Spiral aluminum flux-cored cesium welding ring

Through the spiral structure of aluminum flux cored cesium welding ring, combined with the combination of potassium fluoroaluminate and cesium fluoroaluminate flux and aluminum silicon welding skin, the defects caused by high welding temperature in aluminum alloy brazing are solved and the welding quality is improved. and penetration effect.

CN118808992APending Publication Date: 2024-10-22GUANGDONG HANGJI METAL PRODUCT INDUSTRIES CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411139628.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

In the existing aluminum alloy brazing technology, high welding temperatures lead to defects such as overburning and perforation of the base metal, surface depressions, pitting, etc., and there is also the problem of poor penetration effect.

Method used

An aluminum flux-cored cesium welding ring with a spiral structure is used. The welding core is flux, including potassium fluoroaluminate and cesium fluoroaluminate. The welding skin is an aluminum-silicon alloy. Through the combination of the spiral multi-layer structure and the flux, the welding is improved. Temperature uniformity and solder wettability and fluidity.

Benefits of technology

It can effectively reduce the welding temperature, improve the welding quality, reduce defects such as outflow welding, melting hanging welding and faulty missing welding, and improve the penetration quality of aluminum brazing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808992A_ABST
    Figure CN118808992A_ABST
Patent Text Reader

Abstract

The invention discloses a spiral aluminum flux-cored cesium welding ring which comprises a welding wire, the welding wire is of a spiral structure formed by annularly and vertically surrounding, the welding wire comprises a welding core, the outer side of the welding core is coated with a welding skin, the spiral aluminum flux-cored cesium welding ring is suitable for the technical field of aluminum alloy brazing, the welding skin is aluminum-silicon welding flux, flux is embedded in the flux-cored welding ring, and in the welding heating process, the welding skin is made of aluminum-silicon welding flux; according to the welding ring, the welding skin aluminum-silicon welding flux on the surface of the welding ring and the soldering flux embedded in the core part are heated and combined at the same time, the heating speed of the welding flux and the soldering flux is rapidly increased, and the welding flux can effectively reach the working temperature earlier than before when the soldering flux is melted; and a new element cesium is added into the soldering flux, so that the brazing filler metal can be melted, wettability and flowability can be developed at the same time, and the welding permeation quality of aluminum brazing is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of aluminum alloy brazing, in particular to a spiral aluminum flux-cored cesium brazing ring. Background Art

[0002] The welding melting point of aluminum alloy brazing base material (about 652℃) is lower than the melting point of pure aluminum (660℃). The effective melting point temperature of aluminum silicon composite material welding wire is 578-588℃. When the welding method uses flame brazing heating, due to the high flame core temperature, it is easy to heat the base material to produce defects such as "overburning perforation", "surface depression", "pitting", and poor penetration effect. Quality problems. Based on the current situation of the industry, it is urgent to develop a new type of aluminum alloy welding material "flux core welding ring" to reduce the welding temperature and improve the welding quality of the product. Summary of the invention

[0003] The purpose of the present invention is to overcome the defects of the prior art and provide a spiral aluminum flux-cored cesium welding ring.

[0004] To achieve the above object, the present invention adopts the following technical solutions:

[0005] A spiral aluminum flux-cored cesium welding ring comprises a welding wire. The welding wire adopts a spiral structure formed by vertically winding annularly. The welding wire comprises a welding core, and the outer side of the welding core is covered with a welding skin.

[0006] Preferably, the solder core is a soldering flux, which comprises the following components by mass fraction:

[0007] 18-22 parts of potassium fluoroaluminate;

[0008] 1 to 3 parts of cesium fluoroaluminate.

[0009] Preferably, the welding skin is an aluminum-silicon alloy, wherein the mass content of silicon is 11-13%, the mass content of other elements is 1%, and the mass content of aluminum is 86-88%.

[0010] Preferably, the other metals are one or more of zinc, tin, manganese, iron, magnesium, phosphorus, chromium, boron, carbon, and rare earth elements.

[0011] Preferably, the welding skin adopts a spiral multi-layer structure, the welding core is arranged at the center of the welding skin, and is rolled to form a welding wire.

