A multidentate ligand, a multidentate ligand metal catalyst, and preparation method and application thereof

By designing a multidentate ligand and its preparation method, the problem of insufficient reaction and stability of the existing alkyne metathesis catalyst at high temperature is solved, the high activity and selectivity of the alkyne metathesis reaction is achieved, and the ligand is simplified Synthesis process.

CN118515534BActive Publication Date: 2024-11-05SOUTH CHINA UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410929747.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-11
Publication Date
2024-11-05
Estimated Expiration
2044-07-11

AI Technical Summary

Technical Problem

The existing alkyne metathesis catalysts react at high temperatures and are insufficient in stability and activity, making them difficult to dissolve well in various solvents, especially sensitive to water and oxygen, and the synthesis steps of multidentate ligands are complicated and have poor controllability.

Method used

A multidentate ligand and its preparation method were designed. The reaction of bromine-substituted tritylmethane derivative with aryl boric acid under the action of palladium catalyst and alkali was prepared to prepare a three-dentate ligand with adaptive properties, which significantly improved the reaction activity. and stability and maintain catalytic activity under low loads.

Benefits of technology

The high activity and selectivity of alkyne metathesis reaction are achieved, the reaction rate is significantly improved, the catalyst has good functional group tolerance and long life, is suitable for a variety of substrates, and the synthesis process of multidentate ligands is simplified.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118515534B_ABST
    Figure CN118515534B_ABST
Patent Text Reader

Abstract

The present invention discloses a multidentate ligand, a multidentate ligand metal catalyst, and a preparation method and application thereof. The present invention improves the ligand structure of the molybdenum carbyne catalyst, designs and synthesizes a tridentate ligand with adaptability, significantly improves the reaction activity, and provides a highly active and selective metal catalyst for alkyne metathesis. The multidentate ligand preparation method of the present invention is simple and efficient; the multidentate ligand metal catalyst has high catalytic activity, can still maintain catalytic activity at low loading, and has a wide range of substrate applications.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of metal-catalyzed organic reactions, and in particular to a multidentate ligand, a multidentate ligand metal catalyst, and a preparation method and application thereof. Background Art

[0002] Transition metal catalyst complexes play an important role in the field of catalysis, and their properties are mainly influenced by the characteristics of the metal and the nature of the ligands coordinated to the metal center. The structural characteristics of the ligands can affect the reaction rate, regioselectivity, and stereoselectivity. For example, in coupling reactions, electron-withdrawing ligands may slow down the oxidative insertion of the metal center into the carbon-halogen bond; conversely, electron-rich ligands can accelerate this process.

[0003] Alkyne metathesis can achieve dynamic exchange of carbon-carbon triple bonds and is an important tool in synthetic chemistry. After a period of development, several metathesis catalysts with clear carbyne structures have been reported. With the enhancement of catalytic activity and stability, as well as good tolerance to polar functional groups, alkyne metathesis catalysts have been increasingly widely used. From small molecule endocyclization and intermolecular oligomerization to polymer chemistry, alkyne metathesis has become an important means of organic synthesis.

[0004] The first catalysts that were effective for alkyne metathesis were composed of a heterogeneous mixture of tungsten oxide and silicon dioxide, discovered by Penella et al., and they worked only at very high temperatures (about 200-450 °C) ( J. Chem. Soc. Chem. Commun. 1968, 1548–1549.). Blanchar et al. found that a mixture of [Mo(CO)6] and resorcinol had catalytic properties when heated to 160°C in an inert solvent. On this basis, different molybdenum sources, substituted phenols and solvents were screened and some improvements were made. However, in most cases, high temperature reactions were still required and the nature of the active substances generated in situ remained elusive ( J. Chem. Soc. Chem. Commun. 1974, 786–787.). Schrock et al. found that some molybdenum, tungsten and rhenium carbyne structures showed significant catalytic activity, and the metal cyclobutadiene derived from them was proved to be an intermediate rather than a transition state ( Acc. Chem. Res. 1986, 19, 342–348.). Fürstner et al. found that the molybdenum complex Mo[N(tBu)(Ar)]3 reacts with dichloromethane in toluene, and the resulting mixture can effectively catalyze the metathesis of different aliphatic and aromatic alkynes. They proved that there is a substance with catalytic ability in the mixture: [(Ar)(tBu)N]3MoCl (as shown in formula (I)) J. Am. Chem. Soc.1999, 121, 9453-9454.). Subsequently, Moore et al. found that Mo[N(tBu)(Ar)]3 and alkyl-substituted dichloride can be used to prepare alkyl-substituted metal carbyne structure (as shown in formula (II)) through disproportionation reaction, and the chloride byproduct can be reduced with magnesium powder to convert it into the starting compound Mo[N(tBu)(Ar)] 3, And cyclically participate in the disproportionation reaction. J. Am. Chem. Soc. 2004, 126 , 1, 329–335.). Zhang et al. found that after ligand exchange of carbyne complexes (preferably with p-nitrophenol), very active catalysts can be obtained. For example, alcoholysis with electron-deficient triphenolamine derivatives and attachment of tridentate ligands to the metal center (as shown in formula (III)) can increase the catalyst life. The structure of multidentate ligands provides stronger complexation than monodentate ligands, and exhibits high catalytic activity while also having a wide range of substrates, and can even tolerate aldehyde and nitro groups. Kinetic studies have shown that the presence of nitro groups reduces the electron density of the metal center and can enhance catalytic activity, but the catalyst has low solubility in most solvents and is very sensitive to water and oxygen ( Angew. Chem. Int. Ed. 2011, 50 , 3435–3438.). Fürstner et al. found that triphenylsilanol ligands coordinated with metal centers (as shown in formula (IV)) can provide higher activity and stability. The good match between the characteristics of the high-valent molybdenum center and the electronic and steric properties of triphenylsilane esters gives the metal center a Lewis acidity balance, which is crucial for high activity, and also has excellent tolerance to polar and sensitive functional groups ( Chem. Eur. J. 2012, 18 ,10281–10299.).

[0005]

[0006] Johnson et al. discovered a highly fluorinated alkoxide ligand (shown as formula (V)) that can be easily and efficiently prepared from a molybdenum-nitrogen triple bond compound by alkyne metathesis ( J. Am. Chem. Soc. 2006, 128 , 9614–9615). Fürstner et al. reported a catalyst with a clear structure and easy separation (as shown in formula (VI)). The design of the tridentate silanol ligand formed a larger cavity between Mo and the ligand, which may reduce the activation energy of the exchange. However, the structure is not easy to control and lacks modifiable reaction sites ( J. Am. Chem. Soc. 2020, 142, 11279-11294.). Zhang et al. used a more rigid ligand (as shown in formula (VII)) to improve the catalyst activity by minimizing the configuration entropy of the complex formed with the Mo center. The ligand was insensitive to water and oxygen, and the stability and activity were increased. However, due to the excessive rigidity, more activation energy was required in the catalytic reaction ( Nat. Commun. 2021, 12 , 1136.). In 2023, Fürstner et al. used pyridine to complex Mo centers, which greatly improved the stability of the catalyst (as shown in formula (VIII)). When dissolved in toluene, the ligands that stabilize pyridine will spontaneously dissociate to release active substances with excellent performance and functional group tolerance. In addition, the catalyst can be weighed and handled routinely in air and can be stored for a long time outside the glove box ( J. Am. Chem. Soc. 2023, 145 , 26993-27009.).

[0007]

[0008] The tridentate ligand catalyst reported by Fürstner, Zhang et al. has been greatly improved in stability, catalytic activity and substrate range, but the synthesis of its ligand is complicated and has poor controllability, so there is still a lot of room for improvement in this area. The present invention improves the ligand structure of the molybdenum carbyne catalyst, quickly and efficiently synthesizes ligands with structural diversity, takes both activity and stability into account, and has good functional group tolerance, which can be widely promoted and applied to alkyne metathesis reactions. Summary of the invention

[0009] In view of the shortcomings of the prior art, one of the objectives of the present invention is to provide a multidentate ligand and a preparation method thereof.

[0010] The second object of the present invention is to provide a multidentate ligand metal catalyst and its preparation method and application.

[0011] Alkyne metathesis catalysts with multidentate ligands usually have ideal stability and substrate application range, but their general activity is significantly reduced compared with monodentate ligand catalysts. The present invention improves the ligand structure of the molybdenum carbyne catalyst, designs and synthesizes a tridentate ligand with adaptability, significantly improves the reaction activity, and its reaction rate is nearly 100 times higher than that of the most advanced multidentate ligands, providing a highly active and selective metal catalyst for alkyne metathesis. It is characterized in that it has higher stability and significantly enhanced catalytic activity compared with the corresponding non-quaternized or non-silane multidentate ligand catalyst analogs. On the other hand, it has good functional group tolerance, fast reaction rate and long life. The invention of this adaptive multidentate ligand not only has significant progress in the field of alkyne metathesis, but also provides an important strategy for the design of multidentate ligands in organometallic chemistry.

[0012] The purpose of the present invention is achieved by at least one of the following technical solutions.

