Quaternary ammonium salt surfactant with fluorocarbon-silicon carbon double hydrophobic chains and preparation method thereof
By introducing fluorocarbon-silicon carbon double hydrophobic chain structure into new fluorosurfactants, a simple and gentle preparation method is adopted, the problem of rare types of new fluorosurfactants in the prior art is solved, and the environment is developed Friendly fluorocarbon surfactants have high foaming properties, thermal stability and wetting properties, and replace the use of traditional perfluorooctanyl sulfonyl compounds and perfluorooctanic acid compounds.
Patent Information
- Application Number
- CN202410827720.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-25
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-06-25
AI Technical Summary
The existing new fluorine-containing surfactants have few types, single structure, complex preparation process, harsh reaction conditions, low yields, and high environmental pollution, making it difficult to replace perfluorooctanyl sulfonyl compounds and perfluorooctanic acid compounds.
Quaternary ammonium salt surfactant with fluorocarbon-silicon carbon double hydrophobic chain and its preparation method are used to synthesize products without perfluorooctanoic acid and perfluorohexane sulfonyl through simple and gentle reaction conditions, and use N-(( Dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexamide, 3-chloropropylmethyldimethoxy The raw materials such as silane and potassium iodide are obtained by heating and stirring and under reduced pressure to obtain a quaternary ammonium salt surfactant with fluorocarbon-silicon carbon double hydrophobic chain.
It realizes environmentally friendly fluorocarbon surfactant, reduces the surface tension of the aqueous solution, has high foaming properties and thermal stability. As a foam foaming agent and foam stabilizing agent, it significantly improves the fire extinguishing performance and maintains good moisturization at low concentrations. Wet properties avoid potential harm to human health.
Smart Images

Figure CN118894879A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a surfactant and a preparation method thereof, in particular to a quaternary ammonium salt surfactant with a fluorocarbon-silicon-carbon double hydrophobic chain and a preparation method thereof, belonging to the technical field of surfactants. Background Art
[0002] Fluorocarbon surfactants are a special and important class of fine chemicals, known as "super surfactants". Fluorosurfactants have excellent thermal and chemical stability, high gas solubility, strong hydrophobic and oleophobic properties, and high surface activity. The most commonly used fluorocarbon surfactants are perfluorooctane sulfonyl compounds (PFOS) and perfluorooctanoic acid and its salts (PFOA). Unfortunately, PFOS / PFOA compounds are difficult to degrade in the natural environment. They are not only neurotoxic, but also likely to be enriched through the biological chain. In this context, the use and production of PFOS / PFOA compounds are gradually being restricted. Therefore, it is of great significance to develop new fluorosurfactants that have little environmental pollution, no biological enrichment, and are degradable. According to the exploration of many scholars, the research and development ideas for high-performance non-long-chain fluorosurfactants have been summarized, including ① shortening the length of the fluorocarbon chain, ② branching the fluorocarbon chain, and ③ introducing heteroatoms in the fluorocarbon chain. However, at present, only a few new fluorosurfactants have been proposed in China; and the new fluorocarbon surfactants currently proposed have a single structure, and only use the research and development idea ① (reducing the length of the fluorocarbon chain from 8 to 6). Almost all new fluorocarbon surfactants use 6-carbon fluorine-containing chains as hydrophobic groups, such as perfluorohexylsulfonyl fluoride, perfluorohexylsulfonyl chloride, etc. However, the production process of this type of fluorocarbon surfactant is complex, the yield is low, and the reaction conditions are harsh. Very few fluorocarbon surfactants with new fluorocarbon chain structures have been proposed, and there are almost no fluorocarbon surfactants with Gemini fluorocarbon surfactants and mixed hydrophobic chains (fluorocarbon chain-silicon carbon chain).
