Manufacturing method for exterior decoration effect of thick glass fiber coating film
Through multi-layer structure design and resin selection, combined with UV curing and coating technology, the problem of low transparency and texture of glass fiber material is solved, and the thin, easy processing and diverse decorative effects of glass fiber thick coating are achieved, satisfying the high-end texture and The demand for stable performance.
Patent Information
- Application Number
- CN202410819963.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-24
- Publication Date
- 2024-11-05
AI Technical Summary
Glass fiber materials have low transparency and texture defects in the high-end texture industry, making it difficult to achieve beautiful and stable coating decorative effects, especially in terms of anti-fall, wear, chemical corrosion and complex design.
Using a multi-layer stacked structure design, including primer layer, primer layer, inner texture layer, coating layer, logo layer and outer texture layer, using different types of resin and coating technology, combining UV curing and evaporation sputtering coating to ensure adhesion , water blocking capability and optical effects, suitable for 2D and 3D mobile phone back covers.
It realizes lightweight, easy to process and diversified decoration effects, while meeting performance stability and strict performance testing standards, improving the aesthetics and yield of the product, covering up fiberglass texture problems, and enhancing scratch resistance, wear resistance and Resistance to chemical corrosion.
Smart Images

Figure CN118892976A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of glass fiber thick coating, in particular to a method for producing glass fiber thick coating external decorative effect. Background Art
[0002] With the development of the electronic decoration industry, the market demand for mobile devices is growing, especially in terms of lightweight, beautiful, and drop resistance. Although glass fiber (glass fiber) materials are widely used in many fields due to their advantages of good rigidity, high toughness and lightweight, the problems of glass fiber materials limit their application potential in industries with high-end texture requirements such as mobile phones. Specifically, the transparency of glass fiber materials on the market is generally low, usually not exceeding 89%, and there are defects such as glass fiber grain. These problems affect the visual effect and tactile experience of the product. Therefore, how to maintain the original advantages of glass fiber materials while improving their transparency, eliminating glass fiber texture, and achieving beautiful and stable performance decorative effects on the glass fiber surface has become an important challenge facing the industry.
[0003] In response to this problem, existing solutions often fail to fully meet market demand, especially in terms of coating decoration. How to achieve decorative effects with metallic luster, colorful colors and rich textures on glass fiber and ensure its stable performance has become a key technical problem that needs to be solved urgently. Traditional single coating or simple treatment methods are difficult to solve the low transparency and surface texture problems of glass fiber materials while ensuring the decorative effect. In addition, in practical applications, such as the back cover of a mobile phone, it is also necessary to consider whether it can pass performance tests such as drop resistance, wear resistance, and chemical corrosion resistance, as well as whether it can adapt to the needs of complex designs such as 2D and 3D. As a result, these traditional technologies cannot meet the market's comprehensive requirements for the appearance and performance of mobile devices. Summary of the invention
[0004] The purpose of the present invention is to provide a method for producing a glass fiber thick coating external decorative effect to solve the problems raised in the background technology.
[0005] To achieve the above purpose, the present invention discloses a laminated structure and preparation process for preparing special textures and coatings on the surface of glass fiber, which is light, thin, easy to process, has various effects and stable performance, and is suitable for most 2D & 3D mobile phone back covers on the market.
