Electrometallurgy titanium-iron separation process for ilmenite

Conductive titanium oxide is generated through the direct reduction of iron process and the electrodeposition process is used to separate titanium and iron, which solves the problems of low titanium resource utilization and safety risks of the hydrogen reduction process, and achieves efficient titanium-iron separation and low energy consumption. Ironmaking process.

CN118756246APending Publication Date: 2024-10-11冯采荻
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411060960.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-05
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

The utilization rate of titanium resources in vanadium-titanium magnetite is low. The existing iron-making process has problems such as difficulty in controlling the titanium content in blast furnace slag, poor fluidity of slag caused by low-priced titanium, high carbon emissions, and safety risks in the hydrogen reduction process.

Method used

The direct reduction iron process is used to generate conductive titanium oxide, and the titanium element is separated from iron through the electrodeposition process to avoid the high-temperature melting process. The conductivity of low-priced titanium is used for electrolytic separation, and alkaline, neutral or acidic electrolytes are used. Perform electrodeposition.

Benefits of technology

It achieves the separation of titanium and iron, improves the iron yield and the utilization rate of titanium resources, reduces power consumption and carbon emissions, and avoids high energy consumption and safety risks in the high-temperature melting process.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides an electrometallurgy ferrotitanium separation process for ilmenite. The ilmenite or vanadium titano-magnetite is prepared into direct reduced iron through a direct reduced iron process. In this step, 75% or more of the iron in the oxidation state is reduced to metallized iron. The titanium element in the ilmenite is reduced to a lower valence state in the direct reduction iron process and / or the subsequent deep reduction process, so that the titanium-containing phase material in the solid material has conductivity. And then the direct reduction iron is used as an anode, through an electro-deposition process, iron elements in the direct reduction iron enter an electrolyte solution to form iron ions or complex iron ions, the ions pass through the electrolyte solution and / or a diaphragm and are reduced into pure iron at the cathode, and a titanium-containing phase material is left on one side of the anode, so that separation of the titanium and the iron is completed. The process has the advantages that the melting separation process is not needed, the power consumption is low, the titanium and the iron can be effectively separated, and the titanium resource in the ilmenite can be effectively utilized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of iron and steel metallurgy and relates to a process for separating iron and titanium in an ironmaking process. Background Art

[0002] my country's vanadium-titanium magnetite is widely distributed in Panzhihua and Chengde. According to a report in Panzhi Daily on April 10, 2023, the Panzhihua region has a proven reserve of 8.67 billion tons of vanadium-titanium magnetite, ranking first in the world in terms of titanium resource reserves, but the utilization rate of titanium resources is only 29%. In the process of blast furnace ironmaking, titanium-containing iron ore needs to control the titanium content in blast furnace slag to avoid problems such as excessive viscosity of molten blast furnace slag. Taking the vanadium-iron magnetite in Panzhihua as an example, after beneficiation, balling and oxidative roasting, the oxidized pellets obtained generally have an iron content of 53-55%, and the titanium content is about 10% in terms of titanium dioxide. If such an ore is used entirely in blast furnace ironmaking, the content of titanium dioxide in the slag will be as high as about 43% based on the iron ore grade of 54% and the iron recovery rate of 100% (the actual general ore iron recovery rate is more than 99%, and the vanadium-titanium magnetite iron recovery rate is about 96%) without the addition of other furnace charges. With such a high titanium dioxide content, the viscosity of the molten blast furnace slag is very high. It is necessary to add general ore and / or other slag-making materials to reduce the titanium dioxide content in the blast furnace slag and control the titanium dioxide content below 23%. With such a blast furnace ironmaking process, not only are the raw materials diverse and complicated, but the blast furnace slag cannot be used directly to extract titanium. The most advanced process for blast furnace slag with a titanium dioxide content of 23% is to reduce it to titanium carbide at high temperature, and the titanium carbide reacts with chlorine at a lower temperature to form titanium tetrachloride, which is then used in the production of chloride titanium dioxide or sponge titanium. However, even with such a process, due to its high process difficulty, only one large steel plant has been researched and developed for 10 years, and it has not yet been industrialized. The vast majority of steel mills that use vanadium-titanium magnetite control the titanium dioxide in blast furnace slag to a lower level, generally around 16~18%. Its blast furnace slag is used to produce cement or building bricks. The titanium resources inside are wasted.

