Energy-saving and environment-friendly heat treatment process for 20Cr13 calendering roller

By adopting step-down cooling quenching and speed-limiting heating methods in the 20Cr13 calendering roller heat treatment process, combining low-concentration water-based liquid cooling and high-temperature tempering, the problem that the concentration adjustment of water-based liquid in the prior art cannot meet the cooling conditions of the calendering roller in the prior art is solved. , realizes an efficient and environmentally friendly heat treatment process, and improves product quality and delivery rate.

CN118910388APending Publication Date: 2024-11-08HENAN ZHONGYUAN SPECIAL STEEL EQUIP MFG CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411059587.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-05
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the existing 20Cr13 calendering roller heat treatment process, the adjustment of the water-based liquid concentration cannot meet the quenching cooling conditions of the calendering roller heat treatment, resulting in slow production progress, difficult to meet the delivery progress, and there are problems of high consumption and environmental pollution.

Method used

The heat treatment process of step-down cooling and quenching and speed-limiting heating is adopted. The heating rate of 10℃/h~100℃/h is increased to 1000℃~1040℃, and after insulation, the furnace is cooled to 970℃~990℃, and 6%~ 8.5% low-concentration water-based liquid is quenched and cooled, combined with primary and secondary high-temperature tempering to ensure the stability of carbide particles and the uniformity of hardness.

Benefits of technology

It improves the hardness uniformity and production efficiency of the calendering roller, reduces the consumption of quenching aqueous solution and environmental pollution, improves product quality and delivery rate, and meets market demand.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses an energy-saving and environment-friendly heat treatment process for a 20Cr13 calendering roller, which comprises the following steps: heating to 1000-1040 DEG C in a stepped heating manner, carrying out complete austenitizing, carrying out heat preservation, cooling to 970-990 DEG C along with a furnace, and carrying out heat preservation for a certain time to ensure that carbide particles are dissolved into austenite to stabilize a high-temperature structure; hardening and tempering carbides are prevented from gathering and growing on a grain boundary to influence the on-machine use effect of the calender roll, the thermal stress during quenching is reduced, and the quenching cracking risk of the calender roll is reduced; a low-concentration water base solution with the mass percent concentration of 6%-8.5% is used for quenching cooling, the quenching cooling uniformity and hardness uniformity of the calender roll are improved, the overall-length or total-section hardness deviation is within 15 HB, the overall quality of the calender roll is improved, the production process is efficient and environmentally friendly, consumption of a quenching water solution is reduced, the production cost is reduced, and environmental pollution is reduced; and secondary high-temperature tempering is performed through speed-limiting temperature rise, so that the calender roll has relatively high strength, plasticity and toughness, the service life of the calender roll on a machine is ensured, and the overall quality of the produced calender roll is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of heat treatment of metal materials, and particularly relates to an energy-saving and environmentally friendly heat treatment process for a 20Cr13 calendering roller, which can not only improve the uniformity of quenching cooling and hardness uniformity of a calendering roller, but also keep the full-length or full-section hardness deviation within 15HB, and significantly improve the overall quality of the calendering roller, but also has an efficient and environmentally friendly production process, can reduce the consumption of quenching aqueous solution, reduce production costs and reduce environmental pollution. Background Art

[0002] 2Cr13 material belongs to heat-resistant martensitic stainless steel. After quenching and tempering, it has good corrosion resistance, thermal strength and impact toughness. It has a wide range of uses and is mainly used to manufacture turbine rotors, sleeves, calendering rollers, medical equipment and tableware. At present, when producing this material product, it is mainly used to produce calendering rollers, rotors, valve bodies, round bars and other products. Due to the high Cr alloy content of this material, the Cr alloy range is 12%~14%. In order to avoid quenching cracking of the product during heat treatment production, when producing 20Cr13 calendering rollers, the medium used in conventional heat treatment quenching production is water-based liquid, and its mass percentage concentration is 9%~11.5%. However, due to the need for heat treatment quenching and cooling of other products in the actual production process, the concentration of water-based liquid is adjusted to 6%~8.5%. Therefore, it cannot meet the heat treatment quenching and cooling conditions of the calendering roller, resulting in the calendering roller product cannot be heat treated in time, resulting in slow production progress and difficulty in meeting the delivery schedule. Therefore, in order to break the production bottleneck, a new heat treatment process is urgently needed that can not only ensure product quality, but also meet production needs and improve delivery rate. Summary of the invention

