A complex iron desulfurization system and desulfurization process

Through the combination of a two-phase mixing equipment and an oxidative desulfurization reactor, a stable high-sulfur capacity desulfurization liquid is formed, which solves the problem of difficulty in sedimentation and separation of sulfur particles, improves the desulfurization efficiency and separation effect, and is suitable for a wide range of application scenarios.

CN115957608BActive Publication Date: 2024-12-06CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111177327.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-10-09
Publication Date
2024-12-06
Estimated Expiration
2041-10-09

AI Technical Summary

Technical Problem

In the existing complex iron oxidation and desulfurization system, sulfur particles are difficult to settle and separate, resulting in blocking towers and side reactions, affecting the operating efficiency of the device. In addition, the existing technology has low efficiency in removing sulfides under high pressure and is not thoroughly separated.

Method used

A two-phase mixing equipment is used to form a stable high-sulfur capacity desulfurization liquid, and the catalytic cracked diesel and complex iron solution are cut and mixed through fiber wire assembly to form a micro channel structure, combining the oxidation desulfurization reactor and the two-phase separation zone to realize hydrogen sulfide and oil Rapid dissolution and separation of phases overcome the problem of blocking towers.

Benefits of technology

It improves the mass transfer and reaction efficiency of the liquid phase oxidation and desulfurization process, solves the problem of tower blocking, and realizes effective separation and regeneration of sulfur, which is suitable for a wide range of application scenarios.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115957608B_ABST
    Figure CN115957608B_ABST
Patent Text Reader

Abstract

The present invention discloses a complex iron desulfurization system and a desulfurization process. The complex iron desulfurization system comprises: a two-phase mixing zone, an oxidative desulfurization zone and a two-phase separation zone; a plurality of oil-water mixing devices are arranged in the two-phase mixing zone, and the oil-water two phases are cut and mixed in the oil-water mixing device through fiber filaments to form an oil-water mixed desulfurized liquid; an oxidative desulfurization reactor is arranged in the oxidative desulfurization zone for oxidative desulfurization of hydrogen sulfide-containing gas; the two-phase separation zone is used for oil-water separation of the oil-water mixed desulfurized liquid with saturated sulfur capacity, and an oil-water separation device is arranged in the two-phase separation zone to separate the oil phase and the water phase. The present invention forms a high-sulfur capacity desulfurized liquid with stable properties through a two-phase mixing device, improves the mass transfer and reaction efficiency of reactants in the liquid-phase oxidative desulfurization process, and overcomes the tower blockage problem in conventional desulfurization processes, and has broad application prospects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of waste gas treatment, and specifically relates to a complex iron oxidation desulfurization system and a desulfurization process. Background Art

[0002] The complex iron desulfurization technology is a wet oxidation-reduction method for removing sulfides using iron as a catalyst. It is suitable for situations where the H2S concentration is low or the H2S concentration is high but the gas flow rate is not large. The complex iron desulfurization usually uses an aqueous solution of alkali (Na2CO3 or K2CO3) to absorb sulfides. The H2S gas reacts with the alkali to generate HS - , by reducing high-valent Fe ions to low-valent Fe ions, HS - During the regeneration process, the low-valent complex iron solution is oxidized into a high-valent complex iron solution when in contact with air, restoring the oxidation performance, and the solution circulates to absorb hydrogen sulfide gas.

[0003] There are two main LO-CAT process routes: (1) H2S absorption and catalyst regeneration are carried out in two bubbling towers respectively, and the desulfurization liquid circulates between the two towers; (2) H2S absorption and catalyst regeneration are carried out in different areas of a bubbling tower, such as the self-circulating LO-CAT process, where absorption and regeneration are carried out in the center and annular gap of an inner circulation bubbling tower respectively. However, both methods require that the sulfur particles generated by the reaction be quickly separated from the desulfurization solution, otherwise it will cause tower blockage and side reactions, affecting the normal operation of the device. The particle size of the sulfur particles generated by the reaction is very small (hundreds of nanometers to several microns), and has special surface properties, which are easy to adsorb but not easy to settle. The existing technology increases the sedimentation ratio of sulfur by adding dispersants and flocculants, so that the sulfur settles at the bottom of the reactor, discharges the sedimentation liquid, and then separates the sulfur. Due to the low sulfur content in the sedimentation liquid, a large amount of solution circulates between the filtration unit and the reactor, increasing energy consumption and desulfurization agent loss, and the separation effect is not ideal.

