Bonding method
The adhesive bonding method configured by the clamp member solves the problem of insufficient coating space for dam materials in narrow-edge display modules, achieves high-quality and high-reliability bonding, and ensures the stability of the adhesive layer.
Patent Information
- Application Number
- CN202410508253.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-04-28
- Filing Date
- 2024-04-25
- Publication Date
- 2024-10-29
AI Technical Summary
It is difficult to ensure high-reliability dam and filling bonding in narrow-edge display modules with the existing technology. Especially when there is no coating space for dam materials, problems such as bubble entry, peeling, and poor display are prone to occur.
Adopt an adhesive bonding method using a clamp member. The adhesive is cured through the first clamp member and the second clamp member to ensure the bonding between the display device and the front panel. After curing, the clamp member is removed and UV cured. The device stabilizes the cured adhesive and prevents filling material from flowing into gaps.
It achieves high-quality and reliable bonding in narrow-edge display modules, avoids bubble entry and peeling problems, and ensures the stability and thickness of the adhesive layer.
Smart Images

Figure CN118870928A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a method for laminating a liquid crystal module or an organic EL display module used in a display such as a television device or a monitor to a cover panel. Background Art
[0002] Patent document 1 discloses a method for manufacturing an organic EL display device, which comprises: an array substrate having an organic EL film and an electrode pattern, and signal lines, scanning lines, and switching elements in an image display area where pixels are arranged in a matrix; an opposing substrate bonded to the array substrate; a dam material configured to surround the image display area; and a filling material to fill a gap surrounded by the array substrate, the opposing substrate, and the dam material.
[0003] Prior Art Literature
[0004] Patent Literature
[0005] Patent Document 1: Japanese Patent Application Publication No. 2015-79580 Summary of the invention
[0006] Problems to be solved by the invention
[0007] The present disclosure has been developed in view of the conventional situation and provides a bonding method that can perform dam and filling bonding even in a narrow-edge display module where there is almost no space for applying a dam material, and can ensure the quality and high reliability of the adhesive layer after bonding.
[0008] Means for solving problems
[0009] The present disclosure provides a bonding method for bonding a front panel having a rectangular shape when viewed from above and a display device by means of an adhesive. In the bonding method, a first clamp member that is arranged in contact with four sides of the display device is arranged on a second clamp member, and the second clamp member is arranged on the back of the display device and has an area larger than that of the display device; a first adhesive that surrounds the display device is applied to the upper part of the first clamp member; a second adhesive is used to fill the inner side of the first adhesive and the portion between the display device and the front panel; the first adhesive and the second adhesive are cured, and the first clamp member and the second clamp member are removed after the curing.
[0010] Effects of the Invention
[0011] According to the present disclosure, even in a display module with a narrow edge where there is almost no space for applying a dam material, dam and filling lamination can be performed, and the quality and high reliability of the adhesive layer after lamination can be ensured. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 It is a cross-sectional view of a display module bonded by a conventional dam and fill method.
[0013] Figure 2 is a cross-sectional view of a narrow edge display module bonded by conventional dam and fill bonding.
[0014] Figure 3 This diagram illustrates the issues that arise when applying dam and fill lamination to narrow-edge display modules.
[0015] Figure 4 This is a schematic cross-sectional view showing a basic structural example of a narrow-edge display module according to Embodiment 1.
[0016] Figure 5 This is a schematic cross-sectional view of the adhesive curing step according to the first embodiment.
[0017] Figure 6 This is a schematic cross-sectional view of the clamp member removing step according to the first embodiment.
[0018] Figure 7 This is a schematic cross-sectional view showing an example of the penetration of the filling material in the narrow-edge display module according to the first embodiment.
[0019] Figure 8 This is a schematic cross-sectional view showing a basic structural example of a narrow-edge display module according to the second embodiment.
[0020] Fig. 9 This is a schematic cross-sectional view showing a basic structural example of a narrow-edge display module according to a modification of the second embodiment.
[0021] Fig.10 This is a schematic cross-sectional view of a display device having a warped shape at one end thereof being bonded together by a dam and filling method in the narrow-edge display module according to the first embodiment.
[0022] Fig.11 It is a schematic cross-sectional view showing an example of measuring a height difference value.
[0023] Fig.12 This is a schematic cross-sectional view showing a basic structural example of a narrow-edge display module according to the third embodiment.
