Method for preparing an etching mask, method for etching a structure in a substrate, use of a layer of a group IV element, and structure for preparing a mask
By applying a metal layer and a mask layer on the substrate and forming interdiffusion regions of the fourth group element layer, selectively etching the metal layer, the problem of etching narrow trenches in the prior art is solved, and a higher resolution is achieved and lower load effect etching effect, suitable for CMOS technology and other lithography applications.
Patent Information
- Application Number
- CN202280045780.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2021-06-28
- Filing Date
- 2022-06-20
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-06-20
AI Technical Summary
The prior art is difficult to achieve high resolution and fine structure when etching narrow trenches, and the resist edge shadowing and loading effects are more prominent, making it difficult to overcome the resolution limits of the lithography system.
By adopting a method, by applying a metal layer and a mask layer on the substrate and forming a fourth group element layer at its interface to form an interdiffusion region, the metal layer is selectively etched to achieve etching of narrow trenches, reducing resistance to Corroder edge shadowing and loading effects and achieve tone reversal.
This method can achieve narrower resist strips and higher resolution etching without changing the photomask or paint process, overcoming some inherent difficulties in lithography, especially in CMOS technology and other technologies It is conducive to the preparation of fine products.
Smart Images

Figure CN117581340B_ABST
Abstract
Description
Technical Field
[0001] The method of the present invention relates to a method for preparing an etching mask, a method for etching a structure in a substrate, the use of a Group IV element layer and a structure for preparing a mask.
[0002] Photolithography of titanium, aluminum and tungsten layers is a standard technique widely used in many standard CMOS products. Photolithography of chromium layers is a standard technique widely used in many non-CMOS standard products as a light absorber for a wide wavelength spectrum. Structural techniques such as electron beam lithography or optical lithography have been known in microtechnology and nanotechnology for many years. The same applies to coating processes such as sputtering deposition of chromium (sputter coating) and sputtering deposition of silicon in some cases. For example, dry etching processes are used in the photomask industry, where reactive ion etching of chromium and chromium oxynitride layers with chlorine-based plasmas has been a common method for many years. Background Art
[0003] An etching process using a silicide mask is known from JP H06-061000B2. Another etching process using a silicide mask is known from JP 2007-115830A. A silicide film is known from US 5906950 A. Another etching process using a silicide mask is known from US5001085 A. Another etching process using a silicide mask is known from EP 0284308 A1. Another etching process using a silicide mask is known from DE 3315719A1. A method for preparing an etching mask is known from US5053105A. An electrode is prepared using an etching process from US2002 / 0177280 A1. Another method for preparing a gate electrode using an etching process is known from DE 10355581 A1. The etching processes mentioned all have the disadvantage that it is difficult to etch narrow grooves. Summary of the invention
[0004] Against this background, the invention provides a method for producing an etching mask, a method for etching a structure in a substrate, the use of a layer of a Group IV element, and a structure for producing a mask. Advantageous embodiments result from the corresponding following description.
[0005] The method proposed in this paper advantageously achieves tone inversion without changing the expensive photomask or painting process. In addition, shadowing and loading effects at the edges of the resist can be reduced. In addition, resist strips can be prepared where substrate trenches are created, and these resist strips can be narrower than the resolution limit of the lithography system.
[0006] The present invention provides a method for preparing an etching mask, the method comprising the following steps:
[0007] Setting a substrate;
[0008] applying a metal layer having a metal layer thickness of 1000 Å to the substrate, wherein the metal layer comprises at least one transition metal and / or aluminum or consists of such a metal,
[0009] applying a mask layer having a mask layer thickness to the substrate coated with the metal layer;
[0010] structuring the mask layer, wherein the metal layer is exposed in at least one processing area,
[0011] after coating the substrate with a Group 4 element layer having a Group 4 element layer thickness, coating the substrate with a Group 4 element layer at least partially comprising a Group 4 element, wherein an interdiffusion zone between the transition metal or aluminum and the Group 4 element is formed at an interface between the metal layer and the Group 4 element layer at a processed region,
[0012] removing the mask layer, and
[0013] The metal layer is selectively etched, wherein the substrate is exposed in at least one etched region other than the processed region, and the metal layer is at least partially maintained in the processed region.
[0014] In particular, the Group IV element layer may include silicon or be formed of silicon, and the interdiffusion region may be present as a transition metal silicide layer or an aluminum silicide layer.
[0015] In the setting step, the substrate can be, for example, set to a so-called wafer made of glass, quartz glass, silicon, polymer or other materials. Subsequently, a metal layer is applied to at least one side of a substrate that can be, for example, formed by chromium. In particular, the metal layer can include several or just one transition metal and / or be composed of several or just one transition metal. Suitable transition metals can be chemical elements with atomic numbers of 21 to 30, 39 to 48 and 57 to 79. Advantageously, several transition metals or a basic transition metal in these transition metals can be selected. Metals with negative standard potentials for redox pairs relative to standard hydrogen electrodes can be described as basic metals. The metal layer can particularly advantageously include several or just one refractory metal, such as Ti, Cr, Mo and / or W, or be composed of several or just one refractory metal. Also advantageously, the metal layer can include aluminum or be composed of aluminum.
