Method for producing industrial white oil
By using hydrogenation isomerial cracking catalysts with different activities combined with grading and refining catalysts in industrial white oil production, the problems of high wax content and high normal hydrocarbon content in high wax oil raw materials are solved, and the cracking reaction temperature rise is achieved The uniform distribution of temperature increases the yield and quality of white oil and reduces operating costs.
Patent Information
- Application Number
- CN202310511349.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-08
- Publication Date
- 2024-11-08
AI Technical Summary
The existing industrial white oil production process has harsh operating conditions, high cost and low yield, and has not been effectively studied for raw materials with high wax oil content.
Using the combination of hydroisomer cracking catalysts with different activities and the grading of hydroisomer cracking catalysts and the grading of hydroisomer cracking catalysts and refining catalysts, the temperature rise of the cracking reaction is reduced and the bed temperature is achieved. Evenly distributed, improving the yield and quality of white oil.
The cracking reaction temperature rise is small and the bed temperature is uniform, the yield and quality of white oil are improved, the aromatic content and pour point of the product are reduced, and the device operation cost is low.
Smart Images

Figure CN118909665A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of industrial white oil, and in particular relates to a method for producing industrial white oil. Background Art
[0002] Industrial white oil can be used in the fields of chemistry, textile, chemical fiber, petrochemical, electric power and agriculture. It is mainly used in the production of PE, PS and PU. It can be used as a wetting agent, solvent and lubricant in industries such as synthetic resin and plastic processing. It is also suitable for lubrication of textile machinery and precision instruments and sealing oil for compressors. It is mostly used to assist demoulding and increase product brightness. It can also be used as a lubricant for stamping molds.
[0003] The main white oil production technologies include: sulfuric acid sulfonation, sulfur trioxide gas sulfonation, solvent extraction and hydrogenation. With the increasingly stringent environmental protection requirements and the continuous improvement of white oil variety and quality requirements, the process of producing white oil by hydrogenation has become the mainstream technology at this stage, and a series of improvements have been made to this process in this field.
[0004] Patent document CN 110591757A discloses a hydrocracking reaction of catalytic diesel and coking diesel, and cutting and separating the products after the reaction to obtain naphtha, diesel and industrial white oil. The raw materials are petroleum-based raw materials and the catalyst is a molecular sieve cracking catalyst. The reaction pressure in the reaction of this patent is high (10-14MPa) and the operating conditions are harsh, which can easily cause the reactor to overheat and affect the product quality.
[0005] Patent document CN 110938458A discloses that the raw materials are pretreated to remove alkaline nitride and oxide impurities, and the pretreated products are adsorbed and separated to obtain extracted oil and raffinate oil, which are then separated by distillation to obtain high-quality white oil. The method of this patent has a long operation process and uses a special aromatic adsorbent. The aromatic content in the produced industrial white oil is 2.5-4wt%.
[0006] Patent document CN 101343558A discloses a method for producing high-viscosity industrial white oil, using catalytic cracking medium-quality lubricating oil base oil as raw material, and the kinematic viscosity at 40°C is 36-74mm 2 / s, and through hydrogenation refining, high-viscosity industrial white oil is produced; the method adopted in this patent has very strict requirements on raw materials, which limits its application.
[0007] Patent document CN109722292A discloses a hydrocracking method for producing crude white oil, wherein the raw oil adopts heavy raw oil with an aromatic content of 20-80%, wherein the reaction pressure is high (8-12MPa), the reaction temperature is high (250-450°C), and the hydrocracking catalyst is a molecular sieve catalyst with high cost.
[0008] Patent document CN101429457A discloses a method for hydrogenating distillate oil to produce more white oil. The raw oil is hydrocarbon oil, the reaction pressure is high (10-20 MPa), and the dewaxing catalyst is a precious metal molecular sieve catalyst, which is costly.
[0009] In the above-mentioned methods for producing white oil, the operating conditions are harsh, the cost is high, the yield is low, and no research has been conducted on high-wax oil as a raw material. In view of this, it is worthwhile to continue to develop and improve the process for producing white oil. Summary of the invention
[0010] The purpose of the present invention is to provide a method for producing industrial white oil in view of the problems existing in the white oil production process of the prior art, by utilizing the combined grading of hydroisomerization cracking catalysts with different activities and the grading of the hydroisomerization cracking catalyst and the refining catalyst, so as to achieve the effect of small temperature rise of the cracking reaction and uniform bed temperature distribution, while improving the yield and quality of the white oil.