[0024] Explanation of symbols
[0025] 100 Display Module
[0026] 101 Front Panel
[0027] 102 Screen Printing Department
[0028] 103 Display Devices
[0029] 104 Active Area
[0030] 105 Polarizing Plate
[0031] 106 Filling material
[0032] 107 Dam materials
[0033] 108 frame components
[0034] 109 Transmission
[0035] 200 Narrow Edge Display Module
[0036] 201 Edge Width
[0037] 202 Edge
[0038] 300 Narrow Edge Display Module
[0039] 400 Narrow Edge Display Module
[0040] 401 No. 1 fixture component
[0041] 402 Second clamp component
[0042] 403 Upper surface of the first clamp member
[0043] 404 Top Surface
[0044] 500 Narrow Edge Display Module
[0045] 501 Front UV curing device
[0046] 502 Side UV curing device
[0047] 701 Gap
[0048] 702 Gap
[0049] 801 Liquid Storage Unit
[0050] 901 Liquid Storage Unit
[0051] 1001 Adhesive layer thickness
[0052] 1101 Displacement Meter
[0053] 1102 Difference in height between the end of the display device and the first fixture member
[0054] 1103 Laser
[0055] 1104 Laser
[0056] 1105 Upper surface of the end of the display device
[0057] 1106 Upper surface of the first clamp member
[0058] 1201 Display module right area DETAILED DESCRIPTION
[0059] (The process of realizing the present disclosure)
[0060] In recent years, mobile terminals such as smartphones and other portable phones and tablet terminals are often equipped with both touch panels and display devices. Regarding the display devices mentioned here, for example, liquid crystal modules and organic electroluminescence (EL) modules are representative. In the past, the touch panel and the display device were independent components, and the display device was installed inside the housing of the mobile terminal. In addition, the front side of the display device is also equipped with a touch panel as part of the exterior, and generally an air layer is separated between the two components.
[0061] However, in recent years, the technology of bonding these touch panels and display devices with optical adhesives (hereinafter sometimes referred to as "direct bonding") has been established, centered on small displays, and many products have begun to become popular on the market. As the advantages of direct bonding, various advantages can be expected, such as suppression of reflection, improvement of brightness, improvement of strength, prevention of condensation, and prevention of dust mixing.
[0062] However, on the other hand, the shapes and specifications of the touch panels and display devices to be bonded are becoming more and more diverse, and with their diversification, a variety of bonding methods have been proposed. From the material aspect, there are also a variety of materials used for bonding. For example, there is a highly transmittance double-sided adhesive called optical clear adhesive (OCA, Optical Clear Adhesive), a highly transmittance liquid resin called optical clear resin (OCR, Optical Clear Resin), a liquid resin for semi-cured bonding called mixed OCR, etc. On the other hand, as a bonding method, there is also a roller bonding method that uses OCA in an atmospheric environment and is bonded by roller pressurization, and a dam and filling (dam & filling) method that is bonded by OCR and using two types of dam materials and filling materials to extract air in a vacuum environment (for example, refer to patent document 1). In particular, regarding the latter method of bonding in a vacuum environment, it is known that there are advantages such as bubbles are not easy to enter, and even if they enter, the bubbles are easy to disappear in subsequent processes. Therefore, the thickness of the adhesive layer can be freely controlled by freely adjusting the height of the dam material, and highly reliable bonding can be achieved. Therefore, in recent years, this method has been adopted by many manufacturers in industries such as the automotive industry that attach importance to product reliability.
[0063] In general, the dam and filling method can be said to be oriented towards large-scale lamination. The reason for this is that the thickness of the adhesive layer can be freely adjusted by the dam material (hereinafter, sometimes abbreviated as "dam material"). The larger the size becomes, the more the reliability of the adhesive layer when laminating the touch panel and the display device becomes a problem. The adhesive material (such as OCR) used in the dam and filling method is usually selected to be very soft and have a low storage elastic modulus. However, if the adhesive layer is set to be thin, due to the difference in thermal expansion and thermal contraction between the touch panel and the display device, a load will be applied to the adhesive layer between the touch panel and the display device during heating or cooling, and problems such as peeling of the adhesive layer will occur. Therefore, the larger the size becomes, the method of laminating by setting the adhesive layer to be thicker is usually often used. Therefore, in the dam and filling method, the thickness of the adhesive layer can be controlled by applying the dam material thickly, so it is used more with large sizes as the center. However, this method also has disadvantages.
[0064] For example, in recent years, from the perspective of design, narrow-edge displays have become widely popular in final products such as smartphones and tablets. Usually, the dam material is applied to the area outside the image display area (generally referred to as the "active area") of the display device. However, if it becomes a narrow-edge display, the outer area is narrower than the outer area of the image display area of the previous display device, and there is no space for applying the dam material or it becomes infinitely narrow. As a dam material, a material with a refractive index close to that of a filler material (hereinafter, sometimes abbreviated as "filler") is also selected more. The boundary area between the dam material and the filler is mostly invisible to the eye, so sometimes it is manufactured by applying the dam material close to the outside of the screen display area. However, in the surface where two different materials (dam material, filler) are combined, bubbles will enter during manufacturing, or poor appearance such as peeling will occur near its boundary during the reliability test of the product. Therefore, as a product side, the possibility of a bad situation becomes higher. That is, it can be said that the existing bank and filling methods are not suitable for the production of narrow-edge displays. Since it is difficult to ensure space for applying the bank material, there is a problem that it is difficult to apply to the bonding of touch panels and display devices.
[0065] Therefore, the following embodiments describe an example of a bonding method that enables dam and filling bonding even in a narrow display module such as a space without a dam material coating space, and that can ensure the quality and high reliability of the adhesive layer after bonding.
