Ultraviolet photoelectric detector with high linear dynamic range and preparation method
By using a combination of low-resistance gallium nitride layer and high-resistance gallium oxide layer in the ultraviolet photodetector, and setting up an interdigital electrode structure, the problems of poor response performance and small linear dynamic range are solved, and fast response is achieved. And the effect of high linear dynamic range is suitable for missile warning and other fields.
Patent Information
- Application Number
- CN202410769561.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-14
- Publication Date
- 2024-10-01
AI Technical Summary
Existing ultraviolet photoelectric detectors have poor response performance, small linear dynamic range, and complex processes, which limit their applications in areas such as missile warning, flame detection, local secure communications, and ozone detection.
A high linear dynamic range ultraviolet photodetector is designed by forming a specific combination of a low-resistance gallium nitride layer and a high-resistance gallium oxide layer on a semiconductor substrate, and setting interdigitals on the gallium oxide layer. Type electrode structure, forming a heterojunction to improve response speed and linear dynamic range, and maintain good response performance at lower voltages.
It achieves fast response time and large linear dynamic range, reduces the response time of the device, maintains good response performance at lower voltages, is easy to integrate with signal processing systems, and has a simple process and high economic benefits.
Smart Images

Figure CN118738197A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of semiconductor photoelectric devices, and in particular to an ultraviolet photoelectric detector with a high linear dynamic range and a preparation method thereof. Background Art
[0002] When solar ultraviolet radiation passes through the atmosphere, the ozone layer in the atmosphere has a strong absorption effect on the day-blind ultraviolet light in the band of 200nm to 280nm. The background noise of the day-blind ultraviolet light in this band in the atmosphere is almost zero, which makes the day-blind photodetectors in this band play an important role in missile early warning tracking, flame detection, local confidential communication and ozone detection. At present, the day-blind photodetector devices based on wide-bandgap semiconductor materials on the market have become a research hotspot for scientific researchers in recent years due to their small weight, low power consumption, high quantum efficiency and easy integration. Among them, ultra-wide bandgap semiconductors such as aluminum gallium nitrogen, zinc magnesium oxygen, diamond, and gallium oxide are all potential materials for manufacturing day-blind photodetectors.
[0003] For aluminum gallium nitride materials, the crystal quality of the epitaxial layer of high-aluminum aluminum gallium nitride deteriorates rapidly as the aluminum content increases; for zinc magnesium oxide, due to the phase segregation between zinc oxide wurtzite and magnesium oxide rock salt, single wurtzite zinc magnesium oxide with a high magnesium content is difficult to grow; and the band gap of diamond is 5.5eV, and the sensitivity range of the detector made of this material is limited to wavelengths below 225nm, and cannot be used to detect the entire solar-blind area. Therefore, the above materials have obvious disadvantages in the manufacture of solar-blind photodetectors.
[0004] Among gallium oxide materials, β-phase gallium oxide is the most stable one. Its band gap corresponds to a wavelength of 250nm, which corresponds to the solar-blind band. There is no need to adjust the band gap, and it has obvious advantages in solar-blind photodetectors. At present, gallium oxide-based ultraviolet photodetectors such as MSM (Metal-Semiconductor-Metal) type or Schottky (metal-semiconductor) junction type have the problem of slow response speed. Although avalanche-type ultraviolet photodetectors can induce carrier multiplication through impact ionization, thereby obtaining a higher responsivity without affecting the response speed, they need to work at a higher voltage, which is not conducive to energy saving. Moreover, avalanche-type ultraviolet photodetectors have a complex device structure, and therefore require a strict manufacturing process, which greatly hinders the realization of miniaturization and low-cost goals. In addition, the internal gain of the above-mentioned gallium oxide-based photodetectors usually changes with the change of light intensity, so that the change of photocurrent with light intensity is nonlinear, and the linear dynamic range that can be used for further application research is very small, which is not conducive to the application of actual photodetection. Summary of the invention
[0005] In view of this, the present invention provides an ultraviolet photodetector with a high linear dynamic range and a preparation method thereof, so as to solve the problems of poor response performance, small linear dynamic range and complex process of existing ultraviolet photodetectors.
[0006] In a first aspect, the present invention provides an ultraviolet photodetector with a high linear dynamic range, comprising:
[0007] Semiconductor substrate;
[0008] A gallium nitride layer, disposed on the semiconductor substrate, wherein the gallium nitride layer is of a first conductivity type;
[0009] a gallium oxide layer, disposed on a surface of the gallium nitride layer away from the semiconductor substrate, the gallium oxide layer being of a second conductivity type opposite to the first conductivity type, and having a resistivity higher than that of the gallium nitride layer;
[0010] The electrode structure layer is located on the surface of the gallium oxide layer away from the semiconductor substrate, and the electrode structure layer includes a first electrode and a second electrode arranged at intervals on the same plane and a light-transmitting area arranged in a hollow manner.
