A polymer thickener and preparation method thereof
By designing a device with a stirring, filtering and drying structure, the problem of inconvenient processing after cooling during the preparation of polymer thickeners is solved, rapid drying and modification of polymer powder is achieved, dispersion performance and dissolution speed are improved, and it is suitable for industry Production.
Patent Information
- Application Number
- CN202310705415.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-14
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2043-06-14
Smart Images

Figure CN116672991B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of polymer thickener preparation, in particular to a polymer thickener and a preparation method thereof. Background Art
[0002] Polymer thickeners are additives that can increase the viscosity of liquids and make them thicker. Polymer thickeners are usually high molecular weight compounds, such as polyacrylamide (PAM). They can form viscous gels in water and are often used in oil field exploitation, wastewater treatment, pulp and paper industry and other fields. At the same time, polymer thickeners are also widely used in daily necessities such as personal care and cosmetics to increase their viscosity and texture. However, the existing polymer thickener preparation device cannot be conveniently cooled, filtered and dried during use, making the processing and preparation inconvenient, so a device is needed to solve the above problems. Summary of the invention
[0003] The object of the present invention is to provide a polymer thickener and a preparation method thereof to solve the problems raised in the above background technology.
[0004] To achieve the above object, the present invention provides the following technical solutions:
[0005] A polymer thickener and a preparation method thereof, comprising a stirring and filtering structure, a discharge pipe, an electric control valve, a processing reaction box, a fixed mounting frame, a first electric push rod, a mounting frame, a mounting trough, a sliding limit hole and a drying treatment structure, wherein three discharge pipes are provided, and the three discharge pipes are evenly fixedly connected to the bottom end of the processing reaction box, three electric control valves are provided, and the three electric control valves are respectively fixedly installed on the three discharge pipes, the stirring and filtering structure is arranged at the middle of the upper end of the processing reaction box, and six mounting frames are provided, and the six mounting frames are evenly fixedly distributed on the upper end of the processing reaction box;
[0006] The sliding limit holes are symmetrically arranged on the installation frame, the installation slot is arranged inside the installation frame, the drying processing structure is arranged inside the installation slot, six fixed installation frames are arranged, and the six fixed installation frames are evenly fixedly installed on the outside of the installation frame, and the first electric push rod is symmetrically fixedly installed on the fixed installation frame;
[0007] The drying treatment structure comprises a fixed mounting bolt, a fixed limiting frame and a dryer, wherein the fixed limiting frame is arranged in an L shape, and the dryer is fixedly mounted at the middle part of the bottom end of the fixed limiting frame by means of the fixed mounting bolt;
[0008] The stirring and filtering structure comprises a lifting control body and a rotating filtering body, wherein the lifting control body is arranged at the upper end of the rotating filtering body;
[0009] The rotating filter body comprises a driving rod, a limit lifting column, a filter plate, a limit mounting frame and a rotating stirring wheel, six limit lifting columns are provided, and the six limit lifting columns are evenly distributed on the limit mounting frame in a ring shape, the filter plate is fixedly mounted inside the limit mounting frame, the rotating stirring wheel is rotatably mounted in the middle of the filter plate, and the bottom end of the driving rod is fixedly connected to the middle of the upper end of the rotating stirring wheel;
[0010] The lifting control body includes a motor, a fixedly connected cross column, a lifting adjustment disk, a second electric push rod and a limit snap ring, the second electric push rod is provided with six, and the six second electric push rods are evenly distributed in a ring shape, the lifting adjustment disk is fixedly connected to the upper end of the second electric push rod, the fixedly connected cross column is evenly rotatably installed inside the lifting adjustment disk, the motor is fixedly installed in the middle of the lifting adjustment disk, and the limit snap ring is located below the lifting adjustment disk;
[0011] The processing reaction box is arranged in a hexagonal prism shape, the filter plate and the limiting mounting frame are arranged in a hexagonal prism shape, the rotating stirring wheel is located in the middle of the filter plate, and the rotating stirring wheel is located in the middle of the processing reaction box, and the discharge pipe is connected to the interior of the processing reaction box.
