A harmless treatment device for recycling batteries of new energy vehicles
By using a bearing plate, a sprayer and an air-drying gun in the battery recycling device of new energy vehicles, combined with visual detection technology, the drying parameters of cobalt manganese and nickel solution are optimized, and the problems of drying uniformity and low efficiency of cobalt manganese and nickel solution are solved, and cobalt is improved Recycling efficiency of manganese nickel.
Patent Information
- Application Number
- CN202411159243.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-08-22
AI Technical Summary
The prior art has problems of poor uniformity and low efficiency when drying a large number of cobalt-manganese and nickel solutions. Especially when solutions with different viscous conditions adopt the same drying parameters, which affects the drying effect of cobalt-manganese and nickel solutions.
The new energy vehicle battery recycling harmless treatment device is adopted, including a bearing mechanism, a spray mechanism, a drying mechanism and a visual detection mechanism. The atomized cobalt, manganese and nickel solution is uniformly sprayed on the bearing plate through the spray mechanism, and the air-drying mechanism attaches the The droplets are dried, and the visual detection mechanism monitors and analyzes the surface image, calculates the adhesion characterization parameters to adjust the injection rate and scraper operation frequency, and optimizes the drying parameters.
The uniform drying of cobalt-manganese nickel droplets is achieved, the drying efficiency and recycling efficiency are improved, and the cobalt-manganese nickel solution that is adapted to different viscous conditions is ensured to the full recovery of cobalt-manganese nickel.
Smart Images

Figure CN118681240B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of battery recycling, and in particular to a harmless treatment device for recycling batteries of new energy vehicles. Background Art
[0002] With the widespread use of new energy vehicles, lithium-ion batteries have been widely used in such products due to their excellent performance, and are gradually developing into other product application fields. The important raw materials for manufacturing lithium batteries are cobalt, manganese and nickel. The cobalt, manganese and nickel contained in the earth are limited. If they are consumed blindly, they will run out one day. Therefore, in order to ensure a steady supply of the above raw materials, the recovery of cobalt, manganese and nickel in waste batteries is particularly important.
[0003] In the process of recycling cobalt, manganese and nickel from waste lithium batteries, the drying step involving the solution containing cobalt, manganese and nickel is an important part of the recycling process. Currently, a heating device is generally used to dry the solution containing cobalt, manganese and nickel to obtain a metal solid.
[0004] Chinese patent publication number: CN108553928A, discloses a lithium battery material recycling atomization drying device, including a drying chamber, a hot air conveyor, a feeder, a discharger and a controller, the drying chamber includes a spherical atomization chamber, the spherical atomization chamber has a heating layer outside, a hot air layer is formed between the spherical atomization chamber and the heating layer, the inner wall of the spherical atomization chamber is provided with a plurality of hot air jet nozzles communicating with the hot air layer, an infusion tube is provided at the central axis position of the spherical atomization chamber, the starting end of the infusion tube extends out of the drying chamber and is connected to the feeder, the end of the infusion tube is located at the center of the spherical atomization chamber and extends outward along the radial direction to form a plurality of atomization tubes, each atomization tube surface is provided with a plurality of spray heads, the hot air conveyor is connected to the hot air layer, and a discharge port is formed at the bottom of the spherical atomization chamber. The metal solution is atomized through the atomization tube, and the atomized gas is dried with hot air; it can be seen that the above technical solution has the following problems:
[0005] The simultaneous drying of a large amount of cobalt, manganese and nickel solutions affects the uniformity of the drying of the cobalt, manganese and nickel solutions;
[0006] The same drying parameters are used for cobalt-manganese-nickel solutions with different viscosities, which affects the drying efficiency of the cobalt-manganese-nickel solutions. Summary of the invention
[0007] To this end, the present invention provides a new energy vehicle battery recycling and harmless treatment device to overcome the problem in the prior art that a large amount of cobalt manganese nickel solutions are dried simultaneously, which affects the uniformity of the drying of the cobalt manganese nickel solutions. At the same time, cobalt manganese nickel solutions with different viscosities all use the same drying parameters, which affects the drying efficiency of the cobalt manganese nickel solutions.
