Method and device for calculating N / P ratio of coating and thinning area and computer storage medium

By calculating the thinning contour curve of the battery pole piece and the N/P ratio of the coating thinning area, the problem of thick edges and bulging edges when the edge of the coating area of ​​the lithium-ion battery pole piece is thinned is solved, and the capacity matching and manufacturing efficiency are improved. .

CN118733938APending Publication Date: 2024-10-01QUJING EVE ENERGY CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410864950.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-28
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the existing technology, the edges of the coating area of ​​the lithium-ion battery pole pieces are prone to problems such as thick edges and bulging edges when thinning, resulting in low accuracy in calculating the N/P ratio, which in turn affects the positive and negative electrode capacity matching of the pole pieces. , increasing the risk of insufficient lithium insertion or lithium precipitation.

Method used

By obtaining the pole piece data of the battery pole piece, calculate the thinning curve equation of its thinning profile curve, and calculate the N/P ratio of the coating thinning area based on the thinning curve equation and data, taking into account the pole piece coating data and the thinning curve. Multiple parameters in the thin data include coating area density, roll elongation, active material gram capacity and main material feeding tolerance, etc.

Benefits of technology

It improves the calculation accuracy of the N/P ratio in the thinning area, reduces the problem of insufficient lithium insertion or lithium precipitation caused by the mismatch of positive and negative electrode capacities, and improves the accuracy and manufacturing efficiency of the battery pole piece thinning process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118733938A_ABST
    Figure CN118733938A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of batteries, and discloses a method and device for calculating the N / P ratio of a coating thinned area and a computer storage medium, and the method comprises the steps: obtaining pole piece data of a battery pole piece, calculating a thinned curve equation of a thinned profile curve corresponding to the battery pole piece according to the pole piece data, and calculating the N / P ratio of the coating thinned area according to the thinned curve equation and the pole piece data. And calculating the N / P ratio of the coating and thinning area of the battery pole piece. Therefore, by implementing the method, the accuracy of the calculated N / P ratio can be improved, so that the problem of insufficient lithium precipitation or lithium precipitation of the negative electrode caused by mismatching of positive and negative electrode capacities in a pole piece coating and thinning area is reduced, the control on the accuracy of a battery pole piece thinning process is improved, and the manufacturing efficiency of the battery pole piece is further improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of battery technology, and in particular to a method and device for calculating the N / P ratio of a coating thinning area, and a computer storage medium. Background Art

[0002] Coating is a basic process in the manufacturing process of lithium-ion batteries. Using extrusion coating equipment, one or more layers of positive and negative electrode slurry are evenly coated on aluminum foil or copper foil, and then dried in an oven to obtain the positive and negative electrodes of lithium-ion batteries. However, when using extrusion coating to produce battery electrodes, the edges of the coating area of ​​the electrode are usually prone to abnormalities, such as thick edges, bulging edges, and fluctuations in edge thickness, which seriously affect the processing performance of the electrode. Therefore, it is necessary to thin the edges of the coating area of ​​the electrode.

[0003] In the prior art, the N / P ratio of the thinned area is usually calculated based on the width or thickness of the thinned area, and then the N / P ratio is used to judge whether the thinned area meets the requirements. However, the N / P ratio calculated by these methods usually only considers the width or thickness of the thinned area alone, and the calculated N / P ratio is less accurate, and then the accuracy of judging whether the thinned area meets the requirements is low, resulting in the risk of insufficient lithium insertion or negative electrode lithium deposition in lithium-ion batteries due to the mismatch between the positive and negative electrode capacities in the thinned area. Therefore, it is particularly important to propose a technical solution that can improve the accuracy of calculating the N / P ratio of the thinned area, thereby reducing the risk of insufficient lithium insertion or negative electrode lithium deposition due to the mismatch between the positive and negative electrode capacities in the thinned area. Summary of the invention

[0004] The present invention provides a method and device for calculating the N / P ratio of a coating thinning area, and a computer storage medium, which can help improve the accuracy of calculating the N / P ratio of the thinning area, thereby reducing the risk of insufficient lithium insertion or lithium plating at the negative electrode due to mismatch between the positive and negative electrode capacities in the thinning area.

[0005] In order to solve the above technical problems, the first aspect of the present invention discloses a method for calculating the N / P ratio of the coating thinning area, the method comprising:

[0006] Acquire electrode data of a battery electrode, wherein the battery electrode includes a positive electrode and a negative electrode, and the electrode data includes electrode coating data and electrode thinning data;

[0007] Calculating a thinning curve equation of a thinning profile curve corresponding to the battery electrode piece according to the electrode piece data, wherein the thinning curve equation includes a positive electrode thinning curve equation and a negative electrode thinning curve equation;

[0008] The N / P ratio of the coated thinned area of ​​the battery electrode is calculated based on the thinning curve equation and the electrode data.

[0009] As an optional embodiment, in the first aspect of the present invention, the electrode coating data includes electrode coating surface density, rolling elongation, coating active material gram capacity, coating active material ratio and main material feeding tolerance;

[0010] The calculating the N / P ratio of the coating thinning area of ​​the battery electrode sheet according to the thinning curve equation and the electrode sheet data includes:

[0011] According to the thinning curve equation, calculating the thinning cross-sectional area of ​​the battery electrode sheet, the thinning cross-sectional area includes the positive electrode thinning cross-sectional area and the negative electrode thinning cross-sectional area;

[0012] Calculating the cross-sectional area of ​​the battery electrode sheet coated with active material according to the electrode sheet data and the thinned cross-sectional area of ​​the battery electrode sheet;

[0013] The N / P ratio of the coated thinned area of ​​the battery electrode is calculated based on the electrode coating data and the cross-sectional area of ​​the coated active material.

[0014] As an optional implementation, in the first aspect of the present invention, the pole piece coating data further includes pole piece coating thickness, and the pole piece thinning data includes pole piece thinning width;

[0015] The step of calculating the cross-sectional area of ​​the battery electrode sheet coated with the active material according to the electrode sheet data and the thinned cross-sectional area of ​​the battery electrode sheet comprises:

[0016] Determine a thinning area judgment value corresponding to the battery electrode piece, and calculate a maximum thickness of the thinning area corresponding to the battery electrode piece according to the electrode piece coating thickness and the thinning area judgment value;

[0017] The cross-sectional area of ​​the battery electrode coated with the active material is calculated according to the electrode sheet thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area.

[0018] As an optional implementation, in the first aspect of the present invention, the thinning curve equation for calculating the thinning profile curve corresponding to the battery electrode sheet according to the electrode sheet data includes:

[0019] Determine at least two coordinate points of a thinning profile curve corresponding to the battery electrode according to the electrode coating data and the electrode thinning data;

[0020] A thinning curve equation of a thinning profile curve corresponding to the battery electrode sheet is calculated based on at least two of the coordinate points.

[0021] As an optional implementation, in the first aspect of the present invention, the pole piece thinning data further includes pole piece thinning thickness;

[0022] The step of determining at least two coordinate points of a thinning profile curve corresponding to the battery electrode sheet according to the electrode sheet coating data and the electrode sheet thinning data comprises:

[0023] Calculating the minimum thickness of the thinned area corresponding to the battery electrode sheet according to the electrode sheet coating thickness and the electrode sheet thinning thickness;

[0024] Taking the minimum thickness of the thinned area as the first horizontal coordinate, determining the first coordinate point corresponding to the thinned profile curve corresponding to the battery electrode sheet on the horizontal coordinate axis;

[0025] The second coordinate point corresponding to the thinning profile curve is determined by taking the maximum thickness of the thinned area as the second abscissa and taking the thinned width of the pole piece as the second ordinate.

[0026] As an optional embodiment, in the first aspect of the present invention, the cross-sectional area of ​​the battery electrode coated with active material includes the cross-sectional area of ​​the positive electrode coated with active material and the cross-sectional area of ​​the negative electrode coated with active material, the electrode thinning width includes the positive electrode thinning width and the negative electrode thinning width, and the electrode coating thickness includes the positive electrode coating thickness and the negative electrode coating thickness;

[0027] The calculating the cross-sectional area of ​​the active material coated on the battery electrode sheet according to the electrode sheet thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area comprises:

[0028] Calculate the cross-sectional area of ​​the battery electrode coated with active material according to a first calculation formula based on the electrode sheet thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area;

[0029] Wherein, the first calculation formula includes:

[0030] SC = positive electrode sheet thinning width * (positive electrode sheet coating thickness - i) - S1

[0031] SA = Negative electrode sheet thinning width * (Negative electrode sheet coating thickness - i) - S2

[0032] Among them, SC represents the cross-sectional area of ​​the positive electrode sheet coated with active material, SA represents the cross-sectional area of ​​the negative electrode sheet coated with active material, i represents the thinning area judgment value, S1 represents the positive electrode thinning cross-sectional area, and S2 represents the negative electrode thinning cross-sectional area.

