Quartz crucible preparation mold and preparation method
By installing an air suction device and a multi-stage filtration system in the quartz crucible preparation mold, the problem of microparticle adhesion on the inner wall of the quartz crucible is solved and the yield of single crystal silicon production is improved.
Patent Information
- Application Number
- CN202310323439.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-10-01
AI Technical Summary
During the production process of single crystal silicon, micro-particles tend to adhere to the inner wall of the quartz crucible, resulting in an increase in impurities in the silicon raw material. When the first single crystal is pulled, the buds are prone to breakage and the yield rate is reduced.
Design a quartz crucible preparation mold, which contains an air suction device inside the mold body, including multiple air pipes arranged along the outer wall of the quartz crucible, for sucking incompletely melted quartz sand particles during the melting process through a multi-stage filtration device Purify the air flow to reduce particle adhesion and entry into the crucible.
It effectively reduces the adhesion of microparticles on the inner wall of the quartz crucible, improves the quality of crucible preparation, reduces the breakage of single crystals due to heterogeneity, and increases the yield of the first single crystal by 3-5%.
Smart Images

Figure CN118724438A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of quartz crucible preparation, and in particular relates to a quartz crucible preparation mold and a preparation method. Background Art
[0002] In the important method of producing single crystal silicon - CZ, quartz crucible is an important auxiliary material, mainly playing the role of carrying high-temperature silicon melt. Its quality not only affects the crystal growth rate of crystal growth, but also affects the quality of crystal. The characteristics of arc crucible making are that when the arc is interrupted during the melting process, there will be quartz particles on the inner wall of the crucible that are not firm and have no high-temperature bonding, which will dissolve into the silicon liquid during the high-temperature crystal growth process and affect the crystallization.
[0003] Quartz crucibles produced by arc method, during the melting process, quartz sand is vaporized and gathered on the insulation plate. Most of this is due to the deposition of SiO2 high temperature volatiles on the electrode or quartz cover. After the arc is broken, the temperature drops, and the quartz sand solidifies from gas to solid and falls onto the inner surface of the quartz crucible. High-purity quartz powder is loaded into a rotary molding mold that can be tilted at any angle (a graphite mold is inserted into a metal water-cooling jacket)
[0004] By using centrifugal force and manual forming of the forming rod, the rotating device that has formed a crucible shape is rotated back to the electrode rod, and then the electrode is arced and inserted into the formed powder cavity, and the fused quartz that is quickly melted into the shape of a crucible is used, and taken out after cooling, that is, the blank production of a quartz crucible is completed. However, during the melting process, part of the quartz sand at the upper end of the mold is not completely melted (all melting prevents the quartz crucible from adhering to the steel film, and it cannot be taken out after the melting is completed). After the arc is broken, the temperature drops, and during the rotation of the mold, some unmelted quartz sand microparticles will enter the quartz crucible and adhere to the chamfered surface of the top of the inner wall of the quartz crucible. However, the existing pickling process cannot effectively remove the microparticles attached to the surface, and it is very easy to fall into the crucible of the quartz crucible due to heat, forming granular white spots or attachments, so that it is mixed with the molten silicon raw material during the subsequent crystal pulling preparation, resulting in an increase in the impurity content in the silicon raw material, and it is very easy to break the quartz crucible when the first single crystal is pulled, and the yield is reduced. Summary of the invention
[0005] The invention provides a quartz crucible preparation mold and a preparation method, which solves the technical problem in the prior art that micro particles are easily attached to the inner wall of the quartz crucible when preparing the quartz crucible, resulting in the easy occurrence of broken buds when pulling the first single crystal.
[0006] In order to solve at least one of the above technical problems, the technical solution adopted by the present invention is:
[0007] A quartz crucible preparation mold comprises a mold body for carrying the quartz crucible, wherein an air suction device is arranged in the mold body, and the air suction device comprises at least a first air pipe, which is arranged in the mold body near the outer wall periphery of one end of the top of the quartz crucible.