[0066] Below, with appropriate reference to the attached Figure 1While specifically disclosing the embodiments of the bonding method involved in the present disclosure, the present disclosure is described in detail. However, sometimes more detailed descriptions than necessary are omitted. For example, sometimes detailed descriptions of known and familiar matters and repeated descriptions of substantially the same structures are omitted. This is to avoid the following description from becoming unnecessarily lengthy and to make it easy for those skilled in the art to understand. In addition, the drawings and the following description are provided for those skilled in the art to fully understand the present disclosure, and it is not intended that the subject matter described in the scope of the patent claim be limited by these.
[0067] First, before specifically describing an embodiment of the lamination method according to the present disclosure (this embodiment), Figure 1 to Figure 3 , examples of a display module bonded by a general dam and fill method and a narrow edge display module bonded by a dam and fill method are described. Figure 1 1 is a cross-sectional view of a display module 100 bonded by a conventional dam and fill method. Figure 2 is a cross-sectional view of a narrow edge display module 200 that is bonded by a conventional dam and fill bonding.
[0068] Figure 3 This is an explanatory diagram of the problem when lamination is applied to a narrow edge display module 300 by dam and fill lamination.
[0069] In the following description, the up-down and left-right directions of the display are set to the directions shown in the respective drawings. That is, the up-down direction indicates the thickness direction of the display, and the left-right direction indicates the surface direction of the display. Figure 2 as well as Figure 3 In the description of Figure 1 or Figure 2 For repeated elements in the description, the same symbols are given and the description is simplified or omitted to describe different contents.
[0070] 2. Display module bonded by conventional dam and fill method
[0071] Figure 1 The display module 100 shown is composed of a front panel 101 , a display device 103 , a polarizing plate 105 , a filling material 106 , and a dam material 107 .
[0072] Front panel 101 is, for example, a touch panel, cover glass, a resin cover lens, or the like.
[0073] The display device 103 is a liquid crystal panel, an organic EL display, a micro LED display, or the like, and is covered with a portion of the front surface and the entire circumference of the side surfaces by a frame member 108 . Figure 1The front panel 101 and the display device 103 are bonded together by a dam and fill method using a dam material 107 and a filler material 106. Generally, both the dam material 107 and the filler material 106 are mostly made of a highly transmissive adhesive called an optical adhesive, and acrylic resins and silicone resins are the mainstream materials.
[0074] In the dam and fill method, first, a dam material 107 is applied to the image display region (i.e., active region 104) of the display device 103 which is rectangular in plan view, and then a fill material 106 is applied to the region surrounded by the dam material 107, and the front panel 101 is lowered from above for bonding. The dam and fill method itself is a known technology, and thus a detailed description of the manufacturing process is omitted.
[0075] exist Figure 1 In the cross-sectional structure example, the feature lies in the position of the dam material 107. The front panel 101 has a screen printing portion 102 (non-transmissive portion) on the back side (in other words, the lower side) of which the screen printing process is applied, and a transmissive portion 109 for viewing the image of the display device 103. Most general monitor products adopt this method. In addition, the display device 103 has a portion called an active area 104 for displaying an image, and a polarizing plate 105 having an area wider than the active area 104. The polarizing plate 105 is arranged above the active area 104.
[0076] The dam material 107 is applied to the polarizing plate 105 at a position closer to the outer periphery than the active area 104, and is applied to the back side (in other words, the lower side) of the screen printing part 102. That is, the dam material 107 is applied to a position that is not visible when viewed from the outside. This is because the dam material 107 and the filling material 106 are independent materials and have different refractive indexes (however, relatively close materials are selected), so sometimes the contact interface between the dam material 107 and the filling material 106 can be visually confirmed. Therefore, if the contact interface between the dam material 107 and the filling material 106 enters the active area 104, the image quality will be reduced.
[0077] 3. Narrow edge display modules bonded by conventional dam and fill methods
[0078] In recent years, from the perspective of design, the narrowing of the edge of the monitor component has been promoted. It has become very difficult to apply the dam and filling method to such a component, and its structure has become similar to Figure 1 Different ways. For the example of a display module that has been narrowed by the dam and fill method, use Figure 2 as well as Figure 3 To explain.
[0079] Figure 2 The narrow edge display module 200 shown is Figure 1 The display module 100 shown is also composed of a front panel 101, a display device 103, a polarizing plate 105, a filling material 106 and a dam material 107. Figure 3 The narrow edge display module 300 shown is Figure 1 The display module 100 or Figure 2 The narrow edge display module 200 shown is also composed of a front panel 101 , a display device 103 , a polarizing plate 105 , a filling material 106 and a dam material 107 .
[0080] For example, in the narrow edge display module 200, Figure 1 Compared with the display module 100 of FIG. 1 , the edge width 201 of the screen printed portion 102 of the front panel 101 (in other words, the edge width of the front panel) and the edge 202 of the display device 103 are both narrower. The edge 202 of the display device 103 refers to the portion outside the active area 104.
