has 8 layers, specifically: the first layer is a tungsten film with a thickness of 100nm, the second layer is a silicon dioxide film with a thickness of 131nm, the third layer is a titanium film with a thickness of 6nm, the fourth layer is a silicon dioxide film with a thickness of 200nm, the fifth layer is a titanium film with a thickness of 5nm, the sixth layer is a silicon dioxide film with a thickness of 100nm, the seventh layer is a tungsten film with a thickness of 10nm, and the eighth layer is a silicon dioxide film with a thickness of 113nm; the first layer is a tungsten film with a thickness of 100nm, the second layer is a silicon dioxide film with a thickness of 131nm, the third layer is a titanium film with a thickness of 6nm, the fourth layer is a silicon dioxide film with a thickness of 200nm, the fifth layer is a titanium film with a thickness of 5nm, the sixth layer is a silicon dioxide film with a thickness of 100nm, the seventh layer is a tungsten film with a thickness of 10nm, and the eighth layer is a silicon dioxide film with a thickness of 113nm. The first layer is a tungsten film with a thickness of 100nm, the second layer is a silicon dioxide film with a thickness of 131nm, the third layer is a titanium film with a thickness of 6nm, the fourth layer is a titanium film with a thickness of 200nm, the fifth layer is a titanium film with a thickness of 5nm, the sixth layer is a silicon dioxide film with a thickness of 100nm, the seventh layer is a tungsten film with a thickness of 10nm, and the eighth layer is a silicon dioxide film with a thickness of 113nm. The first layer is a titanium film with a thickness of 6nm, the fourth layer is a silicon dioxide film with a thickness of 200nm, the fifth layer is a titanium film with a thickness of 5nm, the sixth layer is a silicon dioxide film with a thickness of 100nm, the seventh layer is a tungsten film with a thickness of 10nm, and the eighth layer is a silicon dioxide film with a thickness of 113nm; a tungsten film is deposited on the surface of a metal substrate by a magnetron sputtering coating method, specifically in the following steps: a tungsten target is used as a target material, and a tungsten film is sputtered under the conditions that the sputtering power of the RF power supply is 100W, the deposition temperature is room temperature, the protective gas is argon gas, the gas flow rate is 40sccm, and the vacuum chamber pressure is 1.5Pa, and 12.5nm is deposited per minute. The rest is the same as in Example 2.
[0055] The emission spectrum of the thermal emitter was measured. Compared with the emission spectrum of the thermal emitter without depositing the multilayer film, the multilayer film showed good selective high emission in the range of 1 to 2 μm. In the range of 1 to 2 μm, the emissivity of the thermal emitter fluctuated between 0.8 and 0.95. The response spectrum of the GaSb photovoltaic cell was 0.3 to 1.7 μm, and the best was achieved in the range of 1 to 1.6 μm. Therefore, the high emissivity in this section met the requirements for matching the bandgap width of the photovoltaic cell.
[0056] Embodiment 4: This embodiment is different from Embodiment 3 in that: the multilayer film has 8 layers, specifically: the first layer is a titanium film with a thickness of 100nm, the second layer is a silicon dioxide film with a thickness of 101nm, the third layer is a titanium film with a thickness of 10nm, the fourth layer is a silicon dioxide film with a thickness of 200nm, the fifth layer is a tungsten film with a thickness of 4nm, the sixth layer is a silicon dioxide film with a thickness of 200nm, the seventh layer is a titanium film with a thickness of 9nm, and the eighth layer is a silicon dioxide film with a thickness of 113nm; the first layer is a titanium film with a thickness of 100nm, the second layer is a silicon dioxide film with a thickness of 101nm, the third layer is a titanium film with a thickness of 10nm, the fourth layer is a silicon dioxide film with a thickness of 200nm, the fifth layer is a tungsten film with a thickness of 4nm, the sixth layer is a silicon dioxide film with a thickness of 200nm, the seventh layer is a titanium film with a thickness of 9nm, and the eighth layer is a silicon dioxide film with a thickness of 113nm. The other parts are the same as those of Embodiment 3.
