A tertiary amine waste gas treatment process containing a membrane separation unit
Through the multi-link treatment of composite fiber membranes and metal-mesoporous material catalysts in the treatment of tertiary amine exhaust gas, the problem of insufficient treatment in the prior art is solved, and efficient waste gas treatment and emission standards are achieved.
Patent Information
- Application Number
- CN202411310561.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-20
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-09-20
AI Technical Summary
The prior art mostly uses a single technology when treating tertiary amine exhaust gas, resulting in insufficient treatment of waste gas, residual substances entering the environment, causing harm to the human body and the environment.
The composite fiber membrane is used as the membrane separation unit for pre-stage treatment, and a multi-step treatment is carried out in combination with the pickling system and the metal-mesoporous material catalyst, including pre-stage treatment, acid absorption treatment and post-stage catalytic treatment.
Through multi-link treatment, efficient tertiary amine waste gas treatment is achieved, meeting emission standards, and reducing harm to the environment and the human body.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention belongs to the field of waste gas treatment, and in particular relates to a tertiary amine waste gas treatment process containing a membrane separation unit. Background Art
[0002] The production of amines is mostly based on fatty alcohols or fatty acids. The tail gas emitted during the production process mainly includes dimethylamine, trimethylamine and low-carbon chain amines, ammonia, hydrogen, etc. These organic ammonia and amines have low olfactory threshold values and are a typical type of odor pollutants. Organic amines also inhibit the synthesis of macromolecular substances in organisms and have teratogenic effects on animal embryos. Therefore, the odor pollutants emitted during the production of fatty amines have become the research focus of air pollution control. Common treatment methods for ammonia and amine waste gas include water absorption, acid absorption, adsorption, biological method, incineration, catalytic oxidation, and plasma technology. However, most of the existing technologies for tertiary amine waste gas treatment only use a single technology, which is not sufficient for waste gas treatment. Residual substances will enter the environment, causing harm to humans and the environment.
[0003] Therefore, how to improve the existing technology and use a number of improved waste gas treatment technologies in combination to treat tertiary amine waste gas through multi-link coordination to achieve efficient tertiary amine waste gas treatment and meet emission standards has become a direction that needs to be tackled. Summary of the invention
[0004] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a tertiary amine waste gas treatment process containing a membrane separation unit, aiming to solve the problem that most of the existing processes for treating tertiary amine waste gas only use a single technology, the waste gas treatment is not sufficient, and residual substances will enter the environment, causing harm to human body and the environment.
[0005] The present invention uses a composite fiber membrane as a membrane separation unit for tertiary amine waste gas in the pre-stage treatment system, realizes the pre-stage treatment of the waste gas through the composite structure of the fiber membrane, the pickling system uses a sulfuric acid solution in combination with modified sepiolite, and the post-stage treatment system uses a metal-mesoporous material catalyst for catalytic treatment. The waste gas is treated through multi-link coordination to achieve efficient tertiary amine waste gas treatment and meet emission standards.
[0006] The technical solution of the present invention is as follows:
[0007] The present invention provides a tertiary amine waste gas treatment process containing a membrane separation unit, characterized in that it comprises the following steps:
[0008] Step S1: introducing the tertiary amine waste gas into a pre-stage treatment system, and performing pre-stage treatment of the tertiary amine waste gas using a membrane separation unit in the pre-stage treatment system;
[0009] Step S2: passing the tertiary amine waste gas after the previous stage treatment into the acid washing system, and performing acid absorption treatment of the tertiary amine waste gas through the acid washing system;
[0010] Step S3: passing the tertiary amine waste gas after the acid absorption treatment into a post-stage treatment system, and performing post-stage catalytic treatment through a catalyst in the post-stage treatment system;
[0011] The membrane separation unit in step S1 is a composite fiber membrane;
[0012] The pickling system in step S2 is a pickling tower, which contains acid solution and filler. The acid solution in the pickling tower is a sulfuric acid solution with a mass fraction of 30-40%, and the filler in the pickling tower is modified sepiolite.
