A kind of synthesis method of high molecular weight stearic acid polyoxyethylene ester

A two-step method with FeCl3/γ-Al2O3 and alkali metal catalysts addresses the inefficiencies in polyoxyethylene stearate synthesis, producing high molecular weight stearate with reduced impurities and improved properties.

CN116023645BActive Publication Date: 2024-12-03ZHEJIANG HUANGMA TECH CO LTD +3
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202211553630.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-12-06
Publication Date
2024-12-03
Estimated Expiration
2042-12-06

AI Technical Summary

Technical Problem

Existing methods for synthesizing polyoxyethylene stearate face challenges in determining the reaction end point, resulting in dark-colored products with high dioxane and polyethylene glycol content, and existing methods fail to address these issues effectively, leading to inefficiencies and inefficiencies in product quality and cost.

Method used

A two-step method using a supported solid acid catalyst FeCl3/γ-Al2O3 for catalytic reaction, followed by an alkali metal catalyst, to control the reaction conditions and reduce dioxane and polyethylene glycol content, ensuring stable product quality and light color.

Benefits of technology

The method produces high molecular weight polyoxyethylene stearate with reduced dioxane and polyethylene glycol content, achieving stable quality and improved emulsification, wetting, and thickening properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116023645B_ABST
    Figure CN116023645B_ABST
Patent Text Reader

Abstract

The invention discloses a synthesis method of high molecular weight stearic acid polyoxyethylene ester, and belongs to the technical field of polymer compound synthesis. The synthesis method first adds stearic acid and a supported solid acid catalyst to an autoclave, closes the autoclave, opens stirring and evacuates, evacuates after nitrogen is placed, heats up under vacuum conditions, dehydrates, adds ethylene oxide to react, discharges, filters, and obtains ethylene glycol monostearate; then adds ethylene glycol monostearate and an alkali metal catalyst to an autoclave, closes the autoclave, opens stirring and evacuates, evacuates after nitrogen is placed, heats up under vacuum conditions, dehydrates, adds ethylene oxide, matures, cools, degasses, neutralizes, discharges, and obtains stearic acid polyoxyethylene ester. The stearic acid polyoxyethylene ester product obtained by the method of the present invention has stable product quality and light color, and can effectively reduce the content of dioxane and polyethylene glycol in stearic acid polyoxyethylene ester.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of polymer compound synthesis, and in particular to a method for synthesizing high molecular weight polyoxyethylene stearate. Background Art

[0002] Polyoxyethylene stearate is an important surfactant with good emulsification, wetting and thickening properties, and has been widely used in many fields. For example, it is used as an emulsifier, solubilizer, suppository base, and ointment base in the pharmaceutical industry, as an emulsifier and detergent in the cosmetics industry, as a softener and antistatic agent in the textile industry, and as an emulsifying additive in the food industry. It can be seen that the industrial application prospects of polyoxyethylene stearate are very broad and have great development value.

[0003] At present, the method for preparing polyoxyethylene stearate in industry mainly includes esterification and ethoxylation. Among them, the reaction end point of esterification is difficult to determine when preparing polyoxyethylene stearate, so that the obtained product has a dark color, and the process of the method is complicated and the cost is high. Therefore, ethoxylation is generally used in industry to prepare polyoxyethylene stearate. Ethoxylation is to add stearic acid and an alkaline catalyst into a reactor, and react with ethylene oxide at a certain temperature to obtain polyoxyethylene stearate. Ethoxylation has the advantages of easy control of the end point, stable product quality, good color, etc., but the polyoxyethylene stearate prepared by the method has a high content of dioxane and polyethylene glycol polymer, and high content of dioxane and polyethylene glycol polymer greatly affects the use of the product. Summary of the invention

[0004] In order to overcome the shortcomings of the prior art, the purpose of the present invention is to provide a method for synthesizing high molecular weight polyoxyethylene stearate, the polyoxyethylene stearate product prepared by the method has stable quality and light color, and can effectively reduce the content of dioxane and polyethylene glycol in the polyoxyethylene stearate.