[0003] The existing solution generally adopts the direct reduction iron process, which reduces vanadium-titanium magnetite with carbon or reducing gas at about 1000°C to produce direct reduced iron, and then conducts magnetic separation, gravity separation or electric furnace smelting to separate titanium and iron to obtain direct reduced iron and titanium slag. Direct reduced iron can enter the electric furnace for steelmaking, and titanium slag is used to extract titanium. The direct reduction iron process using coke or other coal not only has high carbon emissions, but also carbon will bring in a certain amount of impurities, reducing the grade of titanium in the obtained titanium slag. The key is that the direct reduction iron process using coke or coal, whether it is a rotary kiln or a vertical kiln, is difficult to produce on a large scale. In fact, there is no large-scale production capacity and process route.

[0004] The gas-based reduction ironmaking process is used to produce direct reduced iron, which is applied to vanadium-titanium magnetite, and can solve the problem of iron-titanium separation while maintaining low carbon or even micro-carbon emissions. However, the gas-based (hydrogen) direct reduction iron process currently also has great problems, and there is no safe and feasible process so far. When the gas-based direct reduction ironmaking process is used, because the reduction of ferric oxide by hydrogen is a strong endothermic reaction, heat supply for the reaction becomes a serious problem. Because of the need to provide heat for the gas-based reduction reaction of hematite, the existing process is to preheat the raw gas first, and then add some oxygen to it, and some methane, CO or hydrogen in the raw gas is burned with oxygen to provide heat for the reaction. Even so, the temperature of the reducing gas entering the furnace is generally around 950°C. However, the sensible heat of the oxidized pellets and the gas entering the vertical kiln is still insufficient compared to the latent heat of the reaction required for the reaction. Moreover, hydrogen or hydrogen-rich gas is heated to such a high temperature, and the safety is very low. Furthermore, the combustion reaction of oxygen does not necessarily occur at the site of the reduction reaction of hydrogen and iron oxide (that is, the exothermic and endothermic are not in the same position, and heat transfer is required, and local overheating may also occur). The addition of extra oxygen also wastes reducing gas, generates water or CO2, and is not conducive to the reduction reaction of iron oxide. Moreover, the temperature of gas phase and solid phase materials will drop sharply during the endothermic reaction.

[0005] Due to the huge production capacity of the steel industry, the hydrogen reduction ironmaking process must be planned to have an annual production capacity of at least 500,000 tons. Whether using a vertical kiln or a rotary kiln, for large-scale endothermic reactions, the heating and heat transfer of such a large-scale reactor is a huge challenge. There are huge safety risks in heating hydrogen or hydrogen-rich gas. There is an explosion risk when oxygen is introduced into reducing gases such as hydrogen. Therefore, the reaction temperature of gas-based direct reduction of iron is generally below 950°C.

[0006] The titanium and iron in ilmenite or vanadium-titanium magnetite generally form iron brookite, which is difficult to be reduced below 950°C. In order to improve the iron yield, the direct reduction iron process generally uses coal-based, carbon-containing reducing gas for reduction. In both cases, the titanium dioxide in the ilmenite will be reduced to low-valent titanium or generate titanium carbide. Or in order to improve the iron yield, deep reduction is performed during the melting process, which will also reduce part of the 4-valent titanium oxide to a lower valence state or generate titanium carbide. Of course, the metallization rate of iron in direct reduced iron can also be increased by increasing the reaction temperature, which will also lead to the formation of more low-valent titanium phases.

