A kind of preparation method of alcohol ether carboxylate

Through the combined use of supported metal catalysts and small molecule tertiary alcohols, the problems of high cost and toxic residues in the preparation of alcohol ether carboxylate are solved, and efficient and low-cost preparation of alcohol ether carboxylate is achieved, which is suitable for industrial and cosmetic applications.

CN115894208BActive Publication Date: 2024-11-12WANHUA CHEM GRP CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202211578165.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-12-09
Publication Date
2024-11-12
Estimated Expiration
2042-12-09

AI Technical Summary

Technical Problem

The preparation method of alcohol ether carboxylate in the prior art has high catalyst cost and low yield problems, and the traditional carboxymethylation method produces the toxic residue of chloroacetic acid, which limits its application in cosmetics and personal care products.

Method used

The supported metal catalyst and small molecule tertiary alcohol are used as a promoter to prepare alcohol ether carboxylate salts under mild conditions through catalytic oxidation reaction, reducing the amount of catalyst and by-product generation, increasing yield and reducing costs.

Benefits of technology

It has achieved high yield, low cost, and no irritant residue preparation, and is suitable for industrial production and cosmetics and other purposes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure FHA0000007055290000011
    Figure FHA0000007055290000011
Patent Text Reader

Abstract

The present invention provides a method for preparing alcohol ether carboxylates. The method comprises the following steps: (1) mixing fatty alcohol ether with one or more supported metal catalysts selected from cobalt, silver, platinum, tin, and indium, a promoter, and water, then introducing an oxygen-containing gas, and adding an alkali solution to carry out a catalytic oxidation reaction; (2) filtering the reaction liquid in step (1) to remove the catalyst, and concentrating to remove water and the promoter to obtain alcohol ether carboxylates. The method of the present invention has mild reaction conditions, low product loss rate, high yield, and low cost. The obtained ether carboxylates have the characteristics of no irritant residue, high active matter content, good quality, etc., and are suitable for oil fields, industrial cleaning, and personal care uses such as cosmetics.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of organic chemical synthesis, and particularly relates to a method for preparing alcohol ether carboxylate. Background Art

[0002] Compared with fatty alcohol ether (AEO), alcohol ether carboxylates overcome the weaknesses of low foam and greater skin irritation of AEO surfactants after the introduction of carboxylic acid; the embedding of EO chains can overcome the weaknesses of other anionic surfactants such as poor resistance to hard water, calcium soap dispersibility and water solubility; they can also maintain excellent foam performance, detergency and emulsification performance in hard water. However, the traditional carboxymethylation method inevitably produces residual toxic substances such as chloroacetic acid (salt), which cannot be used in cosmetics, personal care products, etc.

[0003] Patent CN1156419 reported that Pd / C catalyst was used for the oxidation of alcohol ethers, and the yield of carboxylate was >95%, but Pd metal was relatively expensive, and the application activity of the catalyst was not mentioned in the article. Patent CN101675021 also reported that Pd / C catalyst was used for the synthesis of alcohol ether carboxylates, and the resulting product had a low odor, but the yield and application activity of the catalyst were not mentioned. Patent CN101357333 and patent CN101164690 reported Pd / C and Pt / C catalysts for the oxidation of alcohol ethers, respectively, and the yields of alcohol ether carboxylates were as high as 91% and 59%, respectively. Often, high catalyst dosage leads to the decomposition of alcohol ethers and the generation of decarbonylation byproducts at higher temperatures, thereby limiting the improvement of the total yield.

[0004] Therefore, the high catalyst or application costs used in the existing technology bring great pressure to industrial production. Summary of the invention

[0005] In view of the above-mentioned deficiencies in the prior art, the object of the present invention is to provide a method for preparing alcohol ether carboxylates, which adopts a supported metal catalyst and simultaneously introduces a small molecular tertiary alcohol as a promoter. The method has mild conditions, low product loss rate, high yield, and low catalyst cost. The prepared ether carboxylates have the advantages of no irritant residue, high content of active substances (alcohol ether carboxylates), etc., and have industrial prospects.