[0006] The glass fiber substrate described in the above structure can be a 2D or 3D structure, and the glass fiber can also be replaced by a material woven from one or two of carbon fiber, aramid fiber, and basalt fiber. Coating one, primer layer 1 can be one of polyurethane, epoxy resin, acrylic resin, etc. or a combination thereof, and is required to have good adhesion to the glass fiber substrate, and preferably have good water-blocking ability and small curing shrinkage. Coating two, primer layer, can be one of polyurethane, epoxy resin, acrylic resin, etc. or a combination thereof, and is required to have good adhesion to coating one, have certain water-blocking ability, small curing shrinkage, strong covering ability, etc., and can have obvious covering effect on the glass fiber grain of the glass fiber substrate. And it needs to cooperate with the coating layer to present the optical effect specified by the design, such as high-brightness silver, gradient optical plating, solid color optical plating and other coating effects. Coating three, inner texture layer - UV glue, using UV curing glue, the main resin can be one or more of acrylic light curing resin, unsaturated polyester, polyurethane, polyether, thiol / thioether, etc., and it is required to have good adhesion with evaporation coating or sputtering coating, no cracking, good coating performance, etc. Coating layer, the coating layer can be used for decorative effect according to design or cost requirements using coating methods such as evaporation coating and sputtering coating. Coating four, primer layer 2 can be one or more of polyurethane, epoxy resin, acrylic resin, etc., and it is required to have good adhesion with the coating layer, high hardness, excellent weather resistance and anti-aging performance, and can be colorless and transparent or colored semi-transparent, but it will not cause significant corrosion to the coating layer and cause discoloration. Logo layer, using decorative inks such as mirror silver and inkjet ink, prepared on coating four by silk screen printing or spray printing, requiring good adhesion, significant logo, low curing temperature, etc. Coating five, primer layer 3 can be one of polyurethane, epoxy resin, acrylic resin, etc. or a combination thereof. It is required to have good adhesion with highly cured coating four and logo layer, high hardness, excellent weather resistance and anti-aging performance, and can be colorless transparent or colored semi-transparent paint. Coating six, outer texture layer - UV glue, uses UV curing glue, the main resin can be one of acrylic light curing resin, unsaturated polyester, polyurethane, polyether, thiol / thioether, etc. or a combination thereof. It is required to have good adhesion with coating five, high hardness after curing, scratch resistance, anti-fouling, good wear resistance, high toughness, weather resistance, anti-aging, chemical resistance, high water resistance, etc.
[0007] Preferably, the glass substrate is a woven fiber material with a gram weight of 100g, coated with epoxy resin, and has a thickness of 0.5mm after curing and molding, which has price advantages and strong rigidity;
[0008] Preferably, the coating layer 1, primer layer 1 uses polyurethane resin paint; it is processed by silk screen printing or spraying, such as 3D glass fiber substrate, using spraying process, the paint viscosity is 10 to 10.5s, and baking is 80℃ / (15 to 20)min, which is conducive to its adhesion to the glass fiber substrate. The cured film thickness is 15 to 20um, and the filler content in the paint needs to be less than 10% of the resin mass, so that the coating has high adhesion and water-blocking ability.
[0009] Preferably, for coating 2, the primer layer uses polyurethane resin and slow-drying paint; it is processed by silk screen printing or spraying, such as 3D glass fiber substrate, using spraying process, paint viscosity 9-10s, baking 80℃ / (25-30)min, which is conducive to its adhesion with coating 1, and it can be cured to facilitate the processing needs of coating 3, and the cured film thickness is 12-18um. Secondly, the filler content needs to be controlled. For example, fillers such as titanium dioxide are recommended to be 20% to 30% of the resin mass content, which can prevent problems such as oil accumulation and orange peel from occurring during processing, and has high concealment ability.
[0010] Preferably, coating three, inner texture layer - UV glue, uses acrylic light-curing resin; roller transfer or spraying processing, such as 3D glass fiber substrate, using spraying process, glue viscosity 9.5 ~ 10s, baking 65 ℃ / (5 ~ 10) min, curing molding film thickness 20 ~ 25um, the hardness range after curing is recommended to be controlled within 1H ~ 2H, which can reduce the cracking of the coating layer, while meeting the requirements of thick coating, such as hardness reaches 2H, the coating thickness can be 400nm without cracking, so that a wider coating film system can be used. The inner texture can use optical textures, such as CD, SG, light column, etc.; it is more recommended to use textures with style, such as marble, haze, water ripples, etc., because these textures have a certain degree of haze, which can cover some defects and improve the yield of mass production. The texture is processed by profiling rubbing using materials such as silicone and TPU.
