Photocurable resin composition containing self-crosslinkable polymer

By using a photocurable resin composition of an aryl ketone and an aliphatic hydrocarbon residue, an etching-resistant protective film is formed, which solves the problems of metal contamination and cross-contamination in semiconductor manufacturing and improves the manufacturing efficiency and quality of semiconductor devices.

CN118742855APending Publication Date: 2024-10-01NISSAN CHEM CORP
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202380022676.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-02-22
Filing Date
2023-02-21
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the semiconductor device manufacturing process, unintended adhesion of metal resist films causes problems with electrical characteristics, and there is a risk of metal contamination and cross-contamination due to the spread of the coating film, and the etching resistance of existing protective films is insufficient.

Method used

Using a photocurable resin composition containing a self-crosslinking polymer containing an aryl ketone residue and an aliphatic hydrocarbon residue, an etching-resistant protective film can be formed without using a polymerization initiator , covering the ends of semiconductor manufacturing wafers by spin coating to prevent metal contamination and improve manufacturing efficiency.

Benefits of technology

It achieves the formation of a highly etching-resistant protective film, prevents metal contamination, improves the yield of good products in semiconductor manufacturing equipment, and simplifies the manufacturing process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005000885600000031
    Figure BDA0005000885600000031
  • Figure BDA0005000885600000051
    Figure BDA0005000885600000051
  • Figure BDA0005000885600000091
    Figure BDA0005000885600000091
Patent Text Reader

Abstract

Provided is a material capable of forming a protective film having sufficient etching resistance required to protect an end portion of a substrate for semiconductor manufacturing in the manufacturing of a semiconductor device. [Solution] A photocurable composition which contains a solvent and a self-crosslinkable polymer that contains a first monomer unit that contains an aryl ketone residue in a side chain and a second monomer unit that contains an aliphatic hydrocarbon residue and / or an aromatic ring residue in a side chain, the aliphatic hydrocarbon residues comprise carbon atoms which are easy to generate hydrogen abstracting reaction; a method for manufacturing a semiconductor device includes: a step for forming a resist film on a semiconductor substrate; a step for forming a resist pattern by irradiating the resist film with light or an electron beam and then developing the resist film; and a step for processing a semiconductor substrate by etching, the method for manufacturing a semiconductor device further comprising a step for forming a protective film made of the photocurable composition on the front-surface end portion of a wafer for semiconductor manufacturing and optionally on the chamfered portion and / or the back-surface end portion of the wafer, and a step for manufacturing a semiconductor device, the method further comprising a step for forming a protective film made of the photocurable composition on the front-surface end portion of the wafer for semiconductor manufacturing and optionally on the chamfered portion and / or the back-surface end portion of the wafer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field The present invention relates to a photocurable resin composition containing a cross-linkable polymer; further relates to a protective film on the end surface of a substrate (wafer) for semiconductor manufacturing in a semiconductor device manufacturing process, a protective film forming composition for forming the protective film, a semiconductor manufacturing wafer obtained using the protective film, and a method for manufacturing the semiconductor manufacturing wafer and a semiconductor device. Background Art In the manufacture of semiconductor devices, along with the complication of manufacturing processes, for example, for the purpose of improving etching selectivity, a method of applying a chemical solution containing metal to a wafer has been studied. In addition, from the perspective of the resolution of the resist pattern when, for example, extreme ultraviolet light (EUV) is used for exposure, and the aspect of having high etching resistance, a resist containing inorganic metals has been studied to form a resist film. However, the attachment of metal to the non-scheduled parts of the wafer in the manufacturing process of the semiconductor device greatly affects the electrical characteristics of the semiconductor device. However, when forming a coating film containing metal as described above, the chemical solution supplied to the front of the wafer spreads to the peripheral end face of the wafer and the peripheral edge of the back, forming a coating film until these non-scheduled peripheral end faces and the peripheral edge of the back, thus, there is a worry that these parts are contaminated by metal. Moreover, since the contaminated part of the wafer contacts the processing device of the wafer such as the exposure device and the etching device, and the conveying mechanism of the wafer, the wafer that is transported and processed after the wafer via these processing devices and the conveying mechanism is also contaminated by metal, that is, there is a worry that cross contamination is generated. In order to deal with such a problem, the following technology is disclosed: when forming a coating film on the surface of a substrate, a protective film is formed on the peripheral portion of the substrate, at least the peripheral end surface and the peripheral portion of the back side of the substrate, thereby forming the coating film in a manner that the peripheral portion of the substrate, i.e., the peripheral end surface and the peripheral portion of the back side, do not contact the coating film (Patent Document 1). In addition, a method for manufacturing a semiconductor device is disclosed, which suppresses the peeling of the film from the chamfered portion of the substrate by providing a simple additional step (in order to prevent the first mask on the chamfered portion from collapsing, a second mask is formed in a manner that covers the first mask on the chamfered portion) (Patent Document 2). However, a film material that functions as a protective film at the edge of a substrate is required to have high etching resistance, and further improvement is desired. Prior art literature Patent Literature Patent Document 1: Japanese Patent Application Publication No. 2017-098333 Patent Document 2: Japanese Patent Application Publication No. 2011-228340 Summary of the invention Problems to be solved by the invention Therefore, an object of the present invention is to provide a resin material capable of forming a protective film having sufficient etching resistance required for protecting an end portion of a substrate (wafer) for semiconductor manufacturing in the manufacture of a semiconductor device. In addition, the problems to be solved by the invention of this application also include providing a protective film, a protective film forming composition for forming the protective film, a semiconductor manufacturing wafer made using the protective film, a semiconductor manufacturing wafer and a manufacturing method of a semiconductor device, wherein the protective film can completely cover the end of a semiconductor manufacturing substrate (wafer) by adopting a simple coating method in the manufacture of the semiconductor device. Means for solving problems The present invention includes the following contents.

[0001] A photocurable resin composition comprises a self-crosslinking polymer (A) and a solvent (B), wherein the self-crosslinking polymer (A) comprises a first monomer unit (a) and a second monomer unit (b), wherein the first monomer unit (a) comprises an aromatic ketone residue in a side chain; and the second monomer unit (b) comprises an aliphatic hydrocarbon residue (b-1) and / or an aromatic ring residue (b-2) in a side chain, wherein the aliphatic hydrocarbon residue (b-1) comprises a carbon atom that is susceptible to hydrogen abstraction reaction. [1-1] According to the photocurable resin composition described in [1], the self-crosslinking polymer (A) contains a second monomer unit, the second monomer unit contains an aliphatic hydrocarbon residue (b-1) and an aromatic ring residue (b-2), and the aliphatic hydrocarbon residue (b-1) contains a carbon atom that is susceptible to hydrogen abstraction reaction.

[0002] The photocurable resin composition according to [1], further comprising a crosslinkable polymer or a crosslinkable compound (C) other than the self-crosslinkable polymer (A).

[0003] According to the photocurable resin composition described in [2], the crosslinkable group in the crosslinkable polymer or crosslinkable compound (C) is selected from epoxy group, (meth)acrylic group, vinyl group, carboxylic acid group, thiol group, silanol group, cinnamoyl group and hydroxyl group.

[0004] The photocurable resin composition according to any one of [1] to [3], which has a viscosity of 100 cps or less at 25°C.

[0005] A composition for forming a wafer edge protective film for semiconductor manufacturing, comprising the photocurable resin composition according to any one of [1] to [4].

[0006] A protective film is a cured product of a coating film made from the composition for forming a wafer edge protective film for semiconductor manufacturing according to [5].

[0007] The protective film according to [6], which has a thickness of 1 to 500 nm.

[0008] The protective film according to [6] or [7] is used to prevent metal contamination at the edge of the wafer.

[0009] The protective film according to any one of [6] to [8], which is obtained by curing with light having a wavelength of 170 to 800 nm.

[0010] A semiconductor manufacturing wafer having a protected wafer edge, wherein the semiconductor manufacturing wafer is formed by applying the composition for forming a semiconductor manufacturing wafer edge protective film as described in [5] to the edge of a wafer precursor.

[0011] A method for manufacturing a semiconductor device, comprising the following steps: Step (A), forming a resist film on a semiconductor substrate; Step (B) of forming a resist pattern by irradiating the resist film with light or electron beams and then developing the resist film; and Step (C), processing the semiconductor substrate by etching, The method for manufacturing the semiconductor device further includes the following step (X): A protective film made of the composition for forming a semiconductor wafer edge protective film according to [5] is formed on the front edge of a semiconductor wafer and optionally on the chamfered portion and / or back edge of the wafer.

[0012] The method for manufacturing a semiconductor device according to

[11] , further comprising step (X) before step (A).

[0013] The method for manufacturing a semiconductor device according to

[11] , further comprising a step (X) between the step (A) and the step (B).

[0014] The method for manufacturing a semiconductor device according to

[11] , further comprising step (X) after step (B) or step (C).

[0015] The method for manufacturing a semiconductor device according to any one of

[11] to

[14] , further comprising, after step (X), a step (Y) of removing a portion of the resist film on the protective film.

[0016] The method for manufacturing a semiconductor device according to any one of

[11] to

[14] , further comprising a step (Z) of removing the protective film after the step (X).

[0017] The method for manufacturing a semiconductor device according to

[15] , further comprising a step (Z) of removing the protective film after the step (Y).

[0018] The method for manufacturing a semiconductor device according to any one of

[11] to

[17] , wherein the resist film contains a metal.

[0019] The method for manufacturing a semiconductor device according to any one of

[11] to

[18] , wherein in the step (X), the composition for forming a wafer edge protective film for semiconductor manufacturing according to [5] is applied and a predetermined area is exposed and developed.

[0020] The method for manufacturing a semiconductor device according to

[16] or

[17] , wherein step (Z) is performed by ashing, or by treatment with hydrofluoric acid, an organic solvent, an alkaline developer, or a semiconductor cleaning solution.

[0021] A method for manufacturing a semiconductor wafer, comprising the following steps: The composition for forming a wafer edge protective film for semiconductor manufacturing described in [5] is applied to the edge of a wafer precursor to manufacture a wafer with the edge protected.

[0022] The photocurable resin composition according to any one of [1] to [4], wherein the aryl ketone residue is a residue of an aryl ketone selected from acetophenone, benzophenone, anthraquinone, anthrone, a heteroatom-substituted anthrone analog of the following structural formula, and derivatives of these compounds having substituents, X is O, S or NR, and R is a hydrogen atom, a hydrocarbon group or an acyl group.

[0023] The photocurable resin composition according to any one of [1] to [4], wherein the carbon atom in the hydrocarbon chain (b-1) that is susceptible to hydrogen abstraction reaction is selected from a tertiary carbon atom, a secondary carbon atom, and a methyl group, a methylene group, or a methine group directly connected to an aromatic ring.

[0024] The photocurable resin composition according to any one of [1] to [4], wherein the aromatic ring (b-2) is an aromatic ring having 6 to 40 carbon atoms which may have a substituent.

[0025] The photocurable resin composition according to any one of [1] to [4], wherein the ratio of the number of repetitions of the first monomer unit to the number of repetitions of monomer units other than the first monomer unit including the second monomer unit is selected so that when a film having a film thickness of 300 nm is formed, the transmittance of the film at a wavelength of 300 nm is 0.01% or more, preferably 0.1% or more, and more preferably 1% or more.