[0006] In order to achieve the above invention object, the technical solution adopted by the present invention is as follows:

[0007] The present invention provides a method for preparing an alcohol ether carboxylate, comprising the following steps:

[0008] (1) mixing a fatty alcohol ether with one or more supported metal catalysts selected from cobalt, silver, platinum, tin, and indium, a promoter, and water, then introducing an oxygen-containing gas, and adding an alkali solution to carry out a catalytic oxidation reaction;

[0009] (2) filtering the reaction solution in step (1) to remove the catalyst, and concentrating to remove water and promoter to obtain alcohol ether carboxylate.

[0010] In the present invention, the fatty alcohol ether in step (1) has a structure as shown in Formula 1:

[0011]

[0012] In the formula, R 1 A straight chain or branched chain aliphatic alkyl group selected from C2 to C14, preferably a straight chain or branched chain aliphatic alkyl group of C10 to C14; -AO- represents one or more of -C2H4O- (ethoxy), -C3H6O- (propoxy), -C4H8O- (methylethoxy), preferably -C2H4O-; m is 1 to 20, preferably 5 to 13;

[0013] Preferably, the fatty alcohol ether is selected from A 10 EO5, A 10 EO7, A 12 EO7, A 12 EO9, A 14 EO 13 , more preferably A 12 EO7, A 12 EO9;

[0014] Accordingly, in the present invention, the alcohol ether carboxylate prepared in step (2) has a structure as shown in Formula 2:

[0015]

[0016] In the formula, R 1 , AO, m and R in formula 1 1 , AO, m are the same, that is, R 1 A straight chain or branched chain fatty alkyl group selected from C2 to C14, preferably a straight chain or branched chain fatty alkyl group selected from C10 to C14; one or more of -AO-C2H4O-(ethoxy), -C3H6O-(propoxy), -C4H8O-(methylethoxy), preferably -C2H4O-; m is 1 to 20, preferably 5 to 13;

[0017] The M is selected from hydrogen atom, alkali metal, alkaline earth metal, ammonium, preferably sodium atom; the value of n is 1-2, preferably 1.

[0018] In the present invention, the supported metal catalyst in step (1) has a metal loading of 0.05 to 12 wt%, preferably 1 to 5 wt%;

[0019] Preferably, the metal is selected from one or more of cobalt, silver, platinum, tin and indium, preferably a combination of cobalt and at least one of silver, platinum, tin and indium;

[0020] More preferably, the supported metal catalyst comprises: 1-10wt%, preferably 2-5wt% of cobalt, and 0.05-1.2wt%, preferably 0.1-0.5wt% of one or more of silver, platinum, tin and indium.

[0021] In the present invention, there is no particular limitation on the carrier of the supported metal catalyst, and known carriers such as activated carbon, silicon dioxide, aluminum oxide, etc. may be used, preferably activated carbon;

[0022] In the present invention, the source of the supported metal catalyst is not specifically limited, and it can be purchased or prepared by methods known in the art, such as an impregnation method. In some specific examples of the present invention, the preparation method of the supported metal catalyst is to first disperse the carrier in water, and then add a soluble metal salt (preferably a hydrochloride such as silver nitrate, chloroplatinic acid, tin chloride, indium chloride, etc.) to load it on activated carbon, and then reduce it with formaldehyde, hydrazine, sodium borohydride, hydrogen, etc. under heating, and then filter and dry to obtain the supported metal catalyst.

[0023] In the present invention, the amount of the supported metal catalyst in step (1) is 0.1 to 10 wt %, preferably 2 to 10 wt %, of the fatty alcohol ether.

[0024] In the present invention, the promoter in step (1) is selected from tertiary carbons of C4 to C12, preferably tert-butyl alcohol and / or tri-pentanol;

[0025] The amount of the accelerator used is 1-20wt% of the fatty alcohol ether, preferably 5-10wt%.

[0026] In the present invention, the reaction in step (1) is carried out in an aqueous solution, and the amount of water used is 2 to 10 times, preferably 3 to 7 times, the mass of the fatty alcohol ether.

