Electronic tape and preparation method thereof

By designing an electronic tape containing a central base layer and a deformation layer, and utilizing an alternating magnetic field and acetone dissolved in the expansion core to dissolve the adhesive, the problem of slow adhesion reduction of existing tapes at high temperatures was solved, achieving the effect of quick removal of the back cover.

CN117720861BActive Publication Date: 2024-11-26DIYITE (CHONGQING) NEW MATERIAL TECH CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202311781053.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-21
Publication Date
2024-11-26
Estimated Expiration
2043-12-21

AI Technical Summary

Technical Problem

Existing tapes for electronic products exhibit slow degradation of adhesion at high temperatures and require additional tools for disassembly, impacting repair efficiency.

Method used

Design an electronic tape comprising a central base layer, an upper deformation layer, and a lower deformation layer, with through holes and extension arms between the layers. An alternating magnetic field is used to heat and bend the extension arms, causing them to pierce the base layer. Acetone within the expanded core is used to dissolve the adhesive layer, reducing its stickiness.

Benefits of technology

It enables rapid reduction of tape stickiness under the action of an alternating magnetic field, facilitating tool-free removal of the back cover and improving maintenance efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117720861B_ABST
    Figure CN117720861B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of adhesive tapes, and in particular to an electronic adhesive tape and a preparation method thereof, comprising a middle base layer; a plurality of honeycomb holes are provided through the middle base layer; an upper deformation layer and a lower deformation layer are provided at both ends of the middle base layer; the upper deformation layer and the lower deformation layer are provided with through holes matching the honeycomb holes; upper extension arms and lower extension arms are extended at the through holes of the upper deformation layer and the lower deformation layer respectively; an upper base layer is provided at the top of the upper deformation layer; a lower base layer is provided at the bottom of the lower deformation layer; an upper adhesive layer is provided at the top of the upper base layer; a lower adhesive layer is provided at the bottom of the lower base layer; a placement cavity is formed between the upper base layer, the honeycomb holes, the through holes and the lower base layer; an upper filler layer, an expansion core and a lower filler layer are provided in sequence in the placement cavity. The present invention arranges an expansion core, and the expansion core is heated so that the upper extension arm and the lower extension arm penetrate the upper base layer and the lower base layer, and acetone dissolves the upper adhesive layer and the lower adhesive layer, thereby quickly reducing the viscosity of the adhesive tape.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of adhesive tapes, and in particular to an electronic adhesive tape and a preparation method thereof. Background Art

[0002] As the demand for thinner and lighter electronic products becomes higher and higher, adhesive tape is often used to bond and fix the back cover and body of electronic products. The viscosity of the current adhesive tape for electronic products generally decreases with the increase of temperature. When repairing electronic products, the adhesive parts of the tape are often heated from the outside to reduce the viscosity of the tape, so as to facilitate opening the back cover of the electronic product. Although this method can achieve the purpose of opening the back cover, on the one hand, the tape heats up slowly during the heating process and takes a long time. On the other hand, the tape still has a certain viscosity after being heated, and a suction cup or a pick is still needed to remove the back cover during disassembly, which is not convenient for repair work. Summary of the invention

[0003] The object of the present invention is to provide an electronic adhesive tape and a preparation method thereof in view of the above-mentioned deficiencies in the prior art.

[0004] The object of the present invention is achieved by the following technical scheme: an electronic tape, comprising a middle base layer; a plurality of honeycomb holes are provided through the middle base layer; an upper deformation layer and a lower deformation layer are respectively provided at both ends of the middle base layer; the upper deformation layer and the lower deformation layer are respectively provided with through holes matching the honeycomb holes; the upper deformation layer and the lower deformation layer are respectively extended with upper extension arms and lower extension arms at the through holes;

[0005] An upper base layer is disposed on the top of the upper deformation layer; a lower base layer is disposed on the bottom of the lower deformation layer; an upper adhesive layer is disposed on the top of the upper base layer; and a lower adhesive layer is disposed on the bottom of the lower base layer;

[0006] A placement cavity is formed between the upper substrate layer, the honeycomb holes, the through holes and the lower substrate layer; the placement cavity contains an upper filler layer, an expansion core and a lower filler layer in sequence.