[0016] In the application step, the substrate side covered by the metal layer is coated with a mask layer (also referred to as resist), which can be, for example, a photoresist. In the structuring step, the mask layer is structured, for example, by exposing the photoresist. The mask layer is completely removed in at least one processing area (also referred to as the first position) to expose the underlying metal layer. Subsequently, one side of the substrate on which the metal layer and the mask layer are arranged is then additionally coated with a Group IV element layer. Group IV elements are elements of the fourth main group of the periodic table (also referred to as the carbon group, i.e. the 14th group of the current IUPAC symbol). In the context of the present invention, advantageous Group IV elements can be, for example, carbon (C), silicon (Si) or germanium (Ge), particularly advantageously Si. If the metal layer is formed by a base metal, advantageously, for example, by a refractory metal or aluminum, it may be particularly advantageous to use Si or C as Group IV elements. Alternatively, a precious transition metal such as gold can be used for the metal layer. For example, germanium can then be selected as the Group IV element, which can form a gold-germanium alloy at the interface in the interdiffusion zone. The Group IV element layer may be a layer that includes at least one Group IV element, is advantageously composed of one Group IV element, and is particularly advantageously composed of exactly one Group IV element. Semi-metal Group IV elements and non-metal Group IV elements may be particularly suitable, while metal Group IV elements may not be suitable. In the processing area where the metal layer is exposed due to the previous structuring, an interdiffusion zone is generated between the Group IV element and the metal layer. This interdiffusion zone may appear at the interface between the metal layer and the Group IV element layer, and may be formed between the Group IV element of the Group IV element layer and the metal of the metal layer. For example, if silicon is selected as the Group IV element, a metal silicide layer, i.e., a transition metal silicide layer or an aluminum silicide layer, may be formed. The interdiffusion zone may also be referred to as a transition zone, in which the metal and the Group IV element of the metal layer may be mixed. Mixing may be understood to mean that an alloy may exist in the transition zone. The alloy may include one or more intermetallic mixed phases. When the mask layer is subsequently removed, the metal layer coated with the Group IV element layer or the transition metal silicide layer remains in the processing area. In a subsequent selective etching step, the metal layer in the areas not coated with the layer of the fourth group element can be removed. Thus, the substrate is exposed in the etching area, while the substrate arranged at the processing area is passivated by the interdiffusion zone. This takes advantage of the fact that alloys such as chromium silicide differ greatly from pure chromium and pure silicon in their etching behavior. This also applies to contact areas, such as the interdiffusion zone of two continuously deposited layers. Such an interdiffusion zone can be very thin, for example on the order of one nanometer, but is very resistant to certain etching processes. Using the method proposed in this article, such a thin interdiffusion zone can be used to advantageously overcome some inherent difficulties in lithography. The process sequence allows positive and negative reversal, i.e., tone reversal, without changing the exposure mask used or creating a new photomask. In addition, the change of tone can help solve some specific difficulties in lithography.Assuming a positive resist and a given distance to resolve the test grid, it is usually easier to achieve fine resist lines that are less than 50% of the distance, as this can be fine-tuned by some overdose during exposure or overdevelopment to reduce the width of the resist band and sometimes the height of the resist. However, the closer you get to the resolution limit of the lithography system, the more difficult it is to resolve resist grooves that are less than 50% of the test grid distance. With the method proposed in this article, grooves that are less than 50% of the distance can be advantageously resolved. This may enable i-line lithographic production of pulse compression gratings in the future. Additionally, this method may also be used to prepare effective media such as optically effective media from ineffective media by structuring, for example, a chemically resistant AR layer or a refractive index gradient. The present invention may be used to prepare products with CMOS technology and other technologies.
[0017] According to one embodiment, the method may include a step of removing the Group IV layer, wherein the interdiffusion zone may remain at the processing area, wherein the removal of the Group IV layer may occur after the coating step and before the removal step. Additionally or alternatively, in the step of removing the mask layer, the Group IV layer may be at least partially removed. For example, the Group IV layer and the mask layer having the Group IV layer additionally or alternatively may be removed by an etching process. The removal step may differ from a conventional stripping process in that the Group IV layer may be selectively removed from the resist tape. This has the advantage that no silicon flakes or fences are left behind.
[0018] According to another embodiment, the Group IV layer can be removed by wet chemical means using potassium hydroxide (KOH) and additionally or alternatively sodium hydroxide (NaOH) and additionally or alternatively ammonium hydroxide (NH4OH) and additionally or alternatively organic alkaline etchants. The advantage of using these or similar etchants is that the removal step can be performed in a cost-effective manner.
[0019] According to another embodiment, in the structuring step, the mask layer can be structured by exposure and development and additionally or alternatively by electron beam. For example, the mask layer can be a positive resist or a negative resist. These can be exposed in the structuring step, for example, using an exposure mask, and then developed. Advantageously, this method step can be performed in a cost-effective manner. Alternatively, structuring can also be performed by electron beam lithography. The main advantage of using an electron beam is that, compared with photolithography, a structure with significantly smaller size (for example, in the nanometer range) can be prepared.