[0005] To solve the above problems, the technical solution adopted by the present invention is as follows:

[0006] A method for synthesizing high molecular weight polyoxyethylene stearate, comprising the following steps:

[0007] S1. Add stearic acid and supported solid acid catalyst FeCl3 / γ-Al2O3 into a high-pressure reactor, seal the reactor, start stirring and evacuate, replace nitrogen several times and then evacuate, heat to 60-90°C under vacuum, dehydrate for 1-2h, add ethylene oxide to react for 1-3h, discharge after the reaction, filter, and obtain ethylene glycol monostearate;

[0008] S2. Add ethylene glycol monostearate and alkali metal catalyst into a high-pressure reactor, seal the reactor, start stirring and evacuate, replace nitrogen several times and then evacuate, raise the temperature to 90-110°C under vacuum conditions, dehydrate for 1-2 hours, then raise the temperature to 100-140°C, add ethylene oxide, and mature until the pressure remains unchanged while maintaining the internal pressure of the reactor, cool, degas, neutralize, and discharge to obtain polyoxyethylene stearate.

[0009] As a preferred embodiment of the present invention, the weight of the supported solid acid catalyst FeCl3 / γ-Al2O3 is 0.05% to 0.1% of the theoretical weight of ethylene glycol monostearate.

[0010] As a preferred embodiment of the present invention, the weight of the alkali metal catalyst is 0.1% to 0.2% of the theoretical weight of polyoxyethylene stearate.

[0011] As a preferred embodiment of the present invention, the alkali metal catalyst is selected from one of KOH, NaOH, CH3OK or CH3ONa.

[0012] As a preferred embodiment of the present invention, the number of times of adding nitrogen in steps S1 and S2 is 2 to 5 times.

[0013] As a preferred embodiment of the present invention, the molar ratio of stearic acid to ethylene oxide in step S1 is 1:1.1.

[0014] As a preferred embodiment of the present invention, the molar ratio of ethylene glycol monostearate to ethylene oxide in step S2 is 1:39-99.

[0015] As a preferred embodiment of the present invention, the polymerization time of step S1 is 1 to 2 hours.

[0016] As a preferred embodiment of the present invention, in step S2, the ethylene oxide is added within 1 to 4 hours, and the reaction pressure is maintained below 0.4 MPa.

[0017] As a preferred embodiment of the present invention, the molecular weight of the high molecular weight polyoxyethylene stearate is 2027-4667 g / mol.

[0018] Compared with the prior art, the present invention has the following beneficial effects:

[0019] The present invention adopts a two-step method to prepare polyoxyethylene stearate, and uses a supported solid acid catalyst FeCl3 / γ-Al2O3 for catalytic reaction. The catalyst can directly activate epoxy monomers, and the activated monomers react with an initiator. No moisture is generated during the process, and the reaction reacts in the pores of the catalyst, effectively preventing the epoxy monomers from "biting tail" reaction, and the dioxane content decreases. Therefore, the catalyst can effectively prevent the generation of dioxane and moisture in the reaction, thereby significantly reducing the content of dioxane and polyethylene glycol in the product, making the obtained polyoxyethylene stearate product stable in quality, light in color, and having good emulsification, wetting, and thickening properties, and can be widely used in the fields of pharmacy and textiles. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 This is a product photo of polyoxyethylene stearate prepared in Example 6 of the present invention (60° C.);

[0021] Figure 2 This is a product photo (60° C.) of polyoxyethylene stearate prepared in Comparative Example 6 of the present invention. DETAILED DESCRIPTION

[0022] The present invention is further described in detail below in conjunction with specific implementation modes.

[0023] Example 1

[0024] A method for synthesizing high molecular weight polyoxyethylene stearate, comprising the following steps:

[0025] S1. Synthesis of ethylene glycol monostearate: First, add 534g of stearic acid and 0.32g of FeCl3 / γ-Al2O3 catalyst into a 2.5L autoclave, seal the autoclave, start stirring and evacuate, and then replace the gas in the autoclave with nitrogen three times. After nitrogen is replaced, heat to 90°C, add 106g of ethylene oxide dropwise, control the reaction temperature to 90±2°C, and the reaction pressure to 0-0.05MPa. After addition, ripen for 0.5h, degas, and finally cool to 60°C to discharge, and filter to remove the catalyst.

