Multi-layer composite pipe and preparation method of multi-layer composite pipe
By adopting a multi-layer composite pipe structure in plastic water supply pipes, using adhesive resin melt bonding and double-layer reinforced structure, the problem of insufficient pressure-bearing capacity of plastic pipes is solved, safety and anti-corrosion performance are improved, and higher pressure-bearing capacity and flow stability.
Patent Information
- Application Number
- CN202411230626.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-04
- Publication Date
- 2024-10-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing plastic water supply pipes have limited pressure-bearing capacity and cannot completely replace steel pipes and ductile iron pipes. Their performance is low and they cannot meet the increased safety and environmental protection requirements.
It adopts a multi-layer composite pipe structure, which consists of an inner solid wall pipe, a main reinforcement layer, an auxiliary reinforcement layer, an outer anti-corrosion layer and an outer reinforcement layer from the inside to the outside. It is melt-bonded by adhesive resin and the main reinforcement layer is covered with tape. The reinforcement is wound and formed, the auxiliary reinforcement layer is made of woven material, and an outer reinforcement layer is added to the outer layer to improve the pressure-bearing capacity and anti-corrosion performance.
Through the close combination of the multi-layer composite structure and the double-layer reinforced structure, the pressure-bearing capacity and safety factor of the pipe are improved, the anti-corrosion performance is increased, and extrusion deformation is prevented under the action of external forces, ensuring the liquid flow rate and significantly improving the pipe's overall performance.
Smart Images

Figure CN118721871A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of pipe manufacturing, and in particular to a multi-layer composite pipe and a method for preparing the multi-layer composite pipe. Background Art
[0002] At present, steel pipes, ductile iron pipes, cement pipes, etc. are widely used in water supply pipeline systems. However, with the development and construction, the demand for water supply pipelines has increased. At the same time, with the continuous improvement of requirements for the safety, environmental protection, and service life of pipelines, a new idea of replacing steel with plastics has emerged.
[0003] In recent years, the application of plastic pipes in construction and municipal engineering fields has continued to increase, mainly PE solid wall water pipes. However, due to the limited pressure bearing capacity of PE solid wall water pipes and the fact that the pressure bearing capacity continues to decrease as the pipe diameter increases, it is impossible to completely replace steel pipes, ductile iron pipes, etc. in terms of performance. Summary of the invention
[0004] The main purpose of the present application is to provide a multi-layer composite pipe and a method for preparing the multi-layer composite pipe, aiming to solve the problem of low performance of plastic water supply pipes in the prior art.
[0005] To achieve the above objectives, the technical solutions adopted in this application are as follows: In the first aspect, an embodiment of the present application provides a multi-layer composite pipe, which includes, from the inside to the outside, an inner solid wall pipe, a main reinforcement layer, an auxiliary reinforcement layer, an outer anti-corrosion layer and an outer reinforcement layer. The inner solid wall pipe, the main reinforcement layer, the auxiliary reinforcement layer and the outer anti-corrosion layer are melt-bonded with an adhesive resin, the main reinforcement layer is formed by winding a tape-like reinforcement body, and the auxiliary reinforcement layer is formed by weaving a woven material.
[0006] In a possible implementation of the first aspect, the main reinforcement layer is formed by spirally winding a rubber-coated tape-shaped reinforcement body around an inner solid wall tube in one direction or two directions.
[0007] In a possible implementation manner of the first aspect, the material of the rubber-coated tape-shaped reinforcement is a steel tape, a mesh steel tape, or a fiber braided winding tape.
[0008] In a possible implementation manner of the first aspect, the rubber-coated tape-shaped reinforcement is compositely formed of multiple strands of filamentary reinforcements.
[0009] In a possible implementation manner of the first aspect, the filamentary reinforcement is made of steel fiber, steel wire, glass fiber, basalt fiber or carbon fiber.
[0010] In a possible implementation manner of the first aspect, the width of the adhesive-coated tape-shaped reinforcement is not less than 1 centimeter.