[0007] However, since the titanium content in the residue of ilmenite and vanadium-titanium magnetite is relatively high, as long as low-valent titanium and / or titanium nitrides are generated, the viscosity of the slag will increase and the fluidity of the slag will decrease during the melting process, making it difficult to separate the slag from iron.

[0008] In addition, especially for vanadium-titanium magnetite, the total iron content is relatively low and the titanium dioxide content is relatively high, resulting in a relatively large amount of slag. If the smelting process is used to separate the slag and iron, the heating and melting of this part of the slag will also absorb a lot of heat, resulting in high power consumption in the smelting process.

[0009] Some studies have reported the use of electrolysis to produce high-purity iron from iron concentrate. However, since the iron concentrate itself is not conductive or has very poor conductivity, it is difficult for electrons to transfer to the current collector connected to the iron concentrate when it is used as an anode. When an alkaline solution is used as an electrolyte, a large amount of oxygen is precipitated on the anode, and the oxygen precipitation process becomes the main process of power consumption. When an acidic solution is used as an electrolyte, a large amount of hydrogen is precipitated on the cathode, which also wastes a lot of electricity. In an acidic solution, calcium and magnesium oxides in the iron concentrate are also easy to react with acid, which greatly increases the acid consumption and makes the composition of the acidic solution very complicated and difficult to operate. There are few reports on the use of neutral solution as an electrolyte to electrolyze iron concentrate to prepare high-purity iron. The conductivity of the iron concentrate and the ionic conductivity of the solution in the neutral solution are very poor, and the process of electrolytic reduction of iron is difficult to occur.

[0010] In summary, the use of vanadium-titanium magnetite in blast furnace ironmaking has the problem that the titanium content in blast furnace slag cannot be too high and the titanium in blast furnace slag cannot be effectively utilized at present. In order to recover the titanium in vanadium-titanium magnetite, the direct reduction iron process is used, and then the electric furnace is used for slag iron separation, which will eventually encounter the problem of poor slag fluidity caused by low-priced titanium and low iron recovery rate. Summary of the invention

[0011] The purpose of the present invention is to provide a process for separating iron and titanium in ilmenite with low energy consumption on a scale of 100,000 tons or even above 1 million tons, so as to obtain high-grade titanium slag and maintain a high iron yield in the iron-making process, so as to achieve the purpose of separating titanium and iron and effectively utilize the titanium and iron resources in ilmenite.

[0012] The object of the present invention is achieved in this way: using ilmenite or vanadium-titanium magnetite as raw materials, direct reduced iron is prepared by direct reduction iron process. The titanium element in ilmenite is fully or partially reduced in the direct reduction iron process and / or the subsequent deep reduction process to generate one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase material in the obtained solid material acquires conductivity. Subsequently, the solid material is used as an anode and an electrodeposition process is carried out in an electrolytic cell. The iron in the anode solid material enters the electrolyte to form divalent and / or trivalent iron ions, or complexed divalent or trivalent iron ions, and then these iron ions and / or their complexes are reduced to metallic iron at the cathode. The metallic iron obtained in this way has high purity and can also avoid the high-energy consumption melting process of about 1400°C.

[0013] The specific technical scheme of the present invention is a ilmenite electrometallurgical titanium-iron separation process, characterized in that: the ilmenite is prepared into direct reduced iron through a direct iron reduction process, with or without briquetting, and then the iron therein is fully or partially metallized and prepared into pure iron through an electrodeposition process, and the titanium in the ilmenite is retained in the residue. The ilmenite is ilmenite, vanadium-titanium magnetite, ilmenite-iron concentrate, recovered titanium-iron dust particles, and one or more of the above materials' graded preselection, concentrate forming, pre-burning, and pre-reduction products.

[0014] In the direct iron reduction process, more than 75% of the oxidized iron reacts with one or more of hydrogen, CO, solid inorganic carbon, ammonia, volatile organic matter, and solid organic matter to be reduced to metalized iron. Titanium in ilmenite often forms pseudobrookite with iron, which is difficult to reduce. However, in the process of the present invention, a high iron metallization rate is not pursued, because the metalized iron can also be electrolytically reduced to metallic iron in the subsequent electrodeposition process and deposited on the cathode of the electrolytic cell.