[0011] In order to achieve the above object, the present invention provides the following technical solutions:
[0012] A method for producing industrial white oil is provided, comprising the following steps:
[0013] (1) In a hydrofining reactor, the raw wax oil is subjected to a hydrofining treatment to undergo deoxygenation and olefin hydrogenation saturation to obtain a refined wax oil;
[0014] (2) in a hydroisomerization cracking reactor, the refined wax oil is sequentially contacted with a hydroisomerization cracking catalyst and a supplementary refining catalyst laid on a catalyst bed and reacted to obtain isomerized dewaxed oil; wherein:
[0015] The hydroisomerization cracking catalyst is a combination of hydroisomerization cracking catalyst I and hydroisomerization cracking catalyst II (i.e., a combination of catalysts with different reaction activities, and the activity of hydroisomerization cracking catalyst I is higher than that of hydroisomerization cracking catalyst II), which is laid on the upper part of the catalyst bed; the supplementary refining catalyst is laid on the lower part of the catalyst bed;
[0016] (3) separating and cutting the isomerized dewaxed oil to obtain the industrial white oil (with a distillation range of 290° C. to 400° C.); optionally, part or all of the tail oil with a distillation range greater than 400° C. is recycled to the hydroisomerization cracking reactor;
[0017] The hydroisomerization cracking catalyst I and the hydroisomerization cracking catalyst II are both non-precious metal catalysts, and the catalyst carrier does not contain molecular sieves but contains amorphous silicon aluminum;
[0018] The mass ratio of the hydroisomerization cracking catalyst I to the hydroisomerization cracking catalyst II is 1:4-1:1 (e.g., 1:3.5, 1:3, 1:2.5, 1:2).
[0019] According to the method provided by the present invention, in some embodiments, the hydroisomerization cracking catalyst I comprises a carrier and an active component; the carrier is alumina and amorphous silica-alumina; the active component is at least one metal element selected from Group VIII and at least one metal element selected from Group VIB;
[0020] Based on the total weight of the hydroisomerization cracking catalyst I, the following components are included:
[0021] The content of amorphous silicon aluminum is 55-65wt% (e.g., 56wt%, 60wt%, 62wt%, 64wt%),
[0022] The content of aluminum oxide is 5-10wt% (e.g., 5.5wt%, 6wt%, 8wt%, 9wt%),
[0023] The content of the metal element of Group VIII in terms of oxide is 1-10 wt% (e.g., 1.5 wt%, 3 wt%, 4 wt%, 5 wt%, 8 wt%),
[0024] The content of the metal element of Group VIB in terms of oxide is 15-25 wt % (eg, 16 wt %, 18 wt %, 20 wt %, 24 wt %).
[0025] In some embodiments, the hydroisomerization cracking catalyst II comprises a carrier and an active component; the carrier is alumina and amorphous silica-alumina; the active component is at least one metal element selected from Group VIII and at least one metal element selected from Group VIB;
[0026] Based on the total weight of the hydroisomerization cracking catalyst II, the following components are included:
[0027] The amorphous silicon aluminum content is 35-50wt% (e.g., 36wt%, 40wt%, 42wt%, 45wt%, 48wt%),
[0028] The content of aluminum oxide is 10-30wt% (e.g., 12wt%, 14wt%, 15wt%, 20wt%, 25wt%, 28wt%),
[0029] The content of the metal element of Group VIII in terms of oxide is 1-10 wt% (e.g., 1.5 wt%, 3 wt%, 4 wt%, 5 wt%, 8 wt%),
[0030] The content of the metal element of Group VIB in terms of oxide is 20-40 wt % (eg, 22 wt %, 24 wt %, 25 wt %, 30 wt %, 35 wt %, 38 wt %).
[0031] In some embodiments, the metal element of Group VIB is molybdenum and / or tungsten, and the metal element of Group VIII is cobalt and / or nickel.
[0032] According to the method provided by the present invention, in some embodiments, in step (1), the catalyst used in the hydrofining treatment is a sulfided catalyst (that is, it can have the same composition as the supplementary refining catalyst), for example, FF66.