[0003] In summary, the current new fluorinated surfactants have the problems of rare species, single structure, complex preparation process, harsh reaction conditions, low yield, and great environmental harm. Therefore, there is an urgent need for a fluorinated surfactant with simple preparation process, cheap and easy-to-obtain raw materials and excellent performance. Summary of the invention
[0004] The technical problem to be solved by the present invention is to propose a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain and a preparation method thereof in view of the shortcomings of the above prior art. Through a simple and mild preparation method, a surfactant is obtained that can significantly reduce the surface tension of an aqueous solution, generate a large amount of foam, and wet a low-energy surface.
[0005] The technical solution of the present invention to solve the above technical problems is:
[0006] A quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, the structural formula of the surfactant is:
[0007]
[0008] The present invention also provides a method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, which is specifically:
[0009] N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide, 3-chloropropylmethyldimethoxysilane, potassium iodide and solvent are added to a reaction container, heated and stirred until the raw materials are completely dissolved, and then the temperature is continued to react. After the reaction is completed, the solvent and water are removed by distillation under reduced pressure, and washed with ethanol until the washing liquid does not change color to obtain a quaternary ammonium surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain. The chemical reaction formula is as follows:
[0010]
[0012] The technical solution further defined in the present invention is:
[0013] Further, in the preparation method of the aforementioned quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, the molar ratio of N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide:3-chloropropylmethyldimethoxysilane:potassium iodide is 1:(1.0-2.0):(0.01-0.03);
[0014] Preferably, the molar ratio of N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide:3-chloropropylmethyldimethoxysilane:potassium iodide is 1:1.5:0.02.
[0015] In the aforementioned method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, the solvent is one of acetonitrile, toluene, benzene, cyclohexane, chloroform, acetone, N,N-dimethylacetamide or N,N-dimethylformamide;
[0016] Preferably, the solvent is acetonitrile.
[0017] In the preparation method of the quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, the temperature of heating and stirring is 30-50°C;
[0018] Preferably, the temperature for heating and stirring is 40°C.
[0019] In the above-mentioned method for preparing the quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon dual hydrophobic chain, the temperature of the temperature-raising reaction is 60-90°C; preferably, the temperature of the temperature-raising reaction is 75°C.
[0020] In the above-mentioned preparation method of the quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, the temperature-raising reaction time is 4-8 hours; preferably, the temperature-raising reaction time is 6 hours.
[0021] The beneficial effects of the present invention are:
[0022] (1) The new quaternary ammonium surfactant with fluorocarbon-silicon-carbon double hydrophobic chain does not contain perfluorooctanoic acid (PFOS) and perfluorohexane sulfonate (PFH x S), the product is environmentally friendly, has little impact on the environment, and will not affect the human nervous system, immune system, endocrine system and genetic information.
[0023] (2) The raw material used in the present invention is fluorinated alkyl amide, while the raw material of existing fluorocarbon surfactants is generally perfluoroalkyl sulfonyl halide. Not only is the price of the raw material lower, but also no inorganic acid such as HR (R=F, Cl, Br, I) is produced during the production process, and the synthesis route is more environmentally friendly.
[0024] (3) The fluorocarbon surfactant of the present invention contains two hydrophobic chains, a fluorocarbon chain and a silicon-carbon chain, which can reduce the surface tension of the aqueous solution, have high foaming properties and thermal stability, and can be used as a foaming agent and foam stabilizer for fire-fighting foam, and can effectively improve the foaming, fire-extinguishing and fire-resistant properties of the foam fire extinguishing agent.
[0025] (4) The fluorocarbon surfactant of the present invention has good chemical stability and can wet low-energy surfaces well at low concentrations when used as a wetting agent. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 This is the hydrogen nuclear magnetic resonance spectrum of the quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain according to an embodiment of the present invention. DETAILED DESCRIPTION
[0027] The present invention will be described clearly and completely below in conjunction with specific embodiments. Obviously, the described embodiments are only a part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0028] Example 1
[0029] The present embodiment provides a method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, comprising the following steps:
[0030] N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide, 3-chloropropylmethyldimethoxysilane, potassium iodide and acetonitrile are added to a reaction container, wherein the molar ratio of N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide:3-chloropropylmethyldimethoxysilane:potassium iodide is
[0031] 1:1.5:0.02, stir at 40°C until the raw materials are completely dissolved, then continue to heat to 75°C for 6 hours, remove acetonitrile by vacuum distillation after the reaction, wash with ethanol until the washing liquid does not change color, and obtain a quaternary ammonium surfactant with a fluorocarbon-silicon-carbon double hydrophobic chain.