[0015] The titanium element in ilmenite is completely or partially reduced in the direct iron reduction process and / or the subsequent deep reduction process to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase material in the solid material has conductivity. Ilmenite, especially vanadium-titanium magnetite, has a relatively high content of titanium oxide in its slag phase, which will cause it to have a large resistance or be non-conductive. After it is partially reduced, it has good conductivity and can form a good conductor together with metallized iron as an electrode in the electroplating process. Titanium heptoxide obtained by shallow reduction of titanium dioxide, titanium nitride, titanium carbide and / or titanium carbonitride obtained by carbonitridation are all good conductors. Titanium dioxide is a semiconductor. After being shallowly reduced, titanium dioxide semiconductor doped with oxygen vacancies is obtained, which also has good conductivity.

[0016] Titanium makes it difficult to separate slag from iron in the existing ironmaking process, but in the process of the present invention, titanium becomes a favorable factor by utilizing the electrical conductivity of low-valent titanium. According to the test results, when solid carbon or carbon-containing gas is used as a reducing agent, it is more conducive to the formation of a conductive phase of titanium. When ammonia is contained in the reducing gas, it is also easier to generate a conductive phase of titanium. When pure hydrogen is used as a reducing agent, a higher reaction temperature is required to generate enough low-valent titanium oxides.

[0017] In the electroplating process, the titanium-containing solid phase material that has passed the above process is used as the anode, the anode is connected to the positive pole of the power supply, and the cathode is connected to the negative pole of the power supply. Under the action of the DC voltage on the cathode and anode of the electrolytic cell, the iron element in the solid phase material enters the solution to form one or more of divalent iron ions, trivalent iron ions, divalent iron ion complexes, and trivalent iron ion complexes. The iron ions are reduced to pure iron at the cathode through the electrolyte and / or the diaphragm. The titanium-containing phase material remains on one side of the anode, thereby completing the iron-titanium separation process. Since most of the iron elements have been metallized after the direct reduction of iron process, the electrolytic cell can maintain a relatively low voltage in the process of forming pure iron from the anode to the cathode, and does not need to consume too much electric energy. Due to an electrolytic process, the purity of the pure iron obtained at the cathode can reach more than 99.8%. The potential difference between the anode and the cathode is mainly used to overcome the interface potential, concentration difference potential, iron precipitation overpotential and resistance on the path between the anode and the cathode. Electroplating one ton of reduced iron consumes about 400kwh of electricity. The power consumption is less than half of that of electric furnace smelting. The problem is that electric furnace smelting also encounters the problem of low iron recovery rate or poor slag fluidity.

[0018] Even a small amount of iron that is not metallized before the electrodeposition process can be electrolytically reduced during the electrodeposition process and form pure iron at the cathode.

[0019] Furthermore, in the same process of direct reduction of iron, all or part of the titanium element in the ilmenite is reduced to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity. The electroplating process adopts an alkaline solution electroplating process, and the alkaline solution contains one or more of sodium ions, potassium ions, carboxylate ions, ammonia or ammonium ions, and nitrogen-containing organic matter. In the electroplating process of iron in an alkaline solution, there will be a phenomenon that iron ions and hydroxide ions form a precipitate and a phenomenon that the anode metal iron reacts with the alkaline solution to release hydrogen. The occurrence of the above phenomenon can be reduced or eliminated by adding ammonia water or nitrogen-containing organic matter to the solution to form a complex with iron.

[0020] Alternatively, the electrodeposition process adopts an acidic solution electrodeposition process, and the acidic solution contains one or more of sulfuric acid, hydrochloric acid, oxalic acid, formic acid, carboxylic acid, ammonia or ammonium ions, and nitrogen-containing organic matter. In the acidic electrolyte, the cathode metallic iron will produce a side reaction of releasing hydrogen. However, in the specific implementation process, the hydrogen can be collected and used as a reducing gas in the direct reduction of iron process.

