Die manufacturing method, hot pressing die and hot stamping method
Through the mold making method and the replication technology of the master template and the sub-template, the batch manufacturing of hot pressing molds is realized, which solves the problems of low manufacturing efficiency and high cost in the existing technology, and improves the manufacturing efficiency and precision of the microlens array.
Patent Information
- Application Number
- CN202410889852.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-04
- Publication Date
- 2024-10-01
AI Technical Summary
The existing hot-press mold manufacturing technology has the problems of low manufacturing efficiency and high cost, making it difficult to achieve mass manufacturing of microlens arrays.
Adopt mold making methods, including preparing the master template, flipping the mold to make sub-templates, etching the mold base material, and replicating the micro-nano structure through a photoresist mask to achieve simultaneous etching of multiple mold base materials, reducing damage to the master template and production cost.
The batch manufacturing of hot pressing molds is realized, the manufacturing efficiency is improved, the cost is reduced, the high precision and consistency of the microlens array are ensured, and it is suitable for mass production.
Smart Images

Figure CN118721815A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of hot pressing, and in particular relates to a mold manufacturing method, a hot pressing mold and a hot pressing method. Background Art
[0002] At present, microlens arrays have four basic optical functions: collimation, focusing, illumination and imaging, which makes it widely used in imaging systems, sensor systems, lighting systems, photovoltaic systems, digital light processors and optical communications. The materials of microlenses include: oxide glass, plastic, infrared glass, metal (such as lithium, beryllium), etc. Types of microlenses are as follows: Figure 1 As shown in Figure 2. In recent years, with the development of society and the iteration of technology, the shape accuracy requirements of microlens arrays are getting higher and higher, and the demand is also increasing.
[0003] The manufacturing methods of microlens arrays include thermal reflow, grayscale lithography-etching, laser direct writing, micro-nano 3D printing, hot embossing, etc. Thermal reflow technology can only be applied to specific materials, and it is impossible to manufacture certain complex convex lens shapes; grayscale lithography-etching has high requirements for equipment, and the etching cost is relatively high; laser direct writing has the advantages of large processing area and non-contact processing, but there are problems such as difficulty in curved surface processing and poor surface finish; micro-nano 3D printing can only be applied to specific materials, with relatively low efficiency and poor surface finish. Hot embossing technology has the characteristics of high manufacturing efficiency, high material utilization rate, and simple process. Combined with ultra-precision mold manufacturing technology, it can realize mass production of high-precision free-form surface microlens arrays, and has a high prospect for industrial application.
[0004] However, hot embossing technology is limited by the manufacturing of hot embossing molds. Currently, hot embossing molds are generally manufactured by single-point diamond machining, and only one hot embossing mold can be processed at a time, resulting in low manufacturing efficiency and high cost. Summary of the invention
[0005] The purpose of the embodiments of the present application is to provide a method for manufacturing a mold, aiming to solve the problem of how to mass-produce hot pressing molds and reduce costs.
[0006] To achieve the above purpose, the technical solution adopted in this application is: In a first aspect, a method for making a mold is provided, comprising the following steps: Processing, preparing a master template, and processing a first micro-nano structure on the master template; The mold re-molding includes a first mold re-molding, making a first sub-template on the master template, the first sub-template covers and replicates the first micro-nano structure, and forms a second micro-nano structure on the covering surface of the first sub-template; Etching, making a photoresist mask on the mold substrate, and forming a third micro-nano structure on the photoresist mask according to the second micro-nano structure, and etching the mold substrate and the photoresist mask to etch a fourth micro-nano structure on the mold substrate.
[0007] In some embodiments, the one-time mold remodeling comprises the following steps: S21: mixing the microcast substrate and the cross-linking agent and exhausting the gas to form a first mixed glue; S22: placing a first fixed mold on the mother mold plate, and pouring the first mixed glue after exhaust into the mold cavity of the first fixed mold, so that the first mixed glue covers and fills the first micro-nano structure; S23: curing the first mixed glue to form the first sub-template, wherein the second micro-nano structure is formed on the first sub-template; S24: peeling off the first sub-template from the mother template, and transferring the second micro-nano structure to the photoresist mask to form the third micro-nano structure.
