A method for protecting superconducting magnet quench detection line under vacuum pressure impregnation
By using heat shrink sleeves, silicone and self-melting tapes to wrap the overthrust detection line to prevent it from contacting the resin, the problem of line insulation damage during vacuum pressure immersion is solved, efficient line protection is achieved, and the magnet is ensured. Safe operation and stable performance.
Patent Information
- Application Number
- CN202411183920.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-08-27
AI Technical Summary
During vacuum pressure immersion, the superconducting magnet supernatant detection line is prone to contact directly with the resin, causing the resin to become brittle after curing, destroying the high-voltage wire core and insulation, increasing the risk of Paxing discharge accidents.
The overscaling detection line is wrapped with materials such as heat shrink sleeves, silicone, self-melting tape and mold release cloth to prevent it from contacting the resin, and sealed by silicone curing and self-melting tape to ensure the integrity of the line insulation.
It effectively protects the overscaling detection line, avoids the damage to the line by resin, ensures the radiation resistance, high temperature and low temperature resistance of the line, reduces the failure rate of the magnet, and ensures the safe operation of the magnet.
Smart Images

Figure CN118692753B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of superconducting magnet quench detection line protection method, and in particular relates to a superconducting magnet quench detection line protection method under vacuum pressure impregnation. Background Art
[0002] The central solenoid model coil (CSMC) and the toroidal field (TF) magnet are both important subunits of the superconducting magnet research system of the Critical System Integrated Research Facility (CRAFT) of the Fusion Reactor Host. The quench detection line is the lifeline of the safe operation of the superconducting magnet. The quench detection line needs to operate for a long time in an ultra-low temperature, high vacuum, and strong irradiation electromagnetic environment. Once the vacuum is destroyed, the occurrence of Paschen discharge accidents must be prevented. Therefore, the insulation requirements for the high-voltage line of the quench detection line are very high and cannot be damaged. In order to ensure the safety of the magnet, the magnet insulation must be completed by vacuum pressure impregnation (VPI), and the quench detection line must be welded and penetrated before VPI. The quench detection line needs to be protected during the entire VPI process. In the process of removing excess resin after VPI, the high-voltage line core wire and insulation of the quench detection line must be prevented from being damaged. Therefore, how to protect the superconducting magnet quench detection line under vacuum pressure impregnation is crucial. Summary of the invention
[0003] In order to solve the above technical problems, the present invention provides a method for protecting a superconducting magnet quench detection line under vacuum pressure impregnation, which effectively prevents the superconducting magnet quench detection line from passing through the insulating part of the magnet and directly contacting the resin during the vacuum pressure impregnation process, and avoids the resin that becomes brittle after curing from damaging the quench detection line when it is removed later.
[0004] To achieve the above purpose, the technical solution adopted by the present invention is as follows:
[0005] A superconducting magnet quench detection line protection method under vacuum pressure impregnation comprises the following steps:
[0006] Step 1, when the quench detection line at the superconducting magnet armor or helium tube position is unwrapped and passed through the magnet insulation layer, the quench detection line is wrapped with a heat shrink sleeve with a total length of N, with the outermost side of the magnet insulation layer as the boundary, the inner and outer sides of the magnet insulation layer each include a heat shrink sleeve with a length of N / 2, and the total length of the quench detection line is greater than the total length of the heat shrink sleeve; the quench detection line is a high-voltage line, the core wire of the high-voltage line is a single-core multi-strand silver-plated copper wire, and the sheath is made of polyimide insulation material;
[0007] Step 2, coiling the end section of the quench detection line outside the magnet insulation layer into a roll and wrapping it with a release cloth and then putting it into a box body, pouring silica gel into the box body for curing, the release cloth is FEP film, and the silica gel is organic silicon thermal conductive potting glue;
[0008] Step 3: Place the transition section of the quench detection line from the point where the quench detection line passes through the magnet insulation layer to the box body between the two self-fusing tapes for compression and sealing, and coat a silicone layer on the surface of the self-fusing tape, wherein the self-fusing tape is made of silicone material.
[0009] Furthermore, the quench detection wire is a high-voltage wire with an outer diameter of 2.8 mm. The high-voltage wire is made of multiple strands of silver-plated copper wires twisted at a certain pitch into a core wire with a diameter of 1.0 mm. The core wire insulation layer is a polyimide extruded sheath. The quench detection wire insulation is resistant to radiation of 2000 Mrad and serves in the temperature range of 4K~300K.
