Semiconductor structure, manufacturing method of semiconductor structure and memory
By arranging a protective ring of a vertical fragile structure in the protection zone of the semiconductor structure, the problem of damage to the chip area during the cutting process is solved, and the yield and performance of the semiconductor structure are improved.
Patent Information
- Application Number
- CN202310437084.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-19
- Publication Date
- 2024-10-29
AI Technical Summary
Semiconductor structures are easily damaged during the cutting process, affecting their yield and performance.
Design a semiconductor structure, in which a protection zone is set between the chip area and the dicing road area. A protection ring structure is provided in the protection zone. The protection ring structure has a first fragile structure, and the first fragile structure is vertical to the substrate. The surface extends in the direction to absorb stress and guide the stress to be transmitted in the vertical direction to avoid conduction to the chip area.
It effectively improves the yield and performance of the semiconductor structure. By buffering stress and guiding stress transfer, it reduces the risk of damage in the chip area and ensures the stability and performance of the chip.
Smart Images

Figure CN118870804A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure belongs to the field of semiconductors, and in particular relates to a semiconductor structure, a method for manufacturing the semiconductor structure, and a memory. Background Art
[0002] The cutting process of semiconductor structures usually includes three steps. Step 1: Film processing, such as pasting the semiconductor structure on the surface of the ultraviolet irradiated film. Step 2: Laser cutting, using pulsed laser to focus on the scribe area of the semiconductor structure and form a modified layer. The modified layer is a structure with local melting damage caused by the high temperature of the laser. The modified layer usually extends between the upper and lower surfaces of the semiconductor structure. Step 3: Expansion processing, the cut semiconductor structure is evenly expanded in the horizontal direction to increase the spacing between the chips, which is conducive to the subsequent core removal and chip bonding.
[0003] However, the chip region of the semiconductor structure is easily damaged during the cutting process, thereby affecting the yield and performance of the semiconductor structure. Summary of the invention
[0004] The embodiments of the present disclosure provide a semiconductor structure, a method for manufacturing the semiconductor structure, and a memory, which are at least beneficial to improving the yield and performance of the semiconductor structure.
[0005] According to some embodiments of the present disclosure, on one hand, an embodiment of the present disclosure provides a semiconductor structure, wherein the semiconductor structure includes: a substrate, the substrate includes a chip area, a protection area and a dicing area, the protection area is located between the chip area and the dicing area; the protection area has a guard ring structure, the guard ring structure has a first fragile structure, and the first fragile structure extends in a direction perpendicular to the upper surface of the substrate.
[0006] According to some embodiments of the present disclosure, on the other hand, an embodiment of the present disclosure further provides a method for manufacturing a semiconductor structure, the manufacturing method comprising: providing a substrate, the substrate comprising a chip area, a protection area and a scribe line area, the protection area being located between the chip area and the scribe line area; forming a guard ring structure on the protection area; forming a first fragile structure within the guard ring structure, the first fragile structure extending in a direction perpendicular to the upper surface of the substrate.
[0007] According to some embodiments of the present disclosure, another aspect of the embodiments of the present disclosure further provides a memory, the memory comprising: the aforementioned semiconductor structure.
[0008] The technical solution provided by the embodiment of the present disclosure has at least the following advantages: the guard ring structure has a first fragile structure extending in a direction perpendicular to the upper surface of the substrate. The first fragile structure can provide space for the deformation of the guard ring structure and can also guide the stress to be transmitted in the extension direction thereof, thereby preventing the stress from being transmitted to the chip area and causing damage to the chip area. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] The accompanying drawings herein are incorporated into the specification and constitute a part of the specification, illustrate embodiments consistent with the present disclosure, and together with the specification are used to explain the principles of the present disclosure. Obviously, the accompanying drawings described below are only some embodiments of the present disclosure, and for ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without creative work.
[0010] Figure 1 A top view of a semiconductor structure provided by an embodiment of the present disclosure is shown;
[0011] Figure 2-Figure 3 Different local top views of the semiconductor structure provided by the embodiments of the present disclosure are respectively shown;
[0012] Figure 4-Figure 5 Partial cross-sectional views of different semiconductor structures provided by the embodiments of the present disclosure are respectively shown;
[0013] Figure 6-Figure 11 A schematic structural diagram corresponding to each step in a method for manufacturing a semiconductor structure provided by an embodiment of the present disclosure is shown;
[0014] Figure 12-Figure 15 A structural schematic diagram corresponding to each step in another method for manufacturing a semiconductor structure provided by an embodiment of the present disclosure is shown. DETAILED DESCRIPTION
[0015] As can be seen from the background technology, the chip area of the semiconductor structure is easily damaged during the cutting process. After analysis, it is found that the main reason is that a guard ring structure can be set between the dicing area and the chip area. The guard ring structure can prevent the cracks in the dicing area from extending to the chip area, but some stress may still be transmitted to the chip area, thereby increasing the damaged area of the cutting, and further affecting the yield and performance of the chip.