[0026] A self-crosslinking polymer (A) comprises a first monomer unit (a) and a second monomer unit (b), wherein the first monomer unit (a) comprises an aromatic ketone residue in a side chain; and the second monomer unit (b) comprises an aliphatic hydrocarbon residue (b-1) and / or an aromatic ring residue (b-2) in a side chain, wherein the aliphatic hydrocarbon residue (b-1) comprises a carbon atom that is susceptible to hydrogen abstraction reaction. Effects of the Invention The photocurable resin composition as one embodiment of the present invention can form a protective film having sufficient etching resistance even without using a polymerization initiator, particularly a wafer edge protective film for semiconductor manufacturing. In addition, in the manufacture of a semiconductor device which is one embodiment of the present invention, a protective film that can completely cover the end of a semiconductor manufacturing substrate (wafer) is used by a simple coating method. This can prevent cross contamination caused by metal contamination in the subsequent semiconductor device manufacturing process, thereby improving the yield of good semiconductor manufacturing equipment. DETAILED DESCRIPTION <1. Photocurable resin composition [1] / composition for forming a wafer edge protective film for semiconductor manufacturing [5]> (1-1) The photocurable resin composition which is one embodiment of the present invention contains a self-crosslinking polymer (A) and a solvent (B). The photocurable resin composition may further contain a crosslinkable polymer or a crosslinkable compound (C) other than the self-crosslinkable polymer (A). The photocurable resin composition can also be preferably used as a protective film forming composition for protecting the front edge of a wafer for semiconductor manufacturing (a protective film forming composition for wafer edge for semiconductor manufacturing, hereinafter sometimes simply referred to as a "protective film forming composition"). [1-2; Self-crosslinking polymer (A)] (1-2-1) The self-crosslinking polymer (A) is a polymer comprising a first monomer unit (a) and a second monomer unit (b), wherein the first monomer unit (a) comprises an aromatic ketone residue in a side chain; and the second monomer unit (b) comprises an aliphatic hydrocarbon residue (b-1) and / or an aromatic ring residue (b-2) in a side chain, wherein the aliphatic hydrocarbon residue (b-1) comprises a carbon atom that is susceptible to hydrogen abstraction reaction. The self-crosslinking polymer may optionally contain monomer units other than the first and second monomer units as long as the effects of the present invention are not impaired. (1-2-2) First Monomer Unit (1-2-2-1) The aryl ketone residue described in the first monomer unit is a residue of a compound (monoaryl ketone or diaryl ketone) in which one or two aromatic groups are directly bonded to a carbonyl group [-C(=O)-]. The aryl ketone residue acts as a photoreactive group and can be activated by light of a specific wavelength such as ultraviolet light to cause a cross-linking reaction. It should be noted that in this specification, the so-called "residue" of a certain compound is used to indicate an organic group obtained by replacing the hydrogen atoms bonded to the carbon atoms or heteroatoms (nitrogen, oxygen, sulfur atoms, etc.) constituting the compound with a connecting bond for covalent bonding. The aryl ketone residue constitutes the side chain of the self-crosslinking polymer as one embodiment of the present invention through an appropriate linking group such as an ester bond, an amide bond, or the like. It should be noted that the term "side chain" in this specification broadly includes a chemical group covalently bonded to a main chain and suspended from the side, and is used synonymously with a so-called side chain group. Specific examples of aryl ketone residues include acetophenone, benzophenone, anthraquinone, anthrone, heteroatom-substituted anthrone analogs of the following structural formula, and aryl ketone residues obtained by derivatives of these compounds having substituents, wherein X is O, S or NR, and R is a hydrogen atom, a hydrocarbon group (preferably having 1 to 4 carbon atoms) or an acyl group (preferably having 1 to 4 carbon atoms). Substituents such as hydroxyl, amino, and carboxyl groups may exist on the aromatic rings of these aryl ketone residues, or covalent bonds such as ester bonds (-O-CO- or -CO-O-), amide bonds (-NH-CO- or -CO-NH-), carbamate bonds (-NH-CO-O- or -O-CO-NH-), carbonate bonds (-O-CO-O-), and urea bonds (-NH-CO-NH-) may be formed between X of the nitrogen atom-substituted anthrone analog (X=NH) and functional groups such as carboxyl, hydroxyl, and amino groups constituting the main chain of the polymer, thereby constituting side chains of self-crosslinking polymers. Two of the covalent bonds such as an ester bond (-O-CO- or -CO-O-), an amide bond (-NH-CO- or -CO-NH-), a carbamate bond (-NH-CO-O- or -O-CO-NH-), a carbonate bond (-O-CO-O-), a urea bond (-NH-CO-NH-) may be combined, and these two covalent bonds may be connected to each other through a divalent linking group L, such as a hydrocarbon chain whose chain may be interrupted by a heteroatom (oxygen atom, etc.). For example, -CO-O-O-CO-, -CO-NH-L-NH-CO-, etc. may be exemplified. (1-2-2-2) Among these aryl ketone residues, the residue of benzophenone or a derivative thereof having a substituent (hereinafter referred to as "benzophenone compound") is preferable from the viewpoint that the lifetime of the lowest excited triplet state is relatively long and a photochemical reaction easily occurs. Examples of the benzophenone compound include 2,2'-dihydroxy-4-methoxybenzophenone, 2,2'-dihydroxy-4,4'-dimethoxydisulfobenzophenone disodium, 2,2'-dihydroxy-4,4'-dimethoxybenzophenone, 2,2',3,4-tetrahydroxybenzophenone, 2,2',4,4'-tetrahydroxybenzophenone, 2,2',3,4,4'-pentahydroxybenzophenone, 2,2'-dihydroxy-4-methoxybenzophenone, 2,3, 3'4,4',5'-hexahydroxybenzophenone, 2,3,4,4'-tetrahydroxybenzophenone, 2,3,4-trihydroxybenzophenone, 2,4,4'-trihydroxybenzophenone, 2,4,5-trihydroxybenzophenone, 2,4,6-trihydroxybenzophenone, 2,4-dihydroxy-4'-diethylaminobenzophenone, 2,4-dihydroxy-4'-dimethylaminobenzophenone, 2,4-dihydroxybenzophenone, 4,4'-dihydroxybenzophenone, 2-hydroxy-4-( 2-Hydroxy-3-methacryloyloxy)propoxybenzophenone, 2-hydroxy-4'-dimethylaminobenzophenone, 2-hydroxy-4-isooctyloxybenzophenone, 2-hydroxy-4-n-octyloxybenzophenone, 2-hydroxy-4-octyloxybenzophenone, 2-hydroxy-4-acetyloxyethoxybenzophenone, 2-hydroxy-4-octadecyloxybenzophenone, 2-hydroxy-4-dodecyloxybenzophenone, 2-hydroxy-4-methoxy-2'-carboxybenzophenone , 2-hydroxy-4-methoxy-5-sulfonic acid benzophenone, 2-hydroxy-4-methoxybenzophenone, 2-hydroxybenzophenone, 4,4'-dihydroxybenzophenone, 4,4'-bis(diethylamino)benzophenone, 4,4'-bis(dimethylamino)benzophenone, 4',6-dihydroxy-2-naphthobenzophenone, 4-dodecyloxy-2-hydroxybenzophenone, 4-hydroxybenzophenone, N,N,N',N'-tetramethyl-4,4'-diaminobenzophenone, etc. Vinylbenzophenone which may have a substituent may also be mentioned. In addition, examples of structures capable of extracting hydrogen radicals by ultraviolet irradiation include benzyl, o-benzoylbenzoate, thioxanthone, 3-coumarone, 2-ethylanthraquinone, and camphorquinone. Compounds having these structures can be used as compounds from which the first monomer unit is derived. (1-2-2-3) The monomer constituting the main chain portion of the first monomer unit may be any monomer as long as it is a polymerizable monomer having a functional group (carboxyl group, hydroxyl group, amino group, etc.) that can form a covalent bond with an aromatic ketone residue, such as an ester bond (-O-CO- or -CO-O-), an amide bond (-NH-CO- or -CO-NH-), a carbamate bond (-NH-CO-O- or -O-CO-NH-), a carbonate bond (-O-CO-O-), a urea bond (-NH-CO-NH-), or the like. (1-2-2-4) As specific examples of the first monomer unit that can be suitably used, when the aryl ketone residue is a residue of a benzophenone compound, the following compounds can be cited, namely, benzophenone, 4-acryloyloxyethoxy-4'-bromobenzophenone, 4-methacryloyloxybenzophenone, 4-methacryloyloxyethoxybenzophenone, 4-methacryloyloxy-4'-methoxybenzophenone, 4-methacryloyloxyethoxy-4'-methoxybenzophenone, 4-methacryloyloxy-4'-bromobenzophenone, 4-methacryloyloxyethoxy-4'-bromobenzophenone, and the like. (1-2-3) Second Monomer Unit (1-2-3-1) The so-called aliphatic hydrocarbon residue containing carbon atoms that are prone to hydrogen abstraction reaction in the second monomer unit refers to an aliphatic hydrocarbon residue (preferably a monovalent hydrocarbon residue) containing carbon atoms that undergoes hydrogen abstraction reaction and contributes to the crosslinking reaction through a photochemical reaction caused by an aromatic ketone residue in the side chain. For example, it is an aliphatic hydrocarbon chain containing carbon atoms selected from the following carbon atoms: tertiary carbon atoms; secondary carbon atoms, preferably secondary carbon atoms with hydroxyl groups; and methyl, methylene or methine groups directly connected to unsaturated organic groups [aromatic rings, ethylene groups, etc.); methylene or methine groups directly connected to hydroxyl oxygen atoms. It can be arbitrarily substituted with substituents such as hydroxyl groups, alkoxy groups, and aryl groups. The so-called aliphatic hydrocarbon residue here can be explained as follows: in order to facilitate the abstraction reaction of the hydrogen atom bonded to the carbon atom in the residue, substitution may be performed on the aromatic ring, or the chain of the aliphatic hydrocarbon residue may be interrupted by the insertion of an aromatic ring in the middle (for example, -R-Ar-R when R is an aliphatic hydrocarbon chain and Ar is an aromatic ring). The aliphatic hydrocarbon residue in the side chain can be directly covalently bonded to the main chain, or it can form a side chain through a covalent bond such as an ester bond (-O-CO- or -CO-O-), an amide bond (-NH-CO- or -CO-NH-), a carbamate bond (-NH-CO-O- or -O-CO-NH-), a carbonate bond (-O-CO-O-), a urea bond (-NH-CO-NH-) or the like with the functional groups such as the carboxyl group, hydroxyl group, and amino group of the polymer constituting the main chain. As for covalent bonds such as ester bonds (-O-CO- or -CO-O-), amide bonds (-NH-CO- or -CO-NH-), carbamate bonds (-NH-CO-O- or -O-CO-NH-), carbonate bonds (-O-CO-O-), and urea bonds (-NH-CO-NH-), two of them may be combined, and these two covalent bonds may be connected to each other through a divalent linking group L, such as a hydrocarbon chain whose chain may be interrupted by a heteroatom (oxygen atom, etc.). For example, -CO-O-O-CO-, -CO-NH-L-NH-CO-, etc. may be exemplified. The aliphatic hydrocarbon residue preferably has 1 to 18 carbon atoms. In addition, from the viewpoint of improving the adhesion between the self-crosslinking polymer and the coating surface, it is preferred that a hydrophilic substituent such as a hydroxyl group is bonded to the carbon atom that is prone to hydrogen abstraction reaction. For example, -CH(OH)- and the like can be mentioned. As an aliphatic hydrocarbon residue containing such a carbon atom, CH 3 CH(OH)CH 2 - etc. are preferred as the aliphatic hydrocarbon residue. (1-2-3-2) As the second monomer containing an aliphatic hydrocarbon residue in the side chain, the following specific examples can be given. As the alkyl (meth)acrylate, an acrylate monomer having a branched or cyclic alkyl chain having 1 to 22 carbon atoms, such as 2-ethylhexyl (meth)acrylate, isobutyl (meth)acrylate, cyclohexyl (meth)acrylate, isobornyl (meth)acrylate, and dicyclopentyl (meth)acrylate monomers; Hydroxyl group-containing monomers such as 2-hydroxyethyl (meth)acrylate, 2-hydroxypropyl (meth)acrylate, 3-hydroxypropyl (meth)acrylate, 2-hydroxybutyl (meth)acrylate, 4-hydroxybutyl (meth)acrylate, 1,4-cyclohexanedimethanol mono(meth)acrylate, 1-glycerol (meth)acrylate, 2-hydroxyethyl (meth)acrylamide, N-hydroxypropyl (meth)acrylamide, and allyl alcohol. (1-2-3-3) The so-called aromatic ring residue in the second monomer unit can be any aromatic ring residue as long as it is an aromatic ring residue that undergoes a hydrogen abstraction reaction through a photochemical reaction caused by an aromatic ketone residue in the side chain and contributes to the cross-linking reaction. It can be different from the side chain of the first monomer unit containing the aromatic ketone residue mentioned above. More specifically, there can be mentioned a residue having an aromatic ring structure having 6 to 40 carbon atoms which may have a substituent, and specifically, there can be mentioned benzene, naphthalene, anthracene, acenaphthene, fluorene, tri-o-phenylene, phenalene, phenanthrene, indene, indane, indene, pyrene, Perylene, tetracene, pentacene, coronene, heptacene, benzo[a]anthracene, dibenzophenanthrene, dibenzo[a,j]anthracene, etc. The above aromatic ring residue may optionally have a substituent, and examples of the substituent include a hydroxyl group, a halogen atom, a carboxyl group, a nitro group, a cyano group, a methylenedioxy group, an acetoxy group, a methylthio group, an amino group, or an alkoxy group having 1 to 9 carbon atoms, in which a part or all of the hydrogen atoms in the above aromatic ring structure having 6 to 40 carbon atoms are present. Examples of the alkoxy group having 1 to 9 carbon atoms include methoxy, ethoxy, n-propoxy, isopropoxy, n-butoxy, isobutoxy, sec-butoxy, tert-butoxy, n-pentoxy, 1-methyl n-butoxy, 2-methyl n-butoxy, 3-methyl n-butoxy, 1,1-dimethyl n-propoxy, 