[0011] Preferably, coating 4, primer layer 2 uses polyurethane resin paint, screen printing or spraying processing, such as 3D glass fiber substrate, using spraying process, paint viscosity 9 ~ 9.5s, baking 80 ℃ / (25 ~ 30) min, solidification molding film thickness 5 ~ 8um. Because it is above the coating layer, the higher the transmittance, the better the overall effect, so the thinner the thickness is controlled, the higher the transmittance; secondly, because coating 3 and coating 6 belong to a structure with higher hardness, the intermediate structure coating 4 and 5 are PU type paints with relatively low hardness. If the thickness of the intermediate structure is too thick, the lower the support capacity of the outermost layer, it is easy to produce baking cracks, or the outermost layer increases due to the increase in thickness during the bending test, and the bending radius also increases, so that the arc length of the pull-up increases, (L = r × α, L is the arc length of the center angle, r is the radius, α is the degree of the center angle (radian system), α is constant, the larger the r, the larger the L), thus causing the problem of easy cracking during bending.
[0012] Preferably, the primer layer 3 of coating 5 is made of polyurethane resin paint, processed by silk screen printing or spraying, such as 3D glass fiber substrate, using spraying process, paint viscosity 9-9.5s, baking 80℃ / (15-20)min, and curing forming film thickness 4-7um. The main function of this coating is to increase the adhesion between layers. After the silk screen logo is baked on coating 4, the curing degree of coating 4 is too high. If the external texture UV glue is used directly, there will be insufficient bite corrosion and the risk of low adhesion.
[0013] Preferably, coating six, outer texture layer - UV glue, use UV curing glue, the main resin is preferably acrylic light curing resin; roller transfer or spraying processing, such as 3D glass fiber substrate, use spraying process, glue viscosity 9.5 ~ 10s, baking 65℃ / (5 ~ 10)min, curing molding film thickness 20 ~ 25um, hardness range controlled in 2H ~ 3H, biased towards 3H. As the outermost layer, it needs to have good water resistance, temperature shock resistance, weather resistance, aging resistance, chemical resistance and other performance characteristics.
[0014] The 3D glass fiber outer coating (coated with a thickness of 300nm using a magnetron sputtering furnace) prepared using the laminated structure and related processing techniques and materials in this solution has shown good product performance tests.
[0015] Compared with the prior art, the technical effects and advantages of the present invention are as follows:
[0016] This method of making glass fiber thick coating external decoration effect realizes lightness, easy processing and diversified decoration effect through unique laminated structure design, while ensuring the overall stability of the structure and meeting the strict performance test standards required by the back cover of mobile phones. This performance improvement is due to the selection of each layer of materials and the optimization of process parameters, such as the selection of resin with good adhesion and low curing shrinkage as the coating, and the control of appropriate baking time and temperature, ensuring that each layer can fit tightly to form a stable composite structure;
[0017] By combining coating technology with special textures, a variety of decorative effects including metallic luster, colorful colors, gradient optical effects, etc. are created. In particular, the acrylic light-curing resin used in the inner texture layer can form textures with specific styles, such as marble and haze patterns. These textures are not only beautiful, but also can cover the defects of the glass fiber material itself, thus improving the aesthetics and yield rate of the finished product.
