A radar detection method for the position of steel bars and bottom voids in mold bag slope protection projects
By establishing the fitting curve between the moisture content of the mold bag, the radar wave speed and relative dielectric constant, combined with the processing of the radar electromagnetic wave scanning diagram, the problem of steel bar position and bottom discharge detection in the mold bag slope protection project is solved, achieving efficient and accurate The test results avoid potential disasters caused by errors.
Patent Information
- Application Number
- CN202310108293.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-02-14
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2043-02-14
AI Technical Summary
The existing technology is difficult to accurately detect the position and bottom of the steel bars in mold bag slope protection projects, resulting in the inability to detect diseases and hidden dangers in time. Moreover, the relative dielectric constant selection caused by changes in concrete moisture content during radar detection is difficult, resulting in errors in the detection result. .
By establishing the fitting curve of the moisture content of the mold bag and the radar wave velocity fitting curve and the relative dielectric constant fitting curve, combined with the filtering preprocessing and wavelet transformation method of the radar electromagnetic wave scanning diagram, the depth of the target object is calculated, and the position and bottom of the concrete steel bar of the mold bag are realized. Accurate detection of air leakage.
High resolution, fast and efficient detection of the steel bar position and bottom discharge of the mold bag slope protection project is achieved, reducing detection errors, and timely evaluating the overall quality of the mold bag project and taking preventive measures.
Smart Images

Figure CN115963491B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of mold bag slope protection engineering detection, and in particular relates to a radar detection method for steel bar positions and bottom voids in mold bag slope protection engineering. Background Art
[0002] The mold bag slope protection technology is currently a commonly used slope protection technology for water conservancy projects. Due to its neat and beautiful appearance, convenient construction, high efficiency and the fact that it can be constructed both underwater and on the water, it has been widely used at home and abroad. The mold bag project is divided into two forms: simple mold bags and machine-made mold bags. Simple mold bags are also called woven cloth mold bag concrete. The mold bags are hand-sewn, and the internal filler is mortar or fine stone concrete. The average thickness is generally 12-20cm. A steel bar is inserted longitudinally in each bag. The characteristics are simple filling method and saving investment; the machine-made mold bag is a mold bag cloth woven with synthetic fiber filaments as raw materials. It is shaped and produced by the factory. The internal filler is fine stone concrete. The average thickness is generally 12-15cm. A longitudinal steel bar is inserted every 40cm. The characteristics are fast construction speed and high efficiency. The common technical characteristics of the two are good integrity, streamlined structure, strong wind and wave resistance and anti-scouring ability. At present, they have been greatly developed in domestic embankment protection and channel protection.
[0003] The simple mold bag and the mechanical mold bag structure bring difficulties to the detection of the steel bar position. Due to its large thickness, the maximum thickness of the mold bag at the wave crest exceeds 20cm, which cannot be detected by the steel bar locator and the concrete steel bar protective layer thickness meter. Due to its wavy surface, when using ground penetrating radar for detection, the radar antenna or the radar integrated machine cannot move, and it cannot work. The same problem is faced when detecting the bottom of the mold bag. In addition, the moisture content of the concrete in the mold bag slope protection project varies greatly. At the foot of the slope of the mold bag slope protection, due to the presence of water, the moisture content of the mold bag concrete is almost saturated, while the moisture content at the top of the slope is small, or even dry. In addition, due to the influence of groundwater, the moisture content of the mold bag slope protection gradually increases from the top to the foot of the slope, and the change in moisture content has a greater impact on the relative dielectric constant of the concrete, which brings difficulties to the selection of the relative dielectric constant during radar detection. If an average value or a fixed value is selected, it will inevitably bring a large error to the detection result. At the same time, the change in moisture content also has a great impact on the electromagnetic wave velocity of the radar, which will bring a large error to the depth calculation of the target. The above reasons have resulted in the inability to conduct non-destructive testing of the steel bar position and bottom voiding problems in the formwork bag slope protection project, and the inability to timely discover the defects and hidden dangers of the formwork bag project. In order to avoid the occurrence of disasters, a non-destructive testing technology is urgently needed to accurately detect the steel bar position and bottom voiding problems of the formwork bag concrete. Summary of the invention
[0004] The technical problem to be solved by the present invention is: to provide a radar detection method for the position of steel bars and the bottom voids in a mold bag slope protection project, so that a ground penetrating radar can work normally on the mold bag slope protection, and by establishing a mold bag moisture content and radar wave velocity fitting curve, a mold bag moisture content and relative dielectric constant fitting curve, the radar wave velocity and relative dielectric constant of the detection part are calculated, and finally the depth of the target object is calculated, so that the position of the steel bars in the mold bag concrete can be accurately detected, and the depth and range of the voids at the bottom of the mold bag can be accurately detected, thereby evaluating the overall quality of the mold bag project.