1,2-dimethyl n-propoxy, 2,2-dimethyl n-propoxy, 1-ethyl n-propoxy, n-hexyloxy, 1-methyl n-pentoxy, 2-methyl n-pentoxy, 3-methyl n-pentoxy, 4- Methyl-n-pentyloxy, 1,1-dimethyl-n-butoxy, 1,2-dimethyl-n-butoxy, 1,3-dimethyl-n-butoxy, 2,2-dimethyl-n-butoxy, 2,3-dimethyl-n-butoxy, 3,3-dimethyl-n-butoxy, 1-ethyl-n-butoxy, 2-ethyl-n-butoxy, 1,1,2-trimethyl-n-propoxy, 1,2,2-trimethyl-n-propoxy, 1-ethyl-1-methyl-n-propoxy, 1-ethyl-2-methyl-n-propoxy, n-heptyloxy, n-octyloxy and n-nonyloxy, etc. (1-2-3-4) The monomer constituting the main chain portion of the second monomer unit may be any monomer as long as it is a polymerizable monomer having a functional group (carboxyl, hydroxyl, amino, etc.) that can form a covalent bond such as an ester bond (-O-CO- or -CO-O-), an amide bond (-NH-CO- or -CO-NH-), a carbamate bond (-NH-CO-O- or -O-CO-NH-), a carbonate bond (-O-CO-O-), or a urea bond (-NH-CO-NH-). For specific examples, in addition to vinyl monomers such as styrene, the main chain portions of the exemplified monomers in (1-2-3-2) above can also be referred to. Here, the aliphatic hydrocarbon residue can form a covalent bond with a functional group (carboxyl group, hydroxyl group, amino group, etc.) of a monomer constituting the main chain portion through the aliphatic hydrocarbon portion constituting a functional group such as an alkoxy group or an alkylamino group. The aromatic ring residue also has a substituent such as a hydroxyl group, an amino group, or a carboxyl group on the aromatic ring, and can form a covalent bond with a functional group such as a carboxyl group, a hydroxyl group, or an amino group constituting the main chain of the polymer. These covalent bonds include ester bonds (-O-CO- or -CO-O-), amide bonds (-NH-CO- or -CO-NH-), carbamate bonds (-NH-CO-O- or -O-CO-NH-), carbonate bonds (-O-CO-O-), urea bonds (-NH-CO-NH-), and the like. In addition, two of the covalent bonds such as an ester bond (-O-CO- or -CO-O-), an amide bond (-NH-CO- or -CO-NH-), a carbamate bond (-NH-CO-O- or -O-CO-NH-), a carbonate bond (-O-CO-O-), a urea bond (-NH-CO-NH-) may be combined, and these two covalent bonds may be connected to each other through a divalent linking group L, such as a hydrocarbon chain whose chain may be interrupted by a heteroatom (oxygen atom, etc.). For example, -CO-O-O-CO-, -CO-NH-L-NH-CO-, etc. may be exemplified. (1-2-3-5) The second monomer unit undergoes a photochemical reaction caused by the aryl ketone residue of the first monomer unit and is cured by crosslinking. Here, the term "self-crosslinking" means that the polymerization can be cured by a crosslinking reaction without adding a polymerization initiator. The ratio of the number of repetitions of the first monomer unit to the number of repetitions of the second monomer unit can be determined in consideration of the film thickness to be formed by photocuring of the self-crosslinking polymer and the light absorption by the aryl ketone residue. This is because, in order to allow the light used for curing to fully reach the bottom of the film to be formed, it is necessary to consider the ratio of the first monomer unit as a standard of the degree of light absorption and the film thickness corresponding to the distance for the light to reach. The ratio of the repetition number of the first monomer unit to the repetition number of monomer units other than the first monomer unit (including the second monomer unit) can be adjusted so that when a film with a film thickness of 300 nm is formed, the transmittance of the film at a wavelength of 300 nm is greater than 0.01%, preferably greater than 0.1%, and more preferably greater than 1%. (1-2-3-6) When the self-crosslinking polymer contains other monomer units different from the first and second monomers, the above (1-2-3-5) is applied instead of reading the ratio of the number of repetitions of the first monomer unit to the number of repetitions of monomer units other than the first monomer unit including the second monomer unit. (1-2-3-7) The self-crosslinking polymer as one embodiment of the present invention contains the first monomer unit having an aryl ketone residue in a side chain as a monomer unit, and thus can be self-crosslinked without adding a polymerization initiator, and can reduce the oxygen atom content, thereby improving etching resistance. (1-3: Solvent (B)) Examples of the solvent contained in the photocurable resin composition as one embodiment of the present invention include water, ethylene glycol monomethyl ether, ethylene glycol monoethyl ether, methyl cellosolve acetate, ethyl cellosolve acetate, diethylene glycol monomethyl ether, diethylene glycol monoethyl ether, propylene glycol, propylene glycol monomethyl ether, propylene glycol monoethyl ether, propylene glycol monomethyl ether acetate, propylene glycol propyl ether acetate, toluene, xylene, methyl ethyl ketone, methyl isobutyl ketone, cyclopentanone, cyclohexanone, cycloheptanone, 4-methyl- 2-pentanol, methyl 2-hydroxyisobutyrate, ethyl 2-hydroxyisobutyrate, ethyl ethoxylate, 2-hydroxyethyl acetate, methyl 3-methoxypropionate, ethyl 3-methoxypropionate, ethyl 3-ethoxypropionate, methyl 3-ethoxypropionate, methyl pyruvate, ethyl pyruvate, ethyl acetate, butyl acetate, ethyl lactate, butyl lactate, 2-heptanone, methoxycyclopentane, anisole, γ-butyrolactone, N-methylpyrrolidone, N,N-dimethylformamide and N,N-dimethylacetamide. These solvents can be used alone or in combination of two or more. The solvent may be added so that the photocurable resin composition of one embodiment of the present invention has an appropriate viscosity. Generally, the solvent is preferably added in an amount of about 100 to 3,000 parts by mass based on 100 parts by mass of the total amount of the self-crosslinkable polymer (A) and the crosslinkable polymer or compound (C) optionally contained. (1-4: Cross-linking polymer or cross-linking compound (C)) (1-4-1) The photocurable resin composition which is one embodiment of the present invention may further contain a crosslinkable polymer or a crosslinkable compound (C). The crosslinkable polymer or crosslinkable compound (C) refers to a polymer or compound having a crosslinkable group other than the self-crosslinkable polymer (A). Here, the crosslinkable group refers to a group that can form a crosslinked structure by the action of light, electron beams, other electromagnetic waves, free radicals, acid, heat, water, oxygen, etc. Examples thereof include, but are not limited to, epoxy groups, acrylic groups, vinyl groups, carboxylic acid groups, thiol groups, silanol groups, cinnamoyl groups, hydroxyl groups (including phenolic hydroxyl groups), etc. Examples of the crosslinkable polymer or the crosslinkable compound (C) include the following, but are not limited to these. · Epoxy (meth)acrylate, ·Cinnamic acid grafted epoxy phenolic varnish, Bakelite, a thermosetting material obtained by polycondensation of phenol and aldehyde with the removal of water and the formation of a three-dimensional network, For example, melamine resins such as trimethylolmelamine and hexamethylolmelamine, urea resins such as dimethylol propylene urea, dimethylol ethylene urea, and dimethylol hydroxy urea, and aminoplast resins such as dimethylol uron resin. (Blocked) isocyanates, Vinyl ether, ·Polysiloxane resin having (meth)acrylic group Epoxy resin. (1-4-2) The crosslinkable polymer or crosslinkable compound (C) may be a crosslinkable compound described in International Publication No. 2018 / 190380 and comprising at least one, preferably at least two, partial structures selected from the partial structures (I) represented by the following formula (1-1) to (1-7). (Where, R 1 , R 1a , R 3 , R 5a and R 6a each independently represents an alkylene group having 1 to 10 carbon atoms, an arylene group having 6 to 40 carbon atoms (the alkylene group and the arylene group may be arbitrarily substituted with one or more amide groups or amino groups), an oxygen atom, a carbonyl group, a sulfur atom, -C(O)-NR a -、-NR b - or a divalent group formed by a combination thereof, R 5 each independently represents a nitrogen atom or a nitrogen atom and an alkylene group having 1 to 10 carbon atoms, an arylene group having 6 to 40 carbon atoms (the alkylene group and the arylene group may be arbitrarily substituted with one or more amide groups or amino groups), an oxygen atom, a carbonyl group, a sulfur atom, -C(O)-NR a - and -NR b - a trivalent group formed by a combination of at least one of the above groups, R 2 , R 2a , R 4 and R 6 Each independently represents a hydrogen atom, an alkyl group having 1 to 10 carbon atoms, or a hydrogen atom and an alkylene group having 1 to 10 carbon atoms, an oxygen atom, a carbonyl group, -C(O)-NR a - and -NR b -a monovalent group formed by a combination of at least one of the groups above, R a represents a hydrogen atom or an alkyl group having 1 to 10 carbon atoms, R brepresents a hydrogen atom, an alkyl group having 1 to 10 carbon atoms, or an alkylcarbonyl group having 1 to 10 carbon atoms, n represents the number of repeating units from 1 to 10, and Dotted lines represent chemical bonds to adjacent atoms.) The entire disclosure of International Publication No. 2018 / 190380 is incorporated herein by reference. (1-4-3) The crosslinkable polymer or the crosslinkable compound (C) may be a combination of a polyfunctional epoxy (meth)acrylate compound and a polyfunctional thiol compound described in JP-A-2016-003160. The above combination can be suitably crosslinked using a free radical polymerization initiator. The molecular weight of the multifunctional epoxy (meth)acrylate compound may be 300 to 20,000. The multifunctional epoxy (meth)acrylate compound may be a bisphenol type multifunctional epoxy (meth)acrylate compound. The polyfunctional thiol compound may be in a liquid state at 25°C. In addition to the above combination, a polymerization inhibitor may be contained. The entire disclosure of Japanese Patent Application Laid-Open No. 2016-003160 is incorporated herein by reference. (1-4-4) The crosslinkable polymer or the crosslinkable compound (C) may be a photopolymerizable substance described in International Publication No. 2009 / 104643. The photopolymerizable substance may be a compound having at least one reactive group capable of cation polymerization, or may be a compound having at least one reactive group capable of radical polymerization. The photopolymerizable compound may be a sugar compound. The sugar compound may be a monosaccharide or a disaccharide compound. The sugar compound may be represented by formula (10). (Among them, G 1 represents the sugar backbone, T represents a divalent linking group, R 1 represents vinyl or glycidyl, R 2 represents a hydrogen atom or a hydroxyl group. n and L each represent an integer of 0 or 1, p is an integer and is the total number of hydroxyl groups possessed by the sugar. m is an integer satisfying 1≤m≤(pm), preferably 2≤m≤(pm). The photopolymerizable compound may be an alicyclic epoxy compound or an alicyclic oxetane compound. The alicyclic epoxy compound may be a cycloalkylene oxide derivative. The alicyclic epoxy compound may be represented by formula (2) or formula (3). (Among them, G 2 represents an alkylene group, a carbonyloxy group, a heterocyclic ring, an aromatic ring, or a monovalent to pentavalent linking group having a combination thereof, G 3 is an alkyl group, an alkylcarbonyl group, a heterocyclic ring, an aromatic ring, or an organic group having a combination thereof, and n and m each represent an integer of 1 to 5, and m preferably represents an integer of 2 to 5. The entire disclosure of International Publication No. 2009 / 104643 is incorporated herein by reference. (1-5: Resin composition) The preparation method of the photocurable resin composition is not particularly limited. That is, the self-crosslinking polymer (A), the solvent (B), the optional crosslinking polymer or crosslinking compound (C), and other components are mixed in any proportion and in any order to prepare a uniform solution. The photocurable resin composition in a solution state prepared in this way is preferably used after filtering using a filter with a pore size of about 0.2 μm. When a cured film having a thickness of about 300 nm is produced by spin coating, the photocurable resin composition preferably has a viscosity of about 100 cps or less at 25° C. In the present invention, the viscosity is a value measured using an E-type viscometer. (1-6: Composition for forming protective film) The photocurable resin composition as one embodiment of the present invention has excellent etching resistance and can therefore be preferably used as a protective film forming composition for protecting the front end of a wafer for semiconductor manufacturing (a protective film forming composition for the end of a wafer for semiconductor manufacturing, hereinafter sometimes referred to as a "protective film forming composition"). As the characteristics of the protective film covering the end of the substrate (wafer) for semiconductor manufacturing, in addition to the function of preventing the above-mentioned metal contamination, it is also expected to satisfy the following functions: resistance to dry etching, resistance to phosphoric acid, resistance to tetramethylammonium hydroxide (TMAH), HF removability, scratch resistance, good embedding into high-height substrates, low amount of sublimates, affinity with hydrophobic substrates, no residual pits or foreign matter on the side of the wafer, good edge shape, and the function of suppressing internal bulges (the phenomenon in which the film-forming composition remains in the form of a