Carbon nano modified material for shield tail sealing and preparation method thereof

By designing suitable mixing equipment, including mixing devices and raw material addition auxiliary devices, efficient mixing of carbon nano-modified materials is achieved, solving the problem of poor mixing effects in the existing technology, and improving material production quality and work efficiency. .

CN118718801APending Publication Date: 2024-10-01CHINA RAILWAY 24TH BUREAU GRP ANHUI ENG CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410819889.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-24
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the existing technology, there is a lack of suitable mixing devices during the preparation process of shield tail sealing carbon nano-modified materials, resulting in poor mixing effects and affecting the efficiency of material modification work.

Method used

An equipment is designed that includes a mixing device, a mixing motor and an auxiliary device for adding raw materials. Efficient mixing is achieved through the mixing rod and auxiliary components, which saves mixing time. When adding modifying reagents, it can be added adaptively according to needs. .

Benefits of technology

It improves the production quality and work efficiency of carbon nano-modified materials, ensures efficient use of resources, and solves the problem of poor mixing effects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118718801A_ABST
    Figure CN118718801A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of macromolecules, in particular to a carbon nano modified material for shield tail sealing and a preparation method thereof, and the carbon nano modified material comprises alkali metals such as magnesium carbonate, calcium carbonate, nickel carbonate, lead carbonate, lithium carbonate, sodium carbonate and potassium carbonate, alkaline earth metal carbonate and a modification reagent. In the material mixing processing process, material mixing processing is carried out through arranged material mixing equipment, the material mixing equipment comprises a material mixing device, a material mixing rod, a raw material adding auxiliary device and an auxiliary assembly, all materials are efficiently mixed through the material mixing equipment, the material mixing time is saved, and the processing benefit is improved; when a modification reagent is added, the modification reagent can be adaptively added according to actual requirements, so that the preparation quality of the carbon nano modified material is improved; therefore, the problem that an adaptive mixing device is lacked in the preparation process of the shield tail sealing carbon nano modified material in the prior art is solved, and the working benefit of preparation of the carbon nano modified material can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of polymer technology, in particular to a carbon nano-modified material for shield tail sealing and a preparation method thereof. Background Art

[0002] Nanocarbon materials refer to carbon materials with at least one dimension of the dispersed phase smaller than 100nm. The dispersed phase can be composed of carbon atoms or heterogeneous atoms (non-carbon atoms), or even nanopores; nanocarbon materials mainly include three types: carbon nanotubes, carbon nanofibers, and nanocarbon spheres.

[0003] The existing Chinese patent document with announcement number CN114622222A discloses an industrial preparation method of carbon nanomaterials; its scheme adopts molten carbonate as the main electrolyte for electrolysis to prepare carbon nanomaterials. By using abundant carbonate as the main electrolyte raw material, the preparation cost of carbon nanomaterials is greatly reduced. At the same time, by pressurizing treatment, the conversion rate of carbon dioxide into carbon nanomaterials is effectively improved.

[0004] When the carbon nanomaterials are modified and prepared under the above scheme and the prior art, the mixing of the raw materials during the production process is usually done by adding the main material first and then adding the individual component raw materials from the top feed port of the mixing container; during this process, the added component materials are mixed slowly with the main material, and most of them accumulate in the top layer of the main material, resulting in poor mixing effect, which has a negative impact on the efficiency of the subsequent modification of the carbon nanomaterials.

[0005] Therefore, we need a carbon nano-modified material for shield tail sealing and a preparation method thereof to solve the problem of lack of a suitable mixing device in the preparation process of carbon nano-modified materials for shield tail sealing under the above-mentioned existing technology, which can improve the efficiency of carbon nano-modified material preparation work. Summary of the invention

[0006] The purpose of the present invention is to provide a carbon nano-modified material for shield tail sealing and a preparation method thereof, so as to solve the problem of lack of a suitable mixing device in the preparation process of carbon nano-modified materials for shield tail sealing under the existing technology proposed in the above background technology, and to improve the efficiency of the preparation of carbon nano-modified materials.