[0011] Beneficial effects: The ultraviolet photodetector with high linear dynamic range of the present invention forms a heterojunction between the gallium nitride layer and the gallium oxide layer corresponding to the first electrode and the gallium nitride layer and the gallium oxide layer corresponding to the second electrode by constructing a simple specific combination of a low-resistance gallium nitride layer and a high-resistance gallium oxide layer and a structure in which the first electrode and the second electrode are arranged on the same plane on the gallium oxide layer, and the two heterojunction structures are arranged laterally at intervals. The hollow area between the first electrode and the second electrode ensures that the ultraviolet photodetector has a sufficiently large light receiving area. When the ultraviolet photodetector is irradiated by ultraviolet light and the first electrode and the second electrode are connected to the positive and negative electrodes of the external bias voltage respectively, the diffusion and drift of carriers are generated between the gallium nitride layer and the gallium oxide layer in the area below the first electrode and the second electrode, thereby generating current, thereby forming a transistor effect, which can effectively reduce the response time of the device, and expand the linear dynamic range of the device, and can have better response performance at a lower voltage, and the photocurrent hardly changes within a certain voltage range, and is easy to integrate with the signal processing system and has a simple structure.
[0012] In an optional implementation, the first conductivity type is P type, and the second conductivity type is N type.
[0013] After the growth, the gallium oxide material will have some oxygen vacancies, so it will show a weak N-type. The gallium oxide layer of the present invention is not doped and tends to be an intrinsic weak N-type high-resistance state structure, which is simple to prepare and has high economic benefits.
[0014] In an optional embodiment, the first electrode and the second electrode of the electrode structure layer are interdigitated electrodes;
[0015] The first electrode comprises a first electrode body and at least one first extension portion, the first electrode body being arranged on a first side of the surface of the gallium oxide layer, the first extension portion extending from the first electrode body and extending toward a second side of the gallium oxide layer; wherein the first side and the second side are two opposite sides of the surface of the gallium oxide layer (300);
[0016] The second electrode comprises a second electrode body and at least one second extension portion, the second electrode body is disposed on the second side of the gallium oxide layer, and the second extension portion extends from the second electrode body and extends toward the first side of the gallium oxide layer;
[0017] The first extension portion and the second extension portion are arranged crosswise and staggered.
[0018] The preparation is simple and efficient, and can enable the gallium oxide layer and the gallium nitride layer under the electrode structure layer to form a good heterojunction to produce a transistor effect, thereby improving the response speed, ensuring the response performance and a larger linear dynamic range.
[0019] In an optional embodiment, the first electrode body and the second electrode body are parallel to each other, the first extension portion and the second extension portion are parallel to each other, the first electrode body and the first extension portion are perpendicular to each other, and the second electrode body and the second extension portion are perpendicular to each other;
[0020] The distance between adjacent first extension portions and second extension portions is 2 μm-12 μm.
[0021] The structure is stable and can enable the electrode structure layer to have sufficient hollow areas to transmit light and realize photoelectric conversion.
[0022] In an optional implementation, the gallium oxide layer has a thickness of 0.05 μm-0.2 μm.
[0023] The gallium oxide layer is set as a thin film structure. When an external voltage is applied, the carriers in the gallium oxide layer and the gallium nitride layer under the first electrode and the second electrode can diffuse and move rapidly in the vertical direction, greatly improving the response speed of the ultraviolet photodetector.
[0024] In an optional embodiment, the gallium nitride layer has a thickness of 4.5 μm-5 μm. A gallium nitride layer with a thickness of 4.5 μm-5 μm provides sufficient drifting carriers for current generation.
[0025] In an optional embodiment, the semiconductor substrate is a gallium nitride single crystal homogeneous with the gallium nitride layer, or an aluminum nitride single crystal heterogeneous with the gallium nitride layer, or sapphire, or silicon carbide, or single crystal silicon.
[0026] Different semiconductor substrates are selected according to different design requirements to ensure detector performance and improve economic benefits.
[0027] In an optional embodiment, the first electrode and the second electrode are metal composite electrodes of Ti / Au, or Ti / Al / Ni / Au, or Ti / Pt.
[0028] The metal composite electrode has lower roughness, smoother contact interface, and lower lattice mismatch layer thickness. In addition, the film layer in direct contact with the gallium oxide layer serves as an intermediate layer, which helps promote the interdiffusion between the metal electrode and the semiconductor interface, thereby increasing adhesion and reducing potential barriers.
[0029] In a second aspect, the present invention provides a method for preparing an ultraviolet photodetector with a high linear dynamic range, comprising the following steps:
[0030] providing a semiconductor substrate;
[0031] forming a gallium nitride layer on the semiconductor substrate, wherein the gallium nitride layer is of a first conductivity type;
[0032] epitaxially preparing a gallium oxide layer on a surface of the gallium nitride layer on a side away from the semiconductor substrate, wherein the gallium oxide layer is of a second conductivity type opposite to the first conductivity type, and the resistivity of the gallium oxide layer is higher than the resistivity of the gallium nitride layer;
[0033] forming an electrode pattern on a surface of the gallium oxide layer away from the semiconductor substrate;
[0034] An electrode structure layer is prepared on the electrode pattern.
