Device and method for manufacturing dimming film electrode, dimming film manufacturing method and dimming film

By using a slider and an elastic coating tube device in the production of PDLC dimming film electrodes, the automatic supply and precise coating of conductive paste are achieved, the problems of uneven and low efficiency of manual coating are solved, and the electrodes are improved Production efficiency and quality.

CN118444502BActive Publication Date: 2024-11-08SHANGHAI LONGSHENG PHOTOELECTRIC NEW MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410903622.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2024-11-08
Estimated Expiration
2044-07-08

AI Technical Summary

Technical Problem

In the prior art, when making PDLC dimming film electrodes, it is difficult for manual adhesive tape to ensure accurate coating of conductive paste, resulting in uneven coating and limited efficiency.

Method used

The device including the first slider and the elastic coating tube is adopted. The sliding surface of the slider abuts the side of the electrode, and the discharge port and the elastic coating tube move in the electrode extension direction to realize the automatic supply and coating of the slurry to ensure conductivity. Precise coating of slurry.

Benefits of technology

The coating efficiency and accuracy of conductive paste are improved, and the uneven problem during manual coating and the risk of short circuit at the semi-cutting steps of the electrode are avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118444502B_ABST
    Figure CN118444502B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of PDLC dimming film, and specifically relates to a dimming film electrode manufacturing device and method, a dimming film manufacturing method and a dimming film. The manufacturing device includes a first slider, the first slider has a sliding surface, when the first slider slides, the sliding surface is used to abut against the side of the electrode to be manufactured of the PDLC membrane; an elastic coating tube, which is connected to the sliding surface, wherein the axis thereof is perpendicular to the sliding surface, and its length matches the width of the electrode to be manufactured; a discharge pipe, which is arranged inside the first slider, one end of which is connected to the slurry supply module, and the other end of which extends outward through the sliding surface to form an extension section, and the discharge port is arranged at the lower side of the extension section, and the distance between the center of the discharge port and the sliding surface matches the half width of the electrode to be manufactured. When manufacturing the dimming film electrode, the conductive slurry can be efficiently and evenly and accurately coated on the area of ​​the electrode to be manufactured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of PDLC dimming films, and in particular relates to a dimming film electrode manufacturing device and method, a dimming film manufacturing method and a dimming film. Background Art

[0002] PDLC (polymer dispersed liquid crystal) dimming film becomes transparent when power is applied and foggy when power is not applied. It can be used for laminated dimming glass, back-mounted liquid crystal film for projection, etc. It can maintain the transparency of the space while conveniently protecting privacy and is widely used.

[0003] The PDLC dimming film specifically includes a first substrate, a first conductive layer, a first electrode, a polymer dispersed liquid crystal layer, a second electrode, a second conductive layer and a second substrate. An external power source energizes the first electrode and the second electrode, and the first electrode and the second electrode respectively power the first conductive layer and the second conductive layer.

[0004] Since there is a half-cut step between the surface of the PDLC film and the electrode coating area, the prior art usually uses a method of manually coating the conductive paste to form the electrode when making the electrode of the PDLC dimming film. In order to prevent the conductive paste from being coated on the area where the electrode is to be made, resulting in the conductive paste and the contact between the half-cut step and causing short circuit and other problems, it is necessary to stick tape to control the area where the electrode is coated. However, the above operation is more complicated due to the need to stick tape. The accuracy of manual tape sticking affects the area where the electrode is coated, and it is difficult to ensure that the conductive paste is accurately coated on the area where the electrode is to be made. The coating of the electrode varies from person to person, and there is a problem of uneven coating. In addition, the efficiency of manual coating is limited.

[0005] It should be noted that this part of the present invention only provides background technology related to the present invention and does not necessarily constitute prior art or known technology. Summary of the invention

[0006] The purpose of the present invention is to overcome the defects of the prior art in which, when manufacturing PDLC dimming film electrodes, it is necessary to manually stick tape, it is difficult to ensure that the conductive slurry is accurately coated on the area to be manufactured, the slurry coating is uneven, and the efficiency of manual coating is limited. A dimming film electrode manufacturing device and method, a dimming film manufacturing method and a dimming film are provided. When manufacturing dimming film electrodes, the conductive slurry can be efficiently and evenly and accurately coated on the area to be manufactured.

[0007] In order to achieve the above-mentioned object, in a first aspect, the present invention provides a manufacturing device for a PDLC dimming film electrode, comprising:

[0008] A first slider, wherein the first slider has a sliding surface, and when the first slider slides, the sliding surface is used to abut against a side surface of the PDLC film on the electrode side to be manufactured;

[0009] An elastic coating tube connected to the sliding surface, wherein the axis thereof is perpendicular to the sliding surface and the length L1 thereof matches the width of the electrode to be manufactured;

[0010] A discharge pipe is arranged inside the first sliding block, one end of which is connected to the slurry supply module, and the other end of which extends outward through the sliding surface to form an extension section. The discharge port is arranged at the lower side of the extension section, and the distance between the center of the discharge port and the sliding surface matches the half-width of the electrode to be manufactured.