[0007] To achieve the above purpose, the present invention provides the following technical solutions: a carbon nano-modified material for shield tail sealing and a preparation method thereof, comprising alkali metal and alkaline earth metal carbonates such as magnesium carbonate, calcium carbonate, nickel carbonate, lead carbonate, lithium carbonate, sodium carbonate, potassium carbonate, and a modifying agent.

[0008] Preferably, the raw materials are homogenized: first weigh one carbonate by weight, and record it as an electrolytic material after homogenization; then install an anode, a cathode and an electrolyte crucible in a reactor, add the obtained electrolytic material into the electrolyte crucible, and pre-coat the cathode with a nucleating agent material, the reactor is a pressure vessel, and is equipped with a pressurizing device; the electrolytic material is gradually heated, and at the same time, carbon dioxide gas is introduced into the reactor, and the pressurizing device is started to increase the pressure in the bell furnace to 0.1-100MPa to ensure that the atmosphere pressure of the bell furnace is greater than the carbon dioxide partial pressure generated by the decomposition reaction of the carbonate added to the electrolytic material, and continue to heat to 500-880°C, so that the carbonate does not undergo thermal decomposition under the protection of high pressure and carbon dioxide gas and enters a molten state; then the materials are efficiently mixed through a mixing device to save the mixing time and improve the processing efficiency; here, when adding the modifying agent, it is added according to the actual needs to improve the production quality of the carbon nano modified material, and on this basis, no resources will be wasted; the voltage is set to 1.5-2.2V, and the current density is 400-900A / m 2. After the pre-electrolysis lasts for 60 minutes, the voltage is increased to 2-10V, and the current density is increased to 800-12000A / m2, which is continued for 6 hours. During the electrolysis process, the cathode surface will be enriched with deposited carbon products; after the electrolysis is completed, the deposited carbon products are scraped off, crushed into powder, and the obtained powder is subjected to a physical remelting process to melt the deposited carbon product powder, and the obtained molten deposited carbon product powder is put into a centrifugal device for centrifugation to separate the mixed product of deposited carbon and carbonate, and the product obtained by centrifugation is recorded as a product rod; the product rod is cut and separated, and the deposited carbon and carbonate solid parts, as well as the mixed middle layer of deposited carbon and carbonate are taken out respectively, and the three parts are crushed into powder by a crusher respectively, and the deposited carbon powder is the carbon nano-modified material product.

[0009] Preferably, the mixing equipment includes a mixing device, a stirring and mixing motor, a raw material adding auxiliary device and an auxiliary component; a main material feed port is arranged on the top of the mixing device, a discharge port is arranged on the bottom of the mixing device, the stirring and mixing motor is arranged and connected to the mixing device, and the stirring and mixing motor is arranged and connected to the rotating shaft, the rotating shaft extends into the inner cavity of the mixing device, mixing rods are equidistantly arranged on the sides of the rotating shaft, auxiliary inclined surfaces are symmetrically arranged on one side of the mixing rod, raw material adding auxiliary devices are equidistantly arranged on the sides of the mixing device, and the raw material adding auxiliary devices are arranged and connected to the auxiliary component.

[0010] Preferably, the mixing rods are arranged in a ring shape at equal intervals on the rotating shaft, and two mixing rods are arranged as a group.

[0011] Preferably, the raw material adding auxiliary device comprises a feeding tube body, a sealing connecting ring, a connecting pipe mouth, a feeding telescopic control rod, a pushing plunger, a storage barrel, a sealing cover, and a discharge nozzle; the feeding tube body is equidistantly embedded and arranged at the side position of the mixing device, and a sealing connecting ring is fixedly arranged on the feeding tube body, and the sealing connecting ring is fixedly arranged on the side wall of the mixing device by screws, one end of the feeding tube body extends into the inner cavity of the mixing device, and a discharge nozzle is arranged at the end, the connecting pipe mouth is arranged on the feeding tube body, and the connecting pipe mouth is threadedly connected to the barrel mouth of the storage barrel, and a sealing cover is arranged on the storage barrel, the feeding telescopic control rod is fixedly arranged at one end of the feeding tube body, one end of the feeding telescopic control rod extends into the feeding tube body, and a pushing plunger is fixedly arranged at the end, and auxiliary components are equidistantly arranged on the outside of the feeding tube body.