[0035] Beneficial effects: The ultraviolet photodetector with high linear dynamic range prepared by the above method comprises a specific combination of a simple low-resistance gallium nitride layer and a high-resistance gallium oxide layer, and a structure in which a first electrode and a second electrode are arranged on the same plane on the gallium oxide layer at intervals, and heterojunctions are formed between the gallium nitride layer and the gallium oxide layer corresponding to the first electrode and the gallium nitride layer and the gallium oxide layer corresponding to the second electrode, and the two heterojunction structures are arranged at intervals in the transverse direction. The hollow area between the first electrode and the second electrode ensures that the ultraviolet photodetector has a sufficiently large light receiving area. When the ultraviolet photodetector is irradiated by ultraviolet light and the first electrode and the second electrode are connected to the positive and negative electrodes of the external bias voltage respectively, the diffusion and drift of carriers are generated between the gallium nitride layer and the gallium oxide layer in the area below the first electrode and the second electrode, thereby generating current, thereby forming a transistor effect, which can effectively reduce the response time of the device, and expand the linear dynamic range of the device, and can have better response performance at a lower voltage, and the photocurrent hardly changes within a certain voltage range, and is easy to integrate with the signal processing system and has a simple preparation process.
[0036] In an optional embodiment, the forming of the gallium nitride layer on the semiconductor substrate comprises: providing reactants for preparing the gallium nitride layer and mixing them in a pipeline through a carrier gas; passing the uniformly mixed gas into a reaction chamber to grow the gallium nitride layer;
[0037] Before the step of epitaxially preparing a gallium oxide layer on the surface of the gallium nitride layer away from the semiconductor substrate, the method further includes: cleaning and drying the gallium nitride layer;
[0038] The step of epitaxially preparing a gallium oxide layer on a surface of the gallium nitride layer away from the semiconductor substrate comprises: placing the gallium nitride layer in an oxygen plasma molecular beam epitaxy device to prepare a gallium oxide layer;
[0039] The step of forming an electrode pattern on a surface of the gallium oxide layer away from the semiconductor substrate comprises: spin coating a photoresist layer on the gallium oxide layer; exposing the photoresist layer through a mask; and removing the gallium oxide layer in a developer to form an electrode pattern composed of the photoresist.
[0040] The method of preparing the electrode structure layer on the electrode pattern comprises: depositing a metal material on the electrode pattern; and removing the electrode pattern composed of the photoresist to form the electrode structure layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0042] Figure 1 A schematic structural diagram of an ultraviolet photodetector with a high linear dynamic range provided by an embodiment of the present invention;
[0043] Figure 2 A schematic diagram of photocarrier motion in an ultraviolet photodetector with a high linear dynamic range provided by an embodiment of the present invention;
[0044] Figure 3 A schematic diagram of a current-voltage curve of a high linear dynamic range ultraviolet photodetector in a linear coordinate provided by an embodiment of the present invention;
[0045] Figure 4 A schematic diagram of the transient response speed of the ultraviolet photodetector with a high linear dynamic range provided by an embodiment of the present invention under a voltage bias of 0.3V;
[0046] Figure 5 A schematic diagram of the linear dynamic range of the ultraviolet photodetector with a high linear dynamic range provided by an embodiment of the present invention under a voltage bias of 0.3V;
[0047] Figure 6 A schematic diagram of a valence band spectrum of a gallium oxide layer obtained by using X-ray photoelectron spectroscopy (XPS) in a high linear dynamic range ultraviolet photodetector provided by an embodiment of the present invention;
[0048] Figure 7 A schematic diagram of the process of a method for preparing an ultraviolet photodetector with a high linear dynamic range provided by an embodiment of the present invention;
[0049] 100, semiconductor substrate; 200, gallium nitride layer; 300, gallium oxide layer; 400, first electrode; 401, first electrode body; 402, first extension portion; 500, second electrode; 501, second electrode body; 502, second extension portion. DETAILED DESCRIPTION
[0050] The present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It is understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only some structures related to the present invention are shown in the accompanying drawings, rather than all structures. In the following description, the description of known structures and technologies is omitted to avoid unnecessary confusion of the concept of the present invention. Various structural schematic diagrams according to embodiments of the present invention are shown in the accompanying drawings. These figures are not drawn to scale, and some details are magnified for the purpose of clear expression, and some details may be omitted. The shapes of various regions and layers shown in the figures and the relative sizes and positional relationships between them are only exemplary, and may be deviated due to manufacturing tolerances or technical limitations in practice, and those skilled in the art may additionally design regions / layers with different shapes, sizes, and relative positions according to actual needs. In the context of the present invention, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element, or there may be an intermediate layer / element between them. In addition, if one layer / element is "on" another layer / element in one orientation, then when the orientation is reversed, the layer / element may be "below" the other layer / element.
[0051] At present, solar-blind photodetectors in the 200nm to 280nm band can play an important role in missile early warning tracking, flame detection, local confidential communications, and ozone detection. Therefore, solar-blind photodetectors based on wide-bandgap semiconductor materials have become a research hotspot for researchers. Among them, β-phase gallium oxide in gallium oxide materials is the most stable one, and its band gap corresponds to a wavelength of 250nm, which corresponds to the solar-blind band. There is no need to adjust the band gap, and it has obvious advantages in solar-blind photodetectors.
