A high temperature alloy turbine vacuum casting equipment and casting process thereof
By using program-controlled cooling fans and vacuum pumps in high-temperature alloy turbine vacuum casting equipment, combined with heating components and circulating cooling systems, the problem of insufficient cooling speed control is solved, cracks and oxidation of turbine castings are avoided, and product quality and reliability are improved. sex.
Patent Information
- Application Number
- CN202410734435.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-07
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-06-07
AI Technical Summary
During the vacuum casting process of high-temperature alloy turbines, existing cooling treatment methods cannot effectively control the cooling rate, resulting in increased internal stress in the turbine castings and possible cracks, affecting its performance and reliability.
A high-temperature alloy turbine vacuum casting equipment is designed, including casting components and injection molding components. A program-controlled cooling fan is used to gradually increase the wind power. Combined with a vacuum pump and heating components, the cooling rate of turbine castings is controlled through the mold closing state and circulating cooling system. Adaptive adjustment and oxidation prevention.
It effectively avoids surface deformation and pore defects caused by excessive cooling rate of turbine castings, ensuring product quality, reducing oxidation through a vacuum environment, and improving mechanical performance and reliability.
Smart Images

Figure CN118385523B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of casting equipment, and in particular relates to a high-temperature alloy turbine vacuum casting equipment and a casting process thereof. Background Art
[0002] Casting is one of the basic processes in the modern machinery manufacturing industry. As a metal heat processing process, casting has gradually matured in my country. Casting machinery uses this technology to melt metal into a liquid that meets certain requirements and pour it into a mold. After cooling, solidification and cleaning, all mechanical equipment that can be used to obtain castings with predetermined shapes, sizes and performances is also called casting equipment. At present, aluminum alloy casting equipment is widely used in automobile processing, building materials and mechanical processing steps. With the widespread expansion and application of die-casting technology, reducing the loss of alloy metals in the manufacturing process and improving the quality of metal forging have become important requirements.
[0003] At present, in the vacuum casting process of high-temperature alloy turbines, the cooling treatment after the casting of the turbine casting is a crucial link. The cooling process not only affects the microstructure and performance of the casting, but is also directly related to the quality and life of the turbine casting. The existing cooling treatment method has obvious deficiencies in controlling the cooling rate. Since the cooling rate of water is relatively fast, an excessively fast cooling rate may cause stress or cracks inside the turbine casting. This is because the internal organization and structure of the high-temperature alloy undergo a complex phase change process during the solidification process. If the cooling rate is too fast, the temperature gradient inside the turbine casting will increase rapidly, resulting in inconsistent shrinkage rates in different parts, thereby generating internal stress. When the internal stress exceeds the tensile strength of the turbine casting, cracks will occur, seriously affecting the performance and reliability of the turbine casting. Therefore, there are deficiencies and it cannot meet the production and use needs of the turbine. Therefore, further improvements are necessary.
[0004] Therefore, in view of this, the existing structure and defects are studied and improved, and a high-temperature alloy turbine vacuum casting equipment and a casting process thereof are provided, in order to achieve a more practical purpose. Summary of the invention
[0005] In order to solve the above technical problems, the present invention provides a high-temperature alloy turbine vacuum casting equipment, which is achieved by the following specific technical means:
[0006] A high-temperature alloy turbine vacuum casting equipment, comprising a machine base, a fixing frame arranged on the machine base, and a control box arranged on the front side of the machine base, characterized in that it also comprises a casting component arranged on the machine base for casting turbine castings, and an injection molding component arranged on the right side of the machine base for material injection molding;
[0007] The casting assembly comprises a lower mold and an upper mold, wherein the upper mold and the lower mold are provided with a mold cavity for casting the turbine, and the lower mold is provided with an inner cavity, and the inner cavity is provided with cooling water for cooling the turbine casting formed in the mold cavity;
[0008] A cooling mechanism for cooling and circulating cooling water is arranged on the left side of the lower mold, and the cooling mechanism includes a cooling shell fixedly mounted on the left side of the lower mold, a cooling jacket fixedly mounted on the front side of the cooling shell, and a circulation component for circulating and cooling cooling water in the cavity of the lower mold is arranged inside the cooling shell, and a dustproof plate, a cooling fan and an adjustment component are respectively arranged in the cooling jacket from front to back, and the cooling fan is driven to drive external cooling air to enter the cooling shell along the adjustment component, and the cooling air is blown onto the circulation component to gradually cool the circulating cooling water.
[0009] As a further description of the above technical solution: the wind force of the cooling fan is driven to increase gradually from small to large through program control, and the cooling speed of the turbine casting can be adaptively adjusted through this setting, which can effectively avoid the problem of surface deformation, pores and other quality defects of the turbine casting caused by the fast cooling rate of the turbine casting in the mold cavity. The product quality of the turbine casting can be ensured by effectively and reasonably controlling the cooling speed of the turbine casting.
[0010] Further, the casting assembly also includes a bottom plate and a top plate, and the top plate is located directly above the bottom plate, the upper side of the bottom plate is fixedly assembled with the lower mold, the bottom of the top plate is fixedly assembled with the upper mold, and four symmetrically distributed fixed slide bars are fixedly installed on the upper side of the bottom plate and located on the outer periphery of the lower mold, the upper ends of the four fixed slide bars are all passed through the top plate, and at least partially protrude from the upper side of the top plate, and the four fixed slide bars are slidably installed with the top plate;
[0011] Four symmetrically arranged guide columns are fixedly mounted on the bottom of the upper die, and four guide grooves corresponding to the guide columns are opened on the upper side of the lower die. The guide columns and the guide grooves are mounted by matching.
[0012] As a further description of the above technical solution: the piston rod of the hydraulic cylinder pushes the top plate and the upper mold downward, and the top plate slides on the fixed slide rod to ensure the stability of the upper mold downward movement. As the upper mold continues to move downward, the guide column is inserted into the guide groove, so that the upper mold and the lower mold form a closed mold state.
