Preparation method of microbial immobilization carrier
Patent Information
- Application Number
- CN202411088687.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-08
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of carrier materials, and in particular to a method for preparing a microorganism immobilization carrier. Background Art
[0002] Daily agricultural and forestry production generates a large amount of waste biomass materials. In the sewage treatment process, iron-containing flocculants are often added, which will produce a large amount of iron-containing flocculation precipitation waste. In addition, a large amount of waste river and lake silt will be generated during river dredging. The treatment of these wastes also requires a lot of resources or energy.
[0003] When sewage treatment plants use iron-containing flocculants for sewage flocculation and sedimentation, a large amount of iron-containing flocculation sedimentation sludge is produced in the sedimentation tank. The sludge may contain pathogens and other components produced in the sewage treatment process, and the abandoned river and lake sludge formed by river dredging may also contain various pathogens, microorganisms and other components. Sewage treatment plant sludge and river and lake sludge are usually dehydrated and transported to landfills as waste or treated by incineration before landfill. The cost of discarding large amounts of sludge and river and lake sludge is relatively high, and the recycling of waste materials is difficult.
[0004] If these waste materials can be recycled and utilized as resources, the cost of waste treatment and disposal can be greatly saved, and even waste can be turned into treasure. Summary of the invention
[0005] The purpose of the present invention is to provide a method for preparing a microorganism immobilization carrier material to realize resource utilization of waste.
[0006] To achieve the above object, the present invention provides a method for preparing a microorganism immobilization carrier, comprising the following steps:
[0007] (1) carbonizing and crushing waste biomass materials, wherein the waste biomass materials are selected from one or more of reed stalks, straw, and wood chips;
[0008] (2) crushing the iron-containing material, mixing it with the carbonized and crushed waste biomass material, and heating it at a high temperature of 600-950° C., wherein the iron-containing material is selected from one or more of waste ore containing iron oxide, slag containing iron oxide, and iron-containing precipitate produced by water treatment;
[0009] (3) drying river and lake silt to obtain a moisture content of 30-60%, wherein the river and lake silt is selected from silt containing organic matter generated during the process of river and lake dredging and management;
[0010] (4) The mixed material obtained in step (2) after high temperature heating is mixed with the dried river and lake silt and auxiliary additives, and then subjected to stabilization and solidification treatment, and heated to 200-800° C. to form the microorganism immobilization carrier material.
[0011] Preferably, the carbonization temperature in step (1) is 600-950°C.
[0012] Preferably, in step (2), before the iron-containing material is crushed, the step also includes heating and dehydrating the iron-containing material.
[0013] Preferably, the temperature of the heating dehydration is 300-400°C.
[0014] Preferably, the auxiliary additives described in step (4) include: a pore-forming agent and a binder; the pore-forming agent is selected from one or more of calcium carbonate, magnesium carbonate, and ammonium bicarbonate; and the binder is selected from cement or resin.
[0015] Preferably, the usage ratio of the waste biomass material, iron-containing material, river and lake silt and auxiliary additives is (1-10):(1-10):(2-20):(0.5-2).
[0016] Based on the above technical solution, the advantages of the present invention are:
[0017] The preparation method of the microorganism immobilization carrier material of the present invention uses waste biomass materials, waste iron-containing materials, river and lake sludge and other wastes as raw materials to prepare the microorganism immobilization carrier material, has simple conditions, and realizes the resource utilization of waste. DETAILED DESCRIPTION
[0018] The technical solution of the present invention is further described in detail below through embodiments.
[0019] The invention provides a method for preparing a microorganism immobilization carrier material. The raw materials of the microorganism immobilization carrier material include waste biomass materials, iron-containing materials and river and lake sludge.
[0020] The waste biomass material described in the present invention refers to plant waste biomass, which refers to organic matter rich in cellulose, hemicellulose or lignin with low recycling value formed by photosynthesis of green plants. This is a conventional material and the present invention will not be elaborated here.
[0021] The waste biomass material in the present invention is carbonized at high temperature to generate carbon material. On the one hand, it is used to reduce the iron oxide in the iron-containing material after being mixed with the iron-containing material and heated. On the other hand, it can generate iron-carbon material with the reduced iron. In some embodiments of the present invention, the waste biomass material is selected from one or more of reed stalks, straw, and sawdust. Those skilled in the art can select according to the situation of the waste biomass material near the production site, and the present invention is not limited here.