[0011] In a possible implementation of the first aspect, the auxiliary reinforcement layer is formed by braiding a braided material that is alternately braided around the inner solid wall tube and interlocked with each other, and the braided material includes steel wire, carbon fiber wire or rope.
[0012] In a possible implementation manner of the first aspect, the material of the outer reinforcement layer is PVC resin or engineering plastic.
[0013] In a possible implementation of the first aspect, the inner solid wall tube and the outer anti-corrosion layer are made of high-density polyethylene.
[0014] In a second aspect, an embodiment of the present application provides a method for preparing a multilayer composite pipe for a composite material bonding process, which is used to prepare a multilayer composite pipe as provided in any one of the first aspects above, comprising the following steps: The molten high-density polyethylene passes through a vacuum sizing cooling water tank to form an inner solid wall tube; The pipe passes through the winding equipment, and the tape-shaped reinforcement is wound onto the surface of the inner solid wall pipe at a specified angle to form the main reinforcement layer; The pipe passes through the braiding equipment, and the braided material is stacked up and down and braided on the main reinforcement layer at a specified angle to form an auxiliary reinforcement layer; The pipe passes through a high-frequency device to melt the adhesive resin on the tape-shaped reinforcement body, so as to bond the inner solid wall pipe, the main reinforcement layer and the auxiliary reinforcement layer; The pipe passes through the external plastic coating equipment, where the molten high-density polyethylene is covered on the surface and welded with the adhesive resin to form an external anti-corrosion layer; The pipe is passed through an extrusion device, and a material is coated on the outer anti-corrosion layer to form an outer reinforcement layer to obtain a multi-layer composite pipe.
[0015] Compared with the prior art, the beneficial effects of this application are: A multi-layer composite pipe and a method for preparing the multi-layer composite pipe proposed in the embodiments of the present application, wherein the pipe is designed to be a stacked multi-layer composite pipe, and the layers are melt-bonded with an adhesive resin to ensure close bonding of the composite pipe, fully utilize the characteristics of each layer of material, and use a double-layer reinforcement structure of a main reinforcement layer and an auxiliary reinforcement layer to suppress the axial force and radial force inside the pipe, thereby improving the pressure bearing capacity of the pipe and providing a higher safety factor. An outer anti-corrosion layer is also added to improve its anti-corrosion performance. Furthermore, since an outer reinforcement layer is added to the outermost layer, the pipe has a certain rigidity, and the pipe will not be squeezed and deformed after being subjected to external force, thereby ensuring liquid flow and improving the performance of the pipe in many aspects. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 A schematic diagram of the structure of a multilayer composite pipe provided in an embodiment of the present application; Figure 2A schematic diagram of the structure of the main reinforcement layer in the multi-layer composite pipe provided in an embodiment of the present application; Figure 3 A schematic diagram of the structure of an auxiliary reinforcement layer in a multi-layer composite pipe provided in an embodiment of the present application; Figure 4 A schematic diagram of the structure of a rubber-coated tape-shaped reinforcement in a multi-layer composite pipe provided in an embodiment of the present application; Figure 5 A schematic diagram of the structure of another type of adhesive-coated tape-shaped reinforcement in the multi-layer composite pipe provided in an embodiment of the present application; Figure 6 A schematic diagram of the structure of a rubber-coated tape-shaped reinforcement body formed by composite molding of a filamentary reinforcement body in a multi-layer composite pipe provided in an embodiment of the present application; Figure 7 A schematic diagram of the structure of a belt-shaped reinforcement body using a steel belt in a multi-layer composite pipe provided in an embodiment of the present application; Figure 8 A schematic diagram of the structure of a belt-shaped reinforcement body using a mesh steel belt in a multi-layer composite pipe provided in an embodiment of the present application; Fig. 9 A schematic diagram of the structure of a belt-shaped reinforcement body using a fiber braided winding belt in a multi-layer composite pipe provided in an embodiment of the present application; Fig.10 A schematic diagram of a production device in a method for preparing a multilayer composite pipe for a composite material bonding process provided in an