[0008] In some embodiments, the molding step also includes secondary molding, and the secondary molding includes making a second sub-template on the first sub-template, the second sub-template covers and replicates the second micro-nano structure, and forms a fifth micro-nano structure on the covering surface of the second sub-template, the shape of the second micro-nano structure is opposite to the shape of the fifth micro-nano structure, and the fifth micro-nano structure is transferred to the photoresist mask to form the third micro-nano structure.
[0009] In some embodiments, the secondary mold remodeling comprises the following steps: S25: mixing the microcast substrate and the cross-linking agent and exhausting the gas to form a second mixed glue; S26: placing a second fixed mold on the first sub-mold, and pouring the second mixed glue after exhaust into the mold cavity of the second fixed mold, so that the second mixed glue covers and fills the second micro-nano structure; S27: curing the second mixed glue to form the second sub-template, wherein the fifth micro-nano structure is formed on the second sub-template; S28: Peeling the second sub-template off from the first sub-template.
[0010] In some embodiments, the etching comprises the following steps: S31: Spin-coating a photoresist on the mold substrate; S32: using the first sub-template or the second sub-template to imprint the photoresist, so as to imprint the photoresist into a photoresist mask having the third micro-nano structure; S33: dry-etching the mold substrate and the photoresist mask to form the fourth micro-nano structure on the mold substrate.
[0011] In some embodiments, the dry etching includes: placing the photoresist mask and the mold substrate into an etcher, generating plasma using an etching gas, and etching the mold substrate and the photoresist mask using the plasma.
[0012] In some embodiments, the processing step includes using single-point diamond turning to machine the master template to form the first micro-nano structure on the master template.
[0013] In a second aspect, a hot pressing mold is provided, wherein the hot pressing mold is prepared by the mold manufacturing method.
[0014] In a third aspect, a hot stamping method is provided, wherein the hot stamping method uses the hot stamping mold, and the hot stamping method comprises the following steps: Closing the mold, placing the glass element on the loading mold, the loading mold is located below the hot pressing mold, driving the loading mold and the hot pressing mold to close the mold, and the fourth micro-nano structure abuts against the glass element; Heating: heating the glass element to a predetermined temperature; Embossing: applying a predetermined clamping force on the loading mold and the hot pressing mold to transfer and replicate the fourth micro-nano structure to the surface of the glass element, so as to hot-emboss the glass element into a microlens array element; Solidification: reducing the heating power and cooling the microlens array element; Demolding: separating the loading mold and the hot pressing mold, and taking out the microlens array element.
[0015] In some embodiments, the microlens array element is detected, and if the detection result meets a predetermined threshold, the hot pressing mold is determined to be qualified; if the detection result does not meet the predetermined threshold, the shape of the first micro-nano structure is compensated.
[0016] The beneficial effects of the present application are as follows: the mold manufacturing method provided in the embodiment of the present application can manufacture a master template once, and the first sub-template can copy the first micro-nano structure from the master template, and the first sub-template can then transfer the second micro-nano structure to the photoresist mask, which can reduce damage to the master template, and only one master template needs to be prepared, and multiple first sub-templates can copy the first micro-nano structure in turn, effectively reducing the manufacturing cost of the master template, and then the second micro-nano structures on the multiple first sub-templates can be transferred to multiple mold substrates respectively. Through etching technology, multiple mold substrates can be etched simultaneously, thereby making multiple hot pressing molds at the same time, which is efficient and effectively reduces costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the embodiments or exemplary technical descriptions will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0018] Figure 1 It is a schematic diagram of a process for manufacturing a mold provided in an embodiment of the present application; Figure 2 It is a flow chart of a method for manufacturing a mold provided in another embodiment of the present application.
