Device and method for decoloring phosphoric acid
Through the process of homogeneous high-efficiency mixing pump and multi-stage decolorization tower, combined with heat pump and heat exchanger, the problem of low organic matter removal rate and complicated operation in high-concentration phosphoric acid is solved, an efficient and safe phosphoric acid decolorization process is achieved, and the process is improved. Product quality and production efficiency.
Patent Information
- Application Number
- CN202410937315.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-10-29
AI Technical Summary
The existing technology has low organic matter removal rate in high-concentration industrial/food-grade phosphoric acid, high product color, and the activated carbon decolorization process produces hazardous chemical waste. The operation is complex and costly, and it is difficult to meet the quality requirements of industrial-grade or food-grade phosphoric acid. .
Using a homogeneous high-efficiency mixing pump and multi-stage decolorization tower technology, through a combination device of a heat pump, a series decolorization tower and a heat exchanger, the homogeneous mixing of hydrogen peroxide and phosphoric acid and a multi-stage packed tower are used for efficient decolorization to achieve efficient decolorization and exhaust gas washing.
It improves the phosphoric acid decolorization efficiency and product quality, reduces the operational complexity and cost, realizes an efficient and safe decolorization process, and meets the national emission standards.
Smart Images

Figure CN118846583A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of chemical engineering, and in particular to a phosphoric acid decolorization device and method. Background Art
[0002] The color of high-concentration industrial-grade / food-grade phosphoric acid is mainly affected by organic matter, which makes it impossible to meet the color requirements of product quality. Therefore, the organic matter needs to be removed and decomposed to achieve the quality requirements of industrial-grade phosphoric acid or food-grade phosphoric acid.
[0003] There are currently physical and chemical methods for removing organic matter. The physical method uses activated carbon for decolorization, which is a physical absorption method. Activated carbon is the adsorbent and the activated tower is solid. Therefore, it has the following disadvantages:
[0004] (1) Low TOC removal rate
[0005] When activated carbon is used to decolorize wet-process purified phosphoric acid, the TOC removal rate can only reach 60%;
[0006] (2) High product chromaticity
[0007] Using activated carbon for wet purification of phosphoric acid decolorization, the product color can only reach 30 dark blue;
[0008] (3) Hazardous waste disposal
[0009] The use of activated carbon to decolorize high-concentration industrial / food-grade phosphoric acid is a physical adsorption process. The waste carbon after adsorption is a hazardous chemical waste and needs to be disposed of.
[0010] (4) Activated carbon filtration
[0011] The activated carbon particles are 1 to 6 mm in size and need to be added to high-concentration industrial / food-grade phosphoric acid. The particles are stirred by a stirring paddle and heated. After staying for a certain period of time, they are filtered. The filtration is difficult and increases the manual operation load. Multiple filtrations are required to meet the product purity requirements.
[0012] Therefore, it is necessary to develop a decolorization technology that is efficient, low-cost, simple to operate, safe and applicable. Summary of the invention
[0013] Based on the technical problems existing in the background technology, the present invention proposes a phosphoric acid decolorization device, which has the advantages of simple process flow and high decolorization efficiency.
[0014] The phosphoric acid decolorization device proposed by the present invention comprises a heating pump, a plurality of decolorization towers and a heat exchanger which are arranged in sequence, a pipeline at the feed end of the heating pump is provided with a phosphoric acid regulating valve, a homogeneous and efficient mixing pump is provided between the heating pump and the decolorization tower and between adjacent decolorization towers, the homogeneous and efficient mixing pump is also connected to a hydrogen peroxide delivery pipeline, a hydrogen peroxide regulating valve is provided on the hydrogen peroxide delivery pipeline, and a packing washing tower is also connected to the gas outlet of the decolorization tower.
[0015] Preferably, the homogeneous and efficient mixing pump comprises a mixing pump, the mixing pump is provided with a mixing pump inlet pipe and a mixing pump outlet pipe, the mixing pump outlet pipe is connected to a phosphoric acid delivery pipe and a hydrogen peroxide delivery pipe, the hydrogen peroxide delivery pipe is connected to a multi-channel mixing head, and the discharge end of the multi-channel mixing head is located in the phosphoric acid delivery pipe.
[0016] Preferably, the mixing pump is composed of several layers of rotors and stators, and the gear plates of each layer of rotors and stators are from coarse to fine.
