Method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystallization mother liquor
By using hydrophilic modified silica material adsorbent to separate and purify 5-chloronicotinic acid from the 2-chloronicotinic acid crystallization mother liquor, the problem of resource waste and high wastewater treatment costs is solved, and high-purity 5-chloronicotinic acid is achieved. separation and recycling of resources.
Patent Information
- Application Number
- CN202410812951.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-23
- Publication Date
- 2024-10-01
AI Technical Summary
It is difficult to effectively separate and purify 5-chloronicotinic acid from the 2-chloronicotinic acid crystallization mother liquor with the existing technology, resulting in a waste of resources and high wastewater treatment costs.
Hydrophilic modified silica material is used as the adsorbent to separate 5-chloronicotinic acid from the crystallization mother liquor. High-purity 5-chloronicotinic acid is obtained through drying, solution mixing, adsorption column separation, purification and elution steps. .
It achieves high-purity separation of 5-chloronicotinic acid and resource utilization of crystallization mother liquor, reducing waste liquid treatment costs.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of 5-chloronicotinic acid production, and in particular to a method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor. Background Art
[0002] Nicotinic acid and its derivatives are an important class of organic compounds, which are often used as medicines, pharmaceutical intermediates, hair dyeing auxiliaries, polymer stability, etc. Halogenation of nicotinic acid can produce different halogenated hydrochloric acids, such as bromohydrochloric acid, chlorohydrochloric acid, fluorohydrochloric acid, iodohydrochloric acid, etc. Halogenated nicotinic acid and its derivatives are widely used as intermediates for synthetic drugs because of their pharmacological activities such as antibacterial, hypolipidemic, anti-tuberculosis, and inhibition of platelet metabolism in the blood. 5-Halonicotinic acid and its derivatives have special medicinal activity and chemical properties, which can inhibit the synthesis of bacterial coenzymes; can be used as anti-lipolysis agents to reduce cholesterol in the blood; can inhibit the damage of isoproterenol-tartrate to the myocardium and protect the heart; can synthesize novel brain chemical transmission systems, etc., and have very broad application prospects.
[0003] At present, a large amount of mother liquor is produced in the preparation of 2-chloronicotinic acid, and the mother liquor contains a certain amount of 5-chloronicotinic acid. If it is directly discharged, it will not only waste resources, but also increase the cost of wastewater treatment. Therefore, how to separate and purify 5-chloronicotinic acid from the mother liquor is of great significance. Summary of the invention
[0004] The technical problem to be solved by the present invention is: in view of the deficiencies in the prior art, a method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystallization mother liquor is provided, wherein the method can effectively separate 5-chloronicotinic acid from the crystallization mother liquor and obtain high-purity 5-chloronicotinic acid, thereby realizing the resource utilization of the crystallization mother liquor.
[0005] In order to solve the above technical problems, the technical solution of the present invention is:
[0006] A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor comprises the following steps:
[0007] The mother liquor is dried to obtain crude 5-chloronicotinic acid;
[0008] Dissolve crude 5-chloronicotinic acid in methanol and buffer to obtain a crude solution;
[0009] The crude product solution is separated and purified in an adsorption column filled with hydrophilic modified silica material, and then eluted to collect the eluate containing 5-chloronicotinic acid;
[0010] The 5-chloronicotinic acid-containing eluate is dried in vacuo to obtain 5-chloronicotinic acid.
[0011] Preferably, the buffer solution is a potassium dihydrogen phosphate aqueous solution; further, the concentration of the potassium dihydrogen phosphate aqueous solution is 0.01-0.05 mol / L; further, the volume ratio of the methanol to the potassium dihydrogen phosphate aqueous solution is (70-80):(20-30).
[0012] Preferably, the concentration of the crude solution is 0.01-0.05 mg / ml.
[0013] Preferably, during separation and purification, the loading rate of the crude solution is 0.5-1 ml / min, and the volume ratio of the crude solution to the hydrophilic modified silica material is (1-2):1.
[0014] Preferably, the method for preparing the hydrophilic modified silica material comprises the following steps:
[0015] (1) adding silica gel and 3-aminopropyltriethoxysilane into toluene for modification to obtain amino silica gel;
[0016] (2) Add terephthalic acid, 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide and N-hydroxysuccinimide to deionized water and stir once, then add amino silica gel, stir twice at room temperature, and then dry. The obtained organic modified silica gel is added to a DMF solution of zinc acetate dihydrate to react. After the reaction is completed, the reaction solution is filtered, and the solid is dried to obtain a hydrophilic modified silica material.