[0016] The embodiment of the present disclosure provides a semiconductor structure, which includes: a protection zone between a chip zone and a scribe zone, a protection ring structure is provided in the protection zone, a first fragile structure is provided in the protection ring structure, and the first fragile structure extends in a direction perpendicular to the upper surface of a substrate. The first fragile structure can provide space for deformation of the protection ring structure, and can also serve as a stress buffer area to guide the stress to be transmitted in a direction perpendicular to the upper surface of the substrate, thereby avoiding damage to the chip zone, thereby ensuring the yield and performance of the chip.
[0017] The following will describe the various embodiments of the present disclosure in detail with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the various embodiments of the present disclosure, many technical details are provided in order to enable the reader to better understand the embodiments of the present disclosure. However, even without these technical details and various changes and modifications based on the following embodiments, the technical solutions claimed in the embodiments of the present disclosure can be implemented.
[0018] like Figure 1-Figure 5 As shown, an embodiment of the present disclosure provides a semiconductor structure, which includes: a substrate 1, the substrate 1 includes a chip area A, a protection area B and a dicing area C, the protection area B is located between the chip area A and the dicing area C; the protection area B has a protection ring structure 2, the protection ring structure 2 has a first fragile structure 5, and the first fragile structure 5 extends in a direction perpendicular to the upper surface of the substrate 1.
[0019] That is to say, the first fragile structure 5 has a fragile characteristic and can absorb stress well. In addition, the extension direction of the first fragile structure 5 is perpendicular to the upper surface of the substrate 1, so the stress can be transmitted in its extension direction and avoid being transmitted to the chip area A to ensure the yield and performance of the chip area A. It should be noted that due to process reasons, the extension direction of the first fragile structure 5 may not be completely perpendicular to the upper surface of the substrate 1, as long as it is close to a vertical relationship, for example, the angle is between 80° and 100°. The extension direction of the first fragile structure 5 can also be understood as the length direction of the cross section of the first fragile structure 5.
[0020] The semiconductor structure will be described in detail below with reference to the accompanying drawings.
[0021] Figure 1 is a top view of the semiconductor structure, refer to Figure 1 , the protection area B and the scribe line area C are arranged around the chip area A. That is, the protection ring structure 2 can be arranged around the chip area A, thereby protecting the chip area A on multiple sides.
[0022] refer to Figure 2 , Figure 2It is a partially enlarged top view of a semiconductor structure. The protection ring structure 2 includes a peripheral protection ring structure 21 and an inner protection ring structure 22 which are arranged at intervals. The peripheral protection ring structure 21 is located on the side of the inner protection ring structure 22 away from the chip area A. That is, the peripheral protection ring structure 21 is closer to the scribe line area C, and the inner protection ring structure 22 is closer to the chip area A. The peripheral protection ring structure 21 can also be called a scribe line seal ring structure, and the inner protection ring structure 22 can also be called a main chip protection ring structure. The first fragile structure 5 is arranged in the peripheral protection ring structure 21, so that the stress can be guided further away from the chip area A to avoid damage to the chip area A. In other embodiments, the semiconductor structure can also include only the peripheral protection ring structure 21. The inner protection ring structure 22 can be arranged by high-level metal grounding to improve the reliability of the semiconductor structure.
[0023] In some embodiments, the guard ring structure 2 is disposed around the chip region A, and the plurality of first fragile structures 5 are arranged at intervals in the circumferential direction of the chip region A. For example, the plurality of first fragile structures 5 may be arranged at least once around the chip region A. In this way, the first fragile structures 5 may guide stress transfer around the chip region A, thereby reducing the risk of damage to the chip region A.
[0024] refer to Figure 2-Figure 3 In some embodiments, the plurality of first fragile structures 5 located on the same side of the chip region A may be arranged in the same row, for example, the arrangement direction of the plurality of first fragile structures 5 is parallel to the side of the chip region A. This can improve the uniformity of the semiconductor structure, simplify the manufacturing process, and avoid the problem of stress concentration.
[0025] In addition, a plurality of first fragile structures 5 may be arranged at equal intervals, so that the first fragile structures 5 can be distributed more evenly to better disperse stress.
[0026] refer to Figure 2 , in a direction parallel to the upper surface of the substrate 1, the cross-sectional shape of the first fragile structure 5 is a rectangle. The rectangular first fragile structure 5 has a uniform width, which can guide stress transfer more uniformly. In addition, the manufacturing process of the rectangular first fragile structure 5 is simpler.
[0027] refer to Figure 3 , Figure 3It is a partial top view of another semiconductor structure. In the direction parallel to the upper surface of the substrate 1, the cross-sectional shape of the first fragile structure 5 is a triangle. The triangle has better stability and stronger stress resistance. For example, the vertex angles of adjacent triangles can be oriented in opposite directions. For example, the vertex angle of a triangle faces the chip area A, and the vertex angle of the adjacent triangle faces the dicing area C. In addition, the two opposite sides of the adjacent triangles can be arranged in parallel, so that the first fragile structure 5 can make full use of the space in the guard ring structure 2.