[0033] As an optional embodiment, in the first aspect of the present invention, the electrode coating surface density includes the positive electrode coating surface density and the negative electrode coating surface density, the coated active material gram capacity includes the positive electrode coating active material gram capacity and the negative electrode coating active material gram capacity, and the coated active material ratio includes the positive electrode coating active material ratio and the negative electrode coating active material ratio;

[0034] The calculating the N / P ratio of the coating thinning area of ​​the battery electrode sheet according to the electrode sheet coating data and the cross-sectional area of ​​the coated active material comprises:

[0035] Calculating the N / P ratio of the coated thinned area of ​​the battery electrode sheet according to the electrode sheet coating data and the cross-sectional area of ​​the coated active material according to a second calculation formula;

[0036] Wherein, the second calculation formula includes:

[0037]

[0038] Among them, ρ1 represents the coating surface density of the positive electrode sheet, ρ2 represents the coating surface density of the negative electrode sheet, σ represents the rolling elongation, α1 represents the gram capacity of the active material coated on the positive electrode sheet, α2 represents the gram capacity of the active material coated on the negative electrode sheet, β1 represents the ratio of the active material coated on the positive electrode sheet, β2 represents the ratio of the active material coated on the negative electrode sheet, and γ represents the feeding tolerance of the main material.

[0039] As an optional implementation, in the first aspect of the present invention, the electrode coating data further includes the positive and negative electrode Overhang and the electrode coating misalignment value of the battery electrode;

[0040] The thinning curve equation for calculating the thinning profile curve corresponding to the battery electrode sheet according to at least two of the coordinate points includes:

[0041] A thinning curve equation of a thinning profile curve corresponding to the battery electrode is calculated according to the positive and negative electrode sheet Overhang, the electrode sheet coating misalignment value and at least two of the coordinate points.

[0042] The second aspect of the present invention discloses a device for calculating the N / P ratio of the coating thinning area, the device comprising:

[0043] A memory storing executable program code;

[0044] a processor coupled to the memory;

[0045] The processor calls the executable program code stored in the memory to execute the method for calculating the N / P ratio of the coating thinning area disclosed in the first aspect of the present invention.

[0046] The third aspect of the present invention discloses a computer storage medium, wherein the computer storage medium stores computer instructions, and when the computer instructions are called, they are used to execute the method for calculating the N / P ratio of the coating thinning area disclosed in the first aspect of the present invention.

[0047] The fourth aspect of the present invention discloses another device for calculating the N / P ratio of the coating thinning area, the device comprising:

[0048] An acquisition module, used for acquiring electrode data of battery electrodes, wherein the battery electrodes include positive electrodes and negative electrodes, and the electrode data include electrode coating data and electrode thinning data;

[0049] A calculation module, used for calculating a thinning curve equation of a thinning profile curve corresponding to the battery electrode sheet according to the electrode sheet data, wherein the thinning curve equation includes a positive electrode thinning curve equation and a negative electrode thinning curve equation;

[0050] The calculation module is also used to calculate the N / P ratio of the coated thinning area of ​​the battery electrode according to the thinning curve equation and the electrode data.

[0051] As an optional embodiment, in the second aspect of the present invention, the electrode coating data includes electrode coating surface density, rolling elongation, coating active material gram capacity, coating active material ratio and main material feeding tolerance;

[0052] The calculation module calculates the N / P ratio of the coating thinning area of ​​the battery electrode sheet according to the thinning curve equation and the electrode sheet data, specifically including:

[0053] According to the thinning curve equation, calculating the thinning cross-sectional area of ​​the battery electrode sheet, the thinning cross-sectional area includes the positive electrode thinning cross-sectional area and the negative electrode thinning cross-sectional area;

[0054] Calculating the cross-sectional area of ​​the battery electrode sheet coated with active material according to the electrode sheet data and the thinned cross-sectional area of ​​the battery electrode sheet;

[0055] The N / P ratio of the coated thinned area of ​​the battery electrode is calculated based on the electrode coating data and the cross-sectional area of ​​the coated active material.

[0056] As an optional implementation, in the second aspect of the present invention, the pole piece coating data further includes pole piece coating thickness, and the pole piece thinning data includes pole piece thinning width;

[0057] The calculation module calculates the cross-sectional area of ​​the battery electrode sheet coated with the active material according to the electrode sheet data and the thinned cross-sectional area of ​​the battery electrode sheet, specifically including:

[0058] Determine a thinning area judgment value corresponding to the battery electrode piece, and calculate a maximum thickness of the thinning area corresponding to the battery electrode piece according to the electrode piece coating thickness and the thinning area judgment value;

[0059] The cross-sectional area of ​​the battery electrode coated with the active material is calculated according to the electrode sheet thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area.

[0060] As an optional implementation, in the second aspect of the present invention, the calculation module calculates the thinning curve equation of the thinning profile curve corresponding to the battery electrode sheet according to the electrode sheet data, specifically including:

[0061] Determine at least two coordinate points of a thinning profile curve corresponding to the battery electrode according to the electrode coating data and the electrode thinning data;

[0062] A thinning curve equation of a thinning profile curve corresponding to the battery electrode sheet is calculated based on at least two of the coordinate points.

[0063] As an optional implementation, in the second aspect of the present invention, the pole piece thinning data further includes pole piece thinning thickness;

[0064] The method in which the calculation module determines at least two coordinate points of the thinning profile curve corresponding to the battery electrode sheet according to the electrode sheet coating data and the electrode sheet thinning data specifically includes:

[0065] Calculating the minimum thickness of the thinned area corresponding to the battery electrode sheet according to the electrode sheet coating thickness and the electrode sheet thinning thickness;

[0066] Taking the minimum thickness of the thinned area as the first horizontal coordinate, determining the first coordinate point corresponding to the thinned profile curve corresponding to the battery electrode sheet on the horizontal coordinate axis;

[0067] The second coordinate point corresponding to the thinning profile curve is determined by taking the maximum thickness of the thinned area as the second abscissa and taking the thinned width of the pole piece as the second ordinate.

[0068] As an optional embodiment, in the second aspect of the present invention, the cross-sectional area of ​​the battery electrode coated with active material includes the cross-sectional area of ​​the positive electrode coated with active material and the cross-sectional area of ​​the negative electrode coated with active material, the electrode thinning width includes the positive electrode thinning width and the negative electrode thinning width, and the electrode coating thickness includes the positive electrode coating thickness and the negative electrode coating thickness;

[0069] The calculation module calculates the cross-sectional area of ​​the battery electrode sheet coated with the active material according to the electrode sheet thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area, specifically including:

[0070] Calculate the cross-sectional area of ​​the battery electrode coated with active material according to a first calculation formula based on the electrode sheet thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area;

[0071] Wherein, the first calculation formula includes:

[0072] SC = positive electrode sheet thinning width * (positive electrode sheet coating thickness - i) - S1

[0073] SA = Negative electrode sheet thinning width * (Negative electrode sheet coating thickness - i) - S2

[0074] Among them, SC represents the cross-sectional area of ​​the positive electrode sheet coated with active material, SA represents the cross-sectional area of ​​the negative electrode sheet coated with active material, i represents the thinning area judgment value, S1 represents the positive electrode thinning cross-sectional area, and S2 represents the negative electrode thinning cross-sectional area.

[0075] As an optional embodiment, in the second aspect of the present invention, the electrode coating surface density includes the positive electrode coating surface density and the negative electrode coating surface density, the coated active material gram capacity includes the positive electrode coating active material gram capacity and the negative electrode coating active material gram capacity, and the coated active material ratio includes the positive electrode coating active material ratio and the negative electrode coating active material ratio;

[0076] The calculation module calculates the N / P ratio of the coating thinning area of ​​the battery electrode according to the electrode coating data and the cross-sectional area of ​​the coated active material, specifically including:

[0077] Calculating the N / P ratio of the coated thinned area of ​​the battery electrode sheet according to the electrode sheet coating data and the cross-sectional area of ​​the coated active material according to a second calculation formula;

[0078] Wherein, the second calculation formula includes:

[0079]

[0080] Among them, ρ1 represents the coating surface density of the positive electrode sheet, ρ2 represents the coating surface density of the negative electrode sheet, σ represents the rolling elongation, α1 represents the gram capacity of the active material coated on the positive electrode sheet, α2 represents the gram capacity of the active material coated on the negative electrode sheet, β1 represents the ratio of the active material coated on the positive electrode sheet, β2 represents the ratio of the active material coated on the negative electrode sheet, and γ represents the feeding tolerance of the main material.

