Method for preparing sulfoxide through silver catalytic oxidation

Through the oxidation reaction of silver catalyst with thioether under mild conditions, the problems of high energy consumption and environmental pollution in the production of dimethyl sulfoxide in the existing technology are solved, and low-cost and high-efficiency preparation is achieved, which is suitable for industrial application.

CN118724770AActive Publication Date: 2024-10-01NANJING TECH UNIV
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410813483.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-24
Publication Date
2024-10-01
Estimated Expiration
2044-06-24

AI Technical Summary

Technical Problem

The existing technology has problems such as high reaction temperature, high energy consumption, long process flow, many by-products, unsafe production and serious environmental pollution when producing dimethyl sulfoxide. Moreover, the preparation of commonly used catalysts is complicated and costly, making it difficult to be suitable for industrialization. Production.

Method used

Use a silver catalyst to react with potassium halogen salt and carrier with thioether under mild conditions, use hydrogen peroxide as the oxidant, control the reaction temperature at 25-45°C, and the reaction time is 3-20 hours to prepare dimethyl sulfoxide or methyl sulfoxide Phenyl sulfoxide.

Benefits of technology

The low-cost, low-risk, high-efficiency preparation of dimethyl sulfoxide is achieved. The process is simple and the catalyst is easy to separate and recover. It is suitable for industrial production, avoids the use of harmful gases, and reduces environmental hazards.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004906889970000031
    Figure BDA0004906889970000031
  • Figure BDA0004906889970000071
    Figure BDA0004906889970000071
  • Figure BDA0004906889970000072
    Figure BDA0004906889970000072
Patent Text Reader

Abstract

The invention relates to a method for preparing sulfoxide through catalytic oxidation of silver, which comprises the following steps: firstly, preparing a loaded silver catalyst, and catalyzing hydrogen peroxide to oxidize thioether under the action of the silver catalyst to prepare sulfoxide. The silver catalyst prepared by the method is high in stability and can be recycled for multiple times. The catalyst can catalyze thioether oxidation to efficiently obtain sulfoxide. The silver catalytic oxidation sulfoxide reaction process has the advantages of high efficiency and high selectivity, and the catalyst is easy to recover and environment-friendly. And the product is easy to separate and has a good industrial application prospect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for preparing sulfoxide by oxidation, and in particular to a method for preparing sulfoxide by oxidation catalyzed by silver. Background Art

[0002] Sulfoxide is not only a commonly used solvent and extractant in organic synthesis experiments, but also widely used in the synthesis of various drugs. It is an important intermediate for medicines, pesticides and expensive materials. The choice of catalyst to efficiently oxidize sulfide to sulfoxide has always been a hot topic in the field of synthesis. Currently, the commonly used catalysts are mainly hydrogen peroxide, metal compounds and halogen compounds.

[0003] Dimethyl sulfoxide (DMSO) is a sulfur-containing organic compound. It is a colorless, odorless, transparent liquid at room temperature. It has the characteristics of high polarity, high hygroscopicity, flammability, and high boiling point aprotic. It is an important organic solvent. Dimethyl sulfoxide is soluble in water, ethanol, acetone, benzene and chloroform. It is a highly polar inert solvent. It is widely used as a solvent and reaction reagent and is known as a "universal solvent". For example, it is used as a processing solvent and spinning solvent in acrylonitrile polymerization, as a synthetic solvent and spinning solvent for polyurethane, and as a synthetic solvent for polyamide, fluorochloroaniline, polyimide and polysulfone. In addition, dimethyl sulfoxide has a high selective extraction ability and can be used as an extraction solvent for separating alkanes from aromatic hydrocarbons. For example, dimethyl sulfoxide can be used for the extraction of aromatic hydrocarbons or butadiene. At the same time, in the pharmaceutical industry, dimethyl sulfoxide is also a permeability protectant that can lower the freezing point of cells, reduce the formation of ice crystals, reduce the damage of free radicals to cells, and change the permeability of biomembranes to electrolytes, drugs, poisons and metabolites. In addition, dimethyl sulfoxide can also be used as capacitor medium, antifreeze, brake fluid and rare metal extractant, etc.