[0017] Preferably, the decolorization tower includes a tower body, a gas outlet is arranged on the top of the tower body, a first feed pipe and a second feed pipe are respectively connected to both ends of the tower body, a plurality of filling sections are arranged in the tower body, the plurality of filling sections are distributed between the first feed pipe and the second feed pipe, and the pores of each filling section increase along the material flow direction.
[0018] The decolorization method of the phosphoric acid decolorization device proposed by the present invention comprises the following steps:
[0019] S1: transporting high concentration phosphoric acid to a heater for heating;
[0020] S2: The material heated in S1 and the hydrogen peroxide are adjusted in proportion to each other by a hydrogen peroxide regulating valve and then transported to a homogeneous and efficient mixing pump for mixing;
[0021] S3: The mixed material in S2 is decolorized by passing through a plurality of decolorization towers connected in series, and a homogenizing and efficient mixing pump is arranged between adjacent decolorization towers, and the ratio of the material and hydrogen peroxide delivered to the homogenizing and efficient mixing pump is adjusted by a hydrogen peroxide regulating valve;
[0022] S4: The material after decolorization in the decolorization tower enters the heat exchanger for cooling to obtain decolorized phosphoric acid. The gas outlet of the decolorization tower is connected to the packed washing tower to wash the tail gas and discharge it after meeting the standards.
[0023] Preferably, the concentration of high-concentration phosphoric acid in S1 is 30%-64%, TOC is ≥500ppm, and blackness is ≥60 black degrees.
[0024] Preferably, the concentration of hydrogen peroxide in S2 and S3 is 5-30wt%, and the volume ratio of the material to hydrogen peroxide is 1:0.001-0.01.
[0025] Preferably, the residence time of the material in the bleaching tower is 1-5 hours, and the bleaching temperature is 90-150°C.
[0026] Preferably, the decolorizing tower is made of graphite or steel-lined PTFE or steel-lined PFA, and the filler material is PTFE or PFA.
[0027] Preferably, the material temperature after cooling by the heat exchanger in S4 is 40-60°C.
[0028] Beneficial technical effects of the present invention:
[0029] (1) The present invention adopts a homogenizing and efficient mixing pump, which is composed of a multi-tube mixing head and a mixing pump. The mixing pump is composed of 2-5 layers of rotors and stators. The gear plates of each layer of rotors and stators are from coarse to fine, so that the original groups of different components of materials can be efficiently mixed and homogenized in an instant according to the proportion requirements. After using this mixing equipment, the original traditional production process is further simplified, the production efficiency is greatly improved, and the quality of the mixed products is significantly improved.
[0030] (2) The present invention adopts a multi-stage decolorization process, and its decolorization tower is a packed tower. The decolorization tower is made of graphite or steel-lined PTFE or steel-lined PFA. The filler is an irregular filler made of PTFE or PFA. It is a static device and has no power operation. It is also made of non-metallic material, which is more suitable for the selection of phosphoric acid materials above 100°C. It increases the service life, reduces the difficulty of selecting metal materials, reduces costs, and is easier to realize automated operation, thereby realizing a more efficient decolorization technology.
[0031] (3) After the decomposition gas overflows from the decolorization tower, a packing washing tower is used. The material is 316L composite 904 or steel lined PTFE or PFA. The packing is PTFE or PFA, which is an irregular packing, so that the decomposition gas can be effectively absorbed and meet the national emission standards. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 This is a schematic diagram of the structure of the phosphoric acid decolorization device proposed by the present invention;
[0033] Figure 2 This is a schematic diagram of the structure of the homogeneous and efficient mixing pump proposed by the present invention;
[0034] Figure 3 It is a schematic diagram of the structure of the decolorization tower proposed by the present invention.
[0035] In the figure: 10-heater, 20-first homogeneous and efficient mixing pump, 201-mixing pump, 202-mixing pump inlet pipe, 203-mixing pump outlet pipe, 204-phosphoric acid delivery pipe, 205-hydrogen peroxide delivery pipe, 206-multi-pipe mixing head, 30-first bleaching tower, 301-tower body, 302-filling section, 303-first feed pipe, 304-second feed pipe, 40-third homogeneous and efficient mixing pump, 50-second bleaching tower, 60-second homogeneous and efficient mixing pump, 70-third bleaching tower, 80-heat exchanger, 90-filling washing tower, 100-phosphoric acid regulating valve, 110-first hydrogen peroxide regulating valve, 120-second hydrogen peroxide regulating valve, 130-third hydrogen peroxide regulating valve. DETAILED DESCRIPTION
[0036] The present invention will be further explained below in conjunction with specific embodiments.