[0013] A multidentate ligand, the general structural formula is as follows:

[0014]

[0015] Wherein, Z is selected from carbon, R 4 is selected from hydrogen, alkoxy; or Z is selected from silicon, R 4 is selected from fluoroalkyl, phenyl; or Z is selected from phosphorus, R 4 Selected from oxygen subunits;

[0016] R 1 , R 2 , R 3 Each is independently selected from hydrogen, halogen, trifluoromethyl, cyano, acetyl, methyl, methoxy, methylthio, isopropyl, phenoxy, 1,1,3,3-tetramethylbutyl, 4-tert-butylphenyl, 4-methoxyphenyl, 4-N,N-dimethylaminophenyl, 4-methoxyformylphenyl, 4-(2,4,6-trimethyl)phenyl, 4-carbazolylphenyl;

[0017] Ar independently represents naphthalene, indane, 1-indanone, dimethylfluorene, or estrone.

[0018] Preferably, the structural formula of the multidentate ligand is L1-L51.

[0019] The preparation method of the above-mentioned multidentate ligand, the multidentate ligands L1, L2, L3, L4, L5, L6, L7, L8, L11, L14, L15, L16, L17, L18, L19, L20, L22, L23, L24, L25, L26, L27, L35, L36, L37, L38, L42, L43, L44, L45, L46, L47, L48, L49, L50, L51 are synthesized by scheme 1; the multidentate ligands L9, L10, L12, L13, L21, L28 are synthesized by scheme 2; the multidentate ligands L29, L30, L31, L32, L33, L34, L39, L40, L41 are synthesized by scheme 3;

[0020] Plan 1 is as follows:

[0021]

[0022] Under protective atmosphere, in the presence of a palladium catalyst and a base, a bromine-substituted triphenylmethane derivative reacts with an arylboronic acid in a mixed solvent of an organic solvent and water to obtain a multidentate ligand;

[0023] The structural formula of the bromine-substituted triphenylmethane derivative is one of the following:

[0024]

[0025] The aryl boronic acid is 2-hydroxyphenylboric acid, (3-chloro-2-hydroxyphenyl)boric acid, (4-chloro-2-hydroxyphenyl)boric acid, (5-chloro-2-hydroxyphenyl)boric acid, (3-fluoro-2-methoxyphenyl)boric acid, (4-fluoro-2-hydroxyphenyl)boric acid, (5-fluoro-2-hydroxyphenyl)boric acid, (4-trifluoromethyl-2-hydroxyphenyl)boric acid, (5-acetyl-2-hydroxyphenyl)boric acid, (4-isopropyl-2-hydroxyphenyl)boric acid, (5-isopropyl-2-methoxyphenyl)boric acid, (5-methoxy-2-hydroxyphenyl)boric acid, (4-methoxy-2-hydroxyphenyl)boric acid, Boric acid, (phenyl)boric acid, (5-methylthio-2-hydroxyphenyl)boric acid, (5-phenoxy-2-hydroxyphenyl)boric acid, (5-isopropyl-4-methyl-2-hydroxyphenyl)boric acid, (5-chloro-4-chloro-2-methoxyphenyl)boric acid, (5-fluoro-4-fluoro-2-methoxyphenyl)boric acid, (3-hydroxynaphthalen-2-yl)boric acid, (6-hydroxy-2,3-dihydro-1H-inden-5-yl)boric acid, (6-hydroxy-1-oxo-2,3-dihydro-1H-inden-5-yl)boric acid, (2-methoxy-9,9-dimethyl-9H-fluoren-3-yl)boric acid;

[0026] Solution 2 is as follows:

[0027]

[0028] Under protective atmosphere, in the presence of palladium catalyst and base, triphenylmethane substituted with boric acid pinacol ester reacts with aryl halide in a mixed solvent of organic solvent and water to obtain a multidentate ligand;

[0029] The structural formula of triphenylmethane substituted with boric acid pinacol ester is:

[0030]

[0031] The aryl halide is one of 4-bromo-3-hydroxybenzonitrile, 3-bromo-4-hydroxybenzonitrile, 2-bromo-4-methylphenol, 2-bromo-5-methylphenol, 2-bromo-4-(2,4,4-trimethylpentan-2-yl)phenol, (8R, 9S, 13S)-3-hydroxy-2-iodo-13-methyl-6,7,8,9,11,12,13,14,15,16-decahydro-17H-cyclopenta[a]phenanthrene-17-one;

[0032] Option three is as follows:

[0033]

[0034] Under protective atmosphere, in the presence of palladium catalyst and base, halogen-substituted tri(biphenyl)methane reacts with arylboronic acid in a mixed solvent of organic solvent and water to obtain a multidentate ligand;

[0035] The structural formula of halogen-substituted tris(biphenyl)methane is:

[0036]

[0037] The aryl boronic acid is one of (4-(tert-butyl)phenyl)boric acid, (4-methoxyphenyl)boric acid, (4-(dimethylamino)phenyl)boric acid, (4-(methoxycarbonyl)phenyl)boric acid, (2',4',6'-trimethyl-[1,1'-biphenyl]-4-yl)boric acid and (4-(9H-carbazol-9-yl)phenyl)boric acid.

[0038] Preferably, in scheme 1,

[0039] The molar ratio of the bromine-substituted triphenylmethane derivative to the aryl boronic acid is 1:5-6;

[0040] The palladium catalyst is selected from at least one of tetrakistriphenylphosphine palladium, methanesulfonyloxy (diadamantyl-n-butylphosphino)-2'-amino-1,1'-biphenyl-2-yl palladium (II);

[0041] The base is selected from at least one of carbonate and phosphate;

[0042] The organic solvent is selected from at least one of tetrahydrofuran and 1,4-dioxane;

[0043] The reaction temperature is 60-100° C., and the reaction time is 12-24 hours. The solution after the reaction is quenched, extracted, concentrated, and purified by column chromatography to obtain a multidentate ligand.

[0044] Preferably, in scheme 2,

[0045] The molar ratio of triphenylmethane substituted with boric acid pinacol ester to aryl halide is 1:5-6;

[0046] The palladium catalyst is selected from at least one of bistriphenylphosphine palladium dichloride, tetrakistriphenylphosphine palladium, and methanesulfonyloxy (diadamantyl-n-butylphosphino)-2'-amino-1,1'-biphenyl-2-yl palladium (II);

[0047] The base is selected from at least one of carbonate and phosphate;

[0048] The solvent is selected from at least one of tetrahydrofuran and 1,4-dioxane;

[0049] The reaction temperature is 60-100° C., and the reaction time is 12-24 hours. The solution after the reaction is quenched, extracted, concentrated, and purified by column chromatography to obtain a multidentate ligand.

[0050] Preferably, in scheme three,

[0051] The molar ratio of the halogen-substituted tri(biphenyl)methane to the arylboronic acid is 1:5-6;

[0052] The palladium catalyst is selected from at least one of tetrakistriphenylphosphine palladium, methanesulfonyloxy (diadamantyl-n-butylphosphino)-2'-amino-1,1'-biphenyl-2-yl palladium (II);

[0053] The base is selected from at least one of carbonate and phosphate;

[0054] The organic solvent is selected from at least one of tetrahydrofuran and 1,4-dioxane;

[0055] The reaction temperature is 60-100° C. and the reaction time is 12-24 hours. The solution after the reaction is quenched, extracted, concentrated, and purified by column chromatography to obtain a multidentate ligand.

[0056] Preferably,

[0057] The preparation method of compound 1 comprises the following steps:

[0058] Under a protective atmosphere, m-dibromobenzene or 1-bromo-3-iodobenzene and n-butyl lithium are reacted in tetrahydrofuran at -78 to -85°C to generate benzene lithium salt, and diethyl carbonate is added. The reaction solution is warmed to room temperature and stirred for 24 to 48 hours. The mixture is quenched, extracted, and purified to obtain compound 1.

[0059] The structural formula of compound 1 is as follows:

[0060]

[0061] The preparation method of compound 2 comprises the following steps:

[0062] Compound 1 is reacted with formic acid at 120-140°C for 24-48 hours, cooled to room temperature, neutralized, extracted, and purified to obtain compound 2;

[0063] The preparation method of compound 3 and compound 4 comprises the following steps:

[0064] Under protective atmosphere, in an ice bath, compound 1 and sodium hydride react in N,N-dimethylformamide, and then a solution of alkyl bromide (n-butyl bromide or n-decyl bromide) in N,N-dimethylformamide is added, and the reaction is continued at 50-60°C, quenched, extracted, and purified to obtain the corresponding compounds 3 and 4, respectively.

[0065] The preparation method of compound 5 comprises the following steps:

[0066] Under protective atmosphere, 1-bromo-3-iodobenzene and n-butyl lithium were reacted in tetrahydrofuran at -78°C to generate benzene lithium salt, and phenyltrichlorosilane was added. The reaction solution was warmed to room temperature and stirred for 24 to 48 hours. The solution was quenched, extracted, and purified to obtain compound 5.

