Piezoresistive MEMS pressure chip preparation method and piezoresistive MEMS pressure chip wafer

By preparing varistor and electrical connection structures on SOI wafers, combining temporary bonding and eutectic bonding technology to thin the substrate surface, the problem of limited measurement range of high-temperature piezoresistive MEMS pressure chip is solved, and thinner is achieved Effects of high temperatures and suitable for stimulation and high temperatures.

CN118894487APending Publication Date: 2024-11-05GUANGZHOU ZENGXIN TECH CO LTD
View PDF 0 Cites 3 Cited by

Patent Information

Application Number
CN202410979043.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The measurement range of the piezoresistive MEMS pressure chips for high temperature applications is limited, resulting in limited package size and application range of pressure range.

Method used

By preparing varistor and electrical connection structures on the device layer of the SOI wafer, and using temporary bonding and eutectic bonding technology, the substrate surface is thinned and the substrate thickness of the SOI wafer is controlled to achieve a pressure-sensitive film and The overall chip is thinner.

Benefits of technology

Meets the film thickness requirements of different ranges of micro pressure to high pressure, broadens the application scenarios, and maintains the sensitivity and measurement accuracy of pressure-sensitive films in high temperature environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118894487A_ABST
    Figure CN118894487A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method of a piezoresistive MEMS pressure chip, and the method comprises the steps: providing an SOI wafer, forming a piezoresistor structure and an electrical connection structure on a device layer of the SOI wafer, forming a patterned passivation layer on the surface of the device layer, and exposing at least part of the electrical connection structure; forming a temporary bonding medium on the surface of the passivation layer, and bonding one surface of the device layer of the SOI wafer with a glass wafer; the substrate surface of the SOI wafer bonded in the step S12 is thinned, and an eutectic bonding medium is formed on the thinned substrate surface; providing a bonding wafer, wherein a hole is formed in one surface of the bonding wafer; forming an eutectic bonding medium on one surface of the bonding wafer on which the cavity is formed; and performing eutectic bonding on the surface of the bonding wafer with the cavity in the second part and the substrate surface of the SOI wafer in the first part, and removing the glass wafer to form a cavity corresponding to the piezoresistor. According to the technical scheme provided by the invention, the problem that the measuring range of the piezoresistive MEMS pressure chip is limited is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a semiconductor device, and in particular to a method for preparing a piezoresistive MEMS pressure chip and a piezoresistive MEMS pressure chip wafer. Background Art

[0002] Piezoresistive MEMS pressure chips are one of the most widely used MEMS products. Their basic working principle is the piezoresistive effect of doped silicon. According to the different working temperatures, piezoresistive MEMS pressure chips can be divided into two categories: normal temperature application and high temperature application. Normal temperature application piezoresistive MEMS pressure chips use doped silicon technology based on the PN junction isolation principle. Generally, the operating temperature does not exceed 120 degrees Celsius, otherwise the reverse cutoff function of the PN junction will fail, resulting in abnormal function of the pressure chip. Piezoresistive MEMS pressure chips for high temperature applications generally use SOI wafers, and form a spatially physically isolated doped silicon sensitive structure on the device layer of the SOI wafer. Such structures can operate above 120 degrees Celsius and do not exceed 500 degrees Celsius.

[0003] Piezoresistive MEMS pressure chips for high-temperature applications are widely used in the fields of industry, automobiles, aerospace, and defense. High-temperature piezoresistive MEMS pressure chips generally use SOI wafers to prepare doped silicon resistors with physical isolation in space, and prepare back cavities on the SOI wafers. They are then bonded to another glass wafer through an anodic bonding process to complete the preparation of high-temperature piezoresistive MEMS pressure chips. However, this preparation process requires two layers of wafer bonding, and the thickness of the prepared pressure chip is generally more than 800um. Too thick a pressure chip will limit the package size and the applicable range of the pressure range.

[0004] Therefore, the problem of limited measurement range of piezoresistive MEMS pressure chips for high-temperature applications has become a technical problem that needs to be urgently solved by those skilled in the art. Summary of the invention

[0005] The present invention provides a method for preparing a piezoresistive MEMS pressure chip and a piezoresistive MEMS pressure chip wafer, so as to solve the problem of limited measurement range of the piezoresistive MEMS pressure chip for high temperature applications.