[0021] Alternatively, the electrodeposition process adopts a neutral solution electrodeposition process, wherein the neutral solution contains one or more of sulfate ions, chloride ions, carboxylate ions, ammonia or ammonium ions, and nitrogen-containing organic matter. Ammonium or nitrogen-containing organic matter is also added to form a complex with iron ions to avoid the formation of iron hydroxide precipitation.

[0022] Furthermore, in the direct reduction iron process, ilmenite is fed into an electric heating kiln, and the ilmenite and / or the material obtained by the change in the heating process (hereinafter referred to as the material) are directly energized through the power supply electrode, and the material pile heats the material itself and / or the gas in the kiln by its own resistance heating. The material passes through the preheating section and the heating section in the electric heating kiln in sequence, and then is discharged; or the material passes through the preheating section, the heating section and the cooling section in the electric heating kiln in sequence, and then is discharged to obtain direct reduced iron.

[0023] The highest temperature of the material in the electric heating kiln is not less than 900°C, and all or part of the titanium element in the ilmenite is reduced to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity. The direct electric heating method can increase the temperature of the iron reduction reaction, increase the metallization rate of iron, and more importantly, is conducive to the formation of a conductive titanium phase.

[0024] Likewise, in the subsequent electrodeposition process, an alkaline, neutral or acidic electrolyte may also be used.

[0025] Furthermore, according to the ilmenite electrometallurgical titanium-iron separation process described in claim 1, the obtained direct reduced iron is subjected to a smelting process, and molten iron and titanium slag are obtained by heating and melting separation. The titanium slag is cooled and then subjected to the electroplating process to separate the residual iron from the titanium-containing phase material. Similarly, in the subsequent electroplating process, an alkaline, neutral or acidic electrolyte can also be used. Due to the smelting process, the material entering the subsequent electroplating process is greatly reduced, and the load of the process is also greatly reduced.

[0026] Alternatively, the obtained direct reduced iron is subjected to a melting process, and molten iron and titanium slag are obtained by heating and melting separation; the titanium slag is then subjected to a deep reduction process, and all or part of the titanium element therein is reduced to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity. The deep reduction process can be carried out immediately after the separation of slag and iron using the slag in a high temperature state. The deep reduction process will also metalize the unmetallized iron in the direct reduced iron process.

[0027] After cooling, the titanium slag is subjected to the electrodeposition process to separate the residual iron from the titanium-containing phase material. Similarly, in the subsequent electrodeposition process, an alkaline, neutral or acidic electrolyte may also be used.

[0028] Alternatively, the obtained direct reduced iron is subjected to a melting process, and molten iron and titanium slag are obtained by heating and melting separation. In the heating and melting process, deep reduction is performed to reduce all or part of the titanium element therein to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity. Then, slag-iron separation is performed to obtain titanium slag and molten iron. Due to the introduction of deep reduction before slag-iron separation, the viscosity of the titanium slag becomes larger, and a part of metallic iron will be mixed in it.

[0029] After cooling, the titanium slag is subjected to the electrodeposition process to separate the residual iron from the titanium-containing phase material. Similarly, in the subsequent electrodeposition process, an alkaline, neutral or acidic electrolyte may also be used.

[0030] Compared with the prior art, the present invention has the following advantages: 1) Compared with the existing process of direct reduction of iron followed by smelting and separation of slag and iron, the process of the present invention does not require a high-temperature smelting process, and the slag and iron separation process saves energy and reduces consumption significantly.

[0031] 2) Compared with the existing process of direct reduction of iron followed by smelting and separation of slag iron, the iron obtained by the process of the present invention has higher purity.

[0032] 3) Compared with the existing process of direct reduction of iron followed by smelting, slag iron separation and deep reduction, the process of the present invention avoids the problems of high viscosity of high-temperature titanium slag, low iron recovery rate and high iron content in titanium slag.