[0005] A radar detection method for the position of steel bars and bottom voids in a mold bag slope protection project comprises the following steps, which are performed in sequence:
[0006] Step 1: Through the indoor mold bag slope protection model test, the mold bag moisture content and radar wave velocity fitting curve, and the mold bag moisture content and relative dielectric constant fitting curve are obtained;
[0007] Step 2: Lay an auxiliary pad on the surface of the mold bag slope protection at the project site, and use radar electromagnetic wave scanning to obtain a radar scanning image;
[0008] Step 3: Perform filtering preprocessing on the radar scan image obtained in step 2, remove the DC component of the signal, remove low-frequency interference and high-frequency noise, and determine the zero depth point, then perform filtering processing, use wavelet transform and KL transform to remove irrelevant signals, eliminate interference noise in the time dimension, and obtain an effective radar scan image;
[0009] Step 4: The concrete moisture content at the target position of the effective radar scanning image is obtained by the indoor mold bag slope protection model test in step 1, and the radar wave velocity and relative dielectric constant at the target position are obtained by fitting curves of mold bag moisture content and radar wave velocity, and fitting curves of mold bag moisture content and relative dielectric constant;
[0010] Step 5: By reading the two-way travel time t1 of the steel layer through the electromagnetic wave reflection data, the depth of the steel layer can be calculated; by reading the two-way travel time t2 of the void layer through the electromagnetic wave reflection data, the depth of the top of the void layer can be calculated.
[0011] The specific steps of the indoor mold bag slope protection model test in step 1 are:
[0012] ① Make a bracket with the same oblique support angle as the slope of the project site, lay the mold bag on the bracket, and the filling material in the mold bag is the same as the filling material in the mold bag used on the project site. At the same time, set up a comparison test piece, simulate the pouring process on the project site for pouring and drainage, and put it into the standard curing room after 24 hours;
[0013] ② After curing, remove the mold bag cloth, grind the thickness to the same standard, test the radar propagation time in the concrete, and calculate the radar wave velocity and the relative dielectric constant of the concrete;
[0014] ③ After the mold bag and the specimen are fully soaked, the saturated mass M1 of the core sample of the specimen is tested, and a portable concrete moisture content meter is used to test and correct the upper surface of the core sample; aluminum foil is laid on the lower surface of the mold bag as a reflection interface, and the propagation time t1 of the ground penetrating radar in the concrete is measured, the thickness h of the mold bag is measured, the propagation speed υ1 is calculated, and the relative dielectric constant ε of the concrete is calculated. r1 ;
[0015] ④ Dry the mold bag and the specimen naturally, compare the constant weight of the specimen, and obtain the dry mass of the specimen M0; test and compare the mass of the specimen M every 6 to 10 hours. i and the propagation velocity of ground penetrating radar in bagged concrete i And calculate the relative dielectric constant ε of concrete ri ;
[0016] ⑤Through the moisture content of concrete Where i is the number of tests; w i The moisture content of the i-th test; M i is the mass of the specimen in the i-th test;
[0017] ⑥ The correlation formula is established by using the radar wave velocity υ and the corresponding concrete moisture content w, and the fitting curve is υ=(a1+b1×w)×10 8 ; In the formula, a1 is the intercept and b1 is the slope;
[0018] The relative dielectric constant ε of concrete r The correlation formula is established with the corresponding concrete moisture content w, and the fitting curve is ε r =a2+b2×w, where a2 is the intercept and b2 is the slope;
[0019] The auxiliary pad in step 2 is a polyvinyl chloride (PVC), polyethylene (PE) or polypropylene (PP) sheet, and has a width greater than that of the radar antenna or the radar integrated machine.