[0004] CN1554467A discloses a method for removing sulfide from carbon dioxide-rich gas by complex iron method. The method adopts complex iron desulfurizer and high-efficiency spray tower and fluidized bed combined process, improves gas-liquid mass transfer efficiency, solves the problem of sulfur tower blocking, and improves purification degree. However, the method is only applicable to sulfide removal under relatively low pressure, and the complex iron desulfurization liquid is not completely separated from the sulfur particles during the regeneration process, which will affect the subsequent circulation process.

[0005] CN101870884A discloses a method for complex iron liquid phase oxidation absorption of hydrogen sulfide gas and sulfur recovery. The method includes a regeneration separation tower composed of a bubbling reaction section, a gas-liquid separation section and a foam collection section. In the bubbling reaction section, the catalyst is oxidized and regenerated, and sulfur particles are enriched at the bubble interface. In the gas-liquid separation section, the regenerated desulfurization solution and the foam are separated, and the desulfurization solution is returned to the absorption tower for recycling. The sulfur is carried to the foam collection section by the foam, which improves the sulfur particle separation rate and the regeneration reaction rate. However, this method does not completely solve the problems of tower blockage and foaming that have always existed. C104548905A discloses an emulsion oxidation desulfurization and sulfur recovery method. The method allows hydrogen sulfide-containing gas to enter the absorber and contact with the oil-complex iron emulsion, hydrogen sulfide reacts to generate sulfur, sulfur is dissolved in the oil phase, and the purified gas is discharged from the top of the absorber; the sulfur-containing oil-complex iron emulsion is demulsified, then oil and water are separated, and sulfur is recovered from the oil phase. In this method, relatively large bubbles are easily generated during the reaction process, and the reaction uniformity needs to be improved. At the same time, the oil-complex iron emulsion is not easy to exist stably during a long reaction process. Summary of the invention

[0006] In view of the deficiencies in the prior art, the present invention provides a complex iron desulfurization system and a desulfurization process. The present invention forms a high-sulfur capacity desulfurization liquid with stable properties through a two-phase mixing device, thereby improving the mass transfer and reaction efficiency of reactants in the liquid-phase oxidation desulfurization process, while overcoming the tower blockage problem in conventional desulfurization processes, and has broad application prospects.

[0007] The complex iron desulfurization system of the present invention comprises: a two-phase mixing zone, an oxidative desulfurization zone and a two-phase separation zone;

[0008] Among them, a number of oil-water mixing devices are arranged in the two-phase mixing zone, and the oil-water mixing devices include a fiber filament assembly and a shell, the fiber filament assembly is fixed in the shell, an inlet is arranged at one end of the shell for feeding oil and water two phases (catalytic cracking diesel and complex iron solution), and an oil-water mixed desulfurization liquid outlet is arranged at the other end; the fiber filament assembly comprises a plurality of stacked thin sheets and oleophilic fiber filaments and / or (preferably and) hydrophilic fiber filaments filled in the gaps between adjacent thin sheets, a number of microchannels are formed between the fiber filaments, and the fiber filaments are clamped and fixed by the thin sheets; the oil and water two phases are cut and mixed by the fiber filaments in the oil-water mixing device to form an oil-water mixed desulfurization liquid;

[0009] An oxidative desulfurization reactor is provided in the oxidative desulfurization zone for oxidative desulfurization of hydrogen sulfide-containing gas. A liquid phase feed port is provided at the top or side of the reactor, a purified gas outlet is provided at the top or side, and a hydrogen sulfide-containing gas inlet and a liquid phase material outlet are provided at the bottom or side of the reactor; the oil-water mixed desulfurization liquid outlet of the oil-water mixing device is connected to the liquid phase feed port of the oxidative desulfurization reactor; the hydrogen sulfide-containing gas contacts the oil-water mixed desulfurization liquid in the oxidative desulfurization reactor, and hydrogen sulfide is oxidized to sulfur under the action of the water phase and dissolved in the oil phase;

[0010] The two-phase separation zone is used to achieve oil-water separation of the oil-water mixed desulfurized liquid with saturated sulfur capacity. The oil-water separation equipment is arranged in the two-phase separation zone to separate the oil phase and the water phase. After the separated oil phase is cooled, the solid-liquid separation is performed to obtain sulfur and catalytic cracking diesel. After the separated water phase is oxidized, it is regenerated and recycled.