[0013] The following are preferred technical solutions of the present invention, but are not intended to limit the technical solutions provided by the present invention. Through the following preferred technical solutions, the objectives and beneficial effects of the present invention can be better achieved and realized.
[0014] As a preferred technical solution of the present invention, the preparation method of the composite fiber membrane is: using the shell layer solution as the shell layer spinning solution and the core layer solution as the core layer spinning solution, obtaining core-shell structure fibers by coaxial electrospinning, and drying at 50°C for 6 hours to obtain a composite fiber membrane.
[0015] As a preferred technical solution of the present invention, the shell solution is prepared by adding 50 parts of sodium alginate to 1000 parts of deionized water, stirring evenly, adding 5 parts of sodium hydroxide and stirring for 0.5 hours, then adding 120 parts of hydrogen peroxide and stirring at room temperature for 1 hour to obtain a shell solution.
[0016] As a preferred technical solution of the present invention, the method for preparing the core layer solution is: adding 10 parts of polyvinyl pyrrolidone, 5 parts of ferric fluoride oxide, and 2 parts of mupirocin calcium to 100 parts of dichloromethane, and magnetically stirring at room temperature for 12 hours to obtain the core layer solution.
[0017] As a preferred technical solution of the present invention, 5 parts of iron powder are added to 350 parts of silicic acid, stirred at 50°C for 24 hours, and dried to obtain crystals; 6 parts of the crystals are added to 300 parts of n-propanol, mixed evenly to obtain a precursor solution; the precursor solution is transferred to a reactor, reacted at 200°C for 24 hours, and after the reaction is completed, solid-liquid separation is performed, and the obtained solid is vacuum dried at 100°C for 12 hours to obtain iron fluoride oxide.
[0018] Preferably, the conditions for the coaxial electrospinning are: the syringe propulsion speed of the shell layer spinning solution is 0.5-1.0 mL / h, the syringe propulsion speed of the core layer spinning solution is 0.1-0.3 mL / h, the needle voltage is 18-25 kV, the receiving distance is 15-18 cm, the temperature is 30-40°C, the humidity is 35-45%, and the spinning time is 2-4 h.
[0019] The membrane separation unit of the present invention adopts a composite fiber membrane, wherein the shell layer of the composite fiber membrane is a sodium alginate fiber loaded with hydrogen peroxide. When the waste gas contacts the membrane separation unit, it first contacts the shell material. Hydrogen peroxide, as a strong oxidant, can promote the rupture of macromolecular segments in the tertiary amine waste gas to form low-carbon chain fatty amines. Low-carbon chain fatty amines, dimethylamine, etc. will form an emulsion with water decomposed from hydrogen peroxide, thereby achieving the treatment of tertiary amine waste gas. The core layer of the composite fiber membrane is a polyvinyl pyrrolidone fiber coated with fluorinated iron. After the hydrogen peroxide loaded on the shell absorbs the tertiary amine waste gas, an oxidation reaction occurs to generate water. The polyvinyl pyrrolidone can be dissolved in water, thereby allowing the fluorinated iron to contact the hydrogen peroxide in the shell. The strong electron-withdrawing ability of the coordinated F atoms of the fluorinated iron can greatly reduce the local electron density of the Fe site, significantly improve the activation speed of hydrogen peroxide, promote the rapid decomposition of hydrogen peroxide to produce more hydroxyl radicals, and have a good chain-breaking effect on macromolecular organic matter in the tertiary amine waste gas. In addition, since mupirocin calcium soluble in dichloromethane is added to the core layer, the calcium salt is provided through the core layer, so that the sodium alginate of the shell layer can quickly gel and wrap hydrogen peroxide in the calcium salt environment, thereby ensuring the retention of hydrogen peroxide and exerting its effect.
