Glue solution coating control method of water-based pressure-sensitive adhesive coating compound equipment

By constructing the substrate parameter grid and optimizing the coating process, the problem of inaccurate flow and drying control of glue liquid in water-based pressure-sensitive adhesive coating is solved, and the technical effect of coating uniformity and thickness consistency is achieved, which improves the product Quality and productivity.

CN118904663AActive Publication Date: 2024-11-08GUANGDONG JUDE MASCH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411053328.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-11-08
Estimated Expiration
2044-08-01

AI Technical Summary

Technical Problem

In the existing water-based pressure-sensitive adhesive coating technology, the flow and drying of the glue liquid are inaccurate, resulting in uneven coating, inconsistent thickness and poor drying effect, affecting product quality and production efficiency.

Method used

By obtaining the substrate information and coating position information of medical substrates, the substrate parameter grid is constructed, the grid is merged and the grid is coated in one go, the deviation coefficient and state results are analyzed, the grid is arranged with priority, and the expected data is calculated to achieve a secondary Coating, precisely control the glue coating process.

Benefits of technology

Accurate control of the coating process is achieved, coating uniformity is improved, coating thickness is ensured, and product quality and production efficiency are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118904663A_ABST
    Figure CN118904663A_ABST
Patent Text Reader

Abstract

The invention provides a glue solution coating control method of water-based pressure-sensitive adhesive coating composite equipment, and relates to the technical field of coating control, and the glue solution coating control method comprises the following steps: constructing a base material parameter grid, and merging to obtain a base material merged grid; carrying out primary coating on the base material parameter grids one by one to obtain first coating data of the base material combined grids; performing deviation analysis of a first coating reference value on the first coating data to generate a first coating deviation coefficient of each base material parameter grid; performing state evaluation on the base material combined grid to generate a first coating state result; performing priority arrangement on the base material parameter grids to obtain a second coating grid queue; and performing secondary coating on the second coating grid queue to obtain second coating data. The technical problem that in the prior art, the coating process is not accurate due to flowing and drying control of the glue solution can be solved, the technical aim of accurately controlling the glue solution coating process is achieved, and the technical effects of improving the coating uniformity and ensuring the consistent coating thickness are achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of coating control, and in particular to a method for controlling adhesive coating of a water-based pressure-sensitive adhesive coating composite device. Background Art

[0002] In the medical industry, water-based pressure-sensitive adhesive coating technology is widely used in the manufacture of medical tapes, patches and other products. However, the existing coating technology has some obvious defects. First, due to the limited precision of the coating equipment, the glue coating is uneven, affecting the product quality. Secondly, the flow and drying control of the glue is not precise enough, which is prone to problems such as inconsistent coating thickness and poor drying effect. In addition, environmental factors such as temperature and humidity in the coating process have not been fully considered, resulting in unstable production process. In order to overcome these defects, more advanced coating control methods need to be developed to improve coating uniformity and stability and ensure product quality and production efficiency.

[0003] In summary, the prior art has technical problems in that the coating process is not precisely controlled due to the flow and drying of the glue, resulting in uneven coating, inconsistent thickness and poor drying effect during multiple glue coating processes, further affecting product quality and production efficiency. Summary of the invention

[0004] The purpose of the present application is to provide a method for controlling the coating of a water-based pressure-sensitive adhesive coating composite device, so as to solve the technical problem in the prior art that the coating process control is not accurate due to the flow and drying control of the glue, resulting in uneven coating, inconsistent thickness and poor drying effect during multiple glue coating processes, further affecting product quality and production efficiency.

[0005] In view of the above problems, the present application provides a method for controlling the coating of an adhesive solution of a water-based pressure-sensitive adhesive coating composite device.

[0006] The present application provides a method for controlling glue coating of a water-based pressure-sensitive adhesive coating composite device, comprising: acquiring substrate information and coating position information of a medical substrate to construct a substrate parameter grid, merging the substrate parameter grids to obtain a substrate merged grid; coating the medical substrate once per substrate parameter grid with a first coating reference value to obtain first coating data of the substrate merged grid; performing a deviation analysis of the first coating reference value on the first coating data to generate a first coating deviation coefficient for each substrate parameter grid; performing a state evaluation on the substrate merged grid based on a first glue state threshold to generate a first coating state result; prioritizing the substrate parameter grids according to the first coating state result and the first coating deviation coefficient to obtain a second coating grid queue; calculating the expected second coating data to perform a second coating on the second coating grid queue to obtain second coating data.