[0007] The present invention is further configured such that the end of the upper extension arm is provided with an upper puncturing portion for puncturing the upper substrate layer; the end of the lower extension arm is provided with a lower puncturing portion for puncturing the lower substrate layer.

[0008] The present invention is further configured such that the number of the upper extension arms is the third; the three upper extension arms are arranged at equal angles in the placement cavity; the number of the lower extension arms is the third; the three lower extension arms are arranged at equal angles in the placement cavity.

[0009] The present invention is further configured such that the upper deformation layer includes a first expansion layer and a second expansion layer; the first expansion layer is arranged on the top of the middle base layer; the second expansion layer is arranged on the top of the first expansion layer; the upper base layer is arranged on the top of the second expansion layer; the thermal expansion coefficient of the first expansion layer is greater than the thermal expansion coefficient of the second expansion layer;

[0010] The lower deformation layer includes a third expansion layer and a fourth expansion layer; the third expansion layer is arranged at the bottom of the middle base layer; the fourth expansion layer is arranged at the bottom of the third expansion layer; the lower base layer is arranged at the bottom of the fourth expansion layer; the thermal expansion coefficient of the third expansion layer is greater than the thermal expansion coefficient of the fourth expansion layer.

[0011] The present invention is further configured such that an upper release layer is provided on the top of the upper adhesive layer; and a lower release layer is provided on the bottom of the lower adhesive layer.

[0012] The present invention is further configured such that the expansion core includes a glass fiber layer, an upper inorganic foaming agent layer arranged on the top of the glass fiber layer, and a lower inorganic foaming agent layer arranged on the bottom of the glass fiber layer; acetone is adsorbed in the glass fiber layer; and metal particles are provided in both the upper inorganic foaming agent layer and the lower inorganic foaming agent layer.

[0013] The present invention is further configured such that the material of the middle base layer is PET, PE or PP; the material of the upper base layer and the material of the lower base layer are PET, PE or PP.

[0014] The present invention is further configured such that the material of the first expansion layer and the material of the third expansion layer are LDPE; the material of the second expansion layer and the material of the fourth expansion layer are PET.

[0015] The present invention is further configured that the material of the upper inorganic foaming agent layer and the material of the lower inorganic foaming agent layer are sodium bicarbonate, ammonium bicarbonate or ammonium nitrite; the metal particles are iron, ferrosoferric oxide and / or aluminum;

[0016] The material of the upper filler layer and the material of the lower filler layer are resins soluble in acetone.

[0017] Beneficial effects of the present invention: the present invention provides an expandable core, and the expandable core is heated so that the upper extension arm and the lower extension arm penetrate the upper base layer and the lower base layer, and acetone dissolves the upper adhesive layer and the lower adhesive layer, thereby quickly reducing the viscosity of the tape. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] The invention is further described using the accompanying drawings, but the embodiments in the accompanying drawings do not constitute any limitation to the invention. A person skilled in the art can obtain other drawings based on the following drawings without creative work.

[0019] Figure 1 It is a schematic diagram of the structure of the present invention;

[0020] Figure 2 is a cross-sectional view of the present invention;

[0021] Figure 3is a cross-sectional view of the present invention after hiding the upper filler layer, the expansion core and the lower filler layer;

[0022] Figure 4 is a structural exploded view of the present invention;

[0023] Figure 5 It is a schematic diagram of the structure of the present invention after hiding the upper release layer, the lower release layer, the upper adhesive layer, the lower adhesive layer, the upper base layer and the lower base layer;

[0024] Figure 6 It is a structural exploded view of the present invention after hiding the upper release layer, the lower release layer, the upper adhesive layer, the lower adhesive layer, the upper base layer and the lower base layer;

[0025] Figure 7 An exploded view of the structure of the upper filler layer, the expansion core and the lower filler layer of the present invention;

[0026] Among them: 1. middle base layer; 11. honeycomb hole; 2. upper deformation layer; 21. first expansion layer; 22. second expansion layer; 23. through hole; 24. upper extension arm; 25. upper stab part; 3. lower deformation layer; 31. third expansion layer; 32. fourth expansion layer; 33. lower extension arm; 34. lower stab part; 41. upper base layer; 42. lower base layer; 51. upper adhesive layer; 52. lower adhesive layer; 6. placement cavity; 61. upper filler layer; 62. lower filler layer; 71. upper release layer; 72. lower release layer; 8. glass fiber layer; 81. upper inorganic foaming agent layer; 82. lower inorganic foaming agent layer. DETAILED DESCRIPTION

[0027] The present invention is further described in conjunction with the following examples.