[0008] To achieve the above-mentioned purpose, the present invention provides a new energy vehicle battery recycling harmless treatment device, comprising:
[0009] A receiving mechanism, comprising a receiving plate and a scraper arranged on the receiving plate for scraping off objects attached to the surface of the receiving plate;
[0010] A spray mechanism, comprising an atomizer arranged on one side of the receiving plate for uniformly spraying the atomized cobalt-manganese-nickel solution onto the receiving plate;
[0011] A drying mechanism, comprising a plurality of air drying guns arranged between the receiving mechanism and the spraying mechanism for drying the cobalt, manganese and nickel droplets attached to the receiving plate;
[0012] A visual inspection mechanism, which is arranged on a side of the spray mechanism away from the drying mechanism, and is used to obtain an image of the surface of the receiving plate;
[0013] The upper computer is connected to the receiving mechanism, the spraying mechanism, the drying mechanism and the visual detection mechanism respectively, and includes an experimental unit, a scraper control unit and an actual control unit:
[0014] The experimental unit is used to control the atomizer to spray the receiving plate at a predetermined spraying time to perform experimental analysis, including determining the displacement characteristics corresponding to each droplet profile based on the receiving plate surface image, determining the drying characteristics based on the grayscale change rate, and calculating the adhesion characterization parameter in combination with the displacement characteristics and the drying characteristics;
[0015] The scraper control unit is used to determine the deposition parameter based on the gray value in the receiving plate surface image, and control the scraper to start;
[0016] The actual control unit is used to control the atomizer based on the adhesion characterization parameter, including adjusting the injection rate of the atomizer based on the adhesion characterization parameter, and obtaining the operating frequency of the scraper to determine whether to correct the injection rate of the atomizer or maintain the operating parameters of the atomizer according to the operating frequency.
[0017] Further, the experimental unit is used to determine the displacement characteristics of the cobalt-manganese-nickel droplet based on the surface image of the receiving plate, including:
[0018] Used to randomly mark a predetermined number of droplet contour features in the receiving plate surface image;
[0019] To determine the displacement of each droplet profile feature within a predetermined time interval;
[0020] Used to determine the average value of each displacement as the displacement feature.
[0021] Further, the experimental unit is used to determine the drying characteristics based on the grayscale change rate, including:
[0022] To obtain the average grayscale of the surface image of the receiving plate;
[0023] Used to draw an average grayscale time domain curve based on the average grayscale of the surface image of each receiving plate;
[0024] Used to respectively calculate the slope of the average grayscale time domain curve within a predetermined time period;
[0025] The maximum value among the slopes is determined as the drying characteristic.
[0026] Furthermore, the experimental unit is used to calculate the adhesion characterization parameter according to formula (1),
[0027]
[0028] Where F represents the adhesion characterization parameter, L represents the displacement characteristic, D represents the drying characteristic, α represents the displacement weight coefficient, β represents the drying weight coefficient, L0 represents the average value of each historical displacement characteristic, and D0 represents the average value of each historical drying characteristic.
[0029] Furthermore, the scraper control unit is used to obtain deposition parameters based on the receiving plate surface image, including:
[0030] The grayscale average value of the acquired receiving plate surface image is determined as the deposition parameter.
[0031] Further, the scraper control unit is used to control the start-up of the scraper based on the deposition parameter, including:
[0032] If the deposition parameter is less than or equal to the preset deposition parameter, the scraper is controlled to operate to scrape off the attachments on the surface of the receiving plate;
[0033] If the deposition parameter is greater than the preset deposition parameter, the scraper is controlled to remain stationary.
[0034] Furthermore, the actual control unit is used to control the atomizer based on the adhesion characterization parameter, including:
[0035] If the adhesion characterization parameter is greater than or equal to the preset adhesion characterization parameter, maintaining the operating parameters of the atomizer;
[0036] If the adhesion characteristic parameter is less than the preset adhesion characteristic parameter, the spray rate of the atomizer is adjusted based on the adhesion characteristic parameter.
