Method for preparing manganese-zinc-iron-based positive electrode material of sodium-ion battery by recycling waste zinc-manganese battery

Preparing manganese-zinc-iron-based cathode materials for sodium-ion batteries by recycling zinc-manganese batteries solves the problems of complex and high-cost traditional recycling processes, enables the production of high value-added materials, reduces recycling costs and improves industrial production efficiency.

CN118738376AActive Publication Date: 2024-10-01GANNAN NORMAL UNIV
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411217375.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-02
Publication Date
2024-10-01
Estimated Expiration
2044-09-02

AI Technical Summary

Technical Problem

Traditional recycling of zinc-manganese batteries has complex processes, high energy consumption, high costs, and low added value of recycled products, resulting in poor industrial production efficiency and difficulty in promotion.

Method used

A method of recycling waste zinc-manganese batteries to prepare manganese-zinc-iron-based cathode materials for sodium-ion batteries includes recycling, crushing, washing, drying, sorting, adding metal powder, stirring reaction, co-precipitation and high-temperature calcination to synthesize high added value Sodium manganese zinc ferrite cathode material for sodium ion batteries.

Benefits of technology

It reduces recycling costs, improves the utilization rate of manganese, zinc, and iron, reduces secondary pollution, and forms a high value-added sodium-ion battery material suitable for industrial production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738376A_ABST
    Figure CN118738376A_ABST
Patent Text Reader

Abstract

The invention discloses a method for preparing a manganese-zinc-iron-based positive electrode material of a sodium-ion battery by recycling a waste zinc-manganese battery, and relates to the technical field of recycling of electronic wastes. The general formula of the manganese-zinc-iron-based positive electrode material of the sodium-ion battery is NanMn < 1-x-y > Zn < x > Fe < y > O < 2, 0.3 lt >, n is less than or equal to 1.0, 0.01 lt; x is less than or equal to 0.5, 0.01 lt; and y < = 0.5. According to the method for preparing the manganese-zinc-iron-based positive electrode material of the sodium-ion battery by recycling the waste zinc-manganese battery, after manganese-zinc-iron substances of the waste zinc-manganese battery are leached out by adopting a solution leaching method, impurities are removed by utilizing a replacement method; proper materials are added according to the component proportion requirement of the sodium-ion battery manganese-zinc-iron-based positive electrode material, so that a sodium-ion battery manganese-zinc-iron-based positive electrode material product is prepared, and the sodium-ion battery manganese-zinc-iron-based positive electrode material is excellent in electrochemical performance and high in added value; and the problems of high energy consumption and low separation purity caused by separation of manganese, zinc and iron in the recycling process of the waste zinc-manganese battery are solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of recycling and cyclic utilization of electronic waste, and in particular to a method for recycling waste zinc-manganese batteries to prepare manganese-zinc-iron-based positive electrode materials for sodium ion batteries. Background Art

[0002] Zinc-manganese dry batteries have the advantages of low cost and large capacity, and are currently the most widely used consumer primary batteries. The global annual consumption of zinc-manganese batteries is about 14 billion, and it is still growing. Waste zinc-manganese batteries contain a large amount of manganese and zinc and other heavy metal elements. Improper handling of a large number of discarded zinc-manganese batteries will cause soil, water and air pollution. Therefore, it is very important to develop an economically feasible recycling and high-value utilization technology. Recycling waste zinc-manganese batteries to prepare functional materials has gradually become a research hotspot.

[0003] However, waste zinc-manganese dry batteries contain heavy metals such as manganese, zinc, iron, and copper. Traditional recycling methods are too complicated, with high recycling costs and low added value. Most of them only recycle specific metals in waste batteries, and there is also secondary pollution in the recycling process, which is not conducive to promotion and application in actual projects.

[0004] Waste zinc-manganese batteries contain more manganese and zinc. Manganese is usually recovered to prepare MnSO4 or MnCO3; zinc is recovered to prepare zinc chloride. Although the above-mentioned recycled products are in great demand and have a wide range of applications in industrial production, these products are the most basic raw materials in industrial production and have low added value; and the recycling process often involves complex separation and purification processes, and the recycling cost is high. This directly affects the benefits of industrial production, making it difficult for the recycling of zinc-manganese batteries to develop on a large scale in industrial production. Therefore, it is necessary to develop new low-cost recycling processes and high-value-added recycling products, increase the value of product recycling, improve the technical content of production, and synthesize high-value-added products, so as to achieve the purpose of reducing costs and increasing efficiency. Summary of the invention

[0005] In view of the problems of complex separation process, high energy consumption, high cost and low added value of recycled products in existing zinc-manganese battery recycling technology, the present invention provides a method for recycling waste zinc-manganese batteries to prepare manganese-zinc-iron-based positive electrode materials for sodium ion batteries.