[0013] Furthermore, the casting assembly also includes a hydraulic cylinder, which is fixedly mounted on the upper surface of the fixing frame, and the bottom of the hydraulic cylinder passes through the fixing frame and is fixedly connected to the top plate by a piston rod, and the right sides of the lower mold and the upper mold are both provided with injection ports for pouring alloy materials;
[0014] Among them, a vacuum pump is fixedly installed on the front side of the upper mold, a ventilation channel is opened on the front side of the upper mold, and an exhaust one-way valve is provided in the ventilation channel. The vacuum pump is fixedly connected to the exhaust one-way valve via a ventilation pipe. By driving the vacuum pump to operate, the mold cavities of the upper mold and the lower mold are evacuated to a vacuum environment.
[0015] As a further description of the above technical solution: the environment of the mold cavity in the upper mold and the lower mold is evacuated to a vacuum environment through a vacuum pump, and by evacuating the mold cavity environment to a vacuum environment, it helps to reduce the contact of the alloy material with oxygen in the air during the melting and pouring process, effectively preventing oxidation, and at the same time being able to provide high-quality turbine castings to ensure the mechanical properties and reliability of the turbine castings.
[0016] Furthermore, a heating assembly is provided in the machine base, and the heating assembly includes a heater fixedly assembled in the machine base and a heating tube arranged in the cavity in the lower mold, and the lower end of the heating tube is fixedly connected to the heater. The heater is driven to make the heating tube generate heat to heat the cooling water in the cavity in the lower mold.
[0017] As a further description of the above technical solution: the cooling water in the cavity of the lower mold is preheated by a heating pipe to avoid the low cooling water temperature affecting the product quality of the turbine casting, so that it can be gradually cooled and formed.
[0018] Furthermore, the circulation component includes a circulation pump fixedly mounted on the cooling shell, a connecting head fixedly mounted on the side of the circulation pump close to the lower mold, and an end of the connecting head away from the circulation pump passes through the lower mold and communicates with the cooling water in the inner cavity, a circulation pipe for cooling the cooling water is fixedly mounted on the side of the circulation pump away from the connecting head, and the circulation pipe is in a conical shape that is narrow in front and wide in the back.
[0019] As a further description of the above technical solution: the cooling water in the cavity of the lower mold is driven into the circulation pipe for cooling through a circulation pump. At the same time, the circulation pipe is arranged to be narrow in the front and wide in the back, so that the cooling air can cool the circulation pipe from front to back, which can effectively speed up the cooling rate of the cooling water in the circulation pipe.
[0020] Furthermore, a fixing bracket is fixedly mounted on the cooling fan, and an outer wall of the fixing bracket is fixedly mounted on an inner wall of the cooling jacket;
[0021] A cleaning assembly is provided on the inner side of the circulation pipe, and the cleaning assembly includes a rotating rod fixedly mounted on the cooling fan, and one end of the rotating rod away from the cooling fan passes through the adjusting assembly and is located at the central axis of the circulation pipe, a cleaning rod is fixedly mounted on the outer periphery of the rotating rod, and a cleaning brush for cleaning dust on the surface of the circulation pipe is fixedly mounted on the outer end of the cleaning rod.
[0022] As a further description of the above technical solution: the dust on the surface of the circulation pipe can be effectively removed by using a cleaning brush, which can effectively prevent dust from accumulating on the surface of the circulation pipe and affecting the cooling effect of the cooling water in the circulation pipe. This setting can further improve the cooling effect of the cooling water in the circulation pipe, thereby ensuring the molding quality of the turbine casting.
[0023] Furthermore, the adjustment assembly includes an adjustment seat fixedly mounted on the inner wall of the cooling jacket, an air inlet for cooling air to enter is opened at the central axis of the adjustment seat, a plurality of adjustment plates for shielding the air inlet are movably mounted on the adjustment seat, the adjustment plate is movably mounted on the adjustment seat by rotating the connecting shaft, and a support spring is fixedly connected between the rear side of the adjustment plate and the adjustment seat.
[0024] As a further description of the above technical solution: when the kinetic energy of the cooling fan is large, the wind force of the cooling fan also increases synchronously. Based on the force of the cooling wind, the opening angle of the adjustment plate increases synchronously, so that the cooling channel between the adjustment plates is also increased. At this time, the cooling wind can be blown to all positions on the circulation pipe to achieve cooling of the cooling water inside the circulation pipe.
[0025] Further, the injection molding assembly includes a fixed seat fixedly assembled on the right side of the machine base, a stabilizing slide bar is fixedly installed on the right side of the fixed seat, a fixed plate is fixedly installed on the end of the stabilizing slide bar away from the fixed seat, an injection molding electric telescope is fixedly assembled on the right side of the fixed plate, a movable plate is slidably installed on the stabilizing slide bar, the left side of the injection molding electric telescope is fixedly connected to the movable plate by means of an injection molding telescopic rod, a movable push rod is fixedly installed on the side of the movable plate facing the fixed seat, and the end of the movable push rod away from the movable plate passes through the fixed seat and is fixedly connected to the injection molding device;
[0026] The injector is fixedly equipped with an injection head for turbo-molding the mold cavities in the upper and lower molds, and the upper side of the injector is fixedly equipped with a feed pipe for connecting with external injection materials. The injection electric telescopic device is driven to make the movable push rod push the injector to perform turbo-molding on the mold cavities in the upper and lower molds.
[0027] As a further description of the above technical solution: the injection head on the injection molding machine is connected to the injection port between the upper mold and the lower mold by driving the injection molding electric telescopic device, and then the injection molding machine is driven to drive the alloy material along the injection head to be injected into the mold cavity in the upper mold and the lower mold, thereby realizing the casting of the turbine casting.