[0037] Further, the actual control unit is used to adjust the injection rate of the atomizer based on the adhesion characterization parameter, wherein:
[0038] The adhesion characterization parameters are positively correlated with the spray rate of the atomizer.
[0039] Furthermore, the actual control unit is used to obtain the operating frequency of the scraper, including:
[0040] The number of times the scraper runs in a cycle is periodically obtained, and the ratio of the number of times the scraper runs to the duration of the cycle is calculated to obtain the running frequency;
[0041] The actual control unit is used to determine whether to correct the injection rate of the atomizer according to the operating frequency, including:
[0042] If the operating frequency is less than or equal to the preset operating frequency, the spray rate of the atomizer is corrected based on the operating frequency;
[0043] If the operating frequency is greater than the preset operating frequency, the atomizer is controlled to continue to operate with the current operating parameters.
[0044] Further, the actual control unit is used to correct the injection rate of the atomizer based on the operating frequency, wherein:
[0045] The operating frequency is negatively correlated with the correction amplitude of the atomizer's injection rate.
[0046] Compared with the prior art, the beneficial effect of the present invention lies in that the present invention sprays the atomized cobalt-manganese-nickel solution onto a receiving plate through a spray mechanism, the air-drying mechanism dries the cobalt-manganese-nickel droplets attached to the receiving plate, dries the cobalt-manganese-nickel droplets evenly and fully, and the visual inspection mechanism monitors the conditions of the cobalt-manganese-nickel droplets on the receiving plate under different conditions; the experimental unit determines the displacement characteristics and drying characteristics of the cobalt-manganese-nickel droplets based on the receiving plate surface image obtained by the visual inspection mechanism through experimental analysis, and calculates the adhesion characterization parameters in combination with the drying characteristics and the displacement characteristics to characterize the drying difficulty of the cobalt-manganese-nickel solution; after the experimental unit completes the calculation of the adhesion characterization parameters, the scraper control unit starts to operate, and the scraper control unit periodically obtains the completed image through the visual inspection mechanism. The surface image of the receiving plate after drying determines the deposition parameters of the receiving plate to control the start-up of the scraper; the actual control unit controls the operation of the atomizer based on the adhesion characterization parameter. When the adhesion characterization parameter is less than the preset adhesion characterization parameter, the cobalt manganese nickel solution is difficult to be fully dried by the air-drying mechanism. In this case, the injection rate of the atomizer is adjusted; when the cobalt manganese nickel solution is difficult to be fully dried by the air-drying mechanism, the air-drying condition of the cobalt manganese nickel solution is continuously detected. When the operating frequency of the scraper is less than or equal to the preset operating frequency, the air-drying efficiency of the cobalt manganese nickel solution is too low. The injection rate of the atomizer is increased to balance the drying efficiency and drying effect. Targeted drying parameters are adopted for cobalt manganese nickel solutions with different viscosities to improve the drying efficiency of the cobalt manganese nickel solution.