[0057] The emission spectrum of the thermal emitter was measured. Compared with the emission spectrum of the thermal emitter without depositing the multilayer film, the multilayer film showed good selective high emission in the range of 1 to 2 μm. In the range of 1 to 2 μm, the emissivity of the thermal emitter fluctuated between 0.8 and 1. The response spectrum of the GaSb photovoltaic cell was 0.3 to 1.7 μm, and the best was achieved in the range of 1 to 1.6 μm. Therefore, the high emissivity in this section met the requirements for matching the bandgap width of the photovoltaic cell.
Claims
1. A thermophotovoltaic system based on a multilayer film selective emitter, characterized in that It includes a heat source, a heat emitter, heat-conducting steel and a photovoltaic cell, and the heat-conducting steel is located between the heat source and the heat emitter; The thermal emitter is composed of a metal substrate and a multi-layer film, and the multi-layer film is located on the surface of the metal substrate; The multilayer film is composed of a first layer of tungsten film with a thickness of 57nm, a second layer of silicon dioxide film with a thickness of 47nm, a third layer of tungsten film with a thickness of 7nm, a fourth layer of silicon dioxide film with a thickness of 40nm, a fifth layer of tungsten film with a thickness of 7nm and a sixth layer of silicon dioxide film with a thickness of 25nm; The metal substrate is a steel sheet; The heat source is a silicon nitride electric heating rod; The photovoltaic cell is a GaAs photovoltaic cell; The above-mentioned method for preparing a thermophotovoltaic system based on a multilayer film selective emitter is carried out according to the following steps: A first layer of tungsten film with a thickness of 57 nm, a second layer of silicon dioxide film with a thickness of 47 nm, a third layer of tungsten film with a thickness of 7 nm, a fourth layer of silicon dioxide film with a thickness of 40 nm, a fifth layer of tungsten film with a thickness of 7 nm and a sixth layer of silicon dioxide film with a thickness of 25 nm are sequentially deposited on the surface of a metal substrate to obtain a heat emitter, the heat emitter is fixed to the outer surface of a heat-conducting steel, and finally a heat source is fixed to the hollow interior of the heat-conducting steel; A tungsten film is deposited on the surface of a metal substrate by a magnetron sputtering coating method, specifically in the following steps: a tungsten target is used as a target material, and a tungsten film is sputtered at a deposition rate of 12.5 nm per minute under the conditions that the sputtering power of the radio frequency power supply is 100 W, the deposition temperature is room temperature, the protective gas is argon gas, the gas flow rate is 40 sccm, and the vacuum chamber pressure is 1.5 Pa; A silicon dioxide film was deposited on the surface of a metal substrate using a magnetron sputtering coating method, specifically in the following steps: a silicon dioxide target was used as the target material, and the silicon dioxide film was sputtered under the conditions of a sputtering power of 100 W of an RF power supply, a deposition temperature of room temperature, an argon protective gas, a gas flow rate of 40 sccm, and a vacuum chamber pressure of 1.5 Pa, with a deposition rate of 4.17 nm per minute.
2. A thermophotovoltaic system based on a multilayer film selective emitter according to claim 1, characterized in that The heat-conducting steel is a hollow hexagonal heat-conducting steel, the heat source is arranged in the hollow part of the heat-conducting steel, the heat emitter is arranged on the outer surface of the heat-conducting steel, the photovoltaic cells are evenly arranged around the heat-conducting steel, and a cooling device is arranged on the back of the photovoltaic cells; The heat source, heat-conducting steel, heat emitter and photovoltaic cells are all covered with heat-insulating materials on the upper and lower sides. A sealed top cover is arranged above the upper heat-insulating material, and a base is arranged below the lower heat-insulating material.
3. A thermophotovoltaic system based on a multilayer film selective emitter according to claim 2, characterized in that The cooling device is a liquid cooling device, an air cooling device, a heat dissipation fin, or a phase change cooling device; the heat insulating material is asbestos, glass fiber, rock wool, or aluminum silicate.