A method for determining the threshold value of magnetic field parameters for negative pressure arc welding

By establishing a mathematical model of negative voltage arc and numerical simulation method, the threshold of magnetic field parameter of negative voltage arc welding was determined, which solved the problem of uncertainty in magnetic field parameter threshold in the prior art, improved the welding quality and efficiency, and was suitable for thin-wall surfacing and Inclined welding.

CN118468736BActive Publication Date: 2024-12-06SHANGHAI UNIV OF ENG SCI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410238313.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-03-03
Publication Date
2024-12-06
Estimated Expiration
2044-03-03

AI Technical Summary

Technical Problem

The prior art is difficult to accurately determine the threshold of the magnetic field parameter of the negative voltage arc welding, resulting in unstable flow of the molten pool and welding defects during the welding process, and consumes a lot of resources to conduct creative experiments.

Method used

By establishing a mathematical model of negative voltage arcs, numerical simulation methods are used to calculate and fit the magnetic field parameter threshold under different conditions, the equation for determining the magnetic field parameters of negative voltage arc welding is obtained, and the uncertainty problem of magnetic field parameter threshold is solved.

Benefits of technology

It realizes more accurately predicting the negative voltage arc welding conditions, improves welding quality and efficiency, and is suitable for controlling the flow behavior of the molten pool during thin-wall surfacing and inclined welding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118468736B_ABST
    Figure CN118468736B_ABST
Patent Text Reader

Abstract

The invention provides a method for determining a threshold value of a magnetic field parameter of a negative pressure arc welding, comprising: forming a control equation by using a Navier-Stokes equation, a heat transfer equation and a Maxwell electromagnetic equation; establishing a geometric model and meshing; setting material parameters; setting initial conditions and boundary conditions; performing a parametric scan and setting a solver; collecting negative pressure threshold data and fitting a negative pressure threshold function; through the above steps, numerically simulating and calculating the negative pressure threshold under different conditions, and then fitting the calculated negative pressure threshold data, an equation for determining the threshold value of the magnetic field parameter of the negative pressure arc welding is obtained, so that the welding threshold condition of the negative pressure arc can be more accurately predicted, and guidance can be provided for the negative pressure arc welding technology; and the flow and instability behavior of the molten pool caused by gravity, positive arc pressure and plasma flow force in the molten pool during conventional positive pressure arc thin-wall cladding, thin-wall additive manufacturing and inclined welding is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of arc welding, and in particular to a method for determining a threshold value of a magnetic field parameter of negative pressure arc welding. Background Art

[0002] Gas Tungsten Arc Welding (GTAW) is a common technology in the field of welding. It has good weld formation and less spatter. It is mainly used for welding thin walls and non-ferrous metals. However, the excavation effect of the positive pressure of the conventional GTAW welding arc on the molten pool will cause the molten pool to be unstable and produce welding defects. In thin-wall cladding and inclined welding, the welding molten pool will flow to the side wall under the action of gravity, arc blowing force and surface tension, reducing the accuracy and performance of the welded workpiece. Although the side wall flow phenomenon of the welding molten pool can be improved by the method of physical constraints, the physical constraints occupy a large welding workpiece and have poor flexibility in dealing with different welding situations, which cannot meet the welding and forming of complex components. At the same time, excessive arc pressure will also produce spatter during the welding process, reducing the welding quality.

[0003] By forming an arc negative pressure on the surface of the welding molten pool in the opposite direction of gravity, the molten pool can be sucked upward and the flow behavior of the molten pool can be changed. The use of arc negative pressure can improve the molten pool flow problem and welding defects during the welding process, thereby improving the welding quality and efficiency, which has important research significance.

[0004] At present, the main means of forming a negative pressure arc is to apply a longitudinal magnetic field. However, due to the different currents or other conditions in the arc welding process, the magnetic field transition threshold for converting positive pressure into negative pressure is also different. Currently, a large number of creative experiments are required to determine it, which consumes a lot of energy, time, manpower and financial costs. The uncertainty of this magnetic field parameter threshold is a major problem that needs to be solved in the current in-depth research and technology of negative pressure arc welding.

[0005] In view of this, the present invention proposes a method for determining a threshold value of a magnetic field parameter of negative pressure arc welding to solve the above problem. Summary of the invention

[0006] To solve the above problems, the purpose of the present invention is to propose a method for determining the threshold value of magnetic field parameters of negative pressure arc welding, and further use numerical simulation methods to quantitatively formulate and determine the threshold value of magnetic field parameters under different conditions.