[0020] As a preferred technical solution of the present invention, the preparation method of the modified sepiolite is: add 100 parts of sepiolite to 200 parts of deionized water, ultrasonically treat for 0.5h at 25°C, add 20 parts of hexadecyltrimethylammonium bromide, magnetically stir for 6h, let stand to precipitate and filter, vacuum dry the filter residue at 70°C for 4h, and grind to obtain the modified sepiolite.
[0021] Hexadecyltrimethylammonium bromide is introduced into the modified sepiolite. The hexadecyltrimethylammonium bromide enters the internal pores of the sepiolite. The presence of oxygen atoms at the corners of the tetrahedral sheets in the sepiolite structure causes the lattice to expand slightly during modification by the hexadecyltrimethylammonium bromide, thereby increasing the pore volume. In addition, the hexadecyltrimethylammonium bromide enters the interlayer spacing of the sepiolite, causing an increase in the interlayer spacing, increasing the pore volume and specific surface area of the sepiolite, and improving the adsorption performance of the sepiolite. The sepiolite is capable of adsorbing sulfate formed after the acid absorption, thereby avoiding being brought into the next stage of the waste gas treatment process.
[0022] As a preferred technical solution of the present invention, the catalyst in step S3 is a metal-mesoporous material catalyst. The preparation method of the metal-mesoporous material catalyst is as follows: 15 parts of copper nitrate, 15 parts of cerium nitrate and 15 parts of manganese nitrate are added to 200 parts of deionized water, stirred for 1 hour, and an impregnation solution is obtained; 100 parts of mesoporous material are added to 200 parts of the impregnation solution, impregnated for 48 hours, and after the impregnation is completed, the mesoporous material is taken out, and then dried at 80°C for 24 hours, and finally calcined at 500°C for 5 hours to obtain a metal-mesoporous material catalyst.
[0023] Preferably, the preparation method of the mesoporous material is: mix 120 parts of anhydrous ethanol and 30 parts of deionized water to obtain a mixed solution, weigh 2 parts of ferrosoferric oxide and add it to the mixed solution to obtain a suspension, ultrasonically disperse for 1 hour, drop 20 parts of tetraethyl silicate and 30 parts of ammonia water into the suspension, stir and react at room temperature for 8 hours, filter after the reaction is completed, and wash the filter residue with anhydrous ethanol and deionized water to obtain composite particles, and dry the composite particles in a vacuum oven at 50°C for 12 hours to obtain the mesoporous material.
[0024] The metal-mesoporous material catalyst uses mesoporous material as a carrier and has a porous structure. It has a high specific surface area, a large specific pore volume, and a relatively narrow pore size distribution. The porous structure of the mesoporous material can improve the adsorption efficiency; the loaded oxides such as copper, cerium, and manganese further increase the specific surface area of the mesoporous material and can form high-temperature hotspots on the catalyst surface, thereby enhancing the overall reaction activity of the catalyst, which is beneficial to the catalytic oxidation of remaining low-molecular fatty amines, fatty nitriles, etc. in the exhaust gas, ensuring that the pollutant emission standards are met.
[0025] Compared with the prior art, the present invention has the following beneficial effects:
[0026] (1) The present invention introduces a membrane separation unit into the tertiary amine waste gas treatment process, and adopts a composite fiber membrane as the membrane separation unit. The hydrogen peroxide supplied by the shell layer in the composite fiber membrane can promote the breakage of the macromolecular chain segments in the tertiary amine waste gas, and the water decomposed by the hydrogen peroxide forms an emulsion with low molecular weight ammonia and dimethylamine; after the polyvinyl pyrrolidone of the core layer is dissolved in water, the coated fluorine oxide can serve as a catalyst for hydrogen peroxide, further accelerating the oxidation reaction of hydrogen peroxide; through the coordinated cooperation of the shell layer and the core layer, the comprehensive treatment of the tertiary amine waste gas is achieved.