[0047] Furthermore, the displacement characteristics and drying characteristics of the cobalt-manganese-nickel droplets are determined by calculating the adhesion characterization parameters; in actual situations, the drying difficulty of cobalt-manganese-nickel solutions of different concentrations is different. The higher the concentration of the cobalt-manganese-nickel solution, the more viscous the cobalt-manganese-nickel solution is, and the better the adhesion to the receiving plate is. A large amount of atomized cobalt-manganese-nickel solution can be sprayed at one time for drying, and it is also easier to be dried by the drying mechanism. The viscosity of the cobalt-manganese-nickel solution is characterized by the displacement characteristics; when conducting experimental analysis in the experimental unit, several images of the receiving plate surface after the spraying are obtained to obtain the drying parameters of the drying process, determine the drying characteristics, and further determine The difficulty of drying the cobalt, manganese and nickel solution; in particular, the cobalt, manganese and nickel solution that is difficult to dry is prone to insufficient drying during the drying process, resulting in the cobalt, manganese and nickel particles that are not fully dried falling off the receiving plate, affecting the overall drying quality of the cobalt, manganese and nickel solution; in order to ensure the full recovery of cobalt, manganese and nickel while balancing the drying efficiency of the solution, the adhesion characterization parameters are calculated based on the displacement characteristics and drying characteristics of the cobalt, manganese and nickel droplets. The adhesion characterization parameters record the difficulty of drying each cobalt, manganese and nickel solution, provide data support for the determination of subsequent drying parameters, and effectively determine the difficulty of drying the cobalt, manganese and nickel solution while improving the recovery efficiency of cobalt, manganese and nickel. BRIEF DESCRIPTION OF THE DRAWINGS
[0048] Figure 1 This is a module block diagram of a new energy vehicle battery recycling and harmless treatment device according to an embodiment of the present invention;
[0049] Figure 2 A logic decision diagram for controlling a scraper based on deposition parameters according to an embodiment of the present invention;
[0050] Figure 3 This is a logic decision diagram for controlling an atomizer based on adhesion characterization parameters according to an embodiment of the present invention;
[0051] Figure 4 This is a logic determination diagram for determining whether to correct the injection rate of the atomizer according to the operating frequency according to an embodiment of the present invention. DETAILED DESCRIPTION
[0052] In order to make the objects and advantages of the present invention more clearly understood, the present invention is further described below in conjunction with embodiments; it should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0053] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood by those skilled in the art that these embodiments are only used to explain the technical principles of the present invention and are not intended to limit the protection scope of the present invention.
[0054] It should be noted that, in the description of the present invention, terms such as "up", "down", "left", "right", "inside" and "outside" indicating directions or positional relationships are based on the directions or positional relationships shown in the drawings. This is merely for the convenience of description and does not indicate or imply that the device or element must have a specific orientation, be constructed and operated in a specific orientation. Therefore, it cannot be understood as a limitation on the present invention.
[0055] In addition, it should be noted that in the description of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0056] See also Figure 1 , Figure 2 , Figure 3 as well as Figure 4 As shown, they are respectively a block diagram of a harmless treatment device for recycling new energy vehicle batteries according to an embodiment of the present invention, a logic determination diagram for controlling a scraper based on a deposition parameter, a logic determination diagram for controlling an atomizer based on an adhesion characterization parameter, and a logic determination diagram for determining whether to correct the injection rate of the atomizer according to the operating frequency; a harmless treatment device for recycling new energy vehicle batteries according to an embodiment of the present invention, comprising:
[0057] A receiving mechanism, comprising a receiving plate and a scraper arranged on the receiving plate for scraping off objects attached to the surface of the receiving plate;
[0058] A spray mechanism, comprising an atomizer arranged on one side of the receiving plate for uniformly spraying the atomized cobalt-manganese-nickel solution onto the receiving plate;
[0059] A drying mechanism, comprising a plurality of air drying guns arranged between the receiving mechanism and the spraying mechanism for drying the cobalt, manganese and nickel droplets attached to the receiving plate;
[0060] A visual inspection mechanism, which is arranged on a side of the spray mechanism away from the drying mechanism, and is used to obtain an image of the surface of the receiving plate;
[0061] The upper computer is connected to the receiving mechanism, the spraying mechanism, the drying mechanism and the visual detection mechanism respectively, and includes an experimental unit, a scraper control unit and an actual control unit:
[0062] The experimental unit is used to control the atomizer to spray the receiving plate at a predetermined spraying time to perform experimental analysis, including determining the displacement characteristics corresponding to each droplet profile based on the receiving plate surface image, determining the drying characteristics based on the grayscale change rate, and calculating the adhesion characterization parameter in combination with the displacement characteristics and the drying characteristics;
[0063] The scraper control unit is used to determine the deposition parameter based on the gray value in the receiving plate surface image, and control the scraper to start;
[0064] The actual control unit is used to control the atomizer based on the adhesion characterization parameter, including adjusting the injection rate of the atomizer based on the adhesion characterization parameter, and obtaining the operating frequency of the scraper to determine whether to correct the injection rate of the atomizer or maintain the operating parameters of the atomizer according to the operating frequency.