[0081] exist Figure 2 The narrow edge display module 200, with Figure 1 Unlike the display module 100 of FIG. 1 , there is no sufficient space on the polarizing plate 105 for applying the dam material 107. Figure 2 In the narrow edge display module 200, the position of the dam material 107 when the front panel 101 and the display device 103 are attached becomes a position falling on both a part of the outer peripheral end of the polarizing plate 105 and a part of the frame member 108 of the display device 103 on the side of the polarizing plate 105. Here, the frame member 108 is usually mostly a strip or metal, and the strip is the mainstream for small sizes. At this time, in the case where the frame member 108 is a strip, the height of the dam material 107 is unstable due to the wrinkles of the strip, and the thickness of the adhesive layer cannot be made uniform, sometimes causing display defects such as display streaks. In addition, since the dam material 107 is applied across the frame member 108 and the polarizing plate 105, there is an area where three different materials are mixed. Due to the difference in the thermal expansion amount of each component, it becomes a cause of poor product quality such as bright spots that peel or cracks in reliability tests with heat applied. On the other hand, in the bonding method, since only a portion of the dam material 107 is high, the filling material 106 may flow to the outside of the dam material 107, which may cause manufacturing problems such as contamination or damage of the component.
[0082] In addition, compared with the Figure 2 The state of narrow marginalization has been further advanced, using Figure 3 Schematic diagram for illustration.
[0083] exist Figure 3 The narrow edge display module 300, with Figure 2 Compared with the narrow edge display module 200, the edge width 201 of the screen printing part 102 and the edge width 202 of the display device 103 are narrower. Figure 3 The construction example shown. Figure 3 , but depending on the situation, the frame member 108 may be omitted. Figure 3 In the structural example, there is no physical space for applying the dam material 107, and the dam material 107 is almost squeezed out of the display device 103. Therefore, when manufacturing the narrow edge display module 300, there is a problem that the dam and filling method cannot be applied.
[0084] (Implementation Method 1)
[0085] Next, based on Figure 1 to Figure 3 For instructions, refer to Figures 4 to 6 Embodiment 1 of the bonding method according to the present disclosure will be described. Figure 4 1 is a schematic cross-sectional view showing a basic structural example of a narrow-edge display module 400 according to the first embodiment. Figure 5 This is a schematic cross-sectional view of the adhesive curing step according to the first embodiment. Figure 6 1 is a schematic cross-sectional view of the clamp member removal process involved in Embodiment 1. Figures 4 to 6 In the description of Figure 1 to Figure 3 The same symbols are given to repeated elements in the description, and the description is simplified or omitted to describe different contents.
[0086] Figure 4 The narrow edge display module 400 shown in the figure is composed of a front panel 101, a display device 103, a polarizing plate 105, a filler material 106, and a dam material 107. In addition, the dam material 107 may be omitted. Figure 3 The construction example is similar to Figure 2 Compared with the narrow edge display module 200 , the edge width 201 of the screen printing portion 102 and the edge width of the edge portion 202 of the display device 103 are further narrowed.
[0087] 4. Detailed steps of the dam and filling method according to Embodiment 1
[0088] exist Figure 4In the illustrated narrow-edge display module 400 , a dam and filling method (more specifically, a dam and filling bonding method) for bonding a narrow-edge front panel 101 and a narrow-edge display device 103 will be described.
[0089] In Embodiment 1, a first clamp member 401 is disposed around the periphery of the display device 103, and a second clamp member 402 is disposed on the back side (in other words, the lower side) of the display device 103. The first clamp member 401 cooperates with the second clamp member 402. An upper surface 403 of the first clamp member 401 is at the same height as or lower than an upper surface 404 of a polarizing plate 105 disposed on the upper side of an active region 104 of the display device 103. In addition, preferably, the first clamp member 401 and the peripheral side surface of the display device 103 are in contact with each other without a gap. In order to eliminate such a gap, for example, pressing by a spring or the like, or contact by an elastomer or an adhesive can be considered.
[0090] The bonding method using the dam and filling method according to the first embodiment is performed through the following steps.
[0091] (Step 1) Step of mounting the display device 103 using two jig members
[0092] (Step 2) Step of bonding the front panel 101 and the display device 103
[0093] (Step 3) Adhesive curing step for two types of adhesives
[0094] (Step 4) Removal process of two clamp members
[0095] Hereinafter, each step will be described in sequence.
[0096] (Step 1) Step of mounting the display device 103 using two jig members
[0097] The display device 103 is mounted on the first clamp member 401 and the second clamp member 402. Specifically, the outer peripheral side of the display device 103 is held by the first clamp member 401, and in this state, the first clamp member 401 and the display device 103 are arranged on the second clamp member 402. The display device 103 has an active region 104, and a polarizing plate 105 having an area larger than the active region 104 is arranged on the upper side of the display device 103, which is similar to the polarizing plate 105 of FIG. Figure 1 to Figure 3 The construction example has not changed.
[0098] (Step 2) Step of bonding the front panel 101 and the display device 103
[0099] After (step 1), the front panel 101 and the display device 103 are attached by the dam and fill method. At this time, the dam material 107 is applied to the back side (in other words, the lower side) of the screen printing part 102, which is the same as Figure 1 to Figure 3 The structural examples are common. However, the characteristic is that the dam material 107 is applied neither on the polarizing plate 105 nor on the frame member 108, but on the first clamp member 401. In the bonding process based on the dam and filling method (step 2), more specifically, the dam material 107 is first applied. Thereafter, the filling material 106 is applied in the area surrounded by the dam material 107. Thus, the front panel 101 and the display device 103 are bonded.