[0012] Preferably, the feeding tube body corresponds to the setting position of the mixing rod.

[0013] Preferably, the pushing plunger slides in the feeding tube body under the driving action of the feeding telescopic control rod.

[0014] Preferably, the auxiliary component comprises a limiting annular groove, a semi-ring body, a docking plate, a rotating auxiliary ball, a reagent holding chamber, a filling nozzle, a fixed body, a movable column needle, a connecting plate, a discharge groove, a blocking ring cone, an auxiliary spring, and an auxiliary convex particle; the limiting annular groove is equidistantly arranged on the outer side wall of the feeding tube body, the two ends of the semi-ring body are symmetrically fixed with docking plates, the inner side wall of the semi-ring body is equidistantly and movably provided with rotating auxiliary balls, the semi-ring body is provided with a reagent holding chamber, the filling nozzle is fixedly arranged on the semi-ring body, and the filling nozzle is connected to the reagent holding chamber. The fixed body is arranged on the semi-ring body, and a discharge groove is arranged in the fixed body, the movable column needle is movably inserted in the discharge groove, and one end of the movable column needle extends to the fixed body, and a connecting plate is fixedly arranged on the end, the blocking ring cone is fixedly arranged on the movable column needle, and the blocking ring cone corresponds to the setting position of the discharge groove and the setting number is the same, auxiliary springs are fixedly arranged on the connecting plate at equal distances, one end of the auxiliary spring is fixedly arranged in the fixed body, the other end of the movable column needle is provided with a conical surface, and auxiliary protrusions are fixedly arranged on the conical surface at equal distances.

[0015] Preferably, the two semi-ring bodies form a movable ring, and the butt joint plates at the ends of the two semi-ring bodies are connected and fixed by screws.

[0016] Preferably, the discharge trough is configured as a cylindrical trough, and the diameter of the discharge trough is smaller than the diameter of the movable cylindrical needle.

[0017] Compared with the prior art, the present invention has the following beneficial effects:

[0018] The shield tail seal carbon nano modified material preparation method designed by the present invention performs mixing processing by means of a mixing device during the mixing process, and the mixing device comprises a mixing device, a mixing rod, and a raw material adding auxiliary device and an auxiliary component, and each material is efficiently mixed through the mixing device, thereby saving the mixing time and improving the processing efficiency; and when adding the modifying agent, it can be added in accordance with the actual needs, thereby improving the production quality of the carbon nano modified material; therefore, the present invention solves the problem of lack of a suitable mixing device in the shield tail seal carbon nano modified material preparation process under the prior art, and can improve the efficiency of the carbon nano modified material preparation work. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 This is a schematic diagram of the structure of the mixing equipment for preparing the shield tail seal carbon nano-modified material of the present invention;

[0020] Figure 2 It is a schematic diagram of the internal structure connection of the mixing equipment of the present invention;

[0021] Figure 3 This is a schematic diagram of the connection between the raw material adding auxiliary device and the auxiliary component structure of the present invention;

[0022] Figure 4 For the present invention Figure 3 A magnified schematic diagram of the local structural connection;

[0023] Figure 5 It is a schematic diagram of the local structural connection of the mixing rod of the present invention;

[0024] Figure 6 It is a partial cross-sectional view of the auxiliary component structure connection of the present invention;

[0025] Figure 7 For the present invention Figure 6 Enlarged schematic diagram of local structural connection.

[0026] In the figure: mixing device 1, main material feed port 2, discharge port 3, stirring mixing motor 4, rotating shaft 5, mixing rod 6, auxiliary inclined surface 7, raw material adding auxiliary device 8, feeding tube body 801, sealing connecting ring 802, connecting pipe mouth 803, feeding telescopic control rod 804, pushing plunger 805, storage barrel 806, sealing cover 807, discharge nozzle 808, auxiliary component 9, limiting annular groove 901, semi-ring body 902, docking plate 903, rotating auxiliary ball 904, reagent accommodating chamber 905, filling nozzle 906, fixed body 907, movable column needle 908, connecting plate 909, discharge trough 910, sealing ring cone 911, auxiliary spring 912, auxiliary convex particle 913. DETAILED DESCRIPTION

[0027] The technical solutions in the embodiments of the present invention are described clearly and completely below. The embodiments of the present invention and all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present invention.