nodule just below the ejection hole of the nozzle). In addition, the protective film forming composition as one embodiment of the present invention is photosensitive. For example, it can be a negative solvent development type. After applying the photosensitive protective film forming composition (negative) on the front end of the above-mentioned substrate and optionally on the chamfered portion and / or back end of the above-mentioned substrate, the portion where the film is to be cured is exposed and developed, thereby accurately covering the chamfered portion with the above-mentioned protective film. Because it is photosensitive, there are the following advantages: the film thickness control of the protective film on the end face of the wafer becomes easy, the internal protrusion can be removed, the edge shape can be improved, and the deviation of the center position during spin coating can be corrected. (1-7: Polysiloxane) (1-7-1) The photocurable resin composition as one embodiment of the present invention may optionally contain polysiloxane. The polysiloxane may be a modified polysiloxane in which a part of the silanol groups is modified, for example, a modified polysiloxane in which a part of the silanol groups is modified with alcohol or protected with acetal. In addition, as an example, the polysiloxane may be a hydrolysis condensate of a hydrolyzable silane, or a modified product obtained by alcohol-modifying or acetal-protecting at least a portion of the silanol groups of the hydrolysis condensate (hereinafter sometimes referred to as "modified product of the hydrolysis condensate"). The hydrolyzable silane involved in the hydrolysis condensate may include one or more hydrolyzable silanes. The polysiloxane may have any structure of a cage type, a ladder type, a straight chain type, or a branched chain type main chain. Commercially available polysiloxanes may also be used. It should be noted that the "hydrolysis condensate" of the hydrolyzable silane, i.e., the product of hydrolysis and condensation, includes not only polyorganosiloxane polymers which are condensates obtained by complete condensation, but also polyorganosiloxane polymers which are partially hydrolyzed condensates which are not completely condensed. Such partially hydrolyzed condensates are polymers obtained by hydrolysis and condensation of the hydrolyzable silane, similarly to the condensates obtained by complete condensation, but partially hydrolyzed and stopped without condensation, so that Si-OH groups remain. Examples of the polysiloxane include hydrolysis-condensation products of hydrolyzable silanes containing at least one type of hydrolyzable silane represented by the following formula (1) or modified products thereof. 《Formula (1)》 R 1 a Si(R 2 ) 4-a (1) In formula (1), R 1is a group bonded to a silicon atom, and independently represents an alkyl group which may have a substituent, an aryl group which may have a substituent, an aralkyl group which may have a substituent, a halogenated alkyl group which may have a substituent, a halogenated aryl group which may have a substituent, a halogenated aralkyl group which may have a substituent, an alkoxyalkyl group which may have a substituent, an alkoxyaryl group which may have a substituent, an alkoxyaralkyl group which may have a substituent, or an alkenyl group which may have a substituent, or represents an organic group having an epoxy group, an organic group having an acryloyl group, an organic group having a methacryloyl group, an organic group having a mercapto group, an organic group having an amino group, an organic group having an alkoxy group, an organic group having a sulfonyl group, or an organic group having a cyano group, or a combination of two or more thereof. In addition, R 2 is a group or atom bonded to a silicon atom, and each independently represents an alkoxy group, an aralkyloxy group, an acyloxy group or a halogen atom. a represents an integer of 0-3. (1-7-2: Specific examples of the hydrolyzable silane represented by the formula (1)) Specific examples of the hydrolyzable silane represented by the formula (1) include tetramethoxysilane, tetrachlorosilane, tetraacetoxysilane, tetraethoxysilane, tetra-n-propoxysilane, tetraisopropoxysilane, tetra-n-butoxysilane, methyltrimethoxysilane, methyltrichlorosilane, methyltriacetoxysilane, methyltriethoxysilane, methyltripropropoxysilane, methyltributoxysilane, methyltripentoxysilane, methyltriphenoxysilane, methyltripenyloxysilane, methyltriphenylethyloxysilane, glycidoxymethyltrimethoxysilane, glycidoxymethyltriethoxysilane, α-glycidoxyethyltrimethoxysilane, α-glycidoxyethyltriethoxysilane, β-glycidoxyethyltrimethoxysilane, β-glycidoxyethyltriethoxysilane, α-Glycidoxypropyl trimethoxysilane, α-Glycidoxypropyl triethoxysilane, β-Glycidoxypropyl trimethoxysilane, β-Glycidoxypropyl triethoxysilane, γ-Glycidoxypropyl trimethoxysilane, γ-Glycidoxypropyl triethoxysilane, γ-Glycidoxypropyl tripropoxysilane, γ-Glycidoxypropyl tributoxysilane, γ-Glycidoxypropyl triphenoxysilane, α-Glycidoxybutyl trimethoxysilane, α-Glycidoxybutyl triethoxysilane, β-Glycidoxybutyl triethoxysilane, γ-Glycidoxybutyl trimethoxysilane, γ-Glycidoxybutyl triethoxysilane, δ-Glycidoxybutyl trimethoxysilane, δ- Glycidoxybutyltriethoxysilane, (3,4-epoxycyclohexyl)methyltrimethoxysilane, (3,4-epoxycyclohexyl)methyltriethoxysilane, β-(3,4-epoxycyclohexyl)ethyltrimethoxysilane, β-(3,4-epoxycyclohexyl)ethyltriethoxysilane, β-(3,4-epoxycyclohexyl)ethyltripropoxysilane, β-(3,4-epoxycyclohexyl)ethyltributoxysilane, β-(3,4-epoxycyclohexyl)ethyltriphenoxysilane, γ-(3,4-epoxycyclohexyl)propyltrimethoxysilane, γ-(3,4-epoxycyclohexyl)propyltriethoxysilane, δ-(3,4-epoxycyclohexyl)butyltrimethoxysilane, δ-(3,4-epoxycyclohexyl)butyltriethoxysilane Alkane, glycidoxymethylmethyldimethoxysilane, glycidoxymethylmethyldiethoxysilane, α-glycidoxyethylmethyldimethoxysilane, α-glycidoxyethylmethyldiethoxysilane, β-glycidoxyethylmethyldimethoxysilane, β-glycidoxyethylethyldimethoxysilane, α-glycidoxypropylmethyldimethoxysilane, α-glycidoxypropylmethyldiethoxysilane, β-glycidoxypropylmethyldimethoxysilane, β-glycidoxypropylethyldimethoxysilane, γ-glycidoxypropylmethyldimethoxysilane, γ-glycidoxypropylmethyldiethoxysilane, γ-glycidoxypropylmethyldipropoxysilane, γ-glycidoxypropylmethyldibutoxysilane,γ-Glycidoxypropylmethyldiphenoxysilane, γ-Glycidoxypropylethyldimethoxysilane, γ-Glycidoxypropylethyldiethoxysilane, γ-Glycidoxypropylvinyldimethoxysilane, γ-Glycidoxypropylvinyldiethoxysilane, ethyltrimethoxysilane, ethyltriethoxysilane, vinyltrimethoxysilane, vinyltriethoxysilane, vinyltrichlorosilane, vinyltriacetoxysilane, methylvinyldimethoxysilane, methylvinyldiethoxysilane, methylvinyldichlorosilane, methylvinyldiacetoxysilane, dimethylvinylmethoxysilane, dimethylvinylethoxysilane, dimethylvinylchlorosilane, dimethylvinylacetoxysilane, divinyl Dimethoxysilane, divinyldiethoxysilane, divinyldichlorosilane, divinyldiacetoxysilane, γ-glycidoxypropylvinyldimethoxysilane, γ-glycidoxypropylvinyldiethoxysilane, allyltrimethoxysilane, allyltriethoxysilane, allyltrichlorosilane, allyltriacetoxysilane, allylmethyldimethoxysilane, allylmethyldiethoxysilane, allylmethyldichlorosilane, allylmethyldiacetoxysilane, allyldimethylmethoxysilane, allyldimethylethoxysilane, allyldimethylchlorosilane, allyldimethylacetoxysilane, diallyldimethoxysilane, diallyldiethoxysilane, diallyldichlorosilane, diallyldiacetoxysilane Oxysilane, 3-allylaminopropyltrimethoxysilane, 3-allylaminopropyltriethoxysilane, p-phenyltrimethoxysilane, phenyltrimethoxysilane, phenyltriethoxysilane, phenyltrichlorosilane, phenyltriacetoxysilane, phenylmethyldimethoxysilane, phenylmethyldiethoxysilane, phenylmethyldichlorosilane, phenylmethyldiacetoxysilane, phenyldimethylmethoxysilane, phenyldimethylethoxysilane, phenyldimethylchlorosilane, phenyldimethylacetoxysilane, diphenylmethylmethoxysilane, diphenylmethylethoxysilane, diphenylmethylchlorosilane, diphenylmethylacetoxysilane, diphenyldimethoxysilane, diphenyldiethoxysilane, diphenyldichlorosilane, diphenyldiacetoxysilane Oxysilane, triphenylmethoxysilane, triphenylethoxysilane, triphenylacetoxysilane, triphenylchlorosilane, 3-phenylaminopropyltrimethoxysilane, 3-phenylaminopropyltriethoxysilane, dimethoxymethyl-3-(3-phenoxypropylthiopropyl)silane, triethoxy((2-methoxy-4-(methoxymethyl)phenoxy)methyl)silane, benzyltrimethoxysilane, benzyltriethoxysilane, benzylmethyldimethoxysilane, benzylmethyldiethoxysilane, benzyldimethylmethoxysilane, benzyldimethylethoxysilane, benzyldimethylchlorosilane, phenethyltrimethoxysilane, phenethyltriethoxysilane, phenethyltrichlorosilane, phenethyltriacetoxysilane, phenethylmethyldimethoxysilane,Phenethylmethyldiethoxysilane, phenethylmethyldichlorosilane, phenethylmethyldiacetoxysilane, methoxyphenyltrimethoxysilane, methoxyphenyltriethoxysilane, methoxyphenyltriacetoxysilane, methoxyphenyltrichlorosilane, methoxybenzyltrimethoxysilane, methoxybenzyltriethoxysilane, methoxybenzyltriacetoxysilane, methoxybenzyltrichlorosilane, methoxyphenethyltrimethoxysilane, methoxyphenethyltriethoxysilane, methoxyphenethyltriacetoxysilane, methoxyphenethyltrichlorosilane, ethoxyphenyltrimethoxysilane, ethoxyphenyltriethoxysilane, ethoxyphenyltriacetoxysilane, ethoxyphenyltrichlorosilane, ethoxybenzyltrimethoxysilane, ethoxybenzyl triethoxysilane, ethoxybenzyl triacetoxysilane, ethoxybenzyl trichlorosilane, isopropoxyphenyl trimethoxysilane, isopropoxyphenyl triethoxysilane, isopropoxyphenyl triacetoxysilane, isopropoxyphenyl trichlorosilane, isopropoxybenzyl trimethoxysilane, isopropoxybenzyl triethoxysilane, isopropoxybenzyl triacetoxysilane, isopropoxybenzyl trichlorosilane, tert-butoxyphenyl trimethoxysilane, tert-butoxyphenyl triethoxysilane, tert-butoxyphenyl triacetoxysilane, tert-butoxyphenyl trichlorosilane, tert-butoxybenzyl trimethoxysilane, tert-butoxybenzyl triethoxysilane, tert-butoxybenzyl triacetoxysilane, tert-butoxybenzyl trichlorosilane, methoxynaphthyl trimethoxysilane Silane, methoxynaphthyl triethoxysilane, methoxynaphthyl triacetoxysilane, methoxynaphthyl trichlorosilane, ethoxynaphthyl trimethoxysilane, ethoxynaphthyl triethoxysilane, ethoxynaphthyl triacetoxysilane, ethoxynaphthyl trichlorosilane, γ-chloropropyl trimethoxysilane, γ-chloropropyl triethoxysilane, γ-chloropropyl triacetoxysilane, 3,3,3-trifluoropropyl trimethoxysilane, γ-methacryloxypropyl trimethoxysilane, γ-mercaptopropyl trimethoxysilane, γ-mercaptopropyl triethoxysilane, β-cyanoethyl triethoxysilane, thiocyanate propyl triethoxysilane, chloromethyl trimethoxysilane, chloromethyl triethoxysilane, triethoxysilylpropyl diallyl Isocyanurate, bicyclo[2,2,1]heptenyltriethoxysilane, benzenesulfonylpropyltriethoxysilane, benzenesulfonamidopropyltriethoxysilane, dimethylaminopropyltrimethoxysilane, dimethyldimethoxysilane, phenylmethyldimethoxysilane, dimethyldiethoxysilane, phenylmethyldiethoxysilane, γ-chloropropylmethyldimethoxysilane, γ-chloropropylmethyldiethoxysilane, dimethyldiacetoxysilane, γ-methacryloxypropylmethyldimethoxysilane, γ-methacryloxypropylmethyldiethoxysilane, γ-mercaptopropylmethyldimethoxysilane, γ-mercaptomethyldiethoxysilane, methylvinyldimethoxysilane, methylvinyldiethoxysilane, but not limited thereto. (1-8: other optional ingredients) In addition, the photocurable resin composition as one embodiment of the present invention may contain a radical polymerization initiator (photopolymerization initiator, etc.), an acid (catalyst), a thermal acid generator, a photoacid generator, a base (catalyst), a thermal base generator, a photobase generator, an antioxidant, a polymerization inhibitor, a crosslinking agent (multifunctional acrylic crosslinking agent, etc.), an adhesion improver, an adhesion aid (silane coupling agent), a surfactant, a defoaming agent, a rheology modifier, a pigment, a dye, a storage stabilizer, a dissolution accelerator such as a polyphenol or a polycarboxylic acid, a sensitizer, and the like, as needed. However, since the self-crosslinking polymer (A) contained in the photocurable resin composition which is one embodiment of the present invention is self-crosslinking, it is not necessary to add a photopolymerization initiator at least for curing the self-crosslinking polymer (A). (1-8-1: Radical polymerization initiator) The free radical polymerization initiator may be any substance capable of releasing a substance that initiates free radical polymerization by light irradiation and / or heating. For example, the photo-free radical polymerization initiator may include benzophenone derivatives, imidazole derivatives, bisimidazole derivatives, N-arylglycine derivatives, organic azide compounds, titanocene compounds, aluminate complexes, organic peroxides, N-alkoxypyridines, More specifically, benzophenone, 1,3-di(tert-butyldioxycarbonyl)benzophenone, 3,3',4,4'-tetra(tert-butyldioxycarbonyl)benzophenone, 3-phenyl-5-isothiazolinone, oxadiazole, 2-mercaptobenzimidazole, bis(2,4,5-triphenyl)imidazole, 2,2-dimethoxy-1,2-diphenylethane-1-one, 1-hydroxycyclohexyl phenyl ketone, 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-butane-1-one, bis(η 5 -2,4-cyclopentadien-1-yl)-bis(2,6-difluoro-3-(1H-pyrrol-1-yl)phenyl)titanium), etc., but not limited thereto. As the above-mentioned photoradical polymerization initiator, commercial products can also be used, for example, IRGACURE (registered trademark) 651, 184, 369, 784, etc. manufactured by BASF. In addition, commercial products other than the above can also be used, specifically, IRGACURE (registered trademark) 500, 907, 379, 819, 127, 500, 754, 250, 1800, 1870, OXE01, DAROCUR (registered trademark) TPO, 1173 manufactured by BASF; Speedcure (registered