[0007] To achieve the above technical objectives, the present invention provides a method for determining the threshold value of the magnetic field parameter of negative pressure arc welding. First, a negative pressure arc mathematical model is established, the negative pressure threshold value under different conditions is calculated, and then the calculated negative pressure threshold value data is fitted to obtain an equation for determining the threshold value of the magnetic field parameter of negative pressure arc welding;

[0008] Step 1: Establish the governing equations: The governing equations consist of the Navier-Stokes equations, the heat transfer equations, and the Maxwell electromagnetic equations:

[0009] The velocity and pressure distribution of arc plasma are determined according to the mass conservation equation and momentum conservation equation:

[0010]

[0011]

[0012] Among them, ρ is density; v is velocity vector; P is pressure; μ is viscosity; I is the identity matrix; F is the momentum source term;

[0013] Solve the arc temperature T according to the energy conservation equation:

[0014]

[0015] Where k is the thermal conductivity; T is the temperature; Cp is the specific heat capacity; Q is the source term of the energy conservation equation;

[0016] The electric potential and magnetic vector potential distribution are calculated based on the current continuity equation and Ohm's law:

[0017]

[0018]

[0019] Where V is the electric potential, A is the magnetic vector potential, and σ is the conductivity;

[0020] According to V and A, we can obtain the current density J, electric field E and magnetic induction intensity B:

[0021]

[0022]

[0023]

[0024] Among them, J is the current density, E is the electric field, and B is the magnetic induction intensity;

[0025] The arc energy source term consists of three parts: Joule heat, electron enthalpy transfer and arc radiation loss:

[0026]

[0027] Among them, K B is the Boltzmann constant; e is the electron charge; T is the temperature field of the arc shape; Q is the heat source term; Q rad is the arc radiation loss;

[0028] According to the arc self-induced magnetic field intensity B, current density J and momentum conservation equation, the momentum source term in the momentum conservation equation is solved:

[0029] F=J×B (10)

[0030] Step 2: Establish geometric model and mesh division: Establish geometric model of hollow tungsten arc and solid tungsten arc, and then selectively mesh the model;

[0031] Step 3: Set material parameters: Selectively set material parameters for each area of ​​the geometric model;

[0032] Step 4: Set initial conditions and boundary conditions: consisting of boundary heat flux, cathode boundary, anode boundary, pressure, current density and potential, and loading volume force J*(B+B0);

[0033] The boundary conditions are as follows:

[0034] (1) Solid current density input:

[0035]

[0036] (2) Current density of hollow tungsten electrode:

[0037]

[0038] (3) Shielding gas flow rate:

[0039]

[0040] I is the welding current, Q is the shielding gas flow rate, Rn is the shielding gas inlet radius, Rw is the tungsten electrode radius, Ri is the inner diameter of the hollow cavity, and r is the distance from the shielding gas inlet to the center;

[0041] (4) The specific formula for cathode is as follows:

[0042]

[0043] J e =J r [(|J·n|-J r )>0]+|J·n|[(|J·n|-J r )<0] (15)

[0044] J i =|J·n|-J e (16)

[0045]

[0046] (5) The specific formula for anode is as follows:

[0047]

[0048] Among them, |J i |V i is cathode ion heat, It is the electronic heat that plays a cooling role; is the surface work function; V i is the ionization potential of argon; A r is the Richardson constant, is the cathode effective work function, e is the elementary charge, k b is the Boltzmann constant.

[0049] (6) Add external electromagnetic force by changing the momentum source term:

[0050] F=J×(B+B0) (19)

[0051] Wherein, B0 is the magnetic induction intensity of the external longitudinal magnetic field;

[0052] Step 5: Parametric scanning, set up the solver: According to the above steps, perform calculations and solve, and verify whether the calculation results are consistent with the experimental results under the same conditions. If they are consistent, proceed to the next step; otherwise, return to step 2, adjust the model or boundary conditions, and repeat the cycle of modeling and numerical simulation calculations until the calculation results are consistent with the experimental results under the same conditions, completing the model accuracy verification;

[0053] Step 6: Fix the model and solution method, perform parameterized batch calculation to obtain the negative pressure welding parameter thresholds under various other conditions, process the negative pressure welding threshold data, and determine the negative pressure welding threshold function: fit multiple groups of negative pressure welding threshold data under different conditions to obtain the function equation of the negative pressure arc welding longitudinal magnetic field parameter threshold.