[0020] According to another embodiment, in the removal step, the mask layer can be removed by ashing and additionally or alternatively in a wet chemical manner and additionally or alternatively by dissolving in a solvent and additionally or alternatively by a combination of dissolving and chemical removal. Additionally or alternatively, in the step of selective etching, the etching of the metal layer can be performed in a wet chemical manner using reactive ion beam etching (RIE) and additionally or alternatively non-reactive ion beam etching and additionally or alternatively using an acidic etchant and additionally or alternatively a halogen-containing etchant. The reagents used in the removal process and during selective etching can be matched with the materials of the mask layer and the metal layer. Advantageously, the method can be optimally adapted to a given environment and the solvents and materials available for the method.
[0021] According to another embodiment, in the applying step, the metal layer may be composed of titanium (Ti), zirconium (Zr), tantalum (Ta), chromium (Cr), molybdenum (Mo) and additionally or alternatively tungsten (W), or include at least one of these metals. Additionally or alternatively, in the arranging step, the substrate may be arranged as a wafer made of glass, quartz glass, quartz single crystal, silicon (Si), germanium (Ge), BiTe, gallium arsenide (GaAs), silicon carbide (SiC), indium phosphide (InP), GaInAsP, lithium niobate (LiNbO3) or a polymer. The material used may advantageously be adapted to the existing requirements.
[0022] According to another embodiment, the metal layer thickness can be between 1nm and 2000nm, and additionally or alternatively, the mask layer thickness can be between 1nm and 500nm, and additionally or alternatively, the fourth group element layer thickness can be between 1nm and 30nm, particularly between 1nm and 5nm and between 1nm and 2nm. For example, the metal layer thickness and the mask layer thickness can be, for example, between 20nm and 200nm. This advantageously achieves overcoming the common obstacles of structured chromium layers with high resolution. When structured in this way, the high aspect ratio of the resist may sometimes become an obstacle, especially for the resist with fine features. For example, a 300nm thick resist layer can be used for a structured 100nm thick Cr layer. In order to dissolve a 100nm groove, etching can be performed in a resist cavity with a depth that is three times the width. This is not the only reason for size-dependent etching depth or size-dependent undercut (RIE hysteresis), but it is an important reason. The method proposed herein can be advantageously used to prepare a thinner etching mask, such as one or two nanometers. This can significantly reduce effects such as shadowing of the resist sidewalls or the so-called loading effect. In addition, stresses can be avoided by introducing dense features into the substrate. This can be an advantage compared to alternative coatings with functional layers, especially for products that are sensitive to bending.
[0023] In an advantageous embodiment, the layer of the Group IV element can be applied so thinly that the applied Group IV element is completely absorbed into the interdiffusion zone at the treated area. The surface there can then be free of pure Group IV elements.
[0024] According to another embodiment, in the applying step, the metal layer can be applied by sputtering or vapor deposition, and / or additionally or alternatively, in the coating step, the substrate can be coated with the Group IV element layer by sputtering or vapor deposition. Advantageously, time and cost can be saved by using this known method.
[0025] According to another embodiment, the method may include a step of cleaning the exposed surface of the treated area, wherein the cleaning step may be performed after the structuring step and before the coating step. For example, the cleaning may be performed by dry etching, in particular sputter etching or plasma etching or plasma-free hot gas etching. Advantageously, in the cleaning step, the surface of the structured mask layer and the metal layer exposed by the structuring can be optimally prepared for coating with a layer of a Group IV element.
[0026] In addition, a method for etching a structure in a substrate is proposed, wherein the method comprises a step of preparing an etching mask according to a variant of the method proposed above and a step of deep etching in the substrate using the etching mask. Advantageously, by using an etching mask prepared according to the preparation method proposed above, all the above-mentioned advantages can be optimally achieved.
[0027] For example, a structure etched in a substrate can have an array of fine SiO2 pillars with high resolution and low exposure cost. These could be advantageous for optical immersion sensors or as metamaterials with a specific refractive index, for example. A very thin hydrophobic coating on these pillars can create a lotus effect to make the surface extremely hydrophobic. For example, the pillars can be made of pure SiO2 and be highly resistant to degradation caused by UV radiation and corrosion.
[0028] According to one embodiment, deep etching can be performed in the substrate by reactive ion etching (RIE) or reactive ion deep etching (DRIE). Advantageously, deep etching can therefore be highly controllably performed in terms of uniformity, etching rate, etching profile, and selectivity, such as for the preparation of topographic structures for microsystem technology and nanosystem technology.