[0020] The calculation method of the depth of the steel bar layer in step 5 is:
[0021] The depth h1 of the steel bar layer is Where V1 is the propagation speed of radar electromagnetic waves in the steel bar layer, ε r1 is the relative dielectric constant of concrete, and x is the antenna receiving and transmitting distance.
[0022] The calculation method of the top of the de-hollowing layer in step 5 is:
[0023] The top depth of the de-hollowing layer h2 is V2 is the propagation speed of radar electromagnetic waves in the void layer, ε r2 is the relative dielectric constant of the hollow layer, and x is the antenna receiving and transmitting distance.
[0024] Through the above-mentioned design scheme, the present invention can bring the following beneficial effects: a radar detection method for the position of steel bars and the bottom voids of mold bag slope protection projects, which is convenient, high-resolution, fast and efficient. The position of steel bars and the bottom voids of mold bag slope protection projects can be detected, and after the moisture content is determined, the relationship between the radar wave velocity and the relative dielectric constant and the moisture content of the mold bag mortar and the linear fitting curve can be calculated. After the dielectric constant and the radar wave velocity are calculated, the accurate position and depth are calculated, so as to evaluate the overall quality of the mold bag project, so as to promptly deal with the mold bag project with hidden dangers, or take necessary preventive measures to avoid the occurrence of slope failure disasters. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] The present invention is further described below with reference to the accompanying drawings and specific embodiments:
[0026] Figure 1 The present invention is a schematic flow chart of a radar detection method for detecting the position of steel bars and bottom voids in a mold bag slope protection project.
[0027] Figure 2 A radar detection method for detecting the position of steel bars and bottom voids in a mold bag slope protection project according to the present invention is shown in the following specific implementation manner: 1. A schematic diagram of the relationship curve between the radar wave velocity υ and the concrete moisture content w.
[0028] Figure 3 A radar detection method for the position of steel bars and bottom voids in a mold bag slope protection project according to the present invention. Specific implementation method 1. Relative dielectric constant ε of concrete r Schematic diagram of the relationship curve with concrete moisture content w.
[0029] Figure 4 A radar detection method for detecting the position of steel bars and bottom voids in a mold bag slope protection project according to the present invention is shown in FIG1 . Schematic diagram of radar scanning at a location without voids.
[0030] Figure 5 A radar detection method for detecting the position of steel bars and bottom voids in a mold bag slope protection project according to the present invention is shown in FIG1 . 1 is a schematic diagram of radar scanning at the voids.
[0031] Figure 6 A radar detection method for detecting the position of steel bars and bottom voids in a mold bag slope protection project according to the present invention is shown in a specific implementation manner 2, and a schematic diagram of a curve showing the relationship between radar wave velocity υ and mortar moisture content w.
[0032] Figure 7A radar detection method for detecting the position of steel bars and bottom voids in a mold bag slope protection project according to the present invention. Specific implementation method 2. Relative dielectric constant ε of mortar r Schematic diagram of the relationship curve with mortar moisture content w.
[0033] Figure 8 Schematic diagram of radar scanning of the hollowing out of mortar in mold bag according to a specific implementation method of a radar detection method for the position of steel bars and the hollowing out of the bottom of a mold bag slope protection project of the present invention. DETAILED DESCRIPTION
[0034] A radar detection method for the position of steel bars and bottom voids in a mold bag slope protection project, using a high-frequency electromagnetic wave of a geological radar method, which is sent into the mold bag concrete medium in a direction in the form of pulses through a transmitting antenna. When the electromagnetic wave propagates in the mold bag concrete, when it encounters steel bars or voids, the electromagnetic wave generates a strong reflection signal, which is received by a receiving antenna and displayed by a radar acquisition system. On the basis of data processing of the collected radar waves, the spatial position and burial depth of the steel bar position and the void layer at the bottom of the concrete are inferred according to the waveform, amplitude intensity and time variation characteristics of the radar wave, thereby achieving the purpose of detecting the steel bar position and the void layer depth.
[0035] Radar detection calculation formula:
[0036] The propagation speed of radar electromagnetic waves in the first layer of matter:
[0037] In formula (1), C is the propagation speed of electromagnetic waves in vacuum, that is, the speed of light, which is 0.30 m / ns.
[0038] The depth of the first target layer can be calculated by reading the two-way travel time t1 of the first target layer from the electromagnetic wave reflection data, that is,
[0039] In formula 2), x is the antenna transmission and reception distance.
