Automotive upholstery and processing technology thereof

By placing the plate between the covering and the plastic shell during the processing of automotive interior parts, the problem of high-temperature plastic damage and raw material thickness limitations is solved, and the production of interior parts using softer materials and simplified processes is realized.

CN118769591APending Publication Date: 2024-10-15KUNSHAN ESON PRECISION ENGINEERING CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411037364.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

In the existing technology, during the processing of automobile interior parts, high-temperature plastic directly contacts leather or fabric, which can easily cause damage, and requires the use of thicker raw materials, making it difficult to process softer materials, and the process is complicated.

Method used

The method of placing the plate between the covering part and the plastic shell is used. By fixing the covering part on the plate, heating and pre-pressing the mold and then injecting the plastic, an interior part with the covering part is formed to avoid high temperatures. Direct contact with plastic and reduced raw material thickness requirements.

Benefits of technology

It effectively avoids damage to the covering parts, allows the use of softer materials and simplifies the process, enabling the production of interior parts with hardness and thickness that meet the requirements without increasing the thickness of leather or fabric.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118769591A_ABST
    Figure CN118769591A_ABST
Patent Text Reader

Abstract

The invention discloses an automotive upholstery and a processing technology thereof in the field of automotive upholstery, and aims to solve the problems that in the prior art, the processing technology of the upholstery is complicated, and raw materials of the upholstery are limited. Selecting a coating piece and a plate which are the same in size, and fixing the coating piece on one surface of the plate; placing the plate fixed with the coating piece on a mold of an injection molding machine, and starting the injection molding machine; the mold is closed to heat the plate, so that the plate is pre-pressed and formed; plastic is injected to the other face of the pre-pressed and formed plate to form a plastic shell, and the automotive interior trim part is obtained after forming. The plate is arranged in the middle layer of the product so as to isolate damage caused by direct contact between high-temperature plastic and a coating part during injection molding, the overall hardness and thickness of the interior trim part can be increased, and during injection molding, the needed interior trim part can be machined with few raw materials or soft raw materials, so that the production cost is reduced, and the production efficiency is improved. And the used leather or fabric can be normally produced without increasing the thickness.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of automobile interior decoration parts, and in particular to an automobile interior decoration part and a processing technology thereof. Background Art

[0002] Automobile interior parts are usually covered with a layer of leather or fabric to increase the three-dimensional sense and beauty of the interior parts structure and improve the overall grade. The existing technology forms interior parts with leather or fabric by artificially covering leather or fabric, or placing leather or fabric directly on a mold and then injection molding. However, this method has certain requirements on the thickness of the leather or fabric, and the raw materials for injection molding also need to use harder materials to meet the use requirements of interior parts. If the thickness of the leather or fabric used is small, the high-temperature injection molding raw materials will directly contact the leather or fabric and will be damaged. The above method cannot process softer raw materials and requires thicker leather or fabric, which has the problem of limited raw material material and coating thickness. Summary of the invention

[0003] The purpose of the present application is to provide an automotive interior trim and its processing technology, which adopts a method of placing a plate between a covering part and a plastic shell to avoid high-temperature plastic damaging the covering part during processing, and can quickly process an interior trim with a covering part without using a thicker covering part.

[0004] In order to solve the above technical problems, the following technical solutions are adopted: In a first aspect, the present application provides a process for processing automotive interior trim parts, comprising the following steps: Selecting a covering piece and a plate of the same size, and fixing the covering piece on one side of the plate; Placing the plate with the covering member fixed thereon on a mold of an injection molding machine, and starting the injection molding machine; The mold is closed and the plate is heated to pre-press the plate into shape; Plastic is injected into the other side of the pre-pressed plate to form a plastic shell, and the automobile interior decoration part is obtained after molding.

[0005] Optionally, before placing the plate with the covering member fixed thereto on a mold of an injection molding machine, the plate with the covering member fixed thereto is cut according to the shape and size of the automobile interior decoration member.

[0006] Optionally, after molding, the automobile interior decoration component is cooled to room temperature, and then the cooled automobile interior decoration component is trimmed.

[0007] Optionally, the covering comprises any one of leather and fabric.

[0008] Optionally, the covering member is fixed to one surface of the plate by an adhesive.

[0009] Optionally, the adhesive is glue.

[0010] Optionally, the plate is made of polypropylene or nylon reinforced material.

[0011] In a second aspect, the present application provides an automobile interior decoration part, which is manufactured using the automobile interior decoration part processing technology described in the first aspect.

[0012] Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention fixes the covering part required for the interior decoration part on one side of the plate, and then places it on the mold and injects plastic into the other side of the plate to form a plastic shell with the covering part and the plate. The plate is located in the middle layer of the shell to isolate the high-temperature plastic from direct contact with the covering part during injection molding to cause damage, and can also increase the hardness and thickness of the overall interior decoration part. During injection molding, less raw materials can be used to obtain interior decoration parts with desired hardness and thickness, and softer raw materials can also be used to process the desired interior decoration parts. The leather or fabric used can be produced normally without increasing the thickness.

[0013] 2. The present invention fixes a large piece of leather or fabric on one side of a large plate, and then cuts it into the required shape and size, thereby reducing the process flow. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 This is a schematic diagram of the plate structure of Example 1 in this application Figure 2 It is a schematic diagram of the structure of the formed composite plate of Example 1 in the present application; Figure 3 It is a schematic diagram of the interior decoration structure of Example 1 in this application.