[0033] In some embodiments, the reaction conditions of the hydrofining treatment include: a reaction temperature of 200-350°C (e.g., 220°C, 250°C, 280°C, 300°C, 330°C), preferably 200-300°C, a reaction pressure of 2-12MPa (e.g., 3MPa, 4MPa, 5MPa, 8MPa), preferably 6-10MPa, and a liquid hourly volume space velocity of 0.5-10h -1 (For example, 0.6h -1 , 1.0h -1 , 2.5h -1 , 5.0h -1 , 8.0h -1 ), preferably 0.5-2h -1 .
[0034] In some embodiments, the raw wax oil is a hydrocarbon oil having a wax content greater than or equal to 40 wt% (e.g., 50 wt%, 60 wt%, 80 wt%) and a melting point greater than or equal to 50°C (e.g., 60°C, 80°C, 95°C), which is selected from one or more of petroleum-based hydrocracking tail oil, Fischer-Tropsch wax oil, hydrotreated wax oil, vacuum wax oil and coker wax oil, and is preferably Fischer-Tropsch wax oil.
[0035] In some embodiments, in step (1), the sulfur content of the refined wax oil is less than or equal to 10 ppm (e.g., 0 ppm, 1 ppm, 2 ppm, 4 ppm, 5 ppm, 8 ppm), and the nitrogen content is less than or equal to 5 ppm (e.g., 0 ppm, 0.5 ppm, 1 ppm, 2 ppm, 4 ppm).
[0036] In some embodiments, in step (2), the supplementary refined catalyst is a sulfided catalyst; for example, a catalyst of model FF-66.
[0037] In some embodiments, in step (2), the amount of the supplementary refining catalyst used is 5-25% (e.g., 6%, 10%, 15%, 20%) of the total mass of the hydroisomerization cracking catalyst I and the hydroisomerization cracking catalyst II.
[0038] In some embodiments, in step (2), the conversion depth of the hydroisomerization cracking reaction zone is controlled so that the single-pass conversion rate of the fraction >390°C is controlled to be 20-70% (e.g., 25%, 40%, 50%, 55%, 65%), preferably 30-60%.
[0039] In order to process high-wax oil to obtain high-quality industrial white oil, it is necessary to control the conversion depth of the hydroisomerization cracking reaction zone; if the conversion depth is low, the pour point of the white oil is unqualified, which will make the properties of the industrial white oil product poor; if the conversion depth is too high, although the properties of the industrial white oil product are qualified, the cracking reaction conditions are harsh, which will result in a low yield of the white oil product.
[0040] In some embodiments, in step (2), the hydroisomerization cracking reaction conditions include: a reaction temperature of 320-370°C (e.g., 325°C, 340°C, 355°C, 360°C), preferably 330-350°C, a reaction pressure of 5-12MPa (e.g., 5.5MPa, 8MPa, 9MPa, 11MPa), preferably 6-10MPa, and a liquid hourly volume space velocity of 0.5-10h -1 (For example, 0.6h -1 , 1.0h -1 , 2.5h -1 , 5.0h -1 , 8.0h -1 ), preferably 0.5-2h -1 .
[0041] The present invention grades a hydroisomerization cracking catalyst I and a hydroisomerization cracking catalyst II. The cracking activity of the hydroisomerization cracking catalyst I (its amorphous silicon aluminum content is high, the catalyst acidity is strong, and the activity is high) is higher than that of the hydroisomerization cracking catalyst II. In an industrial adiabatic reactor, the temperature rise of the cracking reaction can be reduced, the temperature distribution in the reactor is uniform, and excessive cracking is prevented, which can improve the yield of white oil. In addition, the use of amorphous silicon aluminum with a large pore size and weak acidity as a catalyst carrier can prevent the normal hydrocarbons in the wax oil from being excessively cracked, which is conducive to the diffusion of hydrocracking products. Hydroisomerization is carried out under the matching of hydrogenation function and acid function, which can reduce the pour point of the product to below -30°C, so that the condensation point of the raw material converted into the product can be reduced by more than 80°C, and the product yield is high and not less than 53%. At the same time, the proportion of the supplementary refining catalyst agent is controlled within a suitable range, which can reduce the content of olefins and aromatics in the product, and can make the Saybolt color number of the industrial white oil not less than +30 and the aromatics content not higher than 0.1%.