[0081] As an optional implementation, in the second aspect of the present invention, the electrode coating data further includes the positive and negative electrode Overhang and the electrode coating misalignment value of the battery electrode;

[0082] The method in which the calculation module calculates the thinning curve equation of the thinning profile curve corresponding to the battery electrode sheet according to at least two of the coordinate points specifically includes:

[0083] A thinning curve equation of a thinning profile curve corresponding to the battery electrode is calculated according to the positive and negative electrode sheet Overhang, the electrode sheet coating misalignment value and at least two of the coordinate points.

[0084] Compared with the prior art, the embodiments of the present invention have the following beneficial effects:

[0085] In an embodiment of the present invention, the pole piece data of the battery pole piece is obtained, and the thinning curve equation of the thinning profile curve corresponding to the battery pole piece is calculated according to the pole piece data, and the N / P ratio of the coated thinning area of ​​the battery pole piece is calculated according to the thinning curve equation and the pole piece data. It can be seen that the implementation of the present invention can improve the accuracy of the calculated N / P ratio, thereby reducing the problem of insufficient negative electrode lithium deposition or negative electrode lithium deposition caused by the mismatch of the positive and negative electrode capacities in the pole piece coated thinning area, improving the control of the accuracy of the battery pole piece thinning process, and thereby improving the manufacturing efficiency of the battery pole piece. BRIEF DESCRIPTION OF THE DRAWINGS

[0086] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0087] Figure 1 It is a flow chart of a method for calculating the N / P ratio of a coating thinning area disclosed in an embodiment of the present invention;

[0088] Figure 2 It is a flow chart of another method for calculating the N / P ratio of the coating thinning area disclosed in an embodiment of the present invention;

[0089] Figure 3 It is a schematic diagram of a structure in which the edge of a membrane region of a battery electrode is thinned according to an embodiment of the present invention;

[0090] Figure 4 It is a schematic diagram of the structure of a pole piece partition disclosed in an embodiment of the present invention;

[0091] Figure 5 It is a schematic diagram of a structure in which the edge and the middle of the membrane area of ​​a battery electrode disclosed in an embodiment of the present invention are thinned;

[0092] Figure 6 It is a schematic diagram of the structure of a device for calculating the N / P ratio of a coating thinning area disclosed in an embodiment of the present invention;

[0093] Figure 7 It is a schematic structural diagram of another device for calculating the N / P ratio of the coating thinning area disclosed in an embodiment of the present invention. DETAILED DESCRIPTION

[0094] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0095] The terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish different objects rather than to describe a specific order. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions. For example, a process, method, device, product or end including a series of steps or units is not limited to the listed steps or units, but may optionally include steps or units that are not listed, or may optionally include other steps or units inherent to these processes, methods, products or ends.

[0096] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present invention. The appearance of the phrase in various places in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.

[0097] The present invention discloses a method and device for calculating the N / P ratio of a coating and thinning area, and a computer storage medium, which can improve the accuracy of the calculated N / P ratio, thereby reducing the problem of insufficient negative electrode lithium deposition or negative electrode lithium deposition caused by the mismatch of the positive and negative electrode capacities in the coating and thinning area of ​​the electrode piece, improving the control of the accuracy of the battery electrode piece thinning process, and thereby improving the manufacturing efficiency of the battery electrode piece. The following are detailed descriptions.

[0098] Embodiment 1

[0099] See also Figure 1 , Figure 1 : is a flow chart of a method for calculating the N / P ratio of the coating thinning area disclosed in an embodiment of the present invention. Figure 1 The method for calculating the N / P ratio of the coating thinning area described above can be applied to a device for calculating the N / P ratio of the coating thinning area, wherein the device for calculating the N / P ratio of the coating thinning area can include an intelligent server or an intelligent platform for calculating the N / P ratio, and the intelligent server includes a local server or a cloud server, which is not limited in the embodiment of the present invention. Figure 1 As shown, the calculation method of the N / P ratio of the coating thinning area may include the following operations:

[0100] 101. Obtain electrode data of battery electrodes, where the battery electrodes include positive electrodes and negative electrodes, and the electrode data include electrode coating data and electrode thinning data.

[0101] In an embodiment of the present invention, optionally, the battery electrode may include a positive electrode and a negative electrode, and the positive and negative electrode correspond to each other, and the electrode data may include electrode coating data and electrode thinning data, wherein coating is a basic process in the manufacturing process of lithium-ion batteries, and one or more layers of positive and negative electrode slurries are uniformly coated on aluminum foil or copper foil respectively by extrusion coating equipment, and the coating amount is adjusted by controlling the gap between the die head and the coating roller, and the surface density and size consistency of the coated product are controlled. After oven drying, the positive and negative electrode sheets of the lithium-ion battery are obtained, that is, the electrode coating data may include one or more of the electrode coating surface density, rolling elongation, gram capacity of the coated active material, coating active material ratio, main material feeding tolerance and electrode coating thickness, and the electrode thinning data may include the electrode thinning width and / or the electrode thinning thickness, which is not limited by the present invention.

[0102] 102. According to the electrode data, a thinning curve equation of a thinning profile curve corresponding to the battery electrode is calculated, and the thinning curve equation includes a positive electrode thinning curve equation and a negative electrode thinning curve equation.

[0103] In the embodiment of the present invention, optionally, a coated dry film surface density and thickness measuring machine can be used to measure the electrode thickness through the principle of laser triangulation, and then the dry film contour curve after the electrode is coated can be measured in real time and accurately. The positive and negative electrode Overhang can be obtained after actual measurement, or an average value can be taken after actual measurement. Optionally, in order to simplify the model, in this embodiment, the positive and negative electrode Overhang can take a fixed value, such as 1.5mm, and the electrode coating surface misalignment can take 0mm. According to the electrode data, the thinning curve equation of the thinning contour curve corresponding to the battery electrode is calculated. Specifically, the thinning curve equation of the thinning contour curve corresponding to the battery electrode can be calculated according to the electrode thinning width, the electrode thinning thickness and the electrode coating thickness. The thinning curve equation may include a positive electrode thinning curve equation and a negative electrode thinning curve equation, which is not limited by the present invention.

[0104] 103. Calculate the N / P ratio of the coated thinning area of ​​the battery electrode based on the thinning curve equation and electrode data.

[0105] In an embodiment of the present invention, optionally, the thinned cross-sectional area and the cross-sectional area coated with active material of the battery electrode can be calculated according to the thinning curve equation, and the N / P ratio of the coated thinned area of ​​the battery electrode can be calculated according to the thinned cross-sectional area, the cross-sectional area coated with active material and the electrode data.

[0106] It can be seen that implementation Figure 1The described method for calculating the N / P ratio of the coated thinning area can obtain the pole piece data of the battery pole piece, and calculate the thinning curve equation of the thinning profile curve corresponding to the battery pole piece based on the pole piece data. The N / P ratio of the coated thinning area of ​​the battery pole piece is calculated based on the thinning curve equation and the pole piece data, which can improve the accuracy of the calculated N / P ratio, thereby reducing the occurrence of insufficient lithium deposition on the negative electrode or lithium deposition on the negative electrode caused by the mismatch between the positive and negative electrode capacities in the coated thinning area of ​​the pole piece, improve the control over the accuracy of the battery pole piece thinning process, and thereby improve the manufacturing efficiency of the battery pole piece.

[0107] Embodiment 2

[0108] See also Figure 2 , Figure 2 : is a flow chart of a method for calculating the N / P ratio of the coating thinning area disclosed in an embodiment of the present invention. Figure 2 The method for calculating the N / P ratio of the coating thinning area described above can be applied to a device for calculating the N / P ratio of the coating thinning area, wherein the device for calculating the N / P ratio of the coating thinning area can include an intelligent server or an intelligent platform for calculating the N / P ratio, and the intelligent server includes a local server or a cloud server, which is not limited in the embodiment of the present invention. Figure 2 As shown, the calculation method of the N / P ratio of the coating thinning area may include the following operations:

[0109] 201. Obtain electrode data of a battery electrode, where the battery electrode includes a positive electrode and a negative electrode, and the electrode data includes electrode coating data and electrode thinning data.