[0054] Furthermore, in step 2, the hollow tungsten arc is subjected to vacuum pressure to study the effect of vacuum pressure on the physical properties of the hollow tungsten arc;

[0055] Furthermore, the mesh division in step 2 may be tetrahedron or hexahedron;

[0056] Furthermore, the protective gas in step 4 is 99.99% argon, or helium, or a mixed inert gas, and the external magnetic field is a longitudinal magnetic field mode, a uniform alternating magnetic field mode, an intermittent alternating magnetic field mode, or a pulsed alternating magnetic field mode.

[0057] Furthermore, for welding current 80-200A, arc length 3mm, 100% pure argon protection, and solid tungsten electrode conditions, the functional relationship between welding current and magnetic field strength that constitutes the negative pressure GTAW welding threshold is: B(I)=0.0225+2.56e-5*exp(I / 29.9).

[0058] Furthermore, it is applicable to negative pressure arc welding technology, or negative pressure arc additive manufacturing technology, or negative pressure arc-laser composite welding technology, or negative pressure arc-laser composite cladding technology, or negative pressure arc-laser composite additive manufacturing technology, or negative pressure arc-high energy beam composite welding technology, or negative pressure arc-high energy beam composite cladding technology, or negative pressure arc-high energy beam composite additive manufacturing technology.

[0059] The beneficial effects of the present invention are as follows: by establishing a negative pressure arc mathematical model, analyzing the distribution of electric pressure under an applied longitudinal magnetic field and exhaust pressure, performing numerical simulation calculations on the negative pressure thresholds under different conditions, and then fitting the calculated negative pressure threshold data, an equation for determining the threshold of the magnetic field parameter of negative pressure arc welding is obtained, which can more accurately predict the occurrence of negative pressure and provide guidance for negative pressure arc welding technology; and solving the problem of the molten pool flow behavior formed by gravity, arc pressure and plasma flow force in the process of GTAW thin-wall cladding and inclined welding.

[0060] The purpose, features and advantages of the present invention will be further described with reference to the accompanying drawings in conjunction with the embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0061] Figure 1 It is a schematic diagram of the process of the present invention;

[0062] Figure 2 It is a geometric model diagram of the solid tungsten pole of the present invention;

[0063] Figure 3 It is a geometric model diagram of the hollow tungsten pole of the present invention;

[0064] Figure 4 It is the center pressure diagram of the workpiece of the present invention at different currents of 0 to 0.04T in the solid tungsten arc;

[0065] Figure 5 It is a magnetic field parameter threshold diagram of the workpiece center pressure change of 0-0.04T at different currents in a solid tungsten pole arc of the present invention;

[0066] Figure 6 It is a workpiece center pressure diagram of 0-0.05T at different exhaust pressures during hollow tungsten arc of the present invention;

[0067] Figure 7It is a magnetic field parameter threshold diagram of the workpiece center pressure transition of 0-0.05T at different exhaust pressures during hollow tungsten pole arc of the present invention. DETAILED DESCRIPTION

[0068] The following embodiments of the present invention are described in further detail in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0069] In the description of the present invention, unless otherwise specified, "plurality" means two or more than two; the orientations or positional relationships indicated by the terms "upper", "lower", "left", "right", "inner", "outer", "front end", "rear end", "head", "tail", etc. are based on the orientations or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", "third", etc. are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.

[0070] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "connected" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0071] 1. Combine the following Figures 1 to 7 A method for determining a negative pressure arc welding magnetic field parameter threshold value provided by the present invention is described: firstly, a negative pressure arc mathematical model is established, the negative pressure threshold values ​​under different conditions are calculated, and then the calculated negative pressure threshold value data is fitted to obtain an equation for determining the negative pressure arc welding magnetic field parameter threshold value;

[0072] like Figure 1 The schematic flow diagram of the present invention shown specifically comprises the following steps:

[0073] Step 1: Establish the governing equations: The governing equations consist of the Navier-Stokes equations, the heat transfer equations, and the Maxwell electromagnetic equations:

[0074] The velocity and pressure distribution of arc plasma are determined according to the mass conservation equation and momentum conservation equation:

[0075]

[0076]