[0011] In some preferred embodiments, at least one annular groove is circumferentially provided at both ends of the elastic coated tube, and the portion where the annular groove is located forms the end of the elastic coated tube close to the sliding surface and the end away from the sliding surface. The elastic coated tube also includes a middle portion, and the length L2 of the middle portion is the width value of the electrode to be manufactured, and the sum of the length L3 of the end close to the sliding surface and the length L4 of the end away from the sliding surface is the tolerance value of the width of the electrode to be manufactured.

[0012] In some preferred embodiments, the discharge pipe includes a first discharge pipe arranged parallel to the sliding surface and a second discharge pipe perpendicular to the first discharge pipe, the first discharge pipe and the second discharge pipe both having a first end and a second end, the first end of the first discharge pipe is connected to the slurry supply module, the first end of the second discharge pipe extends outward through the sliding surface to form an extension section, the second end of the first discharge pipe is connected to the second end of the second discharge pipe, the second end of the first discharge pipe protrudes from the second discharge pipe, and the second end of the second discharge pipe protrudes from the first discharge pipe.

[0013] Preferably, the inner diameter of the first discharge pipe is greater than the inner diameter of the second discharge pipe, and the ratio of the inner diameter of the first discharge pipe to the inner diameter of the second discharge pipe is 1.5-10.

[0014] In some preferred embodiments, a speed sensor is further provided on the first sliding block, and the manufacturing device further includes a slurry supply control unit. The speed sensor, the slurry supply control unit, and the slurry supply module are electrically connected in sequence.

[0015] In some preferred embodiments, a first slider contact detection component is further provided on the first slider, and the manufacturing device also includes a discharge control unit, the first slider contact detection component is electrically connected to the discharge control unit, and when the first slider contact detection component detects that the sliding surface abuts against the side surface of the electrode to be manufactured of the PDLC membrane, the discharge control unit does not operate, and the slurry flows out from the discharge port.

[0016] Preferably, a recess is provided on the sliding surface of the first slider directly below the elastic coating tube, and the first slider contact detection component is embedded in the recess. The first slider contact detection component includes an elastic member, a second slider and a pressure sensor, and the pressure sensor is electrically connected to the discharge control unit. The elastic deformation direction of the elastic member is perpendicular to the sliding surface, and the elastic member has a first end and a second end along the elastic deformation direction. The first end of the elastic member is connected to the inner wall of the recess, and the second end of the elastic member is connected to one end of the second slider. The second slider has an end facing away from the elastic member. When the elastic member is in a natural state, the end facing away from the elastic member protrudes from the sliding surface, and when the end facing away from the elastic member is flush with the sliding surface, the end of the second slider connected to the elastic member abuts against the pressure sensor, and the discharge control unit does not operate.

[0017] In some preferred embodiments, a fixed shaft is connected to the sliding surface, the fixed shaft is perpendicular to the sliding surface, the elastic coated tube is sleeved on the outer circumference of the fixed shaft and has an interference fit with the outer circumference of the fixed shaft, and the central axis of the fixed shaft coincides with the central axis of the elastic coated tube.

[0018] In a second aspect, the present invention provides a method for manufacturing a PDLC dimming film electrode, which adopts the manufacturing device described in the first aspect, and the manufacturing method includes: half-cutting the electrode side of the PDLC film to be manufactured to form a half-cut step, so that the sliding surface of the first slider is in contact with the side of the electrode side to be manufactured, and the slurry supply module provides slurry to the discharge pipe so that the slurry flows out of the discharge port, so that the first slider moves along the extension direction of the electrode to be manufactured, and the first slider drives the discharge port and the elastic coating tube on the discharge pipe to move along the extension direction, and the discharge port provides slurry to the area of ​​the electrode to be manufactured and the elastic coating tube coats the slurry simultaneously.

[0019] In some preferred embodiments, after the slurry supply control unit receives the moving speed of the first slider transmitted by the speed sensor, it calculates the slurry supply speed and controls the slurry supply module to supply slurry according to the slurry supply speed, wherein the slurry supply speed is the product of the moving speed of the first slider and the preset slurry consumption per unit length of the electrode.

[0020] In some preferred embodiments, when the first slider contact detection component detects that the sliding surface abuts the side of the electrode to be manufactured, the discharge control unit does not operate, and the slurry flows out from the discharge port; when the first slider contact detection component does not detect that the sliding surface abuts the side of the electrode to be manufactured, the discharge control unit operates, and the slurry does not flow out from the discharge port.

[0021] Preferably, the end of the second slider facing away from the elastic member is flush with the sliding surface, the elastic member is compressed, the end of the second slider connected to the elastic member abuts against the pressure sensor, and the discharge control unit does not operate.

[0022] In a third aspect, the present invention provides a method for manufacturing a PDLC dimming film, wherein the manufacturing device described in the first aspect and / or the manufacturing method described in the second aspect are used to manufacture a PDLC dimming film electrode.

[0023] In a fourth aspect, the present invention provides a PDLC dimming film, which is manufactured by the manufacturing method of the PDLC dimming film described in the third aspect.