[0006] To achieve the above object, the present invention provides a sodium ion battery manganese zinc iron based positive electrode material, the sodium ion battery manganese zinc iron based positive electrode material general formula is Na n Mn 1-x-y Zn x Fe y O2, 0.3< n ≤1.0、0.01< x≤0.5, 0.01 <y≤0.5。

[0007] A method for preparing the above-mentioned manganese-zinc-iron-based positive electrode material for a sodium ion battery comprises the following steps: S1, recycling and crushing waste zinc-manganese batteries to prepare a first battery powder; S2, washing and filtering the first battery powder to obtain a first solution and a second battery powder respectively; S3, drying, sorting and removing impurities from the second battery powder to obtain the third battery powder; S4, add strong acid solution and co-solvent to the aqueous solution of the third battery powder, and then n Mn 1-x- y Zn x Fe y Add metal zinc powder, iron powder or manganese powder in a stoichiometric ratio in O2 to adjust the manganese-zinc-iron metal ratio in the third battery powder, stir to complete the reaction, and filter to obtain a filter residue and a second solution; S5, using the first solution as an alkali solution and a complexing agent and the second solution as a metal solution for a coprecipitation reaction, filtering, washing, and drying to obtain manganese, zinc, and iron hydroxide; S6. Mix manganese-zinc-iron hydroxide and sodium salt, and calcine at high temperature to synthesize manganese-zinc-iron based positive electrode material for sodium ion battery.

[0008] Preferably, in step S2, the water washing conditions are: deionized water, water temperature 20-100° C., and the amount of water used is 0.1-10 times the mass of the first battery powder.

[0009] Preferably, in step S3, the drying temperature is 80°C, and the sorting includes: air sorting and screening, wherein the screening uses vibrating screening with a mesh size of 10-300 meshes.

[0010] Preferably, in step S4, the co-solvent includes one or a combination of sodium sulfite, sodium thiosulfate, hydrogen peroxide solution, hydrazine hydrate, and ascorbic acid.

[0011] Preferably, in step S6, the sodium salt includes one or a combination of sodium hydroxide, sodium carbonate, sodium bicarbonate, sodium nitrate and sodium oxalate.

[0012] Preferably, in step S6, the molar ratio of manganese zinc iron hydroxide to sodium salt is: (Mn+Zn+Fe):Na=1.0:(0.3-1.05).

[0013] Preferably, in step S6, the high temperature calcination conditions are: calcination at a temperature of 200-500° C. for 1-24 hours, or calcination at a temperature of 600-1000° C. for 1-48 hours in air or oxygen.

[0014] The present invention discloses a method for recycling waste zinc-manganese batteries to prepare manganese-zinc-iron-based positive electrode materials for sodium ion batteries, which has the following beneficial effects: (1) After extracting the inherent elements manganese, zinc and iron in the waste zinc-manganese batteries by solution leaching method, the impurities are removed by replacement method, and appropriate materials are added according to the composition ratio requirements of the manganese, zinc and iron-based positive electrode materials of sodium ion batteries to synthesize high-value-added sodium ion battery manganese zinc ferrite positive electrode materials; while solving the environmental pollution of waste zinc-manganese batteries, high-quality and efficient utilization of the main substances contained in the waste zinc-manganese batteries is achieved; (2) The traditional recycling of waste zinc-manganese batteries requires the gradual separation of metal elements, which has a long recycling process, high energy consumption and high cost. The obtained products have no clear means of utilization and low added value. The present invention directly crushes the waste zinc-manganese batteries and removes impurities, and analyzes the content and proportion of metal elements in the battery powder through ICP element analysis, thereby avoiding the complex separation process of the main elements manganese, zinc and iron in the recycling process and reducing the recycling cost. (3) The method of the present invention rationally utilizes manganese dioxide, metallic zinc, iron sheet, potassium hydroxide and ammonium chloride, which are the main components of waste zinc-manganese batteries, with a high recovery rate and less secondary pollutants.