[0028] Furthermore, a unloading assembly for unloading the turbine casting is provided inside the machine base, and the unloading assembly includes a fixed base fixedly assembled inside the machine base, and a unloading electric telescope is fixedly assembled on the fixed base. The upper end of the unloading electric telescope is fixedly connected to a unloading ejector pin by a unloading piston rod, and the upper end of the unloading ejector pin is flush with the bottom of the mold cavity of the lower mold. The unloading electric telescope is driven to make the unloading piston rod push the unloading ejector pin to move upward, and the turbine product formed in the mold cavity of the lower mold is ejected and demolded by the unloading ejector pin.
[0029] As a further description of the above technical solution: the unloading electric telescopic device drives the unloading ejector pin to eject the turbine casting formed in the lower mold cavity, thereby realizing the unloading of the formed turbine casting product.
[0030] A high-temperature alloy turbine vacuum casting process comprises the following steps:
[0031] S1: The piston rod of the hydraulic cylinder pushes the upper die downward, causing the upper die and the lower die to form a clamping state;
[0032] S2: The piston rod of the electric injection expander is used to push the injection molding machine to move toward the upper mold and the lower mold, and the injection head on the injection molding machine is connected with the injection port between the upper mold and the lower mold;
[0033] S3: Start the vacuum pump through program control, and use the vacuum pump to evacuate the environment of the upper mold and the lower mold cavity to a vacuum environment, which helps to reduce the contact of the alloy material with oxygen in the air during the melting and pouring process;
[0034] S4: The alloy material is then driven by the injection molding machine to be injected into the mold cavities of the upper mold and the lower mold along the injection head, thereby realizing the casting of the turbine casting;
[0035] S5: The cooling water in the cavity of the lower mold is driven by the circulation pump to enter the circulation pipe for circulation cooling and cooling. At the same time, the cooling fan drives the external cooling air flow to blow onto the circulation pipe to realize the cooling operation of the cooling water in the circulation pipe, so that the turbine casting in the mold cavity is gradually cooled and formed;
[0036] S6: After the turbine casting in the mold cavity is cooled and formed, the unloading piston rod is driven by the unloading electric telescopic device to push the unloading ejector pin upward, and the turbine casting formed in the lower mold cavity is ejected by the unloading ejector pin, thereby realizing the unloading of the formed turbine casting product, and then the next cycle operation is carried out.
[0037] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are:
[0038] 1. The high-temperature alloy turbine vacuum casting equipment drives the wind force of the cooling fan to increase gradually from small to large through program control. When the kinetic energy of the cooling fan is small, the opening angle of the adjustment plate is small. At this time, the cooling wind blows at the narrower position on the front side of the circulation pipe. When the kinetic energy of the cooling fan is large, the opening angle of the adjustment plate increases synchronously. At this time, the cooling wind can be blown at all positions on the circulation pipe to realize the cooling operation of the cooling water inside the circulation pipe. Through this setting, the cooling speed of the turbine casting can be adaptively adjusted, which can effectively avoid the problem of surface deformation and pores of the turbine casting caused by the fast cooling rate of the turbine casting in the mold cavity. The product quality of the turbine casting is ensured by effectively and reasonably controlling the cooling speed of the turbine casting.
[0039] 2. The high-temperature alloy turbine vacuum casting equipment sets the circulation pipe to be narrow in the front and wide in the back, so that the cooling air can cool the circulation pipe from front to back. At the same time, the cooling speed of the cooling water in the circulation pipe is gradually increased and adaptively changed, which can effectively control the cooling rate of the cooling water in the circulation pipe, thereby ensuring the production quality of vortex castings.
[0040] 3. The high-temperature alloy turbine vacuum casting equipment, through the continuous downward movement of the upper mold, prompts the upper mold and the lower mold to form a mold-closing state, and uses a vacuum pump to evacuate the environment of the mold cavity between the upper mold and the lower mold to a vacuum environment. By evacuating the mold cavity environment to a vacuum environment, it helps to reduce the contact of the alloy material with oxygen in the air during the melting and pouring process, effectively preventing oxidation, and at the same time being able to provide high-quality turbine castings to ensure the mechanical properties and reliability of the turbine castings.
[0041] 4. The high-temperature alloy turbine vacuum casting equipment uses a cooling fan to drive a rotating cleaning brush to effectively remove dust from the surface of the circulation pipe, effectively preventing dust from accumulating on the surface of the circulation pipe and affecting the cooling effect of the cooling water in the circulation pipe. This setting can further improve the cooling effect of the cooling water in the circulation pipe, thereby ensuring the molding quality of the turbine casting. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.
[0043] Figure 1 It shows a schematic diagram of an overall three-dimensional structure provided according to an embodiment of the present invention;
[0044] Figure 2A schematic diagram of the installation structure of a machine base and a casting assembly provided according to an embodiment of the present invention is shown;
[0045] Figure 3 A schematic diagram of the mold opening structure of the upper mold and the lower mold provided according to an embodiment of the present invention is shown;
[0046] Figure 4 A schematic diagram of the mold closing structure of the upper mold and the lower mold provided in an embodiment of the present invention is shown;
[0047] Figure 5 A schematic diagram of the installation structure of the unloading assembly and the lower mold provided according to an embodiment of the present invention is shown;
[0048] Figure 6 It shows a schematic diagram of the overall structure of a discharge assembly provided according to an embodiment of the present invention;
[0049] Figure 7 A schematic diagram of the overall structure of an injection molding assembly provided according to an embodiment of the present invention is shown;
[0050] Figure 8 A schematic diagram of the installation structure of the lower mold and the cooling mechanism provided in an embodiment of the present invention is shown;
[0051] Fig. 9 A schematic diagram of a local structure of an upper mold provided according to an embodiment of the present invention is shown;
[0052] Fig.10 A schematic diagram of the internal structure of a lower mold according to an embodiment of the present invention is shown;
[0053] Fig.11 A schematic diagram of the installation structure of the lower mold and the heating assembly provided in an embodiment of the present invention is shown;
[0054] Fig.12 The schematic diagram of the internal local structure of the cooling mechanism provided by the embodiment of the present invention is shown. Figure 1 ;
[0055] Fig.13 The schematic diagram of the internal local structure of the cooling mechanism provided by the embodiment of the present invention is shown. Figure 2 ;
[0056] Fig.14 A schematic diagram of the installation structure of the cooling jacket, cooling fan and adjustment assembly provided in an embodiment of the present invention is shown;
[0057] Fig.15 It shows a schematic diagram of the overall structure of a circulation component provided in an embodiment of the present invention;
[0058] Fig.16 A schematic diagram of the installation structure of a cooling fan and an adjustment assembly provided in an embodiment of the present invention is shown;
[0059] Fig.17 A schematic diagram of the installation structure of a cooling fan and a cleaning assembly provided in an embodiment of the present invention is shown;
[0060] Fig.18 A schematic diagram of a local structure of an adjustment component provided according to an embodiment of the present invention is shown.