[0067] The preparation method of compound 6 comprises the following steps:

[0068] Under a protective atmosphere, 1-bromo-3-iodobenzene and n-butyl lithium were reacted in tetrahydrofuran at -78°C to generate benzene lithium salt, and then heptadecafluorodecyltrimethoxysilane was added. The reaction solution was warmed to room temperature and stirred for 24 to 48 hours. The solution was quenched, extracted, and purified to obtain compound 6.

[0069] The preparation method of compound 7 comprises the following steps:

[0070] Under protective atmosphere, compound 2 and pinacol diboron were heated and stirred in 1,4-dioxane at 100°C for 24 hours, washed with n-hexane, and recrystallized from methanol to obtain compound 7.

[0071] The preparation method of compound 8 comprises the following steps:

[0072] Under protective atmosphere, compound 2 was stirred with 2-hydroxy-4-chlorophenylboronic acid in a mixed solvent of tetrahydrofuran and water at 80° C. for 24 hours, quenched, extracted and purified to obtain compound 8.

[0073] The preparation method of compound 9 comprises the following steps:

[0074] Under protective atmosphere, compound 3 and 2-hydroxy-4-chlorophenylboronic acid were heated and stirred at 80° C. in a mixed solvent of tetrahydrofuran and water for 24 hours, quenched, extracted, and purified to obtain compound 9.

[0075] The above-mentioned protective atmosphere is nitrogen or inert gas (argon, etc.).

[0076] A multidentate ligand metal catalyst, the structural formula is as follows:

[0077]

[0078] Wherein, Z is selected from carbon, R 4 is selected from hydrogen, alkoxy; or Z is selected from silicon, R 4 is selected from fluoroalkyl, phenyl; or Z is selected from phosphorus, R 4 Selected from oxygen subunits;

[0079] R 1 , R 2 , R 3 Each is independently selected from hydrogen, halogen, trifluoromethyl, cyano, acetyl, methyl, methoxy, methylthio, isopropyl, phenoxy, 1,1,3,3-tetramethylbutyl, 4-tert-butylphenyl, 4-methoxyphenyl, 4-N,N-dimethylaminophenyl, 4-methoxyformylphenyl, 4-(2,4,6-trimethyl)phenyl, 4-carbazolylphenyl;

[0080] Ar independently represents naphthalene, indane, 1-indanone, dimethylfluorene, or estrone.

[0081] The method for preparing the above-mentioned multidentate ligand metal catalyst comprises the following steps:

[0082] The multidentate ligand and the metal ion precursor are mixed in an organic solvent and stirred to obtain a multidentate ligand metal catalyst;

[0083] The metal ion precursor is a carbyne structure with a molybdenum center, and the structural formula is as follows:

[0084]

[0085] Preferably, the molar ratio of the multidentate ligand to the metal ion precursor is 0.5 to 2:1;

[0086] Further preferably, the molar ratio of the multidentate ligand to the metal ion precursor is 1:1;

[0087] Preferably, the concentration of the multidentate ligand in the organic solvent is 0.5-5 mM.

[0088] Preferably, the stirring temperature is 20-70°C and the stirring time is 10-30 minutes;

[0089] Preferably, the organic solvent is CCl4.

[0090] The use of the above-mentioned multidentate ligand metal catalyst in catalyzing the metathesis of alkynes.

[0091] Preferably, the molar ratio of the multidentate ligand metal catalyst to the alkyne is 0.6 to 3:100.

[0092] Preferably, the temperature for catalyzing the metathesis of alkynes is 25-70°C.

[0093] Compared with the prior art, the present invention has the following beneficial effects:

[0094] (1) The preparation method of the present invention is simple and efficient, and realizes the preparation of diversified ligands. As many as 51 tridentate ligands were prepared by the synthesis method of the present invention.

[0095] (2) The catalyst prepared by the ligand of the present invention has high catalytic activity, can still maintain catalytic activity under low loading (dosage), and has a wide range of substrate applicability. BRIEF DESCRIPTION OF THE DRAWINGS

[0096] Figure 1 The structural formulas of the L1, L3, and L29 ligands and the corresponding metal catalysts.

[0097] Figure 2 The catalytic activity curve of the metal catalyst corresponding to the ligand of formula VI, formula VII and L1 in Example 3.

[0098] Figure 3 This is the catalytic activity curve of the metal catalyst corresponding to the L1, L3, and L4 ligands in Example 3.

[0099] Figure 4 This is the catalytic activity curve of the metal catalyst corresponding to the L3 ligand (0.6%) in Example 3. DETAILED DESCRIPTION

[0100] The specific implementation of the present invention is further described below in conjunction with the accompanying drawings and examples, but the implementation and protection of the present invention are not limited thereto. It should be noted that if there are processes that are not particularly described in detail below, they can be implemented or understood by those skilled in the art with reference to the prior art. If the manufacturer of the reagents or instruments used is not indicated, they are deemed to be conventional products that can be purchased commercially.

[0101] The ligand structural formula prepared in the embodiment of the present invention is as follows:

[0102]

[0103] (In L33, the Mes group is 4-(2,4,6-trimethyl)phenyl; in L18, the MeS group is methylthio)

[0104] Example 1

[0105] Synthesis of compound 1

[0106]

[0107] Under argon atmosphere, 1-bromo-3-iodobenzene (14.00 g, 49.49 mmol) and 80 mL of dry tetrahydrofuran were added to a 200 mL dry Schlenk flask. After the solution was cooled to -78 °C, n-butyl lithium (31.24 mL, 49.98 mmol, 1.6 M in hexane) was slowly added dropwise. The reaction mixture was stirred at -78 °C for 1 hour. Diethyl carbonate (1.93 g, 16.30 mmol) was slowly added to the reaction solution. After stirring for 1 hour, the mixture was warmed to room temperature and stirred for 12 hours. The reaction mixture was quenched with saturated ammonium chloride solution (100 mL) and extracted with ethyl acetate (3×75 mL). The organic layers were combined and dried over anhydrous magnesium sulfate, filtered, and concentrated in vacuo. Purification by column chromatography (petroleum ether / dichloromethane = 10:3) gave a colorless solid (6.98 g) with a yield of 86%.

[0108] 1 H NMR (400 MHz, CDCl3) δ 7.50 – 7.42 (m, 6H), 7.21 (t, J =7.8 Hz, 3H), 7.16 – 7.11 (m, 3H), 2.75 (s, 1H). 13 C NMR (101 MHz, CDCl3) δ 147.8, 131.0,130.6, 129.8, 126.5, 122.7, 80.9. HRMS (APCI) calculated for [MH] + :494.8423; found: 494.8423.

[0109] Synthesis of compound 2

[0110]

[0111] Compound 1 (5.63 g, 11.30 mmol) and formic acid (56 mL) were added to a 200 mL dry round-bottom flask and stirred at 120 °C for 24 hours before returning to room temperature. The reaction mixture was neutralized with aqueous sodium bicarbonate solution, extracted with ethyl acetate (3 × 75 mL), and the organic phase was dried over anhydrous magnesium sulfate, filtered, and concentrated in vacuo. Purification by column chromatography (n-hexane) gave a colorless oily liquid (4.91 g) with a yield of 90%.

[0112] 1 H NMR (400 MHz, CDCl3) δ 7.39 (d, J = 7.9 Hz, 3H), 7.20 (dd, J = 14.7,6.8 Hz, 6H), 7.00 (d, J = 7.8 Hz, 3H), 5.42 (s, 1H). 13 C NMR (126 MHz, CDCl3) δ144.7, 132.3, 130.3, 130.2, 128.0, 122.9, 55.8. HRMS (ESI) calculated for [M+H] + : 478.8474; found: 478.8469.

[0113] Synthesis of compound 3

[0114]

[0115] Under argon atmosphere, sodium hydride (211.0 mg, 5.28 mmol, 60% dispersion in mineral oil) and N,N-dimethylformamide (5 mL) were added to a 200 mL dry Schlenk flask, and the solution was cooled to 0°C. The diluted solution of compound 1 (N,N-dimethylformamide) was slowly added dropwise to the Schlenk flask, returned to room temperature and continued to stir for 10 minutes. The reaction mixture was cooled to 0°C, and the diluted n-butyl bromide solution (N,N-dimethylformamide) was slowly added dropwise to the Schlenk flask, returned to room temperature and continued to stir for 3 hours. The mixture was quenched with saturated ammonium chloride solution (100 mL), extracted with ethyl acetate (3×75 mL), and the organic layer was dried over anhydrous magnesium sulfate, filtered, and concentrated in vacuo. Purification by column chromatography (petroleum ether) gave a colorless oily liquid (700.0 mg) with a yield of 72%.

[0116] 1 H NMR (500 MHz, CDCl3) δ 7.65 – 7.56 (m, 3H), 7.41 (d, J = 7.8 Hz, 3H),7.30 (t, J = 9.3 Hz, 3H), 7.19 (t, J = 7.9 Hz, 3H), 3.04 (q, J = 6.6 Hz, 2H), 1.67– 1.58 (m, 2H), 1.43 (h, J = 7.0 Hz, 2H), 0.91 (q, J = 6.1, 5.5 Hz, 3H). 13 C NMR(126 MHz, CDCl3) δ 145.79, 131.36, 130.70, 129.74, 127.42, 122.51, 85.28,63.86, 32.09, 19.59, 14.12. HRMS (ESI) calculated for [M+H] + : 623.3887,found: 623.3886.