[0008] Furthermore, the tube head of the first gas pipe is arranged close to the chamfer on the inner side of the top of the quartz crucible.
[0009] Furthermore, the first air pipes are evenly arranged along the periphery of the outer wall of the mold body, and the number of the first air pipes is at least 4.
[0010] Furthermore, the height from the first air pipe to the top of the mold body ranges from 10 to 20 mm.
[0011] Furthermore, the air suction device further comprises a second air pipe and a third air pipe located below the first air pipe, the second air pipe is arranged at the straight wall section of the quartz crucible, and the third air pipe is arranged at the bottom of the quartz crucible; the first air pipe, the second air pipe and the third air pipe are all connected to the same main pipe;
[0012] A multi-stage filter net is arranged inside the main pipe.
[0013] Furthermore, the second air pipe and the third air pipe are evenly arranged along the outer wall of the quartz crucible; and the first air pipe and the second air pipe are staggered along the height of the quartz crucible;
[0014] The second gas pipes are arranged in a plurality of rows at intervals along the height of the quartz crucible, and the lowest row is close to the bottom of the quartz crucible.
[0015] Furthermore, the distance between the first gas pipe arranged along the height direction of the quartz crucible and the second gas pipe in the uppermost row ranges from 15 to 30 mm;
[0016] The diameters of the openings of the first air pipe, the second air pipe and the third air pipe are 40-60 mm.
[0017] A method for preparing a quartz crucible, using the mold as described above, comprising the following steps: during melting, turning on the arc and suspending the first air pipe from sucking air, and opening all other air pipes in the air suction device except the first air pipe;
[0018] The arc is disconnected and the first air pipe is opened to inhale air, and all the air pipes in the air inhalation device except the first air pipe continue to inhale air;
[0019] During the entire melting process, the mold body keeps rotating, and the speed of the mold body when the first gas pipe is stopped is different from the speed of the mold body when the first gas pipe is opened.
[0020] Further, the rotation rate of the phantom when the first tracheal inhalation is paused is higher than the rotation rate of the phantom when the first tracheal inhalation is started, and the rotation rate range of the phantom is 62-75 rpm.
[0021] Furthermore, the flow rate of all air pipes in the air suction device is 300-700 L / s.
[0022] The quartz crucible preparation mold designed by the present invention has a simple structure and is easy to control. During melting, the adhesion of microparticles on the inner wall of the quartz crucible can be reduced, and the unmelted quartz sand on the mold body can be quickly extracted, so as to avoid the microparticles entering the quartz crucible due to the rotation and vibration of the mold body when the arc is broken, thereby forming granular white spots or attachments, improving the preparation quality of the quartz crucible, reducing the breaking of the first single crystal due to heterogeneity, and improving the yield of the first single crystal by 3-5%. The present invention also provides a preparation method of a quartz crucible using the mold. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a structural schematic diagram of a quartz crucible preparation mold according to an embodiment of the present invention;
[0024] Figure 2 is a distribution diagram of the air intake device along the outer wall of the quartz crucible according to one embodiment of the present invention;
[0025] Figure 3 is a schematic diagram of a filtering device according to an embodiment of the present invention;
[0026] Figure 4 1 is a distribution diagram of the third gas pipe at the bottom of the quartz crucible according to an embodiment of the present invention.
[0027] In the figure:
[0028] 10. mold body 20. air suction device 21. first air pipe
[0029] 22, second air pipe 23, third air pipe 24, main air pipe
[0030] 30. Quartz crucible 40. Filter device 41. Primary filtration
[0031] 42. Secondary filtration DETAILED DESCRIPTION
[0032] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.
[0033] This embodiment provides a quartz crucible preparation mold, such as Figure 1As shown, it includes a mold body 10 for carrying a quartz crucible 30, and an air suction device 20 for sucking gas and impurities inside the quartz crucible is arranged in the mold body 10. The air suction device 20 includes a plurality of first air pipes 21, a second air pipe 22 and a third air pipe 23, wherein the first air pipe 21 is arranged on the periphery of the outer wall surface of the mold body 10 near the top end of the quartz crucible 30, the second air pipe 22 is arranged on the straight section of the outer wall surface of the quartz crucible 30, and the third air pipe 23 is arranged on the lower bottom surface of the outer wall surface of the quartz crucible 30.
