Photoresist layer defect detection method

By using multi-layer photoresist layer detection and large particle inspection methods in semiconductor manufacturing, the problem of difficulty in identifying the cause of photoresist layer defects is solved, fast and accurate defect location is achieved, and the continuity and quality of the semiconductor process is ensured.

CN118872036APending Publication Date: 2024-10-29BEIJING ADVANCED MEMORY TECH CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380024154.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-07-28
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

It is difficult to quickly and accurately find out the cause of defects in the photoresist layer (PR layer) with existing technology, which affects the smooth progress of subsequent semiconductor integrated circuit manufacturing processes.

Method used

Through a series of detection steps, including forming and detecting multi-layer photoresist layers, using strong light flashlight irradiation and large particle detection, combined with the processing steps of the lithography machine and detection machine, we can gradually eliminate the defects in the lithography machine and chamber. problem and determine the cause of the defect.

Benefits of technology

It can quickly and accurately find out the causes of PR layer defects, ensure the smooth progress of subsequent processes, and avoid production interruptions and quality problems caused by defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118872036A_ABST
    Figure CN118872036A_ABST
Patent Text Reader

Abstract

A photoresist layer defect detection method comprises: a product wafer defect detection step (S100): forming a first photoresist layer (11) on the surface of a product wafer (10), and determining whether there is a defect (12); a machine testing parameter confirmation step (S200): confirming whether the machine testing parameters are normal or not; a testing machine wafer defect detection step (S300): forming a third photoresist layer (22) on the surface of the testing machine wafer (20), and determining whether there is a defect; a large defect detection step (S400): using a glare flashlight to irradiate the surface of the product wafer (10) to confirm whether there is a large defect; an idle running step (S500): putting the machine testing wafer (20) into each chamber of the photoetching machine, performing other treatment except for coating the photoresist, and determining whether large particles exist or not; a re-detection step (S600): forming a fourth photoresist layer (13) on the surface of the product wafer (10), and determining whether there is a defect; and a determination step (S700) for determining the cause of the defect (12). The detection method can quickly and accurately find out the cause of the defect of the photoresist layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor integrated circuit manufacturing, and in particular to a method for detecting photoresist layer defects. Background Art

[0002] In the prior art, the photolithography process needs to form a PR (photoresist) layer on the surface of the wafer first. However, due to various reasons, defects may appear in certain locations of the PR layer, such as PR peeling, etc. These defects will affect the subsequent processes. In order to eliminate the defects of the PR layer, the cause of the defects must be found out first. Therefore, how to quickly and accurately find out the cause of the defects in the PR layer has become an urgent problem to be solved in the industry. Summary of the invention

[0003] The present invention aims to provide a PR layer defect detection method capable of quickly and accurately finding out the cause of defects in the PR layer.

[0004] The detection method of the present invention comprises:

[0005] Product wafer defect detection step: forming a first photoresist layer on the surface of the product wafer by a photolithography machine, and detecting the first photoresist layer by a detection machine to confirm whether there are defects;

[0006] Test machine parameter confirmation step: if the defect exists, confirm the previous test machine parameters to confirm whether the test machine parameters of the second photoresist layer on the surface of the test machine wafer are normal;

[0007] Test wafer defect detection step: if the test parameters of the second photoresist layer are normal, a third photoresist layer is formed on the surface of the test wafer by the photolithography machine, and the third photoresist layer is detected by the detection machine to confirm whether there are defects;

[0008] Large defect detection step: if the third photoresist layer does not have defects, use a strong light flashlight to illuminate the surface of the product wafer to confirm whether there are large defects;

[0009] Empty run step: if there are no large defects on the surface of the product wafer, the test wafer is placed in each chamber of the photolithography machine, and other treatments are performed except for photoresist coating, and the test wafer is tested for large particles by the inspection machine to confirm whether there are large particles;

[0010] Re-detection step: if there are no large particles, remove the first photoresist layer on the surface of the product wafer, then form a fourth photoresist layer on the surface of the product wafer by the photolithography machine, and detect the fourth photoresist layer by the detection machine to confirm whether there are defects;

[0011] Judgment step: Determine the cause of the defect.

[0012] The PR layer defect detection method of the present invention can quickly and accurately find out the cause of the PR layer defects, thereby ensuring the smooth progress of subsequent processes. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 is a flow chart of a PR layer defect detection method of the present invention;

[0014] Figure 2 is a schematic cross-sectional view of the first PR layer of the product wafer of the present invention;

[0015] Figure 3 is a cross-sectional schematic diagram of the second PR layer of the tester wafer of the present invention;

[0016] Figure 4 is a cross-sectional schematic diagram of the third PR layer of the tester wafer of the present invention; and

[0017] Figure 5 It is a cross-sectional schematic diagram of the fourth PR layer of the product wafer of the present invention.