[0032] The nuclear magnetic resonance hydrogen spectrum of the quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain in Example 1 is as follows: Figure 1 As shown, the NMR spectrum is consistent with the structure of the target product.
[0033] Example 2
[0034] The present embodiment provides a method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, comprising the following steps:
[0035] N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide, 3-chloropropylmethyldimethoxysilane, potassium iodide and toluene are added to a reaction container, wherein the molar ratio of N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide:3-chloropropylmethyldimethoxysilane:potassium iodide is
[0036] 1:1.0:0.01, stir at 30°C until the raw materials are completely dissolved, then continue to heat to 60°C for 4 hours, remove toluene by vacuum distillation after the reaction, wash with ethanol until the washing liquid does not change color, and obtain a quaternary ammonium surfactant with a fluorocarbon-silicon-carbon double hydrophobic chain.
[0037] Example 3
[0038] The present embodiment provides a method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, comprising the following steps:
[0039] Add N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide, 3-chloropropylmethyldimethoxysilane, potassium iodide and cyclohexane into a reaction container, wherein the molar ratio of N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide:3-chloropropylmethyldimethoxysilane:potassium iodide is 1:2.0:0.03, and stir at 50°C until the raw materials are completely dissolved. Then continue to heat to 90°C for 8 hours. After the reaction is completed, remove cyclohexane by distillation under reduced pressure, wash with ethanol until the washing liquid does not change color, and obtain a quaternary ammonium salt surfactant with a fluorocarbon-silicon-carbon double hydrophobic chain.
[0040] Example 4
[0041] The present embodiment provides a method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, comprising the following steps:
[0042] N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide, 3-chloropropylmethyldimethoxysilane, potassium iodide and chloroform are added to a reaction container, wherein the molar ratio of N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide:3-chloropropylmethyldimethoxysilane:potassium iodide is
[0043] 1:1.0:0.01, stir at 30°C until the raw materials are completely dissolved, then continue to heat to 90°C for 8 hours, remove chloroform by vacuum distillation after the reaction, wash with ethanol until the washing liquid does not change color, and obtain a quaternary ammonium surfactant with a fluorocarbon-silicon-carbon double hydrophobic chain.
[0044] Example 5
[0045] The present embodiment provides a method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, comprising the following steps:
[0046] N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide, 3-chloropropylmethyldimethoxysilane, potassium iodide and acetone are added to a reaction container, wherein the molar ratio of N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide:3-chloropropylmethyldimethoxysilane:potassium iodide is
[0047] 1:2.0:0.03, stir at 50°C until the raw materials are completely dissolved, then continue to heat to 60°C for 4 hours, remove acetone by vacuum distillation after the reaction, wash with ethanol until the washing liquid does not change color, and obtain a quaternary ammonium surfactant with a fluorocarbon-silicon-carbon double hydrophobic chain.
[0048] Preparation of surface tension test samples: The fluorocarbon surfactants in Examples 1-5 were prepared into aqueous solutions of 0.005 mg / mL, 0.002 mg / mL and 0.001 mg / mL, respectively; commercially available perfluorooctyl sulfonyl quaternary ammonium salt surfactant (PFOS) and commercially available betaine type fluorocarbon surfactant (FS-50) were also prepared into solutions of the above concentrations.
[0049] Experimental design: According to the ring-pull method in GB / T 22237-2008, the surface tension of the new quaternary ammonium surfactant with fluorocarbon-silicon-carbon double hydrophobic chains was measured using an SFZL-A series automatic surface tension tester (Shanghai Yingnuo Precision Instrument Co., Ltd.).