[0052] Among the various types of gallium oxide-based ultraviolet photodetectors in the current related technologies, MSM (Metal-Semiconductor-Metal) type ultraviolet photodetectors or Schottky (metal-semiconductor) junction type ultraviolet photodetectors have the problem of slow response speed; and although avalanche type ultraviolet photodetectors can induce carrier multiplication through impact ionization, thereby obtaining a higher responsiveness without affecting the response speed, they need to work at a higher voltage, which is not conducive to energy saving, and avalanche type photodetectors have a complex device structure, thus requiring a strict manufacturing process, which greatly hinders the realization of miniaturization and low cost goals. In addition, the internal gain of the above-mentioned gallium oxide-based ultraviolet photodetector usually changes with the change of light intensity, so that the change of photocurrent with light intensity is nonlinear, and the linear dynamic range that can be used for further application research is very small, which is not conducive to the application of actual photoelectric detection.
[0053] The embodiments of the present invention provide a high linear dynamic range ultraviolet photodetector, such as Figure 1 and Figure 2 As shown, including:
[0054] A semiconductor substrate 100, a gallium nitride layer 200, a gallium oxide layer 300 and an electrode structure layer, wherein the gallium nitride layer 200 is arranged on the semiconductor substrate 100, and the gallium nitride layer 200 is of a first conductivity type; the gallium oxide layer 300 is arranged on the surface of the gallium nitride layer 200 away from the semiconductor substrate 100, and the gallium oxide layer 300 is of a second conductivity type opposite to the first conductivity type, and the resistivity of the gallium oxide layer 300 is higher than the resistivity of the gallium nitride layer 200; the electrode structure layer is located on the surface of the gallium oxide layer 300 away from the semiconductor substrate 100, and the electrode structure layer includes a first electrode 400 and a second electrode 500 arranged on the same plane at intervals, and a light-transmitting area arranged in a hollow manner.
[0055] Specifically, the ultraviolet photodetector, by constructing a simple specific combination of a low-resistance gallium nitride layer 200 and a high-resistance gallium oxide layer 300 and a structure in which the first electrode 400 and the second electrode 500 are arranged on the same plane on the gallium oxide layer 300, forms heterojunctions between the gallium nitride layer 200 and the gallium oxide layer 300 corresponding to the first electrode 400 and between the gallium nitride layer 200 and the gallium oxide layer 300 corresponding to the second electrode 500, and the two heterojunction structures are arranged in a lateral spacing. The hollow light-transmitting area between the first electrode 400 and the second electrode 500 refers to the area of the electrode structure layer for light transmission. Specifically, when the first electrode 400 and the second electrode 500 are opaque electrodes, the light-transmitting area refers to the area not covered by the first electrode 400 and the second electrode 500; when the first electrode and the second electrode are transparent electrodes, the light-transmitting area includes the area above the entire gallium oxide layer 300. The light-transmitting area ensures that the ultraviolet photodetector has a sufficiently large light-receiving area. When the ultraviolet photodetector is irradiated by ultraviolet light and the first electrode 400 and the second electrode 500 are respectively connected to the positive and negative electrodes of the external bias voltage, diffusion and drift of carriers are generated between the gallium nitride layer 200 and the gallium oxide layer 300 in the area below the first electrode 400 and the second electrode 500, thereby generating current, thereby forming a transistor effect, that is, Figures 3 to 5As shown, the current can rise rapidly with the increase of voltage, and then reach saturation at a smaller voltage, and the saturation current increases linearly with the increase of light intensity; in addition, as the light intensity changes, the internal gain of the detector remains basically constant, so that the responsiveness remains constant with the increase of light intensity, that is, the photocurrent changes linearly, reflecting a larger linear dynamic range. Therefore, the ultraviolet photodetector in this embodiment has better response performance and a larger linear dynamic range at a lower voltage, fast response speed, and the photocurrent hardly changes within a certain voltage range. It is easy to integrate with the signal processing system, save energy, have high system stability, and simple preparation process.
[0056] The linear dynamic range is the range in which the photocurrent changes linearly with the light intensity.
[0057] When the ultraviolet photodetector is irradiated by ultraviolet light, and the first electrode 400 and the second electrode 500 are connected to the positive and negative electrodes of the external bias voltage respectively, the photogenerated carriers inside the detector move as follows: Figure 2 shown.
[0058] Taking the case where the first electrode 400 is connected to an external positive charge and the second electrode 500 is connected to an external negative charge as an example, the region of the gallium oxide layer 300 below the first electrode 400 to which a positive voltage is applied forms a collector, and the region of the gallium oxide layer 300 below the second electrode 500 to which a negative voltage is applied forms an emitter. After light is applied, electron-hole pairs are generated near the collector junction formed between the gallium oxide layer 300 and the gallium nitride layer 200 below the first electrode 400, and the electron-hole pairs are separated under the action of the space charge region to form a photocurrent. At the same time, the holes move downward to the gallium nitride layer 200 region as the base region under the action of diffusion and drift, and further drift laterally toward the bottom of the emitter under the action of the electric field, so that the potential of the gallium nitride layer 200 is higher than that of the emitter. Therefore, the emitter junction formed between the gallium oxide layer 300 and the gallium nitride layer 200 under the forward biased second electrode 500 will allow electrons to be injected downward from the emitter into the base region; at the same time, since the gallium oxide layer 300 of this embodiment is a high-resistance structural layer that is not intentionally doped, the electrons also tend to move from the high-resistance gallium oxide layer 300 to the gallium nitride layer 200 with a lower resistivity, and drift and diffuse under the action of the electric field, with a fast response speed, thereby producing a normal transistor effect.