[0033] 4) Compared with the direct alkaline electrolyte electrolysis ironmaking process of iron ore, this process has low power consumption, does not have the problems of poor solubility of iron ore, poor conductivity making the electrolysis process difficult, and oxygen as a by-product of the process.

[0034] 5) Compared with the direct iron ore electrolytic ironmaking process with acid electrolyte, this process has low power consumption, basically does not consume acids such as sulfuric acid or hydrochloric acid, has low pollution, and can use neutral solution to avoid corrosion and avoid the problem of by-product hydrogen.

[0035] In summary, the present invention has opened up a technical route for the utilization of titanium resources in vanadium-titanium magnetite or other ilmenite ores with low carbon emissions, low power consumption, low investment and operating costs, high reliability, practical technology and high titanium resource utilization. DETAILED DESCRIPTION

[0036] Example 1

[0037] Iron ore pellets are oxidized and roasted to obtain oxidized pellets. In this embodiment, vanadium-titanium magnetite oxidized pellets with an iron content of about 54% and a titanium dioxide content of about 11% are used as raw materials. According to XRD analysis, the titanium dioxide in the raw material exists in the form of iron brookite, which is more difficult to reduce than hematite. The oxidized pellets are not preheated and directly enter the electric heating shaft kiln. After passing through the preheating section, the high-temperature hydrogen and / or CO (containing water vapor generated by the reduction reaction) from the heating section of the shaft kiln are heat exchanged in the preheating section. When it is preheated to about 650°C, the oxidized pellets are partially reduced and obtain conductivity. After the oxidized pellets move to the reduction section and / or heating section of the shaft furnace, the positive and negative electrodes of the heating power supply are set at both ends of the heating section, which feeds current into the material in the heating section, and the material is heated by the current, and the temperature is further increased to 950~1100°C. In the reduction section and / or heating section, the iron oxide in the oxidized pellets is reduced to sponge iron or direct reduced iron. After the cooling stage, the direct reduced iron is obtained. According to analysis, about 90% of the iron in the reduced pellets is reduced to metallic iron. The metallized pellets are pressed into a 20mm thick rectangular block as the anode of the electrolytic cell, in close contact with the anode current collector, with a 1mm thick pure iron sheet as the cathode, and an aqueous solution of ethylenediamine sulfate as the electrolyte, which is neutral. After a certain period of electrolysis, the cathode iron plate is removed and weighed to calculate the amount of pure iron obtained by electrolysis. It is calculated that the power consumption for electrodeposition of 1kg of pure iron is 0.42kwh. The total iron content in the residual titanium slag is ~4%. Based on the total iron in the direct reduced iron, the iron recovery rate in pure iron is ~98%. A small amount of calcium and magnesium ions enter the electrolyte, but their concentration quickly tends to be constant.

Claims

1. A process for separating ilmenite from ferro-titanium by electrosmelting of ilmenite, characterized in that: The ilmenite is subjected to a direct reduction iron process to produce direct reduced iron, with or without briquetting, and then the iron which is fully or partially metallized is subjected to an electrodeposition process to produce pure iron, and the titanium in the ilmenite is retained in the residue; The ilmenite is ilmenite, vanadium-titanium magnetite, ilmenite-containing iron concentrate, recovered titanium-containing iron dust particles, and one or more of the grading preselection, concentrate, molding, pre-burning, and pre-reduction products of the above materials; In the direct iron reduction process, more than 75% of the oxidized iron reacts with one or more of hydrogen, CO, solid inorganic carbon, ammonia, volatile organic matter, and solid organic matter to be reduced to metalized iron; The titanium element in the ilmenite is completely or partially reduced in the direct iron reduction process and / or the subsequent deep reduction process to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase material in the solid material acquires conductivity; In the electrodeposition process, the titanium-containing solid phase material that has undergone the aforementioned process is the anode, and the iron element in the solid phase material enters the solution to form one or more of divalent iron ions, trivalent iron ions, divalent iron ion complexes, and trivalent iron ion complexes. The iron ions pass through the electrolyte and / or the diaphragm and are reduced to pure iron at the cathode; the titanium-containing phase material remains on the anode side.