embodiment of the present application; Fig.11 A schematic diagram of the structure of a belt-wrapped wheel in a method for preparing a multilayer composite pipe for a composite material bonding process provided in an embodiment of the present application; Fig.12 A schematic structural diagram of a wire-holding wheel in a method for preparing a multilayer composite pipe for a composite material bonding process provided in an embodiment of the present application; Fig.13 A schematic flow chart of a method for preparing a multilayer composite pipe for a composite material bonding process provided in an embodiment of the present application; Markings in the figure: 1-inner solid wall tube, 2-main reinforcement layer, 3-auxiliary reinforcement layer, 4-outer anti-corrosion layer, 5-outer reinforcement layer, 6-extrusion die, 7-heating coil, 8-extrusion main machine, 9-vacuum sizing cooling water tank, 10-winding equipment, 11-rubber-coated tape-shaped reinforcement, 12-weaving equipment, 13-high frequency equipment, 14-outer plastic coating equipment, 15-extrusion equipment, 16-tape winding wheel, 17-line holding wheel, 111-filamentary reinforcement, 112-ribbon reinforcement. DETAILED DESCRIPTION
[0017] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0018] It should be noted that all directional indications in the embodiments of the present application (such as up, down, left, right, front, back, etc.) are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.
[0019] In this application, unless otherwise clearly specified and limited, the terms "connection", "fixation", etc. should be understood in a broad sense. For example, "fixation" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0020] In addition, if there are descriptions involving "first", "second", etc. in the embodiments of the present application, the descriptions of "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the meaning of "and / or" appearing in the full text includes three parallel schemes. Taking "A and / or B" as an example, it includes scheme A, or scheme B, or a scheme that satisfies both A and B. In addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the ability of ordinary technicians in the field to implement. When the combination of technical solutions is contradictory or cannot be implemented, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection required by this application.
[0021] The present application provides a multi-layer composite pipe, as shown in the attached Figure 1 -Attached Fig. 9 As shown, from inside to outside, it includes: an inner solid wall tube 1, a main reinforcement layer 2, an auxiliary reinforcement layer 3, an outer anti-corrosion layer 4 and an outer reinforcement layer 5. The inner solid wall tube 1, the main reinforcement layer 2, the auxiliary reinforcement layer 3 and the outer anti-corrosion layer 4 are melt-bonded with an adhesive resin, the main reinforcement layer 2 is formed by winding a tape-like reinforcement body 11, and the auxiliary reinforcement layer 3 is formed by weaving a woven material.
[0022] In this embodiment, the pipe is designed as a stacked multi-layer composite pipe, and the layers are melt-bonded with an adhesive resin to ensure the close bonding of the composite pipe. The characteristics of each layer of material are fully utilized. The double-layer reinforcement structure of the main reinforcement layer 2 and the auxiliary reinforcement layer 3 suppresses the axial force and radial force inside the pipe, improves the pressure bearing capacity of the pipe, and has a higher safety factor. An outer anti-corrosion layer 4 is added to improve its anti-corrosion performance. In addition, since an outer reinforcement layer 5 is added to the outermost layer, the pipe has a certain rigidity. After being subjected to external force, the pipe will not be squeezed and deformed, thereby ensuring the liquid flow rate and improving the performance of the pipe in many aspects.
[0023] In one embodiment, as shown in the attached Figure 2 As shown, the main reinforcement layer 2 is formed by spirally winding the rubber-coated tape-shaped reinforcement body 11 around the inner solid wall tube 1 in one direction or two directions, and the angle formed by the rubber-coated tape-shaped reinforcement body 11 and the axial direction of the tube is between 54° and 60°. The rubber-coated tape-shaped reinforcement body 11 can be made of the following Figure 4 The multi-strand filament reinforcement 111 shown in the figure is obtained by composite molding. The adhesive tape reinforcement 11 can also be made of the following Figure 5 The strip reinforcement 112 shown is prepared by applying a layer of adhesive resin on the surface of the filamentary reinforcement 111 and the strip reinforcement 112 through a heated extrusion die 6 to preform a coated strip reinforcement 11 of a specified width. Specifically, the specified width is the width marked with w in the accompanying drawing, which is not less than 1 cm.