trademark) MBB, PBZ, ITX, CTX, EDB manufactured by Lambson; Esacure (registered trademark) ONE, KIP150, KTO46 manufactured by Lamberti; KAYACURE (registered trademark) DETX-S, CTX, BMS, DMBI manufactured by Nippon Kayaku Co., Ltd., etc. In addition, examples of the thermal radical polymerization initiator include peroxides such as acetyl peroxide, benzoyl peroxide, methyl ethyl ketone peroxide, cyclohexanone peroxide, hydrogen peroxide, tert-butyl hydroperoxide, cumene hydroperoxide, di-tert-butyl peroxide, dicumyl peroxide, dilauroyl peroxide, tert-butyl peroxyacetate, peroxypivalyl tert-butyrate, and tert-butyl peroxy-2-ethylhexanoate; 2,2'-azobisisobutyronitrile, 2,2'-azobis(2,4-dimethylvaleronitrile), (1-phenylethyl)azodiphenylmethane, 2, Azo compounds such as 2'-azobis(4-methoxy-2,4-dimethylvaleronitrile), 2,2'-azobisdimethylisobutyrate, 2,2'-azobis(2-methylbutyronitrile), 1,1'-azobis(1-cyclohexanecarbonitrile), 2-(carbamoylazo)isobutyronitrile, 2,2'-azobis(2,4,4-trimethylpentane), 2-phenylazo-2,4-dimethyl-4-methoxyvaleronitrile, and 2,2'-azobis(2-methylpropane); persulfates such as ammonium persulfate, sodium persulfate, and potassium persulfate, but not limited thereto. Examples of commercially available thermal radical polymerization initiators include PALOIL (registered trademark) IB, NPP, IPP, SBP, TCP, OPP, SA, 355, L, PARBUTL (registered trademark) ND, NHP, MA, PV, 355, A, C, D, E, L, I, O, P, Z, PAHECIL (registered trademark) ND, PV, D, I, O, Z, PAROKTA (registered trademark) ND, Nanopa (registered trademark) PMB, BMT, BW, Parterra (registered trademark) A, Parthexer (registered trademark) MC, TMH, HC, 250, 25B, C, 25Z, 22, V, Parker (registered trademark) O, Parkmil (registered trademark) ND, D, Parker (registered trademark) H, Nofmar (registered trademark) BC; Wako Pure Chemical Industries, Ltd. V-70, V-65, V-59, V-40, V-30, VA-044, VA-046B, VA-061, V-50, VA-057, VA-086, VF-096, VAm-110, V-601, V-501; BASF IRGACURE (registered trademark) 184, 369, 651, 500, 819, 907, 784, 2959, CGI1700, CGI1750, CGI1850, CG24-61 , DAROCUR (registered trademark) 1116, 1173, LUCIRIN (registered trademark) TPO; UVECRYL (registered trademark) P36 manufactured by ScienceSpecialties; Esacure (registered trademark) KIP150, KIP65LT, KIP100F, KT37, KT55, KTO46, KIP75 / B manufactured by Lamberti, but not limited to these. The free radical polymerization initiator may be used alone or in combination of two or more. The content of the free radical polymerization initiator is preferably 1 part by mass or more, 2 parts by mass or more, 3 parts by mass or more, 50 parts by mass or less, 20 parts by mass or less, or 10 parts by mass or less relative to 100 parts by mass of the polymer or compound having a crosslinking group. (1-8-2: Inhibitor) As the polymerization inhibitor, a hindered phenol compound can be used, and specific examples thereof include 2,6-diisobutylphenol, 3,5-di-tert-butylphenol, 3,5-di-tert-butylcresol, hydroquinone, hydroquinone monomethyl ether, N-nitroso-N-phenylhydroxylamine aluminum, pyrogallol, tert-butylcatechol, 4-methoxy-1-naphthol, 2,6-di-tert-butyl-4-methylphenol, 2,5-di-tert-butylhydroquinone, octadecyl 3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate, isooctyl 3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate, 4,4'-methylenebis(2,6-di-tert-butylphenol), 4,4'-thio-bis(3-methyl-6-tert-butylphenol), 4,4'-butylene-bis(3-methyl-6-tert-butylphenol), -tert-butylphenol), triethylene glycol-bis[3-(3-tert-butyl-5-methyl-4-hydroxyphenyl) propionate], 1,6-hexanediol-bis[3-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate], 2,2-thio-diethylenebis[3-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate], N,N'-hexamethylenebis(3,5-di-tert-butyl-4-hydroxy-hydrocinnamic acid), 2,2'-methylene-bis(4-methyl-6-tert-butylphenol), 2,2'-methylene-bis(4-ethyl-6-tert-butylphenol), pentaerythritol-tetrakis[3-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate], tris-(3,5-di-tert-butyl-4-hydroxybenzyl)-isocyanurate esters, 1,3,5-trimethyl-2,4,6-tris(3,5-di-tert-butyl-4-hydroxybenzyl)benzene, 1,3,5-tris(3-hydroxy-2,6-dimethyl-4-isopropylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris(4-tert-butyl-3-hydroxy-2,6-dimethylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris(4-sec-butyl-3-hydroxy-2,6-dimethylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris[4-(1-ethylpropyl)-3-hydroxy-2,6-dimethylbenzyl ]-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris[4-triethylmethyl-3-hydroxy-2,6-dimethylbenzyl]-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris(3-hydroxy-2,6-dimethyl-4-phenylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris(4-tert-butyl-3-hydroxy-2,5,6-trimethylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris(4-tert-butyl-5-ethyl-3-hydroxy-2,6-dimethylbenzyl)-1,3,5-Triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris(4-tert-butyl-6-ethyl-3-hydroxy-2-methylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris(4-tert-butyl-6-ethyl-3-hydroxy-2,5-dimethylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris(4-tert-butyl-5,6-diethyl-3-hydroxy-2-methylbenzyl)-1,3,5-triazine-2 ,4,6-(1H,3H,5H)-trione, 1,3,5-tris(4-tert-butyl-3-hydroxy-2-methylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris(4-tert-butyl-3-hydroxy-2,5-dimethylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, 1,3,5-tris(4-tert-butyl-5-ethyl-3-hydroxy-2-methylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione, etc. , Among the hindered phenol compounds, 1,3,5-tris(4-tert-butyl-3-hydroxy-2,6-dimethylbenzyl)-1,3,5-triazine-2,4,6-(1H,3H,5H)-trione is preferred. A commercially available product may be used as the polymerization inhibitor, and a specific example thereof is Irganox-3114 (manufactured by BASF Japan Co., Ltd.). The polymerization inhibitor may be used alone or in combination of two or more. The content of the polymerization inhibitor is preferably 0.01 to 1 part by mass, more preferably 0.01 to 0.5 parts by mass, based on 100 parts by mass of the total amount of the self-crosslinking polymer (A) and the crosslinking polymer or crosslinking compound (C) optionally contained. (1-8-3: Surfactants) Examples of the surfactant include polyoxyethylene alkyl ether compounds such as polyoxyethylene lauryl ether, polyoxyethylene stearyl ether, and polyoxyethylene oleyl ether, polyoxyethylene alkyl allyl ether compounds such as polyoxyethylene octylphenol ether and polyoxyethylene nonylphenol ether, polyoxyethylene / polyoxypropylene block copolymer compounds, sorbitan fatty acid ester compounds such as sorbitan monolaurate, sorbitan monopalmitate, sorbitan monostearate, sorbitan trioleate, and sorbitan tristearate, and polyoxyethylene sorbitan fatty acid ester compounds such as polyoxyethylene sorbitan monolaurate, polyoxyethylene sorbitan monopalmitate, polyoxyethylene sorbitan monostearate, and polyoxyethylene sorbitan tristearate. Examples of the products include the trade names of Effort EF301, EF303, and EF352 (manufactured by Tow Fiber Co., Ltd.), and the trade names of Effort.クF171, F173, R-08, R-30 (manufactured by Dainippon Technology Co., Ltd.), FC430, FC431 (Sumitomo スリーエCo., Ltd.), trade names: Aeser AG710, S-382, SC101, SC102, SC103, SC104 , SC105, SC106 (manufactured by Asahi Glass Co., Ltd.) and other fluorine-based surfactants, and organosiloxane polymer KP341 (manufactured by Shin-Etsu Chemical Industry Co., Ltd.), etc. The surfactant may be used alone or in combination of two or more. The content of the surfactant is preferably 0.1 parts by mass or more, 0.5 parts by mass or more, 5 parts by mass or less, or 2 parts by mass or less, relative to 100 parts by mass of the total amount of the self-crosslinking polymer (A) and the crosslinking polymer or crosslinking compound optionally contained. (1-8-4: Acid-base catalyst and other ingredients) As the acid catalyst or the base catalyst, an acidic compound, a basic compound, or various compounds that generate an acid or a base by heat or light can be used. As the acidic compound, a sulfonic acid compound or a carboxylic acid compound can be used. Examples of the sulfonic acid compound or carboxylic acid compound include p-toluenesulfonic acid, trifluoromethanesulfonic acid, pyridine Trifluoromethanesulfonate (=pyridine Trifluoromethanesulfonic acid), pyridine - p-Toluenesulfonate, pyridine -4-Hydroxybenzenesulfonate, salicylic acid, camphorsulfonic acid, 5-sulfosalicylic acid, 4-chlorobenzenesulfonic acid, 4-phenolsulfonic acid, pyridine -4-Phenolsulfonate, benzene disulfonic acid, 1-naphthalenesulfonic acid, 4-nitrobenzenesulfonic acid, citric acid, benzoic acid, hydroxybenzoic acid. As the basic compound, an amine compound or an ammonium hydroxide compound can be used, and as the compound that generates a base by heat, urea can be used. Examples of the amine compound include tertiary amines such as triethanolamine, tributanolamine, trimethylamine, triethylamine, tri-n-propylamine, triisopropylamine, tri-n-butylamine, tri-tert-butylamine, tri-n-octylamine, triisopropanolamine, phenyldiethanolamine, stearyldiethanolamine, and diazabicyclooctane, and aromatic amines such as pyridine and 4-dimethylaminopyridine. In addition, examples of the amine compound include primary amines such as benzylamine and n-butylamine, and secondary amines such as diethylamine and di-n-butylamine. Examples of the ammonium hydroxide compound include tetramethylammonium hydroxide, tetraethylammonium hydroxide, tetrapropylammonium hydroxide, tetrabutylammonium hydroxide, benzyltrimethylammonium hydroxide, benzyltriethylammonium hydroxide, cetyltrimethylammonium hydroxide, phenyltrimethylammonium hydroxide, and phenyltriethylammonium hydroxide. As the acid generator, any of a thermal acid generator and a photoacid generator can be used. Examples of the thermal acid generator include p-toluenesulfonic acid, trifluoromethanesulfonic acid, pyridine - p-Toluenesulfonate (pyridine -p-Toluenesulfonic acid), pyridine -p-Hydroxybenzenesulfonic acid (pyridinium phenolsulfonate Salt), pyridine - Sulfonic acid compounds and carboxylic acid compounds such as trifluoromethanesulfonic acid, salicylic acid, camphorsulfonic acid, 5-sulfosalicylic acid, 4-chlorobenzenesulfonic acid, 4-hydroxybenzenesulfonic acid, benzenedisulfonic acid, 1-naphthalenesulfonic acid, citric acid, benzoic acid, and hydroxybenzoic acid. Examples of commercially available products include K-PURE [registered trademark] CXC-1612, K-PURE CXC-1614, K-PURE TAG-2172, K-PURE TAG-2179, K-PURE TAG-2678, and K-PURE TAG2689 (all manufactured by King Industries), and SI-45, SI-60, SI-80, SI-100, SI-110, and SI-150 (all manufactured by Sanshin Chemical Industry Co., Ltd.). As photoacid generators, including sulfonium salts, iodine Salts, sulfonyldiazomethane, N-sulfonyloxyimide, benzoin sulfonate type photoacid generator, pyrogallol trisulfonate type photoacid generator, sulfone type photoacid generator, glyoxime derivative type photoacid generator, oxime-O-sulfonate type acid generator, bis-oxime sulfonate type acid generator, etc. For example, bis(4-tert-butylphenyl)iodide trifluoromethanesulfonate, triphenylsulfonium trifluoromethanesulfonate, phenyl-bis(trichloromethyl)-s-triazine, benzoin tosylate and N-hydroxysuccinimide trifluoromethanesulfonate, etc. Examples of the thermal base generator include carbamates such as 1-methyl-1-(4-biphenylyl)ethyl carbamate and 2-cyano-1,1-dimethylethyl carbamate; ureas such as urea and N,N-dimethyl-N'-methylurea; guanidines such as guanidine trichloroacetate, guanidine phenylsulfonyl acetate and guanidine phenylpropiolate; dihydropyridines such as 1,4-dihydronicotinamide; dimethylpiperidines such as N-(isopropoxycarbonyl)-2,6-dimethylpiperidine, N-(tert-butoxycarbonyl)-2,6-dimethylpiperidine and N-(benzyloxycarbonyl)-2,6-dimethylpiperidine; quaternary ammonium salts such as tetramethylammonium phenylsulfonyl acetate and tetramethylammonium phenylpropiolate; dicyandiamide and the like. In addition, U-CAT (registered trademark) SA810, U-CAT SA831, U-CAT SA841, and U-CAT SA851 (all manufactured by Sanapro Co., Ltd.), which are salts of 1,8-diazabicyclo[5.4.0]undec-7-ene (DBU), can be cited. Examples of the photobase generator include alkylamine photobase generators such as 9-anthrylmethyl-N,N-diethyl carbamate; 9-anthryl-N,N-dicyclohexyl carbamate, 1-(9,10-anthraquinone-2-yl)ethyl-N,N-dicyclohexyl carbamate, 2-(3-benzoylphenyl)propionic acid dicyclohexyl ammonium salt, 9-anthryl-N-cyclohexyl carbamate, 1-(9,10-anthraquinone-2-yl)ethyl-N-cyclohexyl carbamate, 2-(3-benzoylphenyl)propionic acid dicyclohexyl ammonium salt, cycloalkylamine photobase generators such as (E)-N-cyclohexyl-3-(2-hydroxyphenyl)acrylamide; piperidine photobase generators such as 9-anthrylmethylpiperidine-1-carboxylate, (E)-1-piperidino-3-(2-hydroxyphenyl)-2-propen-1-one, (2-nitrophenyl)methyl-4-hydroxypiperidine-1-carboxylate, (2-nitrophenyl)methyl-4-(methacryloyloxy)piperidine-1-carboxylate; guanidine =2-(3-benzoylphenyl) propionate, 1,2-diisopropyl-3-(bis(dimethylamino)methylene)guanidine =2-(3-benzoylphenyl) propionate, 1,2-dicyclohexyl-4,4,5,5-tetramethylbiguanide-n-butyltriphenylborate, 1,5,7-triazabicyclo[4.4.0]dec-5-ene -2-(9-oxoxanthene-2-yl) propionate and other guanidine-based photobase generators; 1-(9,10-anthraquinone-2-yl)ethyl-imidazole-1-carboxylate and other imidazole-based photobase generators, etc. The above components may be used alone or in combination of two or more. In this case, they are used in an amount of usually 10% by mass or less, preferably 3% by mass or less, based on the solid content of the photocurable resin composition of the present application. <2. Protective film [6] / wafer for semiconductor manufacturing