[0015] Description of reference numerals: 1. Covering parts; 2. Glue layer; 3. Board material; 4. Molded composite board material; 5. Interior decoration parts. DETAILED DESCRIPTION

[0016] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present application and its application or use. Example 1

[0017] like Figure 1-3 As shown, this embodiment provides a process for processing automobile interior decoration parts, comprising the following steps: A covering part 1 and a plate 3 of the same size are selected. The covering part 1 is made of leather or fabric. The thickness of the covering part 1 can be the same as that of an ordinary hand-wrapped covering part. The thickness of the plate 3 is selected according to the requirements of the interior decoration parts to be processed and the plastic raw materials used. When a softer plastic raw material is selected, a thicker plate 3 is selected to meet the hardness requirements of the interior decoration parts. When a harder plastic raw material is selected, a thinner plate 3 is selected. At this time, the main function of the plate 3 is to separate the covering part 1 from the high-temperature plastic.

[0018] The sheet 3 can be a polypropylene or nylon reinforced material. A glue layer 2 is applied to one side of the sheet 3, and then a covering 1 is placed thereon. After the glue layer 2 is completely dry, the covering 1 is fixed on one side of the sheet 3 to obtain a composite sheet. The obtained composite sheet has a large surface area and is cut into small pieces of composite sheet of the size and shape of the required interior parts.

[0019] Place a small piece of composite sheet with the same shape as the interior part on the mold of the injection molding machine, and position it on the mold so that it completely covers the mold, ensuring that it will not move during the injection molding process, and start the injection molding machine.

[0020] The mold is closed to heat the composite sheet, and the composite sheet is pre-pressed and formed by the preset temperature on the mold to become a formed composite sheet 4 with the same shape as the required interior decoration part.

[0021] High-temperature liquid plastic is injected into the other side of the molded composite sheet 4, and the high-temperature liquid plastic is molded in the mold and bonded together with the side in contact with the molded composite sheet 4 to form a plastic shell. After molding, the robot takes out the plastic shell, and after the plastic shell is cooled, it is trimmed to obtain the interior decoration part 5.

[0022] When processing interior parts, adding sheets, compared with general plastic molding, only a few seconds are required to pre-press and mold the sheets with covering parts. The surface of the interior parts after injection molding has covering parts, and no subsequent manual covering is required, which simplifies the process flow.

[0023] The interior parts obtained through the above steps have a covering on the upper surface, which does not need to be covered manually. The covering is fixed on the plate to form a composite plate, and then plastic is injected into the side of the composite plate without the covering fixed. The plastic forms a plastic shell and is bonded to the plate with the covering. Softer plastic can be used to increase the thickness of the plate to meet the required hardness and compressive strength of the interior parts. The thickness and material of the plate can be selected according to the plastic material and the requirements of the finished product. Increasing the selectivity of plastic raw materials can separate the covering from the high-temperature plastic liquid during the injection molding process to avoid high temperature damage to the covering. Example 2

[0024] This embodiment provides an automobile interior decoration part based on Embodiment 1. The interior decoration part is produced by the automobile interior decoration part processing technology provided in Embodiment 1. The interior decoration part is a three-layer structure, the upper surface of which is a covering part, the middle is a plate material, and the lower surface is the injection molded plastic shell. Since a plate material is arranged in the middle, the plastic shell can be made of a softer material, and an interior decoration part that meets the required hardness can also be processed. The plate material in the middle can also prevent the high-temperature plastic liquid from contacting the covering part during the processing of the interior decoration part.

[0025] The above is only a preferred implementation of the present application. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present application. These improvements and modifications should also be regarded as the scope of protection of the present application.

Claims

1. A process for processing automobile interior decoration parts, characterized in that: The following steps are involved: Selecting a covering piece and a plate of the same size, and fixing the covering piece on one side of the plate; Placing the plate with the covering member fixed thereon on a mold of an injection molding machine, and starting the injection molding machine; The mold is closed and the plate is heated to pre-press the plate into shape; Plastic is injected into the other side of the pre-pressed plate to form a plastic shell, and the automobile interior decoration part is obtained after molding.

2. The automotive interior trim processing technology according to claim 1, characterized in that: Before placing the plate with the covering part fixed thereto on the mold of the injection molding machine, the plate with the covering part fixed thereto is cut according to the shape and size of the automobile interior decoration part.

3. The automotive interior trim processing technology according to claim 1, characterized in that: After forming, the automobile interior decoration part is cooled to room temperature, and then the cooled automobile interior decoration part is trimmed.

4. The automotive interior trim processing technology according to claim 1, characterized in that: The covering element comprises any one of leather and fabric.

5. The automotive interior trim processing technology according to claim 1, characterized in that: The covering member is fixed on one side of the plate material by means of an adhesive.

6. The automotive interior trim processing technology according to claim 5, characterized in that: The bonding material is glue.

7. The automotive interior trim processing technology according to claim 1, characterized in that: The material of the plate is polypropylene or nylon reinforced material.

8. An automotive interior component, characterized in that: The automotive interior decoration part is manufactured by the processing technology of any one of claims 1 to 7.

Citation Information

Patent Citations

  • Decorative components for motor vehicle interiors

    CN1938140A

  • Three layer plastic panel and method of making same

    EP1477367A1

  • Interior trim component and method of forming same

    US20030080466A1

  • Trim component for vehicle interior

    US20170043514A1