[0027] (2) The tertiary amine waste gas treatment process of the present invention includes a pre-stage treatment system, a pickling system and a post-stage treatment system, and technical improvements are made in each system. The pre-stage treatment system uses a composite fiber membrane as a membrane separation unit for tertiary amine waste gas, and the pre-stage treatment of waste gas is achieved through the composite structure of the fiber membrane. The pickling system uses a sulfuric acid solution in combination with modified sepiolite, and the post-stage treatment system uses a metal-mesoporous material catalyst for catalytic treatment. The waste gas is treated by multi-link coordination to achieve efficient tertiary amine waste gas treatment and meet emission standards. DETAILED DESCRIPTION
[0028] For the convenience of understanding the present invention, the present invention lists the following embodiments. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.
[0029] The sources of some components in the embodiments and comparative examples are as follows:
[0030] Pre-treatment system: sodium alginate CAS No. 9005-38-3; sodium hydroxide CAS No. 1310-73-2; hydrogen peroxide CAS No. 7722-84-1; polyvinyl pyrrolidone, purchased from Shanghai MacLean Biochemical Technology Co., Ltd.; dichloromethane CAS No. 75-09-2; mupirocin calcium CAS No. 115074-43-6.
[0031] Pickling system: Sepiolite CAS No. 63800-37-3; Cetyltrimethylammonium bromide CAS No. 57-09-0; Sulfuric acid CAS No. 7664-93-9; Activated alumina CAS No. 1344-28-1.
[0032] Post-treatment system: anhydrous ethanol CAS No. 64-17-5; ferrosoferric oxide CAS No. 12227-89-3; tetraethyl silicate CAS No. 78-10-4; ammonia CAS No. 1336-21-6; anhydrous ethanol CAS No. 64-17-5; copper nitrate CAS No. 10031-43-3; cerium nitrate CAS No. 13093-17-9; manganese nitrate CAS No. 10377-66-9; platinum-palladium metal honeycomb catalyst, purchased from Hunan Xintan New Materials Co., Ltd.
[0033] Preparation of iron fluoride oxide: add 5 parts of iron powder to 350 parts of silicic acid, stir at 50°C for 24 hours, and obtain crystals after drying; add 6 parts of crystals to 300 parts of n-propanol, mix evenly to obtain a precursor solution; transfer the precursor solution to a reactor, react at 200°C for 24 hours, perform solid-liquid separation after the reaction is completed, and vacuum dry the obtained solid at 100°C for 12 hours to obtain iron fluoride oxide.
[0034] Preparation of coaxial electrospinning solution: add 50 parts of sodium alginate to 1000 parts of deionized water, stir evenly, add 5 parts of sodium hydroxide and stir for 0.5h, then add 120 parts of hydrogen peroxide and stir at room temperature for 1h to obtain a shell solution; add 10 parts of polyvinyl pyrrolidone, 5 parts of ferric fluoride oxide, and 2 parts of mupirocin calcium to 100 parts of dichloromethane, stir magnetically at room temperature for 12h to obtain a core solution.
[0035] Preparation of modified sepiolite: 100 parts of sepiolite are added to 200 parts of deionized water, ultrasonically treated at 25°C for 0.5 h, 20 parts of hexadecyltrimethylammonium bromide are added, magnetically stirred for 6 h, allowed to stand for precipitation and filtered, the filter residue is vacuum dried at 70°C for 4 h, and the modified sepiolite is obtained after grinding.
[0036] Preparation of mesoporous material: Mix 120 parts of anhydrous ethanol and 30 parts of deionized water to obtain a mixed solution, weigh 2 parts of ferrosoferric oxide and add it to the mixed solution to obtain a suspension, ultrasonically disperse for 1 hour, drop 20 parts of tetraethyl silicate and 30 parts of ammonia water into the suspension, stir and react at room temperature for 8 hours, filter after the reaction is completed, and wash the filter residue with anhydrous ethanol and deionized water to obtain composite particles, and dry the composite particles in a vacuum oven at 50°C for 12 hours to obtain a mesoporous material.