[0019] Among them, the figure marks in the figure are: 11, mother template; 111, first micro-nano structure; 112, second micro-nano structure; 113, third micro-nano structure; 114, fourth micro-nano structure; 115, fifth micro-nano structure; 12, mold substrate; 13, photoresist; 131, photoresist mask; 21, first sub-template; 22, second sub-template; 121, hot pressing mold. DETAILED DESCRIPTION
[0020] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present application.
[0021] It should be noted that when a component is referred to as being "fixed on" or "disposed on" another component, it may be directly on the other component or indirectly on the other component. When a component is referred to as being "connected to" another component, it may be directly or indirectly connected to the other component. The orientation or positional relationship indicated by the terms "upper", "lower", "left", "right", etc. is based on the orientation or positional relationship shown in the accompanying drawings, and is only for the convenience of description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application. For ordinary technicians in this field, the specific meanings of the above terms can be understood according to the specific circumstances. The terms "first" and "second" are only used for the purpose of convenience of description, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features. The meaning of "multiple" is two or more, unless otherwise clearly and specifically defined.
[0022] See also Figure 1 to Figure 2The embodiment of the present application provides a method for making a mold, which is used to make a hot pressing mold 121. The hot pressing mold 121 is used to hot press a glass element, so as to hot press the glass element into a microlens array element. The microlens array element has a plurality of micro-nano structures, and the micro-nano structure refers to a structure with a size of micrometer and / or nanometer. The surface of the micro-nano structure can be a free-form surface, so that a microlens array element with a free-form surface can be processed by the hot pressing mold 121.
[0023] See also Figure 1 to Figure 2 The method for making the mold includes the following steps: S1: Processing, preparing a mother template 11, the material of the mother template 11 can be metal nickel. Processing a first micro-nano structure 111 on the mother template 11; S2: Remolding, including one remolding, one remolding includes making a first sub-template 21 on the mother template 11, the first sub-template 21 covers and replicates the first micro-nano structure 111, and forms a second micro-nano structure 112 on the covered surface of the first sub-template 21; it can be understood that the first micro-nano structure 111 can be accurately replicated and the second micro-nano structure 112 can be formed by the first sub-template 21, and the damage to the mother template 11 during the replication process is low, so that the mother template 11 can be replicated multiple times and meet the predetermined design requirements. The shape of the first micro-nano structure 111 is set opposite to the shape of the second micro-nano structure 112, for example, the first micro-nano structure 111 is a convex spherical shape, and the second micro-nano structure 112 is a concave spherical hole.
[0024] S3: etching, making a photoresist mask 131 on the mold substrate 12, and forming a third micro-nano structure 113 on the photoresist mask 131 according to the second micro-nano structure 112, and etching the mold substrate 12 and the photoresist mask 131 to etch a fourth micro-nano structure 114 on the mold substrate 12.
[0025] It is understandable that the third micro-nano structure 113 can be directly generated by the second micro-nano structure 112, or indirectly generated by the second micro-nano structure 112, and the shape of the third micro-nano structure 113 is directly or indirectly defined by the second micro-nano structure 112. When the second micro-nano structure 112 is a convex micro-nano structure, when the second micro-nano structure 112 is replicated on the photoresist mask 131, the generated third micro-nano structure 113 is a concave micro-nano structure, so that the manufactured hot pressing mold 121 is a concave mold, and when the third micro-nano structure 113 is indirectly embossed on the photoresist mask 131 through the first sub-template 21, the shape of the third micro-nano structure 113 can be the same as the shape of the second micro-nano structure 112, that is, the manufactured hot pressing mold 121 is a convex mold, which is not limited here and can be selected according to actual conditions.
[0026] See also Figure 1 to Figure 2It can also be understood that the shape of the fourth micro-nanostructure 114 is determined by the shape of the third micro-nanostructure 113 , and the shape of the third micro-nanostructure 113 is the same as that of the fourth micro-nanostructure 114 .