[0026] S2. Synthesis of polyoxyethylene stearate 2027: First, 240 g of ethylene glycol monostearate and 1.52 g of KOH catalyst were added into a 2.5 L autoclave, the autoclave was sealed, stirring was started and vacuum was evacuated, then the gas in the autoclave was replaced with nitrogen three times, the temperature was raised to 140° C., 1280 g of ethylene oxide was added dropwise, the reaction temperature was controlled to 140±2° C., and the reaction pressure was controlled to 0-0.4 MPa. After the addition, the mixture was aged for 0.5 h, degassed, neutralized with acetic acid, cooled to 80° C. and discharged to obtain polyoxyethylene stearate.

[0027] Example 2

[0028] A method for synthesizing high molecular weight polyoxyethylene stearate, comprising the following steps:

[0029] S1. Synthesis of ethylene glycol monostearate: First, add 534g of stearic acid and 0.51g of FeCl3 / γ-Al2O3 catalyst into a 2.5L autoclave, seal the autoclave, start stirring and evacuate, and then replace the gas in the autoclave with nitrogen three times. After nitrogen is replaced, heat to 75°C, add 106g of ethylene oxide dropwise, control the reaction temperature to 75±2°C, and the reaction pressure to 0-0.05MPa. After addition, ripen for 0.5h, degas, and finally cool to 60°C to discharge the material, and filter to remove the catalyst.

[0030] S2. Synthesis of polyoxyethylene stearate 2027: First, 240 g of ethylene glycol monostearate and 2.74 g of KOH catalyst were added into a 2.5 L autoclave, the autoclave was sealed, stirring was started and vacuum was evacuated, then the gas in the autoclave was replaced with nitrogen three times, the temperature was raised to 120° C., 1280 g of ethylene oxide was added dropwise, the reaction temperature was controlled to be 120±2° C., and the reaction pressure was 0-0.4 MPa. After the addition, the mixture was aged for 0.5 h, degassed, neutralized with acetic acid, cooled to 80° C. and discharged to obtain polyoxyethylene stearate.

[0031] Example 3

[0032] A method for synthesizing high molecular weight polyoxyethylene stearate, comprising the following steps:

[0033] S1. Synthesis of ethylene glycol monostearate: First, add 534g of stearic acid and 0.64g of FeCl3 / γ-Al2O3 catalyst into a 2.5L autoclave, seal the autoclave, start stirring and evacuate, then replace the gas in the autoclave with nitrogen three times. After nitrogen is replaced, heat to 60°C, add 106g of ethylene oxide dropwise, control the reaction temperature to 60±2°C, and the reaction pressure to 0-0.05MPa. After addition, ripen for 0.5h, degas, discharge, and filter to remove the catalyst.

[0034] S2. Synthesis of polyoxyethylene stearate 2027: First, 240 g of ethylene glycol monostearate and 3.04 g of KOH catalyst were added to a 2.5 L autoclave, the autoclave was sealed, stirring was started and vacuum was evacuated, then the gas in the autoclave was replaced with nitrogen three times, the temperature was raised to 100 ° C, 1280 g of ethylene oxide was added dropwise, the reaction temperature was controlled to be 100 ± 2 ° C, and the reaction pressure was 0-0.4 MPa. After the addition, it was aged for 0.5 h, degassed, neutralized with acetic acid, cooled to 80 ° C and discharged to obtain polyoxyethylene stearate.

[0035] Example 4

[0036] A method for synthesizing high molecular weight polyoxyethylene stearate, comprising the following steps:

[0037] S1. Synthesis of ethylene glycol monostearate: First, add 534g of stearic acid and 0.32g of FeCl3 / γ-Al2O3 catalyst into a 2.5L autoclave, seal the autoclave, start stirring and evacuate, and then replace the gas in the autoclave with nitrogen three times. After nitrogen is replaced, heat to 60°C, add 106g of ethylene oxide dropwise, control the reaction temperature to 90°C, and the reaction pressure to 0-0.05MPa. After addition, ripen for 0.5h, degas, and finally cool to 60°C to discharge the material, and filter to remove the catalyst.