[10] > (2-1: Protective film[6]) The protective film [6] as one embodiment of the present invention is a cured product of a coating film made from the composition [5] for forming a wafer edge protective film for semiconductor manufacturing. This protective film has excellent etching resistance and can therefore be used to prevent metal contamination at the edge of a wafer in semiconductor manufacturing. The thickness of the protective film can be set to, for example, 1 to 500 nm, and light with a wavelength of, for example, 170 to 800 nm can be used in photocuring. (2-2: Wafers for semiconductor manufacturing

[10] ) A semiconductor manufacturing wafer as one embodiment of the present invention is a semiconductor manufacturing wafer having a protected wafer end, wherein the semiconductor manufacturing wafer is formed by coating a protective film forming composition [5] as one embodiment of the present invention (see the above <1. Photocurable resin composition [1] / composition for forming a protective film at the end of a semiconductor manufacturing wafer [5]>) on the wafer end. <3. Method for manufacturing a semiconductor device

[11] > A method for manufacturing a semiconductor device as one embodiment of the present invention is a method for manufacturing a semiconductor device including the following steps: Step (A), forming a resist film on a semiconductor substrate; Step (B) of forming a resist pattern by irradiating the resist film with light or electron beams and then developing the resist film; and Step (C) is a step of processing the semiconductor substrate by etching; or a step of processing the semiconductor substrate by etching through the patterned resist. The method for manufacturing the semiconductor device further includes the following step (X): A protective film made of the protective film-forming composition of [5] as one embodiment of the present invention is formed on the front edge of a wafer for semiconductor manufacturing and optionally on the chamfered portion and / or the back edge of the wafer. The following will explain them one by one. (3-1: Step (A), forming a resist film on a semiconductor substrate) A resist film is formed on a semiconductor substrate. A semiconductor substrate is a wafer used for manufacturing semiconductor elements, etc. In addition to the commonly used silicon wafer and germanium wafer, a compound semiconductor wafer formed by bonding two or more elements such as gallium arsenide, indium phosphide, gallium nitride, indium nitride, and aluminum nitride can be used. They are usually disc-shaped, and the size is, for example, 4, 6, 8, 12 inches. Commercially available products can be used. When a semiconductor substrate having an inorganic film formed on the surface is used, the inorganic film can be formed by, for example, ALD (atomic layer deposition) method, CVD (chemical vapor deposition) method, reactive sputtering method, ion plating method, vacuum evaporation method, spin coating method (spin-on glass: SOG). Examples of the inorganic film include polysilicon film, silicon oxide film, silicon nitride film, BPSG (Boro-Phospho Silicate Glass) film, titanium nitride film, titanium oxide nitride film, tungsten film, gallium nitride film, and gallium arsenide film. On such a semiconductor substrate, a resist underlayer film, a resist film, etc. of a predetermined thickness are formed by an appropriate coating method such as a sprayer, a spinner, a coater, etc. Usually, in the case of a spin coating method, a resist underlayer film forming composition, a resist film forming composition, etc. are each supplied from above the center of a rotating disk-shaped substrate through a nozzle, etc. Usually, these films are baked using a heating means such as a hot plate. As a photoresist for forming a resist film, it is not particularly limited as long as it is a photoresist that is sensitive to light for exposure. Any photoresist of a negative photoresist and a positive photoresist can be used. Including a positive photoresist composed of a novolac resin and 1,2-diazonaphthoquinone sulfonate, a chemically amplified photoresist composed of a binder and a photoacid generator having a group that decomposes by acid and increases the alkali dissolution rate, a chemically amplified photoresist composed of a low molecular compound that decomposes by acid and increases the alkali dissolution rate of the photoresist, an alkali-soluble binder and a photoacid generator, and a chemically amplified photoresist composed of a binder having a group that decomposes by acid and increases the alkali dissolution rate, a low molecular compound that decomposes by acid and increases the alkali dissolution rate of the photoresist, and a photoacid generator, a resist containing a metal element, etc. For example, JSR (trade name V146G), Shipley Co., Ltd. trade name APEX-E, Sumitomo Chemical Co., Ltd. trade name PAR710 and Shin-Etsu Chemical Co., Ltd. trade name AR2772, SEPR430, etc. can be cited. In addition, for example, Proc. SPIE, Vol. 3999, 330-334 (2000), Proc. SPIE, Vol. 3999, 357-364 (2000), Proc. SPIE, Vol. 3999, 365-374 (2000) can be cited. Negative photoresist is preferred. In the resist film forming composition for forming the resist film, one or more metals may be included. As the form of the metal, in addition to the metal element, metal salts, metal complexes, and other metal-containing compounds may also be mentioned. As the type of metal, there is no particular limitation, and examples thereof include tin, indium, antimony, bismuth, gallium, germanium, aluminum, zirconium, hafnium, cerium, lanthanum, cesium, etc. The baking conditions of the resist film can be appropriately selected from a baking temperature of 70°C to 400°C and a baking time of 0.3 to 60 minutes, preferably a baking temperature of 80°C to 350°C and a baking time of 0.5 to 30 minutes, and more preferably a baking temperature of 90°C to 300°C and a baking time of 0.8 to 10 minutes. The lower limit of the average thickness of the resist film is preferably 1 nm, more preferably 3 nm, 5 nm, 10 nm. The upper limit of the average thickness of the resist film is 5,000 nm, 3,000 nm, 2,000 nm, preferably 1,000 nm, more preferably 200 nm, and more preferably 50 nm. (3-2: Step (X) of forming a protective film and optional steps (Y) and (Z)) (3-2-1: Process X) The following step (X) is performed at an arbitrary time point: a protective film made of the protective film forming composition of [5] as one embodiment of the present invention is formed on the front end of a semiconductor manufacturing wafer and optionally on the chamfered portion and / or back end of the wafer. In step (X), as a preferred step, a predetermined area is exposed and developed after applying the protective film forming composition. Step (X) may be performed before step (A), between step (A) and step (B), or after step (B) or step (C). It should be noted that, in the present application, the surface of the substrate on which the device portion such as the resist film is provided is referred to as the front side, and the surface on the opposite side is referred to as the back side. In addition, the so-called front end portion refers to a region generally 1 to 10 mm wide from the end of the device portion provided on the substrate to the chamfered portion, the so-called chamfered portion refers to a curved region connecting the front end portion and the back end portion, and the so-called back end portion refers to a region on the back side of the substrate corresponding to the front end portion. First, a protective film forming composition [5] as one embodiment of the present invention is applied to a semiconductor substrate on which a resist film or the like is formed (see the above <1. Photocurable resin composition [1] / composition for forming a protective film on the edge of a wafer for semiconductor manufacturing [5]>). The method for applying the protective film forming composition is not particularly limited, and known means such as a spin coating method (spin coating method) and a spray method can be used. For example, when a spin coating method is used, the protective film forming composition is supplied from above or near the front end of the rotating disk-shaped substrate through a nozzle while the semiconductor substrate on which a resist film or the like is formed is rotated at a predetermined rotational speed. Preferably, the chamfered portion and / or the back end of the substrate are also supplied from their respective vicinities through a nozzle. The conditions for spin coating can be appropriately selected without any limitation, but typical conditions are exemplified as follows. ·Viscosity of protective film forming composition: about 100 cps or less Wafer rotation speed: ··When supplying the protective film forming composition: 50 to 500 rpm ··Drying and spinning: 700~2,000rpm Protective film thickness: 300nm Next, the protective film-forming composition is exposed. The exposure can be performed as follows: for the protective film-forming composition, ultraviolet rays, visible rays, radiation and other active rays (including i-rays, KrF excimer lasers, ArF excimer lasers, EUV (extreme ultraviolet rays), EB (electron beams)) are irradiated through a mask or without a mask. It should be noted that a mild bake (SB) can be performed before exposure, and post-exposure heating (PEB) can be performed before development after exposure. Preferably, the post-exposure heating temperature is 50°C to 150°C, and the post-exposure heating time is 1 minute to 10 minutes. Next, the exposed protective film-forming composition is developed. The development can be performed by removing the exposed portion of the exposed protective film-forming composition with a developer, and the development temperature can be appropriately selected from 5° C. to 50° C. and the development time can be appropriately selected from 10 seconds to 300 seconds. Examples of the organic solvent contained in the developer include alcohol solvents, ether solvents, ketone solvents, amide solvents, ester solvents, hydrocarbon solvents, etc. The organic solvent of the developer is preferably an ester solvent, a ketone solvent, or a combination thereof. The developer may contain one organic solvent alone or two or more organic solvents. Examples of the alcohol solvent include aliphatic monoalcohol solvents having 1 to 18 carbon atoms such as 4-methyl-2-pentanol and n-hexanol; alicyclic monoalcohol solvents having 3 to 18 carbon atoms such as cyclohexanol; and polyol partial ether solvents having 3 to 19 carbon atoms such as propylene glycol monomethyl ether. Examples of the ether solvent include dialkyl ether solvents such as diethyl ether, dipropyl ether, dibutyl ether, diamyl ether, diisoamyl ether, dihexyl ether, and diheptyl ether; cyclic ether solvents such as tetrahydrofuran and tetrahydropyran; and ether solvents containing an aromatic ring such as diphenyl ether and anisole. Examples of ketone solvents include chain ketone solvents such as acetone, methyl ethyl ketone, methyl n-propyl ketone, methyl n-butyl ketone, diethyl ketone, methyl isobutyl ketone, 2-heptanone, ethyl n-butyl ketone, methyl n-hexyl ketone, diisobutyl ketone, and trimethyl nonanone; cyclic ketone solvents such as cyclopentanone, cyclohexanone, cycloheptanone, cyclooctanone, and methylcyclohexanone; 2,4-pentanedione, acetone acetone, and acetophenone. Examples of the amide solvent include cyclic amide solvents such as N,N'-dimethylimidazolidinone and N-methylpyrrolidone; and chain amide solvents such as N-methylformamide, N,N-dimethylformamide, N,N-diethylformamide, acetamide, N-methylacetamide, N,N-dimethylacetamide, and N-methylpropionamide. Examples of the ester solvent include monocarboxylic acid ester solvents such as n-butyl acetate and ethyl lactate; polyol carboxylic acid ester solvents such as propylene glycol acetate; polyol partial ether carboxylic acid ester solvents such as propylene glycol monomethyl ether acetate; polycarboxylic acid diester solvents such as diethyl oxalate; carbonate solvents such as dimethyl carbonate and diethyl carbonate, etc. Examples of the hydrocarbon solvent include aliphatic hydrocarbon solvents having 5 to 12 carbon atoms such as n-pentane and n-hexane; and aromatic hydrocarbon solvents having 6 to 16 carbon atoms such as toluene and xylene. Among them, ester solvents, ketone solvents, ether solvents and combinations thereof are preferred, and ester solvents, ketone solvents and combinations thereof are more preferred. As the ester solvent, propylene glycol monomethyl ether acetate is preferred. As the ketone solvent, cyclohexanone is preferred. As the ether solvent, propylene glycol monomethyl ether is preferred. The lower limit of the content of the organic solvent in the developer is preferably 80% by mass, more preferably 90% by mass, further preferably 99% by mass, and particularly preferably 100% by mass. By making the content of the organic solvent in the developer be the above range, the dissolution contrast between the exposed portion and the unexposed portion can be improved, and as a result, an excellent resist pattern can be formed using lithography performance. As components other than the organic solvent, for example, water, silicone oil, etc. can be cited. The developer may contain a nitrogen-containing compound. When the developer contains a nitrogen-containing compound, film loss in the formed resist pattern can be further reduced. The developer may be an aqueous solution instead of the organic solvent developer. Specifically, it may be an aqueous alkali solution of sodium hydroxide, potassium hydroxide, sodium silicate, ammonia, monoethylamine, diethylamine, triethylamine, triethanolamine, tetramethylammonium hydroxide, etc. The alkali concentration of these aqueous solutions is not particularly limited, and may be set to 0.1 to 10% by weight, for example. In addition, alcohols and surfactants may be added to the developer. Each of them may be preferably blended in the range of 0.01 to 10 parts by weight, more preferably 0.1 to 5 parts by weight, relative to 100 parts by weight of the developer. Examples of the surfactant include ionic and nonionic fluorine-based surfactants and silicon-based surfactants. As developing methods, for example, the following methods can be cited: a method of immersing a substrate in a tank filled with a developer for a certain period of time (immersion method); a method of utilizing surface tension to pile up the developer on the surface of the substrate and let it stand for a certain period of time to perform development (spin immersion method); a method of spraying the developer onto the surface of the substrate (spray method); a method of continuously applying the developer on a substrate rotating at a certain speed while scanning the developer through a nozzle at a certain speed (dynamic distribution method), etc. Next, the developed protective film-forming composition is baked. By baking the pattern obtained after development, a desired pattern can be formed. The heating temperature in the heat treatment is usually above 150° C. and below 350° C., preferably in the range of 200 to 300° C. The heating treatment time is the time until the protective film-forming composition is cured, and in consideration of productivity, it is preferably less than about 30 minutes. The lower limit of the average thickness of the protective film is preferably 1 nm, and more preferably 3 nm. The upper limit of the average thickness of the protective film is preferably 500 nm, and more preferably 300 nm. (3-2-2: Process Y, Z) After process (X), in process (Y), the resist film of part on protective film can be removed by removing liquid. At this time, similarly to the above-mentioned process (X), it is preferred to apply removing liquid at the front end of semiconductor manufacturing wafer and optionally at the chamfered part and / or the back end of semiconductor manufacturing wafer. As resist removing liquid, for example, propylene glycol monomethyl ether, propylene glycol monomethyl ether acetate, cyclohexanone, water, butyl acetate, tetramethyl ammonium aqueous solution or a mixed solution made of their combination can be cited. Among them, from the viewpoint of the removability of resist film, propylene glycol monomethyl ether acetate and water are preferred. After step (X) or step (Y), in step (Z), the protective film can be removed by ashing or treatment with hydrofluoric acid, an organic solvent, an alkali developer or a semiconductor cleaning solution. Then, it is preferably washed with any solvent, a common semiconductor cleaning solution or the like. Steps (X), (Y), and (Z) can be performed simultaneously with steps (A), (B), and (C) or at any time point before or after each step. For example, when step (X) is included before step (A), step (Y) for removing part of the resist film on the protective film can be performed between step (A) and step (B), and step (Z) for removing the protective film can be performed between step (Y) and step (B). In addition, when step (X) is included between step (A) and step (B) or step (C), step (Z) for removing the protective film can also be performed between step (X) and step (B) or step (C). (3-3: step (B) of irradiating the resist film with light or electron beams and then developing the resist film to form a resist pattern; and step (C) of processing the semiconductor substrate by etching) (3-3-1: Exposure in step (B)) The exposure of the resist film can be performed through a mask (intermediate mask) for forming a predetermined pattern, and for example, i-line, KrF excimer laser, ArF excimer laser, EUV (extreme ultraviolet) or EB (electron beam) can be used. It should be noted that a mild bake (SB) can be performed before exposure, and a post-exposure heating (PEB) can be performed before development after exposure. Preferably, the temperature of the post-exposure heating is 50°C to 150°C, and the time of the post-exposure heating is 1 minute to 10 minutes. (3-3-2: Development in step (B)) In the development, an alkali developer is used, which can be appropriately selected from a development temperature of 5°C to 50°C and a development time of 10 seconds to 300 seconds. As the alkali developer, for example, an aqueous solution of an inorganic base such as sodium hydroxide, potassium hydroxide, sodium carbonate, sodium silicate, sodium metasilicate, ammonia water, a primary amine such as ethylamine, n-propylamine, a secondary amine such as diethylamine, di-n-butylamine, a tertiary amine such as triethylamine, methyldiethylamine, an alcohol amine such as dimethylethanolamine, triethanolamine, a quaternary ammonium salt such as tetramethylammonium hydroxide, tetraethylammonium hydroxide, choline, a cyclic amine such as pyrrole, piperidine, etc. can be used. The alkali concentration of these aqueous solutions is not particularly limited, and for example, it can be set to 0.1 to 10% by weight. In addition, an appropriate amount of alcohols such as isopropyl alcohol and nonionic surfactants may be added to the aqueous solution of the above-mentioned alkalis for use. Each of these may be preferably blended in the range of 0.01 to 10 parts by weight, more preferably 0.1 to 5 parts by weight, relative to 100 parts by weight of the developer. Among them, a preferred developer is a quaternary ammonium salt, and more preferably tetramethylammonium hydroxide and choline. In addition, surfactants may be added to these developers. Alternatively, a method may be adopted in which a polyol solvent having 2 to 18 carbon atoms such as 1,2-propylene glycol or an organic solvent such as butyl acetate is used instead of an alkaline developer to develop the portion of the photoresist where the alkaline dissolution rate is not increased. (3-3-3: Baking in step (B)) Step (B) may include baking the semiconductor substrate after the exposure and development. The baking method is not particularly limited, and for example, a proximity baking furnace is suitable, wherein a plurality of substrate support pins are used between the substrate and the heating plate to ensure a gap. The baking temperature is usually 40° C. to 300° C., preferably 200° C. to 300° C. for 1 to 30 minutes. However, when it is necessary to avoid damage to the resist pattern, the baking temperature may be 90° C. or lower. The baking may be performed on the semiconductor substrate after the exposure and before the development. The means and conditions for baking are as described above, but when it is necessary to avoid damage to the resist pattern, the baking temperature may be set to 90° C. or less. (3-3-4: Etching in step (C)) Next, the resist lower layer film is etched, preferably dry-etched, using the formed resist pattern as a mask to form a patterned resist. At this time, if the inorganic film is formed on the surface of the semiconductor substrate used, the surface of the inorganic film is exposed, and if the inorganic film is not formed on the surface of the semiconductor substrate used, the surface of the semiconductor substrate is exposed. Then, the semiconductor substrate is processed by a method known per se (dry etching method, etc.) using the patterned resist. The etching used to process the above-mentioned semiconductor substrate can be a known method. For example, when the semiconductor substrate is a silicon substrate, in addition to the process of performing shape processing by dry etching using a fluorine-based gas such as carbon tetrafluoride, it also includes a surface treatment process such as removing the silicon nitride film present on the surface of the semiconductor substrate using hot phosphoric acid. <4. Method for manufacturing a wafer for semiconductor manufacturing