[0042] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:
[0043] The method adopts non-precious metal hydrocracking catalysts with different activities for grading, and the grading of refined catalysts and hydrocracking catalysts to produce industrial white oil, which solves the problems of high wax content, high normal hydrocarbon content, easy cracking, difficult to control reaction temperature rise, and low yield in raw wax oil; by using the combined grading of hydroisomerization catalysts with different activities, the advantages and improved effects of small cracking reaction temperature rise, small reactor bed temperature change, and uniform bed temperature distribution can be achieved. Compared with the process using a single catalyst, the industrial white oil production process of the present application avoids the problems of large cracking temperature rise and excessive cracking, which is beneficial to simultaneously improve the yield and quality of white oil (low aromatics content, low pour point, and qualified color), and the operating cost of the device is low. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] Figure 1 The present invention is a schematic diagram of the process of industrial white oil production shown in one embodiment of the present invention. DETAILED DESCRIPTION
[0045] In order to understand the technical features and contents of the present invention in detail, the preferred embodiments of the present invention will be described in more detail below. Although the preferred embodiments of the present invention are described in the embodiments, it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments described here.
[0046] In the present invention, it is possible to Figure 1 The flow chart shown is for the production of industrial white oil, which comprises the following steps:
[0047] (1) A hydrotreating catalyst is placed in a hydrotreating reactor, and Fischer-Tropsch wax is subjected to hydrotreating. The properties of the raw materials are shown in Table 1. Deoxygenation and olefin hydrogenation saturation occur to obtain refined wax oil; the sulfur content in the refined wax oil is less than or equal to 10 ppm, and the nitrogen content is less than or equal to 5 ppm; wherein,
[0048] The hydrotreating catalyst is of Ni-Mo series, which may be FF-66;
[0049] (2) laying a hydroisomerization cracking catalyst I, a hydroisomerization cracking catalyst II, and a supplementary refining catalyst in order from top to bottom in a hydroisomerization cracking reactor, introducing the refined wax oil obtained in step (1) into contact with the hydroisomerization cracking catalyst and the supplementary refining catalyst laid in the catalyst bed in order and reacting to obtain an isomerized dewaxed oil; wherein:
[0050] The hydroisomerization cracking catalyst is a combination of hydroisomerization cracking catalyst I and hydroisomerization cracking catalyst II, both of which can be prepared according to the method disclosed in patent CN107661756A;
[0051] The cracking activity of the hydroisomerization cracking catalyst I is higher than that of the hydroisomerization cracking catalyst II, and the mass ratio of the hydroisomerization cracking catalyst I to the hydroisomerization cracking catalyst II is 1:4 to 1:1;
[0052] The model of the supplementary refining catalyst laid at the bottom of the catalyst bed is FF-66, and its usage accounts for 5-20% of the total mass of the hydroisomerization cracking catalyst I and the hydroisomerization cracking catalyst II;
[0053] (3) Separating and cutting the isomerized dewaxed oil obtained in step (2) to obtain the industrial white oil (distillation range of 290° C.-400° C.), naphtha, and diesel (distillation range of 150-290° C.); part or all of the tail oil with a distillation range greater than 400° C. is recycled to the hydroisomerization cracking reactor.
[0054] <Source of raw materials>
[0055] Table 1 Physical and chemical properties of Fischer-Tropsch wax oil
[0056]
[0057] Example 1
[0058] Method for producing industrial white oil, with reference to Figure 1 The flowchart shown includes the following steps:
[0059] (1) A hydrorefining catalyst is placed in a hydrorefining reactor, and Fischer-Tropsch wax is hydrorefined. The properties of the raw materials are shown in Table 1. Deoxygenation and olefin hydrogenation saturation occur to obtain refined wax oil. The sulfur content and nitrogen content of the refined wax oil are 0 ppm and 0 ppm, respectively.