[0117] Synthesis of compound 4

[0118]

[0119] According to the preparation procedure of compound 3, compound 1 was reacted with n-decyl bromide and purified to obtain a colorless oily liquid (0.30 g) with a yield of 67%.

[0120] 1 H NMR (500 MHz, CDCl3, ppm) δ 7.57 (t, 3H), 7.40 (d, J = 9.0 Hz, 3H),7.28 (d, J = 8.3 Hz, 3H), 7.18 (d, J = 7.9 Hz, 3H), 3.01 (t, J = 6.5 Hz, 2H), 1.60(q, J = 6.5, 5.0 Hz, 2H), 1.41 (h, J = 8.1 Hz, 2H), 0.92 – 0.87 (m, 3H); 13 C NMR (126 MHz, CDCl3, ppm) δ 145.8, 131.3, 130.7, 129.7, 127.4, 122.4, 85.2, 63.8, 32.0, 19.5, 14.1.

[0121] Synthesis of compound 5

[0122]

[0123] Under argon atmosphere, add 1-bromo-3-iodobenzene (1.50 g, 5.30 mmol) and dry tetrahydrofuran (60 mL) to a 200 mL dry Schlenk flask. Cool the solution to -78 °C, slowly add n-butyl lithium (3.35 mL, 5.36 mmol, 1.6 M) dropwise, and stir for 1 hour. Slowly add trimethoxyphenylsilane to the reaction solution, continue stirring at -78 °C for 1 hour, warm to room temperature, and stir overnight. The reaction mixture was quenched with saturated ammonium chloride solution (100 mL), extracted with ether (3×75 mL), and the organic phase was dried over anhydrous magnesium sulfate, filtered, and concentrated in vacuo. Purification by column chromatography (petroleum ether) gave a white solid (630.0 mg) with a yield of 63%.

[0124] 1 H NMR (500 MHz, CDCl3) δ 7.64 – 7.59 (m, 6H), 7.53 – 7.48 (m, 3H), 7.47 – 7.41 (m, 5H), 7.29 (t, J = 7.6 Hz, 3H). 13C NMR (126 MHz, CDCl3) δ 138.6,136.3, 136.1, 134.8, 133.4, 131.8, 130.5, 130.0, 128.5, 123.3.

[0125] Synthesis of compound 6

[0126]

[0127] Under argon atmosphere, add 1-bromo-3-iodobenzene (1.50 g, 5.30 mmol) and dry tetrahydrofuran (60 mL) to a 200 mL dry Schlenk flask. Cool the solution to -78 °C, slowly add n-butyl lithium (3.35 mL, 5.36 mmol, 1.6 M) dropwise, and stir for 1 hour. Slowly add heptafluorodecyltrimethoxysilane to the reaction solution, continue stirring at -78 °C for 1 hour, warm to room temperature, and stir overnight. The reaction mixture was quenched with saturated ammonium chloride solution (100 mL), extracted with ether (3×75 mL), and the organic phase was dried over anhydrous magnesium sulfate, filtered, and concentrated in vacuo. Purification by column chromatography (petroleum ether) gave a white solid (442.0 mg) with a yield of 27%.

[0128] Synthesis of compound 7

[0129]

[0130] In a glove box, compound 2 (0.21 g, 0.45 mmol), pinacol diboronate (0.45 g, 1.78 mmol), bistriphenylphosphine palladium dichloride (31.3 mg, 0.04 mmol), potassium acetate (174.9 mg, 1.78 mmol) and 1,4-dioxane (20 mL) were added to a dry Schlenk flask, sealed and transferred out of the glove box. The reaction mixture was stirred at 100 °C for 24 hours, quenched with H2O (20 mL), and extracted with ethyl acetate (3×30 mL). The organic phase was dried over anhydrous sodium sulfate, filtered, and concentrated in vacuo. The crude product was washed with n-hexane and recrystallized in methanol to obtain a white solid (0.16 g) with a yield of 58%.

[0131] 1 H NMR (500 MHz, CDCl3) δ 7.65 – 7.60 (m, 6H), 7.25 – 7.22 (m, 3H), 7.11 (dt, J = 7.8, 1.7 Hz, 3H), 5.59 (s, 1H), 1.29 (s, 37H).13 C NMR (126 MHz, CDCl3) δ 143.1, 136.0, 132.8, 132.3, 127.8, 83.8, 57.0, 25.0. HRMS (ESI)calculated for [M+H] + : 623.3887; found: 623.3886.

[0132] Synthesis of compound 8

[0133]

[0134] In a glove box, compound 2 (1.05 g, 2.18 mmol), (4-chloro-2-hydroxyphenyl)boronic acid (1.88 g, 10.91 mmol), tetrakistriphenylphosphine palladium (0.25 g, 0.22 mmol), potassium carbonate (1.81 g, 13.10 mmol) and dry tetrahydrofuran (60 mL) were added to a dry Schlenk flask, which was sealed and transferred out of the glove box. Bubbling deoxygenated water was added under argon conditions, and the reaction mixture was stirred at 80 ° C for 24 hours and then cooled to room temperature. The organic layer was extracted with ethyl acetate (3×30 mL) and washed with water. Dry over anhydrous magnesium sulfate, filter, and concentrate in vacuo. Purification by column chromatography (petroleum ether: ethyl acetate = 3:1) gave a white solid (0.98 g) with a yield of 72%.

[0135] 1 H NMR (400 MHz, CDCl3) δ 7.44 (t, J = 7.7 Hz, 3H), 7.31 (dt, J = 7.7, 1.4Hz, 3H), 7.24 (s, 3H), 7.20 (d, J = 7.8 Hz, 3H), 7.12 (d, J = 8.5 Hz, 3H), 6.95(d, J = 7.5 Hz, 6H), 5.68 (s, 1H), 5.23 (s, 3H). 13 C NMR (101 MHz, CDCl3) δ152.9, 144.5, 136.5, 134.3, 131.1, 130.0, 129.7, 129.1, 127.3, 126.5, 121.2,116.3, 56.8. HRMS (ESI) calculated for [M+Na] +: 645.0762; found: 645.0755.

[0136] Synthesis of compound 9

[0137]

[0138] According to the preparation procedure of compound 8, compound 3 was reacted with (4-chloro-2-hydroxyphenyl)boronic acid by Suzuki coupling to synthesize compound 9, which was purified to obtain a colorless oily liquid with a yield of 62%.

[0139] 1 H NMR (500 MHz, CDCl3) δ 7.59 – 7.53 (m), 7.44 (t, J = 7.7 Hz), 7.32(dt, J = 7.5, 1.3 Hz), 7.12 (d, J = 8.0 Hz), 6.95 (dd, J = 9.9, 1.9 Hz), 5.28, 3.14(t, J = 6.5 Hz), 1.65 – 1.60 (m), 1.40 (dt, J = 14.9, 7.4 Hz), 0.86 (t, J = 7.4Hz). 13 C NMR (126 MHz, CDCl3) δ 153.1, 145.4, 136.3, 135.9, 134.4, 134.4,131.2, 131.1, 129.3, 129.2, 128.5, 128.3, 127.9 127.5, 126.7, 126.6, 121.4,121.3, 116.5, 116.4, 86.3, 63.9, 32.1, 31.7, 22.8, 19.6, 14.1. HRMS (ESI)calculated for [MH] - : 693.1372; found: 693.1384.

[0140] Example 2

[0141] Synthesis of ligand L1

[0142]

[0143] According to the general preparation procedure of Scheme 1: In a glove box, compound 2 (0.30 g, 0.63 mmol), 2-hydroxyphenylboronic acid (0.52 g, 3.75 mmol), tetrakistriphenylphosphine palladium (72.1 mg, 0.06 mmol), potassium carbonate (0.52 g, 3.75 mmol) and dry tetrahydrofuran (15 mL) were added to a dry Schlenk flask, sealed and transferred out of the glove box. Bubbling deoxygenated water (5 mL) was added under argon conditions, and the reaction mixture was stirred at 80 ° C for 24 hours and quenched with water (10 mL), and extracted with ethyl acetate (3×30 mL). The organic phase was dried over anhydrous magnesium sulfate, filtered, and concentrated in vacuo. Purification by column chromatography (dichloromethane: petroleum ether = 6:1) gave a white solid (0.25 g) with a yield of 76%.

[0144] 1 H NMR (400 MHz, CDCl3) δ 7.43 (t, J = 7.6 Hz, 3H), 7.38 – 7.31 (m, 6H), 7.26 – 7.19 (m, 9H), 7.00 – 6.92 (m, 6H), 5.70 (s, 1H), 5.16 (s, 3H). 13 C NMR(101 MHz, CDCl3) δ 152.4, 144.5, 137.4, 130.3, 130.2, 129.4, 129.2, 128.8,128.0, 127.4, 120.9, 116.0, 56.9. HRMS (ESI) calculated for [M+Na] + :543.1936; found: 543.1949.