[0037] Reference Figure 1 The phosphoric acid decolorization device proposed in the present invention comprises a heating pump 10, a plurality of decolorization towers and a heat exchanger 80 which are arranged in sequence. The pipeline at the feed end of the heating pump 10 is provided with a phosphoric acid regulating valve 100. A homogeneous and efficient mixing pump is provided between the heating pump 10 and the decolorization tower and between adjacent decolorization towers. The homogeneous and efficient mixing pump is also connected to a hydrogen peroxide delivery pipeline, and a hydrogen peroxide regulating valve is provided on the hydrogen peroxide delivery pipeline. The gas outlet of the decolorization tower is also connected to a packing washing tower 90.
[0038] Reference Figure 2 As a preferred solution of the present invention, the homogeneous and efficient mixing pump includes a mixing pump 201, which is provided with a mixing pump inlet pipe 202 and a mixing pump outlet pipe 203, the mixing pump outlet pipe 203 is connected to a phosphoric acid delivery pipe 204 and a hydrogen peroxide delivery pipe 205, the hydrogen peroxide delivery pipe 205 is connected to a multi-channel mixing head 206, and the discharge end of the multi-channel mixing head 206 is located in the phosphoric acid delivery pipe 204. The mixing pump 201 is composed of several layers of rotors and stators, and the gear disks of each layer of rotors and stators are from coarse to fine.
[0039] The present invention adopts a homogenizing and efficient mixing pump, which is composed of a multi-tube mixing head and a mixing pump. The mixing pump is composed of 2-5 layers of rotors and stators. The gear plates of each layer of rotors and stators are from coarse to fine, so that the original groups of different components of materials can be efficiently mixed and homogenized in an instant according to the proportion requirements. After using this mixing equipment, the original traditional production process is further simplified, the production efficiency is greatly improved, and the quality of the mixed products is significantly improved.
[0040] Reference Figure 3The decolorization tower includes a tower body 301, a gas outlet is arranged at the top of the tower body 301, a first feed pipe 303 and a second feed pipe 304 are respectively connected to both ends of the tower body 301, a plurality of packing sections 302 are arranged in the tower body 301, the plurality of packing sections 302 are distributed between the first feed pipe 303 and the second feed pipe 304, and the pores of each packing section 302 increase along the material flow direction.
[0041] The present invention adopts a multi-stage decolorization process. The decolorization tower is a packed tower. The decolorization tower is made of graphite or steel-lined PTFE or steel-lined PFA. The packing is an irregular packing made of PTFE or PFA. It is a static device with no power operation. It is a non-metallic material and is more suitable for the selection of phosphoric acid materials above 100°C. It increases the service life, reduces the difficulty of selecting metal materials, reduces costs, and is easier to realize automated operation, thereby realizing a more efficient decolorization technology.
[0042] In addition, after the decomposition gas overflows from the decolorization tower of the present invention, a filler washing tower is used, which is made of 316L composite 904 or steel-lined PTFE or PFA, etc. The filler is PTFE or PFA material, which is an irregular filler, so that the decomposition gas can be effectively absorbed and meet the national emission standards.
[0043] Example 1
[0044] The phosphoric acid decolorization method proposed by the present invention has the following steps:
[0045] S1: transporting high concentration phosphoric acid to a heater for heating;
[0046] S2: The heated material in S1 and hydrogen peroxide are adjusted to a volume ratio of 1:0.005 through the first hydrogen peroxide regulating valve 110, and then transported to the first homogeneous and efficient mixing pump 20 for mixing;
[0047] S3: The mixed material in S2 is transported to the first decolorizing tower 30, where the material stays in the first decolorizing tower for 3 hours, and the TOC decomposition rate reaches more than 70%, and then transported to the second homogeneous and efficient mixing pump 40, and the volume ratio of the material and hydrogen peroxide is adjusted to 1:0.005 through the second hydrogen peroxide regulating valve 120, and the mixed material enters the second decolorizing tower 50 for decolorization, where the material stays in the second decolorizing tower 50 for 3 hours, and the total TOC decomposition rate reaches more than 80%, and the decolorized material is transported to the third homogeneous and efficient mixing pump 60, and the volume ratio of the material and hydrogen peroxide is adjusted to 1:0.005 through the third hydrogen peroxide regulating valve 130, and the mixed material is transported to the third decolorizing tower 70 for decolorization, where the material stays in the third decolorizing tower 70 for 3 hours;
[0048] S4: The material after decolorization in the decolorization tower enters the heat exchanger 80 to be cooled to 50°C to obtain decolorized phosphoric acid. The black chromium of the decolorized phosphoric acid is 15, the TOC is 20ppm, and the TOC removal rate is 96%. The gas outlet of the decolorization tower is connected to the packed washing tower 90 to wash the tail gas, and the tail gas is discharged after meeting the standards.