[0110] 202. Calculate a thinning curve equation of a thinning profile curve corresponding to the battery electrode according to the electrode data. The thinning curve equation includes a positive electrode thinning curve equation and a negative electrode thinning curve equation.

[0111] In the embodiment of the present invention, for other descriptions of step 201 and step 202, please refer to the detailed description of step 101 and step 102 in the first embodiment, and the embodiment of the present invention will not be repeated.

[0112] 203. According to the thinning curve equation, calculate the thinning cross-sectional area of ​​the battery electrode, which includes the positive electrode thinning cross-sectional area and the negative electrode thinning cross-sectional area.

[0113] In the embodiment of the present invention, optionally, Figure 3 As shown, Figure 3 Schematic diagram of a thinned film edge structure of a battery electrode disclosed in an embodiment of the present invention, wherein the electrode at point A is a positive electrode, the electrode at point B is a negative electrode, and Figure 3On the negative electrode cutting side in, point A is taken as the coordinate origin, and the equations of the single-sided thinning curve of the positive electrode and the single-sided thinning curve of the negative electrode are established, wherein the positive and negative electrode Overhang can be 1-2mm. In this embodiment, the positive and negative electrode Overhang is 1.5mm. The horizontal axis in the figure represents the thickness of the single-sided coating of the electrode excluding the foil, and the vertical axis represents the thinning width of the electrode. h0 represents the thickness of the single-sided main area of ​​the electrode, that is, the coating thickness of the electrode, x1 = electrode coating thickness - electrode thinning thickness, that is, x1 represents the minimum thickness of the thinning area corresponding to the battery electrode, CL represents the thinning width of the positive electrode, and the thinning curve equation is calculated by calculus according to the points (x1, 0) and (x, CL) to obtain the positive electrode thinning cross-sectional area S1, such as Figure 3 As shown, in Figure 3 On the negative electrode ear side, point B is taken as the coordinate origin, and the calculation method of the negative electrode thinning cross-sectional area S2 is similar, which will not be repeated in this embodiment.

[0114] 204. Calculate the cross-sectional area of ​​the active material coated on the battery electrode based on the electrode data and the thinned cross-sectional area of ​​the battery electrode.

[0115] In the embodiment of the present invention, optionally, Figure 3 As shown, taking the positive electrode profile on the negative electrode cutting side as an example, the cross-sectional area of ​​the positive electrode sheet coated with active material SC = CL*x-S1, and the cross-sectional area of ​​the negative electrode sheet coated with active material SA = the negative electrode sheet coating thickness*(AL-1.5mm).

[0116] 205. Calculate the N / P ratio of the coated thinning area of ​​the battery electrode based on the electrode coating data and the cross-sectional area of ​​the coated active material.

[0117] It can be seen that implementation Figure 2 The described method for calculating the N / P ratio of the coated thinning area can obtain the pole piece data of the battery pole piece, calculate the thinning curve equation of the thinning profile curve corresponding to the battery pole piece according to the pole piece data, calculate the thinning cross-sectional area of ​​the battery pole piece according to the thinning curve equation, calculate the cross-sectional area of ​​the coated active material of the battery pole piece according to the pole piece data and the thinning cross-sectional area of ​​the battery pole piece, calculate the N / P ratio of the coated thinning area of ​​the battery pole piece according to the pole piece coating data and the coated active material cross-sectional area, and can calculate the N / P ratio of the coated thinning area of ​​the battery pole piece based on the pole piece coating data and the coated active material cross-sectional area, thereby improving the accuracy of the calculated N / P ratio, thereby reducing the occurrence of insufficient lithium deposition at the negative electrode or lithium deposition at the negative electrode due to the mismatch between the positive and negative electrode capacities in the coated thinning area of ​​the pole piece, improving the control over the accuracy of the battery pole piece thinning process, and thereby improving the manufacturing efficiency of the battery pole piece.

[0118] In an optional embodiment, the pole piece coating data further includes the pole piece coating thickness, and the pole piece thinning data includes the pole piece thinning width;

[0119] According to the electrode data and the thinning cross-sectional area of ​​the battery electrode, the calculation of the cross-sectional area of ​​the coating active material of the battery electrode may include the following operations:

[0120] Determine the thinning area judgment value corresponding to the battery electrode piece, and calculate the maximum thickness of the thinning area corresponding to the battery electrode piece according to the electrode piece coating thickness and the thinning area judgment value;

[0121] The cross-sectional area of ​​the active material coated on the battery electrode is calculated based on the electrode thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area.

[0122] In this optional embodiment, optionally, as Figure 4 As shown, Figure 4 is a schematic diagram of a structure of a pole piece partition disclosed in an embodiment of the present invention, such as Figure 4 As shown in the figure, after the thinning operation, the electrode sheet can be divided into an empty foil area, a thinning area and a main area. Among them, the electrode sheet coating thickness represents the thickness of the main area of ​​the battery electrode sheet. The electrode sheet coating thickness of the battery electrode sheet can be measured at any point in the main area of ​​the battery electrode sheet, such as Figure 4 The thickness of at least two points in the main area of ​​the battery pole piece can also be measured, and then the average value is calculated as the coating thickness of the battery pole piece, for example, Figure 4 The thickness of the midpoint ①, point ② and point ③ is calculated as the average thickness of the three points as the electrode coating thickness of the battery electrode, which is not limited in this embodiment.

[0123] In this optional embodiment, the thinning area determination value corresponding to the battery electrode sheet can be used to define the thinning area of ​​the battery electrode sheet. The thinning area determination value can be calculated by a computer or set by a staff member, such as 1.5 μm, 2 μm or 3 μm. This embodiment is illustrated by taking the thinning area determination value of 3 μm as an example. Specifically, Figure 4 As shown, when the thickness of point ④ minus the electrode coating thickness = 3 μm, the distance between point ④ and point ⑤ is defined as the electrode thinning width, that is, the distance between point ④ and point ⑤ is the thinning area, and the electrode coating thickness minus the thickness of point ⑤ is defined as the electrode thinning thickness, which is not limited in this embodiment.

[0124] In this optional embodiment, optionally, Figure 4 For example, Figure 4 As shown, the maximum thickness of the thinning area corresponding to the battery electrode is the thickness of point ④, that is, the maximum thickness of the thinning area = the electrode coating thickness - the thinning area judgment value, the cross-sectional area of ​​the coated active material of the battery electrode = the electrode thinning width * the maximum thickness of the thinning area - the thinning cross-sectional area, that is, the cross-sectional area of ​​the coated active material of the battery electrode = the electrode thinning width * (the electrode coating thickness - the thinning area judgment value) - the thinning cross-sectional area, the cross-sectional area of ​​the coated active material of the battery electrode includes the cross-sectional area of ​​the coated active material of the positive electrode and the cross-sectional area of ​​the coated active material of the negative electrode, which is not limited in this embodiment.

[0125] It can be seen that implementing this optional embodiment can determine the thinning area judgment value corresponding to the battery pole piece, and calculate the maximum thickness of the thinning area corresponding to the battery pole piece according to the pole piece coating thickness and the thinning area judgment value, and calculate the cross-sectional area of ​​the coated active material of the battery pole piece according to the pole piece thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area, which can improve the accuracy of the calculated cross-sectional area of ​​the coated active material of the battery pole piece, and thereby improve the accuracy of the calculated N / P ratio.

[0126] In another optional embodiment, according to the pole piece data, calculating the thinning curve equation of the thinning profile curve corresponding to the battery pole piece may include the following operations:

[0127] Determine at least two coordinate points of a thinning profile curve corresponding to the battery electrode according to the electrode coating data and the electrode thinning data;

[0128] A thinning curve equation for a thinning profile curve corresponding to a battery electrode sheet is calculated based on at least two coordinate points.

[0129] In this optional embodiment, optionally, as Figure 3 As shown, the thinning profile curve of the battery pole piece is approximately a parabolic curve, so the curve equation of the thinning profile curve of the battery pole piece is set to y = a·x 2 +c, calculate the coordinates of point (x1, 0) and point (x, CL) according to the electrode coating data and the electrode thinning data, and calculate the thinning curve equation of the thinning contour curve corresponding to the battery electrode according to the coordinates of point (x1, 0) and point (x, CL).