[0011] In the complex iron desulfurization system of the present invention, the fiber filaments are arranged in a single layer or multiple layers, preferably 1 to 50 layers, and more preferably 1 to 5 layers; when arranged in multiple layers, the projection of two adjacent layers of fiber filaments along the vertical direction of the thin sheet is preferably a mesh structure; the grid shape in the mesh structure is an arbitrary shape, such as one or more combinations of polygons, circles, ellipses, etc.; in each layer of fiber filaments, the spacing between adjacent fiber filaments is generally 0.5μm to 50μm, preferably arranged at equal intervals, and the fiber filaments are arranged in any direction such as the horizontal, longitudinal or oblique direction along the surface of the thin sheet; the fiber filaments can be of any curved shape, preferably a periodically changing curved shape, such as a wavy shape, a zigzag shape, etc., preferably the fiber filaments in the same layer have the same shape, and more preferably the fiber filaments in all layers have the same shape.

[0012] The diameter of the fiber is generally 0.5-50 μm, preferably 0.5-5 μm, and more preferably 0.5-1 μm. The oleophilic fiber is generally selected from at least one of polyester fiber, nylon fiber, polyurethane fiber, polypropylene fiber, polyacrylonitrile fiber and polyvinyl chloride fiber, or selected from fiber materials with oleophilic surface treatment; the hydrophilic fiber is selected from polymers containing hydrophilic groups such as carboxyl (-COOH), amide (-CONH-), amino (-NH2-), or hydroxyl (-OH) in the main chain or side chain, such as polypropylene fiber, polyamide fiber, acrylic fiber, or selected from fiber materials with hydrophilic treatment by physical or chemical methods. The thickness of the sheet is generally 0.05 mm to 5 mm, preferably 0.1 to 1.5 mm. The material of the thin sheet is generally determined according to the properties of the flowing material and the operating conditions. It can be any one or more of metal, ceramic, plexiglass or polyester, preferably stainless steel (such as SS30403, SS30408, SS32168, SS31603 and other models). The shape of the thin sheet is not limited, and it can be any one of rectangular, square, polygonal, circular, elliptical, fan-shaped, etc., preferably rectangular or square. In the fiber filament assembly, the size and quantity of the thin sheet can be designed and adjusted according to the actual needs of the reaction. Generally, thin sheets of the same shape and size are used in the fiber filament assembly.

[0013] In the complex iron desulfurization system of the present invention, in order to prevent material short circuit and ensure that the material flows from the inlet end to the outlet end in the fiber filament assembly, except for the inlet end and the outlet end, the remaining ends of the fiber filament assembly are sealed and connected to the shell.

[0014] The present invention also provides a desulfurization process, including the following contents:

[0015] (1) In the two-phase mixing zone, catalytic cracking diesel and complex iron solution enter from the inlet of the oil-water mixing device, and are cut and mixed by the fiber filaments in the fiber filament assembly in the oil-water mixing device to form an oil-water mixed desulfurization liquid that enters the oxidation desulfurization zone;

[0016] (2) In the oxidative desulfurization zone, the oil-water mixed desulfurization liquid enters from the top or side of the oxidative desulfurization reactor and contacts with the hydrogen sulfide-containing gas entering from the bottom or side of the reactor in countercurrent. The hydrogen sulfide reacts with the complex iron solution to generate sulfur, which is dissolved in the surrounding oil phase. The purified gas from which the hydrogen sulfide is removed is discharged from the top of the reactor, and the liquid phase material reaching the saturated sulfur capacity is discharged from the bottom of the reactor into the two-phase separation zone;

[0017] (3) In the two-phase separation zone, the liquid phase material that has reached the saturated sulfur content enters the oil-water separation equipment and is separated into two phases, namely, the oil phase containing sulfur and the water phase containing complex iron. After the oil phase is cooled, the solid-liquid separation is performed to obtain sulfur and catalytic cracking diesel. The separated water phase is oxidized and regenerated for recycling.