[0028] In addition, in the direction parallel to the upper surface of the substrate 1 , the cross-sectional shape of the first fragile structure 5 can also be a circle, a square, a trapezoid, a parallelogram or other irregular shapes.
[0029] Figure 4 and Figure 5 They are different partial cross-sectional views of the semiconductor structure, refer to Figure 4 , at least one of the upper and lower sides of the first fragile structure 5 has a sharp corner. Sharp corners are more likely to accumulate stress, thereby preventing stress from being transferred toward the chip area A. For example, the upper side of the first fragile structure 5 has a sharp corner protruding upward, and the lower side of the first fragile structure 5 has two sharp corners protruding downward. In other words, the sharp corners on the upper and lower sides protrude roughly in a direction perpendicular to the upper surface of the substrate 1, thereby better guiding the stress to be transferred in this direction. In other embodiments, one of the upper and lower sides of the first fragile structure 5 may have a sharp corner. In addition, refer to Figure 5 The cross-sectional shape of the first fragile structure 5 perpendicular to the upper surface of the substrate 1 may also be a rectangle, that is, the upper and lower sides thereof may not have sharp corners.
[0030] The guard ring structure 2 includes a plurality of metal ring structures 210 arranged in a direction parallel to the upper surface of the substrate 1; at least some of the adjacent metal ring structures 210 are arranged at intervals, and the first fragile structure 5 is located between the spaced metal ring structures 210. Thus, the first fragile structure 5 can provide space for the deformation of the metal ring structure 210. In addition, the guard ring structure 2 may also include an interlayer dielectric layer 3, and the interlayer dielectric layer 3 is at least located between the spaced metal ring structures 210. In other words, in combination with reference Figure 2-Figure 5 In a direction parallel to the upper surface of the substrate 1, the guard ring structure 2 as a whole can be a continuous structure with a spacing space inside, in which the interlayer dielectric layer 3 and the first fragile structure 5 can be arranged, and the spacing space divides the guard ring structure 2 into a multi-layer metal ring structure 210.
[0031] For example, refer to Figure 3The metal ring structure 210 includes a plurality of surrounding metal ring structures 213 and a plurality of connecting metal ring structures 214, wherein the surrounding metal ring structure 213 extends in the circumferential direction of the chip region A and surrounds the chip region A, and in the direction from the chip region A to the dicing lane region C, the plurality of surrounding metal ring structures 213 are arranged at intervals. The connecting metal ring structure 214 can be located between two adjacent surrounding metal ring structures 213 and connected to the two adjacent surrounding metal ring structures 213. The first fragile structure 5 can be located in the spacing area between the adjacent surrounding metal ring structures 213 and between the two adjacent connecting metal ring structures 214. Since the spacing area between the adjacent surrounding metal ring structures 213 also surrounds the chip region A, the plurality of first fragile structures 5 can be arranged in the circumferential direction of the chip region A, thereby guiding the stress transfer around the chip region A.
[0032] In some embodiments, reference Figure 2-Figure 4 , the first fragile structure 5 may be a first air gap 51. In some other embodiments, refer to Figure 5 The first fragile structure 5 may also be a first fragile material layer 52, and the first fragile material layer 52 may include brittle materials such as polysilicon. Compared with the first fragile material layer 52, the first air gap 51 has fewer steps in the manufacturing process, which is conducive to reducing production costs; in addition, the first air gap 51 can also provide more sufficient space for the deformation of the guard ring structure 2 to avoid squeezing the devices in the chip area A.
[0033] In some embodiments, reference Figure 4 , the first fragile structure 5 includes a plurality of first sub-fragile structures 50 arranged at intervals in a direction perpendicular to the upper surface of the substrate 1. Compared with a continuous first fragile structure 5 of the same height, the manufacturing difficulty of the plurality of first sub-fragile structures 50 arranged at intervals in a direction perpendicular to the upper surface of the substrate 1 is lower, and the overall stability of the semiconductor structure is better, which can avoid the problem of the semiconductor structure breaking during the non-cutting process. In addition, the height of the first sub-fragile structure 50 in the direction perpendicular to the upper surface of the substrate 1 can be greater than the width of the first sub-fragile structure 50 in the direction parallel to the upper surface of the substrate 1, so as to better guide the stress to propagate in the direction perpendicular to the upper surface of the substrate 1.
[0034] refer to Figure 4 , the first sub-fragile structure 50 is a first sub-air gap 510. Figure 5 The first sub-fragile structure 50 may also be a first sub-fragile material layer 520 .
[0035] In some embodiments, the types of the multiple first sub-fragile structures 50 are the same, such as all being air gaps or all being fragile material layers, which is conducive to unifying the manufacturing process and reducing production costs. In other embodiments, the types of the multiple first sub-fragile structures 50 may also be different. For example, the first sub-fragile structure 50 located in the lower layer may be a fragile material layer, and the first sub-fragile structure 50 located in the upper layer may be an air gap, which is conducive to improving the stability of the structure.