[0049] The concentration of high-concentration phosphoric acid in S1 is 61%, TOC≥500ppm, and blackness≥60 black degrees; the concentration of hydrogen peroxide in S2 and S3 is 20wt%; the decolorization temperature of the decolorization tower is 120°C; the decolorization tower is made of steel-lined PTFE, and the filler material is PTFE.
[0050] Example 2
[0051] The phosphoric acid decolorization method proposed by the present invention has the following steps:
[0052] S1: transporting high concentration phosphoric acid to a heater for heating;
[0053] S2: The heated material in S1 and hydrogen peroxide are adjusted to a volume ratio of 1:0.001 through the first hydrogen peroxide regulating valve 110, and then transported to the first homogeneous and efficient mixing pump 20 for mixing;
[0054] S3: The mixed material in S2 is transported to the first decolorization tower 30, the material stays in the first decolorization tower for 1 hour, and then transported to the second homogeneous and efficient mixing pump 40, the volume ratio of the material and hydrogen peroxide is adjusted to 1:0.001 by the second hydrogen peroxide regulating valve 120, the mixed material enters the second decolorization tower 50 for decolorization, the material stays in the second decolorization tower 50 for 1 hour, the decolorized material is transported to the third homogeneous and efficient mixing pump 60, the volume ratio of the material and hydrogen peroxide is adjusted to 1:0.001 by the third hydrogen peroxide regulating valve 130, the mixed material is transported to the third decolorization tower 70 for decolorization, and the material stays in the third decolorization tower 70 for 1 hour;
[0055] S4: The material after decolorization in the decolorization tower enters the heat exchanger 80 to be cooled to 40° C. to obtain decolorized phosphoric acid. The gas outlet of the decolorization tower is connected to the packed washing tower 90 to wash the tail gas, and then discharged after meeting the standards.
[0056] The concentration of high-concentration phosphoric acid in S1 is 30%, TOC≥500ppm, and blackness≥60 black degrees; the concentration of hydrogen peroxide in S2 and S3 is 50wt%; the decolorization temperature of the decolorization tower is 90°C; the decolorization tower is made of steel-lined PFA, and the filler material is PFA.
[0057] Example 3
[0058] The phosphoric acid decolorization method proposed by the present invention has the following steps:
[0059] S1: transporting high concentration phosphoric acid to a heater for heating;
[0060] S2: The heated material in S1 and hydrogen peroxide are adjusted to a volume ratio of 1:0.01 through the first hydrogen peroxide regulating valve 110, and then transported to the first homogeneous and efficient mixing pump 20 for mixing;
[0061] S3: The mixed material in S2 is transported to the first decolorization tower 30, where the material stays in the first decolorization tower for 5 hours, and then transported to the second homogeneous and efficient mixing pump 40, and the volume ratio of the material to hydrogen peroxide is adjusted to 1:0.01 through the second hydrogen peroxide regulating valve 120, and the mixed material enters the second decolorization tower 50 for decolorization, where the material stays in the second decolorization tower 50 for 5 hours, and the decolorized material is transported to the third homogeneous and efficient mixing pump 60, and the volume ratio of the material to hydrogen peroxide is adjusted to 1:0.01 through the third hydrogen peroxide regulating valve 130, and the mixed material is transported to the third decolorization tower 70 for decolorization, where the material stays in the third decolorization tower 70 for 5 hours;
[0062] S4: The material after decolorization in the decolorization tower enters the heat exchanger 80 to be cooled to 60° C. to obtain decolorized phosphoric acid. The gas outlet of the decolorization tower is connected to the packed washing tower 90 to wash the tail gas and discharge it after meeting the standards.