[0007] One or more technical solutions provided in this application have at least the following technical effects or advantages:

[0008] A substrate parameter grid is constructed by acquiring substrate information and coating position information of a medical substrate, and the substrate parameter grids are merged to obtain a substrate merged grid; the medical substrate is coated once on each substrate parameter grid with a first coating reference value to obtain first coating data of the substrate merged grid; the first coating data is subjected to a deviation analysis of the first coating reference value to generate a first coating deviation coefficient for each substrate parameter grid; the state of the substrate merged grid is evaluated based on a first glue state threshold to generate a first coating state result; the substrate parameter grids are prioritized according to the first coating state result and the first coating deviation coefficient to obtain a second coating grid queue; the expected second coating data is calculated to coat the second coating grid queue for a second time to obtain second coating data, thereby achieving the technical goal of accurately controlling the glue coating process and achieving the technical effect of improving coating uniformity and ensuring consistent coating thickness.

[0009] The above description is only an overview of the technical solution of the present application. In order to more clearly understand the technical means of the present application, it can be implemented according to the contents of the specification, and in order to make the above and other purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are specifically cited below. It should be understood that the content described in this section is not intended to identify the key or important features of the embodiments of the present application, nor is it intended to limit the scope of the present application. Other features of the present application will become easy to understand through the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] In order to more clearly illustrate the technical solutions in the present application or the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings in the following description are only exemplary, and for ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying any creative work.

[0011] Figure 1 This is a schematic flow chart of a method for controlling the coating of adhesive solution of a water-based pressure-sensitive adhesive coating composite device of the present application;

[0012] Figure 2 This is a flow chart of generating a first coating state result in a glue solution coating control method of a water-based pressure-sensitive adhesive coating composite device of the present application. DETAILED DESCRIPTION

[0013] The present application provides a method for controlling the coating of a water-based pressure-sensitive adhesive composite coating device, which solves the technical problem in the prior art that the coating process control is not precise due to the flow and drying control of the adhesive, resulting in uneven coating, inconsistent thickness and poor drying effect during multiple adhesive coating processes, further affecting product quality and production efficiency. The technical goal of accurately controlling the adhesive coating process is achieved, and the technical effect of improving coating uniformity and ensuring consistent coating thickness is achieved.

[0014] Below, the technical solutions in the present application will be clearly and completely described with reference to the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments of the present application. It should be understood that the present application is not limited to the example embodiments described herein. Based on the embodiments of the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present application. It should also be noted that, for the convenience of description, only the parts related to the present application are shown in the accompanying drawings, rather than all of them.

[0015] For examples, please see the attached Figure 1 The present application provides a method for controlling the coating of a water-based pressure-sensitive adhesive composite device, which specifically includes:

[0016] Step 1: Obtain substrate information and coating position information of the medical substrate to construct a substrate parameter grid, and merge the substrate parameter grids to obtain a substrate merged grid.

[0017] Specifically, the substrate information and coating position information of the medical substrate are obtained to collect all necessary data related to the coating process. The coating position information includes the various positions of the substrate during the coating process. The substrate information includes the type, thickness, surface treatment, strength, water absorption, etc. of the substrate, as well as the specific data of the coating position information, such as coating speed, coating thickness, etc. The substrate information and coating position information are the basis for subsequent analysis and optimization to ensure that the entire coating process can be accurately controlled. By comprehensively and accurately acquiring these data, a solid foundation can be laid for building a more refined and accurate substrate parameter grid.

[0018] Then, the construction of the substrate parameter grid is to combine the acquired substrate information and coating position information, that is, to obtain the substrate parameter grid according to the coating position information and the corresponding substrate information. Each substrate parameter grid represents a specific position and the corresponding parameter value, which can intuitively display and analyze the parameter changes at each position during the coating process, and provide clear guidance for subsequent merging and optimization.

[0019] Next, merging substrate parameter grids is to integrate the initially constructed substrate parameter grids to form a comprehensive substrate merged grid, and merging adjacent substrate parameter grids to improve data processing efficiency.

[0020] Step 2: coating the medical substrate once for each substrate parameter grid with a first coating reference value to obtain first coating data of the substrate merged grid.

[0021] Specifically, the first coating reference value is used to coat the medical substrate one by one according to the substrate parameter grid, that is, to perform the initial coating operation on each substrate parameter grid according to the set reference parameters (such as coating thickness, speed, etc.), that is, according to the first coating reference value. The first coating reference value is set according to actual needs and technical requirements to ensure the quality and consistency of the initial coating. During the first coating process, each substrate parameter grid will be coated with a layer of glue to ensure the initial coverage of the entire substrate.