[0010] Furthermore, the heat shrinkable tube is a polyolefin tube with a diameter of 3.0 mm, a shrinkage rate between 50% and 70%, and a high temperature resistance of 300°C. The length N of the heat shrinkable tube is 400 mm. The quench detection line covered with 200 mm heat shrinkable tube is left inside the magnet insulation layer, and the remaining quench detection line covered with 200 mm heat shrinkable tube is left outside the magnet insulation layer.
[0011] Furthermore, the unwinding is a process for the quench detection line to pass through the magnet insulation layer, and the magnet insulation layer is a composite tape composed of a glass ribbon and a polyimide film tape, which is half-lapped on a superconducting magnet armor or a helium tube for multiple times, and then injected with resin under vacuum pressure impregnation and solidified, wherein the width of the glass ribbon is greater than the width of the polyimide film tape.
[0012] Furthermore, the release cloth has no adhesion to resin and silicone, and is resistant to high temperatures of 300° C. The release cloth tightly wraps the rolled quench detection wire.
[0013] Furthermore, the box body is a metal box body, which is resistant to high temperature of 300°C and has no end cover.
[0014] Furthermore, the silicone thermally conductive potting glue and the silicone layer have fluidity and thermal conductivity when in liquid state, and have toughness and are detachable after being cured.
[0015] Furthermore, the self-fusing tape is a self-fusing silicone tape, which is resistant to high temperatures of 150° C. The quench detection line transition section is placed between two self-fusing tapes for compression and sealing.
[0016] Furthermore, the vacuum pressure impregnation temperature ranges from 135 to 150° C., the impregnation pressure is 0.2 MPa, and the impregnation time is 24 hours.
[0017] The beneficial effects of the present invention are:
[0018] (1) The high-voltage line insulation of the quench detection line is made of polyimide material, which is resistant to radiation, high temperature and low temperature, and meets the requirements of various performance tests of the magnet and long-term service under extreme working conditions.
[0019] (2) The heat shrink tubing, silicone, self-fusing tape, and release cloth used to protect the quench detection line are all easily available materials on the market. They are low-cost, economical, and environmentally friendly.
[0020] (3) The quench detection line protection method is simple, the protection area is comprehensive, easy for technicians to understand, and easy to operate. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 The present invention is a principle block diagram of a superconducting magnet quench detection line protection method under vacuum pressure impregnation. DETAILED DESCRIPTION
[0022] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0023] like Figure 1 As shown, the present invention provides a method for protecting a superconducting magnet quench detection line under vacuum pressure impregnation. First, the quench detection line at the position of the superconducting magnet armor or helium tube is unwrapped and passed through the magnet insulation layer, and a polyolefin heat shrink tubing is used for protection. Half of the quench detection line protected by the heat shrink tubing remains inside the magnet insulation layer, and the other half remains outside the magnet insulation layer. The quench detection line is a high-voltage line, the core wire is a single-core multi-strand silver-plated copper wire, and the sheath is a polyimide insulation material; then, the end section of the quench detection line leading out of the magnet insulation layer is coiled into a roll, wrapped with a demoulding cloth and placed in a box body, and silicone is poured in and solidified, and the demoulding cloth is an FEP film; finally, the quench detection line from the point where the quench detection line passes through the magnet insulation layer to the transition section of the quench detection line of the box body is placed between two self-fusing tapes for compression and sealing, and then a silicone layer is applied on the surface of the self-fusing tape, and the silicone layer uses organic silicone thermal conductive potting glue; the self-fusing tape is a silicone material, which plays an isolation and sealing effect during vacuum pressure impregnation. This method is used to prevent the insulation of the quench detection line of the superconducting magnet from being damaged during vacuum pressure immersion, thus providing a guarantee for the subsequent Paschen test and safe operation of the magnet.
[0024] Furthermore, the quench detection wire is a high-voltage wire, the core wire is a plurality of silver-plated copper wires twisted with a certain pitch, the diameter after twisting is φ1.0mm, the insulation is a polyimide extruded sheath, the outer diameter is φ2.8mm; the quench detection wire has an insulation radiation resistance of 2000Mrad and can serve for a long time in the temperature range of 4K~300K.