[0037] Preparation of metal-mesoporous material catalyst: add 15 parts of copper nitrate, 15 parts of cerium nitrate and 15 parts of manganese nitrate into 200 parts of deionized water, stir for 1 hour, and obtain an impregnation solution; add 100 parts of mesoporous material into 200 parts of the impregnation solution, impregnate for 48 hours, take out the mesoporous material after the impregnation is completed, and then dry it at 80°C for 24 hours, and finally calcine it at 500°C for 5 hours to obtain a metal-mesoporous material catalyst.
[0038] Example 1 This example provides a tertiary amine waste gas treatment process containing a membrane separation unit, comprising the following steps:
[0039] Step S1: passing the tertiary amine waste gas into a pre-stage treatment system, and using a composite fiber membrane as a membrane separation unit in the pre-stage treatment system to perform pre-stage treatment of the tertiary amine waste gas; the preparation method of the composite fiber membrane is to use the shell layer solution as the shell layer spinning solution, and the core layer solution as the core layer spinning solution, and control the syringe propulsion speed of the shell layer spinning solution to be 1.0mL / h, the syringe propulsion speed of the core layer spinning solution to be 0.3mL / h, the needle voltage to be 25kV, the receiving distance to be 18cm, the temperature to be 40°C, the humidity to be 35%, the spinning time to be 2h, and obtain the core-shell structure fiber by coaxial electrospinning, and dry it at 50°C for 6h to obtain the composite fiber membrane;
[0040] Step S2: passing the tertiary amine waste gas after the previous stage treatment into the pickling system, and performing acid absorption treatment on the tertiary amine waste gas through the pickling system; the pickling system is a pickling tower, and the pickling tower contains acid solution and filler, the acid solution of the pickling tower is a sulfuric acid solution with a mass fraction of 40%, and the filler of the pickling tower is modified sepiolite;
[0041] Step S3: passing the tertiary amine waste gas after the acid absorption treatment into a post-stage treatment system, and performing post-stage catalytic treatment through the metal-mesoporous material catalyst in the post-stage treatment system.
[0042] Example 2 This example provides a tertiary amine waste gas treatment process containing a membrane separation unit, comprising the following steps:
[0043] Step S1: passing the tertiary amine waste gas into a pre-stage treatment system, and using a composite fiber membrane as a membrane separation unit in the pre-stage treatment system to perform pre-stage treatment of the tertiary amine waste gas; the preparation method of the composite fiber membrane is to use the shell layer solution as the shell layer spinning solution, and the core layer solution as the core layer spinning solution, and control the syringe propulsion speed of the shell layer spinning solution to be 0.5mL / h, the syringe propulsion speed of the core layer spinning solution to be 0.1mL / h, the needle voltage is 18kV, the receiving distance is 15cm, the temperature is 30℃, the humidity is 45%, the spinning time is 4h, and the core-shell structure fiber is obtained by coaxial electrospinning, and dried at 50℃ for 6h to obtain a composite fiber membrane;
[0044] Step S2: passing the tertiary amine waste gas after the previous stage treatment into the pickling system, and performing acid absorption treatment on the tertiary amine waste gas through the pickling system; the pickling system is a pickling tower, and the pickling tower contains acid solution and filler, the acid solution of the pickling tower is a sulfuric acid solution with a mass fraction of 30%, and the filler of the pickling tower is modified sepiolite;
[0045] Step S3: passing the tertiary amine waste gas after the acid absorption treatment into a post-stage treatment system, and performing post-stage catalytic treatment through the metal-mesoporous material catalyst in the post-stage treatment system.