[0012] Preferably, the cross-section of the welding wire is square, and the welding wire is vertically wound inwardly in a ring along one side thereof to form a spiral structure in which adjacent rings are squeezed and fitted with each other.

[0013] Preferably, the welding wire is wound around 3 times.

[0014] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are:

[0015] In the present invention, the solder coating is aluminum silicon solder, and a flux-cored solder ring with flux embedded therein is provided. During the welding heating process, the aluminum silicon solder on the surface of the solder ring and the flux embedded in the core are heated up at the same time, which rapidly increases the heating speed of the solder and the flux. When the flux is melted, the solder can effectively reach the working temperature earlier than before. Moreover, a new element "cesium" is added to the flux, which can melt the solder and develop wettability and fluidity at the same time, thereby improving the welding penetration quality of aluminum brazing. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a schematic diagram of the overall structure of a spiral aluminum flux-cored cesium welding ring of the present invention;

[0017] Figure 2 It is a top view of a spiral aluminum cored cesium welding ring of the present invention;

[0018] Figure 3 The invention discloses a welding wire cross-section of a spiral aluminum flux cored cesium welding ring. Figure 1 ;

[0019] Figure 4 The invention discloses a welding wire cross-section of a spiral aluminum flux cored cesium welding ring. Figure 2 ;

[0020] Figure 5 The invention discloses a welding wire cross-section of a spiral aluminum flux cored cesium welding ring. Figure 3 ;

[0021] Figure 6 The invention discloses a welding wire cross-section of a spiral aluminum flux cored cesium welding ring. Figure 4 .

[0022] Figure numerals: 1, welding wire; 2, welding core; 3, welding skin. DETAILED DESCRIPTION

[0023] The specific embodiments of the present invention are described in detail below.

[0024] The "range" disclosed in the present invention is defined in the form of a lower limit and an upper limit, and a given range is defined by selecting a lower limit and an upper limit, and the selected lower limit and upper limit define the boundaries of the particular range. The range defined in this way can be inclusive or exclusive of the end values, and can be arbitrarily combined, that is, any lower limit can be combined with any upper limit to form a range. For example, if a range of 10 to 50 is listed for a specific parameter, it is understood that the range of 10 to 40 and 20 to 50 is also expected. In addition, if the minimum range values ​​1 and 2 are listed, and if the maximum range values ​​3, 4 and 5 are listed, the following ranges can all be expected: 1 to 3, 1 to 4, 1 to 5, 2 to 3, 2 to 4 and 2 to 5. In this application, unless otherwise specified, the range of values ​​"a to b" represents an abbreviation of any real number combination between a and b, where a and b are both real numbers. For example, the range of values ​​"0 to 5" means that all real numbers between "0 to 5" have been fully listed in this article, and "0 to 5" is only an abbreviation of these numerical combinations.

[0025] Unless otherwise specified, all embodiments and optional embodiments of the present application can be combined with each other to form a new technical solution.

[0026] Unless otherwise specified, all technical features and optional technical features of this application can be combined with each other to form a new technical solution.

[0027] If there is no special explanation, all steps of the present application can be performed sequentially or randomly, preferably sequentially. For example, the method includes steps (a) and (b), which means that the method may include steps (a) and (b) performed sequentially, or may include steps (b) and (a) performed sequentially. For example, the method may further include step (c), which means that step (c) may be added to the method in any order. For example, the method may include steps (a), (b) and (c), or may include steps (a), (c) and (b), or may include steps (c), (a) and (b), etc.

[0028] If there is no special explanation, the "include" and "comprising" mentioned in this application are open-ended or closed-ended. For example, the "include" and "comprising" may mean that other components not listed may also be included or only the listed components may be included or only the listed components may be included.

[0029] Unless otherwise specified, the reaction is carried out at room temperature and pressure.

[0030] Unless otherwise specified, all parts or percentages are by weight.

[0031] In the present invention, all substances used are known substances and can be purchased or synthesized by known methods.

[0032] In the present invention, the devices or equipment used are all conventional devices or equipment known in the art and are commercially available.