[0130] In this optional embodiment, optionally, the electrode coating data may also include the positive and negative electrode Overhang of the battery electrode and the electrode coating misalignment value. The positive and negative electrode Overhang of the battery electrode and the electrode coating misalignment value can be determined, and the thinning curve equation of the thinning contour curve corresponding to the battery electrode is calculated based on the positive and negative electrode Overhang, the electrode coating misalignment value and at least two coordinate points. In order to simplify the model, in this embodiment, the positive and negative electrode Overhang can take a fixed value, such as 1.5mm, and the electrode coating surface misalignment can take 0mm, which is not limited in this embodiment.

[0131] It can be seen that the implementation of this optional embodiment can determine at least two coordinate points of the thinning contour curve corresponding to the battery pole piece according to the pole piece coating data and the pole piece thinning data, and calculate the thinning curve equation of the thinning contour curve corresponding to the battery pole piece according to the at least two coordinate points. The thinning curve equation of the thinning contour curve corresponding to the battery pole piece can be calculated according to the at least two coordinate points of the thinning contour curve corresponding to the battery pole piece, taking into account not only the pole piece thinning width but also the pole piece thinning thickness, thereby improving the accuracy and reliability of calculating the cross-sectional area according to the thinning curve equation, and thereby improving the accuracy of calculating the N / P ratio.

[0132] In yet another optional embodiment, the pole piece thinning data further includes the pole piece thinning thickness;

[0133] According to the electrode coating data and the electrode thinning data, determining at least two coordinate points of the thinning profile curve corresponding to the battery electrode may include the following operations:

[0134] According to the electrode coating thickness and the electrode thinning thickness, calculate the minimum thickness of the thinning area corresponding to the battery electrode;

[0135] Taking the minimum thickness of the thinned area as the first horizontal coordinate, determining the first coordinate point corresponding to the thinned profile curve corresponding to the battery electrode sheet on the horizontal coordinate axis;

[0136] The second coordinate point corresponding to the thinning profile curve is determined by taking the maximum thickness of the thinned area as the second abscissa and taking the thinned width of the pole piece as the second ordinate.

[0137] In this optional embodiment, optionally, Figure 4 For example, Figure 4 As shown, the minimum thickness of the thinning area corresponding to the battery pole piece is the thickness of point ⑤, that is, the minimum thickness of the thinning area = the coating thickness of the pole piece - the thinning thickness of the pole piece. The minimum thickness of the thinning area is used as the first horizontal coordinate to determine the first coordinate point corresponding to the thinning contour curve corresponding to the battery pole piece on the horizontal coordinate axis, that is, x1 = the minimum thickness of the thinning area, and the coordinates of the first coordinate point are (minimum thickness of the thinning area, 0). The maximum thickness of the thinning area corresponding to the battery pole piece is the thickness of point ④, that is, the maximum thickness of the thinning area = the coating thickness of the pole piece - the thinning area judgment value, and the distance between point ④ and point ⑤ is the thinning width of the pole piece. The maximum thickness of the thinning area is used as the second horizontal coordinate, and the thinning width of the pole piece is used as the second vertical coordinate to determine the second coordinate point corresponding to the thinning contour curve, that is, x = the maximum thickness of the thinning area, CL = the thinning width of the pole piece, and the coordinates of the second coordinate point are (maximum thickness of the thinning area, thinning width of the pole piece).

[0138] It can be seen that the implementation of this optional embodiment can calculate the minimum thickness of the thinning area corresponding to the battery pole piece according to the pole piece coating thickness and the pole piece thinning thickness, and determine the first coordinate point corresponding to the thinning contour curve corresponding to the battery pole piece on the horizontal coordinate axis with the minimum thickness of the thinning area as the first horizontal coordinate, and determine the second coordinate point corresponding to the thinning contour curve with the maximum thickness of the thinning area as the second horizontal coordinate and the pole piece thinning width as the second vertical coordinate. The coordinate point corresponding to the thinning contour curve can be determined according to the pole piece thinning data and the coating data, thereby improving the accuracy of the equation for calculating the thinning curve, considering not only the pole piece thinning width but also the pole piece thinning thickness, thereby improving the accuracy and reliability of calculating the cross-sectional area according to the thinning curve equation, and thereby improving the accuracy of calculating the N / P ratio.

[0139] In another optional embodiment, the cross-sectional area of ​​the battery electrode coated with active material includes the cross-sectional area of ​​the positive electrode coated with active material and the cross-sectional area of ​​the negative electrode coated with active material, the electrode thinning width includes the positive electrode thinning width and the negative electrode thinning width, and the electrode coating thickness includes the positive electrode coating thickness and the negative electrode coating thickness;

[0140] According to the electrode sheet thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area, the calculation of the cross-sectional area of ​​the coating active material of the battery electrode sheet may include the following operations:

[0141] Calculate the cross-sectional area of ​​the battery electrode coated with active material according to the first calculation formula based on the electrode thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area;

[0142] The first calculation formula includes:

[0143] SC = positive electrode sheet thinning width * (positive electrode sheet coating thickness - i) - S1

[0144] SA = Negative electrode sheet thinning width * (Negative electrode sheet coating thickness - i) - S2

[0145] Among them, SC represents the cross-sectional area of ​​the positive electrode sheet coated with active material, SA represents the cross-sectional area of ​​the negative electrode sheet coated with active material, i represents the thinning area judgment value, S1 represents the thinning cross-sectional area of ​​the positive electrode, and S2 represents the thinning cross-sectional area of ​​the negative electrode.

[0146] In this optional embodiment, i represents a thinning area determination value. The thinning area determination value corresponding to the battery electrode can be used to define the thinning area of ​​the battery electrode. The thinning area determination value can be calculated by a computer or set by a staff member, such as 1.5 μm, 2 μm or 3 μm. This embodiment is illustrated by taking the thinning area determination value of 3 μm as an example. Specifically, Figure 4As shown, when the thickness of point ④ minus the electrode coating thickness = 3 μm, the distance between point ④ and point ⑤ is defined as the electrode thinning width, that is, the distance between point ④ and point ⑤ is the thinning area, and the electrode coating thickness minus the thickness of point ⑤ is defined as the electrode thinning thickness, which is not limited in this embodiment.

[0147] It can be seen that the implementation of this optional embodiment can calculate the cross-sectional area of ​​the active material coated on the battery electrode according to the electrode thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area according to the first calculation formula, and can quantitatively calculate the cross-sectional area of ​​the active material coated on the battery electrode, thereby improving the calculation accuracy and further improving the accuracy of the calculation of the N / P ratio.

[0148] In another optional embodiment, the electrode coating surface density includes the positive electrode coating surface density and the negative electrode coating surface density, the coating active material gram capacity includes the positive electrode coating active material gram capacity and the negative electrode coating active material gram capacity, and the coating active material ratio includes the positive electrode coating active material ratio and the negative electrode coating active material ratio;

[0149] According to the electrode coating data and the cross-sectional area of ​​the coated active material, the calculation of the N / P ratio of the coating thinning area of ​​the battery electrode may include the following operations:

[0150] According to the electrode coating data and the cross-sectional area of ​​the coated active material, the N / P ratio of the coated thinning area of ​​the battery electrode is calculated according to the second calculation formula;

[0151] The second calculation formula includes:

[0152]

[0153] Among them, ρ1 represents the surface density of the positive electrode sheet coating, ρ2 represents the surface density of the negative electrode sheet coating, σ represents the rolling elongation, α1 represents the gram capacity of the active material coated on the positive electrode sheet, α2 represents the gram capacity of the active material coated on the negative electrode sheet, β1 represents the ratio of the active material coated on the positive electrode sheet, β2 represents the ratio of the active material coated on the negative electrode sheet, and γ represents the feeding tolerance of the main material.