[0059] The ultraviolet photodetector with high linear dynamic range constructed as described above can effectively reduce the response time of the device and expand the linear dynamic range of the device. It can have better response performance at a lower voltage, and the photocurrent hardly changes within a certain voltage range, and is easy to integrate with the signal processing system.
[0060] In this embodiment, the first conductivity type is P type, and the second conductivity type is N type. That is, the ultraviolet photodetector of this embodiment has a P type low resistivity gallium nitride layer 200 deposited on the semiconductor substrate 100, and an N type high resistivity gallium oxide layer 300 deposited on the gallium nitride layer 200. For gallium oxide materials, the preparation of P type gallium oxide is extremely difficult, and the N type gallium oxide in this embodiment is simpler.
[0061] Specifically, the gallium oxide material will have some oxygen vacancies after growth, so it will show a weak N-type. The gallium oxide layer 300 in this embodiment is not doped and tends to be an intrinsic weak N-type high-resistance structure. Figure 6 In the valence band spectrum of the gallium oxide layer 300 obtained by X-ray photoelectron spectroscopy (XPS) in the present embodiment shown in the figure, the linear fitting line of the gallium oxide layer 300 intersects with the horizontal axis at 2.8 eV, which means that the top of the valence band of the prepared oxide layer is located 2.8 eV below the Fermi level. Since the band gap width of gallium oxide is 4.85 eV, the Fermi level of the gallium oxide layer 300 is located above the midline of the band gap, but very close to the midline of the band gap, that is, the gallium oxide layer 300 grown in the present embodiment is N-type and in a high resistivity state.
[0062] Specifically, the gallium oxide layer 300 in this embodiment is an N-type gallium oxide layer 300 that is biased toward intrinsic; the bandgap width of gallium nitride is smaller than the bandgap width of gallium oxide. Due to the high bandgap width of gallium oxide, its resistivity is very high, which is higher than that of intrinsic gallium nitride. Therefore, the resistivity of the P-type doped gallium nitride layer 200 is lower than that of intrinsic gallium nitride, and even lower than that of the gallium oxide layer 300 that is biased toward intrinsic. In fact, the resistivity of the P-type gallium nitride layer 200 is 10 ohm-cm at room temperature, while the resistivity of the gallium oxide layer 300 is a high resistance state that is difficult to detect even by the Hall effect.
[0063] As a preferred implementation, the first electrode 400 and the second electrode 500 of the electrode structure layer in this embodiment are both formed as interdigital electrodes.
[0064] The first electrode 400 includes a first electrode body 401 and four evenly spaced first extensions 402. The first electrode body 401 is disposed on a first side of the gallium oxide layer 300. The four first extensions 402 extend from the first electrode body 401 and extend toward a second side of the gallium oxide layer 300. The first side and the second side are two opposite sides of the surface of the gallium oxide layer 300.
[0065] The second electrode 500 includes a second electrode body 501 and four second extensions 502. The second electrode body 501 is disposed on the second side of the gallium oxide layer 300. The second extensions 502 extend from the second electrode body 501 and extend toward the first side of the gallium oxide layer 300.
[0066] The first extension portion and the second extension portion are arranged crosswise and staggered.
[0067] Specifically, the edge of the first electrode body 401 is aligned with the left edge of the gallium oxide layer 300, i.e., the first end, and the edge of the second electrode body 501 is aligned with the right edge of the gallium oxide layer 300, i.e., the second end, to ensure the maximum lateral excitation current. The first electrode body 401 and the second electrode body 501 are of the same size and shape, both of which are rectangular structures with a length of 300 μm and a width of 200 μm. The size and shape of the single first extension 402 and the single second extension 502 are the same, both of which are long strip structures with a length of 300 μm and a width of 12 μm. The preparation is simple and efficient, and the gallium oxide layer 300 and the gallium nitride layer 200 under the electrode structure layer can form a good heterojunction to produce a transistor effect, improve the response speed, and ensure the response performance and a large linear dynamic range.
[0068] Furthermore, the first electrode body 401 and the second electrode body 501 are parallel to each other, the first extension part 402 and the second extension part 502 are parallel to each other, and the first electrode body 401 and the first extension part 402 are perpendicular to each other, and the second electrode body 501 and the second extension part 502 are perpendicular to each other; the spacing between adjacent first extension parts 402 and second extension parts 502 is 2μm-12μm, such as 2μm, 4μm, 6μm, 8μm, 10μm. The electrode structure layer has enough hollow areas to transmit light to achieve photoelectric conversion.
[0069] In one embodiment, the thickness of the gallium oxide layer 300 is 0.05 μm-0.2 μm, and the thickness of the gallium nitride layer 200 is 4.5 μm-5 μm. The gallium oxide layer 300 is configured as a thin film structure. When an external voltage is applied, the carriers of the gallium oxide layer 300 and the gallium nitride layer 200 under the first electrode 400 and the second electrode 500 can diffuse and move rapidly in the vertical direction, greatly improving the response speed of the ultraviolet photodetector. The gallium nitride layer 200 provides sufficient carriers for current generation.