[0040] When a transceiver is used, the transceiver distance is very small relative to the depth of the target object and can be simplified as
[0041] h1=t1×V1 / 2(3)
[0042] The propagation speed of radar electromagnetic waves in the second layer of matter:
[0043] Finally, the depth of the second layer is obtained:
[0044] When a transceiver is used, it can be simplified to h2 = t2 × V2 / 2. (6)
[0045] Similarly, the depths of multiple target layers can be calculated.
[0046] like Figure 1 As shown, the specific steps include:
[0047] Step 1: Through the indoor mold bag slope protection model test, the mold bag moisture content and radar wave velocity fitting curve, and the mold bag moisture content and relative dielectric constant fitting curve are obtained;
[0048] 1) Make a simple steel bracket for forming the mold bag. Its oblique support angle is the same as the actual slope of the project. During forming, the mold bag is placed obliquely on the bracket.
[0049] 2) Sew the mold bag cloth into a mold bag with a length of 1.2 meters and a width of 0.4 meters, and lay it on the inclined support. Mix the concrete according to the mold bag construction ratio, fill the mold bag with concrete mixture, pour and drain according to the actual project pouring process, and finally seal the upper part tightly (see Figure 1 ), a total of 2 mold bags were made, and 12 150×150×150mm comparison specimens were formed at the same time. The comparison specimens were laid on the mold bag cloth using a bottomless test mold to keep it consistent with the mold bag and allow drainage. After 24 hours, the filled mold bags and comparison specimens were placed in a standard curing room.
[0050] 3) After 28 days, the two mold bags were taken out of the standard curing room, the mold bag cloth was removed, and the upper and lower surfaces of the mold bags were smoothed. The thickness was controlled at 150 mm to test the radar propagation time in the concrete. 10 data were extracted from each mold bag, and a total of 20 data were extracted and averaged to calculate the radar wave velocity and the relative dielectric constant of concrete.
[0051] 4) Take out the two mold bags and 12 comparison specimens after they have been fully soaked (soaked for 4 days). First, test the saturated mass M1 of the core sample, then use a portable concrete moisture content meter to test the upper surface of the core sample and make corrections for use in field detection. Then lay aluminum foil on the lower surface of the large mold bag as a reflection interface, measure the propagation time t1 of the ground penetrating radar in the concrete, measure the thickness h of the large mold bag, calculate the propagation speed υ1, and then calculate the relative dielectric constant ε of the concrete. r1 .
[0052] 5) Then place the two mold bags and 12 comparison specimens in the room to dry naturally, and test the quality M of the comparison specimens every 6 to 10 hours. i and the propagation velocity of ground penetrating radar in bagged concrete i And calculate the relative dielectric constant ε of concrete ri The test time interval can be adjusted in subsequent measurements according to actual conditions.
[0053] 6) After the comparison specimen reaches constant weight, the dry mass M0 of the specimen is obtained.
[0054] 7) The moisture content of the concrete specimens was compared by taking the average value of 12 specimens. The moisture content of concrete was
[0055]
[0056] 8) According to the above test, when the height of the target is known, the radar wave velocity υ can be obtained by back-calculating using formula (3). The radar wave velocity υ and the corresponding concrete moisture content w are used to establish a correlation formula, and the fitting curve is:
[0057] υ=(a1+b1×w)×10 8 (8)
[0058] The relative dielectric constant ε of concrete can be obtained by back calculation using formula (1): r , relative dielectric constant of concrete ε r The correlation formula is established with the corresponding concrete moisture content w, and the fitting curve is:
[0059] ε r =a2+b2×w(9)
[0060] Step 2: Lay an auxiliary pad on the surface of the mold bag slope protection at the project site, and use radar electromagnetic wave scanning to obtain a radar scanning image;
[0061] 1) Radar basic parameter settings:
[0062] The antenna frequency is selected as 2600MHz or MiniXT type 2.7GHz according to the detection depth;
[0063] The time window is 14-20ns. Depending on the depth of the target object, the lower limit is selected for steel bar position detection and the upper limit is selected for void detection.
[0064] The number of sampling points is 512-1536. When the number of sampling points is large, the amount of data is large, and the amount of information about the target object is also large, but the efficiency is low. When the number of sampling points is small, the amount of data is small, and the amount of information about the target object is also small, but the work efficiency will be improved.