[0036] In some embodiments, reference Figure 4 In the direction from the substrate 1 to the guard ring structure 2, the widths of the plurality of first fragile sub-structures 50 may be increased sequentially, which may increase the strength and stability of the semiconductor structure and avoid the problem of collapse in a non-cutting process. Figure 5 The widths of the plurality of first fragile sub-structures 50 may also be the same, which can improve the uniformity of the semiconductor structure and simplify the process.
[0037] In some embodiments, reference Figure 4-Figure 5 The protection ring structure 2 includes a first sub-metal ring structure 211 and a second sub-metal ring structure 212 which are alternately arranged in a direction perpendicular to the upper surface of the substrate 1; in a direction parallel to the upper surface of the substrate 1, the cross-sectional area of the first sub-metal ring structure 211 is greater than the cross-sectional area of the second sub-metal ring structure 212. The first sub-fragile structure 50 is arranged opposite to the first sub-metal ring structure 211.
[0038] The reason for this design is that: the first sub-metal ring structure 211 has a larger volume and a greater degree of deformation. The first sub-fragile structure 50 is arranged relative to the first sub-metal ring structure 211, which can provide sufficient deformation space for the first sub-metal ring structure 211 to release stress. In addition, in the direction parallel to the upper surface of the substrate 1, the spacing between adjacent first sub-metal ring structures 211 is smaller than the spacing between adjacent second sub-metal ring structures 212; thus, the first sub-fragile structure 50 formed between adjacent first sub-metal ring structures 211 has a smaller width-to-length ratio, so that the stress can be better guided to be transmitted in the length direction of the first sub-fragile structure 50 (i.e., the direction perpendicular to the upper surface of the substrate 1), thereby reducing the risk of damage to the chip area A. It should be noted that due to process manufacturing reasons, a partial length of the first sub-fragile structure 50 can also be arranged relative to the second sub-metal ring structure 212, but the main part of the first sub-fragile structure 50 is still arranged relative to the first sub-metal ring structure 211.
[0039] refer to Figure 4-Figure 5 , the interlayer dielectric layer 3 may surround the first fragile structure 5. In other embodiments, the interlayer dielectric layer 3 and the metal ring structure 210 may surround the first fragile structure 5 together. For example, referring to Figure 4, when the first fragile structure 5 is a first air gap 51, each first sub-fragile structure 50 is surrounded by the interlayer dielectric layer 3. This is because the first air gap 51 usually needs to be formed in a region with a higher aspect ratio, and the interlayer dielectric layer 3 can occupy part of the space between adjacent first sub-metal ring structures 211, so that the width of the remaining space between the first sub-metal ring structures 211 is reduced, thereby reducing the difficulty of forming the first air gap 51. In other embodiments, refer to Figure 5 When the first fragile structure 5 is the first fragile material layer 52, the metal ring structure 210 can contact at least two opposite sides of the first sub-fragile structure 50, that is, the first sub-fragile structure 50 can fill the space between adjacent first sub-metal ring structures 211. This is conducive to reducing the process steps, thereby reducing the production cost. This will be described in detail later in conjunction with the manufacturing method.
[0040] In other embodiments, the guard ring structure 2 may also be a columnar structure, that is, the cross-sectional shape of the guard ring structure 2 in a direction perpendicular to the upper surface of the substrate 1 may also be a rectangle with a uniform width, which can simplify the production process.
[0041] In some embodiments, reference Figure 4-Figure 5 , the semiconductor structure further includes: a second fragile structure 8, the second fragile structure 8 extends in a direction perpendicular to the upper surface of the substrate 1; the second fragile structure 8 is located in the substrate 1 of the protection area B and below the first fragile structure 5. The second fragile structure 8 can guide the stress in the substrate 1 to be transmitted in a direction perpendicular to the upper surface of the substrate 1, and provide space for the deformation of the structure in the substrate 1, thereby enhancing the protection of the chip area A. In addition, since the first fragile structure 5 and the second fragile structure 8 are aligned, the conduction direction of the stress can be better limited.
[0042] In some embodiments, reference Figure 4 , the second fragile structure 8 may be a second air gap 83. In some other embodiments, referring to Figure 5 The second fragile structure 8 may also be a second fragile material layer 84, and the second fragile material layer 84 may include a brittle material such as polysilicon. Compared with the second fragile material layer 84, the second air gap 83 has fewer steps in the manufacturing process, which is conducive to reducing production costs, and the second air gap 83 can also provide more sufficient space for the deformation of the structure in the substrate 1.
[0043] In some embodiments, the first fragile structure 5 and the second fragile structure 8 are of the same type, such as both are air gaps or both are fragile material layers, which is conducive to unifying the manufacturing process and reducing production costs. In other embodiments, the first fragile structure 5 and the second fragile structure 8 may also be of different types, such as the first fragile structure 5 is a first air gap 51, and the second fragile structure 8 is a second fragile material layer 84, which is conducive to improving the stability of the structure.