[0029] Advantageously, removal of the etching mask may also be provided. Removal of the etching mask may include removal of the interdiffusion region and the metal layer remaining below the interdiffusion region. The structure etched in the substrate may be retained. The substrate with the etched structure may then be free of the metal layer. This may be particularly advantageous if an optical component is to be prepared. Removal of the etching mask may be performed simultaneously with deep etching in the substrate and / or after deep etching in the substrate. The etching mask may advantageously be removed after deep etching. It is also advantageous that removal of the etching mask has already begun during deep etching. For example, during deep etching, the interdiffusion region may be partially or completely removed. Advantageously, at least a portion of the metal layer may be retained until the end of deep etching, thereby ensuring masking until the end of deep etching.
[0030] In addition, a use of a Group IV element layer in preparing an auxiliary mask which is inverted relative to a resist mask on a metal layer for masking the metal layer is proposed, the metal layer comprising a transition metal and / or aluminum, and the auxiliary mask is formed by an alloy of a Group IV element and a metal, in particular by a metal silicide. The alloy may be present in an interdiffusion zone at the interface between the metal layer and the Group IV element layer.
[0031] The metal layer may advantageously consist of a transition metal or aluminum.A metal layer consisting of a single metal may have the advantage that the metal layer may be produced in a more reproducible manner.
[0032] In addition, a structure for preparing a mask is proposed, which comprises a substrate, a continuous metal layer including at least one transition metal or aluminum arranged on the substrate, and a structured mask layer arranged on the metal layer, wherein the structured mask layer has at least one processing area where the mask layer is interrupted, wherein the metal layer is covered with an interdiffusion zone on the surface of the processing area, and the interdiffusion zone includes an alloy of a transition metal or aluminum and a fourth group element, in particular wherein the alloy includes silicon. The material of the metal layer that is not alloyed with the fourth group element can be arranged between the interdiffusion zone and the substrate. This material can represent a portion of the metal layer in the processing area that does not contain a fourth group element. This can constitute the maximum proportion of the layer thickness, and the layer thickness of the interdiffusion zone can be less than 10% of the total layer thickness of the alloy layer thickness and the layer thickness that does not contain the fourth group element, advantageously less than 2%. For example, the layer thickness of the interdiffusion zone can be between 1nm and 10nm, advantageously between 1nm and 5nm, and particularly advantageously between 1nm and 3nm. Advantageously, the interdiffusion zone can therefore be formed only on the surface of the metal layer, while the metal layer inside and outside the processing area can have a substantially uniform layer thickness. The alloy of metal and Group IV element formed in the interdiffusion zone can only be present at the interrupted positions of the mask layer. At the uninterrupted positions, i.e. outside the processing area, the mask layer can be arranged directly on the metal layer, without the mask layer material in the processing area. The structure for preparing the mask can be understood as a semi-finished product, with which the mask can be prepared. By removing the mask layer, the mask can be made of the structure for preparing the mask. This mask can be regarded as an auxiliary mask inverted with respect to the mask layer. The mask made of such a semi-finished product can be used to etch the structure in the substrate in order to prepare the desired product.
[0033] The proposed method can be implemented, for example, in software or hardware, or in a hybrid form of software and hardware, for example in a control unit.
[0034] The method proposed here also produces an apparatus which is designed to carry out, control or implement the steps in the method variant proposed here in the corresponding apparatus. This embodiment variant of the invention in the form of an apparatus can enable the objects behind the invention to be solved quickly and efficiently.
[0035] For this purpose, the device can have at least one computing unit for processing signals or data, at least one storage unit for storing signals or data, at least one interface for interfacing with a sensor or an actuator for reading a sensor signal from a sensor or for outputting data or a control signal to an actuator, and / or at least one communication interface for reading or outputting data embedded in a communication protocol. The computing unit can be, for example, a signal processor, a microcontroller, etc., wherein the storage unit can be a flash memory, an EEPROM or a magnetic storage unit. The communication interface can be designed to read or output data wirelessly and / or in a line-bound manner, wherein a communication interface that can read or output line-bound data can, for example, read these data from a corresponding data transmission line electrically or optically or output these data into a corresponding data transmission line.