[0046] Example 3 This example provides a tertiary amine waste gas treatment process containing a membrane separation unit, comprising the following steps:
[0047] Step S1: passing the tertiary amine waste gas into a pre-stage treatment system, and using a composite fiber membrane as a membrane separation unit in the pre-stage treatment system to perform pre-stage treatment of the tertiary amine waste gas; the preparation method of the composite fiber membrane is to use the shell layer solution as the shell layer spinning solution, and the core layer solution as the core layer spinning solution, and control the syringe propulsion speed of the shell layer spinning solution to be 0.8mL / h, the syringe propulsion speed of the core layer spinning solution to be 0.2mL / h, the needle voltage is 20kV, the receiving distance is 16cm, the temperature is 34°C, the humidity is 42%, the spinning time is 3h, and the core-shell structure fiber is obtained by coaxial electrospinning, and dried at 50°C for 6h to obtain a composite fiber membrane;
[0048] Step S2: passing the tertiary amine waste gas after the previous stage treatment into the pickling system, and performing acid absorption treatment on the tertiary amine waste gas through the pickling system; the pickling system is a pickling tower, and the pickling tower contains acid solution and filler, the acid solution of the pickling tower is a sulfuric acid solution with a mass fraction of 35%, and the filler of the pickling tower is modified sepiolite;
[0049] Step S3: passing the tertiary amine waste gas after the acid absorption treatment into a post-stage treatment system, and performing post-stage catalytic treatment through the metal-mesoporous material catalyst in the post-stage treatment system.
[0050] Comparative Example 1
[0051] This comparative example provides a tertiary amine waste gas treatment process, comprising the following steps:
[0052] Step S1: introducing the tertiary amine waste gas into a pre-stage treatment system, and using a water scrubber in the pre-stage treatment system to perform pre-stage treatment on the tertiary amine waste gas;
[0053] Step S2: passing the tertiary amine waste gas after the previous stage treatment into the pickling system, and performing acid absorption treatment on the tertiary amine waste gas through the pickling system; the pickling system is a pickling tower, and the pickling tower contains acid solution and filler, the acid solution of the pickling tower is a sulfuric acid solution with a mass fraction of 40%, and the filler of the pickling tower is activated alumina;
[0054] Step S3: The tertiary amine waste gas after the acid absorption treatment is introduced into a post-stage treatment system, and is subjected to post-stage catalytic treatment by a platinum-palladium metal honeycomb catalyst in the post-stage treatment system.
[0055] Comparative Example 2
[0056] This comparative example provides a tertiary amine waste gas treatment process, which is different from comparative example 1 only in that this comparative example uses modified sepiolite instead of activated alumina in the pickling system, and the rest is the same as comparative example 1.
[0057] Comparative Example 3
[0058] This comparative example provides a tertiary amine waste gas treatment process, which is different from comparative example 1 only in that this comparative example uses a metal-mesoporous material catalyst instead of a platinum-palladium metal honeycomb catalyst in the post-treatment system, and the rest is the same as comparative example 1.
[0059] According to GBZ / T 160.69-2004 Determination of Aliphatic Amine Compounds in Toxic Substances in Workplace Air, the concentration of aliphatic amine compounds in the gas after the tertiary amine waste gas treatment of the above-mentioned embodiments and comparative examples was measured, and the measurement data are shown in Table 1:
[0060] Table 1
[0061]
[0062] The applicant declares that the present invention illustrates the detailed process flow of the present invention through the above-mentioned embodiments, but the present invention is not limited to the above-mentioned detailed process flow, that is, it does not mean that the present invention must rely on the above-mentioned detailed process flow to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of various raw materials of the product of the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.
Claims
1. A tertiary amine waste gas treatment process containing a membrane separation unit, characterized in that: The steps include: Step S1: introducing the tertiary amine waste gas into a pre-stage treatment system, and performing pre-stage treatment of the tertiary amine waste gas using a membrane separation unit in the pre-stage treatment system; Step S2: passing the tertiary amine waste gas after the previous stage treatment into the acid washing system, and performing acid absorption treatment of the tertiary amine waste gas through the acid washing system; Step S3: passing the tertiary amine waste gas after the acid absorption treatment into a post-stage treatment system, and performing post-stage catalytic treatment through a catalyst in the post-stage treatment system; The membrane separation unit in step S1 is a composite fiber membrane; The preparation method of the composite fiber membrane comprises: using the shell layer solution as the shell layer spinning solution and the core layer solution as the core layer spinning solution, obtaining core-shell structure fibers by coaxial electrospinning, and drying at 50° C. for 6 hours to obtain the composite fiber membrane; The shell solution is prepared by adding 50 parts of sodium alginate to 1000 parts of deionized water, stirring evenly, adding 5 parts of sodium hydroxide and stirring for 0.5 hours, then adding 120 parts of hydrogen peroxide and stirring at room temperature for 1 hour to obtain a shell solution; The core layer solution is prepared by adding 10 parts of polyvinyl pyrrolidone, 5 parts of ferric fluoride oxide, and 2 parts of mupirocin calcium into 100 parts of dichloromethane, and magnetically stirring at room temperature for 12 hours to obtain a core layer solution; The pickling system in step S2 is a pickling tower, which contains acid solution and filler. The acid solution in the pickling tower is a sulfuric acid solution with a mass fraction of 30-40%, and the filler in the pickling tower is modified sepiolite.