[0022] Then, obtaining the first coating data of the substrate merged grid refers to collecting and recording the actual coating results of each substrate parameter grid after completing the initial coating operation. The first coating data includes various parameters such as actual coating thickness, uniformity, viscosity, and degree of dryness. Through the analysis of the first coating data, the effect and quality of the initial coating can be judged, possible problems and uneven areas can be identified, and the coating data of each substrate parameter grid can be ensured to be accurate, thereby providing a reliable basis for subsequent process adjustments. For example, in the process of obtaining the substrate merged grid, an optical monitoring system and a sensor are used to monitor and record the coating effect of each substrate parameter grid in real time. Through the optical monitoring system, the coating thickness and uniformity data of each substrate parameter grid can be obtained in real time, and the first coating data is transmitted to the control system for analysis and processing. At the same time, the sensor can monitor parameters such as ambient temperature, humidity, and dry state to ensure that the coating conditions of each substrate parameter grid are consistent.

[0023] Step three: performing deviation analysis of the first coating reference value on the first coating data to generate a first coating deviation coefficient for each substrate parameter grid.

[0024] Specifically, the deviation analysis of the first coating data from the first coating reference value refers to comparing the first coating data after actual coating with the preset first coating reference value to find out the difference between each substrate parameter grid and the ideal state. For example, by calculating the difference between the actual coating thickness, uniformity and other parameters of each substrate parameter grid and the reference value, the deviation data is generated to intuitively reflect the problems and non-uniformity in the coating process.

[0025] Then, the first coating deviation coefficient of each substrate parameter grid is generated by quantifying the deviation analysis results. The first coating deviation coefficient is an indicator that describes the degree of difference between the actual coating effect and the ideal reference value, usually expressed as a percentage or numerical value. Specifically, it can be obtained by calculating the ratio of the difference between the first coating data and the first coating reference value to the first coating reference value. By calculating the first coating deviation coefficient of each substrate parameter grid, the deviation of each grid unit can be intuitively displayed. The larger the deviation coefficient, the greater the gap between the actual coating effect and the ideal state, and the need to focus on adjustment and optimization in the subsequent coating process. On the contrary, the smaller the gap between the actual coating effect and the ideal state.

[0026] Step 4: Evaluate the state of the substrate merged grid based on the first glue state threshold to generate a first coating state result.

[0027] Specifically, by conducting a detailed evaluation of the actual coating status of each substrate parameter grid in the substrate merged grid, it is determined whether the coating process has reached the expected standard and a first coating status result is generated. That is, by calculating and analyzing the fitness value of each grid cell, a detailed fitness distribution map is generated, and the coating quality problem areas are identified. Finally, the first coating status result is generated, so that subsequent coating operations can be carried out.

[0028] Step 5: Prioritize the substrate parameter grids according to the first coating state result and the first coating deviation coefficient to obtain a second coating grid array.

[0029] Specifically, after the first coating is completed and the coating effect is analyzed, each substrate parameter grid is evaluated in detail based on the actual state results of the first coating and the deviation coefficient of each grid. The coating state results reflect the performance of each substrate parameter grid in the first coating, such as coating thickness, uniformity, etc., while the deviation coefficient quantifies the difference between the actual performance and the expected standard. By combining the two indicators, the specific situation of each grid can be fully understood, and the second coating grid lineup can be obtained, providing a scientific basis for subsequent optimization and adjustment.

[0030] Step 6: Calculate the expected second coating data and perform a second coating on the second coating grid array to obtain the second coating data.

[0031] Specifically, after obtaining the deviation coefficient of the first coating, the specific coating parameters required for each substrate parameter grid in the second coating are determined. The expected second coating data includes coating thickness, coating speed, glue flow rate, etc., the purpose is to make up for the deviation in the first coating and make the second coating more uniform and meet the standards. For example, for grids with large deviations, it is necessary to increase or decrease the coating amount, adjust the speed, etc. to achieve the expected effect. Then, according to the pre-arranged priority order, the actual secondary coating operation is performed on each substrate parameter grid.

[0032] The glue coating control method of the water-based pressure-sensitive adhesive coating composite equipment can achieve the technical goal of accurately controlling the glue coating process, and achieve the technical effects of improving coating uniformity and ensuring consistent coating thickness.