[0006] According to a first aspect of the present invention, a method for preparing a piezoresistive MEMS pressure chip is provided, comprising:

[0007] Prepare the first part, including:

[0008] Step S11: providing an SOI wafer, wherein a device layer of the SOI wafer is formed with a varistor structure and an electrical connection structure, and a patterned passivation layer is formed on a surface of the device layer to expose at least a portion of the electrical connection structure;

[0009] Step S12: forming a temporary bonding medium on the surface of the passivation layer, and bonding one side of the device layer of the SOI wafer to a glass wafer;

[0010] Step S13: thinning the substrate surface of the SOI wafer bonded in step S12, and forming a eutectic bonding medium on the thinned substrate surface;

[0011] Prepare the second part, including:

[0012] Step S21: providing a bonding wafer, wherein a cavity is formed on one side of the bonding wafer;

[0013] Step S22: forming a eutectic bonding medium on one side of the bonded wafer having the cavity formed therein;

[0014] Prepare the third part, comprising:

[0015] Step S31: eutectic bonding one side of the second part of the bonded wafer with the cavity formed therein with the substrate surface of the SOI wafer in the first part and removing the glass wafer to form a cavity corresponding to the varistor.

[0016] Optionally, the step S31 includes:

[0017] Step S311: aligning the SOI wafer with the bonding wafer so that the cavity corresponds to the varistor and then performing eutectic pre-bonding;

[0018] Step S312: debonding the glass wafer on the SOI wafer;

[0019] Step S313: eutectic bonding the substrate surface of the SOI wafer and the cavity surface of the bonding wafer.

[0020] Optionally, in step S13, the eutectic bonding medium is a metal film.

[0021] Optionally, in step S22, the eutectic bonding medium is silicon.

[0022] Optionally, the metal film is a metal film containing Au.

[0023] Optionally, the temporary bonding medium in step S12 is bonding glue.

[0024] Optionally, the debonding in step S312 is to remove the bonding adhesive and thereby remove the glass wafer.

[0025] According to a second aspect of the present invention, there is provided a piezoresistive MEMS pressure chip wafer, the wafer comprising: an SOI wafer, a device layer of the SOI wafer being provided with a piezoresistive resistance structure and an electrical connection structure, and a substrate layer of the SOI wafer being a thinned substrate;

[0026] A bonding wafer, wherein a cavity is formed on one side of the bonding wafer;

[0027] A eutectic bonding medium, wherein the eutectic bonding medium is at least located between the bonding contact surfaces of the bonding wafer and the SOI wafer; wherein,

[0028] The substrate layer of the SOI wafer and the side of the bonding wafer with the cavity are bonded together through the eutectic bonding medium, and the cavity forms a cavity with the SOI wafer varistor structure.

[0029] Optionally, the thickness of the SOI wafer device layer is less than 2um.

[0030] Optionally, the depth of the cavity is greater than 20 um.

[0031] Compared with the prior art, the present invention has the following advantages:

[0032] The present invention proposes a method for preparing a piezoresistive MEMS pressure chip, first preparing a varistor and an electrical connection structure on a SOI wafer device layer, then temporarily bonding one side of the SOI device layer to a glass wafer by temporary bonding, and then thinning the substrate surface of the SOI wafer, and controlling the thickness of the substrate surface of the SOI wafer to be within the expected thickness; subsequently, the substrate surface of the thinned SOI wafer is bonded to a wafer with a cavity formed therein by eutectic bonding. The method for preparing a piezoresistive MEMS pressure chip provided by the present invention can control the thickness of the pressure sensitive film of the piezoresistive MEMS pressure chip within the expected range of values ​​by controlling the thickness of the substrate surface of the SOI wafer, and meet the film thickness requirements of different ranges from micro-pressure to high pressure. At the same time, this preparation method can control the overall thickness of the piezoresistive MEMS pressure chip by thinning the wafer with a cavity formed therein after eutectic bonding, and can meet the demand for thinning of terminal products. Using SOI wafers for production can enable the piezoresistive MEMS pressure chip proposed by the present invention to be applied to high temperature environments. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0034] Figure 1 It is a schematic flow chart of a method for preparing a piezoresistive MEMS pressure chip provided by one embodiment of the present invention;

[0035] Figure 2 It is a flow chart of step S31 in a method for preparing a piezoresistive MEMS pressure chip provided by an embodiment of the present invention;

[0036] Figure 3-14 It is a cross-sectional view of different process stages of a method for preparing a piezoresistive MEMS pressure chip provided in Embodiment 1 of the present invention;

[0037] Fig.15 is a cross-sectional view of a piezoresistive MEMS pressure chip provided in Embodiment 2 of the present invention;

[0038] Fig.16 is a cross-sectional view of a piezoresistive MEMS pressure chip provided in Embodiment 3 of the present invention;

[0039] 101-SOI wafer;

[0040] 1011- substrate layer;

[0041] 1012- buried oxide layer;

[0042] 102-varistor structure;

[0043] 103- electrical connection structure;

[0044] 104- patterned passivation layer;

[0045] 105- glass wafer;

[0046] 106-eutectic bonding medium;

[0047] 107-temporary bonding medium;