[0050] The test results are shown in Table 1:
[0051] Table 1 Surface tension of aqueous solutions of various substances at different concentrations (mN / m)
[0052]
[0053] As can be seen from Table 1, although the surface tension of the quaternary ammonium salt surfactant with fluorocarbon-silicon-carbon double hydrophobic chain obtained in Examples 1-5 is higher than that of imported PFOS at high concentration (concentration of 0.005 mg / mL), when the concentration is reduced to below 0.002 mg / mL, the surface tension of the novel sulfonate anionic surfactant containing double fluorocarbon short chains is lower than that of imported PFOS and PFOA. This shows that the fluorocarbon surfactant of the present invention is better than imported PFOS and PFOA at low concentrations. In addition, the surface tension of the fluorocarbon surfactant of the present invention at the same concentration is significantly lower than that of commercially available FS-50, that is, the fluorocarbon surfactant of the present invention has stronger surface activity.
[0054] Contact angle test sample preparation: The fluorocarbon surfactants in Examples 1-5 were prepared at 0.005 mg / mL, 0.002 mg / mL, 0.001 mg / mL, 5×10 -4 mg / mL and 2×10 -4 mg / mL aqueous solution; commercially available perfluorooctyl sulfonyl quaternary ammonium salt surfactant (PFOS) and commercially available betaine type fluorocarbon surfactant (FS-50) were also prepared into solutions of the above concentrations.
[0055] Experimental design: According to the contact angle method in GB / T 30693-2014, a JCY-3 contact angle meter (Shanghai Fangrui Instrument Co., Ltd.) was used to measure the contact angle of a new quaternary ammonium surfactant solution with a fluorocarbon-silicon-carbon double hydrophobic chain using a polytetrafluoroethylene plate (PTFE, an ultra-low surface energy hydrophobic material) as the test substrate.
[0056] The test results are shown in Table 2:
[0057] Table 2 Contact angles of aqueous solutions of various substances at different concentrations (°)
[0058]
[0059] As can be seen from Table 2, the contact angles of Examples 1-5 are lower than those of imported PFOS and commercial FS-50, indicating that the wetting performance of the quaternary ammonium salt surfactant solution with fluorocarbon-silicon-carbon double hydrophobic chains is better than that of PFOS and FS-50. -4 At a concentration of 2×10 -4 When the concentration of fluorosilicone surfactant is 200 mg / mL, the contact angle is about 44-46°, and the PTFE plate can be well wetted. This shows that the fluorosilicone surfactant of the present invention not only has excellent wetting properties, but also has a lower usage concentration.
[0060] Preparation of samples for foaming power and foaming stability tests: The fluorocarbon surfactants in Examples 1 and 2 were prepared into aqueous solutions of 0.01 mg / mL, 0.005 mg / mL, 0.002 mg / mL and 0.001 mg / mL, respectively; commercially available perfluorooctyl sulfonyl quaternary ammonium salt surfactant (PFOS) and commercially available betaine type fluorocarbon surfactant (FS-50) were also prepared into solutions of the above concentrations.
[0061] Experimental design: According to the improved Ross-Miles method in GB / T 7462-1994, the foaming power of the new quaternary ammonium surfactant solution with fluorocarbon-silicon-carbon double hydrophobic chains was measured at room temperature (25°C) using an improved Ross foam instrument (Shenzhen Sanli Technology Co., Ltd.). The foam height at 30s and 5min after the liquid flow stopped was observed. The foam height at 30s h was taken as the value of the foam height. 0 As a measure of foaming power, the residual foam ratio R5 is used as a measure of foaming stability (R 5 =h 0 / h 5 ).