[0077] Among them, ρ is density; v is velocity vector; P is pressure; μ is viscosity; I is the identity matrix; F is the momentum source term;

[0078] Solve the arc temperature T according to the energy conservation equation:

[0079]

[0080] Where k is the thermal conductivity; T is the temperature; Cp is the specific heat capacity; Q is the source term of the energy conservation equation;

[0081] The electric potential and magnetic vector potential distribution are calculated based on the current continuity equation and Ohm's law:

[0082]

[0083]

[0084] Where V is the electric potential, A is the magnetic vector potential, and σ is the conductivity;

[0085] According to V and A, we can obtain the current density J, electric field E and magnetic induction intensity B:

[0086]

[0087]

[0088]

[0089] Among them, J is the current density, E is the electric field, and B is the magnetic induction intensity;

[0090] The arc energy source term consists of three parts: Joule heat, electron enthalpy transfer and arc radiation loss:

[0091]

[0092] Among them, K B is the Boltzmann constant; e is the electron charge; T is the temperature field of the arc shape; Q is the heat source term; Q rad is the arc radiation loss;

[0093] According to the arc self-induced magnetic field intensity B, current density J and momentum conservation equation, the momentum source term in the momentum conservation equation is solved:

[0094] F=J×B (10)

[0095] Step 2: Establish geometric model and mesh division: Establish geometric model of hollow tungsten arc and solid tungsten arc, and then selectively mesh the model;

[0096] Step 3: Set material parameters: Selectively set material parameters for each area of ​​the geometric model;

[0097] Step 4: Set initial conditions and boundary conditions: consisting of boundary heat flux, cathode boundary, anode boundary, pressure, current density and potential, and loading volume force J*(B+B0);

[0098] The boundary conditions are as follows:

[0099] (1) Solid current density input:

[0100]

[0101] (2) Current density of hollow tungsten electrode:

[0102]

[0103] (3) Shielding gas flow rate:

[0104] (13)

[0105] I is the welding current, Q is the shielding gas flow rate, Rn is the shielding gas inlet radius, Rw is the tungsten electrode radius, Ri is the inner diameter of the hollow cavity, and r is the distance from the shielding gas inlet to the center;

[0106] (4) The specific formula for cathode is as follows:

[0107]

[0108] J e =J r [(|J·n|-J r )>0]+|J·n|[(|J·n|-J r )<0] (15)

[0109] J i =|J·n|-J e (16)

[0110]

[0111] (5) The specific formula for anode is as follows:

[0112]

[0113] Among them, |J i |V i is cathode ion heat, It is the electronic heat that plays a cooling role; is the surface work function; V i is the ionization potential of argon; A ris the Richardson constant, is the cathode effective work function, e is the elementary charge, k b is the Boltzmann constant.

[0114] (6) Add external electromagnetic force by changing the momentum source term:

[0115] F=J×(B+B0) (19)

[0116] Wherein, B0 is the magnetic induction intensity of the external longitudinal magnetic field;

[0117] Step 5: Parametric scanning, set up the solver: According to the above steps, perform calculations and solve, and verify whether the calculation results are consistent with the experimental results under the same conditions. If they are consistent, proceed to the next step; otherwise, return to step 2, adjust the model or boundary conditions, and repeat the cycle of modeling and numerical simulation calculations until the calculation results are consistent with the experimental results under the same conditions, completing the model accuracy verification;

[0118] Step 6: Fix the model and solution method, perform parameterized batch calculation to obtain the negative pressure welding parameter thresholds under various other conditions, process the negative pressure welding threshold data, and determine the negative pressure welding threshold function: fit multiple groups of negative pressure welding threshold data under different conditions to obtain the function equation of the negative pressure arc welding longitudinal magnetic field parameter threshold.

[0119] In the step 2, the hollow tungsten arc is subjected to exhaust pressure to study the effect of the exhaust pressure on the physical properties of the hollow tungsten arc.

[0120] The mesh division in step 2 may be tetrahedral or hexahedral.

[0121] The protective gas in step 4 is 99.99% argon, or helium, or a mixed inert gas, and the external magnetic field is a longitudinal magnetic field mode, a uniform alternating magnetic field mode, an intermittent alternating magnetic field mode, or a pulsed alternating magnetic field mode.