[0048] 108-bonded wafer;

[0049] 109- Hollow;

[0050] 110-Eutectic bonding medium. DETAILED DESCRIPTION

[0051] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0052] The terms "first", "second", "third", "fourth", etc. (if any) in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0053] The conventional high-temperature pressure chip processing scheme in the industry is: first, prepare varistors, metal pads and passivation layers on the device layer of the SOI wafer; second, thin the SOI wafer and prepare a cavity on the back of the wafer to form a pressure-sensitive film; finally, bond the glass wafer to the SOI wafer to prepare a high-temperature pressure chip. However, this process requires the use of glass wafers, and the thickness of the final chip is generally greater than 600um. Too thick a pressure chip will limit the package size and the applicable range of the pressure range.

[0054] In another high-temperature pressure chip preparation scheme, two silicon-silicon bonding technologies are used to connect the piezoresistive layer to the pressure-sensitive film, and the pressure-sensitive film to the substrate silicon to form a whole. The piezoresistive layer and the pressure-sensitive film are isolated by an oxide insulating layer. The bonding method adopted in this scheme can achieve reliable bonding between the piezoresistive layer and the pressure-sensitive film while preparing the piezoresistors. This method can reduce the overall thickness of the pressure chip device to a certain extent and expand the application range of the device.

[0055] However, since the bonding method adopted in the above scheme is Si-Si bonding, the bonding temperature required is as high as 850-950 degrees Celsius, so the manufacturing process of the metal pad can only be carried out after completing two silicon-silicon bonds. At the same time, in order to avoid the risk of fragmentation of the bonded SOI film layer during the subsequent preparation of the metal pad, the thickness of the SOI film layer must have a certain thickness, for example: greater than 30um, resulting in the pressure chip can only be used for large-range pressure measurement, and cannot be used for lower pressure measurement. Therefore, the pressure range application range of the high-temperature pressure chip prepared by this scheme is also limited.

[0056] In view of this, in order to solve the above problems, the inventors of the present application proposed a method for preparing a piezoresistive MEMS pressure chip, such as Figure 1 As shown, Figure 1 The present invention is a schematic flow chart of a method for preparing a piezoresistive MEMS pressure chip, comprising:

[0057] Preparation of the first part:

[0058] Step S11: providing an SOI wafer, wherein a device layer of the SOI wafer is formed with a varistor structure and an electrical connection structure, and a patterned passivation layer is formed on a surface of the device layer to expose at least a portion of the electrical connection structure;

[0059] Step S12: forming a temporary bonding medium on the surface of the passivation layer, and bonding one side of the device layer of the SOI wafer to a glass wafer;

[0060] Step S13: thinning the substrate surface of the SOI wafer bonded in step S12, and forming a eutectic bonding medium on the thinned substrate surface;

[0061] Preparation of the second part:

[0062] Step S21: providing a bonding wafer, wherein a cavity is formed on one side of the bonding wafer;

[0063] Step S22: forming a eutectic bonding medium on one side of the bonded wafer having the cavity formed therein;

[0064] Preparation of the third part:

[0065] Step S31: eutectic bonding one side of the second part of the bonded wafer with the cavity formed therein with the substrate surface of the SOI wafer in the first part and removing the glass wafer to form a cavity corresponding to the varistor.

[0066] The present invention proposes a method for preparing a piezoresistive MEMS pressure chip, first preparing a piezoresistor and an electrical connection structure on a SOI wafer device layer, then temporarily bonding one side of the SOI device layer to a glass wafer by temporary bonding, and then thinning the substrate surface of the SOI wafer, and controlling the thickness of the substrate surface of the SOI wafer to be within the expected thickness; subsequently, the substrate surface of the thinned SOI wafer is bonded to a wafer with a cavity formed therein by eutectic bonding. In the method for preparing a piezoresistive MEMS pressure chip provided by the present invention, since the bonding temperature of the eutectic bonding between the cavity and the wafer is relatively low, the bonding process will not affect the electrical connection structure formed on the device layer before bonding. In addition, in the technical solution, the SOI wafer on which the electrical connection structure is prepared is thinned, thereby avoiding the limitation on the thinning thickness of the substrate layer caused by preparing the electrical connection structure on the SOI wafer after thinning, so that the thickness of the substrate surface of the SOI wafer can be controlled within the expected range. It can be seen that in the technical solution provided by the present invention, based on the bonding method of eutectic bonding between the cavity and the wafer, and by first preparing the electrical connection structure and then thinning the substrate layer, the electrical connection structure will not be affected, and the thickness of the substrate surface of the SOI wafer can be controlled within the expected range. Furthermore, by controlling the thickness of the substrate surface of the SOI wafer, the thickness of the pressure sensitive film of the piezoresistive MEMS pressure chip can be controlled within the expected range, meeting the film thickness requirements of different ranges from micro-pressure to high pressure.