[0033] Further, if Figure 2 As shown, this application also includes:

[0034] The upper and lower limits of the glue state are extracted according to the key parameters of the glue to form a first glue state threshold; the first glue state is extracted from the first glue state threshold; the first glue state is used as the initial particle, and it is moved in the first glue state threshold according to a preset step size to obtain an iterative particle; the iterative particle is evaluated based on the state function, if the state fitness of any iterative particle is higher than the state fitness of the previous iterative particle, it is retained and updated until an iterative stagnation result is obtained; the iterative result obtained by iterating the iterative stagnation result is used as the first glue state, if the substrate merged grid reaches the first glue state, the state evaluation is qualified, and the first coating state result is generated.

[0035] Specifically, the upper and lower limits of the glue state are extracted according to the key parameters of the glue to form the first glue state threshold, and the acceptable range of the glue state is determined. For example, key parameters include viscosity, degree of dryness, etc., which are set based on experimental data and process requirements. The upper limit represents the maximum acceptable value of the key parameters of the glue, and the lower limit represents the minimum acceptable value. By determining the upper and lower limits to form the first glue state threshold, it can be ensured that the glue remains in the best state during the coating process, thereby achieving an ideal coating effect.

[0036] Then, extracting the first glue state from the first glue state threshold means, after determining the upper and lower limits of the glue key parameters, selecting a specific state of the glue key parameters within its acceptable range as the initial state, for subsequent optimization and adjustment starting from the first glue state. The selection of the first glue state is usually based on empirical data and preliminary experimental results in actual production to ensure that it has high adaptability and feasibility.

[0037] Next, the first glue state is used as the initial particle, and it is moved in the first glue state threshold according to the preset step length to obtain iterative particles, and parameter adjustment and optimization are performed. Based on the initial state, multiple new iterative particles are generated by moving in the parameter space according to the preset step length. Iterative particles represent different glue states, and the purpose is to explore the entire glue state space to find the best combination of glue states for secondary coating.

[0038] Next, the state of the iterative particles is evaluated based on the state function. If the state fitness of any iterative particle is higher than that of the previous generation of particles, the update is retained until the iteration stagnation result is obtained. The fitness of each iterative particle is evaluated by defining a state function, which is usually based on the evaluation index of the actual coating effect, such as coating thickness, viscosity, etc. If the fitness of an iterative particle is higher than that of the previous iterative particle, it is updated to the new optimal particle, and the iteration continues until the fitness is no longer significantly improved, that is, the iteration stagnation state is reached.

[0039] Next, the iterative result obtained by iterating the iterative stagnation result is used as the first glue state. If the substrate merged grid reaches the first glue state, the state evaluation is qualified, and the first coating state result is generated. Finally, through multiple iterations and optimizations, an optimal glue state is determined, which is the first glue state. Then, in the actual coating process, if the coating effect of each substrate parameter grid in the substrate merged grid can reach or approach the first glue state, it means that the coating process meets expectations, the state evaluation is qualified, and finally the first coating state result is generated to ensure coating quality and consistency.

[0040] The first glue state threshold is formed by extracting the upper and lower limits of the key parameters of the glue, from which the initial glue state is extracted and used as the initial particle, and the optimization algorithm is used for iteration. The iterative particles are evaluated and updated based on the state function until the iterative stagnation result is obtained. The iterative result is used as the first glue state, and in the actual coating process, it is verified whether the substrate merged grid reaches this state, thereby ensuring the uniformity and quality of the coating process, which can effectively improve the stability and reliability of the coating process.

[0041] Furthermore, the present application also includes:

[0042] The state function is: Among them, SD fit is the surface dryness adaptability, SD actual is the actual surface dryness, SD std is the standard surface dryness, V fic is the viscosity adaptability, V actual is the actual viscosity, V std is the standard viscosity, SFfit is the flatness adaptability, SF actual is the actual flatness, SF std For standard flatness, DT fit Drying time adaptability, DT actual is the actual drying time, DT std is the standard drying time, T fit is the temperature adaptation, T actual is the actual temperature, T std is the standard temperature, H fit is humidity adaptability, H actual is the actual humidity, H std is the standard humidity, Total fit is state fitness, SD fit 、V fit , SF fit , DT fit , T fit , H fit and Total fit The value range of is [0, 1], ω1, ω2, ω3, ω4, ω5 and ω6 are SD fit 、V fit , SF fit , DT fit , T fit , H fit The weight of .