[0070] In one embodiment, the semiconductor substrate 100 may be a gallium nitride single crystal homogeneous with the gallium nitride layer 200, or an aluminum nitride single crystal heterogeneous with the gallium nitride layer 200, or sapphire, or silicon carbide, or single crystal silicon. Different semiconductor substrates 100 are selected according to different design requirements to ensure detector performance and improve economic benefits.
[0071] In one embodiment, the first electrode 400 and the second electrode 500 may be metal composite electrodes of Ti / Au, or Ti / Al / Ni / Au, or Ti / Pt. Taking the first electrode 400 as a Ti / Au metal composite electrode as an example, the first electrode 400 includes a Ti film layer and an Au film layer, the side of the first electrode 400 close to the gallium oxide layer 300 is a Ti film layer, and the upper side of the Ti film layer is an Au film layer. The metal composite electrode has lower roughness, a smoother contact interface, and a lower lattice mismatch layer thickness. In addition, the film layer in direct contact with the gallium oxide layer 300 as an intermediate layer helps promote the mutual diffusion phenomenon between the metal electrode and the semiconductor interface, which is beneficial to increase adhesion and reduce potential barriers.
[0072] The present invention also provides a method for preparing a UV photodetector with a high linear dynamic range. Figure 7 As shown, the following steps are included:
[0073] S701 , providing a semiconductor substrate 100 .
[0074] The semiconductor substrate 100 may be made of a gallium nitride single crystal that is homogeneous with the gallium nitride layer 200 , or an aluminum nitride single crystal that is heterogeneous with the gallium nitride layer 200 , or sapphire, or silicon carbide, or single crystal silicon.
[0075] S702 , forming a gallium nitride layer 200 on the semiconductor substrate 100 , wherein the gallium nitride layer 200 is of a first conductivity type.
[0076] The first conductivity type may be N type or P type. An epitaxial layer of the gallium nitride layer 200 is grown on the semiconductor substrate 100 by metal organic chemical vapor phase epitaxy technology.
[0077] S703 , epitaxially forming a gallium oxide layer 300 on a surface of the gallium nitride layer 200 away from the semiconductor substrate 100 , wherein the gallium oxide layer 300 is of a second conductivity type opposite to the first conductivity type, and a resistivity of the gallium oxide layer 300 is higher than that of the gallium nitride layer 200 .
[0078] When the gallium nitride layer 200 is N-type doped, the gallium oxide layer 300 is the opposite P-type conductivity type; when the gallium nitride layer 200 is P-type doped, the gallium oxide layer 300 is the opposite N-type conductivity type. A gallium oxide layer 300 with a higher resistivity of a certain thickness is epitaxially grown on the gallium nitride layer 200 by an oxygen plasma assisted molecular beam epitaxy method, and the resistivity of the gallium nitride layer 200 is lower than that of the gallium oxide layer 300.
[0079] S704 , forming an electrode pattern on a surface of the gallium oxide layer 300 away from the semiconductor substrate 100 .
[0080] By using a standard photolithography exposure process on the photoresist layer, an electrode pattern having partial grooves is formed on the surface of the gallium oxide layer 300 .
[0081] S705, preparing an electrode structure layer on the electrode pattern.
[0082] Metal material is deposited on the electrode pattern using magnetron sputtering technology, and the metal material in the groove of the electrode pattern is retained after stripping the photoresist to form an electrode structure layer. The stripped area is the light-receiving area suitable for light to pass through.
[0083] The ultraviolet photodetector with high linear dynamic range prepared by the above method includes a specific combination of a simple low-resistance gallium nitride layer 200 and a high-resistance gallium oxide layer 300, and a structure in which a first electrode 400 and a second electrode 500 are arranged on the same plane of the gallium oxide layer 300 at an interval, and heterojunctions are formed between the corresponding gallium nitride layer 200 and the gallium oxide layer 300 below the first electrode 400 and between the corresponding gallium nitride layer 200 and the gallium oxide layer 300 below the second electrode 500, and the two heterojunction structures are arranged laterally at an interval. The hollow area between the first electrode 400 and the second electrode 500 ensures that the ultraviolet photodetector has a sufficiently large light-receiving area. When the ultraviolet photodetector is irradiated by ultraviolet light and the first electrode 400 and the second electrode 500 are respectively connected to the positive and negative electrodes of the external bias voltage, diffusion and drift of carriers occur between the gallium nitride layer 200 and the gallium oxide layer 300 in the area below the first electrode 400 and the second electrode 500, thereby generating current, thereby forming a transistor effect, which can effectively reduce the response time of the device and expand the linear dynamic range of the device, and can have better response performance at a lower voltage, and the photocurrent hardly changes within a certain voltage range, is easy to integrate with the signal processing system, and has a simple preparation process.
[0084] The following is a detailed description of the method for preparing the ultraviolet photodetector with high linear dynamic range of the present embodiment, which includes the following steps:
[0085] S1, select sapphire as the semiconductor substrate 100 and clean it at high temperature to remove surface contamination.
