Hot-rolled equal-wall-thickness C-shaped steel and production process
By designing hot-rolled C-shaped steel with equal wall thickness, the problems of uneven cooling and welding defects caused by inconsistent wall thickness in the existing technology are solved, and the improvement of full-section equal thickness and welding performance is achieved. It is suitable for automated welding of building steel components .
Patent Information
- Application Number
- CN202310886292.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-07-18
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2043-07-18
AI Technical Summary
The existing hot-rolled C-shaped steels are not uniform in cooling and residual stress due to inconsistent wall thicknesses, which are not suitable for robotic automated welding operations, which are prone to welding defects.
Using hot-rolled wall thickness C-shaped steel, the web and wing plate formed by integrated hot-rolling have the same internal and external arc radius design, and the cross-sectional thickness of the wing plate and web are uniform, and the rib plate welding is added to adapt to robot automation. Welding, production processes include water and iron pretreatment, converter smelting, vacuum degassing and multiple cooling to control material composition and mechanical properties.
C-shaped steel with full-section thickness is realized, which reduces residual stress caused by uneven cooling, adapts to robotic automated welding, improves welding quality and efficiency, and meets the automated welding needs of building steel components.
Smart Images

Figure CN117165846B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of steel structures, and in particular to a hot-rolled C-shaped steel with equal wall thickness and a production process. Background Art
[0002] Hot-rolled steel refers to the steel obtained by heating ordinary steel such as low-carbon steel to a certain temperature and then hot-rolling it. Compared with ordinary bending steel, hot-rolled steel has the advantages of high production efficiency, low cost, short production cycle, high dimensional accuracy, and excellent mechanical properties. At present, hot-rolled steel is widely used in multi-story steel structures.
[0003] The patent with the announcement number CN205244814U discloses a hot-rolled channel steel for tunnels, which is a U-shaped part, including two side wing plates and a middle web plate, the spacing between the outer sides of the two side wing plates of the channel steel is 150±2.0mm, the thickness of the two side wing plates of the channel steel is 12±1.0mm, the length of the wing plates is 90±1.0mm, the thickness d of the web plate is 6.5±0.5mm, and the outer bottom of the wing plates and the web plate and the two side wing plates are all smooth transition arcs. The patent with the publication number CN113405013A discloses a production method of hot-rolled parallel leg C-shaped steel, wherein the height of the C-shaped steel waist plate (web plate) is 300mm~1000mm, the length of the parallel legs (wing plates) is 150mm~500mm, and the thickness of the waist plate and parallel legs is not less than 20mm.
[0004] The above two types of hot-rolled C-shaped steels have the problem of unequal thickness of the web and the two side wing plates. Moreover, the corners of the C-shaped steels are at a gradual transition right angle and are relatively thick. During the hot rolling process of the profiles, there is uneven cooling, which is prone to residual stress. Moreover, after the two C-shaped steels are welded into steel columns, there is a problem of unequal welding passes and layers in the transition section of the web and wing plates, which is very likely to cause welding defects and is not suitable for robot automated welding operations. Summary of the invention
[0005] Therefore, the technical problem to be solved by the present invention is to overcome the defects of the hot-rolled C-shaped steel in the prior art due to inconsistent wall thickness, thicker leg-waist transition section that easily produces residual stress and is not suitable for robot automated welding operations, thereby providing a hot-rolled C-shaped steel with equal wall thickness and a production process.
[0006] In order to solve the above technical problems, the technical solution of the present invention is as follows:
[0007] A hot-rolled C-shaped steel with equal wall thickness comprises a web and two wing plates which are integrally hot-rolled and formed, wherein the two wing plates are respectively located at opposite ends of the web and form a C-shaped structure with the web; the junction between the two wing plates and the web is an arc transition section, and the cross-sectional thicknesses of the web, the two arc transition sections and the two wing plates are equal.
[0008] Furthermore, the inner arc radius of the arc transition section is equal to the cross-sectional thickness of the web; and the outer arc radius of the arc transition section is twice the inner arc radius.
[0009] Furthermore, the cross-sectional lengths of the two wing plates are equal, and the cross-sectional length of the web plate is 2 to 4 times the cross-sectional length of the wing plates.
[0010] Furthermore, the cross-sectional length of the wing plate ranges from 125 mm to 500 mm, and the cross-sectional length of the web plate ranges from 500 mm to 1000 mm.
[0011] Furthermore, the cross-sectional thickness of the web is in the range of 20 mm to 50 mm.