[0060] The hydrotreating catalyst is Ni-Mo series, model FF-66;
[0061] (2) laying a hydroisomerization cracking catalyst I, a hydroisomerization cracking catalyst II, and a supplementary refining catalyst in order from top to bottom in a hydroisomerization cracking reactor, introducing the refined wax oil obtained in step (1) into contact with the hydroisomerization cracking catalyst and the supplementary refining catalyst laid in the catalyst bed in order and reacting to obtain an isomerized dewaxed oil; wherein:
[0062] The hydroisomerization cracking catalyst is a combination of hydroisomerization cracking catalyst I and hydroisomerization cracking catalyst II, both of which are prepared according to the method disclosed in patent CN107661756A;
[0063] The mass fraction of NiO in the hydroisomerization cracking catalyst I (based on the total weight) is 6wt%, the mass fraction of WO3 is 24wt%, the mass fraction of amorphous silicon aluminum is 60wt%, and the mass fraction of aluminum oxide is 10wt%;
[0064] The mass fraction of NiO in the hydroisomerization cracking catalyst II (based on the total weight) is 6wt%, the mass fraction of WO3 is 28wt%, the mass fraction of amorphous silicon aluminum is 40wt%, and the mass fraction of aluminum oxide is 26wt%;
[0065] The cracking activity of the hydroisomerization cracking catalyst I is higher than that of the hydroisomerization cracking catalyst II, and the mass ratio of the hydroisomerization cracking catalyst I to the hydroisomerization cracking catalyst II is 1:4;
[0066] The model of the supplementary refining catalyst laid at the bottom of the catalyst bed is FF-66, and its usage accounts for 20% of the total mass of the hydroisomerization cracking catalyst I and the hydroisomerization cracking catalyst II;
[0067] (3) Separating and cutting the isomerized dewaxed oil obtained in step (2) to obtain the industrial white oil (distillation range of 290° C.-400° C.), naphtha, and diesel (distillation range of 150-290° C.); all the tail oil with a distillation range greater than 400° C. is recycled to the hydroisomerization cracking reactor.
[0068] The process conditions of each step are shown in Table 2, and the experimental results are shown in Table 3.
[0069] Table 2 Process conditions of each step
[0070]
[0071] Table 3 Experimental results
[0072]
[0073] Example 2
[0074] The method for producing industrial white oil is similar to that of Example 1, except that the mass ratio of hydroisomerization cracking catalyst I to hydroisomerization cracking catalyst II is 1:2.
[0075] The process conditions of each step are shown in Table 2, and the experimental results are shown in Table 4.
[0076] Table 4 Experimental results
[0077]
[0078] Example 3
[0079] The method for producing industrial white oil is similar to that of Example 1, except that the mass ratio of hydroisomerization cracking catalyst I to hydroisomerization cracking catalyst II is 1:1.
[0080] The process conditions of each step are shown in Table 2, and the experimental results are shown in Table 5.
[0081] Table 5 Experimental results
[0082]
[0083] Example 4
[0084] The method for producing industrial white oil is similar to that of Example 1, except that the amount of the supplementary refining catalyst used accounts for 10% of the total mass of the hydroisomerization cracking catalyst I and the hydroisomerization cracking catalyst II.
[0085] The process conditions of each step are shown in Table 2, and the experimental results are shown in Table 6.
[0086] Table 6 Experimental results
[0087]
[0088] Comparative Example 1
[0089] The method for producing industrial white oil is similar to that of Example 1, except that: in the hydroisomerization cracking reactor of step (2), the mass ratio of hydroisomerization cracking catalyst I to hydroisomerization cracking catalyst II is 2:1; and the amount of supplementary refining catalyst used accounts for 4% of the total mass of hydroisomerization cracking catalyst I and hydroisomerization cracking catalyst II.
[0090] The process conditions of each step are shown in Table 7, and the experimental results are shown in Table 8.
[0091] Table 7 Process conditions of each step
[0092]
[0093] Table 8 Experimental results
[0094]
[0095] Comparative Example 2
[0096] Method for producing industrial white oil, with reference to Figure 1 The flowchart shown includes the following steps:
[0097] (1) A hydrorefining catalyst is placed in a hydrorefining reactor, and Fischer-Tropsch wax is hydrorefined. The properties of the raw materials are shown in Table 1. Deoxygenation and olefin hydrogenation saturation occur to obtain refined wax oil. The sulfur content of the refined wax oil is less than 1 ppm, and the nitrogen content is 0 ppm.