[0043] Specifically, the state function is used to comprehensively evaluate the state of the glue liquid. fit The value range of is between 0 and 1. The closer the value is to 1, the more suitable the glue state is for the current coating requirements, and vice versa. Among them, the surface dryness adaptability is calculated by comparing the actual surface dryness and the standard surface dryness, ensuring that when the actual surface dryness is close to the standard surface dryness, the adaptability is close to 1, and vice versa it decreases. Similarly, when the actual viscosity is close to the standard viscosity, the adaptability is high, and vice versa it is low. The closer the actual flatness is to the standard value, the higher the adaptability, and vice versa it is low. When the actual drying time is close to the standard drying time, the adaptability is high, and vice versa it is low. When the actual temperature is close to the standard temperature, the adaptability is high, and vice versa it is low. When the actual humidity is close to the standard humidity, the adaptability is high, and vice versa it is low.

[0044] Finally, the fitness of each iteration is weighted and summed to obtain the comprehensive state fitness, which is used to evaluate the overall state of the glue. If the state fitness of a particle in a certain iteration is higher than that of the particle in the previous iteration, it is retained and updated until the iteration stops and the final optimal glue state is determined, ensuring the continuous optimization of the glue state until the optimal conditions are reached.

[0045] Furthermore, the present application also includes:

[0046] According to the iterative stagnation result, the local optimal escape of the iterative particle under the preset local step size is performed, and the iteration is continued according to the local optimal escape result; if the state fitness of any local particle is higher than the state fitness of the local particle of the previous iteration, the update is retained until the local iterative stagnation result is obtained; the local iterative stagnation results are integrated to obtain the iterative result.

[0047] Specifically, the local optimal escape of iterative particles under a preset local step size according to the iterative stagnation result means that after reaching a stagnation state in the initial iteration process, a preset local step size is set to explore near the current parameter space to find a better local solution. The local optimal escape is to avoid the key parameters of the glue liquid from falling into the local optimal solution. The key parameters of the glue liquid are moved and adjusted within a small range near the solution of each current key parameter of the glue liquid to explore new possibilities for each key parameter of the glue liquid. Specifically, the size and direction of the preset step size can be determined by random generation or setting, thereby generating new iterative particles and entering the new parameter space for optimization.

[0048] Then, continuing to iterate based on the local optimal escape result means continuing iterative calculation and optimization based on the local optimal escape. By evaluating the state fitness of the new iterative particles, if the new iterative particles find a better solution in the local range, further optimization and adjustment will be performed based on the new solution. Repeat until no better solution can be found, that is, a new local iterative stagnation state is reached.

[0049] Then, if the state fitness of any local particle is higher than the state fitness of the local particle in the previous iteration, the update is retained until the local iteration stagnation result is obtained. That is, in each local optimal escape and iteration process, if a new particle is found with a state fitness higher than the previous particle, the current optimal solution is updated and the iteration is continued until the fitness of all particles is no longer significantly improved, and the local iteration stagnation result is achieved, ensuring that each iteration can find the optimal solution in the current parameter space.

[0050] Next, integrating the local iteration stagnation results to obtain the iteration results means that after all local iteration processes are completed, the optimal results of each local iteration stagnation are integrated to form a comprehensive iteration result. The iteration result represents the optimal glue state parameter of each key glue parameter found in the glue state after the entire first coating. By integrating various local optimal results, it can be ensured that the glue state setting of the entire coating process reaches the global optimum, thereby achieving the best glue coating effect, which is used for secondary coating when the glue coating state is the best, to prevent the glue after the first coating from being unable to adhere to the glue for the second coating or the glue for the first coating from flowing, resulting in the inability to perform secondary coating.

[0051] Through the initial iterative stagnation results, local optimal escape is performed, and exploration and optimization are continued at the preset step size to find the local optimal solution, and the optimal solution is updated through continuous iteration and evaluation until local iterative stagnation is reached. Finally, all local iterative stagnation results are integrated to obtain the global iterative optimal result. Through systematic exploration and optimization, it is ensured that all parameters in the glue coating process reach the optimal state, providing high-quality and consistent coating effects.

[0052] Furthermore, the present application also includes:

[0053] According to the first coating state result, the substrate parameter grids are arranged with high priority to obtain a second coating grid high priority queue; according to the first coating deviation coefficient, the substrate parameter grids are arranged with low priority to obtain a second coating grid low priority queue; from the second coating grid high priority queue and the second coating grid low priority queue, the same-order substrate parameter grids are extracted, and the same-order substrate parameter grids are fixed to the second coating grid queue; from the second coating grid high priority queue and the second coating grid low priority queue, the different-order substrate parameter grids are extracted, and the different-order substrate parameter grids are fixed to the second coating grid queue according to the different-order evaluation results; the same-order substrate parameter grids and the different-order substrate parameter grids are fixed to obtain the second coating grid queue.