[0012] Furthermore, an inclined surface is provided on the edge end surface of the wing plate away from the web plate, and the inclination angle θ of the inclined surface is ≤22.5°.
[0013] Furthermore, a plurality of ribs arranged at intervals are welded in the length direction of the hot-rolled C-shaped steel with equal wall thickness, and the ribs are welded and connected with the web, a pair of wing plates and two arc transition sections.
[0014] Furthermore, the hot-rolled equal-wall thickness C-shaped steel is Q355 steel, and the mass percentage of the chemical composition of the Q355 steel is: C: 0.22%~0.24%, Si≤0.55%, Mn≤1.60%, P≤0.035%, S≤0.035%, Cr≤0.30%, Ni≤0.30%, Cu≤0.40%, N≤0.012%, and the rest are Fe and other trace residual elements; carbon equivalent CEV≤0.46%, longitudinal elongation after fracture ≥21%, and welding crack sensitivity index Pcm≤0.2%.
[0015] Furthermore, the hot-rolled equal-wall thickness C-shaped steel is Q390 steel, and the mass percentage of the chemical composition of the Q390 steel is: C≤0.20%, Si≤0.55%, Mn≤1.70%, P≤0.035%, S≤0.035%, Cr≤0.30%, Ni≤0.50%, Cu≤0.40%, Nb≤0.05%, Mo≤0.1%, N≤0.015%, and the rest are Fe and other trace residual elements; carbon equivalent CEV≤0.46%, longitudinal elongation after fracture ≥21%, and welding crack sensitivity index Pcm≤0.2%.
[0016] A production process for hot-rolled C-shaped steel with equal wall thickness, the production process comprising the following steps:
[0017] Step S1, molten iron is pretreated and then smelted in a converter;
[0018] Step S2, blowing inert gas argon during the smelting process to purify the molten steel;
[0019] Step S3, refining in a submerged arc barrel furnace and electrically heating to control the nitrogen content of the molten steel;
[0020] Step S4, vacuum degassing is performed in a circulating vacuum degassing furnace to control the components of the steel;
[0021] Step S5, the steel billet is heated in a heating furnace to 1200° C. to 1300° C. for 3 to 4 hours;
[0022] Step S6, the starting rolling temperature in the rough rolling stage is controlled at 1100-1200°C, and the final rolling temperature is controlled at above 1050°C;
[0023] Step S7, after the rough rolling is completed, enter the intermediate rolling 1 and 2, wait until the temperature reaches 980℃~1050℃, and enter the finishing rolling stage;
[0024] Step S8, sawing the steel product;
[0025] Step S9, after rolling, the C-shaped steel enters the QST cooling device and undergoes three coolings; the first cooling is from the final rolling temperature to the Ar3 temperature, the second cooling is to control the phase change product, and the third cooling is air cooling to complete the phase change to room temperature;
[0026] Step S10, straightening the hot-rolled steel product by a straightening machine;
[0027] Step S11: Pack and ship the corrected steel products.
[0028] The technical solution of the present invention has the following advantages:
[0029] 1. The hot-rolled C-shaped steel with equal wall thickness provided by the present invention has the same thickness in the entire cross section. During the hot rolling process of the C-shaped steel, the problem of uneven cooling and easy generation of residual stress due to different cross-sectional thicknesses can be overcome. Compared with the hot-rolled C-shaped steel in the prior art, the hot-rolled C-shaped steel has better mechanical properties. At the same time, the circular arc transition section at the transition position between the web and the wing plate is of the same thickness as the web. When the robot is used for automatic welding, the problem of unequal number of welding passes and layers at the position of the web and the circular arc transition section during the robot's automatic welding process due to the different thicknesses of the circular arc transition section, the web and the wing plate is avoided. The present invention can adapt to the robot's automatic welding operation, and is not easy to cause welding defects when two C-shaped steels are welded to form derivative products such as a large-section box section.
[0030] 2. The hot-rolled C-shaped steel with equal wall thickness provided by the present invention has the same thickness as the wing plate and the web in the arc transition section, which is conducive to the automated welding of on-site butt joint of steel components in civil engineering.
[0031] 3. The hot-rolled C-shaped steel with equal wall thickness provided by the present invention provides a cross-sectional form (such as a groove, etc.) that is easy to weld, which is conducive to the promotion of intelligent production lines, such as robot automatic welding, etc.