[0098] The hydrotreating catalyst is Ni-Mo series, model FF-66;
[0099] (2) laying a hydroisomerization cracking catalyst 1 and a supplementary refining catalyst in a hydroisomerization cracking reactor from top to bottom, introducing the refined wax oil obtained in step (1) into contact with the hydroisomerization cracking catalyst and the supplementary refining catalyst laid in the catalyst bed layer in sequence and reacting to obtain an isomerized dewaxed oil; wherein:
[0100] The hydroisomerization cracking catalyst I is prepared according to the method disclosed in patent CN107661756A; the mass fraction of NiO in the hydroisomerization cracking catalyst I (based on the total weight) is 6%, the mass fraction of WO3 is 24%, the mass fraction of amorphous silicon aluminum is 60%, and the mass fraction of aluminum oxide is 10%;
[0101] The model of the supplementary refining catalyst laid at the bottom of the catalyst bed is FF-66, and its usage accounts for 4% of the mass of the hydroisomerization cracking catalyst 1;
[0102] (3) Separating and cutting the isomerized dewaxed oil obtained in step (2) to obtain the industrial white oil (with a distillation range of 290° C.-400° C.); all the tail oil with a distillation range greater than 400° C. is recycled to the hydroisomerization cracking reactor.
[0103] The process conditions of each step are shown in Table 9, and the experimental results are shown in Table 10.
[0104] Table 9 Process conditions of each step
[0105]
[0106]
[0107] Table 10 Experimental results
[0108]
[0109] Comparative Example 3
[0110] Method for producing industrial white oil, with reference to Figure 1 The flowchart shown includes the following steps:
[0111] (1) A hydrorefining catalyst is placed in a hydrorefining reactor, and Fischer-Tropsch wax is hydrorefined. The properties of the raw materials are shown in Table 1. Deoxygenation and olefin hydrogenation saturation occur to obtain refined wax oil. The sulfur content of the refined wax oil is less than 1 ppm, and the nitrogen content is 0 ppm.
[0112] The hydrotreating catalyst is Ni-Mo series, model FF-66;
[0113] (2) laying a hydroisomerization cracking catalyst II and a supplementary refining catalyst in a hydroisomerization cracking reactor from top to bottom, introducing the refined wax oil obtained in step (1) into contact with the hydroisomerization cracking catalyst and the supplementary refining catalyst laid in the catalyst bed layer in sequence and reacting to obtain an isomerized dewaxed oil; wherein:
[0114] The mass fraction of NiO in the hydroisomerization cracking catalyst II (based on the total weight) is 6%, the mass fraction of WO3 is 28%, the mass fraction of amorphous silicon aluminum is 40%, and the mass fraction of aluminum oxide is 26%;
[0115] The model of the supplementary refining catalyst laid at the bottom of the catalyst bed is FF-66, and its usage accounts for 4% of the total mass of the hydroisomerization cracking catalyst II;
[0116] (3) Separating and cutting the isomerized dewaxed oil obtained in step (2) to obtain the industrial white oil (with a distillation range of 290° C.-400° C.); all the tail oil with a distillation range greater than 400° C. is recycled to the hydroisomerization cracking reactor.
[0117] The process conditions of each step are shown in Table 11, and the experimental results are shown in Table 12.
[0118] Table 11 Process conditions of each step
[0119]
[0120] Table 12 Experimental results
[0121]
[0122] Comparative Example 4
[0123] The method for producing industrial white oil is similar to that of Example 1, except that in the hydroisomerization cracking reactor of step (2), the mass ratio of hydroisomerization cracking catalyst I to hydroisomerization cracking catalyst II is 2:1, and no supplementary refined catalyst agent is loaded.
[0124] The process conditions of each step are shown in Table 13, and the experimental results are shown in Table 14.
[0125] Table 13 Process conditions of each step
[0126]
[0127] Table 14 Experimental results
[0128]
[0129] The experimental results of the above embodiments show that by combining and grading hydroisomerization cracking catalysts and supplementary refining catalysts of different activities, the temperature rise of the cracking reaction can be controlled, so that the reaction temperature is evenly distributed, and the Saybolt color (number) of the produced industrial white oil is not less than +30, the aromatics content is less than 0.1%, and the white oil yield is not less than 53%.
[0130] The embodiments of the present invention have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Many modifications and changes will be apparent to those skilled in the art without departing from the scope and spirit of the described embodiments.