[0067] At the same time, this preparation method controls the overall thickness of the piezoresistive MEMS pressure chip by thinning the wafer in which the cavity is formed after eutectic bonding, thereby meeting the demand for thinning of the terminal product.

[0068] By adopting SOI wafer for manufacturing, the piezoresistive MEMS pressure chip proposed in the present invention can be applied to high temperature environment scenarios.

[0069] The technical solution of the present invention is described in detail with specific embodiments below. The following specific embodiments can be combined with each other, and the same or similar concepts or processes may not be described in detail in some embodiments.

[0070] The present invention provides three embodiments of a method for preparing a piezoresistive MEMS pressure chip provided by the present invention. The difference between the first embodiment, the second embodiment and the third embodiment is that the position for forming the eutectic bonding medium during eutectic bonding is different.

[0071] Embodiment 1:

[0072] The following will be combined Figure 1 ,as well as Figures 2 to 14A method for preparing a piezoresistive MEMS pressure chip according to an embodiment of the present invention is described in detail. Figure 2 is a schematic diagram of the process of preparing the third part in the method for preparing a piezoresistive MEMS pressure chip according to an embodiment of the present invention, Figures 3 to 14 It is a cross-sectional structural schematic diagram of a process of a method for preparing a piezoresistive MEMS pressure chip according to an embodiment of the present invention.

[0073] The method for preparing the piezoresistive MEMS pressure chip provided in this embodiment specifically comprises the following steps:

[0074] Prepare the first part; the process of preparing the first part is as follows Figures 3 to 9 shown.

[0075] Please refer to Figure 1 , executing step S11, providing an SOI wafer, wherein a device layer of the SOI wafer is formed with a varistor junction and an electrical connection structure, and a patterned passivation layer is formed on the surface of the device layer, exposing at least a portion of the electrical connection structure.

[0076] A SOI wafer 101 is provided, and a process of forming a varistor structure 102 and an electrical connection structure 103 on a device layer of the SOI wafer 101 is as follows: Figures 3 to 6 shown.

[0077] Please refer to Figure 3 , provide an SOI wafer 101. The SOI wafer 101 includes a device layer 1013, an oxide buried layer 1012 and a substrate layer 1011. In order to ensure the drift performance of the device, the thickness of the device layer in the SOI wafer 101 is less than 2um. Among them, the device layer 1013 greater than 2um can also realize the piezoresistive MEMS pressure chip described in the present invention, but the temperature drift performance of the prepared device deteriorates.

[0078] The device layer 1013 of the SOI wafer 101 is heavily doped with P-type. Specifically, the doping concentration is generally >1e19cm -3 Among them, the higher the doping concentration, the better the temperature drift performance of the pressure chip.

[0079] Please refer to Figure 4 , the device layer 1013 of the SOI wafer 101 is patterned by photolithography and etching processes to form the varistor structure 102. Please refer to Figure 5, an electrical connection structure 103 is prepared on the varistor structure 102 of the device layer of the SOI wafer 101, and high temperature annealing is performed to achieve ohmic contact between the electrical connection structure 103 and the P-type heavily doped silicon device layer. The electrical connection structure 103 serves as a pad for electrical connection of the package. In some specific examples, the material of the electrical connection structure 103 can be one or a combination of metals such as Ti, Al, Au, Pt, Cr, or a combination with metal compounds such as TiN.

[0080] Please refer to Figure 6 A passivation layer is formed on the front side of the SOI wafer 101, and the passivation layer is etched to form a patterned passivation layer 104, exposing at least a portion of the electrical connection structure 103 for packaging electrical connection. In some specific examples, the patterned passivation layer 104 is one or a combination of SiO2, SiN, etc.

[0081] Please refer to Figure 1 and Figure 7 , executing step S12, forming a temporary bonding medium 107 on the surface of the passivation layer, and bonding one side of the device layer of the SOI wafer 101 to a glass wafer 105.

[0082] In the step S12, the temporary bonding medium 107 is bonding glue.

[0083] Ordinary temporary bonding adhesives are usually able to work at lower temperatures, such as room temperature to around 120°C, which makes it suitable for semiconductor processing that does not require high temperature processing.

[0084] Specifically, the bonding adhesive is an organic polymer material, such as polyamide, polyester, polyurethane, resin, etc., which has a certain bonding strength to various materials such as silicon wafers and glass after curing at room temperature or slightly heating, which is sufficient to maintain the stability of the wafer during processing. Preferably, the bonding adhesive whose main component is resin has a maximum temperature tolerance of 350°C and can withstand 5 minutes.