[0065] Scan density: 4 scans / cm
[0066] 2) Survey line layout. The survey lines of each detection section of the mold bag slope protection site are arranged in two horizontal and one vertical shapes, forming an I-shape. The vertical survey lines are arranged on the mold bag without steel bars, and the distance is 2 meters. If voids are found on site, the scanning range can be expanded to determine the scope of the voids.
[0067] 3) Lay the auxiliary pad. Lay an auxiliary pad on the surface of the wavy mold bag for scanning. The auxiliary pad can be made of polyvinyl chloride (PVC), polyethylene (PE) or polypropylene (PP) plates. The width is slightly wider than the radar antenna or radar integrated machine, and the length is 1 meter. Two plates are used alternately to move forward during detection.
[0068] Step 3: Perform filtering preprocessing on the radar scan image obtained in step 2, remove the DC component of the signal, remove low-frequency interference and high-frequency noise, and determine the zero depth point, then perform filtering processing, use wavelet transform and KL transform to remove irrelevant signals, eliminate interference noise in the time dimension, and obtain an effective radar scan image;
[0069] Step 4: The concrete moisture content at the target position of the effective radar scanning image is obtained by the indoor mold bag slope protection model test in step 1, and the radar wave velocity and relative dielectric constant at the target position are obtained by fitting curves of mold bag moisture content and radar wave velocity, and fitting curves of mold bag moisture content and relative dielectric constant;
[0070] Step 5: The two-way travel time t1 of the steel layer is read out through the electromagnetic wave reflection data, and the depth of the steel layer can be calculated; the two-way travel time t2 of the void layer is read out through the electromagnetic wave reflection data, and the depth of the top of the void layer can be calculated;
[0071] By reading the two-way travel time t of the steel layer through the electromagnetic wave reflection data, the depth of the steel layer can be calculated according to formula (2) or formula (3).
[0072] The two-way travel time t of the de-voided layer is read out through the electromagnetic wave reflection data, and the depth of the top of the de-voided layer is calculated according to formula (2) or formula (3), and the depth of the bottom of the de-voided layer is calculated according to formula (5) or formula (6).
[0073] Example 1
[0074] The connecting channel project uses machine-made mold bag concrete slope protection with an average thickness of 120mm. A grade II steel bar with a diameter of 12mm is inserted every 400mm along the direction of water flow. The strength grade of the machine-made mold bag concrete is C25 and the frost resistance grade is F200.
[0075] The indoor model test was carried out according to the above test steps. The test results are shown in Table 1
[0076] Table 1 Results of indoor model test on machine mold bags
[0077]
[0078]
[0079] According to the radar wave velocity v and the corresponding concrete moisture content w obtained in Table 1, the fitting curve is as follows: Figure 2 As shown, the fitting curve is
[0080] υ=(-2.60224w+1.15466)×10 8
[0081] According to the fitting curve of concrete dielectric constant and corresponding concrete moisture content obtained in Table 1, Figure 3 As shown, the fitting curve is
[0082] ε r =39.66615w+6.68829
[0083] Figure 2 Figure 3 It is shown in the figure that the sum of squares of the relationship between radar wave velocity and relative dielectric constant and concrete moisture content and the residual of the linear fitting curve are 0.00298 and 0.32774 respectively, and the goodness of fit R 2 The smaller the sum of squares of the residuals of a set of data, the better the fit. The goodness of fit R 2 They are all close to 1, which also indicates a good degree of fit.
[0084] from Figure 2 Figure 3 It can be seen that the radar wave velocity is linearly related to the relative dielectric constant of concrete and the moisture content of concrete. The fitted curve fits better. The higher the moisture content of concrete, the greater the relative dielectric constant, and the lower the propagation speed of radar electromagnetic waves in concrete. According to the test fit curve, the accurate wave velocity and relative dielectric constant can be selected during detection and calculation of different parts of the mold bag slope protection, so as to accurately calculate the empty position and depth of the bottom of the mold bag concrete.
[0085] The basic parameters of the radar are set the same as those in the indoor test above. A PVC pad is placed on the surface of the wavy mold bag to assist in scanning. Then, the concrete moisture content meter calibrated in the indoor test above is used to test the moisture content at the trough of the mold bag. The wave velocity and relative dielectric constant of the part are found through the fitting curve above, and the thickness of the first and second layers is calculated to determine the specific location and depth of the steel bar position and the void.