[0122] For welding current of 80-200A, arc length of 3mm, 100% pure argon protection, and solid tungsten electrode conditions, the functional relationship between welding current and magnetic field strength that constitutes the negative pressure GTAW welding threshold is: B(I)=0.0225+2.56e-5*exp(I / 29.9).

[0123] Applicable to negative pressure arc welding technology, or negative pressure arc additive manufacturing technology, or negative pressure arc-laser composite welding technology, or negative pressure arc-laser composite cladding technology, or negative pressure arc-laser composite additive manufacturing technology, or negative pressure arc-high energy beam composite welding technology, or negative pressure arc-high energy beam composite cladding technology, or negative pressure arc-high energy beam composite additive manufacturing technology.

[0124] Embodiment 1

[0125] The method for determining the threshold value of the magnetic field parameter of the solid tungsten electrode negative pressure arc welding of the present embodiment is as follows: the radius of the solid tungsten electrode is 1.6 mm; the angle of the tungsten electrode tip is 60°; the radius of the shielding gas inlet is 5 mm; the radius of the workpiece is 10 mm; the arc length is 3 mm; the input current is 80 A; the range of the applied longitudinal magnetic induction intensity is 0 to 0.04 T; the shielding gas flow rate is 20 L / min; the shielding gas is 99.99% argon, and the shielding gas flow rate is 15 to 25 L / min;

[0126] like Figure 2 As shown in the solid tungsten electrode geometric model diagram of the present invention, according to the geometric model, the boundary conditions and initial conditions of Table 1 are set in the numerical simulation to establish the mathematical model of the solid tungsten electrode negative pressure arc:

[0127] Table 1: GTAW arc boundary conditions for solid tungsten electrode

[0128]

[0129] When the input current is 80A, the external longitudinal magnetic field with magnetic induction intensities of 0, 0.01, 0.02, 0.03 and 0.04T is applied. The five sets of data are numerically simulated and calculated. According to the calculation results, it can be understood that the arc pressure of the conventional GTAW arc is mainly concentrated on the tungsten pole and the workpiece. The peak pressure appears at the tungsten pole, and a small range of negative pressure appears on both sides of the tungsten pole. When the external magnetic induction intensity increases, the overall pressure of the arc decreases. When the magnetic induction intensity reaches 0.02T, the rotating arc plasma causes a concentrated negative pressure area under the tungsten pole under the action of centrifugal force. When the magnetic induction intensity continues to increase, the concentrated negative pressure area under the tungsten pole continues to expand and the pressure continues to decrease. When the negative pressure area expands to the workpiece, negative pressure appears in the center of the workpiece.

[0130] In addition to the case where the input current is 80A, the above numerical simulation calculations are also repeated for 90A, 100A, 110A, 120A and 130A. According to the calculation results, the fitting results are Figure 4The center pressure diagram of the workpiece with different current sizes of 0-0.04T for solid tungsten arc is shown. It can be seen that when the magnetic induction intensity increases from 0.02T to 0.03T, the center pressure changes from positive pressure to negative pressure. In addition, the rate of change of the center pressure increases with the increase of welding current, resulting in a steeper slope. At a magnetic induction intensity of 0.01T, the center pressure difference between 80A and 120A is 133.6Pa. At a magnetic flux density of 0.02T, the center pressure difference between 80k and 120A is 72.3Pa. When the magnetic flux density is less than 0.03T, the influence of the welding current on the center pressure decreases with the increase of the magnetic flux density. In this range, the magnetic field plays a dominant role in the current-pressure-magnetism relationship. At a magnetic induction intensity of 0.03T, the center pressure difference between 80A and 120A is 10.5Pa. At a magnetic flux density of 0.04T, the center pressure difference between 80k and 120A is 72.3Pa. When the magnetic flux density exceeds 0.03 T, the effect of welding current on the center pressure increases with the increase of magnetic flux density. In this range, the magnetic field and welding current play a leading role in the current-pressure-magnetism relationship.