[0054] Specifically, the substrate parameter grids are arranged with high priority according to the first coating state result to obtain a second coating grid high priority queue. Based on the initial coating result, the substrate parameter grids whose coating state after the first coating is suitable for rapid second coating, that is, the substrate parameter grids with higher fitness are arranged with high priority, indicating that the substrate parameter grids have reached or are close to a state suitable for rapid second coating after the first coating, and therefore a high quality standard can continue to be maintained in subsequent coatings.

[0055] Next, the substrate parameter grids are arranged with low priority according to the first coating deviation coefficient to obtain the second coating grid low priority queue, and the substrate parameter grids whose coating effect after the first coating is significantly different from the required benchmark of the first coating, that is, the substrate parameter grids with a larger first coating deviation coefficient are arranged with low priority, indicating that there is a large gap with the ideal state in the first coating, so it needs to be adjusted and optimized in the subsequent coating, but the priority is still lower than the high priority arrangement method in which the glue liquid state reaches the state that can be immediately coated for the second time. Through low priority arrangement, it can be ensured that the problem areas are solved first in the second coating process to improve the overall coating quality.

[0056] Then, the substrate parameter grids of the same order are extracted from the high priority queue and the low priority queue respectively, and the substrate parameter grids of the same order are fixed in the second coating grid queue to be coated for the second time.

[0057] Next, the substrate parameter grids of different priorities are extracted from the high priority queue and the low priority queue, and fixed according to their specific evaluation results. By arranging them in different priorities, it can be ensured that the status and requirements of each substrate parameter grid are fully considered, and targeted adjustments and optimizations can be made during the second coating process.

[0058] By coordinating high and low priorities, the coating quality can be effectively improved during the second coating process. By executing fixed steps, a well-structured and prioritized coating plan can be formed, providing strong guidance for the second coating.

[0059] Furthermore, the present application also includes:

[0060] Extract high-level iso-orders and low-level iso-orders from the second coating grid high-priority queue and the second coating grid low-priority queue, and calculate the iso-order difference between the high-level iso-order and the low-level iso-order; determine whether the iso-order difference satisfies the order difference of the iso-order arrangement threshold; if so, fix the iso-order substrate parameter grid in the second coating grid queue based on the priority order of the high-level iso-order and the low-level iso-order, and obtain a first evaluation result of the iso-order substrate parameter grid and add it to the iso-order evaluation result.

[0061] Specifically, the substrate parameter grids in different orders in the coating grids of the second coating grid high priority queue and the second coating grid low priority queue are extracted respectively. The high order indicates the order in the second coating grid high priority queue, while the low order indicates the order in the second coating grid low priority queue.

[0062] Next, the iso-sequence difference between the high-order iso-sequence and the low-order iso-sequence is calculated, and the difference between the specific parameter values ​​of the high-order iso-sequence and the low-order iso-sequence is calculated.

[0063] Next, it is determined whether the iso-rank difference satisfies the rank difference of the iso-rank arrangement threshold, and it is determined according to the preset iso-rank arrangement threshold whether the calculated iso-rank difference is within the range of the substrate parameter grid that urgently needs to be coated, which is superimposed by two reasons: the state after the first coating is better and the error after the first coating is larger, and thus the second coating is urgently needed. If the iso-rank difference is less than or equal to the iso-rank arrangement threshold, the iso-rank substrate parameter grid is fixed in the second coating grid queue based on the priority of the high-level iso-rank and the low-level iso-rank, and the first evaluation result of the iso-rank substrate parameter grid is obtained and added to the iso-rank evaluation result. Among them, the first evaluation result includes the substrate parameter grid that is the substrate parameter grid that urgently needs to be coated, which is superimposed by two reasons: the state after the first coating is better and the error after the first coating is larger, and thus the second coating is urgently needed.

[0064] By extracting high-level heterologous orders and low-level heterologous orders in the second coating grid high priority queue and the second coating grid low priority queue, calculating the heterologous order difference, judging whether the order difference satisfies the heterologous order arrangement threshold, and fixing it based on the priority order, the priority order in the coating process can be further optimized, and the second coating grid queue can be generated, providing scientific and reasonable guidance for subsequent coating processes.

[0065] Furthermore, the present application also includes:

[0066] If not satisfied, the iso-sequence substrate parameter grid is fixed in the second coating grid queue based on the high-order iso-sequence, and the second evaluation result of the iso-sequence substrate parameter grid is obtained and added to the iso-sequence evaluation result.