[0100] (Step 3) Adhesive curing step for two types of adhesives
[0101] After the front panel 101 and the display device 103 are bonded together by the dam and filling method in step 2, the process proceeds to the curing process of the two adhesives (i.e., the dam material 107 and the filling material 106). Figure 4 The adhesive curing process is performed by operating in a state of Figure 5 ).
[0102] The adhesive curing process is implemented by the front UV curing device 501 and the side UV curing device 502. The front UV curing device 501 is arranged at a position opposite to the transmission part 109 of the front panel 101, and the pair of side UV curing devices 502 are arranged at a position opposite to the outer peripheral side of the front panel 101, respectively, with the screen printing part 102 of the front panel 101 as the main subject.
[0103] The front UV curing device 501 is a device for curing the filling material 106 by irradiating UV (i.e., ultraviolet light) through the transmission portion 109 of the front panel 101, thereby reinforcing the components bonded by the filling material 106. The side UV curing device 502 is a device for curing the back side portion (i.e., the portion not irradiated with UV by the front UV curing device 501) of the screen printing portion 102 of the front panel 101 by irradiating UV (i.e., ultraviolet light), thereby reinforcing the portion of the screen printing portion 102 not irradiated with UV by the front UV curing device 501 and the filling material 106.
[0104] Here, since the upper surface 403 of the first clamp member 401 is located below the upper surface 404 of the polarizing plate 105, the UV irradiated from the side UV curing device 502 reaches deep (in other words, penetrates), so that the curing of the adhesive can be stabilized throughout the back side of the screen printing part 102. In addition, the first clamp member 401 is preferably made of a material that transmits UV, such as a transparent body. The UV from the side should be irradiated to a narrow gap, so the UV is transmitted through the first clamp member 401, so that more UV light can be irradiated to the gap on the back side of the screen printing part 102, and the effect of suppressing poor curing of the adhesive (dam material 107, filling material 106) can be obtained.
[0105] In addition, when a UV-curable resin is used for the adhesive (dam material 107, filling material 106), it is preferred to strengthen the adhesive layer by using these two devices (front UV curing device 501, side UV curing device 502). However, when a room temperature curing adhesive is used, these devices (front UV curing device 501, side UV curing device 502) may not be used. In either case, in the bonding method involved in embodiment 1, the feature is that the display device 103 is fixed in position by the first clamp member 401 and the second clamp member 402, and the adhesive (i.e., dam material 107, filling material 106) is cured in the state after the front panel 101 and the display device 103 are bonded by the dam and filling method.
[0106] (Step 4) Removal process of two clamp members
[0107] After (Step 3), a process of removing the two clamp members is performed. This process is a process of removing the bonded narrow-edge display module 400 from the first clamp member 401 and the second clamp member 402 after the adhesive is cured.
[0108] In this process, the first jig member 401 is separated from the narrow display module 400 by the operator in a state where the dam material 107 is applied, or is removed in a state where the dam material 107 remains on the narrow display module 400. In a case where the bonding force between the dam material 107 and the filling material 106 is stronger than the bonding force between the dam material 107 and the first jig member 401, the dam material 107 often remains on one side of the narrow display module 400. In addition, in a case where a gel-like material is selected as the filling material 106, the bonding force between the dam material 107 and the first jig member 401 becomes stronger, and the dam material 107 is separated from the narrow display module 400 in a state where it is adhered to the first jig member 401.
[0109] In the case where the dam material 107 may also remain in the housing of the final product as designed by the final product, by selecting a material with high mold release properties (e.g., silicon, Teflon (registered trademark)) for the first clamp member 401 and applying a mold release agent to the first clamp member 401, the dam material 107 is separated from the first clamp member 401, and the dam material 107 can remain in the housing of the final product. Generally, the dam material 107 is a material required in manufacturing for the dam and filling process, and does not affect the performance of the final product of the narrow edge display module 400. Therefore, the dam material 107 may remain in the housing of the final product or not, which is a matter that can be appropriately determined by the designer and is not limited in the first embodiment. In addition, the first clamp member 401 and the second clamp member 402 can be separated at the same time. By configuring the first clamp member 401 and the second clamp member 402 to be separable, it is possible to obtain an effect that the first clamp member 401 and the second clamp member 402 can be separated from the narrow edge display module 400 very easily, and the adhesive can be easily removed.
[0110] As described above, according to the bonding method involved in Embodiment 1, the dam and filling method can be implemented even for a display member with a narrow edge, and an effect of obtaining a product with high reliability can be achieved.
[0111] (Implementation Method 2)
[0112] Next, refer to Figure 7 to Figure 9 Embodiment 2 of the bonding method according to the present disclosure will be described. Figure 7 This is a schematic cross-sectional view showing an example of the penetration of the filling material in the narrow-edge display module 400 according to the first embodiment. Figure 8 This is a schematic cross-sectional view showing a basic structural example of a narrow-edge display module according to the second embodiment. Fig. 9 2 is a schematic cross-sectional view showing a basic structural example of a narrow edge display module according to a variation of Embodiment 2. Figure 7 to Figure 9 In the description of Figure 1 to Figure 6 The same symbols are given to repeated elements in the description, and the description is simplified or omitted to describe different contents.