[0032] 4. The production process of hot-rolled C-shaped steel with equal wall thickness provided by the present invention strictly controls the content of each element through the smelting process to ensure low carbon equivalent, and ensures that the hot-rolled C-shaped steel with equal wall thickness has good welding performance at the material level, which is easy to be used in welding in subsequent projects.
[0033] 5. The hot-rolled equal-wall-thickness C-shaped steel provided by the present invention is beyond the specifications prescribed by the current national profile standards, filling the gap in the industry and being conducive to the promotion and application of large-section profiles in the industry. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0035] Figure 1 A schematic diagram of the structure of hot-rolled C-shaped steel with equal wall thickness provided in the first embodiment of the present invention;
[0036] Figure 2 A schematic diagram of the structure of hot-rolled C-shaped steel with equal wall thickness provided in the second embodiment of the present invention;
[0037] Figure 3 It is a cross-sectional schematic diagram of two hot-rolled C-shaped steels with equal wall thickness butt-welded to form a box-shaped steel in the first implementation mode of the second embodiment of the present invention;
[0038] Figure 4 This is a schematic structural diagram of a hot-rolled C-shaped steel with equal wall thickness welded with ribs in the first implementation manner of the second embodiment of the present invention;
[0039] Figure 5 It is a cross-sectional schematic diagram of two hot-rolled C-shaped steels with equal wall thickness welded with ribs to form a box-shaped steel in the first implementation mode of the second embodiment of the present invention;
[0040] Figure 6 It is a cross-sectional schematic diagram of two hot-rolled C-shaped steels with equal wall thickness butt-welded to form a box-shaped steel in the second implementation mode of the second embodiment of the present invention;
[0041] Figure 7 This is a schematic structural diagram of hot-rolled C-shaped steel of equal wall thickness on a rolling die in the first implementation manner of Example 1 of the present invention;
[0042] Figure 8This is a schematic structural diagram of hot-rolled C-shaped steel with equal wall thickness on a rolling die in the second implementation manner of Example 1 of the present invention;
[0043] Fig. 9 This is a schematic structural diagram of hot-rolled C-shaped steel of equal wall thickness on a rolling die in the first implementation manner of Example 2 of the present invention.
[0044] Explanation of the reference numerals: 1. web; 2. wing plate; 3. arc transition section; 4. inclined surface; 5. rib plate. DETAILED DESCRIPTION
[0045] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0046] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0047] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0048] Embodiment 1
[0049] like Figure 1 A hot-rolled C-shaped steel with equal wall thickness shown in the figure comprises a web 1 and two wing plates 2 formed by hot rolling in one piece. The two wing plates 2 are respectively located at opposite ends of the web 1. The two wing plates 2 and the web 1 form a C-shaped structure. The cross-sectional lengths of the two wing plates 2 are equal. The junction of the two wing plates 2 and the web 1 is a circular arc transition section 3. The cross-sectional thicknesses of the web 1, the two circular arc transition sections 3 and the two wing plates 2 are equal. The inner arc radius r of the circular arc transition section 3 is equal to the cross-sectional thickness t of the web 1; the outer arc radius R of the circular arc transition section 3 is twice the inner arc radius r thereof.
[0050] In this embodiment, the cross-sectional length H of the web 1 is 2 to 4 times the cross-sectional length of the wing 2. For example, the cross-sectional length of the web 1 ranges from 500 mm to 1000 mm, and the cross-sectional length of the wing 2 ranges from 125 mm to 500 mm. The cross-sectional thickness of the web ranges from 20 mm to 50 mm. For such a size of hot-rolled equal-wall thickness C-shaped steel, the processed cross-section meets the S1-level cross-section of the steel structure design standard, i.e., the plastic rotation cross-section, which can reach the full cross-sectional plasticity, ensuring that the plastic hinge has the rotation capacity required by the plastic design, and the bearing capacity does not decrease during the rotation process.
[0051] The hot-rolled C-shaped steel with equal wall thickness provided by the present invention has an entire cross-section with equal thickness. During the hot rolling process of the C-shaped steel, the problems of uneven cooling and easy generation of residual stress due to different cross-section thicknesses can be overcome. Compared with the hot-rolled C-shaped steel in the prior art, the hot-rolled C-shaped steel has better mechanical properties and good welding performance.