[0086] S2, forming a low-resistivity P-type gallium nitride layer 200 on the semiconductor substrate 100. The epitaxial layer of the gallium nitride layer 200 is grown on the semiconductor substrate 100 by metal organic chemical vapor phase epitaxy technology, that is, using H2 as a carrier gas, carrying MO source (high-purity metal organic compound) trimethylgallium, bis(ocene magnesium) and ammonia and other reactants through a multi-channel pipeline, and after the gas is evenly mixed, it is introduced into the reaction chamber to grow a P-type gallium nitride layer 200 thin film with a thickness of 4.5μm-5μm on the sapphire semiconductor substrate 100.
[0087] S3, epitaxially prepare a high resistivity N-type gallium oxide layer 300 on the surface of the gallium nitride layer 200. The epitaxial wafer of the gallium nitride layer 200 obtained in S2 is ultrasonically cleaned in acetone, ethanol and deionized water solution for 10 minutes, and then blown dry with nitrogen. An approximately 0.1 μm gallium oxide layer 300 is epitaxially grown on the surface of the gallium nitride layer 2 by an oxygen plasma assisted molecular beam epitaxy device.
[0088] The specific conditions for using oxygen plasma assisted molecular beam epitaxy are: the gallium source temperature is 830°C, the temperature of the semiconductor substrate 100 is 700°C, and the growth gas pressure is 2.6×10 -3 Pa, the oxygen plasma power is 250 W, and the epitaxial growth time is 2.5 h. After the growth is completed, the oxygen plasma source is turned off, and the gallium oxide layer 300 is vacuum annealed at 700° C. for 10 min.
[0089] S4, photolithography is performed to form an electrode pattern on the surface of the gallium oxide layer 300. The specific steps include:
[0090] The gallium oxide layer 300 epitaxial wafer obtained in S3 was dried in an oven at 130° C. for 30 min;
[0091] Spin coating adhesion promoter, using AZ5214 photoresist for coating;
[0092] The coated gallium oxide layer 300 epitaxial wafer was placed on a heating plate at 100° C. and heated for 4 minutes to remove the solvent of the photoresist;
[0093] The epitaxial wafer of the gallium oxide layer 300 after removing the photoresist solvent was placed on a German MA / BA8 Gen4 photolithography machine and used a customized mask for alignment and exposure processing, with an exposure time of 3.7 seconds. The interdigital electrode pattern of the mask is as follows: the size of a single interdigital electrode forming the first electrode 400 and the second electrode 500 is 700 μm in length and 200 μm in width, wherein the electrode body is a rectangular structure with a length of 300 μm and a width of 200 μm, and the first electrode 400 and the second electrode 500 respectively include 4 extensions to form an interdigital electrode structure layer, and a single extension is a strip-shaped structure with a length of 300 μm and a width of 12 μm, and the spacing between adjacent extensions is 12 μm.
[0094] The gallium oxide layer 300 epitaxial wafer with electrode pattern preparation was placed on a heating plate at a temperature of 100°C for 2 minutes and then reversely baked;
[0095] The inversion baked gallium oxide layer 300 epitaxial wafer is placed on the photolithography machine for the second flood exposure, the exposure mode is Flood-E, and the time is set to 5s;
[0096] The exposed gallium oxide layer 300 epitaxial wafer is placed in a developer for development, and the development time is 90 seconds;
[0097] The substrate was washed with deionized water for 1 min, dried with nitrogen gas, and placed under an optical microscope to observe the interdigitated electrode pattern with grooves formed on the photoresist after photolithography.
[0098] S5, preparing an electrode structure layer on the electrode pattern.
[0099] A 10nm / 50nm Ti / Au metal composite layer is deposited on the surface of the gallium oxide layer 300 obtained in S4 by magnetron sputtering, and the corresponding interdigitated electrode structure layer is formed after the photoresist is stripped off. The area where the stripped photoresist is located is the light receiving area suitable for light to pass through.
[0100] In a nitrogen atmosphere at 400° C., the obtained device was subjected to rapid thermal annealing for 5 minutes at a flow rate of 4 slm, thereby completing the preparation of the ultraviolet photodetector with a high linear dynamic range of this embodiment.
[0101] In the above description, the technical details of the patterning and etching of each layer are not described in detail. However, those skilled in the art should understand that various technical means can be used to form layers, regions, etc. of desired shapes. In addition, in order to form the same structure, those skilled in the art can also design methods that are not completely the same as the methods described above. In addition, although the various embodiments are described above separately, this does not mean that the measures in the various embodiments cannot be used in combination to advantage.
[0102] In the description of this specification, the description with reference to the terms "this embodiment", "one embodiment", "some embodiments", "example", "specific example", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, unless they are contradictory.
[0103] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0104] In the description of the present invention, it is to be understood that the terms “center”, “longitudinal”, “lateral”, “length”, “width”, “thickness”, “up”, “down”, “front”, “back”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inside”, “outside”, “clockwise”, “counterclockwise”, “axial”, “radial”, “circumferential”, etc., indicating orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0105] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0106] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and simple improvements made to the essential contents of the present invention should be included in the protection scope of the present invention.