Claims
1. A method for producing industrial white oil, It is characterized in that The steps include: (1) In a hydrotreating reactor, the raw wax oil is subjected to a hydrotreating treatment to undergo deoxygenation and olefin hydrogenation saturation to obtain a refined wax oil; (2) in a hydroisomerization cracking reactor, the refined wax oil is sequentially contacted with a hydroisomerization cracking catalyst and a supplementary refining catalyst laid on a catalyst bed and reacted to obtain isomerized dewaxed oil; wherein: The hydroisomerization cracking catalyst is a combination of hydroisomerization cracking catalyst I and hydroisomerization cracking catalyst II, which is laid on the upper part of the catalyst bed; the supplementary refining catalyst is laid on the lower part of the catalyst bed; (3) separating and cutting the isomerized dewaxed oil to obtain the industrial white oil (with a distillation range of 290° C. to 400° C.); optionally, part or all of the tail oil with a distillation range greater than 400° C. is recycled to the hydroisomerization cracking reactor; The hydroisomerization cracking catalyst I and the hydroisomerization cracking catalyst II are both non-precious metal catalysts, and the catalyst carrier does not contain molecular sieves but contains amorphous silicon aluminum; The mass ratio of hydroisomerization cracking catalyst I to hydroisomerization cracking catalyst II is 1:4-1:
1.
2. The method according to claim 1, It is characterized in that The hydroisomerization cracking catalyst I comprises a carrier and an active component; the carrier is alumina and amorphous silica-alumina; the active component is at least one metal element selected from Group VIII and at least one metal element selected from Group VIB; Based on the total weight of the hydroisomerization cracking catalyst I, the following components are included: The content of amorphous silicon aluminum is 55-65wt%, The content of aluminum oxide is 5-10wt%, The content of metal elements of Group VIII in terms of oxide is 1-10 wt%, The content of the metal elements of Group VIB in terms of oxide is 15-25 wt %.
3. The method according to claim 1, It is characterized in that The hydroisomerization cracking catalyst II comprises a carrier and an active component; the carrier is alumina and amorphous silica-alumina; the active component is at least one metal element selected from Group VIII and at least one metal element selected from Group VIB; Based on the total weight of the hydroisomerization cracking catalyst II, the following components are included: Amorphous silicon aluminum content is 35-50wt%, The content of aluminum oxide is 10-30wt%, The content of metal elements of Group VIII in terms of oxide is 1-10 wt%, The content of the metal elements of Group VIB in terms of oxide is 20-40 wt%.
4. The method according to claim 2 or 3, It is characterized in that The metal element of Group VIB is molybdenum and / or tungsten, and the metal element of Group VIII is cobalt and / or nickel.
5. The method according to claim 1, It is characterized in that In step (1), the catalyst used in the hydrofining treatment is a sulfided catalyst; The reaction conditions of the hydrofining treatment include: a reaction temperature of 200-350°C, preferably 200-300°C, a reaction pressure of 2-12MPa, preferably 6-10MPa, and a liquid hourly volume space velocity of 0.5-10h -1 , preferably 0.5-2h -1 .
6. The method according to claim 1, It is characterized in that In step (1), the raw wax oil is a hydrocarbon oil having a wax content greater than or equal to 40wt% and a drop melting point greater than or equal to 50°C, which is selected from one or more of petroleum-based hydrocracking tail oil, Fischer-Tropsch synthetic wax oil, hydrotreated wax oil, vacuum wax oil and coking wax oil, preferably Fischer-Tropsch synthetic wax oil.
7. The method according to claim 1, It is characterized in that In step (1), the sulfur content of the refined wax oil is less than or equal to 10 ppm, and the nitrogen content is less than or equal to 5 ppm.
8. The method according to claim 1, It is characterized in that In step (2), the supplementary refined catalyst is a sulfided catalyst; In step (2), the amount of the supplementary refining catalyst used is 5-25% of the total mass of the hydroisomerization cracking catalyst I and the hydroisomerization cracking catalyst II.
9. The method according to claim 1, It is characterized in that In step (2), in the hydroisomerization cracking reaction zone, the single-pass conversion rate of the fraction with a temperature of >390°C is controlled to be 20 to 70%, preferably 30 to 60%.
10. The method according to claim 1, It is characterized in that In step (2), the hydroisomerization cracking reaction conditions include: reaction temperature of 320-370°C, preferably 330-350°C, reaction pressure of 5-12MPa, preferably 6-10MPa, liquid hourly volume space velocity of 0.5-10h -1 , preferably 0.5-2h -1 .
Citation Information
Patent Citations
Method for producing white oil
CN103695028A
Hydrocracking method for producing crude mineral oil
CN109722292A
A flexible sequence reversed hydrocracking process
CN109988606A
Method for producing crude white oil
CN110616084A
Two-stage hydrocracking method for increasing yield of industrial white oil
CN116064083A