[0044] In some embodiments, the second fragile structure 8 may be a single-layer structure to simplify the production process. In other embodiments, the second fragile structure 8 may also include a plurality of second sub-fragile structures arranged in a direction perpendicular to the upper surface of the substrate 1, so as to ensure the strength of the substrate 1 while enhancing the guiding effect of the second fragile structure 8 on the stress.
[0045] refer to Figure 4-Figure 5 , in a direction perpendicular to the upper surface of the substrate 1, the cross-sectional shape of the second fragile structure 8 includes a spindle shape. That is, the size of the second fragile structure 8 at the upper and lower ends can be smaller than the size of the middle part. In this way, it is easier to concentrate stress at the upper and lower ends of the second fragile structure 8, and avoid stress transmission to the chip area A.
[0046] In summary, the embodiment of the present disclosure forms the first fragile structure 5 in the guard ring structure 2 as a buffering structure. When external stress is generated and the stress is transmitted to the guard ring structure 2, the first fragile structure 5 will absorb the stress and guide the stress to deform in the vertical direction, thereby reducing the probability of damage such as cracking caused by the stress being transmitted to the chip area A. In addition, a second fragile structure 8 can be formed in the substrate 1 to enhance the protection of the chip area A.
[0047] like Figure 6-Figure 15 As shown, another embodiment of the present disclosure provides a method for manufacturing a semiconductor structure. This manufacturing method can be used to manufacture the semiconductor structure provided by the above embodiment. For detailed description of this semiconductor structure, please refer to the above embodiment and will not be repeated here. It should be noted that in order to facilitate the description and clearly illustrate the steps of the semiconductor structure manufacturing method, Figures 6 to 15 All of them are schematic diagrams of local structures of semiconductor structures.
[0048] refer to Figure 6 , providing a substrate 1, which can be a silicon substrate, a germanium substrate or a silicon germanium substrate. The substrate 1 includes a chip area A, a protection area B and a scribe line area C (refer to Figure 1 ), the protection area B is located between the chip area A and the dicing area C.
[0049] refer to Figure 6-Figure 11, forming a guard ring structure 2 on the protection zone B; forming a first fragile structure 5 in the guard ring structure 2, the first fragile structure 5 extending in a direction perpendicular to the upper surface of the substrate 1. For example, forming the guard ring structure 2 on the protection zone B includes: forming an outer guard ring structure 21 and an inner guard ring structure 22 (refer to Figure 2 ), the peripheral protection ring structure 21 is located on a side of the inner protection ring structure 22 away from the chip area A, and a first fragile structure 5 is formed in the peripheral protection ring structure 21.
[0050] The steps of the protection ring structure 2 and the first fragile structure 5 will be described in detail below.
[0051] refer to Figure 6-Figure 9 , forming a plurality of metal ring structures 210 arranged in a direction parallel to the upper surface of the substrate 1 , and at least some of the adjacent metal ring structures 210 are spaced apart and surround a first groove 42 .
[0052] Specifically, refer to Figure 6 , forming a first dielectric layer 71, a sacrificial layer 72, a first mask layer 73, a second mask layer 74 and a first photoresist layer 75 which are stacked. For example, the first mask layer 73 may be a hard mask layer, and the second mask layer 74 may be an anti-reflection layer. The material of the first dielectric layer 71 may be silicon carbonitride, and the material of the sacrificial layer 72 may be a low dielectric constant material such as silicon dioxide and silicon nitride. In other embodiments, the first dielectric layer 71 may not be formed. In addition, only a single-layer mask layer may be formed, for example, one of the first mask layer 73 and the second mask layer 74 is formed.
[0053] refer to Figure 7 , using the first photoresist layer 75 as a mask, the first mask layer 73, the second mask layer 74, the first dielectric layer 71 and the sacrificial layer 72 are etched to form a groove 41 penetrating the first dielectric layer 71 and the sacrificial layer 72. Thereafter, the first photoresist layer 75, the first mask layer 73 and the second mask layer 74 are removed.
[0054] refer to Figure 8 , a metal ring structure 210 is formed in the groove 41 , for example, the metal ring structure 210 is formed by an electroplating process.
[0055] refer to Fig. 9 , the sacrificial layer 72 is removed to expose the sidewall of the metal ring structure 210. For example, the sacrificial layer 72 is etched by a dry process, and the etching gas may be ammonia or at least one of hydrogen and nitrogen.
[0056] So far, based on Figure 6-Figure 9 The metal ring structures 210 may be formed, and the first grooves 42 may be formed between adjacent metal ring structures 210 .