[0022] The iron-containing material described in the present invention is mainly waste material containing iron oxide or iron hydroxide components. In some embodiments of the present invention, the iron-containing material is selected from one or more of waste ores containing iron oxide, slag containing iron oxide and iron-containing precipitates produced by water treatment; wherein the iron-containing precipitates produced by water treatment can be iron-containing precipitates produced after a water plant uses an iron-containing flocculant.
[0023] In the present invention, the iron-containing material is reduced by the carbonized waste biomass material to generate an iron-carbon material, which can be directly used to degrade pollutants in water bodies. The present invention uses waste materials to prepare the iron-carbon material, thereby realizing waste utilization. Those skilled in the art can select a suitable iron-containing material according to actual conditions, and the present invention is not limited thereto.
[0024] The river and lake silt described in the present invention is mainly silt deposited at the bottom of rivers or lakes and does not contain heavy metals and toxic components. The river and lake silt contains a lot of organic matter and will generate a large amount of gas at high temperature, which can reduce the amount of pore-forming agent used.
[0025] Specifically, the present invention provides a method for preparing a microorganism immobilization carrier material, comprising the following steps:
[0026] (1) carbonizing and crushing waste biomass materials to generate carbon materials;
[0027] (2) crushing the iron-containing material, mixing it with the carbonized and crushed waste biomass material, and heating it at a high temperature of 600-950° C., so that the carbon material generated by the waste biomass reacts with the iron oxide in the iron-containing material to generate an iron-carbon material;
[0028] (3) Drying river and lake silt to reduce its moisture content to 30%-60%;
[0029] (4) The mixed material obtained in step (2) after high temperature heating is mixed with the dried river and lake silt and auxiliary additives, and then subjected to stabilization and solidification treatment, and heated to 200-800° C. to form the microorganism immobilization carrier material.
[0030] In some embodiments of the present invention, the carbonization temperature in step (1) is 600-950°C.
[0031] In the present invention, the carbonized waste biomass material is crushed, which is beneficial for fully mixing it with the crushed iron-containing material and facilitating subsequent reactions.
[0032] In some embodiments of the present invention, in step (2), before the iron-containing material is crushed, the iron-containing material is also heated and dehydrated; especially when the iron-containing precipitate is produced by water treatment, since it contains a large amount of iron hydroxide, heating and dehydration can first generate iron oxide, so that the subsequent reduction reaction is more complete.
[0033] In some embodiments of the present invention, the temperature of the heating dehydration is 300-400°C.
[0034] In some embodiments of the present invention, in order to facilitate operation, the carbonized waste biomass can be cooled before being mixed with the crushed iron-containing material; the mixed material heated at high temperature can be cooled before being mixed with other materials.
[0035] In some embodiments of the present invention, river and lake silt may be dried by pressing, drying, or natural drying, which are commonly used technical means in the art and are not limited thereto in the present invention.
[0036] In some embodiments of the present invention, the auxiliary additives described in step (4) include: a pore former and a binder; the pore former is selected from one or more of calcium carbonate, magnesium carbonate, and ammonium bicarbonate; the binder is selected from cement or resin; the cement and resin are both commonly used binders in the art, and the present invention will not be described in detail here. In some embodiments of the present invention, the binder accounts for 75%-90% of the total mass of the auxiliary additives, and the pore former accounts for 10-25% of the total mass of the auxiliary additives.
[0037] In some embodiments of the present invention, the stabilization solidification treatment described in step (4) can be a method such as heat treatment extrusion, water-based molding, etc., which are conventional technical means in the art and are not limited by the present invention.
[0038] In some embodiments of the present invention, the ratio of the waste biomass material, the iron-containing material, the river and lake silt and the auxiliary additive is (1-10): (1-10): (2-20): (0.5-2). When the reaction is carried out using the ratio, a carrier material with a pore size of 0.1-5 mm can be obtained. The carrier material with this pore size can be conducive to the adsorption of microorganisms, increase the efficiency of microorganism immobilization, increase the specific surface area of the material, and increase the contact efficiency between the carrier material and the water body, thereby increasing the contact area between the microorganisms fixed in the carrier material and the water body, thereby increasing the improvement efficiency of the immobilized microorganisms on the water body.
[0039] In some embodiments of the present invention, the waste biomass material includes at least one of reed stalks, straw, and wood chips; the iron-containing material includes at least one of waste ore containing iron oxide, slag containing iron oxide, and iron-containing precipitates produced by water treatment.