[0154] In this optional embodiment, the second calculation formula may also include coating surface density tolerance, main material gram capacity tolerance, etc., which may be specifically calculated based on actual conditions, and the first calculation formula and the second calculation formula may be programmatically imported to calculate the N / P ratio of the battery electrode in real time, such as Figure 3 As shown, the Overhang value of the positive and negative electrodes is set to 1.5mm, the AB surface offset of the electrode coating is 0mm, the 0.33C gram capacity of the positive electrode main material is 144.4mAh / g, the minimum 0.1C gram capacity of the negative electrode is 350mAh / g, and the single-sided coating surface density of the positive electrode (excluding foil) is 308mg / 1540.25mm 2, negative electrode single-sided coating density (excluding foil) 145mg / 1540.25mm 2 , the positive electrode main material loading is 97%, the negative electrode main material loading is 96.5%, the thickness of the single-sided main area of ​​the positive electrode (excluding foil) is 98μm, and the thickness of the single-sided main area of ​​the negative electrode (excluding foil) is 93μm. According to the first calculation formula and the second calculation formula, the N / P ratio of the thinned area of ​​the positive and negative electrodes of the battery is calculated as shown in Table 1 below:

[0155] Table 1 N / P ratio corresponding to coating only thinning the edge of the film area

[0156]

[0157] In this optional embodiment, optionally, as Figure 5 As shown, Figure 5 is a schematic diagram of a structure in which the edge and the middle of the membrane area of ​​a battery electrode disclosed in an embodiment of the present invention are thinned, such as Figure 5 As shown, the Overhang value of the positive and negative electrodes is set to 1.5mm, the AB surface offset of the electrode coating is 0mm, the 0.33C gram capacity of the positive electrode main material is 144.4mAh / g, the minimum 0.1C gram capacity of the negative electrode is 350mAh / g, and the single-sided coating surface density of the positive electrode (excluding foil) is 308mg / 1540.25mm 2 , negative electrode single-sided coating density (excluding foil) 145mg / 1540.25mm 2 , positive electrode main material loading 97%, negative electrode main material loading 96.5%, positive electrode single-sided main area thickness (excluding foil) 98μm, negative electrode single-sided main area thickness (excluding foil) 93μm, according to the first calculation formula and the second calculation formula, the N / P ratio of the negative electrode cutting side of the battery is calculated as shown in Table 2 below:

[0158] Table 2 The coating thinned the film edge and the middle of the film area, and the corresponding N / P ratio of the negative electrode cutting side

[0159]

[0160]

[0161] The N / P ratio of the negative electrode ear side of the battery is calculated according to the first calculation formula and the second calculation formula as shown in Table 3 below:

[0162] Table 3 The coating thinned the film edge and the middle of the film area, and the corresponding N / P ratio on the negative electrode ear side

[0163]

[0164]

[0165] It can be seen that the implementation of this optional embodiment can calculate the N / P ratio of the coated thinning area of ​​the battery electrode according to the electrode coating data and the cross-sectional area of ​​the coated active material according to the second calculation formula. When calculating the N / P ratio, the coating surface density, the main material gram capacity, the coating surface density tolerance, the main material incoming gram capacity tolerance, the main material feeding tolerance, the rolling elongation, etc. are considered to improve the accuracy of the calculated N / P ratio, thereby reducing the problem of insufficient lithium deposition at the negative electrode or lithium deposition at the negative electrode caused by the mismatch between the positive and negative electrode capacities in the electrode coating thinning area, improving the control of the accuracy of the battery electrode thinning process, thereby improving the manufacturing efficiency of the battery electrode, and the calculation formula can be programmed to further improve the calculation efficiency.

[0166] Embodiment 3

[0167] See also Figure 6 , Figure 6 Schematic diagram of a device for calculating the N / P ratio of a coating thinning area disclosed in an embodiment of the present invention. Figure 6 The calculation device for the N / P ratio of the coating thinning area described may include an intelligent server or intelligent platform for calculating the N / P ratio, and the intelligent server includes a local server or a cloud server, which is not limited in the embodiment of the present invention. Figure 6 As shown, the calculation device of the coating thinning area N / P ratio may include:

[0168] An acquisition module 301 is used to acquire electrode data of a battery electrode, where the battery electrode includes a positive electrode and a negative electrode, and the electrode data includes electrode coating data and electrode thinning data;

[0169] A calculation module 302, for calculating a thinning curve equation of a thinning profile curve corresponding to a battery electrode according to the electrode data, wherein the thinning curve equation includes a positive electrode thinning curve equation and a negative electrode thinning curve equation;

[0170] The calculation module 302 is also used to calculate the N / P ratio of the coated thinning area of ​​the battery electrode according to the thinning curve equation and the electrode data.

[0171] It can be seen that implementation Figure 6 The described device for calculating the N / P ratio of the coated thinning area can obtain the pole piece data of the battery pole piece, and calculate the thinning curve equation of the thinning profile curve corresponding to the battery pole piece according to the pole piece data, and calculate the N / P ratio of the coated thinning area of ​​the battery pole piece according to the thinning curve equation and the pole piece data, which can improve the accuracy of the calculated N / P ratio, thereby reducing the occurrence of insufficient lithium deposition on the negative electrode or lithium deposition on the negative electrode due to the mismatch between the positive and negative electrode capacities in the coated thinning area of ​​the pole piece, improve the control over the accuracy of the battery pole piece thinning process, and thereby improve the manufacturing efficiency of the battery pole piece.

[0172] In an optional embodiment, if Figure 6 As shown, the electrode coating data includes the electrode coating surface density, rolling elongation, coating active material gram capacity, coating active material ratio and main material feeding tolerance;

[0173] The specific method of calculating the N / P ratio of the coating thinning area of ​​the battery electrode sheet by the calculation module 302 according to the thinning curve equation and the electrode sheet data includes:

[0174] According to the thinning curve equation, calculate the thinning cross-sectional area of ​​the battery electrode, which includes the positive electrode thinning cross-sectional area and the negative electrode thinning cross-sectional area;

[0175] Calculate the cross-sectional area of ​​the active material coated on the battery electrode according to the electrode data and the thinned cross-sectional area of ​​the battery electrode;

[0176] According to the electrode coating data and the cross-sectional area of ​​the coated active material, the N / P ratio of the coated thinning area of ​​the battery electrode is calculated.

[0177] It can be seen that implementation Figure 6 The described device for calculating the N / P ratio of the coated thinning area can obtain the pole piece data of the battery pole piece, calculate the thinning curve equation of the thinning profile curve corresponding to the battery pole piece according to the pole piece data, calculate the thinning cross-sectional area of ​​the battery pole piece according to the thinning curve equation, calculate the cross-sectional area of ​​the coated active material of the battery pole piece according to the pole piece data and the thinning cross-sectional area of ​​the battery pole piece, calculate the N / P ratio of the coated thinning area of ​​the battery pole piece according to the pole piece coating data and the coated active material cross-sectional area, and can calculate the N / P ratio of the coated thinning area of ​​the battery pole piece based on the pole piece coating data and the coated active material cross-sectional area, thereby improving the accuracy of the calculated N / P ratio, thereby reducing the occurrence of insufficient lithium deposition at the negative electrode or lithium deposition at the negative electrode due to the mismatch between the positive and negative electrode capacities in the coated thinning area of ​​the pole piece, improving the control over the accuracy of the battery pole piece thinning process, and thereby improving the manufacturing efficiency of the battery pole piece.

[0178] In another optional embodiment, Figure 6 As shown, the pole piece coating data also includes the pole piece coating thickness, and the pole piece thinning data includes the pole piece thinning width;

[0179] The specific method in which the calculation module 302 calculates the cross-sectional area of ​​the battery electrode sheet coated with the active material according to the electrode sheet data and the thinned cross-sectional area of ​​the battery electrode sheet includes:

[0180] Determine the thinning area judgment value corresponding to the battery electrode piece, and calculate the maximum thickness of the thinning area corresponding to the battery electrode piece according to the electrode piece coating thickness and the thinning area judgment value;

[0181] The cross-sectional area of ​​the active material coated on the battery electrode is calculated based on the electrode thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area.

[0182] It can be seen that implementation Figure 6The described device for calculating the N / P ratio of the coated thinning area can determine the thinning area judgment value corresponding to the battery pole piece, and calculate the maximum thickness of the thinning area corresponding to the battery pole piece based on the pole piece coating thickness and the thinning area judgment value, and calculate the cross-sectional area of ​​the coated active material of the battery pole piece based on the pole piece thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area, which can improve the accuracy of the calculated cross-sectional area of ​​the coated active material of the battery pole piece, and thereby improve the accuracy of the calculated N / P ratio.

[0183] In yet another optional embodiment, Figure 6 As shown, the specific method of calculating the thinning curve equation of the thinning profile curve corresponding to the battery electrode sheet according to the electrode sheet data by the calculation module 302 includes:

[0184] Determine at least two coordinate points of a thinning profile curve corresponding to the battery electrode according to the electrode coating data and the electrode thinning data;

[0185] A thinning curve equation for a thinning profile curve corresponding to a battery electrode sheet is calculated based on at least two coordinate points.