[0018] Explanation of symbols

[0019] 10 Product Wafers

[0020] 11First PR layer

[0021] 12 Defects

[0022] 13Fourth PR layer

[0023] 20 tester wafers

[0024] 21 Second PR layer

[0025] 22Third PR layer DETAILED DESCRIPTION

[0026] Refer to the following Figures 1 to 5 The PR layer defect detection method of the present invention is described.

[0027] like Figure 1 As shown, the PR layer defect detection method of the present invention includes: product wafer defect detection step S100, test machine parameter confirmation step S200, test machine wafer defect detection step S300, large defect detection step S400, empty run step S500, re-detection step S600, and judgment step S700. These steps are described in detail below.

[0028] Product wafer defect detection step S100: Figure 1 and Figure 2As shown, a first PR layer 11 is formed on the surface of a product wafer 10 by a photolithography machine, and the first PR layer 11 is inspected by a detection machine to confirm whether there are defects 12 .

[0029] In this embodiment, the lithography machine is the XT-1950Hi of ASML of the Netherlands, and the inspection machine is the automatic optical inspection machine KT 89200ADI. However, the present invention is not limited to this, and the lithography machine and the inspection machine may also be other machines. The first PR layer may be formed by the commonly used methods in the art. In this embodiment, the method for forming the first PR layer is to place the product wafer 10 into each chamber of the lithography machine, and sequentially perform cleaning, cooling, PR coating, baking, edge washing, exposure, baking, cooling, and development. The method for coating PR may be to first coat a layer of BAK (anti-reflection) layer on the surface of the product wafer 10, then coat a layer of PR on the surface of the BAK layer, and finally coat a layer of ITC (waterproof) layer on the surface of the PR. The detection steps may include: exposure accuracy detection and defect detection. In addition, in this embodiment, defect 12 refers to PR peeling off at certain positions.

[0030] Test machine parameter confirmation step S200: Figure 1 and Figure 3 As shown, if there is a defect 12 , the previous test parameters are confirmed to confirm whether the test parameters of the second PR layer 21 on the surface of the test wafer 20 are normal.

[0031] Before forming the first PR layer 11 of the product wafer 10, a test machine is usually performed, that is, a second PR layer 21 is formed on the surface of the test machine wafer 20 using a photolithography machine. The method and process parameters for forming the second PR layer 21 are exactly the same as those for forming the first PR layer 11. Then the test machine parameters of the second PR layer 21 are detected to confirm that everything is normal with the photolithography machine. Therefore, when there is a defect 12 on the surface of the product wafer 10, the previous test machine parameters should be confirmed first. In this embodiment, the test machine parameters are all normal, which means that everything is normal with the photolithography machine during the test machine.

[0032] Wafer defect detection step S300: Figure 1 and Figure 4 As shown, if the test parameters of the second PR layer 21 are normal, a third PR layer 22 is formed on the surface of the test wafer 20 by a photolithography machine, and the third PR layer 22 is tested by a testing machine to confirm whether there are defects.

[0033] In this step, in order to confirm whether the photolithography machine is normal at this time, the test machine wafer 20 is used to apply PR again and perform inspection. The method and process parameters used to form the third PR layer 22 are exactly the same as those used to form the first PR layer 11. This can better restore the situation when the first PR layer 11 is formed. In this embodiment, it is detected that there are no defects in the third PR layer 22. This shows that the photolithography machine is also normal at this time. It can be judged that the defect 12 is not caused by the photolithography machine. In addition, the third PR layer 22 on the surface of the test machine wafer 20 must be removed at last so that the test machine wafer 20 can be used next time.

[0034] Large defect detection step S400: If there is no defect in the third PR layer 22, a strong flashlight is used to illuminate the surface of the product wafer 10 to confirm whether there is a large defect.

[0035] Through this step, it can be confirmed whether there are defects such as large particles visible to the naked eye on the surface of the product wafer 10. In this embodiment, there are no large defects, that is, there are no defects such as large particles visible to the naked eye on the surface of the product wafer 10.

[0036] Empty run step S500: If there are no large defects on the surface of the product wafer 10, the test wafer 20 is placed in each chamber of the photolithography machine, and other treatments except PR coating are performed, and the test wafer 20 is inspected by the inspection machine to confirm whether there are large particles.