[21] > (4-1) A method for manufacturing a semiconductor manufacturing wafer as one embodiment of the present invention comprises the following steps: in the method for manufacturing a semiconductor device as described above, a composition for forming a semiconductor manufacturing wafer edge protective film as one embodiment of the present invention

[10] is applied (or coated) to the front end of a semiconductor manufacturing wafer precursor and optionally to the chamfered portion and / or back end of the wafer precursor to manufacture a semiconductor manufacturing wafer with a protective film. Here, the so-called semiconductor manufacturing wafer precursor refers to a semiconductor manufacturing wafer precursor obtained by subjecting a semiconductor substrate to at least one process of a semiconductor device manufacturing method. For example, the following raw materials can be cited, which are raw materials that have undergone a process of forming an inorganic film, a resist underlayer film, a resist film, etc. on a semiconductor substrate in the semiconductor device manufacturing method as described above, and are raw materials before being supplied to a process of forming a resist pattern by irradiating the resist film with light or electron beams and then developing it. (4-2: Specific method of manufacturing a wafer for semiconductor manufacturing) The composition for forming a semiconductor wafer edge protective film [5] which is one embodiment of the present invention is applied by spin coating on the front edge of a semiconductor manufacturing wafer precursor obtained through one or more steps in a semiconductor device manufacturing process and optionally on the chamfered portion and / or back edge of the semiconductor manufacturing wafer precursor. Then, the semiconductor substrate may be baked. In this case, the baking method is not particularly limited, and for example, a proximity baking furnace is suitable, in which a plurality of substrate support pins are used between the substrate and the heating plate to ensure a gap. The baking temperature is generally 40°C to 300°C, preferably 200°C to 300°C for 1 to 30 minutes. After the protective film-forming composition is applied, the end surface of the protective film may be subjected to known treatments in semiconductor manufacturing processes, such as edge bead removal and backside rinsing. Example <Synthesis example 1> 1 g of 4-benzoylphenyl methacrylate, 10.3 g of 2-hydroxypropyl methacrylate, and 0.2 g of 2,2'-azobis(methyl isobutyrate) were dissolved in 29.5 g of ethyl lactate and 12.6 g of propylene glycol monomethyl ether acetate, and the mixture was heated to 80°C and reacted for 24 hours to obtain a solution of a copolymer polymer compound (having repeating units of the following formulas (I) and (II)) formed of 4-benzoylphenyl methacrylate and 2-hydroxypropyl methacrylate. GPC analysis of the obtained copolymer polymer compound revealed that the weight average molecular weight was 35,000 in terms of standard polystyrene. <Synthesis example 2> 1.5 g of 4-benzoylphenyl methacrylate, 1.6 g of 2-hydroxypropyl methacrylate, 10 g of styrene, and 0.3 g of 2,2'-azobis(methyl isobutyrate) were dissolved in 37.5 g of ethyl lactate and 16.1 g of propylene glycol monomethyl ether acetate, and the mixture was heated to 80°C and reacted for 24 hours to obtain a solution of a copolymerized polymer compound (having repeating units of the following formulas (I) to (III)) formed by 4-benzoylphenyl methacrylate, 2-hydroxypropyl methacrylate, and styrene. The obtained polymer solution was reprecipitated in methanol and then dried in a vacuum oven to obtain a white polymer compound. GPC analysis of the obtained polymer compound was performed, and the weight average molecular weight was 34,000 in terms of standard polystyrene. <Synthesis example 3> 10 g of 2-hydroxypropyl methacrylate and 0.2 g of 2,2'-azobis(methyl isobutyrate) were dissolved in 28.9 g of ethyl lactate and 12.2 g of propylene glycol monomethyl ether acetate, and the mixture was heated to 80°C and reacted for 24 hours to obtain a solution of a polymer compound of 2-hydroxypropyl methacrylate (having a repeating unit of formula (II)). GPC analysis of the obtained copolymer polymer compound was performed, and the weight average molecular weight was 35,000 in terms of standard polystyrene. <Synthesis Example 4> To 30.00 g of a novolak resin having an epoxy group (product name: EPPN-201, epoxy value: 192 g / eq., manufactured by Nippon Kayaku Co., Ltd.), 11.26 g of acrylic acid, 1.99 g of tetrabutylphosphonium bromide, and 0.09 g of hydroquinone, 101.11 g of propylene glycol monomethyl ether acetate was added, and the mixture was heated and stirred at 100°C for 18 hours under a nitrogen atmosphere. To the resulting solution, 43 g of an anion exchange resin (product name: AMBERJET[registered trademark]ESG4002(OH), manufactured by Organo Corporation) and 43 g of a cation exchange resin (product name: Amberlite[registered trademark]15JWET, manufactured by Organo Corporation) were added, and ion exchange treatment was carried out at room temperature for 4 hours. After separating the ion exchange resins, a compound solution was obtained. The obtained compound corresponded to a high molecular compound having a repeating unit of formula (XX), and the weight average molecular weight Mw measured by GPC in terms of polystyrene was 6,900. <b. Preparation of Composition> <Composition 1> To 8 g of the reaction product obtained in Synthesis Example 1, 4.5 g of ethyl lactate and 1.9 g of propylene glycol monomethyl ether acetate were added, and then filtration was carried out using a polyethylene microfilter having a pore size of 0.10 μm to prepare a photocurable resin composition solution. <Composition 2> To 4 g of the reaction product obtained in Synthesis Example 2, 16 g of propylene glycol monomethyl ether acetate was added, and then filtration was carried out using a polyethylene microfilter having a pore size of 0.10 μm to prepare a photocurable resin composition solution. <Comparative Example 1> To 8 g of the reaction product obtained in Synthesis Example 3, 4.5 g of ethyl lactate and 1.9 g of propylene glycol monomethyl ether acetate were added, and then filtration was carried out using a polyethylene microfilter having a pore size of 0.10 μm to prepare a photocurable resin composition solution. <Comparative Example 2> To 11.72 g of the resin solution obtained in Synthesis Example 4 (solid content: 23.73% by mass), 0.28 g of Irgacure Oxe01 (manufactured by BASF Japan Ltd.) as a photoinitiator, 0.008 g of Megafac R-30 (manufactured by Dainippon Ink and Chemicals, Inc.) as a surfactant, 0.042 g of Irganox 3114 (manufactured by BASF Japan Ltd.) as an antioxidant, 0.042 g of KBM-5103 (manufactured by Shin-Etsu Chemical Co., Ltd.) as an adhesion improver, and 17.91 g of propylene glycol monomethyl ether acetate were added, followed by filtration to prepare a photocurable resin composition solution. <c. Dissolution Test in Photoresist Solvent> The photocurable resin composition solutions prepared in Composition Examples 1 to 2 and Comparative Example 1 were applied onto a silicon wafer using a spinner. After baking at 80°C for 1 minute on a hot plate, 254 nm light was irradiated at 300 mJ / cm 2 using an aligner (PLA-501 Canon Inc.) to form a photocured film (film thickness: 0.10 μm). The photocured film was immersed in cyclohexanone, a solvent used for the photoresist. It was confirmed that the film was insoluble in the solvent in Composition Examples 1 to 2, but the film dissolved in the solvent in Comparative Example 1. <d. Solvent Resistance Test in Edge Exposure> The photocurable resin composition solutions prepared in Composition Examples 1 to 2 and Comparative Example 1 were applied onto a 12-inch silicon wafer using a spinner. After baking at 80°C for 1 minute on a hot plate, the edge of the wafer was irradiated at 50 mJ / cm 2 using the WEE of Lithiuspro (Tokyo Electron Limited) to form a photocured film (film thickness: 0.30 μm). The photocured film was immersed in OK73 thinner, a solvent used for the photoresist. It was confirmed that the film was insoluble in the solvent in Composition Examples 1 to 2, but the film dissolved in the solvent in Comparative Example 1. <Measurement of Dry Etching Rate> The photocurable resin composition solutions prepared in Composition Example 2 and Comparative Example 2 were applied onto a silicon wafer using a spinner. Then, 254 nm light was irradiated at 300 mJ / cm 2 using an aligner (PLA-501 Canon Inc.) to form a photocured film (film thickness: 0.10 μm). Then, using a RIE system (RIE-10NR) manufactured by Samco and using CF 4 as a dry etching gas, the dry etching rate (the amount of film thickness reduction per unit time) was measured under this condition. The dry etching rates of the photocurable resins formed from Composition Example 2 and Comparative Example 2 were compared. The results are shown in the table. Table 1 shows the etching rates when the dry etching rate of Comparative Example 2 is set to 1.00. [Table 1] Table 1 This revealed that the photocured film obtained from the photocurable resin-forming composition which is one embodiment of the present invention has greater dry etching resistance than that of Comparative Example 2.