[0027] See also Figure 1 to Figure 2 The mold manufacturing method provided in the embodiment of the present application can reduce the damage to the mother template 11 by manufacturing a mother template 11, and the first sub-template 21 copies the first micro-nano structure 111 from the mother template 11, and the first sub-template 21 then transfers the second micro-nano structure 112 to the photoresist mask 131. Only one mother template 11 needs to be prepared, and multiple first sub-templates 21 can be prepared. The multiple first sub-templates 21 correspond to multiple mold substrates 12 respectively, so that batch manufacturing of hot pressing molds 121 can be carried out, which is efficient and effectively reduces costs.
[0028] See also Figure 1 to Figure 2 Optionally, a plurality of first sub-templates 21 are provided, each of which is replicated with the first micro-nano structure 111 and is formed with the second micro-nano structure 112. The second micro-nano structures 112 on the plurality of first sub-templates 21 are respectively transferred to a plurality of mold substrates 12. Then, through etching technology, the plurality of mold substrates 12 can be etched simultaneously or sequentially, thereby simultaneously making a plurality of hot pressing molds 121, further improving the production efficiency of the hot pressing molds 121 and effectively reducing the cost.
[0029] It can also be understood that when carrying out mass production of microlens array elements, the accuracy of the fourth micronanostructure 114 on the mold substrate 12 can be guaranteed by replicating and transferring the first micronanostructure 111, thereby ensuring that each glass element has consistent optical properties and surface quality in mass production, reducing the defective rate and lowering costs.
[0030] Optionally, the material of the mother template 11 may be metal nickel.
[0031] See also Figure 1 to Figure 2 In some embodiments, a mold remodeling process includes the following steps: S21: mixing the micro-casting substrate and the cross-linking agent and exhausting the gas to form a first mixed glue; the exhausting process can be performed in a vacuum environment to remove bubbles in the first mixed glue.
[0032] S22: cleaning the surface of the mother template 11 processed with the first micro-nano structure 111, placing a first fixed mold on the mother template 11, and pouring the exhausted first mixed glue into the mold cavity of the first fixed mold, so that the first mixed glue covers and fills the first micro-nano structure 111; S23: Curing the first mixed adhesive to form a first sub-template 21, and forming a second micro-nano structure 112 on the first sub-template 21; optionally, baking can be used to cure the first mixed adhesive. The curing temperature range of the first mixed adhesive containing the micro-casting substrate is usually 60 to 80 degrees. The first mixed adhesive is baked and heated to cure the first mixed adhesive into the first sub-template 21. At the same time, the first sub-template 21 replicates the first micro-nano structure 111, and the accuracy and shape of the first micro-nano structure 111 will not be damaged during the replication process.
[0033] S24 : peeling off the first sub-template 21 from the mother template 11 to avoid damaging the second micro-nano structure 112 , and transferring the second micro-nano structure 112 to the photoresist mask 131 to form a third micro-nano structure 113 .
[0034] Optionally, the microcasting substrate can be polydimethylsiloxane (PDMS). Polydimethylsiloxane has excellent elasticity and replication accuracy, can effectively replicate and transfer the first micro-nano structure 111 on the master template 11, and reduce damage to the master template 11. The polydimethylsiloxane material can also ensure the stability and accuracy of the master template 11 during repeated use.
[0035] See also Figure 1 to Figure 2 In some embodiments, the molding step also includes secondary molding, which includes making a second sub-template 22 on the first sub-template 21, the second sub-template 22 covers and replicates the second micro-nano structure 112, and forms a fifth micro-nano structure 115 on the covering surface of the second sub-template 22, the shape of the second micro-nano structure 112 is opposite to the concave-convex shape of the fifth micro-nano structure 115, and the fifth micro-nano structure 115 is transferred to the photoresist mask 131 to form a third micro-nano structure 113.