[0038] S2. Synthesis of polyoxyethylene stearate 2907: First, 160 g of ethylene glycol monostearate and 1.45 g of KOH catalyst were added to a 2.5 L autoclave, the autoclave was sealed, stirring was started and vacuum was evacuated, then the gas in the autoclave was replaced with nitrogen three times, the temperature was raised to 140° C., 1293 g of ethylene oxide was added dropwise, the reaction temperature was controlled to be 140° C., the reaction pressure was 0-0.4 MPa, and after the addition, the mixture was aged for 0.5 h, degassed, neutralized with acetic acid, and finally cooled to 80° C. to discharge the mixture to obtain polyoxyethylene stearate.

[0039] Example 5

[0040] A method for synthesizing high molecular weight polyoxyethylene stearate, comprising the following steps:

[0041] S1. Synthesis of ethylene glycol monostearate: the steps and conditions are the same as those in Example 4.

[0042] S2. Synthesis of polyoxyethylene stearate 3787: First, 160 g of ethylene glycol monostearate and 1.89 g of KOH catalyst were added to a 2.5 L autoclave, the autoclave was sealed, stirring was started and vacuum was evacuated, then the gas in the autoclave was replaced with nitrogen three times, the temperature was raised to 140° C., 1733 g of ethylene oxide was added dropwise, the reaction temperature was controlled to be 140° C., the reaction pressure was 0-0.4 MPa, and after the addition, the mixture was aged for 0.5 h, degassed, neutralized with acetic acid, and finally cooled to 80° C. to discharge the material to obtain polyoxyethylene stearate.

[0043] Example 6

[0044] A method for synthesizing high molecular weight polyoxyethylene stearate, comprising the following steps:

[0045] S1. Synthesis of ethylene glycol monostearate: the steps and conditions are the same as those in Example 4.

[0046] S2. Synthesis of polyoxyethylene stearate 4667: First, 104 g of ethylene glycol monostearate and 1.56 g of KOH catalyst were added to a 2.5 L autoclave, the autoclave was sealed, stirring was started and vacuum was evacuated, then the gas in the autoclave was replaced with nitrogen three times, the temperature was raised to 140° C., 1452 g of ethylene oxide was added dropwise, the reaction temperature was controlled at 140° C., the reaction pressure was 0-0.4 MPa, and after the addition, the mixture was aged for 0.5 h, degassed, neutralized with acetic acid, and finally cooled to 80° C. to discharge the mixture to obtain polyoxyethylene stearate.

[0047] The process parameters of Examples 1 to 6 are compared as shown in Table 1:

[0048] Table 1 Process parameters of Examples 1 to 6

[0049]

[0050]

[0051] Comparative Examples 1 to 6

[0052] The difference between Comparative Examples 1 to 6 and Examples 1 to 6 is that the supported solid catalyst FeCl3 / γ-Al2O3 in S1 of Examples 1 to 6 is replaced with an alkaline metal catalyst KOH; the catalyst dosage, reaction temperature and pressure are the same as those of Examples 1 to 6, and other conditions remain unchanged.

[0053] The process parameters of Comparative Examples 1 to 6 are shown in Table 2:

[0054] Table 2 Process parameters of comparative examples 1 to 6

[0055]

[0056] Comparative Example 7

[0057] A synthesis method of polyoxyethylene stearate 2027 comprises the following steps: firstly, 200g of stearic acid and 1.52g of KOH catalyst are added into a 2.5L high-pressure reactor, the reactor is sealed, stirring is started and vacuum is drawn, then the gas in the reactor is replaced with nitrogen for 3 times, the temperature is raised to 140°C, 1318g of ethylene oxide is added dropwise, the reaction temperature is controlled to be 140±2°C, the reaction pressure is controlled to be 0-0.4MPa, and after the addition, the reaction is aged for 0.5h, degassed, neutralized with acetic acid, cooled to 80°C and discharged to obtain polyoxyethylene stearate.