[0061] Legend:
[0062] 10. Machine base; 11. Fixing frame; 12. Control cabinet; 13. Vacuum pump; 14. Exhaust check valve;
[0063] 20. Casting assembly; 21. Bottom plate; 22. Top plate; 23. Fixed slide bar; 24. Lower die; 241. Guide groove; 25. Upper die; 251. Guide column; 26. Hydraulic cylinder; 27. Injection port;
[0064] 30. Injection molding assembly; 31. Fixed seat; 32. Stabilizing slide bar; 33. Fixed plate; 34. Injection molding electric telescope; 35. Movable plate; 36. Movable push rod; 37. Injection molding device; 371. Injection molding head; 372. Feed pipe;
[0065] 40. Heating assembly; 41. Heater; 42. Heating tube;
[0066] 50. Cooling mechanism; 51. Cooling shell; 52. Cooling jacket; 53. Circulation assembly; 531. Circulation pump; 532. Circulation pipe; 533. Connector; 54. Dustproof plate; 55. Cooling fan; 551. Fixed bracket; 56. Adjustment assembly; 561. Adjustment seat; 562. Air inlet; 563. Adjustment plate; 564. Rotating connecting shaft; 565. Support spring; 57. Cleaning assembly; 571. Rotating rod; 572. Cleaning rod; 573. Cleaning brush;
[0067] 60. Discharging assembly; 61. Fixed base; 62. Discharging electric telescope; 63. Discharging piston rod; 64. Discharging ejector pin. DETAILED DESCRIPTION
[0068] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0069] See also Figures 1 to 18A high-temperature alloy turbine vacuum casting equipment includes a machine base 10, a fixing frame 11 arranged on the machine base 10, and a control box 12 arranged on the front side of the machine base 10, characterized in that it also includes a casting assembly 20 arranged on the machine base 10 for casting a turbine casting, and an injection molding assembly 30 arranged on the right side of the machine base 10 for material injection molding; the casting assembly 20 includes a lower mold 24 and an upper mold 25, a mold cavity for turbine casting is opened in the upper mold 25 and the lower mold 24, an inner cavity is opened inside the lower mold 24, and cooling water for cooling the turbine casting formed in the mold cavity is provided in the inner cavity; a cooling mechanism 50 for cooling and circulating the cooling water is provided on the left side of the lower mold 24, and the cooling mechanism 50 includes a cooling shell 51 fixedly mounted on the left side of the lower mold 24, and a cooling jacket 52 is fixedly mounted on the front side of the cooling shell 51 A circulation component 53 for circulating cooling the cooling water in the cavity of the lower mold 24 is arranged inside the cooling shell 51, and a dustproof plate 54, a cooling fan 55 and an adjustment component 56 are arranged in the cooling sleeve 52 from front to back. The cooling fan 55 drives the external cooling air to enter the cooling shell 51 along the adjustment component 56, and the cooling air is blown onto the circulation component 53 to gradually cool the circulating cooling water; the wind force of the cooling fan 55 is driven to increase gradually from small to large through program control, and the cooling speed of the turbine casting can be adaptively adjusted through this setting, which can effectively avoid the problem of surface deformation and pores of the turbine casting caused by the fast cooling rate of the turbine casting in the mold cavity, and ensure the product quality of the turbine casting by effectively and reasonably controlling the cooling speed of the turbine casting.
[0070] See also Figure 3 to Figure 4 , Figures 8 to 9 The casting assembly 20 also includes a bottom plate 21 and a top plate 22, and the top plate 22 is located directly above the bottom plate 21, the upper side of the bottom plate 21 is fixedly assembled with the lower mold 24, and the bottom of the top plate 22 is fixedly assembled with the upper mold 25. Four symmetrically distributed fixed slide bars 23 are fixedly installed on the upper side of the bottom plate 21 and on the outer periphery of the lower mold 24. The upper ends of the four fixed slide bars 23 are all passed through the top plate 22, and at least partially protrude from the upper side of the top plate 22. The four fixed slide bars 23 are slidably installed with the top plate 22; the bottom of the upper mold 25 is fixed Four symmetrically arranged guide columns 251 are installed, and four guide grooves 241 corresponding to the guide columns 251 are opened on the upper side of the lower mold 24. The guide columns 251 and the guide grooves 241 are installed by matching; the piston rod of the hydraulic cylinder 26 pushes the top plate 22 and the upper mold 25 to move downward, and at the same time, the top plate 22 slides on the fixed slide rod 23 to ensure the stability of the downward movement of the upper mold 25, and as the upper mold 25 continues to move downward, the guide columns 251 are inserted into the guide grooves 241, so that the upper mold 25 and the lower mold 24 form a mold closing state.