[0036] In the present invention, the device can be understood to mean an electrical device that processes sensor signals and outputs control and / or data signals according to these signals. The device can have an interface, which can be designed as hardware and / or software. In a hardware embodiment, the interface can be, for example, a part of a so-called system ASIC, which includes the various functions of the device. However, the interface can also be a separate integrated circuit, or at least partially composed of discrete components. In software design, the interface can be a software module, for example, in addition to other software modules, these software modules are also present on a microcontroller. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Exemplary embodiments of the method proposed here are shown in the drawings and are explained in more detail in the following description. The following drawings are shown:
[0038] Figure 1 A flow chart of an exemplary embodiment of a method for preparing an etch mask;
[0039] Figure 2 A flow chart of an exemplary embodiment of a method for preparing an etch mask;
[0040] Figure 3 is a schematic illustration of an exemplary embodiment of various process steps in a method of preparing an etching mask as compared to conventional process steps;
[0041] Figure 4 is a schematic illustration of a structure for preparing an etching mask prior to applying a Group IV element layer;
[0042] Figure 5 is a schematic illustration of a structure for preparing an etching mask after applying a Group IV element layer;
[0043] Figure 6 is a schematic illustration of a structure for preparing an etching mask at an auxiliary mask stage;
[0044] Figure 7 is a schematic diagram of a prepared etching mask;
[0045] Figure 8 is a schematic illustration of a structure etched in a substrate using an etching mask;
[0046] Fig. 9 is a perspective top view of a structure etched in a substrate and another structure etched in the substrate;
[0047] Fig.10 is a flow chart of an exemplary embodiment of a method for etching a structure in a substrate;
[0048] Fig.11 is a block diagram of an exemplary embodiment of an apparatus for controlling a method for etching a structure in a substrate; and
[0049] Fig.12 is a schematic representation of an exemplary embodiment of various process steps in a method of preparing an etch mask;
[0050] Fig.13 A structure for preparing an etching mask is shown;
[0051] Fig.14 Another structure for preparing an etching mask is shown;
[0052] Fig.15 Another process step is shown. DETAILED DESCRIPTION
[0053] In the following description of advantageous exemplary embodiments of the invention, the same or similar reference numerals are used for elements which are shown in the various figures and have similar effects, wherein a repeated description of these elements is omitted.
[0054] Figure 1 A flow chart of an exemplary embodiment of a method 100 for preparing an etching mask is shown. The method 100 includes a step 105 of providing a substrate, which is a silicon carbide wafer by way of example only. In another exemplary embodiment, the substrate can also be formed of glass, quartz glass, quartz single crystal, silicon (Si), germanium (Ge), BiTe, gallium arsenide (GaAs), indium phosphide (InP), GaInAsP or a polymer.
[0055] After setting step 105, a step 110 of applying a metal layer to the substrate is performed, the metal layer includes a transition metal or aluminum, and the metal layer is chromium (Cr) in this exemplary embodiment. In another exemplary embodiment, the metal layer can also be formed by titanium (Ti), zirconium (Zr), tantalum (Ta), molybdenum (Mo) and additionally or alternatively tungsten (W) and additionally or alternatively aluminum, or include at least one metal in these metals. By way of example only, the metal layer in this exemplary embodiment has a metal layer thickness of 30nm. In other exemplary embodiments, the metal layer thickness can be between 1nm and 200nm. In this exemplary embodiment, the metal layer is applied by vapor deposition. In other exemplary embodiments, the metal layer can also be applied by sputtering.
[0056] Next is step 115, i.e. applying a mask layer to the substrate coated with the metal layer. In this exemplary embodiment, by way of example only, a photoresist layer with a positive resist is used as the mask layer, and the mask layer has a mask layer thickness of 100 nm by way of example only. In another exemplary embodiment, the mask layer thickness may be between 1 nm and 500 nm.
[0057] In a subsequent step 120 of structuring the mask layer, the mask layer is structured, wherein the metal layer is exposed at the processing areas. In this exemplary embodiment, the structuring 120 is performed by exposing and developing a positive resist layer. In another exemplary embodiment, the structuring can also be performed using an electron beam.
[0058] In a subsequent coating step 125, the substrate is coated with a layer of a Group IV element, which in this exemplary embodiment is formed of silicon. In another exemplary embodiment, the Group IV element layer may additionally or alternatively contain other elements of the IV main group, and may additionally or alternatively be formed only of a silicon portion. In this exemplary embodiment, by way of example only, the Group IV element layer has a Group IV element layer thickness of 6nm and is applied by sputtering. In another exemplary embodiment, the Group IV element layer may have a thickness between 1nm and 30nm, and may be applied by vapor deposition. In the coating step 125, an interdiffusion zone between a transition metal or aluminum and a Group IV element is formed in the processing region, at the interface between the metal layer and the Group IV element layer. In this exemplary embodiment, a transition metal silicide layer comprising only Cr3Si is formed. In other exemplary embodiments, TiSi, TiSi2, Ti5Si4, Ti5Si3, ZrSi2, Zr3Si2, Zr3Si, Zr5Si4, TaSi2, Ta5Si3, Cr5Si3, CrSi, CrSi2, MoSi2, Mo3Si, Mo5Si3, WSi2, or W5Si3, or Al xSi y It can also be formed at the interdiffusion region.
[0059] Afterwards, a step 130 of removing the mask layer is performed, wherein in this exemplary embodiment, the Group IV element layer is also at least partially removed. However, the interdiffusion zone remains. Merely by way of example, the mask layer is removed by dissolving it in a solvent. In other exemplary embodiments, the removal step can also be performed by ashing and additionally or alternatively in a wet-chemical manner and additionally or alternatively by a combination of dissolution and chemical removal.
[0060] After removing the mask layer, the next step is to selectively etch the metal layer 135, wherein the substrate is exposed in at least one etching area other than the processing area, and the metal layer is at least partially maintained in the processing area. In this exemplary embodiment, by way of example only, the step 135 of selective etching is performed only by reactive ion beam etching (RIE). In another exemplary embodiment, non-reactive ion beam etching can be used additionally or alternatively. Optionally, selective etching can also and additionally or alternatively utilize acidic etchants and additionally or alternatively halogen-containing etchants to perform in a wet chemical manner.