[0145] Synthesis of ligand L2

[0146]

[0147] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was synthesized by Suzuki coupling with (3-chloro-2-hydroxyphenyl)boronic acid to obtain L2, which was purified to obtain a white solid with a yield of 61%.

[0148] 1 H NMR (400 MHz, CDCl3) δ 7.46 – 7.36 (m, 9H), 7.29 (dd, J = 8.0, 1.6Hz, 3H), 7.25 – 7.15 (m, 6H), 6.90 (t,J = 7.9 Hz, 3H), 5.69 (s, 1H), 5.68 (s, 2H). 13 C NMR (101 MHz, CDCl3) δ 148.4, 143.9, 137.1, 130.4, 129.7, 129.4,128.8, 128.6, 128.3, 127.3, 121.0, 120.7, 57.0. HRMS (ESI) calculated for [MH] - : 621.0796; found: 621.0796.

[0149] Synthesis of ligand L3

[0150]

[0151] According to the preparation procedure of Scheme 1 (same as the preparation procedure of compound 8), compound 2 was synthesized by Suzuki coupling with (4-chloro-2-hydroxyphenyl)boronic acid to obtain L3, which was purified to obtain a white solid with a yield of 72%.

[0152] 1 H NMR (400 MHz, CDCl3) δ 7.44 (t, J = 7.7 Hz, 3H), 7.31 (dt, J = 7.7, 1.4Hz, 3H), 7.24 (s, 3H), 7.20 (d, J = 7.8 Hz, 3H), 7.12 (d, J = 8.5 Hz, 3H), 6.95(d, J = 7.5 Hz, 6H), 5.68 (s, 1H), 5.23 (s, 3H). 13 C NMR (101 MHz, CDCl3) δ152.9, 144.5, 136.5, 134.3, 131.1, 130.0, 129.7, 129.1, 127.3, 126.5, 121.2,116.3, 56.8. HRMS (ESI) calculated for [M+Na] + : 645.0762; found: 645.0755.

[0153] Synthesis of ligand L4

[0154]

[0155] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was Suzuki coupled with (5-chloro-2-hydroxyphenyl)boronic acid to synthesize L4, which was purified to obtain a white solid with a yield of 51%.

[0156] 1 H NMR (400 MHz, CDCl3) δ 7.45 (t, J = 7.7 Hz, 3H), 7.33 (dt, J = 7.6, 1.2Hz, 3H), 7.29 (d, J = 1.6 Hz, 3H), 7.24 – 7.14 (m, 9H), 6.87 (d, J = 8.5 Hz, 3H), 5.69 (s, 1H), 5.14 (s, 3H). 13 C NMR (101 MHz, CDCl3) δ 151.0, 144.4, 136.3,130.0, 129.8, 129.7, 129.3, 129.2, 128.9, 127.3, 125.6, 117.3, 56.8. HRMS(ESI) calculated for [MH] - : 621.0796; found: 621.0798.

[0157] Synthesis of ligand L5

[0158]

[0159] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was Suzuki coupled with (3-fluoro-2-methoxyphenyl)boronic acid to synthesize the precursor compound of L5 (methoxy protection), which was purified to obtain a white solid with a yield of 86%.

[0160] Subsequently, the precursor compound of L5 (methoxy protection) (42.0 mg, 68.11 μmol) and dichloromethane (10 mL) were added to a dry Schlenk flask under an argon atmosphere, and the solution was cooled to 0°C. The boron tribromide solution was slowly added dropwise to the Schlenk flask, and the reaction mixture was stirred after warming to room temperature. After the conversion of the raw material was completely monitored by thin layer chromatography, water (10 mL) was added to quench, and dichloromethane was extracted (3×30 mL). The organic phase was dried over anhydrous magnesium sulfate, filtered, and concentrated in vacuo. Column chromatography (dichloromethane: petroleum ether = 6:1) was purified to obtain a white solid (17.0 mg) with a yield of 43%.

[0161] 1 H NMR (500 MHz, CDCl3) δ 7.42 – 7.35 (m, 9H), 7.19 (dt, J = 7.0, 1.7Hz, 3H), 7.03 (dd, J = 8.1, 3.9 Hz, 6H), 6.85 (td, J = 8.0, 5.3 Hz, 3H), 5.68(s,1H), 5.29 (d, J = 4.5 Hz, 3H). 13 C NMR (126 MHz, CDCl3) δ 152.4, 150.5, 144.1,141.0, 140.9, 136.7, 136.7, 130.4, 130.4, 130.4, 128.9, 128.8, 127.3, 125.8,125.7, 120.3, 120.3, 114.8, 114.6, 57.0. HRMS (ESI) calculated for [M+Na] + :597.1648; found: 597.1641.

[0162] Synthesis of ligand L6

[0163]

[0164] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was Suzuki coupled with (4-fluoro-2-hydroxyphenyl)boronic acid to synthesize L6, which was purified to obtain a white solid with a yield of 95%. HRMS (ESI) calculated for [MH] - :573.1683; found: 573.1686.

[0165] Synthesis of ligand L7

[0166]

[0167] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was coupled with (5-fluoro-2-hydroxyphenyl)boronic acid to synthesize L7, which was purified to obtain a white solid with a yield of 42%. HRMS (ESI) calculated for [M+Na] + :597.1648; found: 597.1646.

[0168] Synthesis of ligand L8

[0169]

[0170] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was synthesized by Suzuki coupling with (4-trifluoromethyl-2-hydroxyphenyl)boronic acid to obtain L8, which was purified to obtain a white solid with a yield of 43%. HRMS (ESI) calculated for [M+Na] + : 747.1558; found: 747.1560.

[0171] Synthesis of ligand L9

[0172]

[0173] According to the general preparation procedure of Scheme 2: In a glove box, compound 7 (50.0 mg, 0.08 mmol), 4-bromo-3-hydroxybenzonitrile (95.5 mg, 0.48 mmol), mesylate (diadamantyl-n-butylphosphine)-2'-amino-1,1'-biphenyl-2-yl) palladium (II) (5.9 mg, 8.0 μmol), potassium phosphate (102.3 mg, 0.48 mmol) and dry tetrahydrofuran (7 mL) were added to a dry Schlenk flask, sealed and transferred out of the glove box. Bubbling deoxygenated water (3 mL) was added under argon conditions. The reaction mixture was stirred at 80 ° C for 24 hours and quenched with water (10 mL), and extracted with ethyl acetate (3×20 mL). The organic layer was dried over anhydrous magnesium sulfate, filtered, and concentrated in vacuo. Purification by thin layer chromatography (methanol: dichloromethane = 6:100) gave a white solid (30.5 mg) with a yield of 64%. HRMS (ESI) calculated for [M+Na] + : 618.1789;found: 618.1779.

[0174] Synthesis of ligand L10 precursor

[0175]

[0176] According to the preparation procedure of Scheme 2 (refer to the preparation procedure of L9), compound 7 was synthesized by Suzuki coupling with 3-bromo-4-hydroxybenzonitrile to synthesize L10, which was purified to obtain a white solid with a yield of 65%. HRMS (ESI) calculated for [M+Na] + :618.1789; found: 618.1779.

[0177] Synthesis of ligand L11

[0178]

[0179] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was coupled with (5-acetyl-2-hydroxyphenyl)boronic acid to synthesize L11, which was purified to obtain a white solid with a yield of 51%. HRMS (ESI) calculated for [M+Na] + : 669.2248; found: 669.2261.

[0180] Synthesis of ligand L12

[0181]

[0182] According to the preparation procedure of Scheme 2 (refer to the preparation procedure of L9), compound 7 was synthesized by Suzuki coupling with 2-bromo-4-methylphenol to obtain L12, which was purified to obtain a white solid with a yield of 62%. HRMS (ESI) calculated for [M+Na] + :585.2401; found: 585.2390.

[0183] Synthesis of ligand L13

[0184]

[0185] According to the preparation procedure of Scheme 2 (refer to the preparation procedure of L9), compound 7 was synthesized by Suzuki coupling with 2-bromo-5-methylphenol to obtain L13, which was purified to obtain a white solid with a yield of 61%. HRMS (ESI) calculated for [M+H] + :561.2435, found: 561.2435.

[0186] Synthesis of ligand L14

[0187]

[0188] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was synthesized by Suzuki coupling with (4-isopropyl-2-hydroxyphenyl)boronic acid to obtain L14, which was purified to obtain a white solid with a yield of 58%. HRMS (ESI) calculated for [M+Na] + : 669.3345, found: 669.3346.

[0189] Synthesis of ligand L15

[0190]

[0191] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was Suzuki coupled with (5-isopropyl-2-methoxyphenyl)boronic acid to synthesize the precursor compound of L15 (methoxy protection), followed by deprotection with boron tribromide to synthesize L15, which was purified to obtain a white solid with a yield of 61%. HRMS (ESI) calculated for [M+Na] + : 669.3340,found: 669.3328.