[0024] The material of the filamentary reinforcement 111 can be steel fiber, steel wire, glass fiber, basalt fiber or carbon fiber, etc. The material of the tape-shaped reinforcement 11, that is, the tape-shaped reinforcement 112 can be steel belt, mesh steel belt or fiber braided winding belt, such as the attached Figure 6 The figure shows a composite-molded tape-shaped reinforcement 11 of a filamentary reinforcement 111, with Figure 7 The following is a steel belt reinforcement 112, attached Figure 8 The following is a belt-shaped reinforcement body 112 using a mesh steel belt. Fig. 9 Shown is a belt-shaped reinforcement 112 that is a fiber braided wrapped tape.
[0025] In one embodiment, as shown in the attached Figure 3 As shown, the auxiliary reinforcement layer 3 is a woven material that is woven around the inner solid wall tube 1 alternately and interlocked, and is coated on the outside of the main reinforcement layer 2. The woven material includes steel wire, carbon fiber wire or rope, etc. The angle formed by a single strand of woven material and the axial direction of the tube is also designed to be between 54° and 60°.
[0026] In one embodiment, the material of the inner solid wall tube 1 and the outer anti-corrosion layer 4 is high-density polyethylene, i.e. HDPE, which is a white powder or granular product, non-toxic, odorless, with a crystallinity of 80% to 90%, a softening point of 125 to 135°C, and an operating temperature of up to 100°C; the hardness, tensile strength and creep properties are better than those of low-density polyethylene; the wear resistance, electrical insulation, toughness and cold resistance are good; the chemical stability is good, at room temperature, it is insoluble in any organic solvent, and is resistant to corrosion by acids, alkalis and various salts.
[0027] In one embodiment, the material of the outer reinforcement layer 5 is PVC resin or engineering plastics. PVC resin has a physical appearance of white powder, which is non-toxic and odorless. The relative density is 1.35-1.46, and the refractive index is 1.544 (20°C). It is insoluble in water, gasoline, alcohol and vinyl chloride, but soluble in solvents such as acetone, dichloroethane, and xylene. It has high chemical stability and good plasticity. Engineering plastics can be used as engineering materials and plastics to replace metals to manufacture machine parts. Engineering plastics have excellent comprehensive properties, such as high rigidity, low creep, high mechanical strength, good heat resistance, and good electrical insulation. They can be used for a long time in harsh chemical and physical environments, and can replace metals as engineering structural materials.
[0028] Based on the same inventive concept as in the above-mentioned embodiment, the present application also provides a method for preparing a multilayer composite pipe for a composite material bonding process, as shown in the attached Fig.10 -Attached Fig.13 As shown, the method for preparing the multilayer composite pipe provided in the embodiment of the present application includes the following steps: S10: The molten high-density polyethylene passes through a vacuum sizing cooling water tank 9 to form an inner layer solid wall tube 1.
[0029] S20: The pipe passes through the winding device 10, and the coated tape-shaped reinforcement 11 is wound onto the surface of the inner solid wall pipe 1 at a specified angle to form a main reinforcement layer 2.
[0030] S30: The pipe passes through the braiding device 12, and the braided material is stacked up and down and braided on the main reinforcement layer 2 at a specified angle to form an auxiliary reinforcement layer 3.
[0031] S40: The pipe passes through the high-frequency device 13 to melt the adhesive resin on the tape-shaped reinforcement 11, so as to bond the inner solid wall pipe 1, the main reinforcement layer 2 and the auxiliary reinforcement layer 3.
[0032] S50: The pipe passes through the outer coating device 14, where the molten high-density polyethylene is covered on the surface and welded with the adhesive resin to form an outer anti-corrosion layer 4.