[0061] Figure 2 An exemplary embodiment of a method 100 for preparing an etching mask is shown. The method 100 shown herein corresponds to or is similar to the method described in the previous figure, except that the method has additional steps. Thus, in this exemplary embodiment, the step 120 of structuring the mask layer is followed by a step 200 of cleaning the surface of the exposed treatment area. Only after cleaning is the step 125 of coating the substrate with the layer of the fourth group element performed in this exemplary embodiment performed.
[0062] Merely by way of example, in this exemplary embodiment, the step 205 of removing the Group IV layer is performed after the coating step 125. The interdiffusion zone remains in the treated area. In this exemplary embodiment, the Group IV layer is removed in a wet chemical manner using potassium hydroxide (KOH). In another exemplary embodiment, the removal step can be performed additionally or alternatively using sodium hydroxide (NaOH) and additionally or alternatively using ammonium hydroxide (NH4OH) and additionally or alternatively using an organic alkaline etchant.
[0063] Figure 3A schematic illustration of an exemplary embodiment of various process steps in a method for preparing an etching mask as described in the previous figures is shown in comparison with conventional process steps. The differences in the conventional structuring strategy are shown in the left column A, and the process steps of the method for preparing an etching mask for tone reversal described in the previous figures are shown in the right column B. In both columns A and B, semi-finished products A1 and B1 of the same shape are shown at the top of the figures shown herein. Semi-finished products A1 and B1 each include a substrate 300, which is a silicon wafer by way of example only, and the substrate 300 is coated with a metal layer 305 in each case, which is a layer formed by chromium by way of example only. In each case, a mask layer 310 is arranged on the metal layer 305, which is formed as a positive photoresist layer in this exemplary embodiment. Semi-finished products A1 and B1 are shown in the step of structuring the mask layer as described in the previous figures, and are therefore under the influence of exposure 315.
[0064] By developing the exposed mask layer 310, structuring is performed, wherein the metal layer 305 is exposed at the processing area 320, as shown in the diagrams shown here using semi-finished products A2 and B2. Up to now, the semi-finished products A1 and B1 and semi-finished products A2 and B2 do not show any difference from each other.
[0065] The difference in the production method can only be identified from the semi-finished product B3 shown in the right column B. The semi-finished product B3 is coated along the mask layer 310 and in the processing area 320 along the metal layer 305 and the additional group IV element layer 325, which in this exemplary embodiment, by way of example only, is formed of silicon and has a group IV element layer thickness of 10 nm. Here, an interdiffusion zone 330 between the transition metal or optionally aluminum and the group IV element is formed in the processing area 320 at the interface between the metal layer 305 and the group IV element layer 325.
[0066] In the figure shown here, the semi-finished product B4 after partial removal of the Group IV element layer 325 is shown in the right column B below the semi-finished product B3. Here, the Group IV element layer 325 is selectively removed except for the interdiffusion region 330 without leaving a silicon sheet or fence.
[0067] In the illustration shown here, a semi-finished product B5 is shown below the semi-finished product B4 in which the mask layer 310 has been removed. The semi-finished product B5 still has an interdiffusion region 330 .
[0068] In the illustration shown here, the semi-finished product B6 shown below the semi-finished product B5 is contrasted with the semi-finished product A6 shown in the left column A. Although on the semi-finished product A6, the substrate 300 is exposed only in the processing area 320 by RIE etching with a resist mask, which is exactly the opposite of the case of the semi-finished product B6. Here, the substrate 300 is exposed in the first etching area 335 and the second etching area 340, while the etching of the metal layer 305 in the processing area 320 has been blocked by the interdiffusion region 330.
[0069] In the conventional structuring strategy shown in column A, the mask layer is only now removed, as shown in semi-finished product A7. Subsequently, it is possible to transfer the pattern to the substrate 300, as shown in semi-finished products A8 and B8. Semi-finished products A8 and B8 therefore have a pattern with a tone inversion. Thus, in the conventionally prepared semi-finished product A8, the pattern is introduced into the substrate 300 below the processing area 320, while in the semi-finished product B8 prepared by the new preparation method proposed in the previous figures, the pattern is introduced into the substrate 300 below the etching areas 335, 340. In other words, compared to the very thin CrSi mask on the semi-finished product B8, the semi-finished product A8 shows chrome etching with a thick resist mask, which avoids shadow effects and charging effects at the edges of the resist.
[0070] Figure 4 Schematic diagram of a structure 400 for preparing an etching mask is shown. The left partial figure shows a cross-sectional view of the structure 400, while the right partial figure shows a top view of the structure 400. The structure 400 is previously Figure 1 and Figure 2 3 and comprises a substrate 300 coated with a metal layer 305 and a structured mask layer 310. In a processed area 320, the metal layer 305 is exposed, resulting in a flat-shaped hole in the structure 400. In other words, this figure shows the resist pattern after development. Figure 1 and Figure 2 Described is a method of etching a mask having 10 10 A pinhole array of 10 holes (also referred to as pinholes) and an exemplary 600 nm hexagonal region were used as demonstration patterns in this exemplary embodiment to test the processing capabilities of key CDs. UV exposure was performed with an i-line stepper.