2. A tertiary amine waste gas treatment process containing a membrane separation unit according to claim 1, characterized in that: The preparation method of the fluorine oxide is as follows: 5 parts of iron powder are added to 350 parts of silicic acid, stirred at 50° C. for 24 hours, and dried to obtain crystals; 6 parts of the crystals are added to 300 parts of n-propanol, and mixed evenly to obtain a precursor solution; The precursor solution was transferred to a reactor and reacted at 200°C for 24 hours. After the reaction was completed, solid-liquid separation was performed and the obtained solid was vacuum dried at 100°C for 12 hours to obtain iron fluoride oxide.
3. A tertiary amine waste gas treatment process containing a membrane separation unit according to claim 1, characterized in that: The conditions for the coaxial electrospinning are: the syringe propulsion speed of the shell layer spinning solution is 0.5-1.0 mL / h, the syringe propulsion speed of the core layer spinning solution is 0.1-0.3 mL / h, the needle voltage is 18-25 kV, the receiving distance is 15-18 cm, the temperature is 30-40° C., the humidity is 35-45%, and the spinning time is 2-4 hours.
4. A tertiary amine waste gas treatment process containing a membrane separation unit according to claim 1, characterized in that: The preparation method of the modified sepiolite is as follows: 100 parts of sepiolite are added to 200 parts of deionized water, ultrasonically treated at 25° C. for 0.5 h, 20 parts of hexadecyltrimethylammonium bromide are added, magnetic stirring is performed for 6 h, the mixture is allowed to stand for precipitation and filtered, the filter residue is vacuum dried at 70° C. for 4 h, and ground to obtain the modified sepiolite.
5. The tertiary amine waste gas treatment process containing a membrane separation unit according to claim 1, characterized in that: The catalyst in step S3 is a metal-mesoporous material catalyst.
6. A tertiary amine waste gas treatment process containing a membrane separation unit according to claim 5, characterized in that: The preparation method of the metal-mesoporous material catalyst is as follows: 15 parts of copper nitrate, 15 parts of cerium nitrate and 15 parts of manganese nitrate are added to 200 parts of deionized water, and stirred for 1 hour to obtain an impregnation solution; 100 parts of mesoporous material were added into 200 parts of impregnation solution and impregnated for 48 hours. After impregnation, the mesoporous material was taken out and then dried at 80°C for 24 hours. Finally, it was calcined at 500°C for 5 hours to obtain a metal-mesoporous material catalyst.
7. A tertiary amine waste gas treatment process containing a membrane separation unit according to claim 6, characterized in that: The preparation method of the mesoporous material is as follows: 120 parts of anhydrous ethanol and 30 parts of deionized water are mixed to obtain a mixed solution, 2 parts of ferrosoferric oxide are weighed and added to the mixed solution to obtain a suspension, ultrasonically dispersed for 1 hour, 20 parts of tetraethyl silicate and 30 parts of ammonia water are dropped into the suspension, stirred at room temperature for reaction for 8 hours, filtered after the reaction is completed, and the filter residue is washed with anhydrous ethanol and deionized water to obtain composite particles, and the composite particles are dried in a vacuum oven at 50° C. for 12 hours to obtain the mesoporous material.