[0131] The linear fitting of the workpiece center pressure and magnetic induction intensity with welding current ranging from 80 to 120A yields the following results: Figure 5 The magnetic field parameter threshold diagram of the workpiece center pressure transition at different currents in the solid tungsten arc is shown, and its equation is:

[0132] B(I)=0.0225+2.56e-5*exp(I / 29.9) (20)

[0133] Embodiment 2

[0134] The method for determining the threshold value of the magnetic field parameters of the hollow tungsten pole negative pressure arc welding of this embodiment, and the geometric model of the hollow tungsten pole arc. The tungsten pole radius of the hollow tungsten pole center negative pressure arc is 1.6mm, the hollow cavity radius is 0.5mm, and the arc length is 3mm. The welding current is 80A, the magnetic induction intensity is 0~0.05T, the magnetic field direction points to +z, and the exhaust pressure is from 0kPa to -20kPa. The pressures described in the present invention are all relative pressures (-20kPa is the atmospheric pressure minus 20kPa); the shielding gas is 99.99% argon, and the shielding gas flow rate is 20~30L / min;

[0135] like Figure 3 As shown in the figure, the geometric model diagram of the hollow tungsten electrode of the present invention is shown. According to the geometric model, the boundary conditions and initial conditions of Table 2 are set in the numerical simulation to establish the mathematical model of the hollow tungsten electrode negative pressure arc:

[0136] Table 2: GTAW welding arc boundary conditions for hollow tungsten electrode

[0137]

[0138] When the exhaust pressure is 0kPa, it is divided into external longitudinal magnetic fields with magnetic induction intensities of 0, 0.01, 0.02, 0.03, 0.04 and 0.05T. These five sets of data are numerically simulated and calculated. According to the calculation results, it can be understood that the arc pressure field without an external magnetic field is bell-shaped. The arc pressure is mainly concentrated at the tungsten pole and the workpiece. The peak arc pressure occurs at the tungsten pole. As the magnetic induction intensity increases, the rotation speed of the arc plasma near the tungsten pole continues to increase, causing the pressure in the center of the arc to continue to decrease. The peak arc pressure at 0.01T occurs at the workpiece. At 0.02T, a concentrated area of ​​negative pressure appears in the center of the arc. As the magnetic induction intensity continues to increase, the negative pressure area continues to expand and forms negative pressure on the workpiece surface;

[0139] In addition to the case of 0 kPa, the above numerical simulation calculations were repeated for the case of -1 kPa, -5 kPa, -10 kPa, -15 kPa and -20 kPa. According to the calculation results, the fitting results show that Figure 6 From the workpiece center pressure diagram of 0~0.05T at different exhaust pressures during hollow tungsten arc welding shown in the figure, it can be seen that the arc pressure change can be divided into two parts. When the magnetic induction intensity is less than 0.03T, the workpiece center pressure first decreases and then increases under the action of the exhaust pressure. When the magnetic induction intensity is greater than 0.03T, the workpiece center pressure shows an overall downward trend. It can be seen that no matter how the exhaust pressure changes, the workpiece center pressure always decreases with the decrease of the external longitudinal magnetic field intensity. As the exhaust pressure is lower than -5kPa, the magnetic induction intensity required for negative pressure to appear on the workpiece surface increases. When the magnetic induction intensity is 0.05T, the exhaust pressure promotes the reduction of arc pressure;

[0140] The linear fitting of the workpiece center pressure and magnetic induction intensity with the exhaust pressure ranging from 0 to -20 kPa is obtained as follows Figure 7 The magnetic field parameter threshold diagram of the workpiece center pressure transition at different exhaust pressures during hollow tungsten arc is shown in the figure

[0141] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the purpose and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.