[0071] Figure 5 A schematic diagram of a structure 400 for preparing an etching mask is shown. The left partial figure shows a cross-sectional view of the structure 400, while the right partial figure shows a top view of the structure 400. The structure shown here corresponds to or is similar to the previous Figure 4, except that the structure 400 shown here is coated with an additional Group IV element layer 325. In other words, this figure shows the resist after being coated with silicon.
[0072] Figure 6 A schematic diagram of a structure 400 for preparing an etching mask in the auxiliary mask stage is shown. The left partial figure shows a cross-sectional view of the structure 400, while the right partial figure shows a top view of the structure 400. The structure shown here corresponds to or is similar to the previous Figure 4 , except that the mask layer is removed in the structure 400 shown here. Therefore, the structure 400 has an interdiffusion zone 330 passivated with a Group IV element layer 325, which is arranged between the etched areas 335, 340 of the exposed metal layer. In other words, this figure shows a modified Cr surface after Si etching with KOH and resist strips. The surface modification shows some contrast in the SEM. Due to the roughness of the Cr surface, the thickness of the modified area is difficult to measure, but the pinholes look more like shallow holes than protrusions.
[0073] Figure 7 A schematic diagram of the prepared etching mask is shown. The left partial figure shows a cross-sectional view of the structure 400, while the right partial figure shows a top view of the structure 400 etched in the substrate. The structure shown here corresponds to or is similar to the previous Figure 4 , except that the metal layer 305 is removed at the etched areas. In other words, this figure shows the chrome after RIE-Cl etching. The result is a reduction in the Cr dot diameter. The right image of the tilted sample shows a very thin under-etched film 700 located on the upper side of the Cr dot. This is probably the interdiffusion area remaining after the under-etching. The tone inversion is produced in this step.
[0074] Figure 8 400 is a schematic diagram of a structure etched in a substrate using an etching mask. The left partial figure shows a cross-sectional view of the structure 400, while the right partial figure shows a top view of the structure 400 etched in the substrate. The structure shown here corresponds to or is similar to the previous Figure 4 The structure described in , except that the substrate 300 below the etched areas 335, 340 is partially removed. Thus, the pattern transferred to the substrate by RIE-F etching is shown. After the pattern is transferred to the substrate using RIE-F, the proposed process is completed. Figure 7 The thin layer residue in the fluorine-based plasma has disappeared. This corresponds to the etching behavior of the interdiffusion zone in the fluorine-based plasma and ToF-SIMS analysis.
[0075] Fig. 9A perspective top view of a structure 400 etched in a substrate and another structure 900 etched in a substrate is shown. Figure 3 Another structure 900 is prepared by the conventional process described above, and conventional positive photolithography and RIE using an aperture mask are shown. Structure 400 is previously Figure 1 and Figure 2 Results of the method described in for preparing an etch mask for tone inversion. The same photomask and the same resist process were used to produce structure 400 and another structure 900. In order to visualize the results of tone inversion, the results are compared with patterns from conventional positive lithography. The same photomask was used for this. The images of the conventional process sequence show the sample after removal of the Cr etch mask. The Cr etch mask is still present in the tone inverted sample. The increased bottom roughness may be due to the special glass substrate, which is known to have increased bottom roughness after RIE etching.
[0076] Fig.10 A flow chart of an exemplary embodiment of a method 1000 for etching a structure in a substrate is shown. The method includes a step 1005 of preparing an etch mask and a step 1010 of performing a deep etch in the substrate using the etch mask. By way of example only, the deep etch in the substrate is performed by RIE or DRIE.
[0077] Fig.11 A block diagram of an exemplary embodiment of an apparatus 1100 for controlling a method for etching a structure in a substrate is shown. The apparatus comprises a preparation unit 1105 for controlling the preparation of an etching mask and an etching unit 1110 for controlling deep etching. In another exemplary embodiment, the apparatus 1100 can also be designed to control the method as previously described. Figure 1 and Figure 2 The method for preparing an etching mask.
[0078] Fig.12 As shown previously Figure 1 and Figure 2 Schematic representation of an exemplary embodiment of various process steps in a method for preparing an etching mask as described in Figure 3 As can be seen from the semi-finished products B6 and B8, a particularly narrow trench is etched in the first etched area 335, especially in accordance with the previously Figure 3 when compared to the process steps shown in the left column. Fig.15 A modification of the exemplary embodiment is shown in which a deep etch in the substrate is followed by subsequent removal of the etching mask, resulting in a semi-finished product or respectively a final product B9 without a metal layer.