[0057] refer to Fig.10 , forming a wrapping layer 76, which at least covers the sidewalls and the upper surface of the metal ring structure 210. For example, a chemical vapor deposition process or an atomic layer deposition process is used to form a wrapping layer 76 that conformally covers the metal ring structure 210. The material of the wrapping layer 76 can be the same as the material of the first dielectric layer 71, for example, both are silicon carbonitride. The wrapping layer 76 can protect the metal ring structure 210 in the subsequent process of forming the interlayer dielectric layer 3 to prevent the reaction gas of the interlayer dielectric layer 3 from invading the metal ring structure 210 and reacting with the metal ring structure 210. In addition, the wrapping layer 76 can also adjust the width of the filling space between adjacent metal ring structures 210, thereby reducing the process difficulty of forming the first air gap 51.
[0058] Continue to refer Fig.10 , forming an interlayer dielectric layer 3, the interlayer dielectric layer 3 is at least located on the upper surface of the plurality of metal ring structures 210, and closes the top opening of the first groove 42 to form a first air gap 51 at the first groove 42, and the first air gap 51 serves as a first fragile structure 5. In addition, the interlayer dielectric layer 3 also covers a portion of the upper surface of the wrapping layer 76. Since the interlayer dielectric layer 3 can span across the plurality of metal ring structures 210, it has good mechanical strength, which is conducive to ensuring the stability of the structure. The guard ring structure 2 includes the interlayer dielectric layer 3 and the metal ring structure 210.
[0059] For example, the interlayer dielectric layer 3 is formed by chemical vapor deposition. During the chemical vapor deposition process, the process parameters need to be adjusted so that the interlayer dielectric layer 3 quickly forms the first groove 42 (refer to Fig. 9 ) to cover the top opening of the first groove 42, thereby reducing the deposition material entering the first groove 42.
[0060] It should be noted that the wrapping layer 76 covering the sidewalls of the metal ring structure 210 is equivalent to reducing the spacing between adjacent metal ring structures 210, avoiding excessive deposition of interlayer dielectric layer materials between adjacent metal ring structures 210 due to excessive spacing, thereby avoiding affecting the size of the first air gap 51. In other words, the first air gap 51 can be formed using a self-alignment process without using a new mask.
[0061] Continue to refer Fig.10In some embodiments, a lower dielectric layer 31 and an upper dielectric layer 32 are stacked and arranged together as an interlayer dielectric layer 3. For example, the material of the lower dielectric layer 31 may be silicon oxycarbide or fluorinated.silicate-glass (FSG). The material of the upper dielectric layer 32 may be silicon oxide or silicon nitride, etc. Taking the material of the lower dielectric layer 31 as FSG as an example, FSG contains fluorine elements, and the wrapping layer 76 can prevent the fluorine elements from entering the metal ring structure 210 during the high-temperature process, thereby protecting the metal ring structure 210. The fluorine element can reduce the dielectric constant and change the gap filling ability when depositing a thin film. The higher the fluorine content, the stronger the gap filling ability. Therefore, the fluorine content of FSG can be set within a smaller range to avoid too much FSG filling in the first groove 42. In other embodiments, the interlayer dielectric layer 3 may also be a single-layer structure, that is, only one of the lower dielectric layer 31 and the upper dielectric layer 32 is formed.
[0062] In other embodiments, the wrapping layer 76 may not be formed before forming the interlayer dielectric layer 3, and the deposition rate may be increased to prevent excessive deposition material from entering the gaps between the metal ring structures 210. Alternatively, the width of the metal ring structure 210 in a direction parallel to the upper surface of the substrate 1 may be increased so that adjacent metal ring structures 210 have a smaller spacing, thereby reducing the difficulty of forming the first air gap 51. Alternatively, another mask may be used to define the pattern of the first air gap 51. For example, after the metal ring structure 210 is formed, the sacrificial layer 72 is not removed, and then, part of the sacrificial layer 72 between the adjacent metal ring structures 210 is etched, thereby transferring the pattern of the mask to the sacrificial layer 72 to form the first groove 42. Thereafter, an interlayer dielectric layer 3 is formed, and the interlayer dielectric layer 3 at least covers the upper surfaces of the metal ring structure 210 and the remaining sacrificial layer 72, and closes the opening of the first groove 42.
[0063] In some embodiments, the width of the first groove 42 is smaller than the height of the metal ring structure 210, that is, the first groove 42 can have a larger aspect ratio, which can reduce the difficulty of forming the first air gap 51 and better guide the stress to be transmitted in a direction perpendicular to the upper surface of the substrate 1.
[0064] In some embodiments, reference Figure 4, the protection ring structure 2 includes a first sub-metal ring structure 211 and a second sub-metal ring structure 212. The first air gap 51 may include a plurality of first sub-air gaps 510 arranged at intervals in a direction perpendicular to the upper surface of the substrate 1, that is, the first sub-air gap 510 serves as a first sub-fragile structure 50. The first sub-air gap 510 may be arranged opposite to the first sub-metal ring structure 211. For example, a plurality of spaced-apart metal ring structures 210 each include a first sub-metal ring structure 211 and a second sub-metal ring structure 212, and the first sub-air gap 510 is formed between adjacent first sub-metal ring structures 211 arranged in the same layer. Since the spacing between adjacent first sub-metal ring structures 211 is smaller than the spacing between adjacent second sub-metal ring structures 212, it is easier to form a first sub-air gap between adjacent first sub-metal ring structures 211.