Claims

1. A photocurable resin composition, comprising a self-crosslinking polymer (A) and a solvent (B), wherein the self-crosslinking polymer (A) comprises a first monomer unit (a) and a second monomer unit (b), wherein the first monomer unit (a) comprises an aromatic ketone residue in a side chain; and the second monomer unit (b) comprises an aliphatic hydrocarbon residue (b-1) and / or an aromatic ring residue (b-2) in a side chain, wherein the aliphatic hydrocarbon residue (b-1) comprises a carbon atom that is susceptible to hydrogen abstraction reaction. 2 . The photocurable resin composition according to claim 1 , further comprising a crosslinkable polymer or a crosslinkable compound (C) other than the self-crosslinkable polymer (A).

3. The photocurable resin composition according to claim 2, wherein the crosslinking group in the crosslinking polymer or crosslinking compound (C) is selected from epoxy group, (meth) acrylic group, vinyl group, carboxylic acid group, thiol group, silanol group, cinnamoyl group and hydroxyl group. 4 . The photocurable resin composition according to claim 1 , which has a viscosity of 100 cps or less at 25° C. 5 . A composition for forming a wafer edge protective film for semiconductor manufacturing, comprising the photocurable resin composition according to claim 1 . 6 . A protective film which is a cured product of a coating film made from the composition for forming a wafer edge portion protective film for semiconductor manufacturing according to claim 5 . The protective film according to claim 6 , having a thickness of 1 to 500 nm. The protective film according to claim 6 or 7, which is used to prevent metal contamination at the end of a wafer. 9 . The protective film according to claim 6 , which is obtained by curing with light having a wavelength of 170 to 800 nm. 10 . A semiconductor manufacturing wafer having a protected wafer edge, wherein the semiconductor manufacturing wafer is formed by applying the composition for forming a semiconductor manufacturing wafer edge protective film according to claim 5 to an edge of a wafer precursor.

11. A method for manufacturing a semiconductor device, comprising the following steps: Step (A), forming a resist film on a semiconductor substrate; Step (B) of forming a resist pattern by irradiating the resist film with light or electron beams and then developing the resist film; and Step (C), processing the semiconductor substrate by etching, The method for manufacturing the semiconductor device further includes the following step (X): A protective film made of the composition for forming a wafer edge protective film for semiconductor manufacturing according to claim 5 is formed on the front edge of a wafer for semiconductor manufacturing and optionally on the chamfered portion and / or the back edge of the wafer. 12 . The method for manufacturing a semiconductor device according to claim 11 , comprising a step (X) before the step (A). 13 . The method for manufacturing a semiconductor device according to claim 11 , further comprising a step (X) between the step (A) and the step (B). 14 . The method for manufacturing a semiconductor device according to claim 11 , further comprising a step (X) after the step (B) or the step (C). 15 . The method for manufacturing a semiconductor device according to claim 11 , further comprising, after the step (X), a step (Y) of removing a portion of the resist film on the protective film. 16 . The method for manufacturing a semiconductor device according to claim 11 , further comprising a step (Z) of removing the protective film after the step (X). 17 . The method for manufacturing a semiconductor device according to claim 15 , further comprising a step (Z) of removing the protective film after the step (Y). 18 . The method for manufacturing a semiconductor device according to claim 11 , wherein the resist film contains a metal.

19. The method for manufacturing a semiconductor device according to any one of claims 11 to 18, wherein in the step (X), the composition for forming a wafer edge protective film for semiconductor manufacturing according to claim 5 is applied and a predetermined area is exposed and developed.

20. The method for manufacturing a semiconductor device according to claim 16 or 17, wherein step (Z) is performed by ashing, or by treating with hydrofluoric acid, an organic solvent, an alkaline developer, or a semiconductor cleaning solution.

21. A method for manufacturing a semiconductor wafer, comprising the following steps: The composition for forming a wafer edge protective film for semiconductor manufacturing according to claim 5 is applied to an edge of a wafer precursor to manufacture a wafer having the edge protected.

22. The photocurable resin composition according to any one of claims 1 to 4, wherein the aryl ketone residue is a residue of an aryl ketone selected from acetophenone, benzophenone, anthraquinone, anthrone, heteroatom-substituted anthrone analogs of the following structural formula, and derivatives of these compounds having substituents, X is O, S or NR, and R is a hydrogen atom, a hydrocarbon group or an acyl group.

23. The photocurable resin composition according to any one of claims 1 to 4, wherein the carbon atom in the hydrocarbon chain (b-1) that is susceptible to hydrogen abstraction reaction is selected from tertiary carbon atoms, secondary carbon atoms, and methyl, methylene or methine groups directly connected to an aromatic ring. 24 . The photocurable resin composition according to claim 1 , wherein the aromatic ring (b-2) is an aromatic ring having 6 to 40 carbon atoms which may have a substituent.

25. According to any one of claims 1 to 4, the ratio of the number of repetitions of the first monomer unit to the number of repetitions of monomer units other than the first monomer unit including the second monomer unit is selected so that when a film with a film thickness of 300 nm is formed, the transmittance of the film at a wavelength of 300 nm is greater than 0.01%.

26. A self-crosslinking polymer (A), comprising a first monomer unit (a) and a second monomer unit (b), wherein the first monomer unit (a) comprises an aromatic ketone residue in a side chain; and the second monomer unit (b) comprises an aliphatic hydrocarbon residue (b-1) and / or an aromatic ring residue (b-2) in a side chain, wherein the aliphatic hydrocarbon residue (b-1) comprises a carbon atom that is susceptible to hydrogen abstraction reaction.

Citation Information

Patent Citations

  • Semiconductor device manufacturing method

    JP2011228340A

  • Glass protection film forming composition and glass protection film

    JP2016003160A

  • Substrate processing method

    JP2017098333A

  • Photocurable film-forming composition and method of forming a photocurable film

    WO2009104643A1

  • Multileveled substrate coating film forming composition containing plasma-curable compound based on unsaturated bonds between carbon atoms

    WO2018190380A1