[0058] Comparative Examples 8 to 9

[0059] The difference between Comparative Examples 8 and 9 and Comparative Example 7 is that the reaction temperatures are 120° C. and 100° C., respectively, and the amounts of catalyst used are 0.18% and 0.2%, respectively. Other conditions are the same as those of Comparative Example 7.

[0060] Comparative Example 10

[0061] A method for synthesizing polyoxyethylene stearate 2907 comprises the following steps: firstly, adding 140g of stearic acid and 1.52g of KOH catalyst into a 2.5L high-pressure reactor, sealing the reactor, stirring and vacuumizing, then replacing the gas in the reactor with nitrogen for 3 times, heating to 140°C, dropwise adding 1384g of ethylene oxide, controlling the reaction temperature to 140°C and the reaction pressure to 0-0.4MPa, aging for 0.5h after the addition, degassing, neutralizing with acetic acid, and finally cooling to 80°C and discharging to obtain polyoxyethylene stearate.

[0062] Comparative Example 11

[0063] A method for synthesizing polyoxyethylene stearate 2907 comprises the following steps: firstly, adding 134g of stearic acid and 1.9g of KOH catalyst into a 2.5L high-pressure reactor, sealing the reactor, stirring and vacuumizing, then replacing the gas in the reactor with nitrogen for 3 times, heating to 140°C, dropwise adding 1767g of ethylene oxide, controlling the reaction temperature to 140°C and the reaction pressure to 0-0.4MPa, aging for 0.5h after the addition, degassing, neutralizing with acetic acid, and finally cooling to 80°C and discharging to obtain polyoxyethylene stearate.

[0064] Comparative Example 12

[0065] A synthesis method of polyoxyethylene stearate 4667 comprises the following steps: firstly, adding 89g of stearic acid and 1.46g of KOH catalyst into a 2.5L high-pressure reactor, sealing the reactor, stirring and evacuating, then replacing the gas in the reactor with nitrogen for 3 times, heating to 140°C, dropwise adding 1367g of ethylene oxide, controlling the reaction temperature to 140°C and the reaction pressure to 0-0.4MPa, aging for 0.5h after the addition, degassing, neutralizing with acetic acid, and finally cooling to 80°C and discharging to obtain polyoxyethylene stearate.

[0066] The process parameter comparison of Comparative Examples 7 to 12 is shown in Table 3:

[0067] Table 3 Process parameters of comparative examples 7 to 12

[0068] Comparative Example Catalyst dosage % Reaction temperature℃ Number of EO moles in the product molecule 7 0.10 140 40 8 0.18 120 40 9 0.20 100 40 10 0.10 140 60 11 0.10 140 80 12 0.10 140 100

[0069] Effect verification experiment:

[0070] The appearance, dioxane content, and polymer content of the stearic acid polyoxyethylene ethers obtained in Examples 1 to 6 and Comparative Examples 1 to 12 were tested. The test results are shown in Tables 4 and Figure 1-2 .

[0071] Table 4 Comparison of product performance obtained in Examples 1 to 6 and Comparative Examples 1 to 12

[0072] project Dioxane content / ppm Polyethylene glycol content / % Example 1 12 0.6 Comparative Example 1 87 3.7 Comparative Example 7 153 6.9 Example 2 8 0.5 Comparative Example 2 65 3.1 Comparative Example 8 129 5.8 Example 3 3 0.4 Comparative Example 3 42 2.6 Comparative Example 9 95 4.9 Example 4 11 0.7 Comparative Example 4 86 4.0 Comparative Example 10 162 7.2 Example 5 13 0.9 Comparative Example 5 85 4.8 Comparative Example 11 149 7.7 Example 6 12 1.0 Comparative Example 6 88 5.3 Comparative Example 12 151 8.2