[0065] For example, a plurality of first sub-metal ring structures 211 arranged at intervals and a first groove 42 located between adjacent first sub-metal ring structures 211 are first formed, and then an interlayer dielectric layer 3 is formed to cover the plurality of first sub-metal ring structures 211 and close the top opening of the first groove 41, thereby forming a first sub-air gap 510. Thereafter, the interlayer dielectric layer 3 above the first sub-metal ring structure 211 is etched to form a through hole, and the through hole exposes a portion of the upper surface of the first sub-metal ring structure 211; and a second sub-metal ring structure 212 filling the through hole is formed. Thereafter, the aforementioned process steps of forming the first sub-metal ring structure 211, the interlayer dielectric layer 3, the first sub-air gap 510, and the second sub-metal ring structure 212 are repeated. Thus, the first sub-air gaps 510 arranged at intervals in a direction perpendicular to the upper surface of the substrate 1 can be formed.
[0066] refer to Fig.11 In some other embodiments, a first fragile material layer 52 may be formed as the first fragile structure 5. For example, after forming the wrapping layer 76, a chemical vapor deposition process is used to deposit polysilicon or other materials between adjacent metal ring structures 210 as the first fragile material layer 52. Thereafter, an interlayer dielectric layer 3 is formed above the metal ring structure 210 and the first fragile material layer 52.
[0067] refer to Figure 12-Figure 15 In some embodiments, before forming the guard ring structure 2, the method further includes: forming a second fragile structure 8 in the substrate 1 in the protection area B; the second fragile structure 8 extends in a direction perpendicular to the upper surface of the substrate 1, and the first fragile structure 5 is also formed above the second fragile structure 8. The second fragile structure 8 serves as a buffer area in the substrate 1 to enhance the protection of the chip area A.
[0068] refer to Figure 12-13 , etching the substrate 1 along a direction perpendicular to the upper surface of the substrate 1 to form a second groove 85 in the substrate 1 .
[0069] Specifically, refer to Fig.12 , forming a second photoresist layer 81 on the upper surface of the substrate 1, and performing exposure and development processing on the second photoresist layer 81 to pattern the second photoresist layer 81. Fig.13 , using the patterned second photoresist layer 81 as a mask, a dry etching process is used to etch a portion of the thickness of the substrate 1 to form a second groove 85. The second groove 85 can be arranged opposite to the first groove 42 formed subsequently. Thereafter, the second photoresist layer 81 is removed to expose the upper surface of the substrate 1, and the substrate 1 is cleaned to remove impurities on the surface of the substrate 1.
[0070] It should be noted that the width of the second groove 85 parallel to the upper surface of the substrate 1 can be smaller than the depth of the second groove 85 perpendicular to the upper surface of the substrate 1. For example, the aspect ratio of the second groove 85 can be greater than 2:1, which can reduce the material of the covering layer 82 subsequently deposited into the second groove 85.
[0071] refer to Fig.14 , forming a capping layer 82, the capping layer 82 closes the opening at the top of the second groove 85 to form a second air gap 83 at the second groove 85, and the second air gap 83 serves as a second fragile structure 8. For example, the capping layer 82 is formed by an epitaxial production process or a chemical vapor deposition process. Thereafter, a high temperature annealing treatment may be performed to repair defects of the substrate 1. In some embodiments, the material of the capping layer 82 may be the same as that of the substrate 1, thereby reducing defects at the interface between the capping layer 82 and the substrate 1.
[0072] In other embodiments, reference Fig.15 A second fragile material layer 84 may also be deposited in the second groove 85 as the second fragile structure 8, and thereafter, a covering layer 82 covering the second fragile material layer 84 and the upper surface of the substrate 1 is formed.
[0073] In summary, the embodiment of the present disclosure forms a first groove 42 between adjacent metal ring structures 210, and forms an interlayer dielectric layer 3 to close the opening of the first groove 42 to form a first air gap 51; or, fills the first fragile material layer 52 in the first groove 42. The first air gap 51 or the first fragile material layer 52 as the first fragile structure 5 can limit the transfer direction of stress and avoid damaging the chip area A. In addition, a second air gap 83 or a second fragile material layer 84 can be formed in the substrate 1 to enhance the guiding effect on the stress.
[0074] Another embodiment of the present disclosure further provides a memory, the memory includes the semiconductor structure provided by the aforementioned embodiment, and the detailed description of the semiconductor structure can refer to the detailed description of the aforementioned embodiment. For example, structures such as capacitors, word lines, bit lines, and transistors can also be formed in the chip area. The memory can be a dynamic random access memory (DRAM), a static random access memory (SRAM), and other memories.