[0071] See also Figure 3 to Figure 4 , Figures 8 to 9 The casting assembly 20 also includes a hydraulic cylinder 26, which is fixedly mounted on the upper surface of the fixing frame 11. The bottom of the hydraulic cylinder 26 passes through the fixing frame 11 and is fixedly connected to the top plate 22 by a piston rod. The right sides of the lower mold 24 and the upper mold 25 are both provided with an injection port 27 for pouring the alloy material. Among them, a vacuum pump 13 is fixedly mounted on the front side of the upper mold 25, and a ventilation channel is opened on the front side of the upper mold 25, and an exhaust check valve 14 is provided in the ventilation channel. The vacuum pump 13 is connected to the exhaust by a ventilation pipe. The one-way valve 14 is fixedly connected, and the vacuum pump 13 is driven to operate, and the mold cavities of the upper mold 25 and the lower mold 24 are evacuated to a vacuum environment; the vacuum pump 13 is started through program control, and the environment of the mold cavity in the upper mold 25 and the lower mold 24 is evacuated to a vacuum environment by the vacuum pump 13. By evacuating the mold cavity environment to a vacuum environment, it helps to reduce the contact of the alloy material with oxygen in the air during the melting and pouring process, effectively preventing oxidation, and at the same time being able to provide high-quality turbine castings to ensure the mechanical properties and reliability of the turbine castings.
[0072] See also Figure 1 , Figure 7 The injection molding assembly 30 includes a fixed seat 31 fixedly assembled on the right side of the machine base 10, a stabilizing slide bar 32 is fixedly installed on the right side of the fixed seat 31, a fixed plate 33 is fixedly installed on the end of the stabilizing slide bar 32 away from the fixed seat 31, an injection molding electric telescopic device 34 is fixedly assembled on the right side of the fixed plate 33, a movable plate 35 is slidably installed on the stabilizing slide bar 32, and the left side of the injection molding electric telescopic device 34 is fixedly connected to the movable plate 35 by an injection molding telescopic rod, and a movable push rod 36 is fixedly installed on the side of the movable plate 35 facing the fixed seat 31, and the end of the movable push rod 36 away from the movable plate 35 passes through the fixed seat 31 and is fixedly connected to the injector 37; an injection head 371 for turbine injection molding the mold cavity in the upper mold 25 and the lower mold 24 is fixedly assembled on the injector 37, and the injection molding A feed pipe 372 for connecting with external injection molding materials is fixedly installed on the upper side of the device 37. The movable push rod 36 pushes the injector 37 to perform turbine injection molding on the mold cavity in the upper mold 25 and the lower mold 24 by driving the injection molding electric telescopic device 34; the movable plate 35 and the injector 37 are pushed to move by the piston rod of the injection molding electric telescopic device 34, and the movable plate 35 is used to slide on the stabilizing slide bar 32 to enhance the stability of the injector 37 when moving. With the continuous pushing of the injector 37, the injection head 371 on the injector 37 is prompted to connect with the injection port 27 between the upper mold 25 and the lower mold 24, and then the injector 37 is driven to drive the alloy material along the injection head 371 to be injected into the mold cavity in the upper mold 25 and the lower mold 24, thereby realizing the casting of turbine castings.
[0073] See also Figure 5 , Figure 10 to Figure 11A heating assembly 40 is provided in the machine base 10. The heating assembly 40 includes a heater 41 fixedly assembled in the machine base 10 and a heating tube 42 arranged in the cavity of the lower mold 24, and the lower end of the heating tube 42 is fixedly connected to the heater 41. The heater 41 is driven to make the heating tube 42 generate heat to heat the cooling water in the cavity of the lower mold 24; the heater 41 is driven to operate through program control, and the heating tube 42 is used to preheat the cooling water in the cavity of the lower mold 24, so as to avoid the low temperature of the cooling water affecting the product quality of the turbine casting, so that it can be gradually cooled and formed.
[0074] See also Figures 12 to 15 The circulation component 53 includes a circulation pump 531 fixedly mounted on the cooling shell 51, a connector 533 is fixedly mounted on the side of the circulation pump 531 close to the lower mold 24, and the end of the connector 533 away from the circulation pump 531 passes through the lower mold 24 and communicates with the cooling water in the inner cavity, and a circulation pipe 532 for cooling the cooling water is fixedly mounted on the side of the circulation pump 531 away from the connector 533, and the circulation pipe 532 is in a conical shape that is narrow in front and wide in the back; the cooling water in the inner cavity of the lower mold 24 is driven by the circulation pump 531 to enter the circulation pipe 532 for cooling, and at the same time, by setting the circulation pipe 532 to be narrow in front and wide in the back, the cooling wind can cool the circulation pipe 532 from front to back, which can effectively accelerate the cooling rate of the cooling water in the circulation pipe 532.
[0075] See also Figures 14 to 17 A fixing bracket 551 is fixedly mounted on the cooling fan 55, and the outer wall of the fixing bracket 551 is fixedly mounted on the inner wall of the cooling jacket 52; a cleaning assembly 57 is arranged on the inner side of the circulation pipe 532, and the cleaning assembly 57 comprises a rotating rod 571 fixedly mounted on the cooling fan 55, and the end of the rotating rod 571 away from the cooling fan 55 passes through the adjusting assembly 56 and is located at the central axis of the circulation pipe 532, and a cleaning rod 572 is fixedly mounted on the outer periphery of the rotating rod 571, and a cleaning brush 573 for cleaning the dust on the surface of the circulation pipe 532 is fixedly mounted on the outer end of the cleaning rod 572; the rotating rod 571 and the cleaning brush 573 are driven by the cooling fan 55 to rotate synchronously, and the rotating cleaning brush 573 is used to effectively remove the dust on the surface of the circulation pipe 532, so as to effectively prevent the dust from accumulating on the surface of the circulation pipe 532 and affecting the cooling effect of the cooling water in the circulation pipe 532.
[0076] See also Figures 14 to 18The adjustment component 56 includes an adjustment seat 561 fixedly mounted on the inner wall of the cooling sleeve 52, an air inlet 562 for cooling air to enter is opened at the central axis of the adjustment seat 561, and a plurality of adjustment plates 563 for shielding the air inlet 562 are movably mounted on the adjustment seat 561, the adjustment plate 563 is movably mounted on the adjustment seat 561 by rotating the connecting shaft 564, and a support spring 565 is fixedly connected between the rear side of the adjustment plate 563 and the adjustment seat 561; when the kinetic energy of the cooling fan 55 is large, the wind force of the cooling fan 55 also increases synchronously, and based on the force of the cooling wind, the opening angle of the adjustment plate 563 increases synchronously, so that the cooling channel between the adjustment plates 563 is also increased, and at this time, the cooling wind can be blown to all positions on the circulation pipe 532, so as to realize the cooling operation of the cooling water inside the circulation pipe 532.