[0003] The purpose of the present invention is to overcome the shortcomings of the prior art and provide an energy-saving and environmentally friendly heat treatment process technology for 20Cr13 calendering rollers. Not only is the production process efficient and environmentally friendly, the consumption of quenching aqueous solution is reduced, the production cost is reduced and environmental pollution is reduced, but also the overall quality of the calendering roller is significantly improved, the full length or full cross-section hardness deviation is within 15HB, the production progress and delivery rate are improved, and the market demand is met.

[0004] In order to achieve the above-mentioned invention object, the present invention adopts the following technical scheme: an energy-saving and environmentally friendly heat treatment process for 20Cr13 calendering roller, characterized in that: the process steps are as follows: Step 1), step cooling quenching: put the calendering roller into a heating furnace with a furnace temperature of ≤500℃, heat it to 600℃~700℃ at a heating rate of 10℃ / h~100℃ / h, keep it warm for 2h~5h, then heat it to 1000℃~1040℃ at a heating rate of 50℃ / h~200℃ / h, keep it warm for 5h~30h, cool it to 970℃~990℃ with the furnace, keep it warm for 0.5h~3h, take it out of the furnace for quenching and cooling, pre-cool it in the air for 180s~230s, then put the calendering roller into The calendering roller is initially cooled in a water-based quenching liquid with a liquid temperature of 30°C to 50°C for 5min to 20min, and the mass percentage concentration of the water-based quenching liquid is 6% to 8.5%. After cooling, the calendering roller is lifted out of the aqueous solution and air-cooled for 30s to 80s. After air-cooling, the calendering roller is placed in the aqueous solution and cooled for 5min to 20min. After cooling, the calendering roller is lifted out of the aqueous solution and air-cooled for 30s to 80s. After air-cooling, the calendering roller is placed in the aqueous solution and cooled for 5min to 20min. After executing step 1), the calendering roller is placed in a heating furnace for a high-temperature tempering. Step 2), primary high-temperature tempering: the furnace temperature is controlled at ≤450°C, and the temperature is raised to 650°C~750°C at a heating rate of 10°C / h~100°C / h. After keeping the temperature for 10h~40h, the roll is taken out of the furnace and air-cooled to room temperature. After the primary high-temperature tempering, the calendering roll is loaded into the heating furnace for secondary high-temperature tempering; Step 3), secondary high temperature tempering: the temperature of the heating furnace is controlled at ≤450℃, and the temperature is increased to 620℃~720℃ at a heating rate of 10℃ / h~100℃ / h. After keeping warm for 10h~40h, take out of the furnace and air cool to room temperature.

[0005] Compared with the prior art, the present invention has the following advantages: 1. Through the step heating method, heat to 1000℃~1040℃ for complete austenitization, cool down to 970℃~990℃ with the furnace after heat preservation, and keep at this temperature for a certain period of time. This method ensures that the carbide particles are fully dissolved in the austenite to stabilize the high-temperature structure, avoids the carbides from aggregating and growing at the grain boundary after quenching and tempering, affecting the use effect of the calendering roller on the machine, and can also reduce the thermal stress during quenching and reduce the risk of quenching cracking of the calendering roller; 2. The use of low-concentration water-based liquid with a mass percentage concentration of 6% to 8.5% for quenching and cooling not only improves the uniformity of quenching and cooling and hardness uniformity of the calendering roller, but also significantly improves the overall quality of the calendering roller by keeping the full length or full cross-section hardness deviation within 15HB. In addition, the production process is efficient and environmentally friendly, reducing the consumption of quenching water solution, reducing production costs and reducing environmental pollution; 3. The calendering roller obtains higher strength, plasticity and toughness through secondary high temperature tempering by speed-limited heating, thus ensuring the service life of the calendering roller on the machine. The 20Cr13 calendering roller produced according to the present invention has improved overall quality and meets the market demand. DETAILED DESCRIPTION