[0015] The technical solution of the present invention is further described in detail below through the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 This is a flow chart of a method for preparing a manganese-zinc-iron-based positive electrode material for a sodium ion battery using waste zinc-manganese batteries in Example 1 of the present invention; Figure 2 This is an XRD diagram of the manganese-zinc-iron-based positive electrode material for a sodium ion battery in Example 1 of the present invention; Figure 3 This is a first charge and discharge curve diagram of the manganese-zinc-iron-based positive electrode material for a sodium ion battery in Example 1 of the present invention; Figure 4 This is a rate performance diagram of the manganese-zinc-iron-based positive electrode material for a sodium ion battery in Example 1 of the present invention; Figure 5 This is a cycle performance diagram of the manganese-zinc-iron based positive electrode material for a sodium ion battery in Example 1 of the present invention. DETAILED DESCRIPTION

[0017] In order to make the purpose, technical scheme and advantages disclosed in the embodiments of the present invention more clearly understood, the embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the embodiments of the present invention and are not intended to limit the embodiments of the present invention. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.

[0018] Embodiment 1 A method for recycling waste zinc-manganese batteries to prepare manganese-zinc-iron-based positive electrode materials for sodium ion batteries, the process is as follows Figure 1 As shown, the specific steps include: (1) 1.0 kg of used zinc-manganese batteries were put into a crusher for crushing to obtain 0.96 kg of first battery powder.

[0019] (2) The first battery powder was washed with 500 mL of deionized water at 55° C. and filtered to obtain 473 mL of a first solution and 1.18 kg of a second battery powder.

[0020] (3) The second battery powder was dried in a forced air drying oven at 80°C for 12 h. The diaphragm was first removed by an air separator. Then, a 100-mesh vibrating screen was used to remove the copper cap and iron cylinder, etc., to obtain 0.672 kg of the third battery powder.

[0021] (4) Pour 100 g of the third battery powder into a 1.0 L reactor, add 100 mL of deionized water base liquid, stir evenly, then add 200 mL of 2.5 mol / L dilute sulfuric acid and 15 mL of 20% hydrogen peroxide solution, stir to dissolve completely, analyze the manganese, zinc and iron metal ratio in the solution by ICP elemental analysis, and then continue to add 4.8 g of metallic zinc powder and 13.5 g of metallic iron powder to adjust the manganese, zinc and iron metal ratio to 0.5:0.25:0.25, stir to react completely, and obtain 18.4 g of filter residue and 304 mL of the second solution after filtration.

[0022] (5) Using the first solution as the base liquid, 500 mL of an alkaline solution of 2.0 mol / L potassium hydroxide and 0.2 mol / L ammonia water was prepared. Using the second solution as the base liquid, 250 mL of a 2.0 mol / L manganese-zinc-iron metal liquid was prepared. The alkaline solution and the metal liquid were added into the reactor at a constant liquid addition rate using a constant flow pump. The co-precipitation reaction was carried out for 5 hours under the conditions of controlling the pH value at 9.2, the reaction temperature at 60°C, and the stirring speed at 300 r / min. The manganese-zinc-iron hydroxide was obtained by filtration, washing with water, and drying.

[0023] (6) 11.6 g of manganese zinc iron hydroxide and 7.42 g of sodium carbonate were mixed evenly, and calcined at 450 °C for 6 h under air flow, and then heated to 920 °C for 12 h to synthesize sodium manganese zinc ferrite positive electrode material Na 0.7 Mn 0.5 Zn 0.25 Fe 0.25 O2.

[0024] The obtained P2-type layered sodium manganese zinc ferrite positive electrode material Na 0.7 Mn 0.5 Zn 0.25 Fe 0.25The XRD spectrum of O2 is as follows Figure 2 As shown in the figure, Na 0.7 Mn 0.5 Zn 0.25 Fe 0.25 The peak shape of O2 is consistent with that of PDF 27-0751, with sharp diffraction peaks and no other obvious impurity peaks, indicating that the synthesized Na 0.7 Mn 0.5 Zn 0.25 Fe 0.25 The O2 positive electrode material has a P2-type layered phase structure and good crystallinity.

[0025] The P2 type layered sodium ion battery sodium manganese zinc ferrite positive electrode material Na prepared in this embodiment 0.7 Mn 0.5 Zn 0.25 Fe 0.25 O2 is used as the positive electrode active material of sodium ion battery to prepare the battery. The specific steps are: Sodium ion button battery was prepared with sodium ion manganese-based positive electrode material as positive electrode active material, metal sodium sheet as negative electrode, 1 mol / L NaPF6 and EC / DMC (volume ratio 1:1) as electrolyte.