[0036] It can be understood that the second micro-nano structure 112 is directly copied from the first sub-template 21 through the second sub-template 22, without copying the first micro-nano structure 111 from the mother template 11 through the second sub-template 22. This can not only reduce the damage to the mother template 11 and ensure the accuracy and life of the mother template 11, but also the second micro-nano structure 112 on the first sub-template 21 and the fifth micro-nano structure 115 on the second sub-template 22 have opposite shapes, so that two different hot pressing molds 121 can be prepared respectively through the first sub-template 21 and the second sub-template 22, further reducing the manufacturing cost of the hot pressing mold 121 and improving the manufacturing efficiency. For example, a concave mold can be prepared through the first sub-template 21, and a convex mold can be prepared through the second sub-template 22. Then, the two mold substrates 12 are etched simultaneously, so that two hot pressing molds 121 with different concave and convex shapes can be prepared simultaneously through the production of the mother template 11 once, reducing the etching cost and manufacturing cost.
[0037] Optionally, the PDMS micro-casting technology can perform a first mold re-molding of the master template 11 through the first sub-template 21, or perform a second mold re-molding of the first sub-template 21 through the second sub-template 22. The PDMS micro-casting technology can ensure the stability and accuracy of the first micro-nano structure 111 during replication and transfer, and can produce a hot pressing mold 121 with a complex geometric structure, and can still maintain the shape and performance of the master template 11 after multiple uses.
[0038] At the same time, the secondary mold remaking step can correct the slight errors in the primary mold remaking, making the mold surface structure more perfect.
[0039] Use of elastic material: Polydimethylsiloxane (PDMS) elastic material is used in both the first and second molding processes. PDMS has good flexibility and elasticity, and can adaptively adjust and compensate for small errors in the first molding during the second molding. This adaptability enables better replication and transfer of the second micro-nano structure 112 during the second molding.
[0040] Hierarchical replication: The secondary mold remodeling step can capture and correct minor structural deviations more precisely by further replicating on the basis of the first mold remodeling. In the first mold remodeling, there may be some minor structural imperfections or errors. Through the secondary mold remodeling, these errors can be refined and corrected, so as to obtain a higher precision micro-nano structure on the final mold.
[0041] Surface stress adjustment: During the secondary mold remodeling process, due to the elastic properties of PDMS materials, the surface stress can be redistributed and adjusted during the secondary mold remodeling. This stress adjustment can correct the structural deviation caused by the slight uneven stress distribution in the primary mold remodeling, making the micro-nano structure of the final mold surface more uniform and accurate.
[0042] Reverse replication characteristics of the material: During the secondary mold re-molding, the fifth micro-nano structure 115 of the second sub-template 22 has an opposite concave-convex shape to the second micro-nano structure 112 of the first sub-template 21. This reverse replication characteristic can effectively compensate and correct the slight errors in the primary mold re-molding. The protrusions or depressions that may exist in the primary mold re-molding can be corrected and adjusted through reverse replication during the secondary mold re-molding, thereby improving the surface accuracy of the hot pressing mold 121.
[0043] See also Figure 1 to Figure 2 In some embodiments, the secondary mold remodeling includes the following steps: S25: mixing the microcast substrate and the cross-linking agent and exhausting the gas to form a second mixed glue; S26: placing a second fixed mold on the first sub-mold 21, and pouring the exhausted second mixed glue into the mold cavity of the second fixed mold, so that the second mixed glue covers and fills the second micro-nano structure 112; S27: curing the second mixed adhesive to form a second sub-template 22, and a fifth micro-nano structure 115 is formed on the second sub-template 22; S28: Peeling off the second sub-template 22 from the first sub-template 21.
[0044] Optionally, the microcasting substrate may also be polydimethylsiloxane (PDMS), which has excellent elasticity and replication accuracy and can effectively replicate and transfer the second micro-nano structure 112 on the first sub-template 21 without contacting the mother template 11, thereby reducing damage to the mother template 11.
[0045] See also Figure 1 to Figure 2 In some embodiments, etching comprises the following steps: S31: Spin-coating a photoresist 13 on the mold substrate 12; S32: Use the first sub-template 21 or the second sub-template 22 to imprint the photoresist 13 to process the photoresist 13 layer into a photoresist mask 131 having a third micro-nano structure 113; by pressing the first sub-template 21 or the second sub-template 22 downward to press the photoresist 13 and holding it for a certain period of time, the third micro-nano structure 113 is fully formed, and the photoresist 13 is cured to form a photoresist mask 131.