[0033] S60: The pipe passes through the extrusion device 15, and a material is coated on the outer anti-corrosion layer 4 to form an outer reinforcement layer 5 to obtain a multi-layer composite pipe.
[0034] The beneficial effects of this embodiment can be referred to the description of the aforementioned multi-layer composite pipe, which will not be repeated here.
[0035] In the specific implementation process, first prepare the filamentary reinforcement 111 and the strip reinforcement 112, arrange the filamentary reinforcement 111 and the strip reinforcement 112 in a straight line, apply a layer of adhesive resin on the surface through the extrusion equipment and the heated extrusion die 6, and preform into a tape-shaped reinforcement 11 with a specified width. The belt-winding wheel 16 is preset on the rotating shaft, and the motor drives the shaft to rotate, and the tape-shaped reinforcement 11 is wound on the belt-winding wheel 16. The belt-winding wheel 16 is as shown in the attached Fig.11 As shown, its rotation direction is unidirectional, that is, as shown in the attached Fig.11 The tape winding reels 16 are prepared to be assembled on the winding device 10 according to a specified number in a clockwise direction or a counterclockwise direction as shown in FIG. 1 , and the number can be set to 1 reel to 8 reels.
[0036] Then the wire wheel 17 is assembled to the braiding device 12 according to the specified number, as shown in the attached Fig.12 As shown, the number of the wire wheels 17 is a multiple of 12, and between 12 reels and 240 reels, the rotation directions of the adjacent wire wheels 17 on the braiding device 12 are opposite, that is, the wire wheels 17 rotate along an "8"-shaped track. The high-strength steel wire is synthesized into a strand according to a specified number of strands, which is formed by continuously winding a strand of steel wire. The number of strands ranges from 1 to 15, and is determined according to the diameter of the steel wire and the pressure grade of the pipe. The tensile strength of the high-strength steel wire is ≥1850MPa, and the diameter of the steel wire ranges from 0.2mm to 1.0mm.
[0037] After the preparation work is completed, production preparation begins: First, the extruder 8 produces a molten high-density polyethylene material. The extruder 8 is equipped with a heating die and a heating ring 7. The heating ring 7 controls the temperature of the heating die to be between 190°C and 235°C, and the temperature of the molten high-density polyethylene material is controlled to be between 150°C and 200°C. The molten high-density polyethylene passes through a vacuum sizing cooling water tank 9 to form an inner solid wall tube 1; The inner solid wall tube 1 passes through the winding device 10, and the tape-shaped reinforcement 11 is wound clockwise or counterclockwise on the surface of the inner solid wall tube 1 at a specified angle to form a main reinforcement layer 2. Figure 2 As shown; The pipe is then passed through a braiding device 12, where the high-strength steel wires are stacked up and down and braided on the main reinforcement layer 2 at a specified angle to form an auxiliary reinforcement layer 3. Figure 3 As shown; The pipe passes through the high-frequency device 13 to fully melt the adhesive resin on the tape-shaped reinforcement 11, so that the inner solid wall pipe 1, the main reinforcement layer 2 and the auxiliary reinforcement layer 3 are bonded together. The heating power of the high-frequency device 13 is ≥15KW, and the temperature range of the molten adhesive resin is controlled to be 100℃-120℃; The pipe passes through the outer coating equipment 14, and the molten high-density polyethylene material is covered on the surface, which is fully welded with the adhesive resin, so that the inner solid wall pipe 1, the main reinforcement layer 2, the auxiliary reinforcement layer 3 and the outer anti-corrosion layer 4 are bonded. The outer coating equipment 14 is also provided with a heating mold and a heating ring. The heating ring controls the temperature of the heating mold at 190°C-235°C, and the temperature of the molten high-density polyethylene material is controlled at 150°C-200°C. The pipe is finally passed through an extrusion device 15, and the PVC resin or engineering plastic is coated with an outer anti-corrosion layer 4 to form an outer reinforcement layer 5, thereby obtaining a multi-layer composite pipe as shown in the attached figure. Figure 1 As shown, engineering plastics can be made of nylon, acrylonitrile butadiene styrene (ABS) and the like.