[0186] In this optional embodiment, the electrode coating data may also include the positive and negative electrode Overhang and electrode coating misalignment values ​​of the battery electrode;

[0187] The specific manner in which the calculation module 302 calculates the thinning curve equation of the thinning profile curve corresponding to the battery electrode sheet according to at least two coordinate points includes:

[0188] The thinning curve equation of the thinning profile curve corresponding to the battery electrode is calculated according to the positive and negative electrode overhangs, the electrode coating misalignment value and at least two coordinate points.

[0189] It can be seen that implementation Figure 6 The described device for calculating the N / P ratio of the coated thinning area can determine at least two coordinate points of the thinning contour curve corresponding to the battery pole piece based on the pole piece coating data and the pole piece thinning data, and calculate the thinning curve equation of the thinning contour curve corresponding to the battery pole piece based on the at least two coordinate points. It can calculate the thinning curve equation of the thinning contour curve corresponding to the battery pole piece based on the at least two coordinate points of the thinning contour curve corresponding to the battery pole piece, taking into account not only the pole piece thinning width but also the pole piece thinning thickness, thereby improving the accuracy and reliability of calculating the cross-sectional area according to the thinning curve equation, and thereby improving the accuracy of calculating the N / P ratio.

[0190] In yet another optional embodiment, Figure 6 As shown, the pole piece thinning data also includes the pole piece thinning thickness;

[0191] The specific method in which the calculation module 302 determines at least two coordinate points of the thinning profile curve corresponding to the battery electrode according to the electrode coating data and the electrode thinning data includes:

[0192] According to the electrode coating thickness and the electrode thinning thickness, calculate the minimum thickness of the thinning area corresponding to the battery electrode;

[0193] Taking the minimum thickness of the thinned area as the first horizontal coordinate, determining the first coordinate point corresponding to the thinned profile curve corresponding to the battery electrode sheet on the horizontal coordinate axis;

[0194] The second coordinate point corresponding to the thinning profile curve is determined by taking the maximum thickness of the thinned area as the second abscissa and taking the thinned width of the pole piece as the second ordinate.

[0195] It can be seen that implementation Figure 6 The described device for calculating the N / P ratio of the coated thinning area can calculate the minimum thickness of the thinning area corresponding to the battery pole piece according to the coating thickness and the thinning thickness of the pole piece, and use the minimum thickness of the thinning area as the first horizontal coordinate to determine the first coordinate point corresponding to the thinning contour curve corresponding to the battery pole piece on the horizontal coordinate axis, and use the maximum thickness of the thinning area as the second horizontal coordinate and the pole piece thinning width as the second vertical coordinate to determine the second coordinate point corresponding to the thinning contour curve. It can determine the coordinate point corresponding to the thinning contour curve according to the pole piece thinning data and the coating data, improve the accuracy of the equation for calculating the thinning curve, consider not only the pole piece thinning width but also the pole piece thinning thickness, improve the accuracy and reliability of calculating the cross-sectional area according to the thinning curve equation, and thus improve the accuracy of calculating the N / P ratio.

[0196] In yet another optional embodiment, Figure 6 As shown, the cross-sectional area of ​​the battery pole piece coated with active material includes the cross-sectional area of ​​the positive pole piece coated with active material and the cross-sectional area of ​​the negative pole piece coated with active material, the pole piece thinning width includes the positive pole piece thinning width and the negative pole piece thinning width, and the pole piece coating thickness includes the positive pole piece coating thickness and the negative pole piece coating thickness;

[0197] The specific method of calculating the cross-sectional area of ​​the battery electrode coated with the active material by the calculation module 302 according to the electrode thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area includes:

[0198] Calculate the cross-sectional area of ​​the battery electrode coated with active material according to the first calculation formula based on the electrode thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area;

[0199] The first calculation formula includes:

[0200] SC = positive electrode sheet thinning width * (positive electrode sheet coating thickness - i) - S1

[0201] SA = Negative electrode sheet thinning width * (Negative electrode sheet coating thickness - i) - S2

[0202] Among them, SC represents the cross-sectional area of ​​the positive electrode sheet coated with active material, SA represents the cross-sectional area of ​​the negative electrode sheet coated with active material, i represents the thinning area judgment value, S1 represents the thinning cross-sectional area of ​​the positive electrode, and S2 represents the thinning cross-sectional area of ​​the negative electrode.

[0203] It can be seen that implementation Figure 6 The described device for calculating the N / P ratio of the coated thinned area can calculate the cross-sectional area of ​​the coated active material of the battery electrode according to the thinning width of the electrode, the maximum thickness of the thinned area and the thinned cross-sectional area according to the first calculation formula, and can quantitatively calculate the cross-sectional area of ​​the coated active material of the battery electrode, improve the calculation accuracy, and thereby improve the accuracy of the calculated N / P ratio.

[0204] In yet another optional embodiment, Figure 6 As shown, the electrode coating surface density includes the positive electrode coating surface density and the negative electrode coating surface density, the coated active material gram capacity includes the positive electrode coating active material gram capacity and the negative electrode coating active material gram capacity, and the coated active material ratio includes the positive electrode coating active material ratio and the negative electrode coating active material ratio;

[0205] The specific method of calculating the N / P ratio of the coating thinning area of ​​the battery electrode sheet by the calculation module 302 according to the electrode sheet coating data and the cross-sectional area of ​​the coated active material includes:

[0206] According to the electrode coating data and the cross-sectional area of ​​the coated active material, the N / P ratio of the coated thinning area of ​​the battery electrode is calculated according to the second calculation formula;

[0207] The second calculation formula includes:

[0208]

[0209] Among them, ρ1 represents the surface density of the positive electrode sheet coating, ρ2 represents the surface density of the negative electrode sheet coating, σ represents the rolling elongation, α1 represents the gram capacity of the active material coated on the positive electrode sheet, α2 represents the gram capacity of the active material coated on the negative electrode sheet, β1 represents the ratio of the active material coated on the positive electrode sheet, β2 represents the ratio of the active material coated on the negative electrode sheet, and γ represents the feeding tolerance of the main material.

[0210] It can be seen that implementation Figure 6The described calculation device for the N / P ratio of the coated thinning area can calculate the N / P ratio of the coated thinning area of ​​the battery electrode according to the electrode coating data and the cross-sectional area of ​​the coated active material according to the second calculation formula. When calculating the N / P ratio, the coating surface density, the main material gram capacity, the coating surface density tolerance, the main material incoming gram capacity tolerance, the main material feeding tolerance, the rolling elongation, etc. are considered to improve the accuracy of the calculated N / P ratio, thereby reducing the problem of insufficient lithium deposition on the negative electrode or lithium deposition on the negative electrode caused by the mismatch between the positive and negative electrode capacities in the coated thinning area of ​​the electrode, improving the control of the accuracy of the battery electrode thinning process, thereby improving the manufacturing efficiency of the battery electrode, and the calculation formula can be programmed to further improve the calculation efficiency.

[0211] Embodiment 4

[0212] See also Figure 7 , Figure 7 FIG. 1 is a schematic diagram of the structure of another device for calculating the N / P ratio of the coating thinning area disclosed in an embodiment of the present invention. Figure 7 As shown, the calculation device of the coating thinning area N / P ratio may include:

[0213] A memory 401 storing executable program codes;

[0214] a processor 402 coupled to the memory 401;

[0215] The processor 402 calls the executable program code stored in the memory 401 to execute the steps in the method for calculating the N / P ratio of the coating thinning area described in the first embodiment of the present invention or the second embodiment of the present invention.

[0216] Embodiment 5

[0217] An embodiment of the present invention discloses a computer storage medium, which stores computer instructions. When the computer instructions are called, they are used to execute the steps in the method for calculating the N / P ratio of the coating thinning area described in Embodiment 1 or Embodiment 2 of the present invention.

[0218] Embodiment 6

[0219] An embodiment of the present invention discloses a computer program product, which includes a non-transitory computer-readable storage medium storing a computer program, and the computer program is operable to enable a computer to execute the steps in the method for calculating the N / P ratio of the coating thinning area described in Example 1 or Example 2.

[0220] The device embodiments described above are only illustrative, wherein the modules described as separate components may or may not be physically separated, and the components displayed as modules may or may not be physical modules, i.e., they may be located in one place, or they may be distributed on multiple network modules. Some or all of the modules may be selected according to actual needs to achieve the purpose of the scheme of this embodiment. Those of ordinary skill in the art may understand and implement it without creative work.