[0037] In this step, the test wafer 20 is placed in each chamber of the photolithography machine, and is sequentially cleaned, cooled, baked, edge washed, exposed, baked, cooled, developed and other processes are performed, except that PR coating is not performed. However, the test wafer 20 is also placed in the PR coating chamber of the photolithography machine for other processes, except that BAK, PR and ITC are not coated on the test wafer 20.

[0038] This is done to confirm whether there are large particles in the chamber of the lithography machine. If there are large particles, after the test machine wafer 20 enters the various chambers of the lithography machine, these large particles will fall on the surface of the test machine wafer 20 and be detected in the subsequent steps, which means that the large particles in the various chambers of the lithography machine cause the surface defect 12 of the product wafer 10. In this embodiment, after detection, there are no large particles on the surface of the test machine wafer 20. This shows that there are no large particles in each chamber of the lithography machine. It can be judged that the defect 12 is not caused by the presence of large particles in each chamber of the lithography machine.

[0039] Re-detection step S600: If there are no large particles, remove the first PR layer 11 on the surface of the product wafer 10, then form a fourth PR layer 13 on the surface of the product wafer 10 by a photolithography machine, and detect the fourth PR layer 13 by a detection machine to confirm whether there are defects 12'.

[0040] In this embodiment, the method and process parameters for forming the fourth PR layer 13 are exactly the same as those for forming the first PR layer 11. Then the fourth PR layer 13 is inspected and it is found that there is still a defect 12', and the position of the defect 12' is exactly the same as that of the previous defect 12.

[0041] Determination step S700: determine the cause of defect 12.

[0042] In this embodiment, the position of defect 12' is exactly the same as that of the previous defect 12, which indicates that the cause of the defect is not the PR layer, but the surface of the product wafer 10 under the PR layer. Because if it is caused by the PR layer itself, the position of the defect should be random. The positions of the two defects are exactly the same, which indicates that the problem lies in the position corresponding to the defect 12 on the surface of the product wafer 10. There may be oil stains at this position, or the surface of the product wafer 10 at this position may be uneven, which makes it impossible for PR to stick to this position on the surface of the product wafer 10, thus causing the PR to peel off at this position.

[0043] It can be judged that the cause of defect 12 is a previous process, that is, the process of forming the top layer of product wafer 10. In this embodiment, the top layer of product wafer 10 is a TiN (titanium nitride) layer, so there is a problem in the process of forming the TiN layer, resulting in oil stains or uneven bumps at the position corresponding to defect 12 in the formed TiN layer. In this way, the cause of the defect in the PR layer is found.

[0044] Therefore, the PR layer defect detection method of the present invention can quickly and accurately find out the cause of the PR layer defects, thereby ensuring the smooth progress of subsequent processes.

[0045] Although the present invention has been disclosed in the above embodiments, it is not intended to limit the present invention. Any professional and technical personnel in the field may make various necessary changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention shall be based on the scope defined by the attached claims.

Claims

1. A method for detecting photoresist layer defects, comprising: Product wafer defect detection step S100: forming a first photoresist layer (11) on the surface of the product wafer (10) by a photolithography machine, and detecting the first photoresist layer (11) by a detection machine to confirm whether there are defects (12); Test machine parameter confirmation step S200: if the defect (12) exists, confirm the previous test machine parameters to confirm whether the test machine parameters of the second photoresist layer (21) on the surface of the test machine wafer (20) are normal; Test machine wafer defect detection step S300: if the test machine parameters of the second photoresist layer (21) are normal, a third photoresist layer (22) is formed on the surface of the test machine wafer (20) by the photolithography machine, and the third photoresist layer (22) is detected by the detection machine to confirm whether there are defects; Large defect detection step S400: if the third photoresist layer (22) does not have defects, use a strong light flashlight to illuminate the surface of the product wafer (10) to confirm whether there are large defects; Empty run step S500: if there are no large defects on the surface of the product wafer (10), the test wafer (20) is placed in each chamber of the photolithography machine, and other treatments are performed except for photoresist coating, and the test wafer (20) is tested for large particles by the detection machine to confirm whether there are large particles; Re-detection step S600: if no large particles exist, the first photoresist layer (11) on the surface of the product wafer (10) is removed, and then a fourth photoresist layer (13) is formed on the surface of the product wafer (10) by the photolithography machine, and the fourth photoresist layer (13) is detected by a detection machine to confirm whether there are defects; Determination step S700: Determine the cause of the defect (12).