[0018] In the process of the present invention, the distillation range of the catalytic cracking diesel is any fraction within the range of 180-380°C, preferably any fraction within the range of 240-330°C; the content of bicyclic aromatic hydrocarbons in the catalytic cracking diesel is 30wt%-80wt%.

[0019] In the process of the present invention, the iron ion concentration in the complex iron solution is 0.05-0.1 mol / L, and the pH value is 8-10; the complex iron solution also contains additives such as alkaline substances, stabilizers and corrosion inhibitors that are well known to those skilled in the art.

[0020] In the process of the present invention, the mass ratio of the complex iron solution to the catalytic cracking diesel is 1:10-2:3.

[0021] In the process of the present invention, the sulfur content of the oil-water mixed desulfurization liquid is 2% to 10% (g / g).

[0022] In the process of the present invention, the fiber filament assembly comprises a plurality of stacked thin sheets and several layers of oleophilic and / or hydrophilic fiber filaments filled in the gaps between adjacent thin sheets, preferably filled with oleophilic and hydrophilic fiber filaments, and the mass ratio of oleophilic fiber filaments to hydrophilic fiber filaments is 100:1~1:100.

[0023] In the process of the present invention, the volume ratio of the hourly volume flow rate of hydrogen sulfide-containing gas to the volume of the oil-water mixed desulfurization liquid is 1:4-10:1.

[0024] In the process of the present invention, the hydrogen sulfide-containing gas is one or a mixture of various hydrogen sulfide-containing waste gases, refinery gas, natural gas, Selexol tail gas and Claus tail gas; the volume percentage of H2S in the hydrogen sulfide-containing gas is 0.01%~20%.

[0025] In the process of the present invention, the reaction temperature in the oxidative desulfurization reactor is 35-85° C., and the reaction pressure is 0.1-2 MPa.

[0026] In the process of the present invention, the sulfur-containing oil phase enters the solid-liquid separator for cooling to precipitate sulfur and separate it, recover the sulfur, and regenerate the sulfur solvent; the solid-liquid separator is cooled by external condensed water or other coolants; the cooling and separation temperature of the sulfur-containing oil phase in the solid-liquid separator is generally 0-30° C., preferably 10-25° C.; the regeneration of the water phase containing complex iron can be performed by conventional methods in the art for off-site regeneration, such as air oxidation method, electrolysis method and biological method.

[0027] Compared with the prior art, the present invention has the following advantages: due to the special microchannel structure of the oil-water mixing equipment and the ultra-fine lipophilic and / or hydrophilic fiber filaments filled between the gaps of adjacent thin sheets, the mixed feed of the complex iron water phase and the catalytic cracking diesel is first forcibly cut into a mixed material containing uniform, micron-sized particles, and the existence state of the mixed material is very stable; the mixed material is also introduced into the oxidative desulfurization reactor as a desulfurization, and reacts with the hydrogen sulfide-containing gas in countercurrent contact, and the sulfur obtained by the reaction can be quickly dissolved in the oil phase, which promotes the reaction and enhances the mass transfer, reaction and dissolution efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 It is a schematic diagram of the complex iron oxidation desulfurization system and desulfurization process of the present invention.

[0029] 1-catalytic cracking diesel, 2-complex iron solution, 3-oil-water mixing equipment, 4-shell, 5-fiber filament assembly, 6-oil-water mixed desulfurization liquid, 7-hydrogen sulfide-containing gas, 8-oxidative desulfurization reactor, 9-purified gas, 10-liquid phase material, 11-oil-water separation equipment, 12-sulfur-containing oil phase, 13-complex iron-containing water phase, 14-solid-liquid separator.

[0030] Figure 2 A schematic diagram of the structure of a fiber filament assembly.

[0031] 15-thin sheet, 16-slit, 17-fiber filament, 18-microchannel. DETAILED DESCRIPTION

[0032] The present invention is further described below in conjunction with the accompanying drawings and examples, but the present invention is not limited thereby. The properties of the catalytic cracking diesel used in the present invention are shown in Table 1.