[0085] The bonded wafers can be separated by chemical solvents, heat treatment or laser treatment.

[0086] Different eutectic bonding media and eutectic points correspond to different bonding adhesive materials. In this embodiment, in the eutectic system corresponding to each eutectic bonding medium, a suitable bonding adhesive material can be selected according to the corresponding eutectic point and the melting point of the bonding adhesive material.

[0087] Please refer to Figure 1 , executing step S13: thinning the substrate surface of the SOI wafer 101 bonded in step S12, and forming a eutectic bonding medium 106 on the thinned substrate surface.

[0088] The process of thinning the substrate surface of the SOI wafer 101 after bonding in step S12 and forming a eutectic bonding medium 106 on the thinned substrate surface is as follows: Figure 8 and Fig. 9 shown.

[0089] Please refer to Figure 8 , thinning the substrate surface of the SOI wafer 101 bonded to a glass wafer 105. The substrate surface refers to: a surface of the SOI wafer 101 opposite to the device layer.

[0090] After the substrate surface of the SOI wafer 101 is thinned, the remaining thickness of the SOI wafer 101 is used as the pressure-sensitive film of the piezoresistive MEMS pressure chip. The piezoresistive MEMS pressure chip prepared by using the substrate surface as the pressure-sensitive film after the substrate surface is thinned has improved sensitivity and measurement accuracy, and the sensor has a strong ability to respond to pressure changes. The thickness of the substrate surface of the SOI wafer 101 after thinning is: less than 30um.

[0091] exist Figure 8 Based on Fig. 9 After thinning the substrate surface of the bonded SOI wafer 101, a layer of eutectic bonding medium 106 is prepared on the substrate surface of the SOI wafer 101. Since bonding is performed through the eutectic bonding medium 106, the bonding temperature can be reduced. The low bonding temperature allows the manufacturing process of the varistor and the electrical connection structure 103 to be performed before bonding, thereby significantly reducing the damage to the SOI wafer 101 when preparing the electrical connection structure 103 and the varistor after bonding, so that the thickness of the SOI wafer 101 can be thinned to any thickness including less than 30um, and does not affect the subsequent process. Even the thickness of the pressure-sensitive film can be customized arbitrarily, so that the piezoresistive MEMS pressure chip involved in the present invention can also be used in special pressure measurement application scenarios, broadening the application scenarios. In the step S13, the eutectic bonding medium 106 is a metal film. In some specific examples, the metal film is a metal film containing Au. In other specific examples, the metal material can also be Al, Cu, Sn, AuSn alloy, etc. The method of preparing a layer of metal film on the substrate surface of the SOI wafer 101 is: evaporation, sputtering or electroplating. The metal film is used in the subsequent low-temperature bonding process of bonding the first part and the second part. The eutectic bonding medium 106 in the step S13 is a semiconductor material. In some specific examples, the semiconductor material is: semiconductor materials such as Ge and In. The method of preparing a layer of semiconductor material on the substrate surface of the SOI wafer 101 is: chemical vapor deposition. The semiconductor material is used in the subsequent low-temperature bonding process of bonding the first part and the second part.

[0092] Preparation of the second part; the process of preparing the second part Fig.10 and Fig.11 shown.

[0093] Please refer to Figure 1 and Fig.10 , executing step S21 , providing a bonding wafer 108 , wherein a cavity 109 is formed on one side of the bonding wafer 108 .

[0094] Providing a bonding wafer 108 , wherein a cavity 109 is formed on one side of the bonding wafer 108 specifically includes: providing a bonding wafer 108 .

[0095] A cavity 109 is formed on one side of the bonding wafer 108 by photolithography and etching processes. The bonding wafer 108 is made of Si. In a typical implementation, the depth of the cavity 109 is generally greater than 20 um.

[0096] Please refer to Figure 1 and Fig.11 , perform step S22, prepare a layer of eutectic bonding medium 110 on one side of the bonding wafer 108 formed with the cavity 109. In step S13, the eutectic bonding medium 110 is a metal film. The metal film is: Au, Al, Cu, Ag, Sn, AuSn alloy, etc.

[0097] The method of preparing a layer of eutectic bonding medium 110 on one side of the bonded wafer 108 with the cavity 109 formed thereon is: evaporation, sputtering or electroplating. The metal film is used in the subsequent low-temperature bonding process of bonding the first part and the second part. The eutectic bonding medium 110 in step S23 is a semiconductor material. In some specific examples, the semiconductor material is: semiconductor materials such as Ge and In. The method of preparing a layer of eutectic bonding medium 110 on one side of the bonded wafer 108 with the cavity 109 formed thereon is: chemical vapor deposition. The semiconductor material is used in the subsequent low-temperature bonding process of bonding the first part and the second part.