[0086] According to the radar scanned images, 7 out of the 10 sections detected were found to have gaps. The scanned images without gaps have common features, see Figure 4 After filtering, the reflection waves from the top of the mold bag, the steel bar reflection waves and the bottom of the mold bag are clearly visible. The 7 voids found also have common image features, see Figure 5 (The dotted line marks the hollow area under the mold bag, and the maximum hollow depth under the mold bag is 26.7 cm). There is a clearly visible reflection interface below the reflected wave at the bottom of the mold bag. According to the above calculation method, its specific position can be calculated, and it can be inferred that there is a hollow at this location. After coring verification, the hollow position and depth are consistent with the calculation results of the ground penetrating radar scanning.
[0087] Example 2
[0088] The auxiliary dam of the reservoir adopts a simple mold bag slope protection, the internal filling is M20 mortar, the average thickness is 15cm, and a steel bar is inserted longitudinally in each bag. The indoor model test is carried out according to the aforementioned test steps, and the test results are shown in Table 2.
[0089] Table 2 Summary of indoor model test results of bag mortar
[0090]
[0091] According to the radar wave velocity υ obtained in Table 2 and the corresponding mortar moisture content w fitting curve, Figure 6 As shown, the fitting curve is υ=(-2.71189w+1.18028)×10 8 .
[0092] According to the fitting curve of the mortar dielectric constant and the corresponding mortar moisture content obtained in Table 2, Figure 7 As shown, the fitting curve is ε r =42.28778w+6.33171.
[0093] Figure 6 Figure 7 It is shown in the figure that the relationship between radar wave velocity and relative dielectric constant and the moisture content of mold bag mortar and the sum of squares of the residuals of the linear fitting curve are 0.00537 and 0.376 respectively, and the goodness of fit R 2 The smaller the sum of squares of the residuals of a set of data, the better the fit. The goodness of fit R 2 They are all close to 1, which also indicates a good degree of fit.
[0094] from Figure 6 Figure 7 It can be seen that the radar wave speed is linearly related to the relative dielectric constant of the mold bag mortar and the moisture content of the mold bag mortar. The fitting degree of the curve fit is better. The higher the moisture content of the mold bag mortar, the greater its relative dielectric constant, and the lower the propagation speed of the radar electromagnetic wave in the mold bag mortar. The on-site detection method is the same as Application Example 1. According to the test fit curve, the accurate wave speed and relative dielectric constant can be selected during detection and calculation of different parts of the mold bag slope protection, so as to accurately calculate the position of the steel bar in the mold bag and the depth of the mortar bottom. During on-site detection, the same as Example 1 also has obvious image characteristics. Figure 8 (The dotted line marks the hollow area under the mold bag, and the maximum hollow depth under the mold bag is 25.1 cm.) The hollow position and depth are consistent with the calculation results of the ground penetrating radar scanning after coring verification.
[0095] Example 1 The position of the steel bars and the bottom of the machine mold bag are detected by the method provided by the present invention, and the accuracy of the calculation results is verified by drilling the core. Application Example 2 The bottom of the simple mold bag mortar was tested by the method provided by the present invention, and the detection result was verified by drilling the core. Through the practical application of mold bag engineering inspection, it is verified that the method provided by the present invention can completely conduct non-destructive testing of the position of steel bars and the bottom of the mold bag, and provide scientific and accurate results.
[0096] As a non-destructive detection technology, radar method has the characteristics of convenience, high resolution, fast and efficient. According to the detection method provided by the present invention, the position and bottom of the steel bars of the mold bag slope protection project can be detected. After determining the moisture content, the relationship between the radar wave speed and relative dielectric constant and the moisture content of the mold bag mortar and the linear fitting curve of the radar mortar in Examples 1 and 2 can be calculated. After calculating the dielectric constant and the radar wave speed, the accurate position and depth can be calculated, so as to evaluate the overall quality of the mold bag project, so as to promptly deal with the mold bag project with hidden dangers, or take necessary preventive measures to avoid the occurrence of slope-off disasters.