[0004] At present, the method for producing dimethyl sulfoxide is mainly obtained by oxidation of dimethyl sulfide. This method has the problems of high reaction temperature, high energy consumption, long process flow, many by-products, unsafe production, etc., and the pollution to the environment is relatively serious. For example, Qian-You Wang (Angew. Chem. Int. Ed. 2022, 61, e202207130 (7 of 7)) et al. used covalent organic frameworks (COFs) as photocatalysts for toxic chemical degradation to oxidize sulfide and synthesized a new type of crystalline, porous amino-linked porphyrin-based COF (Por-AminalCOF). COF showed high catalytic efficiency for the oxidation of sulfur mustard analog CEES with a t1 / 2 of 5 minutes and 100% selectivity under light irradiation. However, the preparation process of the catalyst is relatively complicated and cannot be put into industrial production on a large scale. Kai Liu and Jiaolong Meng (Org. Process Res. Dev. 2023, 27, 1198-1202) et al. used Fe(NO3)3·9H2O as a catalyst and oxygen as an oxidant to selectively oxidize sulfide to sulfoxide under mild conditions. The catalyst can oxidize sulfide to sulfoxide, but the yield of sulfoxide fluctuates greatly under different reaction conditions, and a relatively high yield and selectivity can only be obtained under the condition that the solvent is acetic acid, and the production cost is relatively high in industrial applications.

[0005] Chinese patent document CN116262715A reports a method: in the presence of a nano-carbon-based material and an optional solvent, a sulfide and an oxidant are contacted to carry out an oxidation reaction to obtain an oxidation reaction product; however, the nano-carbon-based material used in this method is relatively complicated to prepare, has low production efficiency and high cost.

[0006] Chinese patent document CN117088794A reports a method for preparing dimethyl sulfoxide, comprising the following steps: A) preheating and mixing hydrogen sulfide and methanol, and then reacting them under the action of a first catalyst to obtain crude dimethyl sulfide; B) condensing and dehydrating the crude dimethyl sulfide obtained in the above steps, and then performing a separation and purification step to obtain high-purity dimethyl sulfide; C) under the action of a second catalyst, the high-purity dimethyl sulfide obtained in the above steps, an oxidant and a solvent are subjected to an oxidation reaction to obtain crude dimethyl sulfoxide; D) evaporating, removing and separating and purifying the crude dimethyl sulfoxide obtained in the above steps to obtain electronic grade dimethyl sulfoxide. The purity of the dimethyl sulfide prepared by the present invention is greater than 99.99%. However, the steps of the method are relatively complicated.

[0007] Chinese patent document CN202110026130.2 reports a method for preparing methyl phenyl sulfoxide: polyoxometalate is used as a catalyst, put into a reaction vessel, organic solvent and methyl phenyl ether are added to the vessel in sequence, and finally an oxidant is added. After heating and stirring the reaction, methyl phenyl sulfoxide is separated. After the reaction, the polyoxometalate can be filtered out, and recovered after treatment. The recovered polyoxometalate is used for the oxidation reaction of methyl phenyl ether. However, the reaction time of this method is as long as 24 hours and the required temperature is as high as 80°C. Summary of the invention

[0008] The purpose of the present invention is to improve the deficiencies of the prior art and provide a method for preparing sulfoxide by silver-catalyzed oxidation.

[0009] The technical scheme of the present invention is: a method for preparing sulfoxide by silver catalytic oxidation, and the specific steps are as follows: a) preparation of silver catalyst: silver nitrate and a carrier are placed in a container, fully stirred for 2-3 hours, potassium halogen salt is added, stirring is continued for 1-2 hours, and then drying is performed to obtain the silver catalyst; wherein the silver halogen salt in the prepared silver catalyst accounts for 0.1% to 10% of the total mass of the catalyst; b) preparation of sulfoxide: thioether is placed in a container, hydrogen peroxide and the silver catalyst prepared in step a) are added, the reaction temperature is controlled to be 25-45°C, the reaction time is 3-20 hours, and sulfoxide is generated by the silver catalyst, as shown in Formula 1.

[0010] Preferably, the mass ratio of silver nitrate to carrier in step a is 1:(6.7-850); the mass ratio of silver nitrate to potassium halogen salt is 1:(0.4-0.7).

[0011] Preferably, the carrier in step a is silicon oxide, aluminum oxide or titanium oxide.

[0012] Preferably, the potassium halogen salt in step a is potassium chloride, potassium bromide or potassium iodide.

[0013] Preferably, the added mass of the silver catalyst in step b is 1.6%-8.5% of the mass of the thioether.