[0033] The specific process of the oxidation desulfurization process of the present invention is as follows: (1) in the two-phase mixing zone, catalytic cracking diesel 1 and complex iron solution 2 enter from the inlet of the oil-water mixing device 3, and in the oil-water mixing device, the fiber filaments in the fiber filament assembly 5 are cut and mixed to form an oil-water mixed desulfurized liquid 6, which enters the oxidation desulfurization zone; (2) in the oxidation desulfurization zone, the oil-water mixed desulfurized liquid 6 enters from the top or side of the oxidation desulfurization reactor 8, and is countercurrently contacted with the hydrogen sulfide-containing gas 7 entering from the bottom or side of the reactor, and hydrogen sulfide reacts under the action of the complex iron solution to generate Sulfur, sulfur is dissolved in the surrounding oil phase, and the purified gas 9 with hydrogen sulfide removed is discharged from the top of the reactor. The liquid phase material 10 reaching the saturated sulfur content is discharged from the bottom of the reactor and enters the two-phase separation zone; (3) In the two-phase separation zone, the liquid phase material 10 reaching the saturated sulfur content enters the oil-water separation equipment 11 and is separated into oil and water phases, namely, the sulfur-containing oil phase 12 and the complex iron-containing water phase 13. The oil phase enters the solid-liquid separator 14 and is cooled. After solid-liquid separation, sulfur and catalytic cracking diesel are obtained. The separated water phase is oxidized and regenerated for recycling.

[0034] The method for determining the mixing and dispersion effect of the desulfurized liquid in this embodiment is as follows: under the same conditions, the complex iron solution (dispersed phase) and the catalytic cracking diesel (continuous phase) are mixed, and at least 10 groups of mixed material samples are obtained for each method. The particle size of the dispersed phase in the mixed material sample is photographed using a British IX i-SPEED 5 high-speed camera, and the dispersed phase particles in the photo are added up, and the percentage of particles of various sizes is calculated to obtain a normal distribution diagram of particles of various sizes, thereby obtaining the particle uniformity.

[0035] Table 1 Properties of catalytic cracking diesel at different distillation ranges.

[0036]

[0037] Example 1

[0038] (1) The hydrogen sulfide gas from a refinery has a hydrogen sulfide content of 1.2% by volume; the Fe ion concentration in the complex iron solution is 0.06 mol / L, and the pH value is 9.5; in the desulfurized liquid, the volume ratio of the complex iron solution to catalytic cracking diesel with a distillation range of 240-260°C is 1:6;

[0039] (2) The thin sheets in the fiber assembly in the oil-water mixing equipment are made of stainless steel with a thickness of 2.0 mm. A layer of fiber with a diameter of 1 μm (the mass ratio of polyacrylonitrile fiber to polypropylene fiber is 3:1) is filled between the thin sheets. The fiber is arranged at equal intervals with a spacing of 2 μm. The fiber is in the shape of a sawtooth-shaped curve with periodic changes; the dispersed size of the complex iron solution droplets in the desulfurization liquid is 200 nm~500 nm;

[0040] (3) In the oxidative desulfurization reactor, the reaction conditions are as follows: the hourly flow rate of H2S-containing gas and the volume ratio of oil-water mixed desulfurization liquid is 12:1; the reaction temperature is 55°C, the reaction pressure is 0.5MPa, and after the desulfurization liquid reaches the saturated sulfur capacity, it is discharged from the bottom of the reactor for regeneration, and fresh desulfurization liquid is added at the same time; after oxidative desulfurization, the H2S concentration in the purified gas is 9mg / m 3 .

[0041] Example 2

[0042] (1) The hydrogen sulfide gas from a refinery has a hydrogen sulfide content of 0.8% by volume; the Fe ion concentration in the complex iron solution is 0.06 mol / L, and the pH value is 9.5; in the desulfurized liquid, the volume ratio of the complex iron solution to catalytic cracking diesel with a distillation range of 260-280°C is 1:6;

[0043] (2) The thin sheets in the fiber filament assembly in the oil-water mixing equipment are made of stainless steel with a thickness of 1.0 mm. Two layers of fiber filaments with a diameter of 1 μm (the mass ratio of nylon fiber filaments to polyamide fiber filaments is 4:1) are filled between the thin sheets. The fiber filaments are arranged at equal intervals with a spacing of 1 μm. The fiber filaments are in the shape of a sawtooth-shaped curve with periodic changes; the dispersed size of the complex iron solution droplets in the desulfurization liquid is 100 nm~300 nm;