[0221] Through the specific description of the above embodiments, those skilled in the art can clearly understand that each implementation method can be implemented by means of software plus a necessary general hardware platform, and of course, it can also be implemented by hardware. Based on such an understanding, the above technical solution can be essentially or partly contributed to the prior art in the form of a software product, and the computer software product can be stored in a computer-readable storage medium, and the storage medium includes a read-only memory (ROM), a random access memory (RAM), a programmable read-only memory (PROM), an erasable programmable read-only memory (EPROM), a one-time programmable read-only memory (OTPROM), an electronically erasable rewritable read-only memory (EEPROM), a compact disc (CD-ROM) or other optical disc storage, magnetic disk storage, magnetic tape storage, or any other computer-readable medium that can be used to carry or store data.

[0222] Finally, it should be noted that the method and device for calculating the N / P ratio of the coating thinning area and the computer storage medium disclosed in the embodiments of the present invention are only preferred embodiments of the present invention, and are only used to illustrate the technical solution of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, it should be understood by those skilled in the art that the technical solutions described in the aforementioned embodiments can still be modified, or some of the technical features therein can be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the various embodiments of the present invention.

Claims

1. A method for calculating the N / P ratio of the coating thinning area, It is characterized in that The method comprises: Acquire electrode data of a battery electrode, wherein the battery electrode includes a positive electrode and a negative electrode, and the electrode data includes electrode coating data and electrode thinning data; Calculating a thinning curve equation of a thinning profile curve corresponding to the battery electrode piece according to the electrode piece data, wherein the thinning curve equation includes a positive electrode thinning curve equation and a negative electrode thinning curve equation; The N / P ratio of the coated thinned area of ​​the battery electrode is calculated based on the thinning curve equation and the electrode data.

2. The method for calculating the N / P ratio of the coating thinning area according to claim 1, It is characterized in that The electrode coating data includes the electrode coating surface density, rolling elongation, coating active material gram capacity, coating active material ratio and main material feeding tolerance; The calculating the N / P ratio of the coating thinning area of ​​the battery electrode sheet according to the thinning curve equation and the electrode sheet data includes: According to the thinning curve equation, calculating the thinning cross-sectional area of ​​the battery electrode sheet, the thinning cross-sectional area includes the positive electrode thinning cross-sectional area and the negative electrode thinning cross-sectional area; Calculating the cross-sectional area of ​​the battery electrode sheet coated with active material according to the electrode sheet data and the thinned cross-sectional area of ​​the battery electrode sheet; The N / P ratio of the coated thinned area of ​​the battery electrode is calculated based on the electrode coating data and the cross-sectional area of ​​the coated active material.

3. The method for calculating the N / P ratio of the coating thinning area according to claim 2, It is characterized in that The pole piece coating data also includes the pole piece coating thickness, and the pole piece thinning data includes the pole piece thinning width; The step of calculating the cross-sectional area of ​​the battery electrode sheet coated with the active material according to the electrode sheet data and the thinned cross-sectional area of ​​the battery electrode sheet comprises: Determine a thinning area judgment value corresponding to the battery electrode piece, and calculate a maximum thickness of the thinning area corresponding to the battery electrode piece according to the electrode piece coating thickness and the thinning area judgment value; The cross-sectional area of ​​the battery electrode coated with the active material is calculated according to the electrode sheet thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area.

4. The method for calculating the N / P ratio of the coating skived area according to claim 3, It is characterized in that The step of calculating the thinning curve equation of the thinning profile curve corresponding to the battery electrode piece according to the electrode piece data comprises: Determine at least two coordinate points of a thinning profile curve corresponding to the battery electrode according to the electrode coating data and the electrode thinning data; A thinning curve equation of a thinning profile curve corresponding to the battery electrode sheet is calculated based on at least two of the coordinate points.

5. The method for calculating the N / P ratio of the coating thinning area according to claim 4, It is characterized in that The pole piece thinning data also includes the pole piece thinning thickness; The step of determining at least two coordinate points of a thinning profile curve corresponding to the battery electrode sheet according to the electrode sheet coating data and the electrode sheet thinning data comprises: Calculating the minimum thickness of the thinned area corresponding to the battery electrode sheet according to the electrode sheet coating thickness and the electrode sheet thinning thickness; Taking the minimum thickness of the thinned area as the first horizontal coordinate, determining the first coordinate point corresponding to the thinned profile curve corresponding to the battery electrode sheet on the horizontal coordinate axis; The second coordinate point corresponding to the thinning profile curve is determined by taking the maximum thickness of the thinned area as the second abscissa and taking the thinned width of the pole piece as the second ordinate.

6. The method for calculating the N / P ratio of the coating thinning area according to any one of claims 3 to 5, It is characterized in that The cross-sectional area of ​​the battery electrode coated with active material includes the cross-sectional area of ​​the positive electrode coated with active material and the cross-sectional area of ​​the negative electrode coated with active material, the electrode thinning width includes the positive electrode thinning width and the negative electrode thinning width, and the electrode coating thickness includes the positive electrode coating thickness and the negative electrode coating thickness; The calculating the cross-sectional area of ​​the active material coated on the battery electrode sheet according to the electrode sheet thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area comprises: Calculate the cross-sectional area of ​​the battery electrode coated with active material according to a first calculation formula based on the electrode sheet thinning width, the maximum thickness of the thinning area and the thinning cross-sectional area; Wherein, the first calculation formula includes: SC = positive electrode sheet thinning width * (positive electrode sheet coating thickness - i) - S 1 SA = Negative electrode sheet thinning width * (Negative electrode sheet coating thickness - i) - S 2 Wherein, SC represents the cross-sectional area of ​​the positive electrode sheet coated with active material, SA represents the cross-sectional area of ​​the negative electrode sheet coated with active material, i represents the thinning area judgment value, S 1 represents the thinned cross-sectional area of ​​the positive electrode, S 2 represents the thinned cross-sectional area of ​​the negative electrode.

7. The method for calculating the N / P ratio of the coating skived area according to claim 6, It is characterized in that The electrode sheet coating surface density includes the positive electrode sheet coating surface density and the negative electrode sheet coating surface density, the coating active material gram capacity includes the positive electrode sheet coating active material gram capacity and the negative electrode sheet coating active material gram capacity, and the coating active material ratio includes the positive electrode sheet coating active material ratio and the negative electrode sheet coating active material ratio; The calculating the N / P ratio of the coating thinning area of ​​the battery electrode sheet according to the electrode sheet coating data and the cross-sectional area of ​​the coated active material comprises: Calculating the N / P ratio of the coated thinned area of ​​the battery electrode sheet according to the electrode sheet coating data and the cross-sectional area of ​​the coated active material according to a second calculation formula; Wherein, the second calculation formula includes: Among them, ρ 1 represents the positive electrode coating surface density, ρ 2 represents the negative electrode sheet coating surface density, σ represents the rolling elongation, α 1 represents the gram capacity of the positive electrode coated with active material, α 2 represents the gram capacity of the negative electrode coated with active material, β 1 represents the ratio of the active material coated on the positive electrode sheet, β 2 represents the ratio of the active material coated on the negative electrode sheet, and γ represents the feeding tolerance of the main material.

8. The method for calculating the N / P ratio of the coating thinning area according to claim 4 or 5, It is characterized in that The electrode coating data also includes the positive and negative electrode overhangs of the battery electrode and the electrode coating misalignment values; The thinning curve equation for calculating the thinning profile curve corresponding to the battery electrode sheet according to at least two of the coordinate points includes: A thinning curve equation of a thinning profile curve corresponding to the battery electrode is calculated according to the positive and negative electrode sheet Overhang, the electrode sheet coating misalignment value and at least two of the coordinate points.

9. A device for calculating the N / P ratio of the coating thinning area, It is characterized in that The device comprises: A memory storing executable program code; a processor coupled to the memory; The processor calls the executable program code stored in the memory to execute the method for calculating the N / P ratio of the coating thinning area according to any one of claims 1 to 8.

10. A computer storage medium, It is characterized in that The computer storage medium stores computer instructions, and when the computer instructions are called, they are used to execute the method for calculating the N / P ratio of the coating thinning area according to any one of claims 1 to 8.

Citation Information

Cited By

  • Calibration method and device for pole piece thickness measurement, computer equipment and storage medium

    CN120426884A