[0192] Synthesis of ligand L16

[0193]

[0194] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was synthesized by Suzuki coupling with (5-methoxy-2-hydroxyphenyl)boronic acid to obtain L16, which was purified to obtain a white solid with a yield of 41%. HRMS (ESI) calculated for [M+Na] + : 633.2248; found: 633.2256.

[0195] Synthesis of ligand L17

[0196]

[0197] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was coupled with (4-methoxy-2-hydroxyphenyl)boronic acid to synthesize L17, which was purified to obtain a white solid with a yield of 67%. HRMS (ESI) calculated for [M+Na] + : 633.2248; found: 633.2250.

[0198] Synthesis of ligand L18

[0199]

[0200] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was synthesized by Suzuki coupling with (5-methylthio-2-hydroxyphenyl)boronic acid to obtain L18, which was purified to obtain a white solid with a yield of 63%. HRMS (ESI) calculated for [M+Na] + : 681.1562; found: 681.1563.

[0201] Synthesis of ligand L19

[0202]

[0203] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was coupled with (5-phenoxy-2-hydroxyphenyl)boronic acid to synthesize L19, which was purified to obtain a white solid with a yield of 79%. HRMS (ESI) calculated for [M+Na] + : 819.2717; found: 819.2719.

[0204] Synthesis of ligand L20

[0205]

[0206] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was synthesized by Suzuki coupling with (5-isopropyl-4-methyl-2-hydroxyphenyl)boronic acid to obtain L20, which was purified to obtain a white solid with a yield of 79%. HRMS (ESI) calculated for [M+Na] + : 711.3809; found: 711.3820.

[0207] Synthesis of ligand L21

[0208]

[0209] According to the preparation procedure of Scheme 2 (refer to the preparation procedure of L9), compound 7 was synthesized by Suzuki coupling with 2-bromo-4-(2,4,4-trimethylpentan-2-yl)phenol to obtain L21, which was purified to obtain a white solid with a yield of 64%. HRMS (ESI) calculated for [M+Na] + : 837.5223; found: 837.1957.

[0210] Synthesis of ligand L22

[0211]

[0212] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was coupled with (5-chloro-4-chloro-2-methoxyphenyl)boronic acid by Suzuki coupling to synthesize the precursor compound of L22 (methoxy protection), followed by deprotection with boron tribromide to synthesize L22, which was purified to obtain a white solid with a yield of 49%. HRMS (ESI) calculated for ESI: [MH] - :724.9597;found:724.9606.

[0213] Synthesis of ligand L23

[0214]

[0215] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was coupled with (5-fluoro-4-fluoro-2-methoxyphenyl)boronic acid by Suzuki coupling to synthesize the precursor compound of L23 (methoxy protection), followed by deprotection with boron tribromide to synthesize L23, which was purified to obtain a white solid with a yield of 52%. HRMS (ESI) calculated for [MH] - : 627.1400;found: 627.1400.

[0216] Synthesis of ligand L24

[0217]

[0218] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was synthesized by Suzuki coupling with (3-hydroxynaphthalen-2-yl)boronic acid to obtain L24, which was purified to obtain a white solid with a yield of 64%. HRMS (ESI) calculated for [MH] - :693.2406; found: 693.2421.

[0219] Synthesis of ligand L25

[0220]

[0221] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was synthesized by Suzuki coupling with (6-hydroxy-2,3-dihydro-1H-inden-5-yl)boronic acid to obtain L25, which was purified to obtain a white solid with a yield of 90%. HRMS (ESI) calculated for [M+Na] + : 663.2870; found: 663.2880.

[0222] Synthesis of ligand L26

[0223]

[0224] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was synthesized by Suzuki coupling with (6-hydroxy-1-oxo-2,3-dihydro-1H-inden-5-yl)boronic acid to obtain L26, which was purified to obtain a white solid with a yield of 90%. HRMS (ESI) calculated for [M+Na] + : 705.2248; found: 705.2264.

[0225] Synthesis of ligand L27

[0226]

[0227] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 2 was coupled with (2-methoxy-9,9-dimethyl-9H-fluoren-3-yl)boronic acid by Suzuki coupling to synthesize the precursor compound of L27 (methoxy protection), followed by deprotection with boron tribromide to synthesize L27, which was purified to obtain a white solid with a yield of 74%. HRMS (ESI) calculated for [M+H] + :891.3814; found: 891.3794.

[0228] Synthesis of ligand L28

[0229]

[0230] According to the preparation procedure of Scheme 2 (refer to the preparation procedure of L9), compound 7 was Suzuki coupled with (8R, 9S, 13S)-3-hydroxy-2-iodo-13-methyl-6,7,8,9,11,12,13,14,15,16-decahydro-17H-cyclopenta[a]phenanthrene-17-one to synthesize L28, which was purified to obtain a white solid with a yield of 67%. HRMS (ESI) calculated for [M+Na] + : 1071.5540;found: 1071.5543.

[0231] Synthesis of ligand L29

[0232]

[0233] According to the general preparation procedure of Scheme 3: In a glove box, compound 8 (28.0 mg, 0.04 mmol), (4-(tert-butyl)phenyl)boronic acid (71.9 mg, 0.40 mmol), mesylate (diadamantyl-n-butylphosphine)-2'-amino-1,1'-biphenyl-2-yl)palladium (II) (6.54 mg, 8.98 μmol), potassium phosphate (128.6 mg, 0.61 mmol) and dry 1,4-dioxane (1.8 mL) were added to a dry Schlenk flask, sealed and transferred out of the glove box. Bubbling deoxygenated water was added under argon, the reaction mixture was stirred at 80 °C for 24 hours and then cooled to room temperature, extracted with ethyl acetate (3×30 mL), and the organic layer was washed with water. Dry over anhydrous magnesium sulfate, filter, and concentrate in vacuo. Purification by column chromatography (petroleum ether: ethyl acetate = 3:1) gave a white solid (25.1 mg) with a yield of 60%. HRMS (ESI) calculated for [M+Na] + :939.4748; found: 939.4741.

[0234] Synthesis of ligand L30

[0235]

[0236] According to the preparation procedure of Scheme 3 (refer to the preparation procedure of L29), compound 8 was synthesized by Suzuki coupling with (4-methoxyphenyl)boronic acid to obtain L30, which was purified to obtain a white solid with a yield of 65%. HRMS (ESI) calculated for [M+Na] + :861.3192; found: 861.3194.

[0237] Synthesis of ligand L31

[0238]

[0239] According to the preparation procedure of Scheme 3 (refer to the preparation procedure of L29), compound 8 was synthesized by Suzuki coupling with (4-(dimethylamino)phenyl)boronic acid to obtain L31, which was purified to obtain a white solid with a yield of 52%. HRMS (ESI) calculated for [M+H] + : 878.4322; found: 878.4314.

[0240] Synthesis of ligand L32

[0241]

[0242] According to the preparation procedure of Scheme 3 (refer to the preparation procedure of L29), compound 8 was synthesized by Suzuki coupling with (4-(methoxycarbonyl)phenyl)boronic acid to obtain L32, which was purified to obtain a white solid with a yield of 95%. HRMS (ESI) calculated for [M+Na] + : 945.3040; found: 945.3035.

[0243] Synthesis of ligand L33

[0244]

[0245] According to the preparation procedure of Scheme 3 (refer to the preparation procedure of L29), compound 8 was synthesized by Suzuki coupling with (2',4',6'-trimethyl-[1,1'-biphenyl]-4-yl)boronic acid to obtain L33, which was purified to obtain a white solid with a yield of 57%. HRMS (ESI) calculated for [M+Na] + : 897.4279;

[0246] found: 897.4273.

[0247] Synthesis of ligand L34

[0248]

[0249] According to the preparation procedure of Scheme 3 (refer to the preparation procedure of L29), compound 8 was synthesized by Suzuki coupling with (4-(9H-carbazol-9-yl)phenyl)boronic acid to obtain L34, which was purified to obtain a white solid with a yield of 35%. HRMS (ESI) calculated for [M+Na] + : 1266.4611; found: 1266.4629.

[0250] Synthesis of ligand L35

[0251]

[0252] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 3 was synthesized by Suzuki coupling with 2-hydroxyphenylboronic acid to obtain L35, which was purified to obtain a white solid with a yield of 77%. HRMS (ESI) calculated for [MH] - :591.2540; found: 591.2540.

[0253] Synthesis of ligand L36

[0254]

[0255] According to the preparation procedure of Scheme 1 (same as the preparation procedure of compound 9), compound 3 was synthesized by Suzuki coupling with (4-chloro-2-hydroxyphenyl)boronic acid to obtain L36, which was purified to obtain a white solid with a yield of 62%. HRMS (ESI) calculated for [MH] - : 693.1372; found: 693.1384.

[0256] Synthesis of ligand L37

[0257]

[0258] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 3 was synthesized by Suzuki coupling with (5-chloro-2-hydroxyphenyl)boronic acid to obtain L37, which was purified to obtain a white solid with a yield of 74%. HRMS (ESI) calculated for [MH] - : 693.1372; found: 693.1379.