[0077] See also Figures 5 and 6 A discharge assembly 60 for discharging the turbine casting is arranged inside the machine base 10. The discharge assembly 60 includes a fixed base 61 fixedly assembled inside the machine base 10. A discharge electric telescopic device 62 is fixedly assembled on the fixed base 61. The upper end of the discharge electric telescopic device 62 is fixedly connected to a discharge ejector pin 64 by a discharge piston rod 63. The upper end of the discharge ejector pin 64 is flush with the bottom of the cavity of the lower mold 24. The discharge electric telescopic device 62 is driven to make the discharge piston rod 63 push the discharge ejector pin 64 to move upward, and the discharge ejector pin 64 is used to eject the turbine product formed in the cavity of the lower mold 24. The discharge electric telescopic device 62 drives the discharge piston rod 63 to push the discharge ejector pin 64 to move upward, and the discharge ejector pin 64 is used to eject the turbine casting formed in the cavity of the lower mold 24, thereby realizing the discharge of the formed turbine casting product.
[0078] A high-temperature alloy turbine vacuum casting process comprises the following steps:
[0079] S1: The piston rod of the hydraulic cylinder 26 pushes the upper mold 25 downward, so that the upper mold 25 and the lower mold 24 are in a mold-closing state;
[0080] S2: The piston rod of the electric injection retractor 34 pushes the injection molding machine 37 to move toward the upper mold 25 and the lower mold 24, and the injection head 371 on the injection molding machine 37 is connected with the injection port 27 between the upper mold 25 and the lower mold 24;
[0081] S3: starting the vacuum pump 13 through program control, and using the vacuum pump 13 to evacuate the environment of the mold cavity in the upper mold 25 and the lower mold 24 to a vacuum environment, which helps to reduce the contact of the alloy material with oxygen in the air during the melting and pouring process;
[0082] S4: The alloy material is then driven by the injection molding device 37 to be injected into the mold cavities of the upper mold 25 and the lower mold 24 along the injection head 371, thereby realizing the casting of the turbine casting;
[0083] S5: The cooling water in the cavity of the lower mold 24 is driven by the circulation pump 531 to enter the circulation pipe 532 for circulation cooling and cooling. At the same time, the cooling fan 55 drives the external cooling air flow to blow onto the circulation pipe 532 to cool the cooling water in the circulation pipe 532, so that the turbine casting in the mold cavity is gradually cooled and formed;
[0084] S6: After the turbine casting in the mold cavity is cooled and formed, the unloading piston rod 63 is driven by the unloading electric telescopic device 62 to push the unloading ejector pin 64 upward, and the turbine casting formed in the mold cavity of the lower mold 24 is ejected by the unloading ejector pin 64, thereby realizing the unloading of the molded turbine casting product, and then the next cycle operation is carried out.
[0085] The specific usage and function of this embodiment are as follows:
[0086] Working principle: When in use, the staff controls the control box 12 to drive the hydraulic cylinder 26 to generate kinetic energy and start running, and uses the piston rod of the hydraulic cylinder 26 to push the top plate 22 and the upper mold 25 to move downward, and in the process of the upper mold 25 moving downward, the top plate 22 slides on the fixed slide bar 23 to ensure the stability of the upper mold 25 moving downward, and as the upper mold 25 continues to move downward, the guide column 251 is inserted into the guide groove 241, so that the upper mold 25 and the lower mold 24 form a mold closing state; at this time, the injection molding electric telescopic device 34 is started through the control of the program, and the piston rod of the injection molding electric telescopic device 34 is used to push the movable plate 35 and the injector 37 to move, and the movable plate 35 slides on the stable slide bar 32 to strengthen the movement of the injector 37 Stability, with the continuous pushing of the injector 37, the injection head 371 on the injector 37 is brought into contact with the injection port 27 between the upper mold 25 and the lower mold 24, and at the same time, the vacuum pump 13 is started through program control, and the environment of the mold cavity in the upper mold 25 and the lower mold 24 is evacuated to a vacuum environment by the vacuum pump 13. The evacuation of the mold cavity environment to a vacuum environment helps to reduce the contact of the alloy material with oxygen in the air during the melting and pouring process, effectively preventing oxidation, and at the same time providing high-quality turbine castings to ensure the mechanical properties and reliability of the turbine castings; the injector 37 is then started through program control, and the injector 37 is driven to drive the alloy material along the injection head 371 to be injected into the mold cavity in the upper mold 25 and the lower mold 24, thereby realizing the casting of the turbine casting;
[0087] During the molding process of the turbine casting in the cavity of the lower mold 24, it is necessary to perform cooling molding treatment on it. The cooling water in the cavity of the lower mold 24 is driven by the circulation pump 531 to enter the circulation pipe 532 for cooling. At the same time, the cooling fan 55 is driven to operate through the control of the program. The cooling airflow from the outside is driven by the cooling fan 55 to be sucked into the cooling sleeve 52, and the adjusting plates 563 are pushed to expand with each other based on the action force of the cooling airflow, and a cooling channel is formed between the adjusting plates 563. At the same time, the airflow is blown onto the circulation pipe 532 along the cooling channel expanded by the adjusting plates 563, thereby realizing the cooling operation of the cooling water in the circulation pipe 532; in addition, the wind force of the cooling fan 55 is driven to operate from small to large by the control of the program. When the kinetic energy of the cooling fan 55 is small, the wind force of the cooling fan 55 is also small synchronously. Based on the action force of the cooling wind, the opening angle of the adjusting plates 563 is small, so that the cooling channel between the adjusting plates 563 is also small. At this time, the cooling wind blows on the circulation pipe 532 is located at a narrow position on the front side, so as to realize cooling operation of the cooling water inside part of the circulation pipe 532; and when the kinetic energy of the cooling fan 55 is large, the wind force of the cooling fan 55 is also increased synchronously, and the opening angle of the adjustment plate 563 is also increased synchronously under the driving force of the cooling wind, so that the cooling channel between the adjustment plates 563 is also increased. At this time, the cooling wind can be blown to all positions on the circulation pipe 532, so as to realize cooling operation of the cooling water inside the circulation pipe 532, and by setting the circulation pipe 532 to be narrow in front and wide in the back, the cooling wind can perform air cooling operation on the circulation pipe 532 from front to back, which can effectively speed up the cooling rate of the cooling water in the circulation pipe 532, and through this setting, the cooling rate of the turbine casting can be adaptively adjusted, which can effectively avoid the problem that the cooling rate of the turbine casting in the mold cavity is too fast, resulting in surface deformation and pores and other quality defects of the turbine casting, and the product quality of the turbine casting can be ensured by effectively and reasonably controlling the cooling rate of the turbine casting;