[0062] The test results are shown in Table 3, Table 4 and Table 5:
[0063] Table 3 Foam height h of each substance solution at different concentrations at 30s 0 (mm)
[0064]
[0065] Table 4 Foam height h of each substance solution at different concentrations at 5 min 5 (mm)
[0066]
[0067] Table 5 Residual foam ratio R of each substance at different concentrations 5 (%)
[0068]
[0069] It can be seen from the foam height of Example 1 and Example 2 in Table 3 that when the solution concentration is high (0.01mg / mL and 0.005mg / mL), the foaming power of the novel quaternary ammonium salt surfactant with fluorocarbon-silicon-carbon double hydrophobic chain of the present invention is approximately equal, but when the concentration decreases (0.002mg / mL and 0.001mg / mL), the foaming power will have a relatively large decrease. Comparing the data in Table 3, it can be found that no matter it is high concentration or low concentration, the foaming power of the fluorosilicone surfactant of the present invention is higher than that of imported PFOS and commercially available FS-50. Comparing the data in Table 5, it can be found that no matter it is the fluorosilicone surfactant of the present invention, or imported PFOS and commercially available FS-50, the residual foam ratio all presents a trend of decreasing as the concentration decreases. Moreover, it can be clearly seen that the residual foam ratio of the fluorosilicone surfactant of the present invention is much higher than that of imported PFOS and commercially available FS-50, that is, the fluorosilicone surfactant of the present invention has better foaming stability.
[0070] The fluorosilicone surfactant of the present invention does not contain perfluorooctanoic acid (PFOA) and perfluorohexane sulfonic acid (PFHxS) substances, has environmentally friendly characteristics, will not affect the human nervous system, immune system, endocrine system and genetic information, etc., can effectively generate foam, has good heat stability, can improve the foaming performance and anti-burning performance of the foam fire extinguishing agent, and as a wetting agent, can reduce the surface tension of the aqueous solution and wet the low-energy surface.
[0071] In addition to the above embodiments, the present invention may also have other implementation modes. Any technical solution formed by equivalent replacement or equivalent transformation falls within the protection scope required by the present invention.
Claims
1. A quaternary ammonium surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain, characterized in that: The structural formula of the surfactant is:
2. A method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain as claimed in claim 1, characterized in that: Specifically: Add N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide, 3-chloropropylmethyldimethoxysilane, potassium iodide and a solvent into a reaction container, heat up and stir until the raw materials are completely dissolved, then continue to heat up to react, and after the reaction is completed, remove the solvent by distillation under reduced pressure, wash with ethanol until the washing liquid does not change color, to obtain a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain.
3. The method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain according to claim 2, wherein: The molar ratio of N-((dimethylamino)methyl)-4,4,5,5,6,6,6-heptafluoro-3,3-bis(trifluoromethyl)hexanamide:3-chloropropylmethyldimethoxysilane:potassium iodide is 1:(1.0-2.0):(0.01-0.03).
4. The method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain according to claim 2, wherein: The solvent is one of acetonitrile, toluene, benzene, cyclohexane, chloroform, acetone, N,N-dimethylacetamide or N,N-dimethylformamide.
5. The method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain according to claim 2, wherein: The temperature of the heating and stirring is 30-50°C.
6. The method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain according to claim 2, wherein: The temperature of the temperature-raising reaction is 60-90°C.
7. The method for preparing a quaternary ammonium salt surfactant having a fluorocarbon-silicon-carbon double hydrophobic chain according to claim 2, characterized in that: The temperature rising reaction time is 4-8h.
Citation Information
Patent Citations
Preparation method and application of quaternary ammonium salt surfactant containing branch-type fluorocarbon chain
CN102921347A
Fluorocarbon surfactant as well as preparation method and application thereof
CN113559783A
Foam extinguishing agent based on fluorocarbon-organosilicon surfactant compound system
CN114618112A
Novel fluorocarbon betaine surfactant and preparation method thereof
CN116144377A
Branched chain type fluorocarbon surfactant and preparation method thereof
CN116410104A
Cited By
Multifunctional organic silicon glycosyl amide cationic surfactant as well as preparation method and application thereof
CN119529857A