[0259] Synthesis of ligand L38

[0260]

[0261] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 3 was synthesized by Suzuki coupling with (4-trifluoromethyl-2-hydroxyphenyl)boronic acid to obtain L38, which was purified to give a white solid with a yield of 54%. HRMS (ESI) calculated for [MH] - : 795.2162; found: 795.2170.

[0262] Synthesis of ligand L39

[0263]

[0264] According to the preparation procedure of Scheme 3 (refer to the preparation procedure of L29), compound 9 was synthesized by Suzuki coupling with (4-(tert-butyl)phenyl)boronic acid to obtain L39, which was purified to obtain a white solid with a yield of 78%. HRMS (ESI) calculated for [M+Na] + :1011.5328; found: 1011.5338.

[0265] Synthesis of ligand L40

[0266]

[0267] According to the preparation procedure of Scheme 3 (refer to the preparation procedure of L29), compound 9 was synthesized by Suzuki coupling with (4-methoxyphenyl)boronic acid to obtain L40, which was purified to obtain a white solid with a yield of 79%. HRMS (ESI) calculated for [M+Na] + :933.3767; found: 933.3769.

[0268] Synthesis of ligand L41

[0269]

[0270] According to the preparation procedure of Scheme 3 (refer to the preparation procedure of L29), compound 9 was synthesized by Suzuki coupling with (4-(dimethylamino)phenyl)boronic acid to obtain L41, which was purified to obtain a white solid with a yield of 76%. HRMS (ESI) calculated for [M+H] + : 950.4897; found: 950.4894.

[0271] Synthesis of ligand L42

[0272]

[0273] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 4 was synthesized by Suzuki coupling with (4-chloro-2-hydroxyphenyl)boronic acid to obtain L42, which was purified to obtain a white solid with a yield of 62%. HRMS (ESI) calculated for [M+Na] + :801.2276; found: 801.2284.

[0274] Synthesis of ligand L43

[0275]

[0276] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 5 was synthesized by Suzuki coupling with 2-hydroxyphenylboronic acid to obtain L43, which was purified to obtain a white solid with a yield of 94%. HRMS (ESI) calculated for [MH] - :611.2047; found:611.2048.

[0277] Synthesis of ligand L44

[0278]

[0279] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 5 was synthesized by Suzuki coupling with (3-chloro-2-hydroxyphenyl)boronic acid to obtain L44, which was purified to obtain a white solid with a yield of 79%. HRMS (ESI) calculated for [M+Na] + :737.0844; found:737.0839.

[0280] Synthesis of ligand L45

[0281]

[0282] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 5 was synthesized by Suzuki coupling with (4-chloro-2-hydroxyphenyl)boronic acid to obtain L45, which was purified to obtain a white solid with a yield of 90%. HRMS (ESI) calculated for [MH] - : 713.0878; found: 713.0878.

[0283] Synthesis of ligand L46

[0284]

[0285] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 5 was synthesized by Suzuki coupling with (5-chloro-2-hydroxyphenyl)boronic acid to obtain L46, which was purified to obtain a white solid with a yield of 90%. HRMS (ESI) calculated for [MH] - : 713.0878; found: 713.0885.

[0286] Synthesis of ligand L47

[0287]

[0288] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 5 was subjected to Suzuki coupling with (3-fluoro-2-methoxyphenyl)boronic acid and then deprotected to synthesize L47, which was purified to obtain a white solid with a yield of 92%. HRMS (ESI) calculated for [M+Na] + : 689.1730; found: 689.1735.

[0289] Synthesis of ligand L48

[0290]

[0291] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), compound 6 was synthesized by Suzuki coupling with (4-chloro-2-hydroxyphenyl)boronic acid to obtain L48, which was purified to obtain a white solid with a yield of 95%. HRMS (ESI) calculated for [M+Na] + :1107.0494; found: 1107.0487.

[0292] Synthesis of ligand L49

[0293]

[0294] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), tris(3-bromophenyl)phosphine oxide and 2-hydroxyphenylboronic acid were Suzuki coupled to synthesize L49, which was purified to obtain a white solid with a yield of 75%. HRMS (ESI) calculated for [M+Na] + : 577.1545; found: 577.1531.

[0295] Synthesis of ligand L50

[0296]

[0297] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), tris(3-bromophenyl)phosphine oxide and (4-chloro-2-hydroxyphenyl)boronic acid were Suzuki coupled to synthesize L50, which was purified to obtain a white solid with a yield of 88%. HRMS (ESI) calculated for [MH] - : 655.0405; found: 655.0424.

[0298] Synthesis of ligand L51

[0299]

[0300] According to the preparation procedure of Scheme 1 (refer to the preparation procedure of L1), tris(3-bromophenyl)phosphine oxide and (5-chloro-2-hydroxyphenyl)boronic acid were Suzuki coupled to synthesize L51, which was purified to obtain a white solid with a yield of 89%. HRMS (ESI) calculated for [M+Na] + : 679.0375; found: 655.0358.

[0301] Example 3

[0302] Taking L1 as an example, ligand L1 (3 μmol) and metal ion (molybdenum) precursor (II) (2.1 mg, 3 μmol) were mixed in dry CCl4 (1.0 mL) solvent and stirred at room temperature for 10 minutes to generate catalyst Cat 1 in situ. A CCl4 (1.0 mL) solution of 4-(hex-1-yn-1-yl) anisole (18.8 mg, 100 μmol) was added to the mixed solution and reacted at room temperature. Strictly timed sampling tests (5 minutes, 15 minutes, 30 minutes and 50 minutes), the reaction was quenched with methanol, and the reaction process was monitored by gas chromatography (GC) after vacuum drying. The reaction equation is as follows:

[0303]

[0304]

[0305] The ligand L1 was replaced by L3, L4, and the multidentate ligands reported by Fürstner (VI) and Zhang Wei (VII), and the other operations were the same as above.

[0306] The ligand L1 was replaced by L3, and the catalyst loading (addition amount) was reduced to 0.6% (molar percentage). Other operations were the same as above.

[0307] Figure 2 The kinetic study of the catalytic activity of the multidentate ligands reported by Fürstner (VI) and Zhang (VII) and a multidentate ligand L1 provided by the present invention on the alkyne metathesis reaction; it can be seen that the catalytic activity of the multidentate ligand L1 provided by the present invention is significantly improved compared with that of Zhang (VII) and is equivalent to that of Fürstner (VI).

[0308] Figure 3 When the multidentate ligand structure contains halogen substitution, such as the multidentate ligand L3 with chlorine substitution at the meta-position of the hydroxyl group and the multidentate ligand L4 with chlorine substitution at the para-position of the hydroxyl group, its catalytic activity is significantly improved.

[0309] Figure 4 When the catalyst loading of the multidentate ligand L3 generated in situ is as low as 0.6% (molar percentage), the catalytic activity can still be maintained at a high level, which proves that the catalyst provided by the present invention still has a high catalytic activity under low loading conditions.

[0310] Example 4

[0311]

[0312] Alkyne metathesis reaction with 4-(prop-1-yn-1-yl)benzaldehyde as substrate: ligand L10 (3 μmol) and metal ion (molybdenum) precursor (II) (2.1 mg, 3 μmol) were mixed in dry CCl4 (2.0 mL) solvent and stirred at 70°C for 10 minutes to generate the catalyst in situ. A CCl4 (1.0 mL) solution of 4-(prop-1-yn-1-yl)benzaldehyde (14.4 mg, 100 μmol) and 5 Å molecular sieves (100 mg) were added to the mixed solution and reacted at 70°C for 1.5 h. The NMR yield was 90%.

[0313] Example 5

[0314]

[0315] Alkyne metathesis reaction with 4-(prop-1-yn-1-yl)aniline as substrate: ligand L10 (3 μmol) and metal ion (molybdenum) precursor (II) (2.1 mg, 3 μmol) were mixed in dry CCl4 (2.0 mL) solvent and stirred at 70°C for 10 minutes to generate the catalyst in situ. A CCl4 (1.0 mL) solution of 4-(prop-1-yn-1-yl)aniline (13.1 mg, 100 μmol) and 5 Å molecular sieves (100 mg) were added to the mixed solution and reacted at 70°C for 2 h. The NMR yield was 60%.

[0316] Example 6

[0317]

[0318] Alkyne metathesis reaction with 4-(prop-1-yn-1-yl)benzonitrile as substrate: ligand L10 (3 μmol) and metal ion (molybdenum) precursor (II) (2.1 mg, 3 μmol) were mixed in dry CCl4 (2.0 mL) solvent and stirred at 70°C for 10 minutes to generate the catalyst in situ. A CCl4 (1.0 mL) solution of 4-(prop-1-yn-1-yl)benzonitrile (14.1 mg, 100 μmol) and 5 Å molecular sieves (100 mg) were added to the mixed solution and reacted at 70°C for 2 h. The NMR yield was 72%.