[0046] S33 : using a dry etching method to etch the mold substrate 12 and the photoresist mask 131 , so as to form a fourth micro-nano structure 114 on the mold substrate 12 .
[0047] Optionally, the photoresist 13 may be a nanoimprint glue, and the second micro-nano structure 112 on the first sub-template 21 or the fifth micro-nano structure 115 on the second sub-template 22 is transferred to the photoresist 13 by nanoimprint technology, and a photoresist mask 131 having a third micro-nano structure 113 is formed, and the photoresist mask 131 covers one surface of the mold substrate 12, and finally a fourth micro-nano structure 114 is etched on the surface of the mold substrate 12 by dry etching, and the residual photoresist mask 131 attached to the mold substrate 12 is removed, and finally a hot pressing mold 121 is obtained. Optionally, the photoresist mask 131 and dry etching technology are used to make the formation of the fourth micro-nano structure 114 on the mold substrate 12 more accurate and controllable. The conventional wet etching may introduce uneven etching and contamination phenomena, which will not occur.
[0048] See also Figure 1 to Figure 2 In some embodiments, dry etching includes: placing the photoresist mask 131 and the mold substrate 12 into an etcher, generating plasma using an etching gas, and etching the mold substrate 12 and the photoresist mask 131 using the plasma to etch a fourth micro-nano structure 114 on the mold substrate 12.
[0049] Optionally, plasma is used to perform plasma etching on the photoresist mask 131 and the mold substrate 12 to remove the area on the surface of the mold substrate 12 that needs to be etched and to remove part of the photoresist mask 131. The area where the photoresist mask 131 is relatively thin is first etched to expose the surface of the mold substrate 12 that needs to be etched. As the etching of the photoresist mask 131 continues, the area where the photoresist mask 131 is relatively thick is gradually etched to expose the surface of the mold substrate 12 covered by it. As the surface of the substrate in the area covered by the photoresist mask 131 is exposed, plasma etches the surface of the substrate, and as the etching of the photoresist mask 131 decreases, the etching of the surface of the mold substrate 12 gradually expands to the area covered by the thickest photoresist mask 131, thereby etching a surface micro-nano morphology close to the texture template of the fourth micro-nano structure 114 on the surface of the mold substrate 12.
[0050] Optionally, etching of micro-nano structures with high precision and high aspect ratio can be achieved by dry etching. In addition, by nanoimprinting technology, the second micro-nano structure 112 or the fifth micro-nano structure 115 can be accurately transferred to the photoresist mask 131, ensuring the high fidelity of the micro-nano structure on the final etched hot pressing mold 121, improving the manufacturing accuracy and consistency of the hot pressing mold 121, and being suitable for high-precision requirements in large-scale production.
[0051] Optionally, during the etching process, the etching process can also be monitored in real time by the monitoring system of the machine to ensure that the etching depth and morphology meet the requirements; finally, a solvent (such as acetone) is used to remove the residual photoresist mask 131.
[0052] See also Figure 1 to Figure 2 In some embodiments, the processing step includes using single-point diamond turning to turn the master template 11 to form a first micro-nano structure 111 on the master template 11 .
[0053] Optionally, the shape of the free-form surface microlens array element is determined according to the optical design requirements, and the master template 11 is processed using a single-point diamond according to this, and the first micro-nano structure 111 processed on the master template 11 using the single-point diamond turning technology can obtain extremely high surface finish and processing accuracy. Compared with traditional mechanical processing methods, diamond turning can be processed at nanometer-level precision, ensuring the accuracy and consistency of the first micro-nano structure 111 on the surface of the master template 11.
[0054] See also Figure 1 to Figure 2The present application also proposes a hot pressing mold 121, which is prepared by the above-mentioned mold manufacturing method. The specific steps of the mold manufacturing method refer to the above-mentioned embodiment. Since the hot pressing mold 121 adopts all the technical solutions of all the above-mentioned embodiments, it also has all the beneficial effects brought by the technical solutions of the above-mentioned embodiments, which will not be repeated here one by one.