[0028] Example 1: Please refer to Figure 1-Figure 2 and Figure 5 , a carbon nano-modified material for shield tail sealing and a preparation method thereof, including alkali metal and alkaline earth metal carbonates such as magnesium carbonate, calcium carbonate, nickel carbonate, lead carbonate, lithium carbonate, sodium carbonate, potassium carbonate, and a modification reagent.

[0029] Homogenization of raw materials: first weigh one carbonate by weight, and record it as electrolytic material after homogenization; then install an anode, a cathode and an electrolyte crucible in a reactor, add the obtained electrolytic material into the electrolyte crucible, and pre-coat the cathode with a nucleating agent material. The reactor is a pressure vessel equipped with a pressurizing device; gradually heat the electrolytic material, and at the same time, introduce carbon dioxide gas into the reactor, start the pressurizing device to increase the pressure in the bell furnace to 0.1-100MPa to ensure that the atmosphere pressure of the bell furnace is greater than the carbon dioxide partial pressure generated by the decomposition reaction of the carbonate added to the electrolytic material, and continue to heat to 500-880°C, so that the carbonate does not undergo thermal decomposition under the protection of high pressure and carbon dioxide gas and enters a molten state; then, the materials are efficiently mixed through a mixing device to save the mixing time and improve the processing efficiency; here, when adding the modifying agent, it is added according to the actual needs to improve the production quality of the carbon nano modified material, and on this basis, no resources will be wasted; the voltage is set to 1.5-2.2V, and the current density is 400-900A / m 2. After the pre-electrolysis lasts for 60 minutes, the voltage is increased to 2-10V, and the current density is increased to 800-12000A / m2, which is continued for 6 hours. During the electrolysis process, the cathode surface will be enriched with deposited carbon products; after the electrolysis is completed, the deposited carbon products are scraped off, crushed into powder, and the obtained powder is subjected to a physical remelting process to melt the deposited carbon product powder, and the obtained molten deposited carbon product powder is put into a centrifugal device for centrifugation to separate the mixed product of deposited carbon and carbonate, and the product obtained by centrifugation is recorded as a product rod; the product rod is cut and separated, and the deposited carbon and carbonate solid parts, as well as the mixed middle layer of the deposited carbon and carbonate are taken out respectively, and the three parts are crushed into powder by a crusher respectively, and the deposited carbon powder is the carbon nano-modified material product; the mixing device comprises a mixing device 1, a stirring and mixing motor 4 and a raw material mixing device 5; A material adding auxiliary device 8 and an auxiliary component 9; a main material feeding port 2 is arranged on the top of the mixing device 1, and a discharge port 3 is arranged on the bottom of the mixing device 1; the stirring and mixing motor 4 is arranged and connected to the mixing device 1, and the stirring and mixing motor 4 is arranged and connected to the rotating shaft 5, the rotating shaft 5 extends into the inner cavity of the mixing device 1, and mixing rods 6 are equidistantly arranged on the sides of the rotating shaft 5, and auxiliary inclined surfaces 7 are symmetrically arranged on one side of the mixing rod 6; raw material adding auxiliary devices 8 are equidistantly arranged on the sides of the mixing device 1, and the raw material adding auxiliary devices 8 are arranged and connected to the auxiliary component 9; the mixing rods 6 are equidistantly arranged in a ring shape on the rotating shaft 5, and two mixing rods 6 are arranged as a group.

[0030] The problem of lack of a suitable mixing device in the preparation process of the shield tail sealed carbon nano-modified material in the prior art is further solved, and the efficiency of the preparation work of the carbon nano-modified material can be improved.