[0024] The manufacturing device of the PDLC dimming film electrode of the present invention comprises a first slider having a sliding surface, an elastic coating tube whose length matches the width of the electrode to be manufactured is connected to the sliding surface, the central axis of the elastic coating tube is perpendicular to the sliding surface, a discharge pipe is penetrated inside the first slider, one end of the discharge pipe is connected to the slurry supply module, the other end of the discharge pipe passes through the sliding surface and extends outward to form an extension section, the lower side of the extension section has a discharge port, the distance between the center of the discharge port and the sliding surface matches the half width of the electrode to be manufactured, when manufacturing the electrode of the PDLC dimming film, the sliding surface of the first slider is abutted against the side surface of the electrode to be manufactured of the PDLC membrane, and under the premise that the sliding surface remains in an abutting state, the slurry supply module provides slurry to the discharge pipe so that the slurry flows out of the discharge port, and at the same time, the first slider moves along the extension direction of the electrode to be manufactured, the discharge port and the elastic coating tube move along the aforementioned extension direction, and the discharge port The front moves to supply slurry to the area where the electrode is to be made, and the elastic coating tube moves at the back to coat the slurry, which can realize automatic supply and automatic coating of the slurry and improve the slurry coating efficiency. Since the sliding surface of the first slider is in contact with the side of the PDLC membrane on the side of the electrode to be made, it can ensure that the position of the discharge port is always located at the half-width of the electrode, one end of the elastic coating tube is always located at the side of the PDLC membrane on the side of the electrode to be made, that is, the outer edge of the area where the electrode is to be made on the PDLC membrane, and the other end of the elastic coating tube is always located at the inner edge of the area where the electrode is to be made on the PDLC membrane, which can ensure that the conductive slurry is accurately coated on the area where the electrode is to be made. The first slider is driven to move at a certain speed by the driving device, so that it can be evenly coated. When the manufacturing device of the present invention manufactures dimming film electrodes, it can efficiently and evenly and accurately coat the conductive slurry on the area to be made. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.

[0026] Figure 1 It is a structural schematic diagram of a specific implementation of the PDLC dimming film electrode manufacturing device of the present invention.

[0027] Figure 2 It is a schematic diagram of the working state of the electrode manufacturing device of the present invention.

[0028] Figure 3 It is a front view of the first slider of the electrode manufacturing device of the present invention.

[0029] Figure 4 It is a top view of the first slider of the electrode manufacturing device of the present invention.

[0030] Figure 5 It is a cross-sectional view of the first sliding block of the present invention at the BB section.

[0031] Figure 6 It is a cross-sectional view of the AA section of the first slider when the first slider of the present invention cooperates with the PDLC film.

[0032] Figure 7 yes Figure 6 A partial enlarged view of part A in the middle.

[0033] Figure 8 yes Figure 6 A partial enlarged view of part B in the middle.

[0034] Fig. 9 It is a structural schematic diagram of a slurry storage barrel of the present invention.

[0035] Description of Reference Numerals

[0036] 1. First slider; 101. Sliding surface; 102. Concave portion; 2. Elastic coating tube; 201. Annular groove; 3. Discharge pipe; 301. Discharge port; 302. First discharge pipe; 303. Second discharge pipe; 4. Slurry supply module; 401. Slurry storage barrel; 5. Speed ​​sensor; 6. First slider contact detection assembly; 601. Elastic member; 602. Second slider; 603. Pressure sensor; 7. Fixed axis; 8. Side of the electrode to be manufactured; 9. Half-cut step; 10. Stirring assembly. DETAILED DESCRIPTION

[0037] The endpoints and any values ​​of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of each range, the endpoint values ​​of each range and the individual point values, and the individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.

[0038] In this document, unless otherwise specified, directional words such as "upper" and "lower" are generally understood in combination with the directions shown in the drawings and actual applications, and "inside" and "outside" refer to the inside and outside of the outline of a component.

[0039] In the description of the present invention, it is necessary to understand that the terms "center", "length", "width", "up", "down", "front", "back", "vertical", "horizontal", "inside", "outside", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0040] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0041] Research has found that when using existing technology to make PDLC dimming film electrodes, it is necessary to manually stick tape, which makes it difficult to ensure that the conductive slurry is accurately coated on the area where the electrode is to be made. The slurry coating is uneven and the efficiency of manual coating is limited.

[0042] In this first aspect, the present invention provides a manufacturing device for a PDLC dimming film electrode, comprising: a first slider 1, wherein the first slider 1 has a sliding surface 101, and when the first slider 1 slides, the sliding surface 101 is used to abut against the side surface of the PDLC film on the electrode side to be manufactured;

[0043] An elastic coating tube 2, which is connected to the sliding surface 101, wherein the axis thereof is perpendicular to the sliding surface 101, and the length L1 thereof matches the width of the electrode to be manufactured;

[0044] The discharge pipe 3 is arranged inside the first slider 1, one end of which is connected to the slurry supply module 4, and the other end of which extends outward through the sliding surface 101 to form an extension section, and the discharge port 301 is arranged at the lower side of the extension section, and the distance between the center of the discharge port 301 and the sliding surface 101 matches the half width of the electrode to be manufactured.