[0065] Specifically, there is no limitation on the specific structure of the scraper, as long as it can scrape off the attachments on the surface of the receiving plate. For example, the scraper can be set on the receiving plate through a slide rail, and the scraper can be moved by sliding on the slide rail to scrape off the attachments on the surface of the receiving plate. Of course, other forms can also be used, which will not be repeated here.
[0066] Specifically, there is no limitation on the specific structure of the atomizer, and those skilled in the art may select any existing atomizer according to their needs, as long as it can realize the function of atomizing and spraying the solution, which will not be described in detail.
[0067] Specifically, there is no limitation on the specific structure of the host computer. The host computer and each unit therein may be composed of logic components, and the logic components include a field programmable processor, a computer or a microprocessor in a computer.
[0068] Specifically, there is no limitation on the specific structure of the visual inspection mechanism, which may adopt a high-precision industrial CCD camera. Of course, other forms of acquiring images may also be adopted, which will not be elaborated here.
[0069] Specifically, it can be understood that the experimental unit can control the visual detection mechanism to obtain the surface image of the receiving plate after completing the spraying of the receiving plate to determine the displacement of each droplet contour feature marked in the surface image of the receiving plate within a predetermined interval time, which will not be repeated.
[0070] Specifically, the present invention sprays the atomized cobalt-manganese-nickel solution onto a receiving plate through a spray mechanism, and an air-drying mechanism dries the cobalt-manganese-nickel droplets attached to the receiving plate, thereby increasing the drying area, improving the efficiency, and evenly and fully drying the cobalt-manganese-nickel droplets; a visual inspection mechanism monitors the conditions of the cobalt-manganese-nickel droplets on the receiving plate under different conditions; an experimental unit determines the displacement characteristics and drying characteristics of the cobalt-manganese-nickel droplets based on the receiving plate surface image obtained by the visual inspection mechanism through experimental analysis, and calculates adhesion characterization parameters in combination with the drying characteristics and displacement characteristics to characterize the degree of drying difficulty of the cobalt-manganese-nickel solution; after the experimental unit completes the calculation of the adhesion characterization parameters, the scraper control unit starts to operate, and the scraper control unit periodically obtains the image of the completed drying through the visual inspection mechanism. The surface image of the receiving plate after drying determines the deposition parameters of the receiving plate to control the start-up of the scraper; the actual control unit controls the operation of the atomizer based on the adhesion characterization parameter. When the adhesion characterization parameter is less than the preset adhesion characterization parameter, the cobalt manganese nickel solution is difficult to be fully dried by the air-drying mechanism. In this case, the injection rate of the atomizer is adjusted; when the cobalt manganese nickel solution is difficult to be fully dried by the air-drying mechanism, the air-drying condition of the cobalt manganese nickel solution is continuously detected. When the operating frequency of the scraper is less than or equal to the preset operating frequency, the air-drying efficiency of the cobalt manganese nickel solution is too low. The injection rate of the atomizer is increased to balance the drying efficiency and drying effect. Targeted drying parameters are adopted for cobalt manganese nickel solutions with different viscosities to improve the drying efficiency of the cobalt manganese nickel solution.
[0071] Specifically, the experimental unit is used to determine the displacement characteristics of the cobalt-manganese-nickel droplet based on the surface image of the receiving plate, including:
[0072] Used to randomly mark a predetermined number of droplet contour features in the receiving plate surface image;
[0073] To determine the displacement of each droplet profile feature within a predetermined time interval;
[0074] Used to determine the average value of each displacement as the displacement feature.
[0075] It is understandable that the droplet contour feature can be obtained by identifying the droplet contour through an image processing algorithm, which will not be described in detail.
[0076] Specifically, the number of selected droplet profile features can be determined by a person skilled in the art. It can be understood that the drop displacement of the cobalt-manganese-nickel droplet can be characterized, and no further details will be given.