[0098] When the eutectic bonding medium formed on the surfaces of the thinned SOI wafer 101 and the bonding wafer 108 are both metal films, bonding modes such as Al-Al, Au-Au, Cu-Cu, and Au-Sn will eventually be formed.

[0099] When the eutectic bonding media formed on the surfaces of the thinned SOI wafer 101 and the bonding wafer 108 are respectively: metal film and semiconductor material, or semiconductor material and metal film, Au-Ge, Ag-Ge, Au-In and the like bonding modes are formed after bonding.

[0100] Since the eutectic bonding medium 106 is prepared on the thinned substrate surface, and the eutectic bonding medium 110 is prepared on the side of the bonding wafer 108 with the cavity 109, any eutectic bonding method of Al-Al, Au-Au, Cu-Cu, Au-Sn, Au-Ge, Ag-Ge, and Au-In will eventually be formed on the bonding surface of the two, which can reduce the bonding temperature during subsequent bonding. Specifically, different eutectic bonding media and different eutectic bonding systems formed have different corresponding eutectic point temperatures, as shown in Table 1:

[0101] Eutectic bonding system <![CDATA[Eutectic point ( o C)]]> Al-Al 250 Au-Au 300 Cu-Cu 350 Au-Sn 280 Ag-Sn 221 Au-In 275 Ag-Ge 420 Au-Ge 400 Pb-Sn 183

[0102] Table 1

[0103] It can be seen from Table 1 that, preferably, the eutectic bonding medium selects the above metal film or semiconductor material, and the third part is performed through the eutectic bonding medium 106 and 110, so that the temperature of the low-temperature wafer bonding process can be controlled at 200 to 500 degrees Celsius.

[0104] Furthermore, when selecting a material as a eutectic bonding medium for low-temperature wafer bonding, it is necessary to consider the available material types and their corresponding melting points to prevent the bonding medium from melting during eutectic bonding and affecting the low-temperature wafer bonding process. The available materials and their corresponding melting points are shown in Table 2:

[0105] Material <![CDATA[Melting point ( o °C)]]> Si 1412 Au 1063 Sn 232 Pb 327 In 156 Al 660 Ge 937 Cu 1084 Ag 961.8

[0106] Table 2

[0107] In combination with Table 1 and Table 2, the melting point of the eutectic bonding medium material in this embodiment is greater than the eutectic point temperature of the eutectic bonding. When the eutectic point of the eutectic bonding medium is ensured to be lower than its melting point, a low-temperature wafer bonding process with a temperature of 200 to 500 degrees Celsius is achieved.

[0108] Prepare the third part; the process of preparing the third part is as follows Figure 2 , Figure 12-13 shown.

[0109] Please refer to Figure 1 , executing step S31, eutectic bonding one side of the bonding wafer 108 with the cavity 109 in the second part with the substrate surface of the SOI wafer 101 in the first part and removing the glass wafer 105 to form a cavity corresponding to the varistor.

[0110] Please refer to Figure 2 , step S31 comprises:

[0111] Step S311, aligning the SOI wafer with the bonding wafer so that the cavity corresponds to the varistor and then performing eutectic pre-bonding;

[0112] Step S312, debonding the glass wafer on the SOI wafer;

[0113] Step S313, eutectic bonding the substrate surface of the SOI wafer and the cavity surface of the bonding wafer.

[0114] The specific process of step S31 is as follows: Figure 2 , 12 to Fig.13 shown.

[0115] exist Figure 1 Based on Figure 2 and Fig.12 , executing step S311: aligning the SOI wafer 101 and the bonding wafer 108 so that the cavity 109 corresponds to the varistor and then performing eutectic pre-bonding.

[0116] exist Figure 1 Based on Figure 2 and Fig.13 , executing step S312: debonding the glass wafer 105 on the SOI wafer 101.

[0117] In step S312 , debonding is to remove the bonding adhesive and thereby remove the glass wafer 105 .

[0118] The bonding adhesive is removed by UV, heating, dissolving with an organic solvent, and the like.

[0119] exist Figure 1 Based on Figure 2 , executing step S313 : eutectic bonding the substrate surface of the SOI wafer 101 and the cavity 109 surface of the bonding wafer 108 .

[0120] The temperature of the low temperature wafer bonding process in which the substrate surface of the SOI wafer 101 and the cavity 109 surface of the bonding wafer 108 are bonded by the eutectic bonding medium can be controlled at 200 to 500 degrees Celsius. Figure 1 Based on Figure 2 and Fig.14 After executing step S313, the method further includes: thinning the other side of the bonded wafer 108. The thickness of a piezoresistive MEMS pressure chip may be less than 100 um.