[0045] The manufacturing device of the PDLC dimming film electrode of the present invention comprises a first slider 1, the first slider 1 has a sliding surface 101, an elastic coating tube 2 is connected to the sliding surface 101, the central axis of the elastic coating tube 2 is perpendicular to the sliding surface, the length of the elastic coating tube matches the width of the electrode to be manufactured, and a discharge pipe is also penetrated inside the slider, one end of the discharge pipe is connected to the slurry supply module, and the other end extends outward through the sliding surface to form an extension section, and a discharge port is provided at the lower side of the extension section, and the distance between the center of the discharge port and the sliding surface matches the half width of the electrode to be manufactured. When manufacturing the PDLC dimming film electrode , the electrode side to be manufactured of the PDLC membrane is half-cut to form a half-cut step, a force perpendicular to the sliding surface is applied to the first slider, so that the sliding surface of the first slider is in contact with the side surface of the electrode side to be manufactured of the PDLC membrane, and under the premise that the sliding surface remains in contact, a force parallel to the sliding surface is applied to the first slider, so that the first slider moves along the extension direction of the electrode to be manufactured, and the discharge port and the elastic coating tube on the discharge pipe on the first slider move along the extension direction. When the sliding surface of the first slider is in contact with the side surface of the electrode side to be manufactured of the PDLC membrane, the slider drives the discharge port and the elastic coating tube to move. During the movement of the tube, the slider can limit the elastic coating tube and the discharge port, and can ensure that the position of the discharge port is always located at the half-width position of the electrode, one end of the elastic coating tube is always located at the side of the PDLC membrane on the side where the electrode is to be made, that is, the outer edge of the area of ​​the PDLC membrane where the electrode is to be made, and the other end of the elastic coating tube is always located at the inner edge of the area of ​​the PDLC membrane where the electrode is to be made, and the slurry is provided to the discharge pipe through the slurry supply module so that the slurry flows out of the discharge port, the discharge port moves in the front to provide slurry to the area where the electrode is to be made, and the elastic coating tube moves in the back to coat the slurry. The slurry is coated, and automatic supply and automatic coating of the slurry can be realized, thereby improving the slurry coating efficiency. Since the two ends of the elastic coating tube are limited during the movement, the discharge port is limited, so the slurry coating range can be kept consistent with the distance from the side of the PDLC membrane, thereby ensuring that the conductive slurry is accurately coated on the area where the electrode is to be manufactured, thereby avoiding the possibility that the conductive slurry may contact the half-cut step of the electrode due to manual coating, and the first slider moves at a certain speed to achieve uniform coating. When manufacturing the dimming film electrode, the manufacturing device of the present invention can efficiently and evenly and accurately coat the conductive slurry on the area where the electrode is to be manufactured.

[0046] The present invention can specifically apply a force inclined relative to the sliding surface to the first slider through a driving device (a driving device with editable paths such as a robotic arm can be used as a driving device after loading the slider), so that the first slider is moved along the extension direction of the electrode to be manufactured under the premise that the sliding surface and the side of the PDLC membrane on the side of the electrode to be manufactured remain in abutment. The elastic coating tube of the present invention can be, for example, a silicone sleeve with elasticity. It can be understood that the end of the extension section of the discharge pipe of the present invention is integrally sealed or sealed with a plug or the like. The extension section of the present invention has a side surface, the side surface corresponds to the side portion of the extension section, and the lower side portion of the extension section refers to the lower side portion. It can be understood that when the elastic coating tube of the present invention is worn, the elastic coating tube can be replaced.

[0047] In some preferred embodiments, at least one annular groove 201 is circumferentially arranged at both ends of the elastic coated tube 2, and the portion where the annular groove 201 is located forms the end of the elastic coated tube 2 close to the sliding surface 101 and the end away from the sliding surface 101. The elastic coated tube 2 also includes a middle portion, and the length L2 of the middle portion is the width value of the electrode to be manufactured, and the sum of the length L3 of the end close to the sliding surface 101 and the length L4 of the end away from the sliding surface 101 is the tolerance value of the width of the electrode to be manufactured.

[0048] The coating of conductive slurry usually allows a certain tolerance value. Under this preferred solution, at least one annular groove is provided along the circumference at both ends of the elastic coating tube. The groove can accommodate excess slurry during coating. The part where the annular groove is located forms the end of the elastic coating tube close to the sliding surface and the end away from the sliding surface, and the middle is the middle part. By making the length L2 of the middle part the width value of the electrode to be made, the sum of the length L3 of the end close to the sliding surface and the length L4 of the end away from the sliding surface is the tolerance value of the width of the electrode to be made, it is more conducive to accurately control the width of the slurry coating, avoid the conductive slurry coating width exceeding the tolerance, ensure that the conductive slurry is accurately coated in the area of ​​the electrode to be made, and avoid the slurry coating on the electrode half-cut step causing a short circuit. The annular groove 201 at the end close to the sliding surface 101 prevents the slurry from overflowing into the gap between the slider and the elastic coating tube, or overflowing to the outside of the PDLC film, affecting the film quality.

[0049] The present invention does not limit the number and shape of the annular grooves. The shape of the groove cross section can be arc-shaped, V-shaped, etc., preferably V-shaped. When there are multiple annular grooves, it is preferred that the multiple annular grooves are arranged continuously. Figure 8 The tolerance value of the width of the electrode to be manufactured refers to the maximum allowable deviation from the preset width value of the electrode to be manufactured. The coating tolerance of the electronic conductive paste is ±0.5mm, and the tolerance value of the width of the electrode to be manufactured is 0.5mm.