2. The ilmenite electrometallurgical ferro-titanium separation process according to claim 1, characterized in that: In the same process of direct reduction of iron, all or part of the titanium element in the ilmenite is reduced to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity; The electrodeposition process adopts an alkaline solution electrodeposition process, and the alkaline solution contains one or more of sodium ions, potassium ions, carboxylate ions, ammonia or ammonium ions, and nitrogen-containing organic matter.

3. The ilmenite electrometallurgical ferro-titanium separation process according to claim 1, characterized in that: In the same process of direct reduction of iron, all or part of the titanium element in the ilmenite is reduced to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity; The electrodeposition process adopts an acidic solution electrodeposition process, and the acidic solution contains one or more of sulfuric acid, hydrochloric acid, oxalic acid, formic acid, carboxylic acid, ammonia or ammonium ions, and nitrogen-containing organic matter.

4. The ilmenite electrometallurgical ferro-titanium separation process according to claim 1, characterized in that: In the same process of direct reduction of iron, all or part of the titanium element in the ilmenite is reduced to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity; The electrodeposition process adopts a neutral solution electrodeposition process, and the neutral solution contains one or more of sulfate ions, chloride ions, carboxylate ions, ammonia or ammonium ions, and nitrogen-containing organic matter.

5. The ilmenite electrometallurgical ferro-titanium separation process according to claim 1, characterized in that: In the direct iron reduction process, ilmenite is fed into an electric heating kiln, and the ilmenite and / or the material obtained by the heating process (hereinafter referred to as the material) in the kiln is directly energized through the power supply electrode, and the material pile heats the material itself and / or the gas in the kiln by its own resistance heating; The material passes through a preheating section and a heating section in an electric heating kiln in sequence, and then the material is discharged to obtain direct reduced iron; or the material passes through a preheating section, a heating section and a cooling section in an electric heating kiln in sequence, and then the material is discharged to obtain direct reduced iron; The maximum temperature of the material in the electric heating kiln is not less than 900°C, and all or part of the titanium element in the ilmenite is reduced to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity; The electrodeposition process adopts an alkaline solution electrodeposition process, and the alkaline solution contains one or more of sodium ions, potassium ions, ammonia or ammonium ions, and nitrogen-containing organic matter.

6. The ilmenite electrometallurgical ferro-titanium separation process according to claim 1, characterized in that: In the direct iron reduction process, ilmenite is fed into an electric heating kiln, and the ilmenite and / or the material obtained by the heating process (hereinafter referred to as the material) in the kiln is directly energized through the power supply electrode, and the material pile heats the material itself and / or the gas in the kiln by its own resistance heating; The material passes through a preheating section and a heating section in an electric heating kiln in sequence, and then the material is discharged to obtain direct reduced iron; or the material passes through a preheating section, a heating section and a cooling section in an electric heating kiln in sequence, and then the material is discharged to obtain direct reduced iron; The maximum temperature of the material in the electric heating kiln is not less than 900°C, and all or part of the titanium element in the ilmenite is reduced to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity; The electrodeposition process adopts an acidic solution electrodeposition process, and the acidic solution contains one or more of sulfuric acid, hydrochloric acid, oxalic acid, carboxylic acid, ammonia or ammonium ions, and nitrogen-containing organic matter.