[0018] Each layer of coating is precisely controlled in terms of viscosity, baking conditions and film thickness to ensure the efficiency and quality of the entire production process. For example, the setting of the viscosity and baking time of the polyurethane resin paint of the primer layer 1 not only strengthens the adhesion to the glass fiber substrate, but also improves the water barrier performance. In addition, the hardness of the inner texture layer-UV glue is controlled between 1H and 2H, which not only reduces the risk of cracking of the coating, but also makes it possible to achieve thicker coatings, broadening the design flexibility;
[0019] Through reasonable lamination design, especially the setting of coating four and coating five, although the hardness is relatively low, it effectively balances the hardness and toughness as the middle layer, avoiding the cracking of the outer layer due to stress concentration during bending or heat treatment. The high hardness characteristics of the outer texture layer-UV glue further enhance the product's wear resistance, scratch resistance and chemical corrosion resistance, extending its service life;
[0020] The multi-layer coating method effectively conceals the problems of insufficient transparency and glass fiber grain of the glass fiber material, especially the obvious concealing effect of the primer layer on the glass fiber grain, and the haze of the inner texture layer on the concealment of defects, which greatly improves the texture and appearance of the final product. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0022] Figure 1 It is a schematic diagram of the laminated structure of the glass fiber thick coating external decorative effect of the present invention;
[0023] Figure 2 This is a product performance test table of the glass fiber thick coating external decoration effect of the present invention;
[0024] Figure 3 The present invention is a flow chart of the method for producing the glass fiber thick coating external decorative effect. DETAILED DESCRIPTION
[0025] In the following description, a large number of specific details are provided to provide a more thorough understanding of the present invention. However, it is apparent to those skilled in the art that the present invention can be implemented without one or more of these details. In other examples, in order to avoid confusion with the present invention, some technical features well known in the art are not described.
[0026] Unless otherwise defined, the up, down, left, right, front, back, inside and outside directions involved in this document are based on the up, down, left, right, front, back, inside and outside directions in the figures shown in the present invention, and are explained here together.
[0027] Provides such as Figure 1-Figure 3 As shown:
[0028] Example 1
[0029] A method for making a glass fiber thick coating external decoration effect, selecting a woven fiber material with a gram weight of 100g as the base material, using epoxy resin for coating, and curing and molding, the final base material thickness is controlled at 0.5mm to ensure both cost advantage and excellent rigidity performance. This step ensures the stability of the base material performance by controlling the resin ratio and curing conditions, such as temperature 80℃ and time 15 to 20 minutes.
[0030] Use polyurethane resin paint as primer layer 1, adopt spraying process, set the paint viscosity within 10-10.5 seconds to ensure good fluidity and coverage. The baking condition is 80℃, and the duration is 15-20 minutes, so that the layer forms a strong bond with the glass fiber substrate, and the film thickness is controlled at 15-20 microns. To enhance the water-blocking ability, ensure that the filler content in the paint is less than 10% of the resin mass.
[0031] Next, use polyurethane resin slow-drying paint as the primer layer, and also use the spraying process, adjust the viscosity to 9-10 seconds, bake at 80°C, and cure for 25-30 minutes. This step is intended to further enhance the bonding with primer layer 1, while effectively covering the fiberglass texture, and the film thickness is controlled at 12-18 microns. Fillers such as titanium dioxide are recommended to be kept at 20% to 30% of the resin mass to prevent orange peel and improve surface flatness. Use acrylic light-curing resin as the UV glue for the inner texture layer. Through the spraying process, the glue viscosity is set at 9.5 to 10 seconds, the baking condition is 65°C, and the curing time is 5 to 10 minutes. The thickness of this layer is about 20 to 25 microns, and the hardness is controlled at 1H to 2H, which can reduce the risk of cracking of the coating and allow thicker coatings (such as 400 nanometers) without cracking. Texture designs such as marble and haze patterns can be shaped and printed with silicone or TPU materials to increase the decorative art sense.
[0032] According to the design requirements, evaporation coating or sputtering coating technology is used to deposit decorative coatings on the inner texture layer, such as high-gloss silver, gradient optical coating, etc., to ensure that the optical effect meets expectations. In order to enhance the bonding with the coating layer, polyurethane resin paint is used as primer layer 2. Through the spraying process, the viscosity is controlled at 9 to 9.5 seconds, the baking conditions are 80°C, the time is 25 to 30 minutes, and the film thickness is 5 to 8 microns. This ensures high transparency and good support, and avoids cracking caused by excessive thickness of the middle layer during bending. The logo is silk-screened or sprayed on primer layer 2. Mirror silver, inkjet ink, etc. are used to ensure clear markings, strong adhesion and low curing temperature to enhance the brand recognition of the product.