[0050] The present invention does not limit the specific structure of the discharge pipe passing through the inside of the first sliding block. In some preferred embodiments, the discharge pipe 3 includes a first discharge pipe 302 arranged parallel to the sliding surface 101 and a second discharge pipe 303 perpendicular to the first discharge pipe 302. The first discharge pipe 302 and the second discharge pipe 303 both have a first end and a second end. The first end of the first discharge pipe 302 is connected to the slurry supply module 4, and the first end of the second discharge pipe 303 extends outward through the sliding surface 101 to form an extension section. The second end of the first discharge pipe 302 is connected to the second end of the second discharge pipe 303. The second end of the first discharge pipe 302 protrudes from the second discharge pipe 303, and the second end of the second discharge pipe 303 protrudes from the first discharge pipe 302.

[0051] Under this preferred embodiment, the discharge pipe includes a first discharge pipe arranged parallel to the sliding surface and a second discharge pipe perpendicular to the first discharge pipe, which are connected through the second end of the first discharge pipe and the second end of the second discharge pipe, the second end of the first discharge pipe protrudes from the second discharge pipe, and the second end of the second discharge pipe protrudes from the first discharge pipe. By setting a protruding structure, the slurry is swirled at the protruding structure, which is more conducive to increasing the turbulent flow of the slurry in the discharge pipe, mixing the slurry, improving the uniformity of the discharged slurry, improving the stability of the prepared electrode, the adhesion and electrical properties after coating, and more conducive to maintaining pressure and material, ensuring the stable discharge of the slurry. It can be understood that the first end of the first discharge pipe is located at the upper part and the second end is located at the lower part, which promotes the smooth flow of the slurry. This structure of increasing the turbulent flow of the slurry of the present invention is easy to process. It can be understood that when the present invention is pumping the slurry, the slurry will not protrude from the second discharge pipe at the second end of the first discharge pipe, and the second end of the second discharge pipe protrudes from the first discharge pipe. The convex structure formed by the first discharge pipe is retained.

[0052] Preferably, the inner diameter of the first discharge pipe 302 is greater than the inner diameter of the second discharge pipe 303, and the ratio of the inner diameter of the first discharge pipe 302 to the inner diameter of the second discharge pipe 303 is 1.5 to 10. Under this preferred embodiment, the inner diameter of the first discharge pipe is greater than the inner diameter of the second discharge pipe, which is conducive to increasing turbulent flow, mixing the slurry, improving the uniformity of the discharged slurry, maintaining pressure and material, and ensuring stable discharge of the slurry. Furthermore, the ratio of the inner diameter of the first discharge pipe to the inner diameter of the second discharge pipe is 1.5 to 10, which is more conducive to mixing the slurry and ensuring stable discharge of the slurry.

[0053] In some preferred embodiments, the first slider 1 is further provided with a speed sensor 5, and the manufacturing device further includes a slurry supply control unit, wherein the speed sensor 5, the slurry supply control unit, and the slurry supply module 4 are electrically connected in sequence. In this preferred solution, the slurry supply control unit obtains the movement speed of the first slider through the speed sensor, and controls the speed of the slurry supply module supplying the slurry according to the movement speed of the first slider, so as to achieve accurate control of the slurry supply amount according to the movement speed of the first slider, and is more conducive to accurately controlling the width of the slurry coating when the movement speed of the first slider deviates under the driving action of the driving device, so as to ensure that the conductive slurry is accurately coated on the area to be manufactured. When the first slider is in a stationary state and does not move, the slurry supply module can also be controlled not to supply slurry.

[0054] In some preferred embodiments, a first slider contact detection component 6 is further provided on the first slider 1, and the manufacturing device also includes a discharge control unit, and the first slider contact detection component 6 is electrically connected to the discharge control unit. When the first slider contact detection component 6 detects that the sliding surface 101 is in contact with the side of the electrode to be manufactured of the PDLC membrane, the discharge control unit does not operate, and the slurry flows out from the discharge port 301. Under this preferred scheme, when the first slider contact detection component detects that the sliding surface abuts the side of the PDLC membrane on the electrode to be manufactured, the discharge control unit is controlled not to operate, and the slurry flows out from the discharge port. When the first slider contact detection component does not detect that the sliding surface abuts the side of the PDLC membrane on the electrode to be manufactured, the discharge control unit is operated to control the slurry not to flow out from the discharge port. Deviations may occur during the movement of the first slider, and the sliding surface does not abut the side of the PDLC membrane on the electrode to be manufactured, resulting in a deviation in the position of the discharge port and a deviation in the coating area of ​​the elastic coating tube. If not handled in time, the slurry coating position is prone to deviation. At this time, stopping the discharge to remind the occurrence of the abnormal situation of the sliding surface not abutting is more conducive to avoiding deviations in the slurry coating position, ensuring that the conductive slurry is accurately coated in the area of ​​the electrode to be manufactured, and also avoiding waste of slurry.

[0055] The present invention does not limit the discharge control unit, which can be set at any position on the discharge pipe, and can be a discharge valve on the discharge pipe. The discharge control unit can also be the aforementioned slurry supply control unit, which controls the slurry supply module to stop supplying, thereby controlling the slurry not to flow out of the discharge port.