[0044] (3) The reaction conditions in the oxidative desulfurization reactor are as follows: the volume ratio of the hourly flow rate of H2S-containing gas to the oil-water mixed desulfurization liquid is 20:1, the reaction temperature is 70°C, the reaction pressure is 1.0 MPa, and after the desulfurization liquid reaches the saturated sulfur capacity, it is regenerated and the fresh desulfurization liquid feed is switched at the same time; after oxidative desulfurization, the H2S concentration in the purified gas is 6 mg / m 3 .

[0045] Example 3

[0046] (1) The hydrogen sulfide gas from a refinery has a hydrogen sulfide content of 2.6%; the Fe ion concentration in the complex iron solution is 0.12 mol / L, and the pH value is 10.0; in the desulfurized liquid, the volume ratio of the complex iron solution to catalytic cracking diesel with a distillation range of 300-330°C is 1:10;

[0047] (2) The thin sheets in the fiber assembly in the oil-water mixing equipment are made of stainless steel with a thickness of 1.0 mm. Three layers of fiber with a diameter of 1 μm are filled between the thin sheets (the mass ratio of acrylic fiber to polyamide fiber is 1:1). The fiber is arranged at equal intervals with a spacing of 1 μm. The fiber is a curve shape with periodic changes of wavy lines; the dispersion size d1 of the complex iron solution droplets in the oil-water mixed desulfurization liquid is 200 nm~400 nm;

[0048] (3) The reaction conditions of the oxidation desulfurization reactor are as follows: the volume ratio of the hourly flow rate of H2S-containing gas to the oil-water mixed desulfurization liquid is 20:1; the reaction temperature is 65°C, the reaction pressure is 0.3MPa, and after the oil-water mixed desulfurization liquid reaches the saturated sulfur capacity, it is regenerated and the fresh oil-water mixed desulfurization liquid is switched to feed; after oxidation desulfurization, the H2S concentration in the purified gas is 8mg / m 3 .

Claims

1. A complex iron desulfurization system, characterized in that include: Two-phase mixing zone, oxidation desulfurization zone and two-phase separation zone; Among them, a number of oil-water mixing devices are arranged in the two-phase mixing zone, and the oil-water mixing devices include a fiber filament assembly and a shell, the fiber filament assembly is fixed in the shell, an inlet is arranged at one end of the shell for catalytic cracking diesel and complex iron solution oil-water two-phase feeding, and an oil-water mixed desulfurization liquid outlet is arranged at the other end; the fiber filament assembly comprises a plurality of stacked thin sheets and oleophilic fiber filaments and / or hydrophilic fiber filaments filled in the gaps between adjacent thin sheets, a number of microchannels are formed between the fiber filaments, and the fiber filaments are clamped and fixed by the thin sheets; the oil-water two-phase is cut and mixed by the fiber filaments in the oil-water mixing device to form an oil-water mixed desulfurization liquid; An oxidative desulfurization reactor is provided in the oxidative desulfurization zone for oxidative desulfurization of hydrogen sulfide-containing gas. A liquid phase feed port is provided at the top or side of the reactor, a purified gas outlet is provided at the top or side, and a hydrogen sulfide-containing gas inlet and a liquid phase material outlet are provided at the bottom or side of the reactor; the oil-water mixed desulfurization liquid outlet of the oil-water mixing device is connected to the liquid phase feed port of the oxidative desulfurization reactor; the hydrogen sulfide-containing gas contacts the oil-water mixed desulfurization liquid in the oxidative desulfurization reactor, and hydrogen sulfide is oxidized to sulfur under the action of the water phase and dissolved in the oil phase; The two-phase separation zone is used to achieve oil-water separation of the oil-water mixed desulfurized liquid with saturated sulfur content. The two-phase separation zone is provided with oil-water separation equipment to separate the oil phase and the water phase. After the separated oil phase is cooled, solid-liquid separation is performed to obtain sulfur and catalytic cracking diesel. After the separated water phase is oxidized, it is regenerated and recycled. The fiber filaments are arranged in a single layer or multiple layers; when arranged in multiple layers, the projection of two adjacent layers of fiber filaments along the vertical direction of the thin sheet is a mesh structure; in each layer of fiber filaments, the spacing between adjacent fiber filaments is 0.5μm to 50μm, and the diameter of the fiber filaments is 0.5~50μm; the thickness of the thin sheet is 0.05mm~5mm; the material of the thin sheet is one or more of metal, ceramic, organic glass or polyester.