[0026] The battery's first charge and discharge curve, rate performance and cycle performance were tested, and the results were as follows: Figure 3~Figure 5 It is shown that the sodium manganese zinc ferrite positive electrode material for sodium ion batteries has a high first discharge capacity (164mAh / g); has excellent rate performance, and under the condition of 5C (500mA / g) current charge and discharge, the discharge capacity can still reach 85mAh / g; has good cycle performance, and the capacity retention rate reaches 77% after 100 charge and discharge cycles at 0.5C current density.

[0027] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that they can still modify or replace the technical solution of the present invention with equivalents, and these modifications or equivalent replacements cannot cause the modified technical solution to deviate from the spirit and scope of the technical solution of the present invention.

Claims

1. A manganese-zinc-iron-based positive electrode material for a sodium ion battery, characterized in that: The general formula of the manganese-zinc-iron-based positive electrode material for sodium-ion batteries is Na n Mn 1-x-y Zn x Fe y O2, 0.3< n ≤1.0、0.01< x ≤0.5, 0.01 <y≤0.5。 2. A method for preparing a manganese-zinc-iron-based positive electrode material for a sodium ion battery as claimed in claim 1, characterized in that: The method comprises the following steps: S1, recovering and crushing waste zinc-manganese batteries to prepare a first battery powder; S2, washing and filtering the first battery powder to obtain a first solution and a second battery powder respectively; S3, drying, sorting and removing impurities from the second battery powder to obtain the third battery powder; S4, add strong acid solution and co-solvent to the aqueous solution of the third battery powder, and then n Mn 1-x-y Zn x Fe y Add metal zinc powder, iron powder or manganese powder in a stoichiometric ratio in O2 to adjust the manganese-zinc-iron metal ratio in the third battery powder, stir to complete the reaction, and filter to obtain a filter residue and a second solution; S5, using the first solution as an alkali solution and a complexing agent and the second solution as a metal solution for a coprecipitation reaction, filtering, washing, and drying to obtain manganese, zinc, and iron hydroxide; S6. Mix manganese-zinc-iron hydroxide and sodium salt, and calcine at high temperature to synthesize manganese-zinc-iron based positive electrode material for sodium ion battery.

3. The method for preparing a manganese-zinc-iron-based positive electrode material for a sodium ion battery according to claim 2, characterized in that: In step S2, the washing conditions are: deionized water, water temperature 20-100°C, and the amount of water used is 0.1-10 times the mass of the first battery powder.

4. The method for preparing a manganese-zinc-iron-based positive electrode material for a sodium ion battery according to claim 2, characterized in that: In step S3, the drying temperature is 80°C, and the sorting includes: air sorting and screening, wherein the screening uses vibrating screening with a mesh size of 10-300 meshes.

5. The method for preparing a manganese-zinc-iron-based positive electrode material for a sodium ion battery according to claim 2, characterized in that: In step S4, the co-solvent is one or a combination of sodium sulfite, sodium thiosulfate, hydrogen peroxide solution, hydrazine hydrate, and ascorbic acid.

6. The method for preparing a manganese-zinc-iron-based positive electrode material for a sodium ion battery according to claim 2, characterized in that: In step S6, the sodium salt is one or a combination of sodium hydroxide, sodium carbonate, sodium bicarbonate, sodium nitrate, and sodium oxalate.

7. The method for preparing a manganese-zinc-iron-based positive electrode material for a sodium ion battery according to claim 2, characterized in that: In step S6, the molar ratio of manganese zinc iron hydroxide to sodium salt is: (Mn+Zn+Fe):Na=1.0:(0.3-1.05).

8. The method for preparing a manganese-zinc-iron-based positive electrode material for a sodium ion battery according to claim 2, characterized in that: In step S6, the high temperature calcination conditions are: calcination at a temperature of 200-500° C. for 1-24 hours, or calcination at a temperature of 600-1000° C. for 1-48 hours under air or oxygen conditions.

Citation Information

Patent Citations

  • Recycling method of waste zinc-manganese batteries

    CN110752384A

  • Method for regenerating sodium battery positive electrode material by using waste lithium manganate

    CN115472948A

  • Method for preparing sodium-ion battery positive electrode material by recycling waste battery positive electrode (nickel cobalt lithium manganate) and application of sodium-ion battery positive electrode material

    CN115611321A

  • Positive electrode material and preparation method and application thereof

    CN117613229A

  • Process for recharging spent batteries involves converting crushed batteries into manganese-zinc-iron solution, precipitating manganese-zinc-iron hydroxides and manganese-zinc-iron carbonates and reacting with iron oxide to form ferrite

    DE102004013531A1