[0056] Preferably, a concave portion 102 is provided on the sliding surface 101 of the first slider 1 directly below the elastic coating tube 2, and the first slider contact detection component 6 is embedded in the concave portion 102. The first slider contact detection component 6 includes an elastic member 601, a second slider 602 and a pressure sensor 603. The pressure sensor 603 is electrically connected to the discharge control unit. The elastic deformation direction of the elastic member 601 is perpendicular to the sliding surface 101. The elastic member 601 has a first end and a second end along the elastic deformation direction. 1 is connected to the inner wall of the recess 102, the second end of the elastic member 601 is connected to one end of the second slider 602, the second slider 602 has one end away from the elastic member 601, when the elastic member 601 is in a natural state, the end away from the elastic member protrudes from the sliding surface 101, when the end away from the elastic member is flush with the sliding surface 101, the end of the second slider 602 connected to the elastic member 601 abuts against the pressure sensor 603, and the discharge control unit does not operate. Under this preferred solution, by embedding the first slider contact detection component in the recess directly below the elastic coating tube, a specific form of the first slider contact detection component is adopted, the pressure sensor is electrically connected to the discharge control unit, and the signal transmitted to the discharge control unit by the pressure sensor controls whether the discharge control unit operates, which is more conducive to avoiding deviations in the slurry coating position, ensuring that the conductive slurry is accurately coated in the area where the electrode is to be made, and avoiding waste of slurry.

[0057] The present invention does not limit the connection method of the elastic coated tube to the sliding surface. In some preferred embodiments, a fixed shaft 7 is connected to the sliding surface 101, and the fixed shaft 7 is perpendicular to the sliding surface 101. The elastic coated tube 2 is sleeved on the outer periphery of the fixed shaft 7 and has an interference fit with the outer periphery of the fixed shaft 7. The central axis of the fixed shaft 7 coincides with the central axis of the elastic coated tube 2.

[0058] The slurry supply module 4 of the present invention may include a slurry storage barrel 401 and a slurry pump. A stirring component 10 may be provided in the slurry storage barrel 401 to mix the slurry and increase the fluidity of the slurry. The wall of the slurry storage barrel 401 may be a double-layer structure with a vacuum layer between the double-layer structure to reduce the effect of the ambient temperature on the viscosity of the electronic slurry. Preferably, the viscosity of the slurry in the slurry storage barrel 401 is controlled within 5000-40000 Pa·s, and the rotation speed of the stirring component 10 is controlled within 20-40 rpm.

[0059] The slurry supply module and the discharge pipe can be connected by a hose, and the hose can be a hose with internal threads to increase the disturbance of the slurry. The present invention can also add a slurry filtering mechanism before the slurry flows into the discharge pipe to prevent impurities in the slurry from entering. In the present invention, the slurry supply control unit can be in the form of a microprocessor, and the slurry supply control unit controls the pumping state such as the speed of the slurry pump pumping the slurry.

[0060] The discharge port 301 of the present invention is arranged at the lower side of the extension section. Figure 5 When the device is configured to protrude downward as shown, the vertical distance between the discharge port and the area where the electrode is to be manufactured is preferably not less than 3 mm to avoid scratching the conductive layer of the PDLC dimming film.

[0061] In a second aspect, the present invention provides a method for manufacturing a PDLC dimming film electrode, which adopts the manufacturing device described in the first aspect, and the manufacturing method includes: half-cutting the electrode side of the PDLC film to be manufactured to form a half-cut step 9, so that the sliding surface 101 of the first slider 1 is in contact with the side surface 8 of the electrode side to be manufactured, the slurry supply module 4 provides slurry to the discharge pipe 3 so that the discharge port 301 flows out the slurry, and the first slider 1 moves along the extension direction of the electrode to be manufactured, the first slider 1 drives the discharge port 301 on the discharge pipe 3 and the elastic coating tube 2 to move along the extension direction, and the discharge port 301 provides slurry to the area of ​​the electrode to be manufactured and the elastic coating tube 2 coats the slurry simultaneously.

[0062] In some preferred embodiments, after receiving the moving speed of the first slider 1 transmitted by the speed sensor 5, the slurry supply control unit calculates the slurry supply speed and controls the slurry supply module 4 to supply slurry according to the slurry supply speed, wherein the slurry supply speed is the product of the moving speed of the first slider 1 and the preset slurry dosage per unit length of the electrode. When the first slider is in a stationary state and does not move, the speed sensor does not detect the speed, and the slurry supply control unit can also control the slurry supply module not to supply slurry. For example, the slurry dosage per unit length of the electrode is N (unit: g / mm), the moving speed of the first slider is V (unit: mm / s), the slurry supply speed is W (unit: g / s), W=N×V, when the electrode width is 5mm, the slurry dosage per unit length of the electrode is 0.0005g / mm, the moving speed of the first slider is 10mm / s, and the slurry supply speed is 0.005g / s.

[0063] In some preferred embodiments, when the first slider contact detection component 6 detects that the sliding surface 101 is in contact with the side 8 of the electrode to be manufactured, the discharge control unit does not operate, and the slurry flows out from the discharge port 301; when the first slider contact detection component 6 does not detect that the sliding surface 101 is in contact with the side 8 of the electrode to be manufactured, the discharge control unit operates, and the slurry does not flow out from the discharge port 301.