Claims
1. A radar detection method for the position of steel bars and bottom emptying in a mold bag slope protection project, characterized by: The method comprises the following steps, and the following steps are performed in sequence: Step 1: Through the indoor mold bag slope protection model test, the mold bag moisture content and radar wave velocity fitting curve, and the mold bag moisture content and relative dielectric constant fitting curve are obtained; Step 2: Lay an auxiliary pad on the surface of the mold bag slope protection at the project site, and use radar electromagnetic wave scanning to obtain a radar scanning image; Step 3: Perform filtering preprocessing on the radar scan image obtained in step 2, remove the DC component of the signal, remove low-frequency interference and high-frequency noise, and determine the zero depth point, then perform filtering processing, use wavelet transform and KL transform to remove irrelevant signals, eliminate interference noise in the time dimension, and obtain an effective radar scan image; Step 4: The concrete moisture content at the target position of the effective radar scanning image is obtained by the indoor mold bag slope protection model test in step 1, and the radar wave velocity and relative dielectric constant at the target position are obtained by fitting curves of mold bag moisture content and radar wave velocity, and fitting curves of mold bag moisture content and relative dielectric constant; Step 5: By reading the two-way travel time t1 of the steel layer through the electromagnetic wave reflection data, the depth of the steel layer can be calculated; by reading the two-way travel time t2 of the void layer through the electromagnetic wave reflection data, the depth of the top of the void layer can be calculated.
2. The radar detection method for the position and bottom emptying of steel bars in a mold bag slope protection project according to claim 1 is characterized by: The specific steps of the indoor mold bag slope protection model test in step 1 are: ① Make a bracket with the same oblique support angle as the slope of the project site, lay the mold bag on the bracket, and the filling material in the mold bag is the same as the filling material in the mold bag used on the project site. At the same time, set up a comparison test piece, simulate the pouring process on the project site for pouring and drainage, and put it into the standard curing room after 24 hours; ② After curing, remove the mold bag cloth, grind the thickness to the same standard, test the radar propagation time in the concrete, and calculate the radar wave velocity and the relative dielectric constant of the concrete; ③ After the mold bag and the specimen are fully soaked, the saturated mass M1 of the core sample of the specimen is tested, and a portable concrete moisture content meter is used to test and correct the upper surface of the core sample; aluminum foil is laid on the lower surface of the mold bag as a reflection interface, and the propagation time t1 of the ground penetrating radar in the concrete is measured, the thickness h of the mold bag is measured, the propagation speed υ1 is calculated, and the relative dielectric constant ε of the concrete is calculated. r1 ; ④ Dry the mold bag and the specimen naturally, compare the constant weight of the specimen, and obtain the dry mass of the specimen M0; test and compare the mass of the specimen M every 6 to 10 hours. i and the propagation velocity of ground penetrating radar in bagged concrete i And calculate the relative dielectric constant ε of concrete ri ; ⑤Through the moisture content of concrete Where i is the number of tests; w i The moisture content of the i-th test; M i is the mass of the specimen in the i-th test; ⑥ The correlation formula is established by using the radar wave velocity υ and the corresponding concrete moisture content w, and the fitting curve is υ=(a1+b1×w)×10 8 ; In the formula, a1 is the intercept and b1 is the slope; The relative dielectric constant ε of concrete r The correlation formula is established with the corresponding concrete moisture content w, and the fitting curve is ε r =a2+b2×w, where a2 is the intercept and b2 is the slope.
3. The radar detection method for the position and bottom emptying of steel bars in a mold bag slope protection project according to claim 1 is characterized by: The auxiliary pad in step 2 is a polyvinyl chloride (PVC), polyethylene (PE) or polypropylene (PP) sheet, and has a width greater than that of the radar antenna or the radar integrated machine.
4. The radar detection method for the position and bottom emptying of steel bars in a mold bag slope protection project according to claim 1 is characterized by: The calculation method of the depth of the steel bar layer in step 5 is: The depth h1 of the steel bar layer is Where V1 is the propagation speed of radar electromagnetic waves in the steel bar layer, ε r1 is the relative dielectric constant of concrete, and x is the antenna receiving and transmitting distance.
5. The radar detection method for the position and bottom emptying of steel bars in a mold bag slope protection project according to claim 1 is characterized by: The calculation method of the top of the de-hollowing layer in step 5 is: The top depth of the de-hollowing layer h2 is V2 is the propagation speed of radar electromagnetic waves in the void layer, ε r2 is the relative dielectric constant of the hollow layer, and x is the antenna receiving and transmitting distance.