[0033] In order to further increase the interlayer adhesion, polyurethane resin paint is used as the primer layer 3, the baking conditions are 80°C, 15 to 20 minutes, and the film thickness is 4 to 7 microns, ensuring good adhesion with the cured coating layer 4 and the Logo layer. The last layer uses acrylic light-curing resin as the UV glue for the outer texture layer. Through spraying or roller transfer process, the viscosity is 9.5 to 10 seconds, the baking conditions are 65°C, 5 to 10 minutes, and the film thickness after curing reaches 20 to 25 microns. The hardness is in the range of 2H to 3H, tending to 3H, to ensure the product's wear resistance, scratch resistance, chemical corrosion resistance and other characteristics.
[0034] In this embodiment, a glass fiber substrate with a 2D or 3D structure is selected as the basis, and the selected substrate is pretreated to adjust the surface cleanliness and roughness, and the coatings are applied on the glass fiber substrate in sequence. Coating 1: polyurethane, epoxy resin, acrylic resin or a composite thereof is used to ensure adhesion and water resistance to the glass fiber substrate. Coating 2: one of the above resins is also used to cover the glass fiber texture through its own hiding power, and cooperate with the subsequent coating layer to show optical functions. Coating 3: UV curing glue is used, and the main body is acrylic light curing resin. A texture layer is formed by roller transfer or spraying to enhance the adhesion of the coating and prevent cracking. Coating 4: polyurethane resin paint is used, processed by silk screen printing or spraying, and a spraying process is used. The paint viscosity is 9 ~9.5s, bake at 80°C / (25~30)min, solidify and form film thickness 5~8um, coating five: use polyurethane resin paint, screen printing or spraying, use spraying process, paint viscosity 9~9.5s, bake at 80℃ / (15~20)min, solidify and form film thickness 4-7um, coating six: outer texture layer - UV glue, use UV curing glue, main body acrylic light curing resin, roller transfer or spraying, use spraying process, glue viscosity 9.5~10s, bake at 65℃ / (5~10)min, solidify and form film thickness 20~25um, hardness range is controlled at 2H~3H, tends to 3H, add mirror silver and spray ink decorative elements by screen printing or spraying to ensure that the logo is obvious and durable.
[0035] In this embodiment, the glass fiber substrate is a woven fiber material with a gram weight of 100 g, which is coated with epoxy resin and cured to a thickness of 0.5 mm to balance the cost and mechanical strength.
[0036] In this embodiment, the coating 1 uses polyurethane resin paint. Through the spraying process, the paint viscosity is controlled at 10 to 10.5 seconds. The baking conditions are 80°C for 15 to 20 minutes to ensure that the film thickness is 15 to 20 microns, and the filler content does not exceed 10% of the resin mass to improve adhesion and water resistance.
[0037] In this embodiment, the second coating uses a polyurethane resin slow-drying paint, which is sprayed with a viscosity set to 9 to 10 seconds. The baking conditions are: 80°C, 25 to 30 minutes, a film thickness of 12 to 18 microns, and a filler such as titanium dioxide content controlled at 20% to 30% to reduce orange peel phenomenon and enhance hiding power.
[0038] In this embodiment, the coating three uses acrylic photocurable resin, which is transferred by spraying or roller pressing, with a viscosity of 9.5 to 10 seconds and a baking condition of 65°C for 5 to 10 minutes. After curing, the film thickness is 20 to 25 microns and the hardness is controlled at 1H to 2H to adapt to thicker coatings without cracking, and can present a variety of textures such as marble and smoky patterns.
[0039] In this embodiment, a coating layer is provided between the spraying third and the spraying fourth, and the coating layer is decorated by using evaporation coating or sputtering coating technology.
[0040] In this embodiment, the texture layer includes a variety of choices of optical textures and stylized textures.