[0025] Further, the heat shrinkable sleeve is a φ3.0mm polyolefin sleeve with a shrinkage rate between 50% and 70%, and a high temperature resistance of up to 300°C. The heat shrinkable sleeve is 400mm long, and is uniformly heated and shrunk with a hot air gun. When passing through the magnet insulation layer, the quench detection line of the 200mm heat shrinkable sleeve is left inside the magnet insulation layer, and the remaining quench detection line with the 200mm heat shrinkable sleeve is left outside the magnet insulation layer. The heat shrinkable sleeve is used to isolate the quench detection line from the resin, preventing the quench detection line from becoming brittle after directly contacting the resin at the passing position, and plays a role in protecting the quench detection line. In fact, the length of the quench detection line is much greater than the length of the heat shrinkable sleeve. For example, for a 10-meter-long quench detection line, the heat shrinkable sleeve is 400mm mainly to protect the part of the quench detection line that passes through the magnet insulation layer.
[0026] Furthermore, the unwrapping is a process for the quench detection line to pass through the magnet insulation layer, the purpose of which is to increase the creepage distance and reduce the gap through which the quench detection line passes. The magnet insulation layer is a composite tape composed of a glass ribbon and a polyimide film tape, which is half-lapped on the magnet armor or helium tube for multiple times and then injected with resin and cured under vacuum pressure impregnation, wherein the width of the glass ribbon is greater than the width of the polyimide film tape, the purpose of which is to enhance the sealing of the magnet insulation layer.
[0027] Furthermore, the release cloth is a FEP film, which has no adhesion to resin and silicone and can withstand a high temperature of 300° C. Before VPI, the rolled quench detection wire is tightly wrapped with the release cloth to prevent direct contact between the silicone and the insulation of the quench detection wire during VPI.
[0028] Furthermore, the box body is a metal box body, which can withstand a high temperature of 300° C., has no end cover on the top of the box body, and the box body itself has no leakage points. The quench detection wire wrapped in a stripping cloth and rolled into a roll is placed inside the box body.
[0029] Furthermore, the silicone thermally conductive potting glue and the silicone layer are silicone thermally conductive potting glue, which has good fluidity and thermal conductivity in liquid state, can be heated at 135°C @ 24h, has good toughness after curing, and is detachable. After VPI, the cured silicone can be easily removed without damaging the insulation of the quench detection line.
[0030] Furthermore, the self-fusing tape is a self-fusing silicone tape that can withstand a temperature of 150°C for a long time. The quench detection line of the transition section is placed between two pieces of self-fusing tape and pressed tightly. The self-fusing tape has a strong adhesiveness and has a very good sealing effect. After VPI, the self-fusing tape can be easily removed without damaging the insulation of the quench detection line.
[0031] Furthermore, the vacuum pressure impregnation temperature is 135-150°C @24h, and the impregnation pressure is 0.2MPa. On the one hand, the resin used for impregnation has good thermal conductivity and is heated evenly. On the other hand, the cured resin does not crack when serving for a long time at liquid helium (-269°C), and has good sealing and insulation properties, providing protection for Paschen test and safe operation of the magnet.
[0032] Furthermore, Figure 1 All parts are in a closed mold before VPI. The mold is equipped with a glue injection port and a glue outlet. During VPI, the mold is in a vacuum-sealed pressure vessel. The inside of the mold is filled with resin, and VPI vacuum casting is completed after heating and pressurization.
[0033] Before use, the protection method of the present invention passes resistance test, insulation DC withstand voltage test, and local Parson test at room temperature to ensure absolute safety and reliability. In addition, the protection method is used in the VPI process of the central solenoid model coil (CSMC) of the key system comprehensive research facility (CRAFT) of the fusion reactor host, and good benefits are achieved. So far, there has been no failure, which provides a guarantee for the safe and stable operation of superconducting magnets.
[0034] The specific embodiments described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.