[0028] Depend on Figures 1 to 7 It can be seen that an electronic tape of this embodiment includes a middle base layer 1; a plurality of honeycomb holes 11 are formed through the middle base layer 1; an upper deformable layer 2 and a lower deformable layer 3 are respectively formed at both ends of the middle base layer 1; the upper deformable layer 2 and the lower deformable layer 3 are respectively provided with through holes 23 matching the honeycomb holes 11; the upper deformable layer 2 and the lower deformable layer 3 are respectively extended with upper extension arms 24 and lower extension arms 33 at the through holes 23;

[0029] An upper base layer 41 is disposed on the top of the upper deformation layer 2; a lower base layer 42 is disposed on the bottom of the lower deformation layer 3; an upper adhesive layer 51 is disposed on the top of the upper base layer 41; and a lower adhesive layer 52 is disposed on the bottom of the lower base layer 42;

[0030] A placement cavity 6 is formed between the upper substrate layer 41 , the honeycomb holes 11 , the through holes 23 and the lower substrate layer 42 ; an upper filler layer 61 , an expansion core and a lower filler layer 62 are sequentially arranged in the placement cavity 6 .

[0031] Specifically, when in use, the edges of the honeycomb holes 11 of the middle base layer 1 are die-cut to form the required shape, and the integrity of the honeycomb holes 11 is maintained during the die-cutting process to prevent the honeycomb holes 11 from being cut; after the die-cutting is completed, the upper release layer 71 and the lower release layer 72 are peeled off, one side is pasted to the specified position of the electronic product body, and the other side is pasted to the specified position of the back cover, thus completing the bonding and fixing of the electronic product and the back cover.

[0032] When the back cover needs to be separated from the electronic product body, an alternating magnetic field is applied to the position where the tape is pasted on the electronic product, so that the expansion core is heated under the action of the external alternating magnetic field; thereby, the upper extension arm 24 and the lower extension arm 33 inside the accommodating cavity are heated and heated, and the upper extension arm 24 and the lower extension arm 33 are bent by the heat, thereby piercing the upper base layer 41 and the lower base layer 42, so that the accommodating cavity is connected with the upper adhesive layer 51 and the lower adhesive layer 52 respectively; the acetone in the expansion core dissolves the upper adhesive layer 51 and the lower adhesive layer 52, so that the viscosity of the upper adhesive layer 51 and the lower adhesive layer 52 is greatly reduced, which facilitates the separation of the back cover and the electronic product body.

[0033] In the electronic tape of this embodiment, an upper piercing portion 25 for piercing the upper base layer 41 is provided at the end of the upper extension arm 24 ; a lower piercing portion 34 for piercing the lower base layer 42 is provided at the end of the lower extension arm 33 .

[0034] In the electronic tape of this embodiment, the number of the upper extension arms 24 is the third; the three upper extension arms 24 are arranged at equal angles in the placement cavity 6; the number of the lower extension arms 33 is the third; the three lower extension arms 33 are arranged at equal angles in the placement cavity 6. Through the above arrangement, the upper base layer 41 and the lower base layer 42 can be effectively punctured.

[0035] In the electronic tape of the present embodiment, the upper deformation layer 2 includes a first expansion layer 21 and a second expansion layer 22; the first expansion layer 21 is arranged on the top of the middle base layer 1; the second expansion layer 22 is arranged on the top of the first expansion layer 21; the upper base layer 41 is arranged on the top of the second expansion layer 22; the thermal expansion coefficient of the first expansion layer 21 is greater than the thermal expansion coefficient of the second expansion layer 22; the lower deformation layer 3 includes a third expansion layer 31 and a fourth expansion layer 32; the third expansion layer 31 is arranged on the bottom of the middle base layer 1; the fourth expansion layer 32 is arranged on the bottom of the third expansion layer 31; the lower base layer 42 is arranged on the bottom of the fourth expansion layer 32; the thermal expansion coefficient of the third expansion layer 31 is greater than the thermal expansion coefficient of the fourth expansion layer 32. In the electronic tape of the present embodiment, an upper release layer 71 is arranged on the top of the upper adhesive layer 51; and a lower release layer 72 is arranged on the bottom of the lower adhesive layer 52. In the electronic tape of the present embodiment, the expansion core comprises a glass fiber layer 8, an upper inorganic foaming agent layer 81 disposed on the top of the glass fiber layer 8, and a lower inorganic foaming agent layer 82 disposed on the bottom of the glass fiber layer 8; acetone is adsorbed in the glass fiber layer 8; metal particles are disposed in both the upper inorganic foaming agent layer 81 and the lower inorganic foaming agent layer 82. The acetone is produced by Panjin Gucheng Chemical Reagent Co., Ltd.