[0031] Example 2: Based on Example 1, please refer to Figure 2-Figure 4The raw material adding auxiliary device 8 here includes a feeding tube body 801, a sealing connection ring 802, a connecting pipe mouth 803, a feeding telescopic control rod 804, a pushing plunger 805, a storage barrel 806, a sealing cover 807, and a discharge nozzle 808; the feeding tube body 801 is equidistantly embedded and arranged at the side position of the mixing device 1, and a sealing connection ring 802 is fixedly arranged on the feeding tube body 801, and the sealing connection ring 802 is fixedly arranged on the side wall of the mixing device 1 by screws, one end of the feeding tube body 801 extends into the inner cavity of the mixing device 1, and a discharge nozzle 808 is arranged at the end, and the connecting pipe mouth 803 is arranged at the The feeding tube body 801 is connected with the connecting pipe mouth 803 and the tube mouth of the storage barrel 806 by threading. The storage barrel 806 is provided with a sealing cover 807. The feeding telescopic control rod 804 is fixedly set at one end of the feeding tube body 801. One end of the feeding telescopic control rod 804 extends into the feeding tube body 801, and a pushing plunger 805 is fixedly set at the end. Auxiliary components 9 are equidistantly arranged on the outside of the feeding tube body 801; the feeding tube body 801 here corresponds to the setting position of the mixing rod 6; the pushing plunger 805 here slides in the feeding tube body 801 under the driving action of the feeding telescopic control rod 804.

[0032] The problem of lack of a suitable mixing device in the preparation process of the shield tail sealed carbon nano-modified material in the prior art is further solved, and the efficiency of the preparation work of the carbon nano-modified material can be improved.

[0033] Example 3: Based on Example 2, please refer to Figure 3-Figure 4 and Figure 6-Figure 7The auxiliary component 9 here includes a limited annular groove 901, a semi-ring body 902, a docking plate 903, a rotating auxiliary ball 904, a reagent holding chamber 905, a filling nozzle 906, a fixed body 907, a movable column needle 908, a connecting plate 909, a discharge groove 910, a blocking ring cone 911, an auxiliary spring 912, and an auxiliary convex particle 913; the limited annular groove 901 is equidistantly arranged on the outer wall of the feeding tube body 801, and the two ends of the semi-ring body 902 are symmetrically fixed with docking plates 903. The two semi-ring bodies 902 here form a movable ring, and the docking plates 903 at the ends of the two semi-ring bodies 902 are connected and fixed by screws; the semi-ring body 902 The inner wall is equidistantly and movably provided with a rotating auxiliary ball 904, the semi-ring body 902 is provided with a reagent containing chamber 905, the filling nozzle 906 is fixedly provided on the semi-ring body 902, and the filling nozzle 906 is communicated with the reagent containing chamber 905, the fixed body 907 is provided on the semi-ring body 902, and a discharge groove 910 is provided in the fixed body 907, the movable column needle 908 is movably inserted in the discharge groove 910, and one end of the movable column needle 908 extends to the fixed body 907, the discharge groove 910 here is provided as a cylindrical groove, and the diameter of the discharge groove 910 is smaller than the diameter of the movable column needle 908; a connecting plate 909 is fixedly provided at the end, The blocking ring cone 911 is fixedly arranged on the movable column needle 908, and the blocking ring cone 911 corresponds to the setting position of the discharge trough 910 and is arranged in the same number of groups. Auxiliary springs 912 are fixedly arranged on the connecting plate 909 at equal intervals, and one end of the auxiliary spring 912 is fixedly arranged in the fixed body 907. The other end of the movable column needle 908 is provided with a conical surface, and auxiliary protrusions 913 are fixedly arranged on the conical surface at equal intervals. Here, the reaction materials or reagents are transported from the feeding tube body 801 to the mixing device 1 through the raw material adding auxiliary device arranged at equal intervals, so as to avoid the accumulation of materials in a certain layer, and the materials are efficiently mixed through the mixing equipment, thereby saving the mixing time. When the mixing rod 6 is driven to rotate by the stirring mixing motor 4, the mixing rod 6 passes through the movable column needle 908 outside the semi-ring body 902, and the movable column needle 908 is squeezed, so that the blocking of the discharge groove 910 by the blocking ring cone 911 is released, and the reaction reagent or catalyst in the reagent containing chamber 905 can be released. In addition, the auxiliary protrusion 913 arranged at the end of the movable column needle 908 can improve the stability of the mixing rod 6 squeezing the movable column needle 908, and can also enable the movable column needle 908 to scrape and clean the condensed material of the mixing rod 6; the storage barrel 806 arranged here is detachable and can also be replaced with a quantitative barrel for quantitative feeding, which has high working flexibility.