[0012] Preferably, the fixed mounting bracket is fixedly mounted on the mounting frame.
[0013] Preferably, the driving end of the first electric push rod is slidably inserted into the sliding limit hole.
[0014] Preferably, the fixed limiting frame and the dryer are arranged inside the installation slot, and the driving end of the first electric push rod is fixedly connected to the fixed limiting frame.
[0015] Preferably, the limiting clamp ring is fixedly mounted on the upper end of the processing reaction box, and the bottom end of the second electric push rod is fixedly connected to the upper end of the mounting frame.
[0016] Preferably, the driving end of the motor is fixedly connected to the driving rod, and the position-limiting lifting column passes through and is slidably clamped inside the position-limiting clamp ring.
[0017] Preferably, the fixed mounting frame is arranged in a U shape.
[0018] Preferably, temperature sensors are evenly and fixedly installed inside the upper end of the processing reaction box.
[0019] A method for preparing a polymer thickener comprises the following steps:
[0020] a. First, petroleum ether with a boiling point of 60-90°C is placed inside the processing reaction box, and then polyacrylamide powder with a hydrolysis degree of 20-45%, n-octanol and organic acid are added in sequence, and heated, stirred and refluxed to react until the reaction is completed;
[0021] b. Filter after cooling, and then dry for 3 to 5 hours in a vacuum environment at 110 to 120°C to obtain polymer powder;
[0022] c. Place the polymer powder in paraffin oil at a mass ratio of 1:(2-4), and obtain a self-suspending polymer thickener by stirring and dispersing.
[0023] Preferably, the raw materials of the polymer thickener include, by weight: 800-1000 parts of petroleum ether, 5-10 parts of n-octanol, and 1-3 parts of organic acid, wherein the organic acid is a mixture of benzenesulfonic acid and trifluoroacetic acid in a mass ratio of 2:1.
[0024] Compared with the prior art, the present invention has the following beneficial effects:
[0025] 1. The present invention can conveniently and quickly adjust and control the temperature in the processing reaction box through the provided drying treatment structure, and can mix and filter the material in the processing reaction box through the provided stirring and filtering structure, so that the material in the processing reaction box can be conveniently and quickly dried to obtain the modified polymer powder.
[0026] Second, the temperature sensor provided in the present invention can conveniently detect the temperature inside the processing reaction box in real time, so that the temperature inside the processing reaction box meets the requirements, and the temperature control and adjustment are convenient.
[0027] 3. The polymer thickener prepared by the present invention has good dispersibility, fast dissolution speed, and a small amount of suspension aid added, which will not cause adverse effects on the properties of fracturing fluid residue, backflow, etc.; at the same time, the process of the present invention is simple, the production efficiency is high, the cost is low, and it is suitable for large-scale industrial production. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.
[0029] Figure 1 It is a schematic diagram of the main three-dimensional structure of the present invention;
[0030] Figure 2 It is a schematic diagram of the main body of the present invention from a top view of a three-dimensional structure;
[0031] Figure 3 It is a structural schematic diagram of the installation frame of the present invention;
[0032] Figure 4 It is a schematic diagram of the upper structure of the processing reaction box of the present invention;
[0033] Figure 5 The upper end internal structure schematic diagram of the processing reaction box of the present invention;
[0034] Figure 6 It is a structural schematic diagram of the drying treatment structure of the present invention;
[0035] Figure 7 It is a structural schematic diagram of the stirring and filtering structure of the present invention;
[0036] Figure 8 It is a structural schematic diagram of the rotary filter body of the present invention;
[0037] Fig. 9 It is a structural schematic diagram of the lifting control body of the present invention;
[0038] Fig.10 It is a schematic structural diagram of a second embodiment of a processing reaction box of the present invention.