2. The complex iron desulfurization system according to claim 1, characterized in that: The oleophilic fiber yarn is selected from at least one of polyester fiber yarn, nylon fiber yarn, polyurethane fiber yarn, polypropylene fiber yarn, polyacrylonitrile fiber yarn and polyvinyl chloride fiber yarn, or is selected from fiber yarn materials with oleophilic surface treatment; the hydrophilic fiber yarn is polypropylene fiber, polyamide fiber, acrylic fiber, or is selected from fiber yarns with hydrophilic treatment by physical or chemical methods.

3. The complex iron desulfurization system according to claim 1, characterized in that: Except for the inlet end and the outlet end, the remaining ends of the fiber filament assembly are sealed and connected to the shell.

4. A desulfurization process used in the complex iron desulfurization system according to claim 1, characterized in that The invention comprises the following contents: (1) in the two-phase mixing zone, catalytic cracking diesel and complex iron solution enter from the inlet of the oil-water mixing device, and are cut and mixed by the fiber filaments in the fiber filament assembly in the oil-water mixing device to form an oil-water mixed desulfurized liquid, which enters the oxidation desulfurization zone; (2) in the oxidation desulfurization zone, the oil-water mixed desulfurized liquid enters from the top or side of the oxidation desulfurization reactor, and is countercurrently contacted with the hydrogen sulfide-containing gas entering from the bottom or side of the reactor. The hydrogen sulfide reacts with the complex iron solution to generate sulfur, and the sulfur is dissolved in the surrounding oil phase. The purified gas from which hydrogen sulfide is removed is discharged from the top of the reactor, and the liquid phase material reaching the saturated sulfur content is discharged from the bottom of the reactor and enters the two-phase separation zone; (3) in the two-phase separation zone, the liquid phase material reaching the saturated sulfur content enters the oil-water separation device and is divided into two phases of oil and water, namely, the oil phase containing sulfur and the water phase containing complex iron. After the oil phase is cooled, the solid-liquid separation is performed to obtain sulfur and catalytic cracking diesel. The separated water phase is oxidized and regenerated for recycling.

5. The desulfurization process according to claim 4, characterized in that: The distillation range of the catalytic cracking diesel is any fraction within the range of 180-380°C; the content of dicyclic aromatic hydrocarbons in the catalytic cracking diesel is 30wt%-80wt%.

6. The desulfurization process according to claim 4, characterized in that: The iron ion concentration in the complex iron solution is 0.05~0.1mol / L, and the pH value is 8~10.

7. The desulfurization process according to claim 4, characterized in that: The mass ratio of the complex iron solution to the catalytic cracking diesel is 1:10-2:

3.

8. The desulfurization process according to claim 4, characterized in that: The sulfur content of the oil-water mixed desulfurization liquid is 2% to 10%.

9. The desulfurization process according to claim 4, characterized in that: The volume ratio of the hourly volume flow rate of hydrogen sulfide-containing gas to the volume of the oil-water mixed desulfurization liquid is 1:4~10:

1.

10. The desulfurization process according to claim 4, characterized in that: The volume percentage of H2S in hydrogen sulfide-containing gas is 0.01%~20%.

11. The desulfurization process according to claim 4, characterized in that: The reaction temperature in the oxidative desulfurization reactor is 35~85°C, and the reaction pressure is 0.1~2MPa.

12. The desulfurization process according to claim 4, characterized in that: The sulfur-containing oil phase enters the solid-liquid separator for cooling to precipitate sulfur and separate it, recover sulfur, and regenerate sulfur solvent; the solid-liquid separator is cooled by external condensed water or other coolants; the cooling and separation temperature of the sulfur-containing oil phase in the solid-liquid separator is 0-30°C.