[0088] In addition, during the operation of the cooling fan 55, the rotating rod 571 is used to drive the cleaning rod 572 and the cleaning brush 573 to rotate synchronously, and the rotating cleaning brush 573 is used to effectively remove the dust on the surface of the circulation pipe 532, effectively preventing dust from accumulating on the surface of the circulation pipe 532 and affecting the cooling effect of the cooling water in the circulation pipe 532. This setting can further improve the cooling effect of the cooling water in the circulation pipe 532, thereby ensuring the molding quality of the turbine casting. When the turbine casting in the mold cavity is cooled and formed, the unloading electric telescopic device 62 is started through program control, driving the unloading piston rod 63 to push the unloading ejector pin 64 upward, and using the unloading ejector pin 64 to eject the turbine casting formed in the mold cavity of the lower mold 24, thereby realizing the unloading of the molded turbine casting product, and then carrying out the next cycle operation.
[0089] The preferred embodiments of the present invention disclosed above are only used to help illustrate the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.
Claims
1. A high-temperature alloy turbine vacuum casting device, comprising a machine base (10), a fixing frame (11) arranged on the machine base (10), and a control box (12) arranged on the front side of the machine base (10), characterized in that: It also includes a casting assembly (20) arranged on the machine base (10) for casting the turbine casting, and an injection molding assembly (30) arranged on the right side of the machine base (10) for injecting material; The casting assembly (20) comprises a lower mold (24) and an upper mold (25), wherein a mold cavity for turbine casting is provided in the upper mold (25) and the lower mold (24), and an inner cavity is provided inside the lower mold (24), and cooling water is provided in the inner cavity for cooling the turbine casting formed in the mold cavity; A cooling mechanism (50) for cooling and circulating cooling water is arranged on the left side of the lower mold (24), the cooling mechanism (50) comprising a cooling shell (51) fixedly mounted on the left side of the lower mold (24), a cooling jacket (52) fixedly mounted on the front side of the cooling shell (51), a circulation component (53) for circulating and cooling cooling water in the cavity of the lower mold (24) is arranged inside the cooling shell (51), a dustproof plate (54), a cooling fan (55) and an adjustment component (56) are arranged in the cooling jacket (52) from front to back, the cooling fan (55) is driven to drive external cooling air along the adjustment component (56) into the cooling shell (51), and the cooling air is blown onto the circulation component (53) to gradually cool the circulating cooling water; The circulation assembly (53) comprises a circulation pump (531) fixedly mounted on the cooling shell (51); a connector (533) is fixedly mounted on a side of the circulation pump (531) close to the lower mold (24); an end of the connector (533) away from the circulation pump (531) passes through the lower mold (24) and communicates with cooling water in the inner cavity; a circulation pipe (532) for cooling the cooling water is fixedly mounted on a side of the circulation pump (531) away from the connector (533); and the circulation pipe (532) is in a conical shape that is narrow at the front and wide at the rear; A fixing bracket (551) is fixedly mounted on the cooling fan (55), and an outer wall of the fixing bracket (551) is fixedly mounted on an inner wall of the cooling jacket (52); A cleaning assembly (57) is arranged on the inner side of the circulation pipe (532), and the cleaning assembly (57) comprises a rotating rod (571) fixedly mounted on the cooling fan (55), and one end of the rotating rod (571) away from the cooling fan (55) passes through the adjustment assembly (56) and is located at the central axis of the circulation pipe (532), and a cleaning rod (572) is fixedly mounted on the outer periphery of the rotating rod (571), and a cleaning brush (573) for cleaning dust on the surface of the circulation pipe (532) is fixedly mounted on the outer end of the cleaning rod (572); The adjustment assembly (56) comprises an adjustment seat (561) fixedly mounted on the inner wall of the cooling sleeve (52); an air inlet (562) for cooling air to enter is provided at the central axis of the adjustment seat (561); a plurality of adjustment plates (563) for shielding the air inlet (562) are movably mounted on the adjustment seat (561); the adjustment plates (563) are movably mounted on the adjustment seat (561) via a rotating connecting shaft (564); and a support spring (565) is fixedly connected between the rear side of the adjustment plate (563) and the adjustment seat (561).
2. A high temperature alloy turbine vacuum casting equipment according to claim 1, characterized in that: The casting assembly (20) further comprises a bottom plate (21) and a top plate (22), wherein the top plate (22) is located directly above the bottom plate (21), the upper side of the bottom plate (21) is fixedly assembled with the lower die (24), the bottom of the top plate (22) is fixedly assembled with the upper die (25), four symmetrically distributed fixed slide bars (23) are fixedly installed on the upper side of the bottom plate (21) and on the outer periphery of the lower die (24), the upper ends of the four fixed slide bars (23) are all passed through the top plate (22) and at least partially protrude from the upper side of the top plate (22), and the four fixed slide bars (23) are slidably mounted on the top plate (22); Four symmetrically arranged guide columns (251) are fixedly mounted on the bottom of the upper die (25), and four guide grooves (241) corresponding to the guide columns (251) are formed on the upper side of the lower die (24), and the guide columns (251) and the guide grooves (241) are mounted by matching.