[0014] Preferably, the ratio of the molar amount of hydrogen peroxide added to the molar amount of thioether in step b is 1:(1.0-1.1).

[0015] Preferably, the sulfide in step b is dimethyl sulfide or methyl phenyl sulfide; the product sulfoxide is preferably dimethyl sulfoxide or methyl phenyl sulfoxide.

[0016]

[0017] Beneficial effects:

[0018] The invention provides a preparation method of a silver catalyst and a method for preparing sulfoxide by oxidation thereof. The method avoids the use of harmful gases, reduces production risks and harm to the environment. The catalyst is stable, efficient and easy to separate. The process is simple and efficient, the conditions are mild, the selectivity is high, the danger is low, and the product is easy to separate. The process has low requirements on equipment, low cost and price, and is suitable for industrial production. DETAILED DESCRIPTION

[0019] Embodiment 1: Preparation of AgCl / SiO2-10% catalyst. Dissolve 10g of silver nitrate in 1000ml of water, wait for it to be completely dissolved, add 67.73g of silicon dioxide, stir for 2 hours, and obtain a mixed solution. Add 6.57g of potassium chloride to the mixed solution, continue stirring for 2 hours, and obtain a mixed solution. Dry the mixed solution in a 120°C oven for 12 hours to obtain a silver chloride catalyst, wherein the mass of silver chloride in the catalyst accounts for 10% of the total mass.

[0020] Embodiment 2: Preparation of AgCl / SiO2-5% catalyst. The amount of silver nitrate added was changed to 10 g, the amount of potassium chloride added was changed to 6.57 g, 152.03 g of silicon dioxide was added, and the remaining operations were as described in Embodiment 1. A silver chloride catalyst was obtained, and the mass of silver chloride in the catalyst accounted for 5% of the total mass.

[0021] Embodiment 3: Preparation of AgCl / SiO2-1% catalyst. The amount of silver nitrate added was changed to 0.5 g, the amount of potassium chloride added was changed to 0.219 g, 41.4 g of silicon dioxide was added, and the remaining operations were as described in Embodiment 1. A silver chloride catalyst was obtained, and the mass of silver chloride in the catalyst accounted for 1% of the total mass.

[0022] Embodiment 4: Preparation of AgCl / SiO2-0.1% catalyst. The amount of silver nitrate added was changed to 0.05 g, the amount of potassium chloride added was changed to 0.0219 g, 41.42 g of silicon dioxide was added, and the remaining operations were as described in Embodiment 1. A silver chloride catalyst was obtained, and the mass of silver chloride in the catalyst accounted for 0.1% of the total mass.

[0023] Embodiment 5: Preparation of AgCl / Al3O2-0.1% catalyst. Dissolve 0.05g of silver nitrate in 1000ml of water, wait for it to be completely dissolved, add 42.05g of aluminum oxide, stir for 3 hours, and obtain a mixed solution A. Add 0.0219g of potassium chloride to the mixed solution, continue stirring and reacting for 2 hours to obtain a mixed solution, dry the mixed solution in an oven at 120°C for 12h, and obtain a silver chloride catalyst, the mass of silver chloride in the catalyst accounting for 0.1% of the total mass.

[0024] Embodiment 6: Preparation of AgCl / TiO2-0.1% catalyst. Dissolve 0.05g of silver nitrate in 1000ml of water, wait until it is completely dissolved, add 42.05g of titanium oxide, stir evenly, and obtain a mixed solution. Add 0.0219g of potassium chloride to the mixed solution, continue stirring and reacting for 1 hour, obtain a mixed solution, dry the mixed solution in an oven at 120°C for 12h, and obtain a silver chloride catalyst, the mass of silver chloride in the catalyst accounts for 0.1% of the total mass.

[0025] Embodiment 7: Preparation of AgBr / TiO2-0.1% catalyst. The amount of silver nitrate added was changed to 0.05 g, the amount of potassium bromide added was 0.035 g, 42.04 g of silicon dioxide was added, and the remaining operations were as described in Embodiment 1. A silver bromide catalyst was obtained, and the mass of silver bromide in the catalyst accounted for 0.1% of the total mass.

[0026] Embodiment 8: Preparation of AgI / TiO2-0.1% catalyst. The amount of silver nitrate added was changed to 0.1 g, the amount of potassium iodide added was 0.049 g, 42.03 g of silicon dioxide was added, and the remaining operations were the same as those described in Embodiment 1. A silver iodide catalyst was obtained, and the mass of silver iodide in the catalyst accounted for 0.1% of the total mass.