[0055] Optionally, the material of the hot pressing mold 121 can be silicon carbide, diamond, glassy carbon, tungsten carbide, sapphire, etc., which is not limited here and can be selected according to actual conditions.
[0056] Optionally, the hot pressing mold 121 prepared by the above method has the advantages of high precision, high durability and high efficiency. The mold manufacturing method can be used for batch manufacturing of the hot pressing mold 121, which significantly reduces the manufacturing cost of the hot pressing mold 121.
[0057] The present application also proposes a hot stamping method, which is implemented by the above-mentioned hot stamping mold 121. The specific structure of the hot stamping mold 121 refers to the above-mentioned embodiment. Since the hot stamping method adopts all the technical solutions of all the above-mentioned embodiments, it also has all the beneficial effects brought by the technical solutions of the above-mentioned embodiments, which will not be repeated here one by one.
[0058] See also Figure 1 to Figure 2 In some embodiments, the hot stamping method comprises the following steps: T1: Mold closing, placing the glass element on the loading mold, the loading mold is located below the hot pressing mold 121, driving the loading mold and the hot pressing mold 121 to close the mold, and the fourth micro-nano structure 114 abuts against the glass element; Optionally, the glass element may be a variable refractive index microlens, a refractive index microlens, a convex spherical microlens, a concave spherical microlens, a Fresnel microlens, a composite microlens or a diffractive binary optical microlens, which is not limited here and can be selected according to actual conditions.
[0059] T2: Heating: Heat the glass element to a predetermined temperature; the predetermined temperature is the glass transition point temperature of the glass element, for example, the transition point temperature of optical glass BK7 is about 550 degrees.
[0060] T3: embossing: applying a predetermined clamping force on the material loading mold and the hot pressing mold 121 to transfer and replicate the fourth micro-nano structure 114 to the surface of the glass element, so as to hot-press the glass element into a microlens array element; T4: Solidification: reduce the heating power and cool the microlens array elements; the cooling rate can be selected according to actual conditions and will not be described here.
[0061] T5: Demolding: Separate the loading mold and the hot pressing mold 121, and take out the microlens array element.
[0062] See also Figure 1 to Figure 2 In some embodiments, the microlens array element is detected. If the detection result meets the predetermined threshold, the hot pressing mold 121 is determined to be qualified; if the detection result does not meet the predetermined threshold, the shape of the first micro-nano structure 111 is compensated.
[0063] Optionally, a white light interferometer, a confocal microscope or a step meter is used to measure the surface morphology or contour of the microlens array element with a free-form surface, and the deviation between the designed shape and the measured shape is calculated. If the shape deviation is relatively small, the deviation value is slightly reduced by appropriate process adjustments, such as increasing the hot pressing temperature, or increasing the etching amount in the etching process to improve the process; if the shape deviation is relatively large, shape compensation is required, that is, the shape deviation is added to the designed shape of the master template 11, the shape deviation is compensated for the processing of the master template 11, and the shape accuracy of the microlens array element is verified again to see if it meets the requirements; if it does not meet the requirements, multiple iterations are required to achieve multiple shape compensations.
[0064] Optionally, a detection and feedback mechanism is introduced to ensure that the microlens array elements produced can meet the predetermined quality standards. By compensating the shape of the first micro-nano structure 111, the consistency and accuracy of the hot pressing mold 121 and the product can be further improved, the stability and reliability of the production process are guaranteed, and the production efficiency and product quality are greatly improved.
[0065] The above are only optional embodiments of the present application and are not intended to limit the present application. For those skilled in the art, the present application may have various changes and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application should be included in the scope of the claims of the present application.
Claims
1. A method for making a mold, characterized in that: The steps include: Processing, preparing a master template, and processing a first micro-nano structure on the master template; The mold re-molding includes a first mold re-molding, making a first sub-template on the master template, the first sub-template covers and replicates the first micro-nano structure, and forms a second micro-nano structure on the covering surface of the first sub-template; Etching, making a photoresist mask on the mold substrate, and forming a third micro-nano structure on the photoresist mask according to the second micro-nano structure, and etching the mold substrate and the photoresist mask to etch a fourth micro-nano structure on the mold substrate.