Claims
1. A superconducting magnet quench detection line protection method under vacuum pressure impregnation, characterized in that: The method comprises: Step 1, when the quench detection line at the superconducting magnet armor or helium tube position is unwrapped and passed through the magnet insulation layer, the quench detection line is wrapped with a heat shrink sleeve with a total length of N, with the outermost side of the magnet insulation layer as the boundary, the inner and outer sides of the magnet insulation layer each include a heat shrink sleeve with a length of N / 2, and the total length of the quench detection line is greater than the total length of the heat shrink sleeve; the quench detection line is a high-voltage line, the core wire of the high-voltage line is a single-core multi-strand silver-plated copper wire, and the sheath is made of polyimide insulation material; Step 2, coiling the end section of the quench detection line outside the magnet insulation layer into a roll and wrapping it with a release cloth and then putting it into a box body, pouring silica gel into the box body for curing, the release cloth is FEP film, and the silica gel is organic silicon thermal conductive potting glue; Step 3, placing the transition section of the quench detection line from the point where the quench detection line passes through the magnet insulation layer to the box body between the two self-fusing tapes for compression and sealing, and coating a silicone layer on the surface of the self-fusing tape, wherein the self-fusing tape is made of silicone material; Step 4: Place all components involved in the processing of the entire quench detection line in steps 1, 2 and 3 into a closed mold for vacuum pressure impregnation, wherein the vacuum pressure impregnation temperature ranges from 135 to 150° C., the impregnation pressure is 0.2 MPa, and the impregnation time is 24 hours.
2. A superconducting magnet quench detection line protection method under vacuum pressure impregnation according to claim 1, characterized in that: The quench detection line is a high-voltage line with an outer diameter of 2.8 mm. The high-voltage line is made of multiple strands of silver-plated copper wires twisted at a certain pitch into a core wire with a diameter of 1.0 mm. The core wire insulation layer is a polyimide extruded sheath. The quench detection line insulation is resistant to radiation of 2000 Mrad and serves in the 4K~300K temperature range.
3. A superconducting magnet quench detection line protection method under vacuum pressure impregnation according to claim 2, characterized in that: The heat shrinkable tube is a polyolefin tube with a diameter of 3.0 mm, a shrinkage rate between 50% and 70%, and a high temperature resistance of 300°C. The length N of the heat shrinkable tube is 400 mm. The quench detection line covered with 200 mm heat shrinkable tube is left inside the magnet insulation layer, and the remaining quench detection line covered with 200 mm heat shrinkable tube is left outside the magnet insulation layer.
4. A superconducting magnet quench detection line protection method under vacuum pressure impregnation according to claim 3, characterized in that: The unwinding is a process for the quench detection line to pass through the magnet insulation layer. The magnet insulation layer is a composite tape composed of a glass ribbon and a polyimide film tape, which is half-lapped on a superconducting magnet armor or a helium tube for multiple times, injected with resin under vacuum pressure impregnation, and then solidified. The width of the glass ribbon is greater than the width of the polyimide film tape.
5. A superconducting magnet quench detection line protection method under vacuum pressure impregnation according to claim 4, characterized in that: The demoulding cloth has no adhesion to resin and silicone and is resistant to high temperature of 300° C. The demoulding cloth tightly wraps the quench detection wire that is coiled.
6. A method for protecting a superconducting magnet quench detection line under vacuum pressure impregnation according to claim 5, characterized in that: The box body is a metal box body, which is resistant to high temperature of 300°C and has no end cover.
7. A superconducting magnet quench detection line protection method under vacuum pressure impregnation according to claim 6, characterized in that: The silicone thermally conductive potting glue and the silicone layer have fluidity and thermal conductivity when in liquid state, and have toughness and are detachable after being cured.
8. A superconducting magnet quench detection line protection method under vacuum pressure impregnation according to claim 7, characterized in that: The self-fusing tape is a self-fusing silicone tape, which is resistant to high temperatures of 150° C. The transition section of the quench detection line is placed between two pieces of the self-fusing tape for compression and sealing.
Citation Information
Patent Citations
Insulating treatment method for superconducting magnet helium inlet tube
CN109712772A
Insulation process for root body of S bending line of superconduction magnet
CN110504098A
Insulated coil, impregnating equipment of resin, curing equipment of resin, method of resin impregnation and method of curing resin
JP2001189226A
Superconducting Magnet System for Nuclear Magnetic Resonance with High Magnetic Field and High Degree of Homogeneity of Magnetic Field
US20130184158A1
Method of manufacturing a superconducting magnet
US6735848B1