[0067] Specifically, when the iso-rank difference does not meet the iso-rank arrangement threshold, the high-level iso-rank is directly used to fix the second coating grid queue. High-level iso-rank means that the glue state is better after the first coating, and it is suitable for the substrate parameter grid of the second coating to be quickly carried out. Therefore, even if the iso-rank difference is large, the use of high-level iso-rank parameters can still optimize the coating effect to a certain extent. After fixing, the iso-rank substrate parameter grid is evaluated to generate a second evaluation result. Among them, the second evaluation result includes that only one of the two reasons for the substrate parameter grid needs to be prioritized, but it is still arranged according to the high priority reason.

[0068] By extracting high-level and low-level isotopes from the isotope substrate parameter grid and calculating the isotope difference, if the difference does not meet the preset threshold, the parameters of the high-level isotope are fixed and a second evaluation result is generated to ensure that even in the case of a large isotope difference, the coating effect can still be optimized by selecting the parameters of the high-level isotope. By integrating the evaluation results, detailed guidance can be provided for the second coating, further improving the coating quality and consistency.

[0069] Furthermore, the present application also includes:

[0070] The expected second coating data is obtained by performing a deviation analysis based on the first coating deviation coefficient and the second coating reference value; and the second coating grid array is subjected to secondary coating based on the expected second coating data to obtain the second coating data.

[0071] Specifically, after the first coating is completed, the difference between the actual coating condition of the first coating and the coating reference value set for the second coating of each substrate parameter grid is calculated, indicating that the difference between the actual coating condition of the first coating and the coating reference value set for the second coating needs to be compensated for during the second coating. Then, using the expected second coating data, the substrate parameter grids in the second coating grid array are coated a second time to obtain the second coating data, ensuring that the second coating meets the standard.

[0072] Through detailed deviation analysis and precise parameter adjustment, the effect of secondary coating is ensured, and the quality and consistency of the coating process are improved.

[0073] In summary, the adhesive coating control method of a water-based pressure-sensitive adhesive coating composite device provided in this application has the following technical effects:

[0074] A substrate parameter grid is constructed by acquiring substrate information and coating position information of a medical substrate, and the substrate parameter grids are merged to obtain a substrate merged grid; the medical substrate is coated once on each substrate parameter grid with a first coating reference value to obtain first coating data of the substrate merged grid; the first coating data is subjected to a deviation analysis of the first coating reference value to generate a first coating deviation coefficient for each substrate parameter grid; the state of the substrate merged grid is evaluated based on a first glue state threshold to generate a first coating state result; the substrate parameter grids are prioritized according to the first coating state result and the first coating deviation coefficient to obtain a second coating grid queue; the expected second coating data is calculated to coat the second coating grid queue for a second time to obtain second coating data, thereby achieving the technical goal of accurately controlling the glue coating process and achieving the technical effect of improving coating uniformity and ensuring consistent coating thickness.

[0075] The above description of the disclosed embodiments enables those skilled in the art to implement or use the present application. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present application. Therefore, the present application will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.

[0076] Obviously, those skilled in the art can make various changes and modifications to the present application without departing from the spirit and scope of the present application. Thus, if these modifications and variations of the present application belong to the scope of the present application and its equivalent technology, the present application is also intended to include these modifications and variations.

Claims

1. A method for controlling the coating of adhesive solution of a water-based pressure-sensitive adhesive coating composite device, characterized in that: include: Acquiring substrate information and coating position information of the medical substrate to construct a substrate parameter grid, and merging the substrate parameter grids to obtain a substrate merged grid; Performing a coating on the medical substrate once for each substrate parameter grid with a first coating reference value to obtain first coating data of the substrate merged grid; Performing deviation analysis of the first coating reference value on the first coating data to generate a first coating deviation coefficient for each substrate parameter grid; Performing a state evaluation on the substrate merged grid based on a first glue state threshold to generate a first coating state result; Prioritizing the substrate parameter grids according to the first coating state result and the first coating deviation coefficient to obtain a second coating grid array; The expected second coating data is calculated, and the second coating grid array is coated a second time to obtain the second coating data.

2. The method for controlling the coating of a water-based pressure-sensitive adhesive composite coating device according to claim 1, characterized in that: The step of evaluating the state of the substrate merged grid based on the first glue state threshold to generate a first coating state result includes: Extracting the upper limit and lower limit of the glue state according to the key parameters of the glue to form a first glue state threshold; extracting a first glue state from the first glue state threshold; Taking the first colloid state as an initial particle, moving within the first colloid state threshold according to a preset step length to obtain an iterative particle; Performing a state evaluation based on a state function on the iterative particles, if the state fitness of any iterative particle is higher than the state fitness of the last iterative particle, retaining the update until an iterative stagnation result is obtained; The iterative result obtained by iterating the iterative stagnation result is used as the first glue liquid state. If the substrate merged grid reaches the first glue liquid state, the state evaluation is qualified, and the first coating state result is generated.