[0036] When it is necessary to separate the back cover from the electronic product body, an alternating magnetic field is applied to the position where the tape is pasted on the electronic product, so that the metal particles in the upper inorganic foaming agent layer 81 and the lower inorganic foaming agent layer 82 are heated under the action of the external alternating magnetic field, and the foaming agent attached to the surface of the metal particles is inductively heated; during the heating process of the metal particles, the upper extension arm 24 and the lower extension arm 33 in the accommodating cavity are heated, because the thermal expansion coefficient of the first expansion layer 21 is greater than that of the second expansion layer 22, and the thermal expansion coefficient of the third expansion layer 31 is greater than that of the fourth expansion layer 32. Thermal expansion coefficient; therefore, the deformation of the first expansion layer 21 is greater than that of the second expansion layer 22 during the temperature increase of the upper extension arm 24; the deformation of the third expansion layer 31 is greater than that of the fourth expansion layer 32 during the temperature increase of the lower extension arm 33; so that the upper extension arm 24 bends toward the top and the lower extension arm 33 bends toward the bottom; during the bending process, the upper stab portion 25 contacts and pierces the upper base layer 41, and the lower stab portion 34 contacts and pierces the lower base layer 42, so that the top and bottom of the accommodating cavity are connected to the upper adhesive layer 51 and the lower adhesive layer 52 respectively;

[0037] At the same time, the upper inorganic foaming agent layer 81 and the lower inorganic foaming agent layer 82 are decomposed under the heating of the metal particles, thereby generating gas and producing a foaming effect on the upper filler layer 61 and the lower filler layer 62, so that the volume of the upper filler layer 61 and the lower filler layer 62 expands, and the liquid acetone and the gaseous acetone in the accommodating cavity are squeezed into the upper adhesive layer 51 and the lower adhesive layer 52, and the upper adhesive layer 51 and the lower adhesive layer 52 are dissolved, so that the viscosity of the upper adhesive layer 51 and the lower adhesive layer 52 is greatly reduced, which facilitates the separation of the back cover and the electronic product body;

[0038] At the same time, after the upper filler layer 61 and the lower filler layer 62 are foamed, the thickness of the entire tape layer will increase, which can further separate the back cover from the electronic product body, so that the operator can separate the back cover from the electronic product body by hand without using tools such as picks.

[0039] In the electronic tape of this embodiment, the material of the middle base layer 1 is PET, PE or PP; the material of the upper base layer 41 and the material of the lower base layer 42 are PET, PE or PP. PET is a PET film with model number PET11 T manufactured by Dongguan Lingmei New Materials Co., Ltd.; PP is a PP film manufactured by Guangzhou Huirui Packaging Materials Co., Ltd.

[0040] In the electronic tape of this embodiment, the material of the first expansion layer 21 and the material of the third expansion layer 31 are LDPE; the material of the second expansion layer 22 and the material of the fourth expansion layer 32 are PET. The LDPE is an LDPE film with a model number of XT2023 produced by Qingdao Sanyuan Packaging Co., Ltd.; the PET is a PET film with a model number of PET11 T produced by Dongguan Lingmei New Materials Co., Ltd.;

[0041] The thermal expansion coefficient of LDPE is 200-400x 10^-6 / ℃; the thermal expansion coefficient of PET is 70-90x 10^-6 / ℃.

[0042] In the electronic tape of the present embodiment, the material of the upper inorganic foaming agent layer 81 and the material of the lower inorganic foaming agent layer 82 are sodium bicarbonate, ammonium bicarbonate or ammonium nitrite; the metal particles are iron, ferroferric oxide and / or aluminum; the sodium bicarbonate is sodium bicarbonate produced by Weifang Ruidesheng Chemical Co., Ltd.; the material of the upper filler layer 61 and the material of the lower filler layer 62 are resins soluble in acetone.