[0073] It can be seen from Table 4 that the stearic acid polyoxyethylene ether prepared by the two-step method of the present invention has a clearer appearance (60°C), a lower dioxane content and a lower polymer content, the stearic acid polyoxyethylene ether prepared at a lower temperature has a clearer appearance (60°C), a lower dioxane content and a lower polymer content, and the stearic acid polyoxyethylene ether prepared by the two-step method and the first step using the supported catalyst FeCl3 / γ-Al2O3 has a clear appearance (60°C), and the dioxane content and the polymer content are the lowest. Figure 1 and Figure 2 The product appearance diagrams of Example 6 and Comparative Example 6 are shown in FIG. Figure 1 and Figure 2 It can be seen that Example 6 using the supported solid acid catalyst FeCl3 / γ-Al2O3 greatly improves the clarity of the product compared to Comparative Example 6 using the traditional alkaline metal catalyst KOH.

[0074] Therefore, the present invention adopts a two-step method, and the stearic acid polyoxyethylene ether prepared in the first step using the supported catalyst FeCl3 / γ-Al2O3 has qualified indicators and stable quality.

[0075] The above-mentioned embodiments are only preferred embodiments of the present invention and cannot be used to limit the scope of protection of the present invention. Any non-substantial changes and substitutions made by technicians in this field on the basis of the present invention shall fall within the scope of protection required by the present invention.

Claims

1. A method for synthesizing high molecular weight polyoxyethylene stearate, Features: The following steps are involved: S1, stearic acid and supported solid acid catalyst FeCl 3 / γ-Al 2 O 3 Add to the high-pressure reactor, close the reactor, start stirring and evacuate, replace nitrogen several times and then evacuate, heat to 60-90°C under vacuum conditions, dehydrate for 1-2h, add ethylene oxide to react for 1-3h, discharge after the reaction, filter, and obtain ethylene glycol monostearate; wherein, the supported solid acid catalyst FeCl 3 / γ-Al 2 O 3 The weight is 0.05% to 0.1% of the theoretical weight of ethylene glycol monostearate; S2. Add ethylene glycol monostearate and an alkali metal catalyst into a high-pressure reactor, seal the reactor, start stirring and evacuate, replace nitrogen several times and then evacuate, raise the temperature to 90-110°C under vacuum conditions, dehydrate for 1-2 hours and then raise the temperature to 100-140°C, add ethylene oxide, and while maintaining the internal pressure of the reactor, ripen until the pressure remains unchanged, cool, degas, neutralize, and discharge to obtain polyoxyethylene stearate; wherein the weight of the alkali metal catalyst is 0.1%-0.2% of the theoretical weight of polyoxyethylene stearate.

2. The method for synthesizing high molecular weight polyoxyethylene stearate according to claim 1, Features: The alkali metal catalyst is selected from KOH, NaOH, CH 3 OK or CH 3 One of ONa.

3. The synthetic method of high molecular weight polyoxyethylene stearate according to claim 1, Features: The number of times of adding nitrogen in steps S1 and S2 is 2 to 5 times.

4. The method for synthesizing high molecular weight polyoxyethylene stearate according to claim 1, Features: In step S1, the molar ratio of stearic acid to ethylene oxide is 1:1.

1.

5. The method for synthesizing high molecular weight polyoxyethylene stearate according to claim 1, Features: In step S2, the molar ratio of ethylene glycol monostearate to ethylene oxide is 1:39-99.

6. The method for synthesizing high molecular weight polyoxyethylene stearate according to claim 1, Features: The polymerization time of step S1 is 1-2 hours.

7. The method for synthesizing high molecular weight polyoxyethylene stearate according to claim 1, Features: In step S2, the ethylene oxide is added within 1 to 4 hours, and the reaction pressure is maintained below 0.4 MPa.

8. The method for synthesizing high molecular weight polyoxyethylene stearate according to claim 1, Features: The molecular weight of the high molecular weight polyoxyethylene stearate is 2027-4667 g / mol.

Citation Information

Patent Citations

  • Preparation method of catalyst for ethylene polymerization or copolymerization

    CN103694384A

  • Polyethylene glycol fatty acid ester and preparation method thereof

    CN108102083A