[0017] Preferably, in step (1), the mass ratio of the silica gel to 3-aminopropyltriethoxysilane is 5:(2-3).
[0018] Preferably, in step (1), the modification temperature is 90-110° C. and the modification time is 20-30 h.
[0019] Preferably, in step (2), the time for the first stirring treatment and the second stirring treatment is 20-30 hours.
[0020] Preferably, in step (2), the mass ratio of terephthalic acid, 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide, N-hydroxysuccinimide, amino silica gel and zinc acetate dihydrate is (0.1-0.2):(0.5-1):(0.1-0.5):1:(1-2).
[0021] Preferably, in step (2), the reaction temperature is 90-110° C. and the reaction time is 10-20 h.
[0022] Preferably, the eluent used for elution is a mixed solution of methanol, n-butane, n-hexane and water, in which the volume ratio of methanol, n-butane, n-hexane and water is (70-80):(5-10):(5-10):10; the loading speed of the eluent during elution is 1-2 ml / min, and the temperature during elution is 30-40°C.
[0023] Due to the adoption of the above technical solution, the beneficial effects of the present invention are:
[0024] The invention uses the crystallization mother liquor in the production of 2-chloronicotinic acid as a raw material, and then uses a hydrophilically modified silica gel material as an adsorbent. Through the different effects of 5-chloronicotinic acid and impurities and the adsorbent, 5-chloronicotinic acid is separated from the crystallization mother liquor, thereby obtaining high-purity 5-chloronicotinic acid and realizing the recycling of waste liquid.
[0025] The present invention first performs amination on the surface of silica gel to preliminarily improve the hydrophilicity of silica gel, and then in situ coats the Zn-MOF material on the surface of silica gel, greatly increasing the specific surface area of the material while ensuring hydrophilicity. The hydrophilic modification makes the surface of silica gel have more hydrophilic functional groups, increasing the ability to interact with water molecules. 5-chloronicotinic acid and 6-chloronicotinic acid are target molecules in the solution. Due to their different hydrophilicity, 5-chloronicotinic acid is more easily adsorbed on the surface of silica gel, thereby achieving the separation and purification of 5-chloronicotinic acid. DETAILED DESCRIPTION
[0026] In order to more clearly understand the above-mentioned objectives, features and advantages of the present invention, the scheme of the present invention will be further described below. It should be noted that the embodiments of the present invention and the features in the embodiments can be combined with each other without conflict.
[0027] In order to further understand the present invention, preferred embodiments of the present invention are described below in conjunction with examples. However, it should be understood that these descriptions are only for further illustrating the features and advantages of the present invention, rather than limiting the claims of the present invention.
[0028] The average particle size of silica gel in the following examples and comparative examples is 5 μm, and the specific surface area is 100 m 2 The mother liquor described below is the mother liquor of crystallization in the process of synthesizing chloronicotinonitrile by POCl3 chlorination using N-oxo-3-cyanopyridine as raw material, and then synthesizing 2-chloronicotinic acid by alkaline hydrolysis and acid crystallization.
[0029] The preparation method of the hydrophilic modified silica material used in the following examples is specifically as follows:
[0030] (1) Add 5 g of silica gel and 2.6 g of 3-aminopropyltriethoxysilane to 50 ml of toluene, stir and react at 100° C. for 24 h, then cool the reaction solution to room temperature and filter, filter and dry the precipitate to obtain amino silica gel;
[0031] (2) 0.166 g of terephthalic acid, 0.5 g of 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide and 0.3 g of N-hydroxysuccinimide were added to 50 ml of deionized water, and stirred once at room temperature for 24 h. Then, 1 g of amino silica gel was added, and stirred twice at room temperature for 24 h. After drying, the obtained organic modified silica gel was added to a solution consisting of 1.1 g of zinc acetate dihydrate and 50 ml of DMF, and reacted at 100° C. for 12 h. After the reaction was completed, the reaction solution was filtered, and the solid was dried to obtain a hydrophilic modified silica material.