[0064] Preferably, the end of the second slider 602 facing away from the elastic member is flush with the sliding surface 101, the elastic member 601 is compressed, the end of the second slider 602 connected to the elastic member 601 abuts against the pressure sensor 603, and the discharge control unit does not operate.

[0065] In a third aspect, the present invention provides a method for manufacturing a PDLC dimming film, wherein the manufacturing device described in the first aspect or the manufacturing method described in the second aspect is used to manufacture a PDLC dimming film electrode. The manufacturing method of the PDLC dimming film of the present invention can efficiently and evenly and accurately coat the conductive paste on the area where the electrode is to be manufactured.

[0066] In a fourth aspect, the present invention provides a PDLC dimming film, which is manufactured by the manufacturing method of the PDLC dimming film described in the third aspect.

[0067] In some specific embodiments of the present invention, a method for manufacturing a PDLC dimming film electrode is as follows: Figures 1 to 9 The production device shown is carried out Figure 2 The middle arrow indicates the movement direction of the first slider, i.e., the extension direction of the electrode to be manufactured, including: half-cutting the electrode side of the PDLC film to be manufactured to form a half-cut step 9, so that the sliding surface 101 of the first slider 1 abuts against the side surface 8 of the electrode side to be manufactured, at this time, the end of the second slider 602 in the first slider contact detection assembly 6 embedded in the recess 102 directly below the elastic coating tube 2, which is away from the elastic member, is flush with the sliding surface 101, the elastic member 601 is compressed, and the end of the second slider 602 connected to the elastic member 601 contacts the pressure sensor 603, and the pressure sensor 603 transmits the pressure to the sliding surface 101 of the first slider 1 of the slurry supply control unit. 1 is in contact with the side surface 8 of the electrode to be manufactured, the slurry supply control unit does not operate, and after the slurry is supplied, the slurry flows out from the discharge port 301, the slurry supply module 4 provides slurry to the discharge pipe 3 so that the slurry flows out from the discharge port 301, and at the same time drives the first slider 1 to move along the extension direction of the electrode to be manufactured through the driving device, the first slider 1 drives the discharge port 301 and the elastic coating tube 2 on the discharge pipe 3 to move along the aforementioned extension direction, the discharge port 301 moves in the front to provide slurry to the area to be manufactured, and the elastic coating tube 2 moves in the back to coat the slurry, and the discharge port 301 provides slurry to the area to be manufactured and the elastic coating tube 2 coats the slurry synchronously and automatically.

[0068] During the movement of the first slider 1, the speed sensor 5 on the first slider 1 transmits the movement speed of the first slider 1 to the slurry supply control unit. After receiving the movement speed of the first slider 1, the slurry supply control unit calculates the slurry supply speed, and the slurry supply control unit controls the slurry supply module 4 to supply slurry according to the calculated slurry supply speed. When the speed sensor 5 detects that the first slider 1 is stationary or in an abnormal situation, the slurry supply control unit controls the slurry supply module 4 not to supply slurry. Deviations may occur during the movement of the first slider 1, and the sliding surface 101 does not abut against the side surface 8 of the electrode side to be manufactured of the PDLC membrane. At this time, the pressure sensor 603 interrupts the signal to the slurry supply control unit that the sliding surface 101 of the first slider 1 abuts against the side surface 8 of the electrode side to be manufactured, and the slurry supply control unit controls the slurry supply module 4 to stop supplying, thereby controlling the slurry not to flow out from the discharge port 301.

[0069] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A manufacturing device for a PDLC dimming film electrode, characterized in that: include: A first slider (1), the first slider (1) having a sliding surface (101), and when the first slider (1) slides, the sliding surface (101) is used to abut against a side surface of the PDLC film on the electrode side to be manufactured; An elastic coating tube (2) connected to the sliding surface (101), wherein the axis thereof is perpendicular to the sliding surface (101), and the length L1 thereof matches the width of the electrode to be manufactured; a discharge pipe (3) passing through the interior of the first sliding block (1), one end of which is connected to the slurry supply module (4), and the other end of which passes through the sliding surface (101) and extends outward to form an extension section, the discharge port (301) being arranged at the lower side of the extension section, and the distance between the center of the discharge port (301) and the sliding surface (101) matching the half width of the electrode to be manufactured; The first slider (1) is also provided with a first slider contact detection component (6), and the manufacturing device further comprises a discharge control unit, the first slider contact detection component (6) being electrically connected to the discharge control unit, and when the first slider contact detection component (6) detects that the sliding surface (101) is in contact with the side surface of the electrode to be manufactured of the PDLC film, the discharge control unit does not operate, and the slurry flows out from the discharge port (301); The sliding surface (101) of the first sliding block (1) is provided with a recess (102) located directly below the elastic coating tube (2), the recess (102) having the first sliding block contact detection assembly (6) embedded therein, the first sliding block contact detection assembly (6) comprising an elastic member (601), a second sliding block (602) and a pressure sensor (603), the pressure sensor (603) being electrically connected to the material discharging control unit, the elastic deformation direction of the elastic member (601) being perpendicular to the sliding surface (101), the elastic member (601) having a first end and a second end along the elastic deformation direction, the first end of the elastic member (601) One end is connected to the inner wall of the recess (102), the second end of the elastic member (601) is connected to one end of the second slider (602), the second slider (602) has one end facing away from the elastic member (601), when the elastic member (601) is in a natural state, the end facing away from the elastic member (601) protrudes from the sliding surface (101), when the end facing away from the elastic member (601) is flush with the sliding surface (101), the end of the second slider (602) connected to the elastic member (601) abuts against the pressure sensor (603), and the discharge control unit does not operate.