[0039] In the figure: 1- stirring and filtering structure, 2- discharge pipe, 3- electric control valve, 4- processing reaction box, 5- fixed mounting frame, 6- first electric push rod, 7- mounting frame, 8- mounting trough, 9- sliding limit hole, 10- fixed mounting bolt, 11- fixed limit frame, 12- drying machine, 13- drying treatment structure, 14- lifting control body, 15- rotating filter body, 16- driving rod, 17- limiting lifting column, 18- filtering plate, 19- limiting mounting frame, 20- rotating stirring wheel, 21- motor, 22- fixed connecting horizontal column, 23- lifting adjustment disk, 24- second electric push rod, 25- limiting clamp ring, 26- temperature sensor. DETAILED DESCRIPTION
[0040] The present invention is further described below in conjunction with the accompanying drawings.
[0041] Example 1
[0042] A method for preparing a polymer thickener comprises the following steps:
[0043] a. First, place petroleum ether with a boiling point of 60°C in the processing reaction box, then add polyacrylamide powder with a hydrolysis degree of 20%, n-octanol and organic acid in sequence, heat, stir and reflux to react until the reaction is completed;
[0044] b. Filter after cooling, and then dry at 110°C in a vacuum environment for 3 hours to obtain polymer powder;
[0045] c. Place the polymer powder in paraffin oil at a mass ratio of 1:2, and obtain a self-suspending polymer thickener by stirring and dispersing.
[0046] The raw materials of the polymer thickener include, by weight: 800 parts of petroleum ether, 5 parts of n-octanol, and 1 part of organic acid, wherein the organic acid is a mixture of benzenesulfonic acid and trifluoroacetic acid in a mass ratio of 2:1.
[0047] Example 2
[0048] A method for preparing a polymer thickener comprises the following steps:
[0049] a. First, petroleum ether with a boiling point of 70°C is placed inside the processing reaction box, and then polyacrylamide powder with a hydrolysis degree of 35%, n-octanol and organic acid are added in sequence, and heated, stirred and refluxed to react until the reaction is completed;
[0050] b. Filter after cooling, and then dry at 115°C in a vacuum environment for 4 hours to obtain polymer powder;
[0051] c. Place the polymer powder in paraffin oil at a mass ratio of 1:3, and obtain a self-suspending polymer thickener by stirring and dispersing.
[0052] The raw materials of the polymer thickener include, by weight: 900 parts of petroleum ether, 7 parts of n-octanol, and 2 parts of organic acid, wherein the organic acid is a mixture of benzenesulfonic acid and trifluoroacetic acid in a mass ratio of 2:1.
[0053] Example 3
[0054] A method for preparing a polymer thickener comprises the following steps:
[0055] a. First, petroleum ether with a boiling point of 90°C is placed inside the processing reaction box, and then polyacrylamide powder with a hydrolysis degree of 45%, n-octanol and organic acid are added in sequence, and heated, stirred and refluxed to react until the reaction is completed;
[0056] b. Filter after cooling, and then dry at 120°C in a vacuum environment for 5 hours to obtain polymer powder;
[0057] c. Place the polymer powder in paraffin oil at a mass ratio of 1:4, and disperse by stirring to obtain a self-suspending polymer thickener.
[0058] The raw materials of the polymer thickener include, by weight: 1000 parts of petroleum ether, 10 parts of n-octanol, and 3 parts of organic acid, wherein the organic acid is a mixture of benzenesulfonic acid and trifluoroacetic acid in a mass ratio of 2:1.
[0059] Based on Examples 1 to 3, it can be concluded that the polymer thickener prepared by the present invention has good dispersibility, fast dissolution speed, and a small amount of suspending agent added, which will not cause adverse effects on the properties of fracturing fluid residue, backflow, etc.; at the same time, the process of the present invention is simple, the production efficiency is high, the cost is low, and it is suitable for large-scale industrial production.