[0032] Example 1
[0033] A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor comprises the following steps:
[0034] The crystallization mother liquor is dried to obtain a crude 5-chloronicotinic acid product;
[0035] A 0.01 mol / L potassium dihydrogen phosphate solution and methanol are mixed at a volume ratio of 3:1 to obtain a solvent, and the above-mentioned crude 5-chloronicotinic acid product is dissolved in the solvent to obtain a crude 5-chloronicotinic acid product solution with a concentration of 0.01 mg / ml;
[0036] The crude product solution is introduced into an adsorption column filled with a hydrophilic modified silica material at a rate of 0.5 ml / min for separation and purification, and the volume ratio of the crude product solution to the hydrophilic modified silica material is 2:1; then, an eluent consisting of methanol, n-butane, n-hexane and deionized water in a volume ratio of 7:1:1:1 is used for elution, the eluent loading rate is 1 ml / min, the elution temperature is 30°C, and the volume ratio of the eluent to the hydrophilic modified silica material is 2:1, and the eluent containing 5-chloronicotinic acid is collected;
[0037] The 5-chloronicotinic acid eluate was vacuum dried to obtain 5-chloronicotinic acid. The purity of the 5-chloronicotinic acid was 98.9% as determined by HPLC.
[0038] Example 2
[0039] A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor comprises the following steps:
[0040] The mother liquor is dried to obtain crude 5-chloronicotinic acid;
[0041] A 0.01 mol / L potassium dihydrogen phosphate solution and methanol are mixed at a volume ratio of 3:1 to obtain a solvent, and the above-mentioned crude 5-chloronicotinic acid product is dissolved in the solvent to obtain a crude 5-chloronicotinic acid product solution with a concentration of 0.01 mg / ml;
[0042] The crude product solution is introduced into an adsorption column filled with a hydrophilic modified silica material at a speed of 1 ml / min for separation and purification, and the volume ratio of the crude product solution to the hydrophilic modified silica material is 2:1; then, an eluent consisting of methanol, n-butane, n-hexane and deionized water in a volume ratio of 7:1:1:1 is used for elution, the eluent loading speed is 1 ml / min, the elution temperature is 30°C, and the volume ratio of the eluent to the hydrophilic modified silica material is 2:1, and the eluent containing 5-chloronicotinic acid is collected;
[0043] The 5-chloronicotinic acid eluate was vacuum dried to obtain 5-chloronicotinic acid. The purity of the 5-chloronicotinic acid was 99.3% as determined by HPLC.
[0044] Example 3
[0045] A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor comprises the following steps:
[0046] The mother liquor is dried to obtain crude 5-chloronicotinic acid;
[0047] A 0.01 mol / L potassium dihydrogen phosphate solution and methanol are mixed at a volume ratio of 3:1 to obtain a solvent, and the above-mentioned crude 5-chloronicotinic acid product is dissolved in the solvent to obtain a crude 5-chloronicotinic acid product solution with a concentration of 0.02 mg / ml;
[0048] The crude product solution is introduced into an adsorption column filled with a hydrophilic modified silica material at a speed of 1 ml / min for separation and purification, and the volume ratio of the crude product solution to the hydrophilic modified silica material is 2:1; then, an eluent consisting of methanol, n-butane, n-hexane and deionized water in a volume ratio of 7:1:1:1 is used for elution, the loading speed of the eluent is 1.5 ml / min, the elution temperature is 30°C, and the volume ratio of the eluent to the hydrophilic modified silica material is 2:1, and the eluent containing 5-chloronicotinic acid is collected;
[0049] The 5-chloronicotinic acid eluate is vacuum dried to obtain 5-chloronicotinic acid. The HPLC spectrum test shows that the purity of the 5-chloronicotinic acid is 99.5%.
[0050] Example 4
[0051] A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor comprises the following steps:
[0052] The mother liquor is dried to obtain crude 5-chloronicotinic acid;
[0053] A 0.01 mol / L potassium dihydrogen phosphate solution and methanol are mixed at a volume ratio of 3:1 to obtain a solvent, and the above-mentioned crude 5-chloronicotinic acid product is dissolved in the solvent to obtain a crude 5-chloronicotinic acid product solution with a concentration of 0.02 mg / ml;
[0054] The crude product solution is introduced into an adsorption column filled with a hydrophilic modified silica material at a speed of 1 ml / min for separation and purification, and the volume ratio of the crude product solution to the hydrophilic modified silica material is 2:1; then, an eluent consisting of methanol, n-butane, n-hexane and deionized water in a volume ratio of 7:1:1:1 is used for elution, the loading speed of the eluent is 2 ml / min, the elution temperature is 30°C, and the volume ratio of the eluent to the hydrophilic modified silica material is 2:1, and the eluent containing 5-chloronicotinic acid is collected;
[0055] The 5-chloronicotinic acid eluate was vacuum dried to obtain 5-chloronicotinic acid. The purity of the 5-chloronicotinic acid was 99.2% as determined by HPLC.