[0113] First, refer to Figure 7 , describing the phenomena that may occur when further improving measures are studied for the bonding method involved in Implementation Example 1.
[0114] In the bonding method according to Embodiment 1, there is a step of applying the filling material 106 after applying the dam material 107 (see step 2). When the filling material 106 is applied around the dam material 107, the filling material 106 may fall into the gap 701 between the display device 103 and the first jig member 401 due to the capillary phenomenon, and may penetrate into the gap 702 between the display device 103 and the second jig member 402.
[0115] This usually depends on the viscosity of the filling material 106. For example, the lower the viscosity of the filling material 106, the higher the possibility of the above-mentioned penetration phenomenon. When the penetration phenomenon occurs, in the process of finally separating the first clamp member 401 and the second clamp member 402 from the narrow edge display module 400, it is difficult to separate the first clamp member 401 and the second clamp member 402 due to the surface tension of the filling material 106, and an external load may be applied to the narrow edge display module 400 during separation. In particular, among the components constituting the narrow edge display in recent years, there are many thin components, which are easily damaged by external loads.
[0116] Therefore, in the following second embodiment, a structural example in which the above-mentioned penetration phenomenon is less likely to occur in a narrow-edge display module manufactured by the bonding method according to the first embodiment will be described.
[0117] 5. Detailed steps of the dam and filling method involved in embodiment 2
[0118] The detailed procedures of the dam and the filling method according to the second embodiment are almost the same as those of the dam and the filling method according to the first embodiment. The contents different from the first embodiment will be described in detail below.
[0119] Figure 8 The narrow edge display module 500 shown in the figure is composed of a front panel 101, a display device 103, a polarizing plate 105, a filler material 106, and a dam material 107. In addition, the dam material 107 may be omitted. Figure 3 or Figure 4 The construction example is similar to Figure 2 Compared with the narrow edge display module 200 , the edge width 201 of the screen printing portion 102 and the edge width of the edge portion 202 of the display device 103 are further narrowed.
[0120] In Embodiment 2, unlike Embodiment 1, a liquid reservoir 801 is provided in the second jig member 402. The liquid reservoir 801 can be provided as a recessed portion formed by cutting out a part of the second jig member 402 in a quadrangular prism shape in a plan view.
[0121] exist Figure 8 In the example, the liquid storage portion 801 is provided in a shape engraved into the second clamp member 402. The liquid storage portion 801 is preferably provided in an area close to the peripheral end side of the display device 103, for example. By configuring in this way, the filling material 106 that flows through the gap 701 between the display device 103 and the first clamp member 401 can be accumulated in the liquid storage portion 801. Therefore, the liquid storage portion 801 functions as a structure for blocking the filling material 106, and can prevent the filling material 106 from flowing into the gap 702 between the display device 103 and the second clamp member 402, and can be removed without applying an external load to the display device 103 during the removal process of the first clamp member 401 and the second clamp member 402 (refer to step 4).
[0122] Fig. 9 The narrow edge display module 600 shown is Figure 8 The narrow edge display module 500 shown in FIG. 1 is similarly composed of the front panel 101, the display device 103, the polarizing plate 105, the filler material 106, and the dam material 107. In addition, the dam material 107 may be omitted. Figure 3 or Figure 4 The construction example is similar to Figure 2 Compared with the narrow edge display module 200 , the edge width 201 of the screen printing portion 102 and the edge width of the edge portion 202 of the display device 103 are further narrowed.
[0123] In addition, the liquid storage part according to the second embodiment is not limited to Figure 8 The example shown can also be used Fig. 9 The liquid storage portion 901 is set as shown.
[0124] exist Fig. 9 In the example, a plurality of steps (e.g., two steps on each side) are pre-formed on the second clamp member 402, and the first clamp member 401 is placed on the surface of the outermost step (i.e., the lowermost step), and the inner step portion is set as the liquid storage portion 901. Fig. 9 In the construction example, the filling material 106 that flows through the gap 701 between the display device 103 and the first clamp member 401 can be prevented from flowing into the gap 702 between the display device 103 and the second clamp member 402. In the removal process of the first clamp member 401 and the second clamp member 402 (refer to step 4), the removal can be performed without applying an external load to the display device 103.
[0125] As described above, according to the bonding step according to the second embodiment, it is possible to obtain an effect of suppressing defects caused by external loads in the manufacturing process.
[0126] (Implementation 3)
[0127] Next, refer to Figure 10 to Figure 12 Embodiment 3 of the bonding method according to the present disclosure will be described. Fig.10 This is a schematic cross-sectional view of a display device having one end side warped and bonded together by a dam and filling method in the narrow-edge display module 400 according to the first embodiment. Fig.11 It is a schematic cross-sectional view showing an example of measuring a height difference value. Fig.12 2 is a schematic cross-sectional view showing a basic structural example of a narrow edge display module 700 according to Embodiment 3. Figure 10 to Figure 12 In the description of Figures 1 to 9 The same symbols are given to repeated elements in the description, and the description is simplified or omitted to describe different contents.