[0060] Example 4
[0061] See also Figure 1 , Figure 2 , Figure 3 , Figure 4 and Figure 5 , an embodiment of the present invention: a polymer thickener and a preparation method thereof, comprising a stirring and filtering structure 1, a discharge pipe 2, an electric control valve 3, a processing reaction box 4, a fixed mounting frame 5, a first electric push rod 6, a mounting frame 7, a mounting trough 8, a sliding limit hole 9 and a drying treatment structure 13, wherein three discharge pipes 2 are provided, and the three discharge pipes 2 are evenly fixedly connected to the bottom end of the processing reaction box 4, three electric control valves 3 are provided, and the three electric control valves 3 are respectively fixedly installed on the three discharge pipes 2, the stirring and filtering structure 1 is arranged in the middle of the upper end of the processing reaction box 4, six mounting frames 7 are provided, and the six mounting frames 7 are evenly fixedly distributed at the upper end of the processing reaction box 4, and the sliding limit The position holes 9 are symmetrically opened on the installation frame 7, the installation slot 8 is opened inside the installation frame 7, the drying processing structure 13 is arranged inside the installation slot 8, six fixed mounting frames 5 are arranged, and the six fixed mounting frames 5 are evenly fixedly installed on the outside of the installation frame 7, and the first electric push rod 6 is symmetrically fixedly installed on the fixed mounting frame 5. The temperature in the processing reaction box 4 can be conveniently and quickly adjusted and controlled by the set drying processing structure 13, and the material body in the processing reaction box 4 can be mixed and filtered by the set stirring and filtering structure 1, so that the material body in the processing reaction box 4 can be conveniently and quickly dried to obtain the modified polymer powder;
[0062] See also Figure 6 The drying treatment structure 13 includes a fixed mounting bolt 10, a fixed limiting frame 11 and a dryer 12. The fixed limiting frame 11 is arranged in an L shape. The dryer 12 is fixedly mounted at the middle of the bottom end of the fixed limiting frame 11 by the fixed mounting bolt 10. The dryer 12 plays an effective role in temperature regulation.
[0063] See also Figure 7 and Figure 8The stirring and filtering structure 1 includes a lifting control body 14 and a rotating filtering body 15. The lifting control body 14 is arranged at the upper end of the rotating filtering body 15. The rotating filtering body 15 includes a driving rod 16, a limit lifting column 17, a filter plate 18, a limit mounting frame 19 and a rotating stirring wheel 20. There are six limit lifting columns 17, and the six limit lifting columns 17 are evenly distributed on the limit mounting frame 19 in a ring shape. The filter plate 18 is fixedly installed inside the limit mounting frame 19, and the rotating stirring wheel 20 is rotatably installed in the middle of the filter plate 18. The bottom end of the driving rod 16 is fixedly connected to the middle of the upper end of the rotating stirring wheel 20. The starting motor 21 drives the driving rod 16 to rotate forward and reversely, which can drive the rotating stirring wheel 20 to rotate forward and reversely, so that various materials in the processing reaction box 4 can be mixed conveniently and quickly;
[0064] See also Fig. 9 The lifting control body 14 includes a motor 21, a fixedly connected cross column 22, a lifting adjustment disk 23, a second electric push rod 24 and a limit snap ring 25. The second electric push rod 24 is provided with six, and the six second electric push rods 24 are evenly distributed in a ring shape. The lifting adjustment disk 23 is fixedly connected to the upper end of the second electric push rod 24, and the fixedly connected cross column 22 is evenly rotated and installed inside the lifting adjustment disk 23. The motor 21 is fixedly installed in the middle of the lifting adjustment disk 23. The limit snap ring 25 is located below the lifting adjustment disk 23. The lifting adjustment disk 23 can be lifted upward by the second electric push rod 24. At this time, the lifting adjustment disk 23 lifted upward can lift the limit installation frame 19 and the filter plate 18 through the limit lifting column 17;
[0065] The processing reaction box 4 is arranged in a hexagonal prism shape, the filter plate 18 and the limiting mounting frame 19 are both arranged in a hexagonal prism shape, the rotating stirring wheel 20 is located in the middle of the filter plate 18, and the rotating stirring wheel 20 is located in the middle of the processing reaction box 4, and the discharge pipe 2 is connected to the interior of the processing reaction box 4, and the liquid in the processing reaction box 4 can be discharged through the discharge pipe 2.
[0066] The fixed mounting frame 5 is fixedly mounted on the mounting frame 7 to play a role of fixed mounting.