[0006] Example 1: A heat treatment process for 20Cr13 calendering roller with energy saving and environmental protection, steel type: 2Cr13, chemical composition: C=0.17%, Si=0.47%, Mn=0.68%, Cr=12.70%, Ni=0.37%, S=0.002%, P=0.016%, Mo=0.11%; specification: Φ465*Φ280*4620mm. The heat treatment process is as follows: Step 1), step cooling quenching: put the calendering roller into a heating furnace with a furnace temperature of 320℃, heat it to 650℃ at a heating rate of 80℃ / h, keep it warm for 2h, then heat it to 1000℃ at a heating rate of 80℃ / h, keep it warm for 5h, cool it to 980℃ with the furnace after keeping it warm, keep it warm for 1h, take it out of the furnace for quenching and cooling, first pre-cool it in the air for 210s, then put the calendering roller into a water-based liquid with a starting liquid temperature of 35℃ and cool it for 8min, the concentration of the water-based liquid is 8.0%, after cooling, hang the calendering roller out of the aqueous solution and air-cool it for 40s, and then put the calendering roller into the aqueous solution and cool it for 6min after air cooling; Step 2) After step 1) is executed, the calendering roll is placed in a heating furnace and subjected to a high-temperature tempering: the furnace temperature is controlled at 215°C, and the temperature is increased to 702°C at a heating rate of 80°C / h. After keeping the temperature for 10 hours, the roll is taken out of the furnace and air-cooled to room temperature; Step 3) After step 2) is executed, the calendering roller is loaded into a heating furnace for secondary high-temperature tempering: the furnace temperature is controlled at 195°C, and the temperature is increased to 680°C at a heating rate of 80°C / h. After keeping the temperature for 10 hours, the roller is taken out of the furnace and air-cooled to room temperature. Table 1 Test results Technical requirements Yield strength ≥440Mpa Tensile strength ≥635Mpa Elongation ≥20% Surface shrinkage ≥50% Impact energy AKU≥63J Surface hardness 200-255HB Grain size ≥ 5 Actual detection 613 795 23.5 62 64 / 70 / 78 217 / 221 / 224 Level 7 After being produced by the energy-saving and environmentally friendly heat treatment process of the 20Cr13 calendering roller of the present invention, the mechanical properties and grain size test results are qualified and meet the technical requirements of customers.

[0007] Example 2: A heat treatment process for 20Cr13 calendering roller with energy saving and environmental protection, steel type: 2Cr13, chemical composition: C=0.17%, Si=0.37%, Mn=0.61%, Cr=12.92%, Ni=0.21%, S=0.002%, P=0.017%, Mo=0.11%, specification: Φ410*Φ230*4100mm. The heat treatment process is as follows: Step 1), step cooling quenching: put the calendering roller into a heating furnace with a furnace temperature of 280℃, heat it to 650℃ at a heating rate of 80℃ / h, keep it warm for 2h, then heat it to 1000℃ at a heating rate of 80℃ / h, keep it warm for 5h, cool it to 980℃ with the furnace after keeping it warm, keep it warm for 1h, take it out of the furnace for quenching and cooling, first pre-cool it in the air for 210s, then put the calendering roller into a water-based liquid with a starting liquid temperature of 38℃ and cool it for 8min, the concentration of the water-based liquid is 8.1%, after cooling, hang the calendering roller out of the aqueous solution and air cool it for 40s, after air cooling, put the calendering roller into the aqueous solution and cool it for 6min, after cooling, hang the calendering roller out of the aqueous solution and air cool it for 40s, after air cooling, put the calendering roller into the aqueous solution and cool it for 6min; Step 2), after step 1) is executed, the calendering roll is loaded into a heating furnace and subjected to a high temperature tempering: the temperature of the heating furnace is controlled at 220°C, and the temperature is increased to 702°C at a heating rate of 80°C / h, and then the roll is taken out of the furnace and air-cooled to room temperature after being kept at this temperature for 10 hours; Step 3), after step 2) is executed, the calendering roller is loaded into the heating furnace and subjected to secondary high-temperature tempering: the temperature of the heating furnace is controlled at 210°C, and the temperature is increased to 680°C at a heating rate of 80°C / h. After keeping the temperature for 10 hours, the roller is taken out of the furnace and air-cooled to room temperature.