[0128] First, refer to Fig.10 , which explains a phenomenon that may occur when further improving measures are studied for the bonding method involved in Embodiment 1. For example, when the bonding method involved in Embodiment 1 is used, a display device with one end side of the display device 103 warped may be used. This is caused, for example, by manufacturing deviations of the display device 103, and can be said to be an unavoidable issue.
[0129] like Fig.10 As shown in FIG. 1 , when one end of the display device 103 is warped, the height of the dam material 107 becomes a given height only according to the heights of the second clamp member 402 and the first clamp member 401. Therefore, a phenomenon occurs in which the thickness h1 of the adhesive layer (dam material 107, filler material 106) on the warped end side (right side) is thinner than the thickness h2 of the adhesive layer (dam material 107, filler material 106) on the other end side (left side) that is not warped.
[0130] In particular, the dam and filling method of the direct bonding technology has the advantage that the thickness of the adhesive layer can be controlled and a thick adhesive layer can be formed, which can achieve highly reliable bonding. However, if a thin adhesive layer is locally present, the reliability will be reduced. Therefore, when the warped display device 103 is bonded, if the bonding method involved in Embodiment 1 is used, a disadvantage will occur.
[0131] Therefore, in the following third embodiment, this disadvantage is solved and an example is described in which an adhesive layer having a predetermined thickness is formed over the entire outer peripheral side surface of the display device 103 even when a warped display device 103 is used.
[0132] 6. Detailed steps of the dam and filling method involved in embodiment 3
[0133] The detailed procedures of the dam and the filling method according to the third embodiment are almost the same as those of the dam and the filling method according to the first embodiment. The contents different from the first embodiment will be described in detail below.
[0134] exist Fig.11 In the embodiment, the display device 103 has a partially warped and deformed portion at one end thereof. In this state, the display device 103 is mounted on the first clamp member 401 and the second clamp member 402 in the same manner as in the first embodiment. In the third embodiment, a displacement meter 1101 is provided for measuring the height of both the upper surface 1105 of the end of the display device 103 and the upper surface 1106 of the first clamp member 401 in this state. In addition, the height mentioned here means, for example, the height from the bottom surface of the second clamp member 402.
[0135] The displacement meter 1101 is preferably a non-contact type such as a laser displacement meter. For example, in the case of a laser displacement meter, the height of the upper surface 1105 of the end of the display device 103 is measured based on the time of the outgoing and returning paths of the laser 1103 irradiated from the displacement meter 1101 and the speed of the laser 1103. Similarly, the height of the upper surface 1106 of the first clamp member 401 is measured based on the time of the outgoing and returning paths of the laser 1104 irradiated from the displacement meter 1101 and the speed of the laser 1104. Thus, information on the difference in height (thickness h3) between one end of the locally warped display device 103 and the first clamp member 401 can be derived.
[0136] In addition, instead of a laser displacement meter, a contact-type displacement meter or the like can be used, but the displacement measuring means is not limited in the third embodiment.
[0137] In addition, the third embodiment is characterized in that the height difference (thickness h1) between the display device 103 and the first jig member 401 is reflected in the height setting of the dam material 107 to be applied later. That is, if the height difference is large, feedback is performed so that the dam material 107 on the side of the partially warped end of the display device 103 is applied higher by the height difference (thickness h3) than the height (given setting value) of the dam material 107 on the side that is not warped.
[0138] In the dam and filling method, the dam material 107 is usually applied from a dispenser, and a higher dam can be formed by increasing the amount of the dispenser sprayed or slowing down the moving speed of the dispenser. Fig.12 .
[0139] exist Fig.12In the figure, the right bank material 107a is applied higher than the left bank material 107 by the difference in height (thickness h3) between the display device 103 and the first fixture member 401. Thus, it is found that a thick adhesive layer can be formed also in the right end region 1201, thereby improving product reliability.
[0140] As described above, according to the bonding method involved in Embodiment 3, the warping of the display device 103 can be taken into consideration and adjusted so that the heights of the dam materials used in the dam and filling methods are the same or different. Therefore, the problem of thinning the thickness of the adhesive layer due to the warping of the display device 103 can be solved, and a highly reliable mutual bonding structure that is a feature of the dam and filling method can be provided.
[0141] As described above, the present disclosure discloses the following technical ideas.
[0142] <Technology 1>
[0143] A bonding method is provided for bonding a front panel (101) and a display device (103) which are rectangular in plan view by means of adhesives (107, 106). In the bonding method, a first clamp member (401) which is arranged in contact with four sides around the display device is arranged on a second clamp member (402), the second clamp member (402) being arranged on the back of the display device and having an area larger than that of the display device, a first adhesive (107) which surrounds the display device is applied to the upper part of the first clamp member, a second adhesive (106) is applied to fill the inner side of the first adhesive and the portion between the display device and the front panel, the first adhesive and the second adhesive are cured, and the first clamp member and the second clamp member are removed after the curing.