[0034] The problem of lack of a suitable mixing device in the preparation process of the shield tail sealed carbon nano-modified material in the prior art is further solved, and the efficiency of the preparation work of the carbon nano-modified material can be improved.

[0035] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A carbon nano-modified material for shield tail sealing and a preparation method thereof, characterized in that: Including magnesium carbonate, calcium carbonate, nickel carbonate, lead carbonate, lithium carbonate, sodium carbonate, potassium carbonate and other alkali metal, alkaline earth metal carbonates, and modification agents.

2. The method for preparing a carbon nano-modified material for shield tail sealing according to claim 1, characterized in that: Homogenization of raw materials: first weigh one carbonate by weight, and record it as electrolytic material after homogenization; then install an anode, a cathode and an electrolyte crucible in a reactor, add the obtained electrolytic material into the electrolyte crucible, and pre-coat the cathode with a nucleating agent material. The reactor is a pressure vessel equipped with a pressurizing device; gradually heat the electrolytic material, and at the same time, introduce carbon dioxide gas into the reactor, start the pressurizing device to increase the pressure in the bell furnace to 0.1-100MPa to ensure that the atmosphere pressure of the bell furnace is greater than the carbon dioxide partial pressure generated by the decomposition reaction of the carbonate added to the electrolytic material, and continue to heat to 500-880°C, so that the carbonate does not undergo thermal decomposition under the protection of high pressure and carbon dioxide gas and enters a molten state; then, the materials are efficiently mixed through a mixing device to save the mixing time and improve the processing efficiency; here, when adding the modifying agent, it is added according to the actual needs to improve the production quality of the carbon nano modified material, and on this basis, no resources will be wasted; the voltage is set to 1.5-2.2V, and the current density is 400-900A / m 2. After the pre-electrolysis lasts for 60 minutes, the voltage is increased to 2-10V and the current density is increased to 800-12000A / m2 for 6 hours. During the electrolysis process, the cathode surface will be enriched with deposited carbon products; After the electrolysis is completed, the deposited carbon product is scraped off, crushed into powder, and the obtained powder is subjected to a physical re-melting process to melt the deposited carbon product powder. The obtained molten deposited carbon product powder is put into a centrifugal device for centrifugation to separate the mixed product of the deposited carbon and carbonate. The product obtained by centrifugation is recorded as a product rod; the product rod is cut and separated, and the deposited carbon and carbonate solid parts, as well as the intermediate layer mixed with the deposited carbon and carbonate are taken out separately, and the three parts are crushed into powder by a crusher respectively. The deposited carbon powder is the carbon nano-modified material product.

3. The method for preparing a carbon nano-modified material for shield tail sealing according to claim 1, characterized in that: The mixing device comprises a mixing device (1), a stirring and mixing motor (4), a raw material adding auxiliary device (8), and an auxiliary component (9); the mixing device (1) is provided with a main material feeding port (2) at the top, and a material discharge port (3) at the bottom; the stirring and mixing motor (4) is connected to the mixing device (1), and the stirring and mixing motor (4) is connected to a rotating shaft (5); the rotating shaft (5) extends into the inner cavity of the mixing device (1); mixing rods (6) are equidistantly arranged on the side of the rotating shaft (5); auxiliary inclined surfaces (7) are symmetrically arranged on one side of the mixing rod (6); raw material adding auxiliary devices (8) are equidistantly arranged on the side of the mixing device (1); and the raw material adding auxiliary devices (8) are connected to the auxiliary component (9).

4. The method for preparing a carbon nano-modified material for shield tail sealing according to claim 3, characterized in that: The mixing rods (6) are arranged in a ring-like shape at equal intervals on the rotating shaft (5), and two mixing rods (6) are arranged as a group.