[0038] It should be noted that, in this article, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or system including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or system. In the absence of further restrictions, an element defined by the sentence "comprises a ..." does not exclude the existence of other identical elements in the process, method, article or system including the element.
[0039] The serial numbers of the above-mentioned embodiments of the present application are for description only and do not represent the advantages or disadvantages of the embodiments.
[0040] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present application should be included in the protection scope of the present application.
Claims
1. A multi-layer composite pipe, characterized in that: From inside to outside, it includes: an inner solid wall tube, a main reinforcement layer, an auxiliary reinforcement layer, an outer anti-corrosion layer and an outer reinforcement layer. The inner solid wall tube, the main reinforcement layer, the auxiliary reinforcement layer and the outer anti-corrosion layer are melt-bonded with an adhesive resin. The main reinforcement layer is formed by winding a tape-like reinforcement body, and the auxiliary reinforcement layer is formed by weaving a woven material.
2. The multi-layer composite pipe according to claim 1, characterized in that: The main reinforcement layer is formed by spirally winding the rubber-coated tape-shaped reinforcement body around the inner solid wall tube in one direction or two directions.
3. The multi-layer composite pipe according to claim 1, characterized in that: The material of the rubber-coated tape-shaped reinforcement is a steel tape, a mesh steel tape or a fiber braided winding tape.
4. The multi-layer composite pipe according to claim 1, characterized in that: The rubber-coated tape-shaped reinforcement is formed by composite molding of multiple strands of filamentary reinforcements.
5. The multi-layer composite pipe according to claim 4, characterized in that: The material of the filamentous reinforcement is steel fiber, steel wire, glass fiber, basalt fiber or carbon fiber.
6. The multi-layer composite pipe according to claim 1, characterized in that: The width of the adhesive-coated tape-shaped reinforcement is not less than 1 cm.
7. The multi-layer composite pipe according to claim 1, characterized in that: The auxiliary reinforcement layer is formed by weaving the braided material around the inner solid wall tube alternately up and down and interlocking with each other, and the braided material includes steel wire, carbon fiber wire or rope.
8. The multi-layer composite pipe according to claim 1, characterized in that: The material of the outer reinforcement layer is PVC resin or engineering plastics.
9. The multi-layer composite pipe according to claim 1, characterized in that: The inner solid wall pipe and the outer anti-corrosion layer are made of high-density polyethylene.
10. A method for preparing a multi-layer composite pipe, characterized in that: The method for preparing the multilayer composite pipe according to any one of claims 1 to 9 comprises the following steps: The molten high-density polyethylene passes through a vacuum sizing cooling water tank to form an inner solid wall tube; The pipe passes through a winding device, and the tape-shaped reinforcement is wound onto the surface of the inner solid wall pipe at a specified angle to form a main reinforcement layer; The pipe passes through a braiding device, and the braided material is stacked up and down and then braided on the main reinforcement layer at a specified angle to form an auxiliary reinforcement layer; The pipe passes through a high-frequency device to melt the adhesive resin on the adhesive tape-shaped reinforcement body, so as to bond the inner solid wall pipe, the main reinforcement layer and the auxiliary reinforcement layer; The pipe passes through an external plastic coating device, where molten high-density polyethylene is covered on the surface and welded with the adhesive resin to form an external anti-corrosion layer; The pipe is passed through an extrusion device, and a material is coated on the outer anti-corrosion layer to form an outer reinforcement layer to obtain a multi-layer composite pipe.
Citation Information
Patent Citations
Multi-layer wound composite tube
CN103712000A
Flexible composite high-pressure delivery pipe
CN104141838A
Glass fiber modification method for enhancing thermoplastic resin
CN109399964A
RTP fiber reinforced flexible plastic composite pipe
CN114962805A
Structure and making method for compound reinforced tube waved by super high molecular weight polythene
CN1221086A