[0067] The driving end of the first electric push rod 6 is slidably inserted into the sliding limit hole 9, so that the driving end of the first electric push rod 6 can move stably.
[0068] The fixed limiting frame 11 and the dryer 12 are arranged inside the mounting groove 8 , and the driving end of the first electric push rod 6 is fixedly connected to the fixed limiting frame 11 , and the movement of the fixed limiting frame 11 can be controlled by the first electric push rod 6 .
[0069] The limiting clamp ring 25 is fixedly mounted on the upper end of the processing reaction box 4 , and the bottom end of the second electric push rod 24 is fixedly connected to the upper end of the mounting frame 7 . The lifting and lowering of the lifting adjustment disk 23 can be controlled by the second electric push rod 24 .
[0070] The driving end of the motor 21 is fixedly connected to the driving rod 16 , and the position-limiting lifting column 17 penetrates and is slidably engaged in the interior of the position-limiting clamp ring 25 to play a role of position limiting.
[0071] The fixed installation frame 5 is arranged in a U shape, and plays a role of fixed installation.
[0072] When this embodiment is implemented, the motor 21 is started to drive the driving rod 16 to rotate forward and backward, which can drive the rotating stirring wheel 20 to rotate forward and backward, so that various materials in the processing reaction box 4 can be mixed conveniently and quickly. After mixing, the second electric push rod 24 is started, and the lifting and adjusting disk 23 can be lifted upward by the second electric push rod 24. At this time, the lifting and adjusting disk 23 lifted upward can lift the limiting installation frame 19 and the filter plate 18 through the limiting lifting column 17, and then the electric control valve 3 is started to open the discharge pipe 2. At this time, the liquid in the processing reaction box 4 can flow out quickly. At this time, the first electric push rod 6 is started, and the six fixed limiting frames 11 drive the dryers 12 to move and discharge from the inside of the installation slot 8 through the first electric push rod 6, and then three of the six dryers 12 are controlled to blow out natural wind to quickly cool down the inside of the processing reaction box 4. After cooling, the other three dryers 12 are started to blow out hot air to heat and control the temperature in the processing reaction box 4 again, so that the material filtered and intercepted by the filter plate 18 is quickly dried to obtain the required material.
[0073] Example 5
[0074] On the basis of Example 4, Fig.10 As shown, temperature sensors 26 are evenly and fixedly installed inside the upper end of the processing reaction box 4.
[0075] When this embodiment is implemented, the temperature sensor 26 can be used to conveniently detect the temperature inside the processing reaction box 4 in real time, so that the temperature inside the processing reaction box 4 meets the requirements, and the temperature can be easily controlled and adjusted.
[0076] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A preparation device for a polymer thickener, comprising a stirring and filtering structure (1), a discharge pipe (2), an electric control valve (3), a processing reaction box (4), a fixed mounting frame (5), a first electric push rod (6), a mounting frame (7), a mounting tank (8), a sliding limit hole (9) and a drying treatment structure (13), Features: The discharge pipes (2) are provided in three pieces, and the three discharge pipes (2) are evenly and fixedly connected to the bottom end of the processing reaction box (4); the electric control valves (3) are provided in three pieces, and the three electric control valves (3) are respectively fixedly installed on the three discharge pipes (2); the stirring and filtering structure (1) is arranged in the middle of the upper end of the processing reaction box (4); the installation frames (7) are provided in six pieces, and the six installation frames (7) are evenly and fixedly distributed on the upper end of the processing reaction box (4); The sliding limit hole (9) is symmetrically opened through the installation frame (7), the installation slot (8) is opened inside the installation frame (7), the drying treatment structure (13) is arranged inside the installation slot (8), six fixed installation frames (5) are provided, and the six fixed installation frames (5) are evenly fixedly installed outside the installation frame (7), and the first electric push rod (6) is symmetrically fixedly installed on the fixed installation frame (5); The drying treatment structure (13) comprises a fixed mounting bolt (10), a fixed limiting frame (11) and a drying