3. A high temperature alloy turbine vacuum casting equipment according to claim 2, characterized in that: The casting assembly (20) further comprises a hydraulic cylinder (26), wherein the hydraulic cylinder (26) is fixedly mounted on the upper surface of the fixing frame (11), the bottom of the hydraulic cylinder (26) is fixedly connected to the top plate (22) by a piston rod passing through the fixing frame (11), and the right sides of the lower mold (24) and the upper mold (25) are both provided with an injection port (27) for pouring alloy material; A vacuum pump (13) is fixedly mounted on the front side of the upper mold (25); a ventilation channel is provided on the front side of the upper mold (25); and an exhaust check valve (14) is provided in the ventilation channel. The vacuum pump (13) is fixedly connected to the exhaust check valve (14) via a ventilation pipe. The vacuum pump (13) is driven to operate and the mold cavities of the upper mold (25) and the lower mold (24) are evacuated to a vacuum environment.
4. The high temperature alloy turbine vacuum casting equipment according to claim 1, characterized in that: A heating assembly (40) is provided in the machine base (10), and the heating assembly (40) comprises a heater (41) fixedly mounted in the machine base (10) and a heating tube (42) provided in a cavity in the lower mold (24), wherein the lower end of the heating tube (42) is fixedly connected to the heater (41), and the heating tube (42) generates heat by driving the heater (41) to heat the cooling water in the cavity in the lower mold (24).
5. The high temperature alloy turbine vacuum casting equipment according to claim 1, characterized in that: The injection molding assembly (30) comprises a fixed seat (31) fixedly mounted on the right side of the machine base (10); a stabilizing slide bar (32) is fixedly mounted on the right side of the fixed seat (31); a fixed plate (33) is fixedly mounted on the end of the stabilizing slide bar (32) away from the fixed seat (31); an injection molding electric telescopic device (34) is fixedly mounted on the right side of the fixed plate (33); a movable plate (35) is slidably mounted on the stabilizing slide bar (32); the left side of the injection molding electric telescopic device (34) is fixedly connected to the movable plate (35) by means of an injection molding telescopic rod; a movable push rod (36) is fixedly mounted on the side of the movable plate (35) facing the fixed seat (31); and the end of the movable push rod (36) away from the movable plate (35) passes through the fixed seat (31) and is fixedly connected to the injection molding device (37); The injection molding machine (37) is fixedly equipped with an injection head (371) for performing turbo injection molding on the mold cavities of the upper mold (25) and the lower mold (24); the upper side of the injection molding machine (37) is fixedly equipped with a feed pipe (372) for connecting with external injection molding materials; the injection molding electric telescopic device (34) is driven to cause the movable push rod (36) to push the injection molding machine (37) to perform turbo injection molding on the mold cavities of the upper mold (25) and the lower mold (24).
6. The high temperature alloy turbine vacuum casting equipment according to claim 1, characterized in that: A discharge assembly (60) for discharging the turbine casting is arranged inside the machine base (10), and the discharge assembly (60) comprises a fixed base (61) fixedly assembled inside the machine base (10), and a discharge electric telescopic device (62) is fixedly assembled on the upper portion of the fixed base (61), and the upper end of the discharge electric telescopic device (62) is fixedly connected to a discharge ejector pin (64) by means of a discharge piston rod (63), and the upper end of the discharge ejector pin (64) is flush with the bottom of the mold cavity of the lower mold (24), and the discharge piston rod (63) is driven by the discharge electric telescopic device (62) to push the discharge ejector pin (64) upward, and the turbine product formed in the mold cavity of the lower mold (24) is ejected and demolded by means of the discharge ejector pin (64).
7. A high-temperature alloy turbine vacuum casting process, applied to a high-temperature alloy turbine vacuum casting equipment according to any one of claims 1 to 6, characterized in that: The following steps are involved: S1: The upper mold (25) is pushed downward by the piston rod of the hydraulic cylinder (26), so that the upper mold (25) and the lower mold (24) are in a mold-closing state; S2: pushing the injection molding machine (37) toward the upper mold (25) and the lower mold (24) through the piston rod of the injection molding electric telescopic device (34), and making the injection head (371) on the injection molding machine (37) and the injection port (27) between the upper mold (25) and the lower mold (24) dock with each other; S3: starting the vacuum pump (13) through program control, and using the vacuum pump (13) to evacuate the environment of the mold cavity of the upper mold (25) and the lower mold (24) to a vacuum environment, which helps to reduce the contact between the alloy material and oxygen in the air during the melting and pouring process; S4: the alloy material is then driven by the injection molding device (37) to be injected into the mold cavities of the upper mold (25) and the lower mold (24) along the injection head (371), thereby achieving the casting of the turbine casting; S5: driving the cooling water in the cavity of the lower mold (24) to enter the circulation pipe (532) for circulation cooling and temperature reduction through the circulation pump (531), and driving the external cooling air flow to blow onto the circulation pipe (532) through the cooling fan (55), so as to cool the cooling water in the circulation pipe (532), thereby gradually cooling and forming the turbine casting in the mold cavity; S6: After the turbine casting in the mold cavity is cooled and formed, the unloading electric telescopic device (62) drives the unloading piston rod (63) to push the unloading ejector pin (64) upward, and the unloading ejector pin (64) is used to eject the turbine casting formed in the mold cavity of the lower mold (24), thereby realizing the unloading of the formed turbine casting product, and then the next cycle operation is carried out.
Citation Information
Patent Citations
Special polyester fiber spinning equipment and spinning process for high-elastic polyester pongee
CN115182059A
Die-casting mold temperature controller and using method thereof
CN115488313A