[0008] Table 2 Test results Technical requirements Yield strength ≥440Mpa Tensile strength ≥635Mpa Elongation ≥20% Surface shrinkage ≥50% Impact energy AKU≥63J Surface hardness 200-255HB Grain size ≥ 5 Actual detection 618 790 23 61 71 / 72 / 75 218 / 225 / 212 6.5 After the 20Cr13 calendering roller is produced by the energy-saving and environmentally friendly heat treatment process method of the present invention, the mechanical properties and grain size test results are qualified and meet the technical requirements of customers.

Claims

1. A heat treatment process for 20Cr13 calendering roller with energy saving and environmental protection, Features: The specific process steps are as follows: Step 1), step cooling quenching: put the calendering roller into a heating furnace with a furnace temperature of ≤500℃, heat it to 600℃~700℃ at a heating rate of 10℃ / h~100℃ / h, keep it warm for 2h~5h, then heat it to 1000℃~1040℃ at a heating rate of 50℃ / h~200℃ / h, keep it warm for 5h~30h, cool it to 970℃~990℃ with the furnace, keep it warm for 0.5h~3h, take it out of the furnace for quenching and cooling, pre-cool it in the air for 180s~230s, then put the calendering roller into The calendering roller is initially cooled in a water-based quenching liquid with a liquid temperature of 30°C to 50°C for 5min to 20min, and the mass percentage concentration of the water-based quenching liquid is 6% to 8.5%. After cooling, the calendering roller is lifted out of the aqueous solution and air-cooled for 30s to 80s. After air-cooling, the calendering roller is placed in the aqueous solution and cooled for 5min to 20min. After cooling, the calendering roller is lifted out of the aqueous solution and air-cooled for 30s to 80s. After air-cooling, the calendering roller is placed in the aqueous solution and cooled for 5min to 20min. After executing step 1), the calendering roller is placed in a heating furnace for a high-temperature tempering. Step 2), primary high-temperature tempering: the furnace temperature is controlled at ≤450°C, and the temperature is raised to 650°C~750°C at a heating rate of 10°C / h~100°C / h. After keeping the temperature for 10h~40h, the roll is taken out of the furnace and air-cooled to room temperature. After the primary high-temperature tempering, the calendering roll is loaded into the heating furnace for secondary high-temperature tempering; Step 3), secondary high temperature tempering: the temperature of the heating furnace is controlled at ≤450℃, and the temperature is increased to 620℃~720℃ at a heating rate of 10℃ / h~100℃ / h. After keeping warm for 10h~40h, take out of the furnace and air cool to room temperature.

Citation Information

Patent Citations

  • Heat treatment process of large-size 2Cr13 hollow pipe

    CN113999964A

  • Heat treatment process for improving hardness uniformity of total cross section of 20CrNiMo calender roll

    CN115354138A

  • Heat treatment process of 1Cr11MoV roller body for calender

    CN115679044A

  • Heat treatment method for improving low-temperature impact toughness of large 42CrMo steel forgings

    CN116656935A

  • Method for removing internal stress of 1Cr11MoV calender roll

    CN117551845A