[0027] In the present invention, the alkali solution in step (1) is an aqueous solution of alkali, and the concentration is 2-15wt%, preferably 3-7wt%; the alkali is selected from alkali metals, alkaline earth metals, and ammonium hydroxides, preferably sodium hydroxide;

[0028] The amount of the alkali solution used is 1 to 2.5 times, preferably 1 to 1.5 times, the molar amount of the hydroxyl group in the fatty alcohol ether based on the molar amount of the alkali contained therein;

[0029] The alkali solution can be added all at once or added dropwise, preferably added dropwise, and the pH of the reaction solution is controlled to be 7-11, preferably 8-10 during the dropping process.

[0030] In the present invention, the oxygen-containing gas in step (1) is selected from a gas having an oxygen volume content of not less than 20%, preferably pure oxygen;

[0031] The oxygen-containing gas is continuously introduced during the reaction, and the system pressure is controlled to be 0-0.5 MPaG, preferably 0.02-0.1 MPaG.

[0032] In the present invention, the reaction in step (1) is carried out at a temperature of 40 to 120° C., preferably 60 to 100° C., and for a time of 2 to 12 hours, preferably 3 to 6 hours.

[0033] In the present invention, the concentration and removal of water and accelerator in step (2) is carried out at a temperature of 30-80°C, preferably 50-70°C; and a pressure of 5-100 hPaA, preferably 10-30 hPaA;

[0034] The concentration and dehydration may be performed by directly concentrating the reaction solution to remove water, or by first neutralizing the reaction solution with an acid (such as dilute hydrochloric acid) and then concentrating to remove water, whereby M in the alcohol ether carboxylate product of Formula 2 obtained is a hydrogen atom; direct concentration and dehydration is preferred.

[0035] In the process of converting fatty alcohol ether into alcohol ether carboxylate of the present invention, the terminal hydroxyl group undergoes dehydrogenation to aldehyde and then oxidation to carboxylic acid, such as Figure 1 The mechanism shows that 1) the outermost layer of the catalytic metal has 1 to 2 electrons, and the metal is easy to combine with hydroxyl alcohol to complete dehydrogenation; 2) at the same time, the auxiliary metal is easier to lose electrons than Co in an oxygen-containing atmosphere, thereby protecting the main catalytic metal Co and keeping it active; 3) the promoter tertiary alcohol, on the one hand, acts as a proton solvent, which can promote the circulation of H participation and improve the activity of non-precious metal catalysts; on the other hand, the small molecule can prevent the combination of metal and carbonyl, avoid further decarbonylation and the poisoning of the decarbonylation product (CO, CO2) to the catalyst, and improve the reaction efficiency.

[0036] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0037] In the reaction of the present invention, a metal-supported catalyst is used, and a small molecular tertiary alcohol is introduced as a promoter. The fatty alcohol ether is catalytically oxidized to ether carboxylates in an oxygen-containing gas atmosphere. The reaction conditions are mild and the yield is high. Compared with the traditional carboxymethylation method, the prepared ether carboxylates have the advantages of no residual irritants such as chloroacetic acid (salt) and high active matter content, and are suitable for oil fields, industrial cleaning, and personal care purposes such as cosmetics. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 This is the mechanism of the dehydrogenation of the terminal hydroxyl group to aldehyde and then oxidation to carboxylic acid during the conversion of fatty alcohol ether to alcohol ether carboxylate. DETAILED DESCRIPTION

[0039] The following examples will further illustrate the method provided by the present invention, but the present invention is not limited to the listed examples, and should also include any other known changes within the scope of the rights claimed by the present invention.

[0040] The main analysis methods used in the embodiments of the present invention are as follows:

[0041] The catalyst metal content was measured by SPECTROGREEN ICP-OES;

[0042] The active matter content of alcohol ether carboxylates was determined by titration;

[0043] CO and CO2 were measured by Agilent 8890 gas chromatograph CO-CO2 analyzer.

[0044] The main sources of reagents used in the embodiments of the present invention are as follows:

[0045] AEO (98%), sodium hydroxide (98%), 5wt% Pd / C Catalyst: Inokite;

[0046] Oxygen (industrial pure): torch gas;

[0047] Preparation of supported metal catalyst cat-1: Add 95 g of activated carbon to a reaction bottle and disperse it in 200 g of pure water, add 11 g of cobalt chloride, 0.25 g of tin chloride and 0.40 g of indium chloride to the pure water to load them on the activated carbon, then reduce them with hydrogen under heating, filter and separate the catalyst, and dry to obtain catalyst cat-1 (metal composition and loading amount: Co5wt%, Sn 0.1wt%, In 0.2wt%).