[0056] Example 5
[0057] A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor comprises the following steps:
[0058] The crystallization mother liquor is dried to obtain a crude 5-chloronicotinic acid product;
[0059] A 0.01 mol / L potassium dihydrogen phosphate solution and methanol are mixed in a volume ratio of 3:1 to obtain a solvent, and the above-mentioned crude 5-chloronicotinic acid is dissolved in the solvent to obtain a crude 5-chloronicotinic acid solution with a concentration of 0.03 mg / ml;
[0060] The crude product solution is introduced into an adsorption column filled with a hydrophilic modified silica material at a rate of 0.5 ml / min for separation and purification, and the volume ratio of the crude product solution to the hydrophilic modified silica material is 1:1; then, an eluent consisting of methanol, n-butane, n-hexane and deionized water in a volume ratio of 7:1:1:1 is used for elution, the eluent loading rate is 1 ml / min, the elution temperature is 30°C, and the volume ratio of the eluent to the hydrophilic modified silica material is 2:1, and the eluent containing 5-chloronicotinic acid is collected;
[0061] The 5-chloronicotinic acid eluate was vacuum dried to obtain 5-chloronicotinic acid. The purity of the 5-chloronicotinic acid was 98.5% as determined by HPLC.
[0062] Example 6
[0063] A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor comprises the following steps:
[0064] The crystallization mother liquor is dried to obtain a crude 5-chloronicotinic acid product;
[0065] A 0.01 mol / L potassium dihydrogen phosphate solution and methanol are mixed at a volume ratio of 3:1 to obtain a solvent, and the above-mentioned crude 5-chloronicotinic acid product is dissolved in the solvent to obtain a crude 5-chloronicotinic acid product solution with a concentration of 0.05 mg / ml;
[0066] The crude product solution is introduced into an adsorption column filled with a hydrophilic modified silica material at a speed of 1 ml / min for separation and purification, and the volume ratio of the crude product solution to the hydrophilic modified silica material is 2:1; then, an eluent consisting of methanol, n-butane, n-hexane and deionized water in a volume ratio of 7:1:1:1 is used for elution, the loading speed of the eluent is 1.5 ml / min, the elution temperature is 30°C, and the volume ratio of the eluent to the hydrophilic modified silica material is 2:1, and the eluent containing 5-chloronicotinic acid is collected;
[0067] The 5-chloronicotinic acid eluate was vacuum dried to obtain 5-chloronicotinic acid. The purity of the 5-chloronicotinic acid was 98.3% as determined by HPLC.
[0068] Comparative Example 1
[0069] Compared with Example 1, the concentration of the crude product solution was controlled to be 0.1 mg / ml, and other conditions were the same as those in Example 1.
[0070] After testing, the purity of the obtained 5-chloronicotinic acid was 73.5%. Compared with Example 1, the purity of the product obtained in this comparative example is greatly reduced, which is mainly because the concentration of the crude solution is too high, which exceeds the adsorption capacity of the adsorption column, resulting in mutual interference and overlap between the adsorption of different substances, thereby reducing the separation effect. Therefore, it is necessary to reasonably control the concentration of the crude solution.
[0071] Comparative Example 2
[0072] Compared with Example 1, the loading speed of the crude solution was 0.1 ml / min, and other conditions were the same as those in Example 1.
[0073] After testing, the purity of the obtained 5-chloronicotinic acid was 88.9%. Due to the slow loading speed, the sample stayed on the column for a long time, which increased the chance of unnecessary interaction between impurities and materials in the adsorption column, thereby reducing the purity of the product.
[0074] Comparative Example 3
[0075] Compared with Example 1, silica gel is directly used for adsorption without hydrophilic modification treatment, and other conditions are the same as those in Example 1.