[0034] During the melting process, since the high-purity quartz powder is completely melted, it will prevent the quartz crucible 30 from adhering to the steel mold 10, making it impossible to remove it after melting. Therefore, some quartz sand will not be completely melted in the upper end of the mold 10. After the arc is broken, the temperature decreases, and some unmelted quartz sand will enter the quartz crucible 30 and adhere to its surface during the rotation of the mold 10, especially at the arc surface of the upper end surface of the inner wall of the quartz crucible 30. That is, at the chamfer, there are some dispersed quartz sand particles that are not completely melted. The tube head of the first gas pipe 21 is close to the chamfer on the inner side of the top of the quartz crucible, that is, its position directly corresponds to the outer wall surface where the arc surface of the inner upper end surface of the quartz crucible 30 is located, so that the microparticles at the arc surface of the upper end surface of the quartz crucible 30 can be specifically sucked to completely absorb these microparticles and prevent them from sliding along the inner wall surface of the quartz crucible 30. It can also prevent these dispersed microparticles from forming granular white electricity or attachments inside the quartz crucible 30, thereby improving the preparation quality of the quartz crucible 30.
[0035] The entire suction device 20 has a simple structure and is easy to control. It can reduce the adhesion of microparticles on the inner wall of the quartz crucible during melting, and can quickly extract the unmelted quartz sand on the mold 10, thereby preventing the microparticles from entering the quartz crucible due to the rotation and vibration of the mold 10 when the arc is broken, thereby preventing the formation of granular white spots or attachments, thereby improving the preparation quality of the quartz crucible and reducing the breakage of the single crystal due to heterogeneity.
[0036] like Figure 2 As shown, based on the height of the chamfer at the top of the mold body 10, only one row of first air pipes 21 is arranged around the outer wall of the quartz crucible 30, and the first air pipes 21 are evenly arranged along the periphery of the outer wall of the mold body 10, and the number of the first air pipes 21 is at least 4, ensuring that the microparticles in the four directions of the mold body 10 can be sucked away by the first air pipes 21.
[0037] Preferably, the height range H1 from the first air pipe 21 to the top of the mold body 10 is 10-20 mm, and the end points can be 10 mm, 20 mm, or the distance between them can be 12 mm, 15 mm, 18 mm, etc. The purpose of setting this distance is to improve the suction efficiency of the first air pipe 21. If it is too close to the top of the mold body 10, its adsorption area cannot be completely radiated to the height of the chamfer at the top of the mold body 10. If it is too far, it cannot completely minimize the entry of microparticles into the quartz crucible 30.
[0038] In this embodiment, the second gas pipe 22 and the third gas pipe 23 are both located below the first gas pipe 21, and the second gas pipe 22 is configured in the straight wall section of the quartz crucible 30, and is provided in several rows along the height direction of the quartz crucible 30, and the distance between the second gas pipes 20 in adjacent rows is constant, so as to improve the uniformity of sucking gas and impurities in the quartz crucible 30. The third gas pipe 23 is configured at the bottom of the quartz crucible 30, and is arranged horizontally along the diameter of the bottom of the quartz crucible 30. All the first gas pipes 21 converge into one pipe, all the second gas pipes 22 also converge into one pipe along the height of the quartz crucible 30, and all the scattered gas pipes 23 also converge into the same pipe along the bottom diameter surface of the quartz crucible 30. And all the first gas pipes 21, the second gas pipes 22 and the third gas pipes 23 are connected to the same main pipe 24 through their own pipes.
[0039] Since the first gas pipe 21 mainly absorbs the microparticles on the inner side of the top of the quartz crucible 30, a number of microparticles of different diameters other than gas will be collected in the main pipe 24. To prevent these microparticles from clogging the main pipe 24 during discharge, a multi-stage filtering device 40 is provided inside the main pipe 24 near the outlet.