[0077] Specifically, the experimental unit is used to determine the drying characteristics based on the grayscale change rate, including:
[0078] To obtain the average grayscale of the surface image of the receiving plate;
[0079] Used to draw an average grayscale time domain curve based on the average grayscale of the surface image of each receiving plate;
[0080] Used to respectively calculate the slope of the average grayscale time domain curve within a predetermined time period;
[0081] The maximum value among the slopes is determined as the drying characteristic.
[0082] It can be understood that the drying characteristics of the cobalt, manganese, nickel droplets are determined by acquiring the average grayscale of several receiving plate surface images during the drying process of the cobalt, manganese, nickel droplets on the receiving plate. The greater the average grayscale of the receiving plate surface images, the greater the degree of drying of the cobalt, manganese, nickel droplets. The greater the slope within a predetermined time period, the faster the drying speed. The maximum value of each slope is selected as the drying characteristic to characterize the drying condition of the cobalt, manganese, nickel droplets, which will not be elaborated here.
[0083] The predetermined time period is selected within the interval [5s, 15s].
[0084] Specifically, the experimental unit is used to calculate the adhesion characterization parameter according to formula (1):
[0085]
[0086] Where F represents the adhesion characterization parameter, L represents the displacement characteristic, D represents the drying characteristic, α represents the displacement weight coefficient, β represents the drying weight coefficient, L0 represents the average value of each historical displacement characteristic, and D0 represents the average value of each historical drying characteristic.
[0087] Specifically, α is set to 0.7 and β is set to 0.3.
[0088] Specifically, it can be understood that the higher the concentration of the cobalt manganese nickel solution, the more viscous the cobalt manganese nickel solution, and the better the adhesion on the receiving plate. Therefore, the smaller the displacement characteristic, the better the adhesion, and the easier it is to dry, which is inversely proportional to the adhesion characterization parameter. The ratio of the displacement characteristic to the average value of the historical drying characteristic indicates the difficulty of drying the current cobalt manganese nickel solution compared with each historical cobalt manganese nickel solution. The smaller the value, the easier it is to dry; and the drying characteristic characterizes the drying speed of the cobalt manganese nickel solution. The larger the drying characteristic, the easier it is to dry, which is directly proportional to the adhesion characterization parameter. The ratio of the drying characteristic to the average value of each historical drying characteristic also indicates the difficulty of drying the drying characteristic of the current cobalt manganese nickel solution compared with each historical cobalt manganese nickel solution. The larger the value, the easier it is to dry.
[0089] Specifically, the displacement characteristics and drying characteristics of the cobalt-manganese-nickel droplets are determined by calculating the adhesion characterization parameters; in actual situations, the drying difficulty of cobalt-manganese-nickel solutions of different concentrations is different. The higher the concentration of the cobalt-manganese-nickel solution, the more viscous the cobalt-manganese-nickel solution is, and the better the adhesion to the receiving plate is. A large amount of atomized cobalt-manganese-nickel solution can be sprayed at one time for drying, and it is also easier to be dried by the drying mechanism. The viscosity of the cobalt-manganese-nickel solution is characterized by the displacement characteristics; when conducting experimental analysis in the experimental unit, several images of the receiving plate surface after the spraying are obtained to obtain the drying parameters of the drying process, determine the drying characteristics, and further determine The difficulty of drying the cobalt, manganese and nickel solution; in particular, the cobalt, manganese and nickel solution that is difficult to dry is prone to insufficient drying during the drying process, resulting in the cobalt, manganese and nickel particles that are not fully dried falling off the receiving plate, affecting the overall drying quality of the cobalt, manganese and nickel solution; in order to ensure the full recovery of cobalt, manganese and nickel while balancing the drying efficiency of the solution, the adhesion characterization parameters are calculated based on the displacement characteristics and drying characteristics of the cobalt, manganese and nickel droplets. The adhesion characterization parameters record the difficulty of drying each cobalt, manganese and nickel solution, provide data support for the determination of subsequent drying parameters, and effectively determine the difficulty of drying the cobalt, manganese and nickel solution while improving the recovery efficiency of cobalt, manganese and nickel.