[0076] After testing, the purity of the obtained 5-chloronicotinic acid is 92.5%. Compared with Comparative Example 3, Example 1 performs hydrophilic modification on the silica gel, thereby greatly increasing the interaction between 5-chloronicotinic acid and the material in the crude solution, thereby better separating 5-chloronicotinic acid from other substances, and significantly improving the purity of the product.
[0077] Comparative Example 4
[0078] Compared with Example 1, the silica gel was only modified by amino modification, and the other conditions were the same as those in Example 1.
[0079] After testing, the purity of the obtained 5-chloronicotinic acid is 93.8%. Compared with Comparative Example 4, Example 1 performs hydrophilic modification on the silica gel, thereby greatly increasing the interaction between 5-chloronicotinic acid and the material in the crude solution, thereby better separating 5-chloronicotinic acid from other substances, and significantly improving the purity of the product.
[0080] Specific examples are used herein to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core ideas, including the best mode, and also enable any technician in the field to practice the present invention, including making and using any device or system, and implementing any combined method. It should be pointed out that for ordinary technicians in this technical field, without departing from the principle of the present invention, the present invention can also be improved and modified, and these improvements and modifications also fall within the scope of protection of the claims of the present invention. The scope of patent protection of the present invention is defined by the claims and may include other embodiments that can be thought of by those skilled in the art. If these other embodiments have structural elements similar to the literal expression of the claims, or if they include equivalent structural elements that are not substantially different from the literal expression of the claims, then these other embodiments should also be included in the scope of the claims.
Claims
1. A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor, It is characterized in that The following steps are involved: The mother liquor is dried to obtain crude 5-chloronicotinic acid; Dissolve crude 5-chloronicotinic acid in methanol and buffer to obtain a crude solution; The crude product solution is separated and purified in an adsorption column filled with hydrophilic modified silica material, and then eluted to collect the eluate containing 5-chloronicotinic acid; The 5-chloronicotinic acid-containing eluate is dried in vacuo to obtain 5-chloronicotinic acid.
2. A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor according to claim 1, It is characterized in that Include at least one of the following characteristics: (1) The buffer solution is potassium dihydrogen phosphate aqueous solution; (2) The concentration of the buffer solution is 0.01-0.05 mol / L; (3) The volume ratio of the methanol to the buffer solution is (70-80):(20-30).
3. A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor according to claim 1, It is characterized in that The concentration of the crude solution is 0.01-0.05 mg / ml.
4. A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor according to claim 1, It is characterized in that During separation and purification, the loading speed of the crude solution is 0.5-1 ml / min, and the volume ratio of the crude solution to the hydrophilic modified silica material is (1-2):
1.
5. A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor according to claim 1, It is characterized in that The preparation method of the hydrophilic modified silica material comprises the following steps: (1) adding silica gel and 3-aminopropyltriethoxysilane into toluene for modification to obtain amino silica gel; (2) Add terephthalic acid, 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide and N-hydroxysuccinimide to deionized water and stir once, then add amino silica gel, stir twice at room temperature, and then dry. The obtained organic modified silica gel is added to a DMF solution of zinc acetate dihydrate to react. After the reaction is completed, the reaction solution is filtered, and the solid is dried to obtain a hydrophilic modified silica material.
6. A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor according to claim 5, It is characterized in that In step (1), the mass ratio of the silica gel to 3-aminopropyltriethoxysilane is 5:(2-3).
7. A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor according to claim 5, It is characterized in that In step (1), the modification temperature is 90-110° C. and the modification time is 20-30 h.
8. A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor according to claim 5, It is characterized in that In step (2), the mass ratio of terephthalic acid, 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide, N-hydroxysuccinimide, amino silica gel and zinc acetate dihydrate is (0.1-0.2):(0.5-1):(0.1-0.5):1:(1-2).
9. A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor according to claim 5, It is characterized in that In step (2), the time for the first stirring treatment and the second stirring treatment is 20-30 hours, and / or the reaction temperature is 90-110° C., and the reaction time is 10-20 hours.
10. A method for separating and purifying 5-chloronicotinic acid from 2-chloronicotinic acid crystal mother liquor according to claim 1, It is characterized in that The eluent used for elution is a mixed solution of methanol, n-butane, n-hexane and water, in which the volume ratio of methanol, n-butane, n-hexane and water is (70-80):(5-10):(5-10):10; the loading speed of the eluent during elution is 1-2 ml / min, and the temperature during elution is 30-40°C.