[0048] Referring to the above method, the metal types and ratios were replaced as needed to prepare supported metal catalysts cat-2 (metal composition and loading amount were Co 2wt%, Ag 0.5wt%, Pt 0.05wt%), catalyst cat-3 (metal composition and loading amount were Co 3wt%, Ag 0.1wt%, Sn 1.0wt%), and catalyst cat-4 (metal composition and loading amount were Co10wt%, Pt 0.2wt%, Sn 1.0wt%).

[0049] Unless otherwise specified, other raw materials were commercially available and reagents were of analytical grade.

[0050] Example 1

[0051] Preparation of alcohol ether carboxylates, the steps are:

[0052] 37.9 g A 10EO5 (0.1 mol), 265.0 g pure water, 1.89 g tert-butanol and 1.89 g catalyst cat-1 were added into a 500 mL stainless steel reactor equipped with a mechanical stirrer, a thermometer and connected to an O2 gas line. The reactor was replaced with O2 three times in the system, the reactor was heated to 100°C, filled with O2 to make the reactor pressure at 0.02 MPaG, the stirring was turned on and set to 800 rpm, 57.1 g of a 7.0 wt% NaOH (4.0 g, 0.1 mol) aqueous solution was added dropwise thereto, the pH of the reaction system was kept at 8-10 during the addition process, the reaction was continued for 6 h, the reaction was stopped, the gas samples in the reactor were collected, and no CO and CO2 were detected by gas chromatography analysis.

[0053] The reaction solution was cooled to room temperature, filtered, and concentrated at 50° C. and 30 hPaA to remove water and tert-butanol to obtain alcohol ether carboxylate with a yield of 98.3%. The active matter content was 97.6% after titration.

[0054] Example 2

[0055] Preparation of alcohol ether carboxylates, the steps are:

[0056] 58.3 g A 12 EO9 (0.1 mol), 174.8 g pure water, 5.83 g tri-amyl alcohol and 5.83 g catalyst cat-2 were added into a 1000 mL stainless steel reactor equipped with a mechanical stirrer, a thermometer and connected to an O2 gas line. The reactor was replaced with O2 three times in the system, the reactor was heated to 60°C, filled with O2 to make the pressure of the reactor at 0.1 MPaG, the stirring was turned on and set to 800 rpm, and 200 g of a 3.0 wt% NaOH (6.0 g, 0.15 mol) aqueous solution was added dropwise thereto. The pH of the reaction system was kept at 8-10 during the addition process. The reaction was continued for 4 h, the reaction was stopped, and the gas samples in the reactor were collected. No CO or CO2 was detected by gas chromatography analysis.

[0057] The reaction solution was cooled to room temperature, filtered, and concentrated at 70°C and 10 hPaA to remove water and tri-amyl alcohol. The yield was 98.1% and the active matter content was 96.5% by titration.

[0058] Example 3

[0059] Preparation of alcohol ether carboxylates, the steps are:

[0060] 49.5 g A 12EO7 (0.1 mol), 247.4 g pure water, 3.46 g tert-butanol and 0.99 g catalyst cat-3 were added into a 1000 mL stainless steel reactor equipped with a mechanical stirrer, a thermometer and connected to an O2 gas line. The reactor was replaced with O2 three times in the system, the reactor was heated to 80°C, filled with O2 to make the reactor pressure at 0.05 MPaG, the stirring was turned on and set to 800 rpm, and 95 g of a 5 wt% aqueous solution of NaOH (4.8 g, 0.12 mol) was added dropwise thereto. The pH of the reaction system was kept at 8-10 during the addition process. The reaction was continued for 5 h, the reaction was stopped, and the gas samples in the reactor were collected. No CO or CO2 was detected by gas chromatography analysis.

[0061] The reaction solution was cooled to room temperature, filtered, and concentrated at 60°C and 20 hPaA to remove water and tert-butanol to obtain alcohol ether carboxylate with a yield of 97.8%. The active matter content was 96.2% after titration.