[0043] The upper filler layer 61 and the lower filler layer 62 are filled in the accommodating cavity, and can be foamed after the upper inorganic foaming agent layer 81 and the lower inorganic foaming agent decompose to generate gas, thereby expanding the volume; the upper filler layer 61 and the lower filler layer 62 are resins soluble in acetone, preferably polyurethane resins; the polyurethane resin can be a polyurethane resin of model C59 D53 produced by BASF; the acetone absorbed in the glass fiber layer 8 can be released into the accommodating cavity to dissolve the upper filler layer 61 and the lower filler layer 62, thereby forming a polyurethane resin solution.

[0044] A method for preparing an electronic tape according to the present embodiment comprises the following steps:

[0045] S1, preparing a plurality of evenly distributed honeycomb holes 11 on the middle base layer 1 by die-cutting process;

[0046] S2, a plurality of through holes 23 corresponding to the honeycomb holes 11 are prepared in the first expansion layer 21, the second expansion layer 22, the third expansion layer 31 and the fourth expansion layer 32 by die-cutting process, and a plurality of upper extension arms 24 and lower extension arms 33 extending into the through holes 23 are retained on the side walls of the through holes 23; sharp upper protruding portions 25 and lower protruding portions 34 are die-cut at the front ends of the upper extension arms 24 and the lower extension arms 33;

[0047] After die-cutting is completed, the first expansion layer 21 and the second expansion layer 22 are welded and compounded to form the upper deformation layer 2, and the third expansion layer 31 and the fourth expansion layer 32 are welded and compounded to form the lower deformation layer 3 through an ultrasonic compounding process; the welding frequency is controlled at 20KHz, the amplitude is controlled within the range of 20-30um; the welding time is controlled within the range of 0.2-0.3S;

[0048] S3, pass the metal particles through a 350 mesh sieve to control the particle size within the range of 30-35um; after completion, fully mix 15-30 parts by weight of an inorganic foaming agent, 25-30 parts by weight of metal particles, and 5-15 parts by weight of an epoxy resin, crush them after curing, pass through a 200 mesh sieve, control the particle size within the range of 70-75um, and obtain an upper inorganic foaming agent layer 81 and a lower inorganic foaming agent layer 82;

[0049] S4, spraying 0.3-0.6 parts by weight of epoxy resin onto the surface of the glass fiber layer 8, and after completion, spraying the upper inorganic foaming agent layer 81 and the lower inorganic foaming agent layer 82 obtained in step S3 onto the surface of the glass fiber; after curing, die-cutting the glass fiber into a granular expansion core having a diameter smaller than the diameter of the honeycomb hole 11;

[0050] S5, attaching the lower deformation layer 3 obtained in step S2 to the lower base layer 42; after completion, attaching the middle base layer 1 obtained in step S1 to the top of the lower deformation layer 3; after completion, welding the lower base layer 42, the lower deformation layer 3 and the middle base layer 1 together through an ultrasonic composite process; the welding frequency is controlled at 20KHz, the amplitude is controlled within the range of 30-35um; the welding time is controlled within the range of 0.3-0.4S;

[0051] S6, after completing step S5, 3-8 parts of the lower filler layer 62 are placed in the accommodating cavity; then the expanded core obtained in step S4 is placed on top of the lower filler layer 62, and 5-15 parts by weight of acetone are dripped into the expanded core until the acetone overflows the glass fiber and is stored in the accommodating cavity; after completion, 3-8 parts of the upper filler layer 61 are placed on top of the expanded core;

[0052] S7, after the upper filler layer 61 and the lower filler layer 62 are dissolved in acetone, the upper deformable layer 2 is attached to the surface of the middle base layer 1; after completion, the upper base layer 41 is attached to the surface of the upper deformable layer 2; after completion, the layers are welded and compounded by an ultrasonic compounding process so that the accommodating cavity forms a closed cavity; the welding frequency is controlled at 20KHz, the amplitude is controlled within the range of 40-60um; the welding time is controlled within the range of 0.3-0.6S;

[0053] S8. After completing step S7, an upper adhesive layer 51 and a lower adhesive layer 52 are coated on the upper base layer 41 and the lower base layer 42 respectively. After completion, an upper release layer 71 and a lower release layer 72 are attached to the upper adhesive layer 51 and the lower adhesive layer 52 respectively. After completion, the adhesive tape is rolled up to obtain the adhesive tape for electronic products.