[0052] Embodiment 2
[0053] like Figure 2 and Figure 3 As shown, the difference from the first embodiment is that a chamfer 4 is provided on the edge end surface of the wing plate 2 away from the web plate 1, and the inclination angle θ of the chamfer 4 is ≤ 22.5°. When two wing plates 2 of hot-rolled equal-wall thickness C-shaped steel are butt-jointed to form a box-shaped steel, the two chamfers 4 on the two wing plates 2 are butt-jointed to form a V-groove, providing a cross-sectional form that is easy to weld, which is conducive to the robot completing the automatic butt welding of two hot-rolled equal-wall thickness C-shaped steels at the groove position, and is conducive to the full-automatic production of the process of welding hot-rolled equal-wall thickness C-shaped steels to form box-shaped steels.
[0054] Figure 4 It is a structural schematic diagram of a hot-rolled C-shaped steel with equal wall thickness, in which a plurality of ribs 5 are welded in sequence in the length direction. Figure 5 The cross-sectional diagram of a box-shaped steel formed by welding two hot-rolled C-shaped steels with equal wall thickness and ribs. Figure 4 and Figure 5As shown, a plurality of ribs 5 are sequentially arranged at intervals along the length direction of the hot-rolled equal-wall thickness C-shaped steel, and the ribs 5 are simultaneously welded and connected to the web 1, wing 2 and arc transition section 3 of the C-shaped steel. In the process of automatically welding the ribs 5 to the C-shaped steel using a robot, since the web 1, wing 2 and arc transition section 3 are designed to be of equal thickness, the number of welding passes and the number of welding layers of the welding gun on the robot passing through each welding position are equal, which is conducive to the automated welding operation of the robot. The robot can weld continuously and uninterruptedly, and it is not easy to cause welding defects when two C-shaped steels are welded to form derivative products such as large-section box sections. In the prior art, due to the inconsistent cross-sectional thicknesses of the web, wing and transition section of the C-shaped steel, in the process of welding the rib plate to the C-shaped steel, in order to ensure the welding quality of the rib plate, the number of welding passes and welding layers at different welding positions of the C-shaped steel are different. In particular, when the cross-sectional thickness of the transition section is large, the number of welding passes and welding layers required for the welding position between the rib plate and the transition section is less than the number of welding passes and welding layers required for the welding position between the rib plate and the web plate and the wing plate. When the robot's welding gun sequentially welds the wing plate, the thicker transition section and the web plate, it is necessary to adjust the welding parameter settings to achieve automated welding and ensure the welding quality. In addition, the cross-sectional thickness of each part of the transition section is usually different, which further increases the difficulty of adjusting the welding parameters of the automatic welding robot. In fact, since the welding time of the welding gun passing through the transition section is very short, it is actually difficult to adjust the welding parameters of the welding gun in real time according to the cross-sectional thickness of each part of the transition section in a very short time. Therefore, the welding of the rib plate on the C-shaped steel in the prior art still adopts the traditional manual welding method, which has the problems of large welding workload, low welding efficiency, poor welding consistency, etc. The present invention provides a C-shaped steel with uniform thickness throughout the entire cross section, and can utilize a robot to realize the automated welding operation of ribs on the C-shaped steel. When two C-shaped steels are welded to form derivative products such as a large-section box section, welding defects are not easily caused, thereby greatly improving the welding efficiency and welding quality.
[0055] Figure 6 The schematic cross-sectional view of a box-shaped steel formed by butt welding two hot-rolled C-shaped steels of equal wall thickness in the second embodiment of the present invention is different from the first embodiment of the second embodiment in that the cross-sectional length H of the web 1 is 4 times the cross-sectional length of the wing 2. For example, when the cross-sectional length of the web 1 is 500 mm, the cross-sectional length of the wing 2 is 125 mm.
[0056] In this embodiment, the hot-rolled C-shaped steel adopts two materials commonly used in the main load-bearing components of the building structure, namely Q355 steel and Q390 steel (refer to "JGJ 99-2015 Technical Specification for Steel Structure of High-rise Civil Buildings" and "Low Alloy High Strength Structural Steel" (GB / T 1591-2018), but not limited to the above two standards). Among them, Q355 steel is composed of the following elements in mass percentage: C: 0.22% to 0.24%, Si≤0.55%, Mn≤1.60%, P≤0.035%, S≤0.035%, Cr≤0.30%, Ni≤0.30%, Cu≤0.40%, N≤0.012%, and the rest is Fe and other inevitable trace residual elements; carbon equivalent CEV≤0.46%, longitudinal elongation after fracture≥21%, welding crack sensitivity index Pcm≤0.2%. Q390 steel is composed of the following elements in mass percentage: C≤0.20%, Si≤0.55%, Mn≤1.70%, P≤0.035%, S≤0.035%, Cr≤0.3%, Ni≤0.5%, Cu≤0.4%, Nb≤0.05%, Mo≤0.1%, N≤0.015%, the rest is Fe and other unavoidable trace residual elements; carbon equivalent CEV≤0.46%, longitudinal elongation ≥20%, welding crack sensitivity index Pcm≤0.2%. Through the smelting process, the content of each element is strictly controlled to ensure that the steel has good welding performance at the material level.