2. The method for making a mold according to claim 1, characterized in that: The one-time mold remodeling comprises the following steps: S21: mixing the microcast substrate and the cross-linking agent and exhausting the gas to form a first mixed glue; S22: placing a first fixed mold on the mother mold plate, and pouring the first mixed glue after exhaust into the mold cavity of the first fixed mold, so that the first mixed glue covers and fills the first micro-nano structure; S23: curing the first mixed glue to form the first sub-template, wherein the second micro-nano structure is formed on the first sub-template; S24: peeling off the first sub-template from the mother template, and transferring the second micro-nano structure to the photoresist mask to form the third micro-nano structure.
3. The method for making a mold according to claim 1, characterized in that: The molding step also includes secondary molding, which includes making a second sub-template on the first sub-template, the second sub-template covering and replicating the second micro-nano structure, and forming a fifth micro-nano structure on the covering surface of the second sub-template, the shape of the second micro-nano structure is opposite to the shape of the fifth micro-nano structure, and transferring the fifth micro-nano structure to the photoresist mask to form the third micro-nano structure.
4. The method for making a mold according to claim 3, characterized in that: The secondary mold remodeling comprises the following steps: S25: mixing the microcast substrate and the cross-linking agent and exhausting the gas to form a second mixed glue; S26: placing a second fixed mold on the first sub-mold, and pouring the second mixed glue after exhaust into the mold cavity of the second fixed mold, so that the second mixed glue covers and fills the second micro-nano structure; S27: curing the second mixed glue to form the second sub-template, wherein the fifth micro-nano structure is formed on the second sub-template; S28: Peeling the second sub-template off from the first sub-template.
5. The method for making a mold according to claim 3, characterized in that: The etching comprises the following steps: S31: Spin-coating a photoresist on the mold substrate; S32: using the first sub-template or the second sub-template to imprint the photoresist, so as to imprint the photoresist into a photoresist mask having the third micro-nano structure; S33: dry-etching the mold substrate and the photoresist mask to form the fourth micro-nano structure on the mold substrate.
6. The method for making a mold according to claim 5, characterized in that: The dry etching includes: placing the photoresist mask and the mold substrate into an etcher, generating plasma using an etching gas, and etching the mold substrate and the photoresist mask using the plasma.
7. The method for making a mold according to any one of claims 1 to 6, characterized in that: The processing step includes using single-point diamond turning to machine the master template to form the first micro-nano structure on the master template.
8. A hot pressing mold, characterized in that: The hot pressing mold is prepared by the mold manufacturing method described in any one of claims 1-7.
9. A hot embossing method, characterized in that: The hot stamping method uses the hot stamping mold as claimed in claim 8, and the hot stamping method comprises the following steps: Closing the mold, placing the glass element on the loading mold, the loading mold is located below the hot pressing mold, driving the loading mold and the hot pressing mold to close the mold, and the fourth micro-nano structure abuts against the glass element; Heating: heating the glass element to a predetermined temperature; Embossing: applying a predetermined clamping force on the loading mold and the hot pressing mold to transfer and replicate the fourth micro-nano structure to the surface of the glass element, so as to hot-emboss the glass element into a microlens array element; Solidification: reducing the heating power and cooling the microlens array element; Demolding: separating the loading mold and the hot pressing mold, and taking out the microlens array element.
10. The hot stamping method according to claim 9, characterized in that: The microlens array element is detected. If the detection result meets the predetermined threshold, the hot pressing mold is determined to be qualified; if the detection result does not meet the predetermined threshold, the shape of the first micro-nano structure is compensated.
Citation Information
Patent Citations
Preparation method of three-dimensional micro-lens array
CN112630872A
Preparation method of anti-reflection microlens array
CN115826106A
Microlens array preparation method based on nanoimprint lithography
CN116125569A