[0079] Fig.13 And from Figure 3 The diagram B4 of shows a structure for preparing a mask. The interdiffusion zone 330 shown by the dotted line is formed by a transition metal of the metal layer or an alloy of aluminum and a fourth group element (preferably silicon), wherein the metal layer 310 is covered by the interdiffusion zone 330 in the processing area 320. The metal layer 305 is designed to be continuous, that is, inside and outside the processing area 320 on the substrate 300. In the processing area 320, the mask layer 310 is interrupted. Outside the processing area, the mask layer 310 is directly arranged on the metal layer 305, and the processing area 320 does not contain the material of the mask layer.
[0080] Fig.14 And from Fig.12 Schematic diagram B4 of shows another structure for preparing a mask. Here, the processing region 320 is shown as the interdiffusion region 330 to the left and right of the masking region of the mask layer 310. This structure for preparing a mask can be used to etch trenches in a substrate thereafter.
Claims
1. A method (100) for preparing an etching mask, wherein the method (100) comprises the following steps (105, 110, 115, 120, 125, 130, 135): Provide (105) a substrate (300); Applying (110) a metal layer (305) having a metal layer thickness onto the substrate (300), wherein the metal layer (305) comprises or is formed of at least one transition metal and / or aluminum; Applying (115) at least one mask layer (310) having a mask layer thickness onto the substrate (300) coated with the metal layer (305); Structuring (120) the mask layer (310), wherein the metal layer (305) is exposed in at least one processing area (320); After structuring (120) the mask layer (310), coating (125) the substrate (300) with a Group IV element layer (325) having a Group IV element layer thickness, the Group IV element layer (325) at least partially comprising a Group IV element, wherein an interdiffusion zone (330) is formed at the processing region (320) at an interface between the metal layer (305) and the Group IV element layer (325), wherein the Group IV element layer (325) comprises silicon or is formed of silicon, and the interdiffusion zone (330) is present as a transition metal silicide layer or an aluminum silicide layer; removing (130) the mask layer (310); and The metal layer (305) is selectively etched (135), wherein the substrate (300) is exposed in at least one etched region (335, 340) other than the processed region (320), and the metal layer (305) is at least partially maintained in the processed region (320).
2. The method (100) according to claim 1, comprising a step (205) of removing the Group IV element layer (325), wherein the interdiffusion zone (330) remains at the processing area (320), wherein the removal of the Group IV element layer (325) is performed after the step (125) of applying the Group IV element layer (325) and before the step (130) of removing the mask layer (310), and / or wherein in the step (130) of removing the mask layer (310), the Group IV element layer (325) is at least partially removed.
3. The method (100) according to claim 2, wherein the removal of the Group IV element layer (325) is performed wet-chemically using KOH and / or NaOH and / or NH4OH and / or an organic alkaline etchant.
4. The method (100) according to any one of the preceding claims, wherein in the structuring step (120), the mask layer (310) is structured by exposure and development and / or by means of an electron beam.
5. The method (100) according to claim 1 or 2, wherein in the step (130) of removing the mask layer (310), the mask layer (310) is removed by ashing and / or wet-chemically and / or by dissolving in a solvent and / or by a combination of dissolving and chemical removal, and / or wherein in the selective etching step (135), the etching of the metal layer (305) is performed by reactive ion beam etching (RIE) and / or non-reactive ion beam etching and / or wet-chemically with an acidic and / or halogen-containing etchant.
6. The method (100) according to claim 1 or 2, wherein in the applying step (110), the metal layer (305) consists of Ti, Zr, Ta, Cr, Mo and / or W or includes at least one of these metals, and / or in the setting step (105), the substrate (300) is set as a wafer of glass, quartz single crystal, Si, Ge, BiTe, GaAs, SiC, InP, GaInAsP or a polymer.
7. The method (100) according to claim 1 or 2, wherein the metal layer has a thickness between 1 nm and 2000 nm, and / or the mask layer has a thickness between 1 nm and 500 nm, and / or the Group IV element layer has a thickness between 1 nm and 30 nm.
8. The method (100) according to claim 1 or 2, wherein in the applying step (110), the metal layer (305) is applied by sputtering or vapor deposition, and / or in the coating step (125), the substrate (300) is coated with the layer of the Group IV element (325) by sputtering or vapor deposition.
9. The method (100) according to claim 1 or 2, comprising a step (200) of cleaning the surface of the treatment area (320) after exposure, wherein the cleaning step (200) is performed after the structuring step (120) and before the coating step (125).
10. A method (1000) for etching a structure in a substrate (300), the method (1000) comprising the following steps (1005, 1010): Preparing (1005) an etching mask according to the method (100) for preparing an etching mask as claimed in any one of the preceding claims; as well as Deep etching (1010) is performed in the substrate (300) using the etching mask.
11. The method (1000) of claim 10, wherein the deep etching in the substrate (300) is performed using RIE.
12. The method (1000) of claim 10, further comprising removing the etching mask after the deep etching (1010) of the substrate (300).
13. An apparatus (1100) configured to execute and / or control in a corresponding unit (1105, 1110) the steps (105, 110, 115, 120, 125, 130, 135, 1005, 1010) of a method (100, 1000) according to any of the preceding claims 1 to 12.