[0033] The following is a further description of the specific implementation of the spiral aluminum flux cored cesium welding ring of the present invention in conjunction with the embodiments. The spiral aluminum flux cored cesium welding ring of the present invention is not limited to the description of the following embodiments.

[0034] Embodiment 1:

[0035] A spiral aluminum flux cored cesium welding ring, such as Figure 1-2 As shown, it includes a welding wire 1, which adopts a spiral structure formed by a ring-shaped vertical winding, and includes a welding core 2, and the outer side of the welding core 2 is covered with a welding skin 3.

[0036] Furthermore, the welding cover 3 adopts a spiral multi-layer structure, the welding core 2 is arranged at the center of the welding cover 3, and is rolled to form the welding wire 1.

[0037] Further, such as Figure 3 As shown, the cross section of the welding wire 1 is square, and the welding wire 1 is vertically wound inward along one side thereof to form a spiral structure in which adjacent rings are squeezed and matched with each other. The square structure can make the adjacent rings fit more tightly and increase the use effect of the welding ring.

[0038] Furthermore, the number of turns of the welding wire 1 is 3.

[0039] Embodiment 2:

[0040] A spiral aluminum flux cored cesium welding ring, the other structures of which are similar to those of Example 1, further, as Figure 4 As shown, the welding skin 3 adopts a single-layer structure, the welding core 2 is arranged at the center of the welding skin 3, and is rolled to form a welding wire 1. Compared with the traditional solid welding ring, the welding skin is thin, the heat absorption area is expanded, the heating is uniform, and the heating welding temperature is reached quickly, which effectively reduces the welding temperature.

[0041] Furthermore, the cross section of the welding wire 1 is circular, and the welding wire 1 is vertically wound inwardly along one side thereof, forming a spiral structure in which adjacent rings are squeezed and matched with each other.

[0042] Embodiment 3:

[0043] A spiral aluminum flux cored cesium welding ring, the other structures of which are similar to those of Example 1, further, as Figure 5 As shown, the welding cover 3 adopts a spiral multi-layer structure, the welding core 2 is arranged at the center of the welding cover 3, and is rolled to form the welding wire 1.

[0044] Furthermore, the cross section of the welding wire 1 is spiral, and the welding wire 1 is vertically wound inwardly along one side thereof, forming a spiral structure in which adjacent rings are squeezed and matched with each other.

[0045] Embodiment 4:

[0046] A spiral aluminum flux cored cesium welding ring, the other structures of which are similar to those of Example 1, further, as Figure 6 As shown, the welding core 2 is evenly laid on the outer surface of the welding skin 3, and the welding skin 32 is evenly spirally curled and extended inward along the cross-sectional direction to form the welding wire 1.

[0047] Furthermore, the cross section of the welding wire 1 is spiral, and the welding wire 1 is vertically wound inwardly along one side thereof, forming a spiral structure in which adjacent rings are squeezed and matched with each other.

[0048] By adopting the above technical solution:

[0049] While the aluminum silicon brazing candle material is being transformed from a flat plate to a coil, the flux powder is embedded and filled, and then rolled into a welding wire. The welding wire is wound one or more times as needed and then sheared to form a "flux cored welding ring". The multi-turn spiral aluminum flux cored cesium welding ring structure effectively solves the problem of outflow welding caused by the original welding ring melting too quickly and the solder flowing and filling the weld slowly. Since the multi-turn welding ring is stacked high, the lower ring welding ring melts and penetrates the flow filling weld slowly. It effectively reduces the occurrence of welding defects such as "outflow welding", "melting hanging welding", and "fault welding".

[0050] Embodiment 5:

[0051] A spiral aluminum flux-cored cesium welding ring, the other structures of which are similar to those of Example 1, further, the welding core 2 is a flux, which comprises the following components by mass fraction:

[0052] 18 parts of potassium fluoroaluminate;

[0053] 1 part cesium fluoroaluminate.

[0054] Furthermore, the welding skin 3 is an aluminum-silicon alloy, in which the mass content of silicon is 11%, the mass content of other elements is 1%, and the mass content of aluminum is 88%.