[0090] Specifically, the scraper control unit is used to obtain deposition parameters based on the receiving plate surface image, including:
[0091] The grayscale average value of the acquired receiving plate surface image is determined as the deposition parameter.
[0092] Specifically, the scraper control unit is used to control the scraper to start based on the deposition parameter, including:
[0093] If the deposition parameter is less than or equal to the preset deposition parameter, the scraper is controlled to operate to scrape off the attachments on the surface of the receiving plate;
[0094] If the deposition parameter is greater than the preset deposition parameter, the scraper is controlled to remain stationary.
[0095] The preset deposition parameter Y0 is selected within the interval [1.2C0, 1.3C0]. The selection process of C0 is to obtain several receiving plate surface images after the cobalt-manganese-nickel particles complete a certain deposition thickness, input each receiving plate surface image into the image processing software to obtain each average grayscale value, and calculate the average of each average grayscale value to obtain C0.
[0096] Specifically, the actual control unit is used to control the atomizer based on the adhesion characterization parameter, including:
[0097] If the adhesion characterization parameter is greater than or equal to the preset adhesion characterization parameter, maintaining the operating parameters of the atomizer;
[0098] If the adhesion characteristic parameter is less than the preset adhesion characteristic parameter, the spray rate of the atomizer is adjusted based on the adhesion characteristic parameter.
[0099] The preset adhesion characterization parameter F0 is selected within the interval [1.27, 1.32].
[0100] Specifically, the actual control unit is used to adjust the injection rate of the atomizer based on the adhesion characterization parameter, wherein:
[0101] The adhesion characterization parameters are positively correlated with the spray rate of the atomizer.
[0102] In this embodiment, optionally,
[0103] The adhesion characterization parameter F is compared with the first preset characterization comparison threshold F1 and the second preset characterization comparison threshold F2,
[0104] If F≤F1, the injection rate is determined as the first injection rate V1, and V1=0.97V0 is set;
[0105] If F1<F≤F2, the injection rate is determined as the second injection rate V2, and V2=0.93V0 is set;
[0106] If F>F2, the injection rate is determined as the third injection rate V3, and V3=0.84V0 is set;
[0107] Where: V0 is the initial injection rate, F1=0.6F0, F2=0.8F0.
[0108] Specifically, the actual control unit is used to obtain the operating frequency of the scraper, including:
[0109] The number of times the scraper runs in a cycle is periodically obtained, and the ratio of the number of times the scraper runs to the duration of the cycle is calculated to obtain the running frequency;
[0110] The actual control unit is used to determine whether to correct the injection rate of the atomizer according to the operating frequency, including:
[0111] If the operating frequency is less than or equal to the preset operating frequency, the spray rate of the atomizer is corrected based on the operating frequency;
[0112] If the operating frequency is greater than the preset operating frequency, the atomizer is controlled to continue to operate with the current operating parameters.
[0113] Specifically, the preset operating frequency X0 is selected within the interval [0.8U0, 0.85U0], and U0 is the average value of each historical operating frequency.
[0114] Specifically, the actual control unit is used to correct the injection rate of the atomizer based on the operating frequency, wherein:
[0115] The operating frequency is negatively correlated with the correction amplitude of the atomizer's injection rate.
[0116] In this embodiment, optionally,
[0117] The operating frequency X is compared with the first preset frequency comparison threshold X1 and the second preset frequency comparison threshold X2,
[0118] If X≤X1, the increase amplitude of the injection rate is determined as the first rate correction amplitude A1, and A1=0.3A0 is set;
[0119] If X1<X≤X2, the increase amplitude of the injection rate is determined as the second rate correction amplitude A2, and A2=0.2A0 is set;
[0120] If X>X2, the increase amplitude of the injection rate is determined as the third rate correction amplitude A3, and A3=0.1A0 is set;
[0121] Where: A0 is the current injection rate of the atomizer, X1=0.5X0, X2=0.7X0.
[0122] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.