Claims
1. A high linear dynamic range ultraviolet photodetector, characterized in that: include: A semiconductor substrate (100); A gallium nitride layer (200) is disposed on the semiconductor substrate (100), and the gallium nitride layer (200) is of a first conductivity type; a gallium oxide layer (300) disposed on a surface of the gallium nitride layer (200) on a side away from the semiconductor substrate (100), the gallium oxide layer (300) being of a second conductivity type opposite to the first conductivity type, and having a resistivity higher than that of the gallium nitride layer (200); The electrode structure layer is located on the surface of the gallium oxide layer (300) on the side away from the semiconductor substrate (100), and comprises a first electrode (400) and a second electrode (500) arranged on the same plane at intervals, and a light-transmitting area arranged in a hollow manner.
2. The ultraviolet photodetector with high linear dynamic range according to claim 1, characterized in that: The first conductivity type is P type, and the second conductivity type is N type.
3. The ultraviolet photodetector with high linear dynamic range according to claim 1 or 2, characterized in that: The first electrode (400) and the second electrode (500) of the electrode structure layer are interdigitated electrodes; The first electrode (400) comprises a first electrode body (401) and at least one first extension portion (402), wherein the first electrode body (401) is arranged on a first side of the surface of the gallium oxide layer (300), and the first extension portion (402) extends from the first electrode body (401) and extends toward a second side of the gallium oxide layer (300); wherein the first side and the second side are two opposite sides of the surface of the gallium oxide layer (300); The second electrode (500) comprises a second electrode body (501) and at least one second extension portion (502), wherein the second electrode body (501) is arranged on the second side, and the second extension portion (502) extends from the second electrode body (501) and extends toward the first side; The first extension portion (402) and the second extension portion (502) are arranged in a cross-staggered manner.
4. The ultraviolet photodetector with high linear dynamic range according to claim 3, characterized in that: The first electrode body (401) and the second electrode body (501) are parallel to each other, the first extension portion (402) and the second extension portion (502) are parallel to each other, the first electrode body (401) and the first extension portion (402) are perpendicular to each other, and the second electrode body (501) and the second extension portion (502) are perpendicular to each other; The distance between adjacent first extension portions (402) and second extension portions (502) is 2 μm-12 μm.
5. The ultraviolet photodetector with high linear dynamic range according to claim 1 or 2, characterized in that: The gallium oxide layer (300) has a thickness of 0.05 μm-0.2 μm.
6. The ultraviolet photodetector with high linear dynamic range according to claim 1 or 2, characterized in that: The gallium nitride layer (200) has a thickness of 4.5 μm-5 μm.
7. The ultraviolet photodetector with high linear dynamic range according to claim 1 or 2, characterized in that: The semiconductor substrate (100) is a gallium nitride single crystal homogeneous with the gallium nitride layer (200), or an aluminum nitride single crystal heterogeneous with the gallium nitride layer (200), or sapphire, or silicon carbide, or single crystal silicon.
8. The ultraviolet photodetector with high linear dynamic range according to claim 1 or 2, characterized in that: The first electrode (400) and the second electrode (500) are metal composite electrodes of Ti / Au, or Ti / Al / Ni / Au, or Ti / Pt.
9. A method for preparing an ultraviolet photodetector with a high linear dynamic range, characterized in that: The steps include: Providing a semiconductor substrate (100); forming a gallium nitride layer (200) on the semiconductor substrate (100), wherein the gallium nitride layer (200) is of a first conductivity type; epitaxially preparing a gallium oxide layer (300) on a surface of the gallium nitride layer (200) away from the semiconductor substrate (100), the gallium oxide layer (300) being of a second conductivity type opposite to the first conductivity type, and the resistivity of the gallium oxide layer (300) being higher than the resistivity of the gallium nitride layer (200); forming an electrode pattern on a surface of the gallium oxide layer (300) that is away from the semiconductor substrate (100); An electrode structure layer is prepared on the electrode pattern.
10. The method for preparing a UV photodetector with a high linear dynamic range according to claim 9, characterized in that: The method of forming a gallium nitride layer (200) on the semiconductor substrate (100) comprises: providing reactants for preparing the gallium nitride layer (200) and mixing them in a pipeline through a carrier gas; and introducing the uniformly mixed gas into a reaction chamber to grow the gallium nitride layer (200); Before the step of epitaxially preparing a gallium oxide layer (300) on a surface of the gallium nitride layer (200) away from the semiconductor substrate (100), the method further includes: cleaning and drying the gallium nitride layer (200); The step of epitaxially preparing a gallium oxide layer (300) on a surface of the gallium nitride layer (200) on one side away from the semiconductor substrate (100) comprises: placing the gallium nitride layer (200) in an oxygen plasma molecular beam epitaxy device to prepare the gallium oxide layer (300); The step of forming an electrode pattern on a surface of the gallium oxide layer (300) on a side away from the semiconductor substrate (100) comprises: spin coating a photoresist layer on the gallium oxide layer (300); exposing the photoresist layer through a mask; and placing the gallium oxide layer (300) in a developer to remove the gallium oxide layer (300) to form an electrode pattern composed of the photoresist; The method of preparing the electrode structure layer on the electrode pattern comprises: depositing a metal material on the electrode pattern; and removing the electrode pattern composed of the photoresist to form the electrode structure layer.
Citation Information
Cited By
Ultraviolet synaptic device based on gallium nitride-gallium oxide heterojunction and preparation method thereof
CN119317199A