[0040] like Figure 3 As shown, the filter device 40 is provided with two-stage filtration, namely, a primary filter screen 41 for filtering large particles and a secondary filter screen 42 for filtering tiny particles, and there is a certain gap between the primary filter screen 41 and the secondary filter screen 42. In this embodiment, the primary filter screen 41 is mainly used to filter microparticles with a particle size less than 5 μm, and the secondary filter screen 42 is mainly used to filter microparticles with a particle size less than or equal to 1 μm.
[0041] The second air pipe 22 and the third air pipe 23 are evenly arranged along the outer wall of the quartz crucible; and the first air pipe 21 and the second air pipe 22 are staggered along the height of the quartz crucible, which is not only convenient for distributing the air pipes, but also can more evenly adsorb impurities and air at the top of the quartz crucible 30 and the intersection of the straight sections, and fully process the microparticles in the transition section to improve the effectiveness and reliability of adsorption. All the second air pipes 22 are arranged in the same row along the height of the quartz crucible 30, which is not only convenient for arrangement, but also can ensure the consistency of their adsorption of air and impurities in the quartz crucible 30.
[0042] The second air pipes 22 are arranged in several rows at intervals along the height of the quartz crucible 30, and the second air pipes 22 in the lowest row are arranged near the bottom of the quartz crucible 30, preferably near the arc corner between the straight section of the quartz crucible 30 and the lower bottom surface, in order to ensure that the second air pipes 20 can be arranged along the straight section of the quartz crucible 30 to adsorb the air and impurities inside. Since the arc at the corner between the straight section of the quartz crucible 30 and the lower bottom surface is large, it is impossible to locate the corresponding pipe head to install the air pipe, and the air pipe is preferably arranged at the straight section and the lower bottom surface of the quartz crucible 30.
[0043] Furthermore, the distance H2 between the first air tube 21 and the second air tube 22 in the uppermost row arranged along the height direction of the quartz crucible 30 is in the range of 15-30 mm; in the straight section of the quartz crucible 30, the distance between adjacent second air tubes 22 in the same row arranged along the height direction thereof is uniformly arranged along the height between the second air tubes 22 in the uppermost row and the second air tubes 22 in the lowermost row, and preferably, the height distance H3 between adjacent second air tubes 22 is 10-15 mm.
[0044] like Figure 4 As shown, in the lower bottom surface of the quartz crucible 30, the third gas pipes 23 are arranged at intervals along the diameter direction of the quartz crucible 30, wherein at least one third gas pipe 23 is arranged at the center position of the lower bottom surface, and a plurality of third gas pipes 23 are symmetrically arranged on both sides of the third gas pipe 23 at the middle position.
[0045] Furthermore, the diameters of the openings of the first air pipe 21, the second air pipe 22 and the third air pipe 23 are 40-60 mm, and a pneumatic valve is provided at the opening of each air pipe to ensure that the flow rates of all air pipes are the same.
[0046] A method for preparing a quartz crucible, using the mold as described above, comprises the following steps:
[0047] During melting, the arc is turned on and the first gas pipe 21 is stopped from sucking gas, and all other gas pipes in the suction device 20 except the first gas pipe 21 are opened, that is, the second gas pipe 22 and the third gas pipe 23 are opened.
[0048] The arc is disconnected and the first air pipe 21 is opened to inhale air, and the second air pipe 22 and the third air pipe 23 continue to inhale air, and the rotation speed of the mold body 10 is adjusted.
[0049] During the entire melting process, the mold body 10 rotates continuously, and the speed of the mold body 10 when the first air pipe 21 stops sucking air is different from the speed when the first air pipe 21 is opened, and the second air pipe 22 and the third air pipe 23 in the suction device 20 are continuously opened.
[0050] Further, the rotation rate of the mold body 10 when the first air pipe 21 is stopped for suction is higher than the rotation rate of the mold body 10 when the first air pipe 21 is opened for suction. When the arc is turned on, the rotation rate of the mold body 10 is high, but when suctioning, the rotation rate of the mold body 10 is relatively uniform and constant, and the rotation rate range of the mold body 10 is 62-75 rpm.