[0057] Embodiment 3
[0058] A production process for hot-rolled C-shaped steel with equal wall thickness, comprising the following steps:
[0059] Step S1, molten iron is pretreated and then smelted in a converter;
[0060] Step S2, blowing inert gas argon during the smelting process to purify the molten steel;
[0061] Step S3, refining in a submerged arc barrel furnace and electrically heating to control the nitrogen content of the molten steel;
[0062] Step S4, vacuum degassing is performed in a circulating vacuum degassing furnace to control the components of the steel;
[0063] Step S5, the steel billet is heated in a heating furnace to 1200° C. to 1300° C. for 3 to 4 hours;
[0064] Step S6, the starting rolling temperature in the rough rolling stage is controlled at 1100-1200°C, and the final rolling temperature is controlled at above 1050°C;
[0065] Step S7: After the rough rolling is completed, the intermediate rolling 1 and 2 are started, and the temperature is raised to 980℃~1050℃, and then the finishing rolling is started; Figure 7This is a schematic structural diagram of hot-rolled C-shaped steel of equal wall thickness on a rolling die in the first implementation manner of Example 1 of the present invention; Figure 8 This is a schematic structural diagram of hot-rolled C-shaped steel of equal wall thickness on a rolling die in the second implementation manner of Example 1 of the present invention; Fig. 9 This is a schematic diagram of the structure of hot-rolled C-shaped steel with equal wall thickness on a rolling die in the first implementation mode of the second embodiment of the present invention; by changing the lateral and bottom rollers of the rolling die, the length and shape of the wing plate of the C-shaped steel can be controlled;
[0066] Step S8, sawing the steel product;
[0067] Step S9, after rolling, the C-shaped steel enters the QST cooling device and undergoes three coolings; the first cooling is from the final rolling temperature to the Ar3 temperature, the second cooling is to control the phase change product, and the third cooling is air cooling to complete the phase change to room temperature;
[0068] Step S10, straightening the hot-rolled steel product by a straightening machine;
[0069] Step S11: Pack and ship the corrected steel products.
[0070] The above production and processing steps are applicable to Q355 and Q390 steel or other steel materials used in the present invention. The production process of hot-rolled equal-wall thickness C-shaped steel strictly controls the content of each element through the smelting process to ensure low carbon equivalent, and ensures that the hot-rolled equal-wall thickness C-shaped steel has good welding performance at the material level, which is easy to be applied and welded in subsequent projects.
[0071] In summary, the present invention provides a hot-rolled C-shaped steel with equal wall thickness and a production process thereof, which has the following beneficial effects: 1. It can produce equal-thickness C-shaped steel with a web length of 500mm to 1000mm, a wing length of 125mm to 500mm, and a maximum wing thickness of 50mm, enriching the types of C-shaped steel production, providing more choices for building steel structure design, and solving the problem of the current shortage of such products in the market; 2. The hot-rolled large-section C-shaped steel produced has equal thickness in the entire cross section, avoiding stress concentration at the corners, and has better mechanical properties, which can be used for and is easy to derive product automation Processing, such as large-section box-shaped butt-welded composite components and welding of steel sections along the length direction; 3. Compared with traditionally produced large-section box-shaped components, the hot-rolled large-section C-shaped steel produced reduces the number of welds and has better overall performance; 4. The corners of the hot-rolled large-section C-shaped steel produced have a smaller thickness, which is conducive to the welding of steel components along the length direction in civil engineering; 5. It is conducive to promoting the application of large-section steel sections, promoting the industrialization and standardization of the construction industry, and promoting the development of the industry; 6. Providing cross-sectional forms that are easy to weld (such as grooves, etc.) is conducive to the promotion of intelligent production lines, such as robot automatic welding.
[0072] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.