[0062] Example 4

[0063] Preparation of alcohol ether carboxylates, the steps are:

[0064] 78.7 g A 14 EO 13 (0.1mol), 787.1g pure water, 3.94g tert-butanol and 0.79g catalyst cat-4 were added into a 2000mL stainless steel reactor equipped with a mechanical stirrer, a thermometer and connected to an O2 gas line. The reactor was replaced with O2 three times in the system, the reactor was heated to 120°C, filled with O2 to make the pressure of the reactor at 0.5MPaG, the stirring was turned on and set to 800rpm, and 100g of 7wt% NaOH (7.2g, 0.18mol) aqueous solution was added dropwise thereto. The pH of the reaction system was kept at 8-10 during the addition process. The reaction was continued for 12h, the reaction was stopped, and the gas samples in the reactor were collected. No CO and CO2 were detected by gas chromatography analysis.

[0065] The reaction solution was cooled to room temperature, filtered, and concentrated at 80°C and 10 hPaA to remove water and tert-butanol to obtain alcohol ether carboxylate with a yield of 98.6%. The active matter content was 95.7% after titration.

[0066] Comparative Example 1

[0067] The alcohol ether carboxylate was prepared by referring to the method of Example 1, except that the promoter tert-butyl alcohol was not added, and the other operations and parameters remained unchanged;

[0068] Gas sample gas chromatography analysis of CO, CO2 are 1640ppm and 2530ppm respectively, A 10 The yield of E5C-Na was 92.1%, and the active matter content was 90.5% by titration.

[0069] Comparative Example 2

[0070] Alcohol ether carboxylates were prepared by referring to the method of Example 1, except that the promoter tert-butyl alcohol was not added, and the catalyst cat-1 was replaced by 1.89 g of Pd / C catalyst (Pd content 5 wt%) of the same mass, and other operations and parameters remained unchanged;

[0071] Gas sample gas chromatography analysis of CO, CO2 are 7210ppm and 9650ppm respectively, A 10 The yield of E5C-Na was 81.3%, and the active matter content was 79.8% by titration.

[0072] Comparative Example 3

[0073] Alcohol ether carboxylates were prepared by referring to the method of Example 1, except that the catalyst cat-1 was replaced with 1.89 g of Pd / C catalyst (Pd content 5 wt%) of the same mass, and other operations and parameters remained unchanged;

[0074] Gas sample gas chromatography analysis of CO, CO2 were 5330ppm and 6240ppm respectively, A 10 The yield of E5C-Na was 83.1%, and the active matter content was 80.2% by titration.

[0075] Comparative Example 4

[0076] The alcohol ether carboxylate was prepared by referring to the method of Example 1, except that the promoter tert-butyl alcohol was replaced by n-butyl alcohol, and the other operations and parameters remained unchanged;

[0077] Gas sample gas chromatography analysis of CO, CO2 are 8530ppm and 10260ppm respectively, A 10 The yield of E5C-Na was 76.3%, and the active matter content was 74.1% by titration.

Claims

1. A method for preparing an alcohol ether carboxylate, characterized in that: The steps include: (1) mixing a fatty alcohol ether with one or more supported metal catalysts selected from cobalt, silver, platinum, tin, and indium, a promoter, and water, then introducing an oxygen-containing gas, and adding an alkali solution to carry out a catalytic oxidation reaction; (2) filtering the reaction solution in step (1) to remove the catalyst, and concentrating to remove water and promoter to obtain alcohol ether carboxylate; The fatty alcohol ether in step (1) has a structure as shown in Formula 1: In the formula, R 1 A straight chain or branched chain fatty alkyl selected from C2 to C14; -AO- represents one of -C2H4O-, -C3H6O-, and -C4H8O-; m is 1 to 20; The alcohol ether carboxylate prepared in step (2) has a structure as shown in Formula 2: In the formula, R 1 , AO, m and R in formula 1 1 , AO, and m are the same; The M is selected from alkali metals, alkaline earth metals, and ammonium; the value of n is 1 to 2; The supported metal catalyst in step (1) has a metal loading of 0.05 to 12 wt %; the supported metal catalyst is used in an amount of 0.1 to 10 wt % of the mass of the fatty alcohol ether; the promoter is selected from tert-butyl alcohol and / or tri-amyl alcohol; and the promoter is used in an amount of 1 to 20 wt % of the mass of the fatty alcohol ether.