[0121] In summary, the piezoresistive MEMS pressure chip provided in this embodiment has a low bonding temperature of the eutectic bonding between the cavity and the wafer, so the bonding process will not affect the electrical connection structure formed on the device layer before bonding. And in this technical solution, the SOI wafer with the electrical connection structure prepared is thinned, which avoids the restriction on the thickness of the substrate layer thinning caused by preparing the electrical connection structure on the SOI wafer after thinning, so that the thickness of the substrate surface of the SOI wafer can be controlled within the expected range. It can be seen that in the technical solution provided by the present invention, based on the bonding method of eutectic bonding between the cavity and the wafer, and by first preparing the electrical connection structure and then thinning the substrate layer, it will not affect the electrical connection structure, and at the same time, the thickness of the substrate surface of the SOI wafer can be controlled within the expected range. Furthermore, by controlling the thickness of the substrate surface of the SOI wafer, the thickness of the pressure sensitive film of the piezoresistive MEMS pressure chip can be controlled within the expected range, meeting the film thickness requirements of different ranges from micro-pressure to high pressure. At the same time, this preparation method controls the overall thickness of the piezoresistive MEMS pressure chip by thinning the wafer with the cavity formed therein after eutectic bonding, which can meet the demand for thinning of terminal products. The use of SOI wafers for production can enable the piezoresistive MEMS pressure chip proposed in the present invention to be applied in high temperature environments.

[0122] Embodiment 2:

[0123] This example is different from the first embodiment in step S22, and the other steps are the same as the first embodiment. Fig.15 It is a cross-sectional structural schematic diagram of the completion process of another method for preparing a piezoresistive MEMS pressure chip according to an embodiment of the present invention.

[0124] In this embodiment, a eutectic bonding medium 106 is formed on the thinned substrate surface. The eutectic bonding medium 106 is a metal film. The metal film is: Au, Al, Cu, Sn, AuSn alloy, etc. or other semiconductor materials. The surface of the bonding wafer 108 can be silicon or other semiconductor materials.

[0125] Preferably, the eutectic bonding medium 106 is a metal film Au, and when the surface of the bonding wafer 108 is silicon, the eutectic point temperature corresponding to the Au-Si eutectic bonding method formed after bonding is 363°C, and the melting point of the bonding medium material is greater than the eutectic point temperature of the eutectic bonding.

[0126] The pressure device formed by the eutectic bonding method in this embodiment can also reduce the bonding temperature during subsequent bonding, and control the bonding temperature at 200-500 degrees Celsius, thereby not affecting the electrical connection structure formed on the device layer before bonding. Furthermore, the SOI wafer with the electrical connection structure prepared is thinned, avoiding the limitation on the thinning thickness of the substrate layer when preparing the electrical connection structure on the SOI wafer after thinning, so that the thickness of the substrate surface of the SOI wafer can be controlled within the expected range.

[0127] Embodiment three:

[0128] Fig.16 It is a cross-sectional structural schematic diagram of the completion process of another method for preparing a piezoresistive MEMS pressure chip according to an embodiment of the present invention.

[0129] In this embodiment, step S13 is different from that in embodiment 1, and other steps are the same as those in embodiment 1. In this embodiment, after executing step S13: thinning the substrate surface of the SOI wafer 101 bonded in step S12, the preparation of the first part is completed.

[0130] The second and third parts were prepared according to Example 1.

[0131] A layer of eutectic bonding medium 110 is prepared on one side of the bonding wafer 108 with the cavity formed therein. The eutectic bonding medium 110 is a metal film. The metal film is: Au, Al, Cu, Sn, AuSn alloy, etc. The eutectic bonding medium formed on the surface of the thinned SOI wafer 101 can be silicon or other semiconductor materials. The eutectic bonding medium formed on the surface of the wafer 101 is related to the selected wafer material, and the present invention is not limited thereto. Those skilled in the art can select suitable materials such as Si, GaAs, etc. as needed.

[0132] Preferably, when the eutectic bonding medium formed on the surface of the SOI wafer 101 is silicon and the eutectic bonding medium 106 is Au, the eutectic point temperature corresponding to the Au-Si eutectic bonding method formed after bonding is 363°C, and the melting points of these bonding medium materials are all greater than the eutectic point temperature of the eutectic bonding.

[0133] The pressure device formed by the eutectic bonding method in this embodiment can also reduce the bonding temperature during subsequent bonding, thereby realizing a low-temperature bonding process, and thus does not affect the electrical connection structure formed on the device layer before bonding; further, the SOI wafer with the electrical connection structure prepared is thinned, thereby avoiding the limitation on the thinning thickness of the substrate layer when the electrical connection structure is prepared on the SOI wafer after thinning, so that the thickness of the substrate surface of the SOI wafer can be controlled within the expected range of values.