5. The method for preparing a carbon nano-modified material for shield tail sealing according to claim 3, characterized in that: The raw material adding auxiliary device (8) comprises a feeding tube body (801), a sealing connection ring (802), a connecting pipe mouth (803), a feeding telescopic control rod (804), a pushing plunger (805), a storage barrel (806), a sealing cover (807), and a discharge nozzle (808); the feeding tube body (801) is equidistantly embedded and arranged at the side position of the mixing device (1), and a sealing connection ring (802) is fixedly arranged on the feeding tube body (801), and the sealing connection ring (802) is fixedly arranged on the side wall of the mixing device (1) by screws, and one end of the feeding tube body (801) extends to the mixing device (1). The feeding device (1) is in the inner cavity, and a discharge nozzle (808) is arranged at the end thereof, the connecting pipe mouth (803) is arranged on the feeding pipe body (801), and the connecting pipe mouth (803) is threadedly connected to the barrel mouth of the storage barrel (806), and a sealing cover (807) is arranged on the storage barrel (806), the feeding telescopic control rod (804) is fixedly arranged at one end of the feeding pipe body (801), one end of the feeding telescopic control rod (804) extends into the feeding pipe body (801), and a pushing plunger (805) is fixedly arranged at the end thereof, and auxiliary components (9) are equidistantly arranged on the outside of the feeding pipe body (801).

6. The method for preparing a carbon nano-modified material for shield tail sealing according to claim 5, characterized in that: The feeding tube body (801) and the mixing rod (6) are arranged at corresponding positions.

7. The method for preparing a carbon nano-modified material for shield tail sealing according to claim 5, characterized in that: The pushing plunger (805) slides in the feeding tube body (801) driven by the feeding telescopic control rod (804).

8. The method for preparing a carbon nano-modified material for shield tail sealing according to claim 3, characterized in that: The auxiliary component (9) comprises a limiting annular groove (901), a semi-ring body (902), a docking plate (903), a rotating auxiliary ball (904), a reagent containing chamber (905), a filling nozzle (906), a fixed body (907), a movable column needle (908), a connecting plate (909), a discharge groove (910), a blocking ring cone (911), an auxiliary spring (912), and an auxiliary convex particle (913); the limiting annular groove (901) is equidistantly arranged on the outer wall of the feeding tube body (801); the docking plates (903) are symmetrically fixedly arranged at both ends of the semi-ring body (902); the inner wall of the semi-ring body (902) is equidistantly and movably provided with a rotating auxiliary ball (904); the semi-ring body (902) is provided with a reagent containing chamber (905); the filling nozzle (906) is fixedly arranged on the semi-ring body (902), and the filling nozzle (906) is connected to the semi-ring body (902). The reagent containing chamber (905) is arranged in communication with each other, the fixed body (907) is arranged on the semi-ring body (902), and a discharge groove (910) is arranged in the fixed body (907), the movable column needle (908) is movably inserted in the discharge groove (910), and one end of the movable column needle (908) extends to the fixed body (907), and a connecting plate (909) is fixedly arranged at the end, the blocking ring cone (911) is fixedly arranged on the movable column needle (908), and the blocking ring cone (911) and the discharge groove (910) are arranged at corresponding positions and have the same number of groups, auxiliary springs (912) are fixedly arranged on the connecting plate (909) at equal intervals, one end of the auxiliary spring (912) is fixedly arranged in the fixed body (907), the other end of the movable column needle (908) is provided with a conical surface, and auxiliary convex particles (913) are fixedly arranged on the conical surface at equal intervals.

9. The method for preparing a carbon nano-modified material for shield tail sealing according to claim 8, characterized in that: The two semi-ring bodies (902) form a movable ring, and the butt joint plates (903) at the ends of the two semi-ring bodies (902) are connected and fixed by screws.

10. The method for preparing a carbon nano-modified material for shield tail sealing according to claim 8, characterized in that: The discharge trough (910) is configured as a cylindrical trough, and the diameter of the discharge trough (910) is smaller than the diameter of the movable cylindrical needle (908).