[0075] In the description of this specification, the description with reference to the terms "some embodiments", "exemplarily", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present disclosure. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0076] Although the embodiments of the present disclosure have been shown and described above, it is to be understood that the above embodiments are exemplary and cannot be construed as limitations on the present disclosure. A person skilled in the art may change, modify, replace and modify the above embodiments within the scope of the present disclosure. Therefore, any changes or modifications made in accordance with the claims and specification of the present disclosure shall fall within the scope covered by the patent of the present disclosure.
Claims
1. A semiconductor structure, characterized in that: include: A substrate, the substrate comprising a chip area, a protection area and a scribe line area, the protection area being located between the chip area and the scribe line area; A guard ring structure is provided on the protection zone, a first fragile structure is provided inside the guard ring structure, and the first fragile structure extends in a direction perpendicular to the upper surface of the substrate.
2. The semiconductor structure according to claim 1, characterized in that: The protection ring structure includes a plurality of metal ring structures arranged in a direction parallel to the upper surface of the substrate; at least some of the adjacent metal ring structures are spaced apart, and the first fragile structure is located between the spaced apart metal ring structures.
3. The semiconductor structure according to claim 2, characterized in that: The first fragile structure includes a plurality of first sub-fragile structures arranged at intervals in a direction perpendicular to the upper surface of the substrate.
4. The semiconductor structure according to claim 3, characterized in that: The metal ring structure includes a first sub-metal ring structure and a second sub-metal ring structure alternately arranged in a direction perpendicular to the upper surface of the substrate; In a direction parallel to the upper surface of the substrate, the cross-sectional area of the first sub-metal ring structure is greater than the cross-sectional area of the second sub-metal ring structure; The first sub-fragile structure is arranged opposite to the first sub-metal ring structure.
5. The semiconductor structure according to claim 1, characterized in that: The guard ring structure is disposed around the chip region, and a plurality of the first fragile structures are arranged at intervals in the circumferential direction of the chip region.
6. The semiconductor structure according to claim 1, characterized in that In a direction parallel to the upper surface of the substrate, a cross-sectional shape of the first fragile structure includes a triangle or a rectangle.
7. The semiconductor structure according to claim 1, characterized in that: At least one of the upper and lower sides of the first fragile structure has a sharp corner.
8. The semiconductor structure according to claim 1, characterized in that: The first fragile structure is a first air gap, or the first fragile structure is a first fragile material layer, and the material of the first fragile material layer includes polysilicon.
9. The semiconductor structure according to any one of claims 1 to 8, characterized in that: Also includes: a second fragile structure extending in a direction perpendicular to the upper surface of the substrate; The second frangible structure is located within the base of the protected area and below the first frangible structure.
10. The semiconductor structure according to claim 9, characterized in that: The second fragile structure is a second air gap, or the second fragile structure is a second fragile material layer, and the material of the second fragile material layer includes polysilicon.
11. The semiconductor structure according to claim 9, characterized in that: In a direction perpendicular to the upper surface of the substrate, a cross-sectional shape of the second fragile structure includes a spindle shape.
12. A method for manufacturing a semiconductor structure, characterized in that: include: Providing a substrate, the substrate comprising a chip area, a protection area and a scribe line area, wherein the protection area is located between the chip area and the scribe line area; forming a protection ring structure on the protection zone; A first fragile structure is formed within the guard ring structure, the first fragile structure extending in a direction perpendicular to the upper surface of the substrate.
13. The method for manufacturing a semiconductor structure according to claim 12, characterized in that: forming a plurality of metal ring structures arranged in a direction parallel to the upper surface of the substrate, wherein at least some of the adjacent metal ring structures are spaced apart and surround a first groove; An interlayer dielectric layer is formed, wherein the interlayer dielectric layer is at least located on the upper surfaces of the plurality of metal ring structures and closes the top opening of the first groove to form a first air gap at the first groove, wherein the first air gap serves as the first fragile structure; and the guard ring structure includes the interlayer dielectric layer and the metal ring structure.
14. The method for manufacturing a semiconductor structure according to claim 13, characterized in that: Before forming the interlayer dielectric layer, the method further includes: forming a wrapping layer, wherein the wrapping layer at least covers the sidewall and the upper surface of the metal ring structure; The interlayer dielectric layer also covers a portion of the upper surface of the wrapping layer.
15. The method for manufacturing a semiconductor structure according to claim 12, wherein: Before forming the protection ring structure, the method further includes: forming a second fragile structure in the substrate of the protection zone; the second fragile structure extends in a direction perpendicular to the upper surface of the substrate; The first frangible structure is also formed over the second frangible structure.
16. The method for manufacturing a semiconductor structure according to claim 15, characterized in that: The step of forming the second fragile structure comprises: Etching the substrate along a direction perpendicular to the upper surface of the substrate to form a second groove in the substrate; A covering layer is formed, wherein the covering layer closes the opening at the top of the second groove to form a second air gap at the second groove, wherein the second air gap serves as the second fragile structure.
17. A memory, characterized in that: include: A semiconductor structure as claimed in any one of claims 1 to 11.