Claims
1. A hot-rolled C-shaped steel with equal wall thickness, characterized in that: It comprises an integrally hot-rolled web (1) and two wing plates (2), wherein the two wing plates (2) are respectively located at opposite ends of the web (1) and form a C-shaped structure with the web (1); the junction between the two wing plates (2) and the web (1) is a circular arc transition section (3), and the cross-sectional thickness of the web (1), the two circular arc transition sections (3) and the two wing plates (2) are equal; a plurality of ribs (5) arranged at intervals are welded in the length direction of the hot-rolled equal-wall-thickness C-shaped steel, and the ribs (5) are welded and connected to the web (1), a pair of wing plates (2) and the two circular arc transition sections (3); The inner arc radius of the arc transition section (3) is equal to the cross-sectional thickness of the web (1); and the outer arc radius of the arc transition section (3) is twice the inner arc radius.
2. The hot-rolled equal-thickness C-shaped steel according to claim 1, characterized in that: The cross-sectional lengths of the two wing plates (2) are equal, and the cross-sectional length of the web plate (1) is 2 to 4 times the cross-sectional length of the wing plate (2).
3. The hot-rolled equal-thickness C-shaped steel according to claim 2, characterized in that: The cross-sectional length of the wing plate (2) ranges from 125 mm to 500 mm, and the cross-sectional length of the web plate (1) ranges from 500 mm to 1000 mm.
4. The hot-rolled equal-wall-thickness C-shaped steel according to claim 1, characterized in that: The cross-sectional thickness of the web (1) is in the range of 20 mm to 50 mm.
5. The hot-rolled equal-wall-thickness C-shaped steel according to claim 1, characterized in that: An inclined surface (4) is provided on the edge end surface of the wing plate (2) away from the web plate (1), and the inclination angle θ of the inclined surface (4) is ≤22.5°.
6. The hot-rolled equal-wall-thickness C-shaped steel according to claim 1, characterized in that: The hot-rolled equal-wall thickness C-shaped steel is Q355 steel, and the mass percentage of the chemical composition of the Q355 steel is: C: 0.22% to 0.24%, Si≤0.55%, Mn≤1.60%, P≤0.035%, S≤0.035%, Cr≤0.30%, Ni≤0.30%, Cu≤0.40%, N≤0.012%, and the rest are Fe and other trace residual elements; carbon equivalent CEV≤0.46%, longitudinal elongation after fracture≥21%, and welding crack sensitivity index Pcm≤0.2%.
7. The hot-rolled equal-thickness C-shaped steel according to claim 1, characterized in that: The hot-rolled equal-wall thickness C-shaped steel is Q390 steel, and the mass percentage of the chemical composition of the Q390 steel is: C≤0.20%, Si≤0.55%, Mn≤1.7%, P≤0.035%, S≤0.035%, Cr≤0.30%, Ni≤0.50%, Cu≤0.40%, Mo≤0.10%, and the rest are Fe and other trace residual elements; carbon equivalent CEV≤0.46%, longitudinal elongation after fracture ≥21%, and welding crack sensitivity index Pcm≤0.2%.
8. A production process for hot-rolled C-shaped steel of equal wall thickness according to any one of claims 1 to 7, characterized in that: The production process includes the following steps: Step S1, molten iron is pretreated and then smelted in a converter; Step S2, blowing inert gas argon during the smelting process to purify the molten steel; Step S3, refining in a submerged arc barrel furnace and electrically heating to control the nitrogen content of the molten steel; Step S4, vacuum degassing is performed in a circulating vacuum degassing furnace to control the components of the steel; Step S5, the steel billet is heated in a heating furnace to 1200° C. to 1300° C. for 3 to 4 hours; Step S6, the starting rolling temperature in the rough rolling stage is controlled at 1100-1200°C, and the final rolling temperature is controlled at above 1050°C; Step S7, after the rough rolling is completed, enter the intermediate rolling 1 and 2, wait until the temperature reaches 980℃~1050℃, and enter the finishing rolling stage; Step S8, sawing the steel product; Step S9, after rolling, the C-shaped steel enters the QST cooling device and undergoes three coolings; the first cooling is from the final rolling temperature to the Ar3 temperature, the second cooling is to control the phase change product, and the third cooling is air cooling to complete the phase change to room temperature; Step S10, straightening the hot-rolled steel product by a straightening machine; Step S11: Pack and ship the corrected steel products.
Citation Information
Patent Citations
Hot-rolled parallel leg channel steel and production method thereof
CN113405013A
Hot -rolled steel channel for tunnel
CN205244814U
J section steel and application thereof
CN103114680A
C-shaped forklift portal hot-rolled section steel
CN107827038A
Hot-rolled thin-web and ultra-deep variable cross-section trapezoidal rib and hot continuous rolling production process thereof
CN111495967A