[0040] The microorganism immobilization carrier material prepared by the method described in the present invention is a granular material, and forms porous particles after high-temperature treatment at 200-800°C; the porous particles can fix specific microorganisms in the gaps of the particles through adsorption, cross-linking, etc., so as to be applied to in-situ treatment of water bodies.
[0041] River and lake silt has natural biological affinity, and the porous material formed can more easily fix microorganisms through adsorption and other means. The carbon-containing and iron-containing components formed in the material can form a micro-battery effect under specific conditions. When this material is put into natural water bodies, on the one hand, it can slowly release microorganisms and act as a carrier for microbial reproduction to promote microorganisms to improve water bodies. On the other hand, the carrier material can use the iron-carbon micro-battery effect at the bottom of natural water bodies to purify the sediment and water bodies.
[0042] The preparation method of the microorganism immobilization carrier material of the present invention uses waste biomass materials, waste iron-containing materials, river and lake sludge and other wastes as raw materials to prepare the microorganism immobilization carrier material, has simple conditions, and realizes the resource utilization of waste.
[0043] Example 1
[0044] Reeds grown on a river beach are used. After they turn yellow and are harvested in autumn, their reed stalks are used as waste biomass materials. The precipitate produced by the use of iron flocculants in the water supply plant around the river is used as the iron-containing material. The silt cleared out during the river management process is used as the river and lake silt material of this application.
[0045] (1) carbonizing the reed stem at 800° C. and then crushing the reed stem;
[0046] (2) dehydrating the iron-containing material at 300° C. to remove organic matter and water in the material and form an iron oxide material;
[0047] (3) mixing the carbonized reed stem and the iron oxide material obtained in step (2) in a mass ratio of 10:3; and heating at a high temperature of 900° C.;
[0048] (4) Dehydrating and drying the riverbed sludge to make the moisture content of the sludge reach about 50%;
[0049] (5) mixing the river silt after airing with the carbonized reed stem and iron oxide mixed material heated at high temperature in step (3) at a mass ratio of 2:1; and adding 1 / 20 of the total mass of the mixed auxiliary additives and stirring and mixing;
[0050] (6) The mixed material obtained in step (5) is subjected to a stabilizing solidification treatment and heated to 600° C. to form a porous granular material, which is the microorganism immobilization carrier material of the present application.
[0051] After the microorganism immobilization carrier material obtained in Example 1 is soaked in a beneficial EM composite microbial bacterial solution, an immobilized microbial material with adsorbed microorganisms is obtained; the immobilized microbial material particles can be scattered into a water body, and can be deposited at the bottom of the water body, continuously releasing beneficial EM composite microorganisms, thereby achieving a continuous improvement effect on the bottom mud.
[0052] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, ordinary technicians in the field should understand that the specific implementation methods of the present invention can still be modified or some technical features can be replaced by equivalents without departing from the spirit of the technical solution of the present invention, which should be included in the scope of the technical solution for protection of the present invention.
Claims
1. A method for preparing a microorganism immobilization carrier, characterized in that: The steps include: (1) carbonizing and crushing waste biomass materials, wherein the waste biomass materials are selected from one or more of reed stalks, straw, and wood chips; (2) crushing the iron-containing material, mixing it with the carbonized and crushed waste biomass material, and heating it at a high temperature of 600-950° C., wherein the iron-containing material is selected from one or more of waste ore containing iron oxide, slag containing iron oxide, and iron-containing precipitate produced by water treatment; (3) drying river and lake silt to obtain a moisture content of 30-60%, wherein the river and lake silt is selected from silt containing organic matter generated during the process of river and lake dredging and management; (4) The mixed material obtained in step (2) after high temperature heating is mixed with the dried river and lake silt and auxiliary additives, and then subjected to stabilization and solidification treatment, and heated to 200-800° C. to form the microorganism immobilization carrier material.
2. The preparation method according to claim 1, characterized in that: The carbonization temperature in step (1) is 600-950°C.
3. The preparation method according to claim 1, characterized in that: In step (2), before the iron-containing material is crushed, the step of heating and dehydrating the iron-containing material is also included.
4. The preparation method according to claim 1, characterized in that: The auxiliary additives described in step (4) include pore-forming agents and binders; the pore-forming agent is selected from one or more of calcium carbonate, magnesium carbonate, and ammonium bicarbonate; and the binder is selected from cement or resin.
5. The preparation method according to claim 1, characterized in that: The weight ratio of the waste biomass material, iron-containing material, river and lake silt and auxiliary additives is (1-10):(1-10):(2-20):(0.5-2).