[0123] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A new energy vehicle battery recycling and harmless treatment device, It is characterized in that include: A receiving mechanism, comprising a receiving plate and a scraper arranged on the receiving plate for scraping off objects attached to the surface of the receiving plate; A spray mechanism, comprising an atomizer arranged on one side of the receiving plate for uniformly spraying the atomized cobalt-manganese-nickel solution onto the receiving plate; A drying mechanism, comprising a plurality of air drying guns arranged between the receiving mechanism and the spraying mechanism for drying the cobalt, manganese and nickel droplets attached to the receiving plate; A visual inspection mechanism, which is arranged on a side of the spray mechanism away from the drying mechanism, and is used to obtain an image of the surface of the receiving plate; The upper computer is connected to the receiving mechanism, the spraying mechanism, the drying mechanism and the visual detection mechanism respectively, and includes an experimental unit, a scraper control unit and an actual control unit: The experimental unit is used to control the atomizer to spray the receiving plate at a predetermined spraying time to perform experimental analysis, including determining the displacement characteristics corresponding to each droplet profile based on the receiving plate surface image, determining the drying characteristics based on the grayscale change rate, and calculating the adhesion characterization parameter in combination with the displacement characteristics and the drying characteristics; The scraper control unit is used to determine the deposition parameter based on the gray value in the receiving plate surface image, and control the scraper to start; The actual control unit is used to control the atomizer based on the adhesion characterization parameter, including adjusting the injection rate of the atomizer based on the adhesion characterization parameter, and obtaining the operating frequency of the scraper to determine whether to correct the injection rate of the atomizer according to the operating frequency; The experimental unit is used to determine the displacement characteristics of the cobalt-manganese-nickel droplet based on the surface image of the receiving plate, including: Used to randomly mark a predetermined number of droplet contour features in the receiving plate surface image; To determine the displacement of each droplet profile feature within a predetermined time interval; Used to determine the average value of each displacement as the displacement feature; The experimental unit is used to determine the drying characteristics based on the grayscale change rate, including: To obtain the average grayscale of the surface image of the receiving plate; Used to draw an average grayscale time domain curve based on the average grayscale of the surface image of each receiving plate; Used to respectively calculate the slope of the average grayscale time domain curve within a predetermined time period; The maximum value among the slopes is determined as the drying characteristic; The experimental unit is used to calculate the adhesion characterization parameter according to formula (1), ; In the formula, F represents the adhesion characterization parameter, L represents the displacement characteristic, D represents the drying characteristic, α represents the displacement weight coefficient, β represents the drying weight coefficient, and L 0 is the average value of each historical displacement feature, D 0 is the average value of each historical drying characteristic; The scraper control unit is used to obtain deposition parameters based on the receiving plate surface image, including: Determine the grayscale average value of the acquired receiving plate surface image as a deposition parameter; The scraper control unit is used to control the scraper to start based on the deposition parameter, including: If the deposition parameter is less than or equal to the preset deposition parameter, the scraper is controlled to operate to scrape off the attachments on the surface of the receiving plate; If the deposition parameter is greater than the preset deposition parameter, the scraper is controlled to remain stationary; The actual control unit is used to control the atomizer based on the adhesion characterization parameter, including: If the adhesion characterization parameter is greater than or equal to the preset adhesion characterization parameter, maintaining the operating parameters of the atomizer; If the adhesion characterization parameter is less than a preset adhesion characterization parameter, adjusting the spray rate of the atomizer based on the adhesion characterization parameter; The actual control unit is used to adjust the injection rate of the atomizer based on the adhesion characterization parameter, wherein: The adhesion characterization parameters are positively correlated with the spray rate of the atomizer.
Citation Information
Patent Citations
Lithium battery material recycling, atomizing and drying device
CN108553928A
A method and a system for monitoring spray nozzles in a spray drying or spray cooling chamber
CN107533011A
Image processing method and device in 3D printing, storage medium and terminal
CN115187469A
Improvements in or relating to spray-drying apparatus
GB382129A
Electrode drying device and electrode drying method
US20230016387A1