[0134] In summary, the piezoresistive MEMS pressure chip provided by the present invention has a low bonding temperature due to the eutectic bonding between the cavity and the wafer, so the bonding process will not affect the electrical connection structure formed on the device layer before bonding. Furthermore, the SOI wafer with the electrical connection structure prepared is thinned, which avoids the restriction on the thickness of the substrate layer thinning caused by preparing the electrical connection structure on the SOI wafer after thinning, so that the thickness of the substrate surface of the SOI wafer can be controlled within the expected range of values. Based on the eutectic bonding between the cavity and the wafer, and by first preparing the electrical connection structure and then thinning the substrate layer, it will not affect the electrical connection structure, and at the same time, the thickness of the substrate surface of the SOI wafer can be controlled within the expected range of values. Furthermore, by controlling the thickness of the substrate surface of the SOI wafer, the thickness of the pressure-sensitive membrane of the piezoresistive MEMS pressure chip can be controlled within the expected range of values, meeting the membrane thickness requirements of different ranges from micro-pressure to high pressure. At the same time, this preparation method controls the overall thickness of the piezoresistive MEMS pressure chip by thinning the wafer with the cavity formed therein after eutectic bonding, which can meet the demand for thinning of terminal products. The use of SOI wafers for production can enable the piezoresistive MEMS pressure chip proposed in the present invention to be applied in high temperature environments.

[0135] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for preparing a piezoresistive MEMS pressure chip, characterized in that: include: Prepare the first part, including: Step S11: providing an SOI wafer, wherein a device layer of the SOI wafer is formed with a varistor structure and an electrical connection structure, and a patterned passivation layer is formed on a surface of the device layer to expose at least a portion of the electrical connection structure; Step S12: forming a temporary bonding medium on the surface of the passivation layer, and bonding one side of the device layer of the SOI wafer to a glass wafer; Step S13: thinning the substrate surface of the SOI wafer bonded in step S12, and forming a eutectic bonding medium on the thinned substrate surface; Prepare the second part, including: Step S21: providing a bonding wafer, wherein a cavity is formed on one side of the bonding wafer; Step S22: forming a eutectic bonding medium on one side of the bonded wafer having the cavity formed therein; Prepare the third part, comprising: Step S31: eutectic bonding one side of the second part of the bonded wafer with the cavity formed therein with the substrate surface of the SOI wafer in the first part and removing the glass wafer to form a cavity corresponding to the varistor.

2. The method for preparing a piezoresistive MEMS pressure chip according to claim 1, characterized in that: The step S31 comprises: Step S311: aligning the SOI wafer with the bonding wafer so that the cavity corresponds to the varistor and then performing eutectic pre-bonding; Step S312: debonding the glass wafer on the SOI wafer; Step S313: eutectic bonding the substrate surface of the SOI wafer and the cavity surface of the bonding wafer.

3. The method for preparing the piezoresistive MEMS pressure chip according to claim 2, characterized in that: In step S13, the eutectic bonding medium is a metal film.

4. The method for preparing the piezoresistive MEMS pressure chip according to claim 3, characterized in that: In step S22, the eutectic bonding medium is silicon.

5. The method for preparing the piezoresistive MEMS pressure chip according to claim 4, characterized in that: The metal film is a metal film containing Au.

6. The method for preparing the piezoresistive MEMS pressure chip according to claim 2, characterized in that: The temporary bonding medium in step S12 is bonding glue.

7. The method for preparing the piezoresistive MEMS pressure chip according to claim 5, characterized in that: In step S312 , debonding is to remove the bonding adhesive and thereby remove the glass wafer.

8. A piezoresistive MEMS pressure chip wafer, characterized in that: The wafer comprises: an SOI wafer, a device layer of the SOI wafer is provided with a varistor structure and an electrical connection structure, and a substrate layer of the SOI wafer is a thin substrate; A bonding wafer, wherein a cavity is formed on one side of the bonding wafer; A eutectic bonding medium, wherein the eutectic bonding medium is at least located between the bonding contact surfaces of the bonding wafer and the SOI wafer; wherein, The substrate layer of the SOI wafer and the side of the bonding wafer with the cavity are bonded together through the eutectic bonding medium, and the cavity forms a cavity with the SOI wafer varistor structure.

9. The method for preparing a piezoresistive MEMS pressure chip according to claim 1, characterized in that: The thickness of the SOI wafer device layer is less than 2um.

10. The method for preparing a piezoresistive MEMS pressure chip according to claim 1, characterized in that: The depth of the cavity is greater than 20 um.

Citation Information

Cited By

  • Preparation method of MEMS cavity structure

    CN119873730A

  • Preparation method of MEMS structure

    CN121341937A

  • MEMS chip preparation method based on piezoelectric laminated structure

    CN121449011A