[0041] In this embodiment, the texture layer is made of silica gel and TPU material through contour rubbing processing.
[0042] It should be noted that, in this article, relational terms such as one and two are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions. The sentence "includes an element defined by ... does not exclude the existence of other identical elements in the process, method, article or device including the element".
[0043] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for producing a glass fiber thick coating external decorative effect, characterized in that: The following steps are involved: S1. Use 2D or 3D structured glass fiber substrate as the basis; S2. Pre-treating the selected substrate to adjust the surface cleanliness and roughness and sequentially applying the coating on the glass fiber substrate; S3, coating 1: using polyurethane, epoxy resin, acrylic resin or their composites to ensure adhesion and water barrier properties with the glass fiber substrate; S4, coating 2: also uses one of the above resins, uses its own hiding power to cover the glass fiber texture, and cooperates with the subsequent coating layer to show the optical function; S5, coating three: using UV curing glue, the main body is acrylic light curing resin, through roller transfer or spraying to form a texture layer, so as to enhance the adhesion of the coating and prevent cracking; S6, coating 4: use polyurethane resin paint, processed by silk screen printing or spraying, using spraying process, paint viscosity 9 ~ 9.5s, baking 80 ℃, curing forming film thickness 5 ~ 8um; S7, coating five: use polyurethane resin paint, screen printing or spraying, use spraying process, paint viscosity 9 ~ 9.5s, baking 80 ℃, curing film thickness 4 ~ 7um; S8, coating six: outer texture layer - UV glue, using UV curing glue, main body acrylic light curing resin, roller transfer or spraying processing, using spraying process, glue viscosity 9.5 ~ 10s, baking 65 ℃, curing molding film thickness 20 ~ 25um, hardness range controlled in 2H ~ 3H, biased towards 3H; S9. Add mirror silver and spray ink decorative elements by silk screen printing or spraying to ensure that the logo is obvious and durable.
2. The method for producing a glass fiber thick coating external decorative effect according to claim 1, characterized in that: The glass fiber substrate is a woven fiber material with a gram weight of 100 g, which is coated with epoxy resin and cured to a thickness of 0.5 mm to balance cost and mechanical strength.
3. The method for producing a glass fiber thick coating external decorative effect according to claim 1, characterized in that: The coating is made of polyurethane resin paint, and the paint viscosity is controlled at 10 to 10.5 seconds through a spraying process. The baking conditions are 80° C. for 15 to 20 minutes to ensure a film thickness of 15 to 20 microns, and the filler content does not exceed 10% of the resin mass to improve adhesion and water resistance.
4. The method for producing a glass fiber thick coating external decorative effect according to claim 1, characterized in that: The second coating uses a polyurethane resin slow-drying paint, which is sprayed with a viscosity set to 9 to 10 seconds, a baking condition of 80°C, 25 to 30 minutes, a film thickness of 12 to 18 microns, and a filler such as titanium dioxide content controlled at 20% to 30% to reduce orange peel and enhance hiding power.
5. The method for producing a glass fiber thick coating external decorative effect according to claim 1, characterized in that: The coating three uses acrylic light-curing resin, which is transferred by spraying or roller pressing, with a viscosity of 9.5 to 10 seconds and a baking condition of 65°C for 5 to 10 minutes. After curing, the film thickness is 20 to 25 microns and the hardness is controlled at 1H to 2H to adapt to thicker coatings without cracking and to present a variety of textures.
6. The method for producing a glass fiber thick coating external decorative effect according to claim 1, characterized in that: A coating layer is provided between the spraying third and the spraying fourth, and the coating layer is decorated by using evaporation coating or sputtering coating technology.
7. The method for producing a glass fiber thick coating external decorative effect according to claim 1, characterized in that: The texture layer includes a diverse selection of optical and stylized textures.
8. The method for producing a glass fiber thick coating external decorative effect according to claim 1, characterized in that: The texture layer is made of silica gel and TPU materials through contour rubbing processing.