7. The ilmenite electrometallurgical ferro-titanium separation process according to claim 1, characterized in that: In the direct iron reduction process, ilmenite is fed into an electric heating kiln, and the ilmenite and / or the material obtained by the heating process (hereinafter referred to as the material) in the kiln is directly energized through the power supply electrode, and the material pile heats the material itself and / or the gas in the kiln by its own resistance heating; The material passes through a preheating section and a heating section in an electric heating kiln in sequence, and then the material is discharged to obtain direct reduced iron; or the material passes through a preheating section, a heating section and a cooling section in an electric heating kiln in sequence, and then the material is discharged to obtain direct reduced iron; The maximum temperature of the material in the electric heating kiln is not less than 900°C, and all or part of the titanium element in the ilmenite is reduced to form one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity; The electrodeposition process adopts a neutral solution electrodeposition process, and the neutral solution contains one or more of sulfate ions, chloride ions, carboxylate ions, ammonia or ammonium ions, and organic amines.

8. The ilmenite electrometallurgical ferro-titanium separation process according to claim 1, characterized in that: The obtained direct reduced iron is subjected to a melting and separation process, and molten iron and titanium slag are obtained by heating and melting. The titanium slag is cooled and then subjected to the electrodeposition process to separate the residual iron and titanium-containing phase materials; The electrodeposition process adopts an alkaline solution electrodeposition process, and the alkaline solution contains one or more of sodium ions, potassium ions, ammonia or ammonium ions, and nitrogen-containing organic matter; or, the electrodeposition process adopts an acidic solution electrodeposition process, and the acidic solution contains one or more of sulfuric acid, hydrochloric acid, oxalic acid, carboxylic acid, ammonia or ammonium ions, and nitrogen-containing organic matter; or, the electrodeposition process adopts a neutral solution electrodeposition process, and the neutral solution contains one or more of sulfate ions, chloride ions, carboxylate ions, ammonia or ammonium ions, and organic amines.

9. The ilmenite electrometallurgical ferro-titanium separation process according to claim 1, characterized in that: The obtained direct reduced iron is subjected to a melting and separation process, and molten iron and titanium slag are obtained by heating, melting and separation; the titanium slag is subjected to a deep reduction process, and all or part of the titanium element in the titanium slag is reduced to generate one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity; The titanium slag is cooled and then subjected to the electrodeposition process to separate the residual iron from the titanium-containing phase material; The electrodeposition process adopts an alkaline solution electrodeposition process, and the alkaline solution contains one or more of sodium ions, potassium ions, ammonia or ammonium ions, and nitrogen-containing organic matter; or, the electrodeposition process adopts an acidic solution electrodeposition process, and the acidic solution contains one or more of sulfuric acid, hydrochloric acid, oxalic acid, carboxylic acid, ammonia or ammonium ions, and nitrogen-containing organic matter; or, the electrodeposition process adopts a neutral solution electrodeposition process, and the neutral solution contains one or more of sulfate ions, chloride ions, carboxylate ions, ammonia or ammonium ions, and organic amines.

10. The ilmenite electrometallurgical ferro-titanium separation process according to claim 1, characterized in that: The obtained direct reduced iron is subjected to a melting process, and is separated by heating and melting to obtain molten iron and titanium slag; deep reduction is performed in the heating and melting process, and all or part of the titanium element therein is reduced to generate one or more of titanium nitride, titanium carbide, titanium carbonitride, and titanium oxide with a valence lower than 4, so that the titanium-containing phase in the solid material acquires conductivity; then slag and iron are separated to obtain titanium slag and molten iron; The titanium slag is cooled and then subjected to the electrodeposition process to separate the residual iron from the titanium-containing phase material; The electrodeposition process adopts an alkaline solution electrodeposition process, and the alkaline solution contains one or more of sodium ions, potassium ions, ammonia or ammonium ions, and nitrogen-containing organic matter; or, the electrodeposition process adopts an acidic solution electrodeposition process, and the acidic solution contains one or more of sulfuric acid, hydrochloric acid, oxalic acid, carboxylic acid, ammonia or ammonium ions, and nitrogen-containing organic matter; or, the electrodeposition process adopts a neutral solution electrodeposition process, and the neutral solution contains one or more of sulfate ions, chloride ions, carboxylate ions, ammonia or ammonium ions, and organic amines.