2. The preparation method according to claim 1, characterized in that: The R 1 A straight chain or branched chain fatty alkyl group selected from C10 to C14; -AO- represents -C2H4O-; and m is 5 to 13.

3. The preparation method according to claim 1, characterized in that: The M is a sodium atom; the value of n is 1.

4. The preparation method according to claim 1, characterized in that: The supported metal catalyst in step (1) has a metal loading of 1 to 5 wt%; The metal is selected from a combination of cobalt and at least one of silver, platinum, tin and indium; The amount of the supported metal catalyst used is 2-10 wt % of the mass of the fatty alcohol ether.

5. The preparation method according to claim 4, characterized in that: The supported metal catalyst comprises: 1-10 wt% of cobalt, and 0.05-1.2 wt% of one or more of silver, platinum, tin and indium.

6. The preparation method according to claim 5, characterized in that: The supported metal catalyst comprises: 2-5 wt% of cobalt, and 0.1-0.5 wt% of one or more of silver, platinum, tin and indium.

7. The preparation method according to claim 1, characterized in that: Step (1) The amount of the accelerator used is 5-10wt% of the mass of the fatty alcohol ether.

8. The preparation method according to claim 1, characterized in that: The amount of water used in step (1) is 2 to 10 times the mass of the fatty alcohol ether.

9. The preparation method according to claim 8, characterized in that: The amount of water used is 3 to 7 times the mass of the fatty alcohol ether.

10. The preparation method according to claim 1, characterized in that: The alkali solution in step (1) is an aqueous solution of alkali with a concentration of 2 to 15 wt %; the alkali is selected from alkali metals, alkaline earth metals, and ammonium hydroxides; The amount of the alkali solution used is 1 to 2.5 times the molar amount of the hydroxyl group in the fatty alcohol ether based on the molar amount of the alkali contained therein; The alkali solution is added all at once or dropwise, and the pH of the reaction solution is controlled to be between 7 and 11 during the dropwise addition process.

11. The preparation method according to claim 10, characterized in that: The concentration of the alkali solution is 3-7 wt %; the alkali is selected from sodium hydroxide.

12. The preparation method according to claim 10, characterized in that: The amount of the alkali solution used is 1 to 1.5 times the molar amount of the hydroxyl group in the fatty alcohol ether based on the molar amount of the alkali contained therein.

13. The preparation method according to claim 10, characterized in that: The alkali solution is added dropwise, and the pH of the reaction solution is controlled to be between 8 and 10 during the addition process.

14. The preparation method according to claim 1, characterized in that: The oxygen-containing gas in step (1) is selected from a gas having an oxygen volume content of not less than 20%; The oxygen-containing gas is continuously introduced during the reaction to control the system pressure to be 0-0.5 MPaG, and not 0.

15. The preparation method according to claim 14, characterized in that: The oxygen-containing gas is pure oxygen.

16. The preparation method according to claim 14, characterized in that: The system pressure was controlled to be 0.02~0.1MPaG.

17. The preparation method according to claim 1, characterized in that: The reaction in step (1) is carried out at a temperature of 40 to 120° C. for 2 to 12 hours.

18. The preparation method according to claim 17, characterized in that: The reaction temperature is 60-100°C and the reaction time is 3-6 hours.

19. The preparation method according to claim 1, characterized in that: The concentration and removal of water and accelerator in step (2) is carried out at a temperature of 30-80° C. and a pressure of 5-100 hPaA; The concentration and dehydration may be performed by directly concentrating the reaction solution to remove water, or by first neutralizing the reaction solution with an acid and then concentrating the solution to remove water.

20. The preparation method according to claim 19, characterized in that: The concentration removes water and accelerator at a temperature of 50-70° C. and a pressure of 10-30 hPaA.

Citation Information

Cited By

  • Fatty alcohol ether carboxylic acid and preparation method thereof

    CN120987751A