[0054] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention, rather than to limit the scope of protection of the present invention. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the essence and scope of the technical solution of the present invention.

Claims

1. An electronic tape, characterized in that: The method comprises the following preparation steps: S1, preparing a plurality of evenly distributed honeycomb holes on the middle base layer through a die-cutting process; S2, a plurality of through holes corresponding to the honeycomb holes are prepared in the first expansion layer, the second expansion layer, the third expansion layer and the fourth expansion layer by a die-cutting process, and a plurality of extension arms extending into the through holes are retained on the side walls of the through holes; a sharp thorn portion is die-cut at the front end of the extension arm; After die-cutting is completed, the first expansion layer and the second expansion layer are welded and compounded to form an upper deformation layer, and the third expansion layer and the fourth expansion layer are welded and compounded to form a lower deformation layer through an ultrasonic compound process; the welding frequency is controlled at 20KHz, and the amplitude is controlled within the range of 20-30um; the welding time is controlled within the range of 0.2-0.3S; the thermal expansion coefficient of the first expansion layer is greater than the thermal expansion coefficient of the second expansion layer; the thermal expansion coefficient of the third expansion layer is greater than the thermal expansion coefficient of the fourth expansion layer; S3, the metal particles are sieved through a 350 mesh sieve to control the particle size within the range of 30-35um; after completion, 15-30 parts by weight of an inorganic foaming agent, 25-30 parts by weight of metal particles, and 5-15 parts by weight of an epoxy resin are fully mixed, crushed after curing, sieved through a 200 mesh sieve, and the particle size is controlled within the range of 70-75um to obtain an upper inorganic foaming agent layer and a lower inorganic foaming agent layer; S4, spraying 0.3-0.6 parts by weight of epoxy resin onto the surface of the glass fiber layer, and after completion, spraying the upper inorganic foaming agent layer and the lower inorganic foaming agent layer obtained in step S3 onto the surface of the glass fiber; after curing, die-cutting the glass fiber into a granular expansion core having a diameter smaller than the diameter of the honeycomb hole; S5, attaching the lower deformation layer obtained in step S2 to the lower base layer; after completion, attaching the middle base layer obtained in step S1 to the top of the lower deformation layer; after completion, welding the lower base layer, the lower deformation layer and the middle base layer together through an ultrasonic composite process; the welding frequency is controlled at 20KHz, the amplitude is controlled within the range of 30-35um; the welding time is controlled within the range of 0.3-0.4S; S6, after completing step S5, 3-8 parts of the lower filler layer are placed in the accommodating cavity; then the expanded core obtained in step S4 is placed on top of the lower filler layer, and 5-15 parts by weight of acetone are dripped into the expanded core until the acetone overflows the glass fiber and is stored in the accommodating cavity; after completion, 3-8 parts of the upper filler layer are placed on top of the expanded core; S7, after the upper filler layer and the lower filler layer are dissolved in acetone, the upper deformation layer is attached to the surface of the middle base layer; after completion, the upper base layer is attached to the surface of the upper deformation layer; after completion, the layers are welded and compounded by an ultrasonic compound process so that the accommodating cavity forms a closed cavity; the welding frequency is controlled at 20KHz, the amplitude is controlled within the range of 40-60um; the welding time is controlled within the range of 0.3-0.6S; S8. After completing step S7, an upper adhesive layer and a lower adhesive layer are coated on the upper base layer and the lower base layer respectively. After completion, an upper release layer and a lower release layer are attached to the upper adhesive layer and the lower adhesive layer respectively; after completion, the adhesive is rolled up.

Citation Information

Patent Citations

  • Adhesive tape capable of losing stickiness through pyrolysis

    CN105131860A

  • Expansion debonding adhesive tape and production method thereof

    CN108913051A

  • Vertical conductive pyrolysis adhesive tape and preparation method thereof

    CN109762483A

  • Adhesive and preparation method thereof, and adhesive layer and heat-reducing adhesive tape prepared from adhesive

    CN110938394A

  • Low-temperature thermal visbreaking adhesive tape and preparation method thereof

    CN111647365A