2. The manufacturing device according to claim 1, characterized in that: Both ends of the elastic coating tube (2) are provided with at least one annular groove (201) along the circumferential direction, and the portion where the annular groove (201) is located forms an end portion of the elastic coating tube (2) close to the sliding surface (101) and an end portion away from the sliding surface (101). The elastic coating tube (2) also includes a middle portion, the length L2 of the middle portion is the width value of the electrode to be manufactured, and the sum of the length L3 of the end portion close to the sliding surface (101) and the length L4 of the end portion away from the sliding surface (101) is the tolerance value of the width of the electrode to be manufactured.

3. The manufacturing device according to claim 1, characterized in that: The discharge pipe (3) comprises a first discharge pipe (302) arranged parallel to the sliding surface (101) and a second discharge pipe (303) perpendicular to the first discharge pipe (302), the first discharge pipe (302) and the second discharge pipe (303) both having a first end and a second end, the first end of the first discharge pipe (302) being connected to the slurry supply module (4), the first end of the second discharge pipe (303) extending outward through the sliding surface (101) to form an extension section, the second end of the first discharge pipe (302) and the second end of the second discharge pipe (303) being connected, the second end of the first discharge pipe (302) protruding from the second discharge pipe (303), and the second end of the second discharge pipe (303) protruding from the first discharge pipe (302).

4. The manufacturing device according to claim 3, characterized in that: The inner diameter of the first discharge pipe (302) is greater than the inner diameter of the second discharge pipe (303), and the ratio of the inner diameter of the first discharge pipe (302) to the inner diameter of the second discharge pipe (303) is 1.5-10.

5. The manufacturing device according to claim 1, characterized in that: The first slider (1) is also provided with a speed sensor (5), and the manufacturing device further comprises a slurry supply control unit, wherein the speed sensor (5), the slurry supply control unit, and the slurry supply module (4) are electrically connected in sequence.

6. The manufacturing device according to claim 1, characterized in that: The sliding surface (101) is connected to a fixed shaft (7), the fixed shaft (7) being perpendicular to the sliding surface (101), the elastic coating tube (2) being sleeved on the outer circumference of the fixed shaft (7) and having an interference fit with the outer circumference of the fixed shaft (7), and the central axis of the fixed shaft (7) coincides with the central axis of the elastic coating tube (2).

7. A method for manufacturing a PDLC dimming film electrode, characterized in that: The manufacturing device according to any one of claims 1 to 6 is used, and the manufacturing method comprises: half-cutting the electrode side of the PDLC film to be manufactured to form a half-cut step (9), so that the sliding surface (101) of the first slider (1) is in contact with the side surface (8) of the electrode side to be manufactured, the slurry supply module (4) provides slurry to the discharge pipe (3) so that the slurry flows out of the discharge port (301), so that the first slider (1) moves along the extension direction of the electrode to be manufactured, the first slider (1) drives the discharge port (301) on the discharge pipe (3) and the elastic coating tube (2) to move along the extension direction, and the discharge port (301) provides slurry to the area of ​​the electrode to be manufactured and the elastic coating tube (2) coats the slurry synchronously.

8. The method according to claim 7, characterized in that: After receiving the moving speed of the first slider (1) transmitted by the speed sensor (5), the slurry supply control unit calculates the slurry supply speed and controls the slurry supply module (4) to supply slurry according to the slurry supply speed, wherein the slurry supply speed is the product of the moving speed of the first slider (1) and a preset slurry consumption per unit length of the electrode.

9. The manufacturing method according to claim 7, characterized in that: When the first slider contact detection component (6) detects that the sliding surface (101) is in contact with the side surface (8) of the electrode to be manufactured, the discharge control unit does not operate, and the slurry flows out from the discharge port (301); when the first slider contact detection component (6) does not detect that the sliding surface (101) is in contact with the side surface (8) of the electrode to be manufactured, the discharge control unit operates, and the slurry does not flow out from the discharge port (301).

10. The manufacturing method according to claim 9, characterized in that: The end of the second sliding block (602) facing away from the elastic member is flush with the sliding surface (101), the elastic member (601) is compressed, the end of the second sliding block (602) connected to the elastic member (601) is in contact with the pressure sensor (603), and the material discharging control unit does not operate.

11. A method for manufacturing a PDLC dimming film, characterized in that: The PDLC dimming film electrode is manufactured by using the manufacturing device described in any one of claims 1 to 6 and / or the manufacturing method described in any one of claims 7 to 10.

12. A PDLC dimming film, characterized in that: The PDLC dimming film is manufactured by the manufacturing method of the PDLC dimming film according to claim 11.