[0055] Furthermore, the other metal is one of zinc, tin, manganese, iron, magnesium, phosphorus, chromium, boron, carbon, and rare earth elements.

[0056] Embodiment 6:

[0057] A spiral aluminum flux-cored cesium welding ring, the other structures of which are similar to those of Example 5, further, the welding core 2 is a flux, which comprises the following components by mass fraction:

[0058] 20 parts of potassium fluoroaluminate;

[0059] 2 parts cesium fluoroaluminate.

[0060] Furthermore, the welding skin 3 is an aluminum-silicon alloy, wherein the mass content of silicon is 12%, the mass content of other elements is 1%, and the mass content of aluminum is 87%.

[0061] Furthermore, other metals are zinc, tin, manganese, iron, magnesium, phosphorus, chromium, boron, carbon, and rare earth elements.

[0062] Embodiment 7:

[0063] A spiral aluminum flux-cored cesium welding ring, the other structures of which are similar to those of Example 5, further, the welding core 2 is a flux, which comprises the following components by mass fraction:

[0064] 22 parts of potassium fluoroaluminate;

[0065] 3 parts cesium fluoroaluminate.

[0066] Furthermore, the welding skin 3 is an aluminum-silicon alloy, in which the mass content of silicon is 13%, the mass content of other elements is 1%, and the mass content of aluminum is 86%.

[0067] Furthermore, other metals are zinc, tin, manganese, iron, magnesium, phosphorus and chromium.

[0068] By adopting the above technical solution:

[0069] Flux FLUX adds a rare element "cesium", which helps solve the problem of poor penetration of magnesium and aluminum. Cesium fluoroaluminate is beneficial to the solder to develop advantages such as wettability and fluidity, and improve welding quality.

[0070] A flux-cored solder ring with an outer layer of aluminum-silicon solder and an inner layer of flux FLUX. The purpose is to heat up the outer layer of aluminum-silicon solder on the surface of the solder ring and the inner layer of flux FLUX embedded in the core at the same time during the welding heating process, so as to quickly increase the heating rate of the solder and flux FLUX, and make the solder reach the working temperature earlier than before when the flux FLUX melts. A new element "cesium" is added to the inner layer of the flux FLUX, which can melt the solder and develop wettability and fluidity at the same time, thereby improving the welding penetration quality of aluminum brazing.

[0071] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.

Claims

1. A spiral aluminum flux cored cesium welding ring, characterized in that: The invention comprises a welding wire (1), wherein the welding wire (1) adopts a spiral structure formed by vertically winding annularly, and comprises a welding core (2), and the outer side of the welding core (2) is covered with a welding skin (3).

2. A spiral aluminum flux cored cesium welding ring as claimed in claim 1, characterized in that: The welding core (2) is a soldering flux, which comprises the following components by mass fraction: 18-22 parts of potassium fluoroaluminate; 1 to 3 parts of cesium fluoroaluminate.

3. A spiral aluminum flux cored cesium welding ring as claimed in claim 1, characterized in that: The welding skin (3) is an aluminum-silicon alloy, wherein the mass content of silicon is 11-13%, the mass content of other elements is 1%, and the mass content of aluminum is 86-88%.

4. A spiral aluminum flux cored cesium welding ring as claimed in claim 3, characterized in that: The other metals are one or more of zinc, tin, manganese, iron, magnesium, phosphorus, chromium, boron, carbon, and rare earth elements.

5. A spiral aluminum flux cored cesium welding ring as claimed in claim 1, characterized in that: The welding skin (3) adopts a spiral multi-layer structure, and the welding core (2) is arranged at the center of the welding skin (3) and is rolled to form a welding wire (1).

6. A spiral aluminum flux cored cesium welding ring as claimed in claim 1, characterized in that: The welding wire (1) has a square cross-section, and the welding wire (1) is vertically wound inwardly along one side thereof, forming a spiral structure in which adjacent rings are squeezed and fitted with each other.

7. A spiral aluminum flux cored cesium welding ring as claimed in claim 1, characterized in that: The welding wire (1) is wound around 3 times.

Citation Information

Cited By

  • Coating type preformed brazing filler metal and preparation method and application thereof

    CN119635074A