3. The method for controlling the coating of a water-based pressure-sensitive adhesive composite coating device according to claim 2, characterized in that: The state function is: Among them, SD fit is the surface dryness adaptability, SD actual is the actual surface dryness, SD std is the standard surface dryness, V fit is the viscosity adaptability, V actual is the actual viscosity, V std is the standard viscosity, SF fit is the flatness adaptability, SF actual is the actual flatness, SF std For standard flatness, DT fit Drying time adaptability, DT actual is the actual drying time, DT std is the standard drying time, T fit is the temperature adaptation, T actual is the actual temperature, T std is the standard temperature, H fit is humidity adaptability, H actual is the actual humidity, H std is the standard humidity, Total fit is state fitness, SD fit 、V fit , SF fit , DT fit 、T fit , H fit and Total fit The value range of is [0, 1], ω1, ω2, ω3, ω4, ω5 and ω6 are SD fit 、V fit , SF fit , DT fit 、T fit , H fit The weight of .

4. The method for controlling the coating of adhesive solution of a water-based pressure-sensitive adhesive coating composite device according to claim 3, characterized in that: The iterative result obtained by iterating the iterative stagnation result includes: Performing a local optimal escape of the iterative particle under a preset local step size according to the iterative stagnation result, and continuing to perform iteration according to the local optimal escape result; If the state fitness of any local particle is higher than the state fitness of the local particle in the previous iteration, the update is retained until the local iteration stagnation result is obtained; The local iteration stagnation results are integrated to obtain the iteration result.

5. The method for controlling the coating of adhesive solution of a water-based pressure-sensitive adhesive coating composite device according to claim 1, characterized in that: The step of prioritizing the substrate parameter grids according to the first coating state result and the first coating deviation coefficient to obtain a second coating grid array includes: Arranging the substrate parameter grids in high priority according to the first coating state result to obtain a second coating grid high priority queue; Arranging the substrate parameter grids in low priority according to the first coating deviation coefficient to obtain a second coating grid low priority queue; Extracting the same-order substrate parameter grids from the second coating grid high-priority queue and the second coating grid low-priority queue, and fixing the same-order substrate parameter grids to the second coating grid queue; Extracting heterogeneous substrate parameter grids from the second coating grid high priority queue and the second coating grid low priority queue, and fixing the heterogeneous substrate parameter grids to the second coating grid queue according to the heterogeneous evaluation results; The second coating grid array is obtained by fixing the same-sequence substrate parameter grid and the different-sequence substrate parameter grid.

6. The method for controlling the coating of adhesive solution of a water-based pressure-sensitive adhesive coating composite device according to claim 5, characterized in that: Get the evaluation results of the different rankings, including: Extracting high-level iso-sequences and low-level iso-sequences from the second coating grid high-priority queue and the second coating grid low-priority queue, and calculating iso-sequence differences between the high-level iso-sequences and the low-level iso-sequences; Determine whether the out-of-order difference value satisfies the out-of-order arrangement threshold value; If satisfied, the iso-sequence substrate parameter grid is fixed in the second coating grid queue based on the priority of the high-order iso-sequence and the low-order iso-sequence, and the first evaluation result of the iso-sequence substrate parameter grid is obtained and added to the iso-sequence evaluation result.

7. The method for controlling the coating of adhesive solution of a water-based pressure-sensitive adhesive coating composite device according to claim 6, characterized in that: If not satisfied, the iso-sequence substrate parameter grid is fixed in the second coating grid queue based on the high-order iso-sequence, and the second evaluation result of the iso-sequence substrate parameter grid is obtained and added to the iso-sequence evaluation result.

8. The method for controlling the coating of adhesive solution of a water-based pressure-sensitive adhesive coating composite device according to claim 1, characterized in that: The calculating of the expected second coating data performs secondary coating on the second coating grid array to obtain the second coating data, including: Performing deviation analysis based on the first coating deviation coefficient and the second coating reference value to obtain the expected second coating data; The second coating grid array is coated a second time based on the expected second coating data to obtain second coating data.

Citation Information

Patent Citations

  • Self-adaptive spraying method

    CN111495635A

  • PVDC coating method based on finite element analysis, electronic equipment and system

    CN115526083A

  • Full-automatic coating machine and operation system

    CN116880391A

  • Layer thickness optimization and programming methods for a coating system and corresponding coating system

    DE102019113341A1