[0319] The above embodiments are preferred implementation modes of the present invention, but the implementation modes of the present invention are not limited to the above embodiments. Any other changes, modifications, substitutions, combinations, and simplifications made without departing from the spirit and principle of the present invention shall be equivalent replacement modes and shall be included in the protection scope of the present invention.

Claims

1. A multidentate ligand, characterized in that: The general structural formula is as follows (1) or (2): Wherein, Z is selected from carbon, R 4 is selected from hydrogen, alkoxy; or Z is selected from silicon, R 4 is selected from fluoroalkyl, phenyl; or Z is selected from phosphorus, R 4 Selected from =O; R 1 , R 2 , R 3 Each is independently selected from hydrogen, halogen, trifluoromethyl, cyano, acetyl, methyl, methoxy, methylthio, isopropyl, phenoxy, 1,1,3,3-tetramethylbutyl, 4-tert-butylphenyl, 4-methoxyphenyl, 4-N,N-dimethylaminophenyl, 4-methoxyformylphenyl, 4-(2,4,6-trimethylphenyl)phenyl, 4-carbazolylphenyl; Ar each independently represents naphthalene, indane, 1-indanone, 9,9-dimethylfluorene, or estrone.

2. The multidentate ligand according to claim 1, characterized in that The structural formula is one of the following: 。 3. The method for preparing the multidentate ligand according to claim 2, characterized in that: The multidentate ligands L1, L2, L3, L4, L5, L6, L7, L8, L11, L14, L15, L16, L17, L18, L19, L20, L22, L23, L24, L25, L26, L27, L35, L36, L37, L38, L42, L43, L44, L45, L46, L47, L48 were synthesized by Scheme 1; Multidentate ligands L9, L10, L12, L13, L21, and L28 were synthesized by Scheme 2; Multidentate ligands L29, L30, L31, L32, L33, L34, L39, L40, and L41 were synthesized by Scheme 3; The first scheme is as follows: Under protective atmosphere, in the presence of a palladium catalyst and a base, a bromine-substituted triphenylmethane derivative reacts with an arylboronic acid in a mixed solvent of an organic solvent and water to obtain a multidentate ligand; The structural formula of the bromine-substituted triphenylmethane derivative is one of the following: The aryl boronic acid is 2-hydroxyphenylboric acid, (3-chloro-2-hydroxyphenyl)boric acid, (4-chloro-2-hydroxyphenyl)boric acid, (5-chloro-2-hydroxyphenyl)boric acid, (3-fluoro-2-methoxyphenyl)boric acid, (4-fluoro-2-hydroxyphenyl)boric acid, (5-fluoro-2-hydroxyphenyl)boric acid, (4-trifluoromethyl-2-hydroxyphenyl)boric acid, (5-acetyl-2-hydroxyphenyl)boric acid, (4-isopropyl-2-hydroxyphenyl)boric acid, (5-isopropyl-2-methoxyphenyl)boric acid, (5-methoxy-2-hydroxyphenyl)boric acid, (4-methoxy-2-hydroxyphenyl)boric acid, Boric acid, (phenyl)boric acid, (5-methylthio-2-hydroxyphenyl)boric acid, (5-phenoxy-2-hydroxyphenyl)boric acid, (5-isopropyl-4-methyl-2-hydroxyphenyl)boric acid, (5-chloro-4-chloro-2-methoxyphenyl)boric acid, (5-fluoro-4-fluoro-2-methoxyphenyl)boric acid, (3-hydroxynaphthalen-2-yl)boric acid, (6-hydroxy-2,3-dihydro-1H-inden-5-yl)boric acid, (6-hydroxy-1-oxo-2,3-dihydro-1H-inden-5-yl)boric acid, (2-methoxy-9,9-dimethyl-9H-fluoren-3-yl)boric acid; The second scheme is as follows: Under protective atmosphere, in the presence of palladium catalyst and base, triphenylmethane substituted with boric acid pinacol ester reacts with aryl halide in a mixed solvent of organic solvent and water to obtain a multidentate ligand; The structural formula of triphenylmethane substituted with boric acid pinacol ester is: The aryl halide is one of 4-bromo-3-hydroxybenzonitrile, 3-bromo-4-hydroxybenzonitrile, 2-bromo-4-methylphenol, 2-bromo-5-methylphenol, 2-bromo-4-(2,4,4-trimethylpentan-2-yl)phenol, (8R, 9S, 13S)-3-hydroxy-2-iodo-13-methyl-6,7,8,9,11,12,13,14,15,16-decahydro-17H-cyclopenta[a]phenanthrene-17-one; The third scheme is as follows: Under protective atmosphere, in the presence of palladium catalyst and base, halogen-substituted tri(biphenyl)methane reacts with arylboronic acid in a mixed solvent of organic solvent and water to obtain a multidentate ligand; The structural formula of halogen-substituted tris(biphenyl)methane is one of the following: The aryl boronic acid is one of (4-(tert-butyl)phenyl)boric acid, (4-methoxyphenyl)boric acid, (4-(dimethylamino)phenyl)boric acid, (4-(methoxycarbonyl)phenyl)boric acid, (2',4',6'-trimethyl-[1,1'-biphenyl]-4-yl)boric acid and (4-(9H-carbazol-9-yl)phenyl)boric acid.

4. The method for preparing a multidentate ligand according to claim 3, characterized in that: In the first scheme, The molar ratio of the bromine-substituted triphenylmethane derivative to the aryl boronic acid is 1:5-6; The palladium catalyst is selected from at least one of tetrakistriphenylphosphine palladium, methanesulfonyloxy (diadamantyl-n-butylphosphino)-2'-amino-1,1'-biphenyl-2-yl palladium (II); The base is selected from at least one of carbonate and phosphate; The organic solvent is selected from at least one of tetrahydrofuran and 1,4-dioxane; The reaction temperature is 60-100° C., and the reaction time is 12-24 hours. The solution after the reaction is quenched, extracted, concentrated, and purified by column chromatography to obtain a multidentate ligand. In the second scheme, The molar ratio of triphenylmethane substituted with boric acid pinacol ester to aryl halide is 1:5-6; The palladium catalyst is selected from at least one of bistriphenylphosphine palladium dichloride, tetrakistriphenylphosphine palladium, and methanesulfonyloxy (diadamantyl-n-butylphosphino)-2'-amino-1,1'-biphenyl-2-yl palladium (II); The base is selected from at least one of carbonate and phosphate; The solvent is selected from at least one of tetrahydrofuran and 1,4-dioxane; The reaction temperature is 60-100° C., and the reaction time is 12-24 hours. The solution after the reaction is quenched, extracted, concentrated, and purified by column chromatography to obtain a multidentate ligand. In the third scheme, The molar ratio of the halogen-substituted tri(biphenyl)methane to the arylboronic acid is 1:5-6; The palladium catalyst is selected from at least one of tetrakistriphenylphosphine palladium, methanesulfonyloxy (diadamantyl-n-butylphosphino)-2'-amino-1,1'-biphenyl-2-yl palladium (II); The base is selected from at least one of carbonate and phosphate; The organic solvent is selected from at least one of tetrahydrofuran and 1,4-dioxane; The reaction temperature is 60-100° C. and the reaction time is 12-24 hours. The solution after the reaction is quenched, extracted, concentrated, and purified by column chromatography to obtain a multidentate ligand.

5. A multidentate ligand metal catalyst, characterized in that: The structural formula is as follows (3) or (4): Wherein, Z is selected from carbon, R 4 is selected from hydrogen, alkoxy; or Z is selected from silicon, R 4 is selected from fluoroalkyl, phenyl; or Z is selected from phosphorus, R 4 Selected from =O; R 1 , R 2 , R 3 Each independently selected from hydrogen, halogen, trifluoromethyl, cyano, acetyl, methyl, methoxy, methylthio, isopropyl, phenoxy, 1,1,3,3-tetramethylbutyl, 4-tert-butylphenyl, 4-methoxyphenyl, 4-N,N-dimethylaminophenyl, 4-methoxyformylphenyl, 4-(2,4,6-trimethylphenyl)phenyl, 4-carbazolylphenyl; Ar independently represents naphthalene, indane, 1-indanone, 9,9-dimethylfluorene, or estrone.

6. The method for preparing a multidentate ligand metal catalyst according to claim 5, characterized in that: The following steps are involved: The multidentate ligand of claim 1 and the metal ion precursor are mixed in an organic solvent and stirred to obtain a multidentate ligand metal catalyst; The metal ion precursor is a molybdenum-centered carbyne structure, and the structural formula is one of the following: 。 7. The preparation method according to claim 6, characterized in that: The molar ratio of the multidentate ligand to the metal ion precursor is 0.5 to 2: 1; The concentration of the multidentate ligand in the organic solvent is 0.5-5 mM.

8. The preparation method according to claim 6, characterized in that: The stirring temperature is 20-70°C and the stirring time is 10-30 minutes; The organic solvent is CCl4.

9. Use of the multidentate ligand metal catalyst according to claim 5 in catalyzing alkyne metathesis.

10. The use according to claim 9, characterized in that: The molar ratio of the multidentate ligand metal catalyst to the alkyne is 0.6-3:100.