Claims

1. A method for determining a threshold value of a magnetic field parameter for negative pressure arc welding, characterized in that: Firstly, a negative pressure arc mathematical model is established, and the negative pressure threshold under different conditions is calculated. Then, the calculated negative pressure threshold data is fitted to obtain an equation for determining the threshold of the magnetic field parameter of negative pressure arc welding. The specific steps include: Step 1: Establish the governing equations: The governing equations consist of the Navier-Stokes equations, the heat transfer equations, and the Maxwell electromagnetic equations: The velocity and pressure distribution of arc plasma are determined according to the mass conservation equation and momentum conservation equation: Among them, ρ is density; v is velocity vector; P is pressure; μ is viscosity; I is the identity matrix; F is the momentum source term; Solve the arc temperature T according to the energy conservation equation: Where k is the thermal conductivity; T is the temperature; Cp is the specific heat capacity; Q is the source term of the energy conservation equation; The electric potential and magnetic vector potential distribution are calculated based on the current continuity equation and Ohm's law: Where V is the electric potential, A is the magnetic vector potential, and σ is the conductivity; According to V and A, we can obtain the current density J, electric field E and magnetic induction intensity B: Among them, J is the current density, E is the electric field, and B is the magnetic induction intensity; The arc energy source term consists of three parts: Joule heat, electron enthalpy transfer and arc radiation loss: Among them, K B is the Boltzmann constant; e is the electron charge; T is the temperature field of the arc shape; Q is the heat source term; Q rad is the arc radiation loss; According to the arc self-induced magnetic field intensity B, current density J and momentum conservation equation, the momentum source term in the momentum conservation equation is solved: F=J×B (10) Step 2: Establish geometric model and mesh division: Establish geometric model of hollow tungsten arc and solid tungsten arc, and then selectively mesh the model; Step 3: Set material parameters: Selectively set material parameters for each area of ​​the geometric model; Step 4: Set initial conditions and boundary conditions: consisting of boundary heat flux, cathode boundary, anode boundary, pressure, current density and potential, and loading volume force J*(B+B0); The boundary conditions are as follows: (1) Solid current density input: (2) Current density of hollow tungsten electrode: (3) Shielding gas flow rate: I is the welding current, Q is the shielding gas flow rate, Rn is the shielding gas inlet radius, Rw is the tungsten electrode radius, Ri is the inner diameter of the hollow cavity, and r is the distance from the shielding gas inlet to the center; (4) The specific formula for cathode is as follows: I e =J r [(|J·n|-J r )>0]+|J·n|[(|J·n|-J r )<0] (15) I i =|J·n|-J e (16) (5) The specific formula for anode is as follows: Among them, |J i |V i is cathode ion heat, It is the electronic heat that plays a cooling role; is the surface work function; V i is the ionization potential of argon; A r is the Richardson constant, is the cathode effective work function, e is the elementary charge, k b is the Boltzmann constant; (6) Add external electromagnetic force by changing the momentum source term: F=J×(B+B0) (19) Wherein, B0 is the magnetic induction intensity of the external longitudinal magnetic field; Step 5: Parametric scanning, set up the solver: According to the above steps, perform calculations and solve, and verify whether the calculation results are consistent with the experimental results under the same conditions. If they are consistent, proceed to the next step; otherwise, return to step 2, adjust the model or boundary conditions, and repeat the cycle of modeling and numerical simulation calculations until the calculation results are consistent with the experimental results under the same conditions, completing the model accuracy verification; Step 6: Fix the model and solution method, perform parameterized batch calculation to obtain the negative pressure welding parameter thresholds under various other conditions, process the negative pressure welding threshold data, and determine the negative pressure welding threshold function: fit multiple groups of negative pressure welding threshold data under different conditions to obtain the function equation of the negative pressure arc welding longitudinal magnetic field parameter threshold.

2. The method for determining a negative pressure arc welding magnetic field parameter threshold according to claim 1, characterized in that: In the step 2, the hollow tungsten arc is subjected to exhaust pressure to study the effect of the exhaust pressure on the physical properties of the hollow tungsten arc.

3. The method for determining a negative pressure arc welding magnetic field parameter threshold according to claim 1, characterized in that: The mesh division in step 2 is tetrahedron or hexahedron.

4. The method for determining a negative pressure arc welding magnetic field parameter threshold according to claim 1, characterized in that: The protective gas in step 4 is 99.99% argon, or helium, or a mixed inert gas, and the external magnetic field is a longitudinal magnetic field mode, a uniform alternating magnetic field mode, an intermittent alternating magnetic field mode, or a pulsed alternating magnetic field mode.

5. The method for determining the threshold value of magnetic field parameters of negative pressure arc welding according to claim 1, characterized in that: For welding current 80-200A, arc length 3mm, 100% pure argon protection, solid tungsten electrode conditions, the functional relationship between welding current and magnetic field strength that forms the negative pressure GTAW welding threshold is: B(I)=0.0225+2.56e-5*exp(I / 29.9).

6. The method for determining a negative pressure arc welding magnetic field parameter threshold according to claim 1, characterized in that: Applicable to negative pressure arc welding technology, or negative pressure arc additive manufacturing technology, or negative pressure arc-laser composite welding technology, or negative pressure arc-laser composite cladding technology, or negative pressure arc-laser composite additive manufacturing technology, or negative pressure arc-high energy beam composite welding technology, or negative pressure arc-high energy beam composite cladding technology, or negative pressure arc-high energy beam composite additive manufacturing technology.