[0051] Further, the velocity range of the first air pipe 21, the second air pipe 22 and the third air pipe 23 in the air intake device 20 is 300-700 L / s, preferably 600 L / s.
[0052] The quartz crucible preparation mold designed by the present invention has a simple structure and is easy to control. During melting, the adhesion of microparticles on the inner wall of the quartz crucible can be reduced, and the unmelted quartz sand on the mold body can be quickly extracted, so as to avoid the microparticles entering the quartz crucible due to the rotation and vibration of the mold body when the arc is broken, thereby forming granular white spots or attachments, improving the preparation quality of the quartz crucible, reducing the breaking of the first single crystal due to heterogeneity, and improving the yield of the first single crystal by 3-5%. The present invention also provides a preparation method of a quartz crucible using the mold.
[0053] The above embodiments of the present invention are described in detail, and the contents are only preferred embodiments of the present invention, and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made according to the scope of application of the present invention should still fall within the scope of the patent coverage of the present invention.
Claims
1. A quartz crucible preparation mold, characterized in that: The invention comprises a mold body for carrying a quartz crucible, wherein an air suction device is arranged in the mold body, and the air suction device comprises at least a first air pipe, which is arranged at the periphery of the outer wall surface of the mold body near the top end of the quartz crucible.
2. A quartz crucible preparation mold according to claim 1, characterized in that: The tube head of the first gas tube is arranged close to the chamfer on the inner side of the top of the quartz crucible.
3. A quartz crucible preparation mold according to claim 1 or 2, characterized in that: The first air pipes are evenly arranged along the periphery of the outer wall of the mold body, and the number of the first air pipes is at least 4.
4. A quartz crucible preparation mold according to claim 3, characterized in that: The height from the first air tube to the top of the mold body ranges from 10 to 20 mm.
5. A quartz crucible preparation mold according to any one of claims 1-2 and 4, characterized in that: The air suction device further includes a second air pipe and a third air pipe located below the first air pipe, the second air pipe is arranged at the straight wall section of the quartz crucible, and the third air pipe is arranged at the bottom of the quartz crucible; the first air pipe, the second air pipe and the third air pipe are all connected to the same main pipe; A multi-stage filter net is arranged inside the main pipe.
6. A quartz crucible preparation mold according to claim 5, characterized in that: The second air pipe and the third air pipe are evenly arranged along the outer wall of the quartz crucible; and the first air pipe and the second air pipe are staggered along the height of the quartz crucible; The second gas pipes are arranged in a plurality of rows at intervals along the height of the quartz crucible, and the lowest row is close to the bottom of the quartz crucible.
7. A quartz crucible preparation mold according to claim 6, characterized in that: The distance between the first gas pipe arranged along the height direction of the quartz crucible and the second gas pipe in the uppermost row is in the range of 15-30 mm; The diameters of the openings of the first air pipe, the second air pipe and the third air pipe are 40-60 mm.
8. A method for preparing a quartz crucible, characterized in that: Using the mold according to any one of claims 1 to 7, the steps include: during melting, turning on the arc and suspending the first air pipe from sucking air, and opening all other air pipes in the air suction device except the first air pipe; The arc is disconnected and the first air pipe is opened to inhale air, and all the air pipes in the air inhalation device except the first air pipe continue to inhale air; During the entire melting process, the mold body keeps rotating, and the speed of the mold body when the first gas pipe is stopped is different from the speed of the mold body when the first gas pipe is opened.
9. The method for preparing a quartz crucible according to claim 8, characterized in that: The rotation rate of the phantom when the first tracheal suction is paused is higher than the rotation rate of the phantom when the first tracheal suction is started, and the rotation rate range of the phantom is 62-75 rpm.
10. The method for preparing a quartz crucible according to claim 9, characterized in that: The flow rate of all air pipes in the air suction device is 300-700 L / s.