[0027] Embodiment 9: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 500 mg of catalyst AgCl / SiO2-10% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.34 g of dimethyl sulfoxide, with a yield of 99%.

[0028] Embodiment 10: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 500 mg of catalyst AgCl / SiO2-5% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.34 g of dimethyl sulfoxide, with a yield of 99%.

[0029] Embodiment 11: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 500 mg of catalyst AgCl / SiO2-1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.34 g of dimethyl sulfoxide with a yield of 99%, as shown in Table 1 below.

[0030] Embodiment 12: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 500 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.34 g of dimethyl sulfoxide, with a yield of 99%, as shown in Table 1 below.

[0031] Embodiment 13: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 500 mg of catalyst AgCl / Al3O2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.08 g of dimethyl sulfoxide, with a yield of 95%.

[0032] Embodiment 14: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 500 mg of catalyst AgCl / TiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 5.76 g of dimethyl sulfoxide, with a yield of 90%.

[0033] Embodiment 15: 6.2 g (100 mmol) of dimethyl sulfide and 12.1 g (110 mmol) of hydrogen peroxide (30%) and 500 mg of catalyst AgBr / TiO2-0.1% were added to a reaction container, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver bromide catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 5.76 g of dimethyl sulfoxide, with a yield of 90%.

[0034] Embodiment 16: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 500 mg of catalyst AgI / TiO2-0.1% were added to a reaction container, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver iodide catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 5.64 g of dimethyl sulfoxide, with a yield of 88%.

[0035] Embodiment 17: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 200 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.28 g of dimethyl sulfoxide with a yield of 98%, as shown in Table 1 below.

[0036] Embodiment 18: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 150 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 5.9 g of dimethyl sulfoxide with a yield of 92%, as shown in Table 1 below.

[0037] Embodiment 19: 6.2 g (100 mmol) of dimethyl sulfide and 1.1 g (100 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.27 g of dimethyl sulfoxide with a yield of 98%, as shown in Table 1 below.

[0038] Table 1: Reaction status of AgCl / SiO2 at different addition amounts and reaction times

[0039]

[0040]

[0041] (TOF indicates the amount of sulfide converted by a single silver catalyst per unit time)

[0042] Embodiment 20: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgBr / TiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 5.63 g of dimethyl sulfoxide, with a yield of 88%.

[0043] Embodiment 21: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgI / TiO2-0.1% were added to a reaction container, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver iodide catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 5.12 g of dimethyl sulfoxide, with a yield of 80%.

[0044] Embodiment 22: 6.2 g (100 mmol) of dimethyl sulfide and 12.1 g (110 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.34 g of dimethyl sulfoxide, with a yield of 99%.

[0045] Embodiment 23: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 5.95 g of dimethyl sulfoxide, with a yield of 93%.

[0046] Embodiment 24: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 20 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 5.76 g of dimethyl sulfoxide, with a yield of 90%.

[0047] Embodiment 25: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 35 degrees for 5 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.08 g of dimethyl sulfoxide, with a yield of 95%.

[0048] Embodiment 26: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 3 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 5.44 g of dimethyl sulfoxide, with a yield of 85%.

[0049] Embodiment 27: 6.2 g (100 mmol) of dimethyl sulfide and 12.1 g (110 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgCl / SiO2-0.1% were added to a reaction container, and the mixture was stirred at 25 degrees for 3 h. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 5.632 g of dimethyl sulfoxide, with a yield of 88%.

[0050] Embodiment 28: 6.2 g (100 mmol) of dimethyl sulfide and 11 g (100 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 20 hours. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.34 g of dimethyl sulfoxide, with a yield of 99%.

[0051] Embodiment 29: 6.2 g (100 mmol) of dimethyl sulfide and 12.1 g (110 mmol) of hydrogen peroxide (30%) and 100 mg of catalyst AgCl / SiO2-0.1% were added to a reaction vessel, and the mixture was stirred at 25 degrees for 20 hours. After the reaction, the silver chloride catalyst was separated by filtration, the solution was extracted with ethyl acetate, the organic phases were combined, and the solvent was evaporated under reduced pressure to obtain 6.34 g of dimethyl sulfoxide, with a yield of 99%.