[0063] The concentration of high-concentration phosphoric acid in S1 is 64%, TOC≥500ppm, and blackness≥60 black degrees; the concentration of hydrogen peroxide in S2 and S3 is 30wt%; the decolorization temperature of the decolorization tower is 150°C; the decolorization tower is made of steel-lined PTFE, and the filler material is PTFE.
Claims
1. A phosphoric acid decolorization device, characterized in that: The invention comprises a heating pump (10), a plurality of decolorizing towers connected in series, and a heat exchanger (80) which are arranged in sequence. A phosphoric acid regulating valve (100) is arranged on the pipeline at the feed end of the heating pump (10). A homogeneous and efficient mixing pump is arranged between the heating pump (10) and the decolorizing towers and between adjacent decolorizing towers. The homogeneous and efficient mixing pump is also connected to a hydrogen peroxide delivery pipeline. A hydrogen peroxide regulating valve is arranged on the hydrogen peroxide delivery pipeline. The gas outlet of the decolorizing tower is also connected to a packing washing tower (90).
2. The phosphoric acid decolorization device according to claim 1, characterized in that: The homogeneous and efficient mixing pump comprises a mixing pump (201), wherein the mixing pump (201) is provided with a mixing pump liquid inlet pipe (202) and a mixing pump liquid outlet pipe (203), wherein the mixing pump liquid outlet pipe (203) is connected to a phosphoric acid delivery pipe (204) and a hydrogen peroxide delivery pipe (205), wherein the hydrogen peroxide delivery pipe (205) is connected to a multi-channel mixing head (206), and a discharge end of the multi-channel mixing head (206) is located in the phosphoric acid delivery pipe (204).
3. The phosphoric acid decolorization device according to claim 2, characterized in that: The mixing pump (201) is composed of several layers of rotors and stators, and the gear plates of each layer of rotors and stators are arranged from coarse to fine.
4. The phosphoric acid decolorization device according to claim 1, characterized in that: The decolorizing tower comprises a tower body (301), a gas outlet is arranged at the top of the tower body (301), a first material delivery pipe (303) and a second material delivery pipe (304) are respectively connected at both ends of the tower body (301), a plurality of packing sections (302) are arranged in the tower body (301), the plurality of packing sections (302) are distributed between the first material delivery pipe (303) and the second material delivery pipe (304), and the pores of each packing section (302) increase along the material flow direction.
5. The decolorization method of the phosphoric acid decolorization device according to any one of claims 1 to 4, characterized in that: The steps are as follows: S1: transporting high concentration phosphoric acid to a heater (10) for heating; S2: The material heated in S1 and the hydrogen peroxide are adjusted in proportion to each other by a hydrogen peroxide regulating valve and then transported to a homogeneous and efficient mixing pump for mixing; S3: The mixed material in S2 is decolorized by passing through a plurality of decolorization towers connected in series, and a homogenizing and efficient mixing pump is arranged between adjacent decolorization towers, and the ratio of the material and hydrogen peroxide delivered to the homogenizing and efficient mixing pump is adjusted by a hydrogen peroxide regulating valve; S4: The material decolorized by the decolorization tower enters the heat exchanger (80) for cooling to obtain decolorized phosphoric acid. The gas outlet of the decolorization tower is connected to a packing washing tower to wash the tail gas, and then discharged after meeting the standards.
6. The decolorization method of the phosphoric acid decolorization device according to claim 5, characterized in that: The concentration of high concentration phosphoric acid in S1 is 30%-64%, TOC ≥ 500ppm, and blackness ≥ 60 black degrees.
7. The decolorization method of the phosphoric acid decolorization device according to claim 5, characterized in that: The concentration of hydrogen peroxide in S2 and S3 is 5-30wt%, and the volume ratio of the material to hydrogen peroxide is 1:0.001-0.
01.
8. The decolorization method of the phosphoric acid decolorization device according to claim 5, characterized in that: The residence time of the material in the bleaching tower is 1-5h, and the bleaching temperature is 90-150°C.
9. The decolorization method of the phosphoric acid decolorization device according to claim 5, characterized in that: The decolorization tower is made of graphite or steel-lined PTFE or steel-lined PFA, and the filler material is PTFE or PFA.
10. The decolorization method of the phosphoric acid decolorization device according to claim 5, characterized in that: The material temperature after cooling in the heat exchanger (80) in S4 is 40-60°C.
Citation Information
Cited By
Device and method for treating high-COD (Chemical Oxygen Demand) organic wastewater in 1-chlorobutane production process
CN119390158A