machine (12); the fixed limiting frame (11) is arranged in an L shape, and the drying machine (12) is fixedly mounted on the middle part of the bottom end of the fixed limiting frame (11) by means of the fixed mounting bolt (10); The stirring and filtering structure (1) comprises a lifting control body (14) and a rotating filtering body (15); the lifting control body (14) is arranged at the upper end of the rotating filtering body (15); The rotating filter body (15) comprises a driving rod (16), a limit lifting column (17), a filter plate (18), a limit mounting frame (19) and a rotating stirring wheel (20), wherein six limit lifting columns (17) are provided, and the six limit lifting columns are evenly distributed on the limit mounting frame (19) in a ring shape (17), the filter plate (18) is fixedly mounted inside the limit mounting frame (19), the rotating stirring wheel (20) is rotatably mounted in the middle of the filter plate (18), and the bottom end of the driving rod (16) is fixedly connected to the middle of the upper end of the rotating stirring wheel (20); The lifting control body (14) comprises a motor (21), a fixedly connected cross column (22), a lifting adjustment disk (23), a second electric push rod (24) and a limit snap ring (25); six second electric push rods (24) are provided, and the six second electric push rods (24) are evenly distributed in a ring shape; the lifting adjustment disk (23) is fixedly connected to the upper end of the second electric push rod (24); the fixedly connected cross column (22) is evenly rotatably mounted inside the lifting adjustment disk (23); the motor (21) is fixedly mounted in the middle of the lifting adjustment disk (23); and the limit snap ring (25) is located below the lifting adjustment disk (23); The fixed mounting frame (5) is fixedly mounted on the mounting frame (7); the driving end of the first electric push rod (6) is slidably inserted into the interior of the sliding limit hole (9); the fixed limit frame (11) and the dryer (12) are arranged inside the mounting groove (8), and the driving end of the first electric push rod (6) is fixedly connected to the fixed limit frame (11); a temperature sensor (26) is evenly fixedly mounted inside the upper end of the processing reaction box (4); When the preparation device is working, the motor (21) is started to drive the driving rod (16) to rotate forward and reverse, thereby driving the rotating stirring wheel (20) to rotate forward and reverse, so that various materials in the processing reaction box (4) can be conveniently and quickly mixed. After mixing, the second electric push rod (24) is started, and the lifting adjustment plate (23) can be lifted upward by the second electric push rod (24). At this time, the lifting adjustment plate (23) that is lifted upward can lift the limit installation frame (19) and the filter plate (18) through the limit lifting column (17), and then the electric control valve (3) is started to open the discharge pipe (2). At this time, the processing The liquid in the reaction box (4) can flow out quickly. At this time, the first electric push rod (6) is started. The six fixed limit frames (11) are driven by the first electric push rod (6) to move and discharge the liquid from the inside of the installation slot (8). Then, three of the six dryers (12) are controlled to blow out natural wind to quickly cool the inside of the processing reaction box (4). After the temperature is cooled, the other three dryers (12) are started to blow out hot air to heat and control the temperature in the processing reaction box (4) again, so that the material body filtered and intercepted by the filter plate (18) is quickly dried to obtain the desired material body.
2. A method for preparing a polymer thickener, using the device for preparing a polymer thickener according to claim 1, It is characterized in that The following steps are involved: a. First, petroleum ether with a boiling point of 60 to 90° C. is placed in a processing reaction box (4), and then polyacrylamide powder with a hydrolysis degree of 20 to 45%, n-octanol and an organic acid are added in sequence, and heated, stirred and refluxed to react until the reaction is completed; b. Filter after cooling, and then dry for 3 to 5 hours in a vacuum environment at 110 to 120°C to obtain polymer powder; c. Place the polymer powder in paraffin oil at a mass ratio of 1:(2-4), and disperse by stirring to obtain a self-suspending polymer thickener; The raw materials of the polymer thickener include, by weight: 800-1000 parts of petroleum ether, 5-10 parts of n-octanol, and 1-3 parts of organic acid, wherein the organic acid is a mixture of benzenesulfonic acid and trifluoroacetic acid in a mass ratio of 2:1.