[0144] Thus, according to the lamination method, even in a display module with a narrow edge such as a space where there is no application space for the dam material, dam and filling lamination can be performed, and the quality and high reliability of the adhesive layer after lamination can be ensured.
[0145] <Technology 2>
[0146] According to the bonding method described in Technology 1, the front panel has: a transmissive portion (109) that enables visual identification of an image from the display device; a non-transmissive portion (102) that is arranged around the transmissive portion and has a width that is smaller than the width of the transmissive portion, and the first adhesive bonds the upper portion of the first clamp member and the lower portion of the non-transmissive portion.
[0147] Thus, according to the lamination method, even if the edge of the front panel is narrowed, the adhesive layer between the front panel and the display device can be formed stably and with high quality.
[0148] <Technology 3>
[0149] According to the bonding method described in the first or second technique, the first jig member and the display device are in contact with each other without a gap.
[0150] Therefore, according to the bonding method, it is possible to prevent the filling material from falling into between the display device and the first and second clamp members.
[0151] <Technique 4>
[0152] According to the bonding method described in any one of Technologies 1 to 3, a polarizing plate having an area larger than that of the image display area is placed on the upper surface of the image display area of the display device, and the upper surface of the first clamp member is lower than the upper surface of the image display area of the display device on which the polarizing plate is placed.
[0153] Thus, according to the bonding method, stable curing of the filling material can be provided in response to UV irradiation from the side.
[0154] <Technique 5>
[0155] According to the bonding method described in any one of techniques 1 to 4, a liquid reservoir (801, 901) is provided on the end side of the display device and on the second clamp member, and the liquid reservoir prevents the second adhesive from flowing into the bottom surface of the display device.
[0156] Thus, according to the bonding method, it is possible to prevent the second adhesive (ie, the filler 106 ) from flowing into the bottom surface of the display device 103 .
[0157] <Technique 6>
[0158] According to the bonding method described in any one of Technologies 1 to 5, a first height representing the height of the upper surface of the end of the display device and a second height representing the height of the upper surface of the first clamp member are respectively measured, and the difference between the first height and the second height is derived, and the derived value of the difference is set as the height of at least one side of the first adhesive.
[0159] Thus, according to the bonding method, even when the display device 103 is partially warped and deformed, the thickness of the adhesive layer can be kept substantially constant in the entire display device 103, thereby suppressing degradation of product reliability.
[0160] <Technique 7>
[0161] According to the bonding method described in any one of techniques 1 to 6, the first adhesive is a dam material, and the second adhesive is a filler material.
[0162] Thus, according to the lamination method, a well-known dam and filling method can be used, and a high-quality adhesive layer can be realized.
[0163] The above, while referring to the attached Figure 1 While various embodiments are described, the present disclosure is not limited to these examples. If it is a person skilled in the art, various modification examples, correction examples, substitution examples, additional examples, deletion examples, and equivalent examples can be thought of within the scope of the scope of the patent claim, which is self-evident, and it should be understood that these also belong to the scope of the technology disclosed in the present disclosure. In addition, the various constituent elements in the above-mentioned various embodiments can also be arbitrarily combined within the scope of the main purpose of the invention.
[0164] Industrial Applicability
[0165] The present disclosure can be applied to bonding a narrow-edge type front panel (eg, cover glass or touch panel) and a display device (eg, liquid crystal module) where there is almost no space for applying a dam material.
Claims
1. A bonding method, wherein a front panel having a rectangular shape when viewed from above and a display device are bonded together by an adhesive, wherein: The first clamp member disposed in contact with four sides of the display device is disposed on a second clamp member, wherein the second clamp member is disposed on the back side of the display device and has an area larger than that of the display device. applying a first adhesive to surround the display device on the upper portion of the first fixture member, The second adhesive fills the inner side of the first adhesive and the portion between the display device and the front panel. The first adhesive and the second adhesive are cured, and after the curing, the first clamp member and the second clamp member are removed.
2. The laminating method according to claim 1, wherein: The front panel has: a transmissive portion that enables visual recognition of an image from the display device; and a non-transmitting portion disposed around the transmitting portion and having a width smaller than that of the transmitting portion, The first adhesive bonds the upper portion of the first clamp member and the lower portion of the non-transmitting portion.
3. The laminating method according to claim 1, wherein: The first clamp member is in contact with the display device without a gap.
4. The laminating method according to claim 1, wherein: A polarizing plate having an area larger than that of the image display area is placed on the upper surface of the image display area of the display device. The upper surface of the first clamp member is lower than the upper surface of the image display region of the display device on which the polarizing plate is placed.
5. The laminating method according to claim 1, wherein: A liquid reservoir is provided on the second clamp member at an end portion of the display device, and the liquid reservoir prevents the second adhesive from flowing into the bottom surface of the display device.
6. The lamination method according to any one of claims 1 to 5, wherein: measuring a first height indicating the height of the upper surface of the end portion of the display device and a second height indicating the height of the upper surface of the first clamp member, respectively; A difference between the first height and the second height is derived, and a value of the derived difference is set as at least one height of the first adhesive.
7. The laminating method according to claim 1, wherein: The first adhesive is a dam material, and the second adhesive is a filling material.