[0052]

[0053] Embodiment 30: Preparation of methyl phenyl sulfoxide as shown in Formula 2. 6.2 g (50 mmol) of methyl phenyl sulfide, 5.5 g (50 mmol) of hydrogen peroxide (30%), and 500 mg of the catalyst prepared in Embodiment 4 were added to a reaction container, stirred at 45 degrees for 5 h, extracted with ethyl acetate after the reaction, filtered to separate the silver chloride catalyst, and the solvent was evaporated under reduced pressure to obtain 7.23 g of methyl phenyl sulfoxide, with a yield of 95%.

[0054] Embodiment 31: Preparation of methyl phenyl sulfoxide as shown in Formula 2. 6.2 g (50 mmol) of methyl phenyl sulfide, 5.5 g (50 mmol) of hydrogen peroxide (30%), and 100 mg of the catalyst prepared in Embodiment 4 were added to a reaction container, stirred at 45 degrees for 5 hours, extracted with ethyl acetate after the reaction, filtered to separate the silver chloride catalyst, and the solvent was evaporated under reduced pressure to obtain 7.46 g of methyl phenyl sulfoxide, with a yield of 98%.

[0055] Embodiment 32: Preparation of methyl phenyl sulfoxide as shown in Formula 2. 6.2 g (50 mmol) of methyl phenyl sulfide, 6.6 g (60 mmol) of hydrogen peroxide (30%), and 100 mg of the catalyst prepared in Embodiment 4 were added to a reaction container, stirred at 45 degrees for 5 h, extracted with ethyl acetate after the reaction, filtered to separate the silver chloride catalyst, and the solvent was evaporated under reduced pressure to obtain 7.566 g of methyl phenyl sulfoxide, with a yield of 99%.

[0056] The catalyst after washing and drying after the reaction in Implementation Example 19 is reused. The process flow is consistent with the implementation case, and the catalyst recovery and use are as shown in Table 2:

[0057] Table 2:

[0058] Recycling times Dimethyl sulfoxide yield 1 98% 2 98% 3 97% 4 98% 5 97%

[0059] The catalyst washed and dried after the reaction in Implementation Example 31 is reused. The process flow is consistent with the implementation case, and the catalyst recovery and use are shown in Table 3 below:

[0060] Table 3:

[0061] Recycling times Yield of methyl phenyl sulfoxide 1 98% 2 96% 3 94% 4 93% 5 94%

[0062] From the experimental results of catalyst recycling in Table 2 and Table 3, it can be seen that the silver catalyst has good recyclability.

Claims

1. A method for preparing sulfoxide by silver-catalyzed oxidation, the specific steps of which are as follows: a) preparation of a silver catalyst: silver nitrate and a carrier are placed in a container, fully stirred for 2-3 hours, potassium halogen salt is added, stirring is continued for 1-2 hours, and then dried to obtain a silver catalyst; wherein the silver halogen salt in the prepared silver catalyst accounts for 0.1% to 10% of the total mass of the catalyst; b) preparation of sulfoxide: thioether is placed in a container, hydrogen peroxide and the silver catalyst prepared in step a) are added, the reaction temperature is controlled to be 25-45° C., the reaction time is 3-20 hours, and sulfoxide is generated by the silver catalyst.

2. The method according to claim 1, characterized in that The mass ratio of silver nitrate to the carrier in step a is 1:(6.7-850); the mass ratio of silver nitrate to the halogen salt of potassium is 1:(0.4-0.7).

3. The method according to claim 1, characterized in that The carrier in step a is silicon oxide, aluminum oxide or titanium oxide.

4. The method according to claim 1, characterized in that The potassium halogen salt in step a is potassium chloride, potassium bromide or potassium iodide.

5. The method according to claim 1, characterized in that In step b, the sulfide is dimethyl sulfide or methyl phenyl sulfide; and the sulfoxide is dimethyl sulfoxide or methyl phenyl sulfoxide.

6. The method according to claim 1, characterized in that The added mass of the silver catalyst in step b is 1.6%-8.5% of the mass of the thioether.

7. The method according to claim 1, characterized in that The ratio of the added molar amount of hydrogen peroxide to the molar amount of thioether in step b is 1:(1.0-1.1).

Citation Information

Patent Citations

  • Preparation method for sulfoxide and sulphone

    CN102838516A

  • Method for synthesizing sulfoxide from thioether through catalytic oxidation

    CN103664715A

  • Method for preparing sulfoxide and sulfone through water phase oxidation of thioether

    CN108586297A